A high-density, high-temperature resistant, solid-free saline test solution and its preparation method
By using a combination of composite brine, metal salts, and stabilizers in the test fluid for high-temperature and high-pressure deep oil and gas wells to form a network structure, the problem of density and viscosity fluctuations in the test fluid at high temperatures is solved, density and viscosity stability is achieved, and the risk of wellbore pressure fluctuations and reservoir damage is reduced.
Patent Information
- Application Number
- CN202510623850.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-15
- Publication Date
- 2026-11-17
AI Technical Summary
Existing high-temperature and high-pressure deep oil and gas well test fluids exhibit significant fluctuations in density and viscosity when the temperature rises to 200°C, leading to unstable wellbore pressure and potentially causing blowouts or well leakage, severely damaging the reservoir.
A combination of a complex salt solution, metal salt 1, metal salt 2, and a stabilizer is used to form a network structure through electrostatic interaction and coordination bonds. The stabilizer generates a network structure, which hinders the high-temperature hydrolysis of the complex salt and maintains the stability of viscosity and density.
The density change is less than 0.35% and the viscosity change is less than 2% at 200℃, which significantly improves the high-temperature stability of the test fluid and reduces the risk of reservoir damage.
Smart Images

Figure CN123107640A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of solid-free brine test solution technology for oilfields, and in particular to a high-density, high-temperature resistant solid-free brine test solution and its preparation method. Background Technology
[0002] In the exploration and development of oil and gas resources, there are five main methods to directly obtain formation fluid characteristics and formation parameters: seismic exploration, cuttings logging, coring, electrical logging, and formation testing. Among these, formation testing is the most direct method for obtaining production data and evaluating reservoirs. In my country, formation testing is divided into two types: drilling-in testing, which is called mid-course testing, and testing after casing completion, which is called well completion testing. Both types of testing require running the testing tools into the test section using drill pipe or tubing, then initiating unsteady gauging operations to obtain data such as reservoir production, temperature, and pressure, plotting bottom hole pressure-time curves, and obtaining formation fluid samples.
[0003] Testing fluid is the lifeblood of oil and gas testing and well completion operations. Its performance directly impacts the quality and safety of well completion testing. Primarily used to balance formation pressure, high-density fluids are needed to maintain high well pressure and prevent reservoir fluids from overflowing into the wellbore. With the progress of oilfield exploration and development, newly developed reservoirs are reaching greater depths, leading to increased reservoir temperature and pressure. Consequently, the requirements for testing fluids during oil and gas well completion testing are becoming increasingly stringent. High-density brine testing fluid is currently a research hotspot. It not only possesses superior well-killing capabilities but also avoids the reservoir damage and solids deposition problems associated with conventional testing fluids, thus increasing the success rate of well workover testing.
[0004] Currently, most low-corrosion, low-damage solids-free testing fluids and well-killing fluids in China use inorganic and organic salt systems, with a maximum density of only 1.50 g / cm³. 3 The required density of mud is insufficient to meet the requirements for deep exploration, development, and well control operations in the South China Sea. High-density bromide testing fluid is unusable due to its strong corrosiveness and system instability, while high-density cesium formate testing fluid is prohibitively expensive. This necessitates the use of weighted mud during high-temperature, high-pressure deep testing and well completion. This results in severe reservoir damage, affecting the accuracy of testing in evaluating the producing formation and the post-completion gas well productivity.
[0005] There is an urgent need to research and develop a material with a temperature resistance of over 180℃ and a density of 1.70 g / cm³. 3 The above are low-corrosive and low-damage high-density solid-free organic salt test fluids and kill fluids. Phosphate test fluids have a high density (up to 1.82 g / cm³). 3It is low in cost, low in toxicity, low in reservoir damage, and has good formation compatibility, making it a viable alternative high-density cleaning test fluid during well workover and completion testing in high-temperature oil reservoirs. However, as the temperature rises to 200℃, its density and viscosity fluctuate significantly. A decrease in test fluid density can lead to a drop in wellbore pressure, causing reservoir fluids to flow into the wellbore, potentially resulting in a blowout. Conversely, an increase in test fluid density may lead to an increase in wellbore pressure, potentially causing well leakage and allowing large amounts of test fluid to enter the formation, resulting in severe reservoir damage and increasing the risk of downhole accidents.
[0006] Therefore, there is an urgent need to develop a phosphate test solution that exhibits minimal changes in density and viscosity as the temperature rises to 200°C, and that is low-cost, heat-resistant, and has high density. Summary of the Invention
[0007] In view of the shortcomings of the prior art described above, the purpose of this invention is to provide a high-density, high-temperature resistant, solid-free saline test solution and its preparation method, which solves the problem that the density and viscosity of the test solution fluctuate greatly as the temperature rises to 200°C in the prior art.
[0008] To achieve the above and other related objectives, the present invention is obtained through the following technical solution.
[0009] The first aspect of this invention is to provide a high-density, high-temperature resistant, solid-free saline test solution, the test solution comprising the following raw materials: a composite salt aqueous solution, metal salt 1, metal salt 2, a stabilizer, and a solvent, wherein, by mass percentage of the composite salt aqueous solution, the metal salt comprises 10.01-0.25%, the metal salt 2 comprises 0.1-0.5%, the stabilizer comprises 1-2%, and the solvent comprises 1-2%; the composite salt aqueous solution comprises a composite salt and water, the composite salt being selected from at least one of composite salt 1 or composite salt 2; the composite salt 1 is selected from one or more of sodium monohydrogen phosphate, sodium dihydrogen phosphate, sodium phosphate, potassium phosphate, potassium monohydrogen phosphate, potassium dihydrogen phosphate, sodium chloride, and potassium chloride; the composite salt 2 is selected from one or more of sodium pyrophosphate, potassium pyrophosphate, sodium hexametaphosphate, and sodium tripolyphosphate; the metal salt 1 is selected from one or more of copper chloride or copper sulfate; and the metal salt 2 is selected from one or more of zinc nitrate, zinc chloride, manganese chloride, calcium chloride, and calcium nitrate.
[0010] A second aspect of this invention is to provide a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0011] (1) Mix compound salt 1, compound salt 2 and water to obtain compound salt water;
[0012] (2) Mix metal salt 1, metal salt 2 and solvent to obtain a composite solution;
[0013] (3) Add the composite solution and stabilizer obtained in step (2) to the composite salt water obtained in step (1), stir and mix to obtain a high-density high-temperature resistant solid-free salt water test solution.
[0014] A third aspect of the present invention is to provide the use of the high-density, high-temperature resistant, solid-free brine test fluid as described above in well workover and completion testing in high-pressure deep oil reservoirs at 200°C.
[0015] As described above, the high-density, high-temperature resistant, solid-free saline test solution and its preparation method of the present invention have the following beneficial effects:
[0016] (1) The high-density, high-temperature resistant, solid-free saline test solution of the present invention has a density exceeding 1.75 g / cm³. 3 The density of this test solution is higher than that of the currently prepared test solution. Moreover, after aging at 200℃ for 4 days, the minimum density change is 0.22%, and the minimum viscosity change is 2.0% at 46.93 mPa·s. The density and viscosity are relatively stable at 200℃, and the high temperature resistance is good.
[0017] (2) The high-density, high-temperature resistant, solid-free saline test solution of the present invention is made by adding multiple components such as phosphate composite salt, metal salt 1, metal salt 2, and stabilizer. The multiple components work together to make the viscosity and density of the solution fluctuate less after aging. Attached Figure Description
[0018] Figure 1 The diagram shows the viscosity changes of the high-density, high-temperature resistant, solid-free brine test solution in Examples 1a-1d of this invention.
[0019] Figure 2 The diagram shows the density changes of the high-density, high-temperature resistant, solid-free saline test solution in Examples 1a-1d of this invention.
[0020] Figure 3 The diagram shows the density change of the high-density, high-temperature resistant, solid-free saline test solution in Examples 2a-2c of this invention.
[0021] Figure 4 The diagram shows the viscosity change of the high-density, high-temperature resistant, solid-free saline test solution in Example 3a of the present invention.
[0022] Figure 5 The diagram shows the density changes of the high-density, high-temperature resistant, solid-free saline test solution in Examples 3a-3c of this invention.
[0023] Figure 6 The diagram shows the viscosity and density of the high-density, high-temperature resistant, solid-free saline test solution in Example 4 of this invention. Detailed Implementation
[0024] To make the inventive objectives, technical solutions, and beneficial effects of this invention clearer, the invention will be further described in detail below with reference to embodiments. Those skilled in the art can easily understand other advantages and effects of this invention from the content disclosed in this specification.
[0025] The first aspect of this invention is to provide a high-density, high-temperature resistant, solid-free saline test solution, the test solution comprising the following raw materials: a composite salt aqueous solution, metal salt 1, metal salt 2, a stabilizer, and a solvent, wherein, by mass percentage of the composite salt aqueous solution, the metal salt comprises 10.01-0.25%, the metal salt 2 comprises 0.1-0.5%, the stabilizer comprises 1-2%, and the solvent comprises 1-2%; the composite salt aqueous solution comprises a composite salt and water, the composite salt being selected from at least one of composite salt 1 or composite salt 2; the composite salt 1 is selected from one or more of sodium monohydrogen phosphate, sodium dihydrogen phosphate, sodium phosphate, potassium phosphate, potassium monohydrogen phosphate, potassium dihydrogen phosphate, sodium chloride, and potassium chloride; the composite salt 2 is selected from one or more of sodium pyrophosphate, potassium pyrophosphate, sodium hexametaphosphate, and sodium tripolyphosphate; the metal salt 1 is selected from one or more of copper chloride or copper sulfate; and the metal salt 2 is selected from one or more of zinc nitrate, zinc chloride, manganese chloride, calcium chloride, and calcium nitrate.
[0026] In this invention, the copper salt in metal salt 1 first adsorbs with negatively charged phosphate ions through electrostatic interaction to form a new salt. Under stirring conditions, this new salt system further combines with the lone pairs of oxygen atoms on the phosphate ion surface via empty orbitals of copper ions to form a metal chelate salt. This causes the scattered anions and cations in the high-density, solid-free saline test solution to form a network structure, increasing the overall viscosity and physically binding the migration of phosphate ions. This also prevents high-temperature hydrolysis of the saline solution. Furthermore, it increases the electrostatic repulsion between particles, inhibiting the aggregation of phosphate particles under high-temperature conditions, thus achieving a certain degree of high-temperature stability. Simultaneously, the zinc, manganese, and calcium ions in metal salt 2 can form coordinate bonds with the lone pairs of oxygen and phosphorus ions in the composite salt ions. On one hand, the composite salt and metal salt 1 work together to form a complex network structure, preventing density loss due to high-temperature hydrolysis of the composite salt. On the other hand, the coordinate bonds formed by metal salt 2 are easily broken, ensuring that the overall viscosity of the solution remains unchanged after aging, thus guaranteeing the high-density test solution's temperature resistance.
[0027] In some embodiments of the present invention, the test solution comprises the following raw materials by weight percentage as a percentage of the composite salt aqueous solution: composite salt aqueous solution, 10.01-0.15% metal salt, 20.1-0.2% metal salt, 1-1.5% stabilizer, and 1-2% solvent.
[0028] In some embodiments of the present invention, the test solution comprises the following raw materials by weight percentage as a percentage of the composite salt aqueous solution: composite salt aqueous solution, 10.15-0.25% metal salt, 20.2-0.5% metal salt, 1.5-2% stabilizer, and 1-2% solvent.
[0029] In some embodiments of the present invention, the test solution comprises the following raw materials by weight percentage as a percentage of the composite salt aqueous solution: composite salt aqueous solution, 10.25% metal salt, 20.5% metal salt, 2% stabilizer, and 1.7% solvent.
[0030] In some embodiments of the present invention, the test solution comprises the following raw materials by weight percentage as a percentage of the composite salt aqueous solution: composite salt aqueous solution, 10.01% metal salt, 20.1% metal salt, 1% stabilizer, and 1.7% solvent.
[0031] In some embodiments of the present invention, the stabilizer is polyethyleneimine. The present invention does not specifically limit the source of polyethyleneimine; commercially available polyethyleneimine products commonly used by those skilled in the art can be used. Specifically, the weight-average molecular weight of the polyethyleneimine is 70,000. The cations in the polyethyleneimine molecule combine with the anions in the complex salt to form a network structure, wherein the stabilizer molecule acts as the main chain and the complex salt molecule acts as the branch chain. The generated network structure simultaneously forms a multi-level network structure under the electrostatic and coordination effects of metal salt 1 and metal salt 2, which can further hinder the high-temperature hydrolysis of the complex salt, and at the same time prevent anions such as phosphate and hydroxide from combining with cations such as copper, zinc, and manganese ions to form precipitates, thereby ensuring the viscosity and density stability of the system.
[0032] During the experiments, the inventors also discovered that when only one type of metal salt 2, such as zinc nitrate, zinc chloride, manganese chloride, calcium chloride, or calcium nitrate, is used, the high-density test solution is prone to solid precipitation, and the density decreases after aging, while the viscosity fluctuates significantly with aging time. This refers to the case where only metal salt 2 is added, without adding metal salt 1.
[0033] Through extensive experimentation, the inventor discovered:
[0034] When metal salt 1 and metal salt 2 are added simultaneously, the temperature resistance is better when the concentration of metal salt 1 is between 0.01% and 0.25%, and performance will decrease if the concentration is below or above this range; the temperature resistance is better when the concentration of metal salt 2 is between 0.1% and 0.5%, and density will decrease if the concentration is below or above this range.
[0035] When only metal salt 1 is added, the viscosity of the test solution changes by a maximum of 17.15% when the concentration of metal salt 1 is between 0.01% and 0.25%.
[0036] When metal salt 1 and metal salt 2 are added simultaneously, and the concentration of metal salt 1 is between 0.01% and 0.25%, and the concentration of metal salt 2 is between 0.1% and 0.5%, the viscosity change range of the test solution is less than or equal to 6.9%.
[0037] When the concentration of metal salt 2 is 0% to 0.1%, the viscosity of the test solution varies from 73.2% to 177.57% (177.57% is the viscosity change of the composite salt test solution without the addition of metal salt 1, metal salt 2 and stabilizer);
[0038] When only metal salt 1 is added, and the concentration of metal salt 1 is greater than 0.25%, the viscosity of the test solution changes by more than 50%.
[0039] When only metal salt 2 is added, the viscosity of the test solution changes by more than 45.6% when the concentration of metal salt 2 is greater than 0.5%.
[0040] In some embodiments of the present invention, the solvent is water.
[0041] In some embodiments of the present invention, the ratio of compound salt g to water ml in the compound salt aqueous solution is 180-190:100.
[0042] In some embodiments of the present invention, the composite salt is composed of composite salt 1 and composite salt 2 in a mass ratio of 1-3:2-3. Specifically, the mass ratio of composite salt 1 and composite salt 2 can be 1:2, 1:3, or 3:2.
[0043] In some embodiments of the present invention, the density of the test solution is 1.70-1.82 g / cm³. 3 Specifically, the density of the test solution can be 1.70-1.75 g / cm³. 3 1.75-1.82 g / cm³ 3 Typical but not limiting, for example, 1.70 g / cm³. 3 1.75g / cm 3 1.82g / cm 3 .
[0044] In some embodiments of the present invention, the test solution prepared in step (3) after aging at 200°C for 96 hours has a density change rate of <0.35% and a viscosity change rate of ≤2%.
[0045] A second aspect of this invention is to provide a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0046] (1) Mix compound salt 1, compound salt 2 and water to obtain compound salt water;
[0047] (2) Mix metal salt 1, metal salt 2 and solvent to obtain a composite solution;
[0048] (3) Add the composite solution and stabilizer obtained in step (2) to the composite salt water obtained in step (1), stir and mix to obtain a high-density high-temperature resistant solid-free salt water test solution.
[0049] In some embodiments of the present invention, the mixing time in step (1) is 10-30 hours. Specifically, the mixing time can be 10-20 hours or 20-30 hours; typically, but not limitingly, it is 10 hours, 20 hours, or 30 hours.
[0050] In some embodiments of the present invention, the composite saline solution in step (1) is clear and transparent.
[0051] In some embodiments of the present invention, the mixing time in step (2) is 25-40 min. Specifically, the mixing time can be 25-30 min, 30-40 min; typically, but not limitingly, it is 25 min, 30 min, or 40 min.
[0052] In some embodiments of the present invention, the mixing time in step (3) is 4-6 hours.
[0053] In some embodiments of the present invention, the density of the test solution prepared in step (3) is 1.70-1.82 g / cm³. 3 .
[0054] In some embodiments of the present invention, the test solution prepared in step (3) after being aged at 200°C for 96 hours has a density change rate of <0.35% and a viscosity change rate of ≤2%.
[0055] A third aspect of the present invention is to provide the use of the high-density, high-temperature resistant, solid-free brine test fluid as described above in well workover and completion testing in high-pressure deep oil reservoirs at 200°C.
[0056] The present invention will be further illustrated by the following examples, but these examples do not limit the scope of the invention.
[0057] When numerical ranges are given in the embodiments, it should be understood that, unless otherwise stated in the present invention, both endpoints of each numerical range and any value between the two endpoints may be selected. Unless otherwise defined, all technical and scientific terms used in this invention have the same meaning as commonly understood by one of ordinary skill in the art. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. All reagents or instruments whose manufacturers are not specified are conventional products that can be purchased commercially. In addition to the specific methods, equipment, and materials used in the embodiments, based on the knowledge of the prior art possessed by one of ordinary skill in the art and the description of this invention, any prior art methods, equipment, and materials similar to or equivalent to those described, used, and materials in the embodiments of this invention may be used to implement this invention.
[0058] The following examples and embodiments use the following methods to test the high-temperature resistance of the test solution:
[0059] Take 100 ml of the high-density, high-temperature resistant, solid-free saline test solution prepared below and place it in a high-temperature, high-pressure aging reactor. After sealing the reactor, place it in an electrically heated constant-temperature drying oven and statically age it at 200℃. Every 24 hours, take out 20 ml of sample and test the viscosity and density of the aged test solution using a viscometer and a specific gravity bottle, respectively. The results of the density change rate and viscosity change rate are as follows: Figure 1-5 As shown. The formulas for the rate of change of density and the rate of change of viscosity are as follows:
[0060] Density change rate = |Pre-aging density - Density after different aging times| / Pre-aging density * 100%
[0061] Viscosity change rate = |Viscosity before aging - Viscosity after different aging times| / Viscosity before aging * 100%
[0062] Among them, the density before aging is the density before aging; the density after different aging times is the density after aging for 24h, 48h, 72h, and 96h respectively.
[0063] The viscosity before aging is the viscosity before aging; the viscosity after different aging times is the viscosity after aging for 24h, 48h, 72h, and 96h respectively.
[0064] The following examples and embodiments use the following methods to test the corrosion and damage properties of the test solution:
[0065] Corrosion performance testing method: weight loss method, which calculates the amount of mass reduction of a steel specimen (P110 steel) after immersion in the test solution for a certain period of time at a certain temperature.
[0066] Damage performance evaluation method: Core permeability recovery rate evaluation; The damage of the test fluid is evaluated by measuring the permeability recovery rate of the test fluid before and after passing through the saturated formation water core.
[0067] Example
[0068] Example 1
[0069] Example 1a
[0070] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0071] (1) Mix 100g potassium phosphate, 80g sodium hexametaphosphate and 100ml water for 24 hours to disperse evenly to obtain a composite salt solution; the composite salt solution is clear and transparent.
[0072] (2) Mix 0.25g copper chloride, 0.35g zinc chloride and 5ml water for 30min to disperse evenly and obtain a composite solution;
[0073] (3) Add the composite solution obtained in step (2) and 2.8 g of stabilizer to the composite salt solution obtained in step (1), stir, and obtain a solution with a density of 1.802 g / cm³. 3 A high-density, high-temperature resistant, solid-free saline test solution with a viscosity of 46.88 mPa·s. The stabilizer is polyethyleneimine.
[0074] The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density change rate and viscosity change rate of the test solution were measured. The viscosity change rate is as follows: Figure 1 As shown in Table 1. (Through) Figure 1 As shown in Table 1, the high-density, high-temperature resistant, solid-free saline solution prepared in Example 1 exhibits minimal viscosity fluctuation during aging at 200°C for 96 hours, with a maximum viscosity change rate of only 1.3%. The high-density, high-temperature resistant, solid-free saline solution prepared in Example 1 demonstrates superior high-temperature resistance and exhibits minimal viscosity fluctuation. The density change rate is shown in Table 2. Figure 2 As shown, the density change rate of the test liquid after aging for 96 hours was 0.22%.
[0075] Example 1b: Only compound salt added
[0076] This embodiment provides a method for preparing a solid-free saline test solution. The difference from Embodiment 1 is that it only includes step (1), which is as follows: 100g of potassium phosphate, 80g of sodium hexametaphosphate, and 100ml of water are mixed and dispersed evenly for 24 hours to obtain a solution with a density of 1.802g / cm³. 3A high-density, high-temperature resistant, solid-free brine test solution with a viscosity of 42.18 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the test solution were measured. The viscosity change rates are shown in Table 1 and... Figure 1 As shown, the viscosity change rate after aging can reach a maximum of 177.57%; the density change rate is shown in Table 2 and... Figure 2 As shown, the density change rate reached a maximum of 5.83%.
[0077] Example 1c did not include metal salt 2 and stabilizer; instead, it included a composite salt plus metal salt 1.
[0078] This embodiment provides a method for preparing a solid-free saline test solution. The difference from Example 1 is that metal salt 2 and a stabilizer are not added. Specifically, 100g of potassium phosphate, 80g of sodium hexametaphosphate, and 100ml of water are mixed and dispersed evenly for 24 hours to obtain a composite saline solution. Then, 0.25g of copper chloride is dissolved in 5ml of water and stirred, followed by mixing with the composite saline solution and stirring for 30 minutes to obtain a density of 1.799g / cm³. 3 A high-density, high-temperature resistant, solid-free brine test solution with a viscosity of 48.52 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the test solution were measured. The viscosity change rates are shown in Table 1 and... Figure 1 As shown, the viscosity change rate is 4.49%, and the density change rate is as follows: Figure 2 As shown in Table 2, the density change rate is 0.43%.
[0079] Example 1d: No stabilizer was added; the mixture consisted of a complex salt + metal salt 1 + metal salt 2.
[0080] This embodiment provides a method for preparing a solid-free saline test solution, which differs from Example 1 in that no stabilizer is added. Specifically, 100g of potassium phosphate, 80g of sodium hexametaphosphate, and 100ml of water are mixed and dispersed evenly for 24 hours to obtain a composite saline solution; the composite saline solution is clear and transparent. Then, 0.25g of copper chloride, 0.35g of zinc chloride, and 5ml of water are mixed and dispersed evenly for 30 minutes to obtain a solution with a density of 1.801g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution with a viscosity of 49.41 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the solution were measured. The viscosity change rate is shown in the figure below. Figure 1 As shown in Table 1, the viscosity change rate after 96 hours was 6.90%, and the density change rate was as follows: Figure 2 As shown in Table 2, the density change rate is 0.32%.
[0081] Example 1e did not include stabilizer and metal salt 1; instead, it included a complex salt plus metal salt 2.
[0082] This embodiment provides a method for preparing a solid-free saline test solution, which differs from Example 1 in that no stabilizer and metal salt 1 are added. Specifically, 100g of potassium phosphate, 80g of sodium hexametaphosphate, and 100ml of water are mixed and dispersed evenly for 24 hours to obtain a composite saline solution; the composite saline solution is clear and transparent. Then, 0.35g of zinc chloride and 5ml of water are mixed and dispersed evenly for 30 minutes to obtain a solution with a density of 1.808g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution with a viscosity of 50.22 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the solution were measured. The viscosity was 88.67 mPa·s, the change rate was 77.0%, and the density was 1.75 g / cm³. 3 The rate of change was 3.21%.
[0083] Table 1. Viscosity change rate test results of solid-free brine test solution in Examples 1a-1d
[0084]
[0085] Table 2. Test results of density change rate of solid-free saline solution in Example 1a-1d.
[0086]
[0087] Example 1b, i.e., without the addition of metal salt 1 and metal salt 2, showed a corrosion rate of 4-6 mm / a; Example 1c, i.e., with the addition of only metal salt 1, showed a corrosion rate of 0.1-0.3 mm / a; Example 1e, i.e., with the addition of only metal salt 2, showed a corrosion rate of 1.5-2 mm / a; Example 1a, i.e., with the addition of both metal salt 1 and metal salt 2, showed a corrosion rate of 0.1-0.2 mm / a.
[0088] Example 1b, i.e., without the addition of metal salt 1 and metal salt 2 to the test solution, showed a core permeability recovery rate of 15% to 20%; Example 1c, i.e., with only metal salt 1 added, showed a recovery rate of 88% to 95%; Example 1e, i.e., with only metal salt 2 added, showed a corrosion rate of 30% to 46%; and Example 1a, i.e., with both metal salt 1 and metal salt 2 added, showed a recovery rate of 89% to 95%.
[0089] Example 2
[0090] Example 2a
[0091] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0092] (1) Mix 150g potassium phosphate, 40g potassium pyrophosphate and 100ml water for 20h to disperse evenly to obtain a compound salt solution; the compound salt solution is clear and transparent.
[0093] (2) Mix 0.2g copper sulfate, 0.5g zinc nitrate, 0.1g calcium nitrate and 5ml water for 30min to disperse evenly and obtain a composite solution;
[0094] (3) Add the composite solution obtained in step (2) and 3g of stabilizer to the composite saline solution obtained in step (1), stir, and obtain a high-density, high-temperature resistant, solid-free saline test solution. The stabilizer is polyethyleneimine.
[0095] The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density change rate of the test solution was measured. The density change rate is shown in the figure below. Figure 3 As shown in Table 3, after aging at 200℃ for 24 hours, the density is 1.7956 g / cm³. 3 After aging for 96 hours, the density was 1.809 g / cm³. 3 ,like Figure 3 As shown in Table 3, the density change rate after aging was 0.22%.
[0096] Example 2b: Only compound salt added
[0097] This embodiment provides a method for preparing a solid-free saline test solution. The difference from Embodiment 1 is that it only includes step (1), which is as follows: 150g of potassium phosphate, 40g of potassium pyrophosphate, and 100ml of water are mixed and dispersed evenly for 20 hours to obtain a solution with a density of 1.803g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution with a viscosity of 43.78 mPa·s was prepared. After aging at 200℃ for 24 hours, the density change rate of the solution was measured. The density change rate is shown in the figure below. Figure 3 As shown in Table 3.
[0098] Example 2c: No stabilizer was added; the mixture consisted of a complex salt + metal salt 1 + metal salt 2.
[0099] This embodiment provides a method for preparing a solid-free saline test solution, which differs from Example 1 in that no stabilizer is added. Specifically, 150g of potassium phosphate, 40g of potassium pyrophosphate, and 100ml of water are mixed and dispersed evenly for 20 hours to obtain a composite saline solution; the composite saline solution is clear and transparent. 0.2g of copper sulfate, 0.5g of zinc nitrate, 0.1g of calcium nitrate, and 5ml of water are mixed and dispersed evenly for 30 minutes to obtain a solution with a density of 1.80g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution with a viscosity of 42.13 mPa·s was prepared. After aging at 200℃ for 96 hours, the density change rate of the solution was measured. The density change rate is shown in the figure below. Figure 3 As shown in Table 3.
[0100] Table 3. Test results of density change rate of solid-free saline solution in Examples 2a-2c
[0101]
[0102] Example 3
[0103] Example 3a
[0104] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0105] (1) Mix 115g potassium phosphate, 25g potassium chloride, 20g sodium hexametaphosphate, 10g sodium tripolyphosphate and 100ml water for 10 hours to disperse evenly to obtain a composite salt solution; the composite salt solution is clear and transparent.
[0106] (2) Mix 0.125g copper sulfate, 0.5g zinc chloride, 0.15g zinc nitrate, 0.05g manganese chloride, 0.03g calcium chloride, 0.1g calcium nitrate and 5ml water for 30min to disperse evenly and obtain a composite solution;
[0107] (3) Add the composite solution obtained in step (2) and 2.50 g of stabilizer to the composite salt solution obtained in step (1), stir, and obtain a solution with a density of 1.7980 g / cm³. 3 A high-density, high-temperature resistant, solid-free saline test solution. The stabilizer is polyethyleneimine.
[0108] The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density and viscosity changes were measured. Viscosities at different aging times are shown below. Figure 4 As shown, after aging at 200℃ for 96 hours, the viscosity change was measured to be 1.16%, with a viscosity value of 46.92 mPa·s. The density change rate is as follows. Figure 5 As shown in Table 4, the density change rate after adding metal salt 1, metal salt 2 and stabilizer was 0.22%.
[0109] Example 3b: Only compound salt added
[0110] This embodiment provides a method for preparing a solid-free saline test solution. The difference from Embodiment 1 is that it only includes step (1), specifically as follows: 115g potassium phosphate, 25g potassium chloride, 20g sodium hexametaphosphate, 10g sodium tripolyphosphate, and 100ml water are mixed and dispersed evenly for 10 hours to obtain a solution with a density of 1.802g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution was prepared. The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density change rate of the solution was measured. The density change rate is shown in the figure below. Figure 5 As shown in Table 4.
[0111] Example 3c: No stabilizer was added; the mixture consisted of a complex salt + metal salt 1 + metal salt 2.
[0112] This embodiment provides a method for preparing a solid-free saline test solution, which differs from Example 1 in that no stabilizer is added. Specifically, 115g potassium phosphate, 25g potassium chloride, 20g sodium hexametaphosphate, 10g sodium tripolyphosphate, and 100ml water are mixed and dispersed evenly for 10 hours to obtain a composite saline solution; the composite saline solution is clear and transparent. 0.125g copper sulfate, 0.5g zinc chloride, 0.15g zinc nitrate, 0.05g manganese chloride, 0.03g calcium chloride, 0.1g calcium nitrate, and 5ml water are mixed and dispersed evenly for 30 minutes to obtain a solution with a density of 1.7993g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution was prepared. The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density change rate of the solution was measured. The density change rate is shown in the figure below. Figure 5 As shown in Table 4.
[0113] Table 4. Test results of density change rate of solid-free saline solution in Examples 3a-3c
[0114]
[0115] Example 4
[0116] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps:
[0117] (1) Mix 100g sodium phosphate, 85g potassium pyrophosphate and 100ml water for 20h to disperse evenly to obtain a compound salt solution; the compound salt solution is clear and transparent.
[0118] (2) Mix 0.2g of copper chloride, 1g of manganese chloride and 5ml of water for 30min to disperse evenly and obtain a composite solution;
[0119] (3) Add the composite solution obtained in step (2) and 3.6g of stabilizer to the composite saline solution obtained in step (1), and stir to obtain a high-density, high-temperature resistant, solid-free saline test solution. The stabilizer is polyethyleneimine.
[0120] The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density and viscosity changes were measured. The density and viscosity at different aging times are shown below. Figure 6 As shown, after aging at 200℃ for 96 hours, its density was measured to be 1.806 g / cm³ by volumetric method. 3 The density changed by 0.033%, and the viscosity changed by 1.44% to 47.92 mPa·s. Figure 6 As shown.
[0121] Example 5 (compound salt 2 plus metal salt 1 plus metal salt 2)
[0122] This embodiment provides a method for preparing a solid-free saline test solution, which differs from Example 4 in that: composite salt 1 is not added. Specifically, 185g of potassium pyrophosphate and 100ml of water are mixed and dispersed evenly for 20 hours to obtain an aqueous solution of composite salt 2; 0.2g of copper chloride, 0.1g of manganese chloride, 2.5g of stabilizer, and 5ml of water are mixed and dispersed evenly for 30 minutes to obtain a solution with a density of 1.79g / cm³. 3 A high-density, high-temperature resistant, solid-free saline solution with a viscosity of 51.78 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the solution were measured. The viscosity change rate was 4.7%, and the density change rate was 0.23%.
[0123] Example 6
[0124] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps: mixing 100g potassium phosphate, 80g sodium hexametaphosphate, and 100ml water for 24 hours to disperse evenly, obtaining a composite saline solution; then dissolving 0.8g copper chloride in 5ml water and stirring, then mixing with the composite saline solution and stirring for 30 minutes to obtain a density of 1.802g / cm³. 3 A high-density, high-temperature resistant, solid-free brine test solution with a viscosity of 46.32 mPa·s was prepared. After aging at 200℃ for 96 hours, the density and viscosity changes of the test solution were measured. The viscosity change rate was 10.23%, and the density change rate was 6.33%.
[0125] Example 7
[0126] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution, comprising the following steps: mixing 100g potassium phosphate, 80g sodium hexametaphosphate, and 100ml water for 24 hours to disperse evenly, obtaining a composite saline solution; then dissolving 0.5g ferrous chloride in 5ml water and stirring for 30 minutes to obtain a density of 1.798g / cm³. 3 The test solution has a viscosity of 48.12 mPa·s. Ferrous chloride easily forms ferric hydroxide precipitate upon addition to the system, making it unsuitable for maintaining the high-temperature density and viscosity stability of the test solution.
[0127] Example 8
[0128] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution. The difference from Example 2a is that the metal salt 2 is ferrous sulfate, not the metal salt 2 mentioned in this application. Similarly, a suspended precipitate is formed after its addition to the system.
[0129] Example 9
[0130] This embodiment provides a method for preparing a high-density, high-temperature resistant, solid-free saline test solution. The difference from Example 1a is that the stabilizer is not the stabilizer mentioned in this application, but ethylenediaminetetraacetic acid (EDTA). The preparation method is as follows:
[0131] (1) Mix 100g sodium phosphate, 85g potassium pyrophosphate and 100ml water for 20h to disperse evenly to obtain a compound salt solution; the compound salt solution is clear and transparent.
[0132] (2) Mix 0.2g of copper chloride, 1g of manganese chloride and 5ml of water for 30min to disperse evenly and obtain a composite solution;
[0133] (3) Add the composite solution obtained in step (2) and 3.6g of stabilizer to the composite saline solution obtained in step (1), and stir to obtain a high-density, high-temperature resistant, solid-free saline test solution. The stabilizer is ethylenediaminetetraacetic acid.
[0134] The high-density, high-temperature resistant, solid-free saline solution prepared above was aged at 200℃ for 96 hours, and the density and viscosity changes were measured. The results showed a viscosity change rate of 47.23% and a density change rate of 5.98%. Compared with the results of the polyethyleneimine stabilizer experiment, ethylenediaminetetraacetic acid (EDTA) failed to act as a stabilizer, possibly due to oxidative decomposition and inactivation of the stabilizer at high temperatures.
[0135] In summary, the high-temperature resistant solid-free brine test solution of this invention exhibits good density and viscosity stability under high-temperature (200℃) conditions, meeting the needs of actual well completion testing operations. Furthermore, its cost is relatively low, making it suitable for large-scale application. Although the embodiments of this invention only list a temperature of 200℃ and a density of 1.81–1.82 g / cm³,… 3 Examples of high-temperature resistant, solid-free saline test solutions are given, but those skilled in the art know that for high-temperature resistant, solid-free saline test solutions, the higher the temperature, the greater the change in density and viscosity, and ultimately the more serious the high-temperature sedimentation problem. The high-temperature resistant, solid-free saline test solution of the present invention has good density and viscosity stability at a temperature of 200°C. Therefore, those skilled in the art can deduce that it also has good technical effects at lower temperatures and lower densities.
[0136] The above embodiments are merely illustrative of the principles and effects of the present invention and are not intended to limit the invention. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in the present invention should still be covered by the claims of the present invention.
Claims
1. A high-density, high-temperature resistant, solid-free saline test solution, characterized in that, The test solution comprises the following raw materials: a composite salt aqueous solution, metal salt 1, metal salt 2, stabilizer, and solvent, in the mass percentage of the composite salt aqueous solution, wherein the metal salt is 10.01-0.25%, the metal salt is 20.1-0.5%, the stabilizer is 1-2%, and the solvent is 1-2%; the composite salt aqueous solution comprises a composite salt and water, wherein the composite salt is selected from at least one of composite salt 1 or composite salt 2; the composite salt 1 is selected from one or more of sodium monohydrogen phosphate, sodium dihydrogen phosphate, sodium phosphate, potassium phosphate, potassium monohydrogen phosphate, potassium dihydrogen phosphate, sodium chloride, and potassium chloride; the composite salt 2 is selected from one or more of sodium pyrophosphate, potassium pyrophosphate, sodium hexametaphosphate, and sodium tripolyphosphate; the metal salt 1 is selected from one or more of copper chloride or copper sulfate; the metal salt 2 is selected from one or more of zinc nitrate, zinc chloride, manganese chloride, calcium chloride, and calcium nitrate.
2. The high-density, high-temperature resistant, solid-free saline test solution according to claim 1, characterized in that: The composition, by mass percentage of the composite salt aqueous solution, is 10.15-0.25% metal salt, 20.2-0.5% metal salt, 1-2% stabilizer, and 1-2% solvent.
3. The high-density, high-temperature resistant, solid-free saline test solution according to claim 1, characterized in that: The stabilizer is polyethyleneimine; and / or the solvent is water.
4. The high-density, high-temperature resistant, solid-free saline test solution according to claim 1, characterized in that: The composite salt includes composite salt 1 and composite salt 2; preferably, the mass ratio of composite salt 1 to composite salt 2 is 1-3:2-3.
5. The high-density, high-temperature resistant, solid-free saline test solution according to claim 1, characterized in that: The density of the test solution is 1.70-1.82 g / cm³. 3 ; and / or, after the test liquid is aged at 200℃ for 96 hours, the density change rate is <0.35% and the viscosity change rate is ≤2%.
6. A method for preparing a high-density, high-temperature resistant, solid-free saline test solution as described in any one of claims 1-5, characterized in that, Includes the following steps: (1) Mix compound salt 1, compound salt 2 and water to obtain compound salt water; (2) Mix metal salt 1, metal salt 2 and solvent to obtain a composite solution; (3) Add the composite solution and stabilizer obtained in step (2) to the composite salt water obtained in step (1), stir and mix to obtain a high-density high-temperature resistant solid-free salt water test solution.
7. The method for preparing a high-density, high-temperature resistant, solid-free saline test solution according to claim 6, characterized in that: It also includes one or more of the following features: 11) The mixing time in step (1) is 10-30 hours; 12) The compound saline solution in step (1) is clear and transparent; 21) The mixing time in step (2) is 25-40 min.
8. The method for preparing a high-density, high-temperature resistant, solid-free saline test solution according to claim 6, characterized in that: It also includes one or more of the following features: 31) The mixing time in step (3) is 4-6 hours. 32) The density of the test solution prepared in step (3) is 1.70-1.82 g / cm³. 3 .
9. The method for preparing a high-density, high-temperature resistant, solid-free saline test solution according to claim 6, characterized in that: The test solution prepared in step (3) has a density change rate of <0.35% and a viscosity change rate of ≤2% after aging at 200℃ for 96 hours.
10. The use of the high-density, high-temperature resistant, solid-free brine test fluid as described in any one of claims 1-5 in well workover and completion testing in high-pressure deep oil reservoirs at 200℃.