ALD film growth using enhanced RF power at the bottom of the pulse
By using pulsed bottom RF power and inert gas purging during plasma-enhanced atomic layer deposition (PEALD), the problems of film conformability and underlying layer damage during PALD were solved, achieving high-quality film uniformity and conformability.
Patent Information
- Application Number
- CN202610637931.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-14
- Filing Date
- 2026-05-11
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies suffer from conformal issues in plasma-enhanced atomic layer deposition (PEALD), particularly in forming films of uniform thickness between gaps on the substrate, which may also lead to damage to the underlying layers.
By employing a pulsed bottom RF power method, when the plasma source and RF power source are activated, the pulse is connected to the substrate support, and a film is formed on the substrate surface using reactive substances. This is combined with an inert gas purging step to improve the uniformity and conformability of the film.
This improves the uniformity and shape retention of the film, reduces damage to the underlying layer, and enables high-quality film deposition between substrate gaps.
Smart Images

Figure CN123108528A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method and system for enhancing ALD film growth in a deposition chamber while simultaneously applying RF power at the bottom of a pulse, and more particularly, to a method and system for enhancing ALD film growth with uniform thickness. Background Technology
[0002] Fabricating modern semiconductor devices requires the precise deposition of materials with carefully controlled thickness and composition. Ideally, the desired material composition could be deposited directly in a single-step process, but this is typically not feasible, and a material layer must be deposited and then transformed into a layer with the desired elemental composition and properties. Using a CVD process with precursor chemicals containing the desired elements would be an option, but this introduces issues with film conformability and composition control. Alternative processing schemes exist to enhance the usability of CVD precursors, where the precursor is exposed to a low-power plasma that partially breaks down molecules to produce more reactive material more likely to adhere to the substrate surface. This so-called precursor radicalization method makes CVD precursors usable for ALD processing, and it requires a method that exposes the precursor stream to direct plasma without affecting the substrate.
[0003] Plasma-enhanced atomic layer deposition (PEALD) is a widely used deposition method in which plasma is used to generate high-energy ions and reactive radicals that can greatly benefit the deposition process. However, due to the inherent anisotropic nature of ion flux on the substrate, the PEALD process often suffers from conformal issues in the deposited film. To address this problem, radical-enhanced ALD (REALD) was developed as a variant of PEALD, in which ions formed in the plasma sheath are not allowed to reach the substrate, and film growth depends solely on reactive radicals in the plasma. This approach results in a process with characteristics between PEALD and thermal ALD, and it can be very useful, especially for applications requiring high levels of conformal performance. However, some applications will benefit from the possibility of using both direct plasma treatment and radical exposure in the same process. Summary of the Invention
[0004] Embodiments of the present invention provide a method for forming a film between gaps on a substrate. The method includes introducing a substrate onto a substrate support in a reaction chamber, introducing a precursor into the reaction chamber, causing the precursor to react with the surface of the substrate, and introducing plasma from a plasma source into the reaction chamber. The method also includes introducing a reactant gas into the reaction chamber, pulse-connecting an RF power source to the substrate support, generating a reactive substance from the reactant gas when both the plasma source and the RF power source are activated, and causing the reactive substance to react with the precursor on the surface to form a film on the substrate.
[0005] In some embodiments, the precursor comprises silane, silane, propane, di(isopropylamino)silane, dichlorosilane, trichlorosilane, or monomethylsilane. In some embodiments, the reactant gas comprises oxygen or hydrogen peroxide. In some embodiments, the time period for introducing plasma into the reaction chamber is substantially the same as the time period for pulsed connection to the RF power source of the substrate support. In some embodiments, the method further includes a purging step after introducing the precursor into the reaction chamber and before introducing the reactant gas into the reaction chamber. In some embodiments, the flow rate of the introduced precursor is greater than 0 and less than 3000 sccm. In some embodiments, the flow rate of the introduced reactant gas is greater than 0 and less than 3000 sccm. In some embodiments, the power of the plasma source is greater than 0 and less than 6000 W. In some embodiments, the power of the RF power source is greater than 0 and less than 1000 W. In some embodiments, the duty cycle of the RF power source is greater than 10% and less than 90%. In some embodiments, the pulse frequency of the RF power is greater than 0 and less than 100 kHz. In some embodiments, the RF frequency of the RF power is greater than 13.56 MHz and less than 60 MHz. In some embodiments, the process pressure for reacting the reactant gas with the precursor is higher than 1 Torr and lower than 9 Torr. In some embodiments, the process temperature for reacting the reactant gas with the precursor is higher than 0°C and lower than 1000°C.
[0006] Embodiments of the present invention provide a method for forming material between gaps on a substrate. The method includes introducing a substrate onto a substrate support in a reaction chamber, introducing a precursor into the reaction chamber, reacting the precursor with the surface of the substrate, and purging the reaction chamber with an inert gas after the precursor reaction. The method includes introducing a reactant gas into the reaction chamber after purging, activating a plasma source to introduce plasma into the reaction chamber, pulse-connecting an RF power source to the substrate support, and generating a reactive material from the reactant gas while both the plasma source and the RF power source are activated. The method further includes reacting the reactive material with the reactant precursor to form material between gaps, and deactivating the plasma source when the pulse of the RF power source ends.
[0007] In some embodiments, the method further includes introducing an inert gas into the reaction chamber simultaneously with introducing the precursor and reactant gases. In some embodiments, the method further includes purging the reaction chamber with an inert gas after the plasma source has been deactivated.
[0008] Embodiments of the present invention provide a semiconductor processing apparatus including a reaction chamber and a plasma source, the plasma source being located at the upper part of the reaction chamber. The semiconductor processing apparatus includes a substrate support located at the lower part of the reaction chamber and supporting the substrate. The semiconductor processing apparatus includes an ion filter located between the plasma source and the substrate support. The semiconductor processing apparatus includes an RF power source connected to the substrate support and configured to radially distribute plasma on the substrate. The semiconductor processing apparatus also includes a precursor source and a reactant source in fluid communication with the reaction chamber.
[0009] In some embodiments, the semiconductor processing apparatus further includes a controller configured to: introduce a precursor from a precursor source into a reaction chamber; purge the reaction chamber after introducing the precursor; introduce a reactant gas from a reactant source into the reaction chamber; activate a plasma source and pulse an RF power source to form a film on a substrate by reacting the reactant gas with the precursor; and purge the reaction chamber after forming the film on the substrate. In some embodiments, the plasma source is an inductively coupled plasma source. Attached Figure Description
[0010] The invention can be more fully understood by reading the following detailed description and embodiments and by referring to the accompanying drawings, wherein:
[0011] Figure 1 This is a schematic diagram of a semiconductor processing apparatus according to some embodiments of the present disclosure;
[0012] Figure 2 This is a schematic diagram of a method for forming a film between gaps on a substrate according to some embodiments of the present disclosure;
[0013] Figure 3 This is a timing diagram according to some embodiments of the present disclosure;
[0014] Figure 4A This is a schematic diagram of the surface of a substrate according to some embodiments of the present disclosure;
[0015] Figure 4B This is a graph showing the thickness of a film on the surface of a substrate according to some embodiments of the present disclosure; and
[0016] Figures 5A to 5C This is a cross-sectional view of a semiconductor structure according to some embodiments of the present disclosure. Detailed Implementation
[0017] This disclosure will now be described more fully below with reference to the accompanying drawings. However, this disclosure may be implemented in many different forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of this disclosure to those skilled in the art.
[0018] It will be understood that although the terms “first,” “second,” etc., may be used herein to describe various components, regions, layers, and / or parts, these components, regions, layers, and / or parts should not be limited by these terms. These terms do not refer to a particular order, vertical relationship, or preference, and are used only to distinguish one component, region, or part from another. Therefore, without departing from the teachings of this disclosure, the first component, region, or part described below may refer to the second component, region, or part.
[0019] As used herein, "basic" or "approximately equivalent" means ±5%, ±2%, ±1%, or ±0.5% of another value or shape (e.g., one or more cross-sectional dimensions of a shape). Percentages can be absolute or relative.
[0020] In the accompanying drawings, the shapes illustrated may vary due to factors such as manufacturing techniques and / or tolerances. Therefore, embodiments should not be construed as limited to a specific shape within the areas shown herein, but may include shape variations, for example, due to manufacturing processes. Furthermore, the drawings may be used to illustrate various features, which may not be drawn to scale.
[0021] When a phrase such as "at least one of..." follows an element in a column, it modifies the entire column, rather than a single element in that column.
[0022] As used herein, "atomic layer deposition," abbreviated as "ALD," refers to a method of depositing a film on a substrate by sequentially exposing the substrate surface to alternating gaseous reactants. Unlike chemical vapor deposition, the different reactants are not present simultaneously in the reactor, but are introduced as a series of sequential, non-overlapping pulses. In each of these pulses, the reactant reacts with the surface in a self-limiting or substantially self-limiting manner. Furthermore, as used herein, ALD may also be intended to include processes specified by related terms such as chemical vapor atomic layer deposition, atomic layer epitaxy (ALE), molecular beam epitaxy (MBE), gas-source MBE or organometallic MBE, and chemical beam epitaxy when performed with alternating pulses of reactants.
[0023] As used in this article, "boron carbide" or "B" x C y "Borne carbide" refers to a material containing boron and carbon. In some embodiments, boron carbide may not include elements other than boron and carbon in significant proportions. In some embodiments, boron carbide contains B4C. In some embodiments, boron carbide may consist essentially of B4C. In some embodiments, boron carbide may not include stoichiometric amounts of boron carbide. In some cases, boron carbide may include other elements, such as hydrogen.
[0024] As used in this article, "boron carbonitride" or "B" x C y Nz "" refers to materials containing boron, carbon, and nitrogen. Boron carbonitride can be produced by formula B x C y N z This indicates that the sum of x, y, and z equals 3. In some cases, boron carbonitride may include other elements, such as hydrogen. Boron carbonitride can include both boron carbide and boron nitride.
[0025] As used in this article, "boron nitride" or "B" x N y "Boron nitride" refers to a material containing boron and nitrogen. In some embodiments, boron nitride may not include elements other than boron and nitrogen in significant proportions. In some embodiments, boron nitride contains BN. In some embodiments, boron nitride may consist essentially of BN. In some cases, boron nitride may not include stoichiometric amounts of boron nitride. In some cases, boron nitride may include other elements, such as hydrogen.
[0026] As used in this article, "boron oxide" or "B" x O y "" refers to a material containing boron and oxygen. In some embodiments, boron oxide may not include a significant proportion of elements other than boron and oxygen. Boron oxide can be produced by formula B x O y This indicates that x can range from about 0 to about 6, and y can range from about 0 to about 3. In some embodiments, boron oxide comprises B₂O₃. In some embodiments, boron oxide may consist essentially of B₂O₃. In some cases, boron oxide may not include stoichiometric amounts of boron oxide. In some cases, boron oxide may include other elements, such as carbon and / or hydrogen.
[0027] As used herein, "chemical vapor deposition," abbreviated as "CVD," refers to a method of depositing a film on a substrate by exposing the substrate surface to one or more gaseous reactants, which react and / or decompose on the substrate surface to produce the desired film. Typically, CVD is performed by co-introducing the reactants into a reactor.
[0028] As used herein, “chemisorption” refers to an adsorption process caused by a reaction on an exposed surface, which creates, for example, covalent or ionic bonds between the surface and the adsorbate.
[0029] As used herein, a “film” refers to a continuous, substantially continuous, or discontinuous material that extends in a direction perpendicular to its thickness direction to cover at least a portion of a surface. Films can include two-dimensional materials, three-dimensional materials, nanoparticles, or even partial or complete molecular layers, partial or complete atomic layers, or atomic and / or molecular clusters. Films can consist of one or more indistinguishable layers (e.g., monolayers or submonolayers) to produce a homogeneous or substantially homogeneous material, wherein the number of layers affects the thickness of the material.
[0030] As used herein, “gas” refers to a state of matter consisting of atoms or molecules that have neither a defined volume nor a defined shape. Gases include evaporated solids and / or liquids, and may, depending on the circumstances, consist of a single gas or a mixture of gases.
[0031] As used herein, “plasma” refers to an ionized gas containing approximately equal numbers of negatively and positively charged matter (typically electrons and ions). Excited and reactive matter is also included within plasma, such as atoms and free radicals, metastable atoms and molecules, and photons. Plasma discharge requires an externally applied electric or magnetic field to ionize the gas. Plasma generation schemes and geometries include, but are not limited to, capacitively coupled plasma (CCP), inductively coupled plasma (ICP), and RF hollow cathode (HC) plasma, which differ in the generation of excited and reactive matter and therefore can provide very different fluxes of various substances.
[0032] As used herein, a "precursor" refers to a compound that participates in a chemical reaction to form another compound or element, wherein a portion of the precursor (an element or group within the precursor) is incorporated into the compound or element produced by the chemical reaction. The compound or element produced by the chemical reaction can be a layer and / or film formed on a substrate surface.
[0033] As used herein, "reactant" refers to a compound that participates in a chemical reaction to form another compound or element. In some cases, a reactant is a precursor. In other cases, the compound or element produced by a chemical reaction does not contain any part of the reactant (the element or group within the reactant), and therefore the reactant is not a precursor.
[0034] As used herein, "self-limiting" refers to a process that proceeds through a finite process and terminates upon completion of that process. For example, a self-limiting surface reaction terminates when the surface becomes saturated and all available and / or accessible surface reactive sites are exhausted. At most, a single monolayer can form on a surface.
[0035] As used herein, “silicon carbide” or “SiC” refers to a material comprising silicon and carbon. In some embodiments, silicon carbide may not include a significant proportion of elements other than silicon and carbon. Silicon carbide may be represented by the formula SiC. In some embodiments, silicon carbide comprises SiC. In some embodiments, silicon carbide may consist essentially of SiC. Silicon carbide is not necessarily a stoichiometric composition. The amount of silicon may range from 5% to 50%; the amount of carbon may range from about 50% to about 95%. In some embodiments, the SiC film may contain one or more elements other than silicon and carbon, such as hydrogen and / or nitrogen.
[0036] As used in this article, "silicon carbonitride" or "Si" xC y N z "Silicon carbonitride" or "SiCN" refers to a material containing silicon, carbon, and nitrogen. Silicon carbonitride can be produced by the formula Si x C y N z In some embodiments, silicon carbonitride may contain more Si-N bonds than Si-C bonds, for example, the ratio of Si-N bonds to Si-C bonds may be from about 1:10 to about 10:1. In some embodiments, the silicon carbonitride film may contain about 0% to about 50% carbon on an atomic basis. In some embodiments, silicon carbonitride may contain about 0.1% to about 40%, about 0.5% to about 30%, about 1% to about 30%, or about 5% to about 20% carbon on an atomic basis. In some embodiments, silicon carbonitride may contain about 0% to about 70% nitrogen on an atomic basis. In some embodiments, silicon carbonitride may contain about 10% to about 70%, about 15% to about 50%, or about 20% to about 40% nitrogen on an atomic basis. In some embodiments, silicon carbonitride may contain about 0% to about 50% silicon on an atomic basis. In some embodiments, silicon carbonitride may contain about 10% to about 50%, about 15% to about 40%, or about 20% to about 35% silicon on an atomic basis. In some cases, silicon carbonitride may include other elements, such as hydrogen. Silicon carbonitride may include both silicon carbide and silicon nitride.
[0037] As used in this article, "silicon nitride" or "Si" x N y "Silicon nitride" refers to a material comprising silicon and nitrogen. In some embodiments, silicon nitride may not include a significant proportion of elements other than silicon and nitrogen. Silicon nitride may be represented by the formula Si3N4. In some embodiments, silicon nitride comprises Si3N4. In some embodiments, silicon nitride may consist essentially of Si3N4. In some cases, silicon nitride may not include stoichiometric amounts of silicon nitride. In some cases, silicon nitride may include other elements, such as carbon, oxygen, and / or hydrogen.
[0038] As used in this article, "silicon oxide" or "SiO" x "Silicon oxide" refers to materials containing silicon and oxygen. Silicon oxide can be produced by the formula SiO2. x The expression indicates that x can be between 0 and 2. In some embodiments, silicon oxide may not include a significant proportion of elements other than silicon and oxygen. Silicon oxide may be represented by the formula SiO2. In some embodiments, silicon oxide comprises SiO2. In some embodiments, silicon oxide may consist essentially of SiO2. In some cases, silicon oxide may not include stoichiometric amounts of silicon oxide. In some cases, silicon oxide may include other elements, such as carbon, nitrogen, and / or hydrogen.
[0039] As used in this article, "silicon oxide" or "Si" z O x Cy "SiOC" or "SiO2O2" refers to a material comprising silicon, oxygen, and carbon. As used herein, unless otherwise stated, SiOC is not intended to limit, constrain, or define bonding or chemical states, such as the oxidation states of any of Si, O, C, and / or any other elements in the film. In some embodiments, SiO2... z O x C y It may contain Si-C bonds and / or Si-O bonds. In some embodiments, SiOC may contain Si-C bonds and Si-O bonds, and may not contain Si-N bonds. In some embodiments, in addition to Si-C and / or Si-O bonds, SiOC may also contain Si-H bonds. In some embodiments, SiOC may contain more Si-O bonds than Si-C bonds, for example, the ratio of Si-O bonds to Si-C bonds may be from about 1:10 to about 10:1. In some embodiments, SiOC may contain about 0% to about 50% carbon on an atomic basis. In some embodiments, SiOC may contain about 0.1% to about 40%, about 0.5% to about 30%, about 1% to about 30%, or about 5% to about 20% carbon on an atomic basis. In some embodiments, SiOC may contain about 0% to about 70% oxygen on an atomic basis. In some embodiments, SiOC may contain about 10% to about 70%, about 15% to about 50%, or about 20% to about 40% oxygen on an atomic basis. In some embodiments, SiOC may contain about 0% to about 50% silicon on an atomic basis. In some embodiments, the SiOC film may comprise about 10% to about 50%, about 15% to about 40%, or about 20% to about 35% on an atomic basis. In some embodiments, silicon carbide may be derived from silicon (Chemical Formula Si). z O x C y It is indicated that z can be in the range of about 0 to about 2, x can be in the range of about 0 to about 2, and y can be in the range of about 0 to about 5.
[0040] As used in this article, "silicon oxide carbonitride" or "Si" z O x C y N w "SiOCN" or "SiOCN" refers to a material comprising silicon, oxygen, nitrogen, and carbon. As used herein, unless otherwise stated, SiOCN is not intended to limit, constrain, or define the bonding or chemical state, such as the oxidation state of any of the elements Si, O, C, N, and / or any other elements in the material. In some embodiments, SiOCN is a material that can be produced from the chemical formula Si z O x C y N wThe material represents the range of z from about 0 to about 2, x from about 0 to about 2, y from about 0 to about 2, and w from about 0 to about 2.
[0041] As used in this article, "silicon oxynitride" or "SiO2" x N y "SiO" refers to materials containing silicon, oxygen, and nitrogen. As used herein, unless otherwise stated, SiO x N y This is not intended to limit, constrain, or define the bonding or chemical state, such as the oxidation state of any of Si, O, N, and / or any other element in the material. In some embodiments, SiO x N y It can be made using the chemical formula SiO. x N y The material is indicated by the range x, which can be in the range of about 0 to about 2, and y, which can be in the range of about 0 to about 2. Silicon oxynitride can include silicon oxide and silicon nitride.
[0042] As used herein, "substrate" refers to one or more underlying materials on which devices, circuits, materials, or material layers can be formed or on which they are formed. Substrate can be continuous or discontinuous; rigid or flexible; solid or porous; and combinations thereof. Substrate can be in any form, such as powder, plate, or workpiece. Plate-type substrates can include wafers of various shapes and sizes. Substrate can be made of semiconductor materials, including, for example, silicon, silicon germanium, silicon oxide, gallium arsenide, gallium nitride, and silicon carbide. Substrate can include one or more layers covering a bulk material; for example, substrate can include nitrides (e.g., TiN), oxides, insulating materials, dielectric materials, conductive materials, metals (e.g., tungsten, ruthenium, molybdenum, cobalt, aluminum, or copper), or metallic materials, crystalline materials, epitaxial, heteroepitaxial, and / or single-crystal materials. Substrate can include various topologies, such as gaps, including spaces between recesses, lines, trenches, or raised portions (e.g., fins) formed within or on at least a portion of the layers of the substrate.
[0043] As used herein, an "ion trap" refers to a structure, region, apparatus, or configuration within a semiconductor processing chamber (e.g., a plasma-enhanced atomic layer deposition (PE-ALD) or radical-enhanced atomic layer deposition (RE-ALD) chamber) designed to selectively capture, retain, and control ionic material generated during the deposition process. Ion traps may be integrated into or positioned adjacent to the inner surface of the chamber and may include, for example, chamber walls, gas distribution plates, or other internal components to manage the energy, directionality, and concentration of ions within the reaction space. By influencing ion trajectories and reducing unwanted ion bombardment or plasma-induced damage to the substrate and underlying device structures, ion traps can help maintain optimal conditions for uniform and conformal film growth. Ion traps can be formed from a variety of conductive, semiconductive, or dielectric materials and may include engineered geometries, patterned surfaces, coatings, or other configurations tailored to specific process chemistry, power levels, and plasma conditions of interest. In some embodiments, ion traps can be dynamically adjusted or tuned to accommodate varying process parameters, thereby improving process stability, film quality, and overall device performance in advanced semiconductor manufacturing environments.
[0044] As used herein, a "substituent" is an atom or group of atoms that replaces one or more atoms (e.g., hydrogen atoms) or groups of atoms in a parent compound, thereby producing a new compound. A substituent replaces an original atom or group of atoms in the parent molecule. For simplicity, a substituent may be represented in a chemical formula as an "R" group, and each "R" group in the compound may be chosen independently unless otherwise specifically stated otherwise. Examples of substituents include, but are not limited to: hydrogen atoms (H); "alkyl", such as saturated straight-chain or branched C1 to C2 groups. 10 Hydrocarbons, preferably C1 to C6 hydrocarbons (e.g., methyl, ethyl, propyl, isopropyl, butyl, isobutyl, sec-butyl, tert-butyl, pentyl, 3-pentyl, neopentyl, and hexyl); "cycloalkyl", such as C3 to C6 cyclic hydrocarbons (e.g., cyclopropyl, cyclobutyl, cyclopentyl, and cyclohexyl); "alkenyl", such as C2 to C6 straight-chain or branched unsaturated hydrocarbons (e.g., vinyl, allyl, propenyl, butenyl, pentenyl, hexenyl, butadienyl, pentadienyl, hexadienyl, ethynyl, propargyl, butynyl, pentynyl, and hexynyl); "aryl", such as phenyl, benzyl, tolyl, xylyl, naphthyl, cyclopentadienyl, and methyl, dimethyl, or ethylcyclopentadienyl; hydroxyl (OH); "alkoxy", such as straight-chain or branched C1 to C6 hydrocarbons. 10 Alkoxy groups, typically C1 to C4 alkoxy groups (e.g., methoxy, ethoxy, n-propoxy, isopropoxy, butoxy, isobutoxy, sec-butoxy, and tert-butoxy); hydroxyalkyl groups, such as straight-chain or branched C1 to C4 alkoxy groups. 10Hydroxyalkyl, typically straight-chain or branched C1 to C4 hydroxyalkyl (e.g., hydroxymethyl, hydroxyethyl, hydroxypropyl, hydroxybutyl, hydroxypentyl, and hydroxyhexyl); "alkoxycarbonyl", such as straight-chain or branched C1 to C6 carbonyl hydrocarbons (e.g., methoxycarbonyl, ethoxycarbonyl, propoxycarbonyl, isopropoxycarbonyl, butoxycarbonyl, pentoxycarbonyl, and hexoxycarbonyl); thiol (SH); "alkylthiol", such as straight-chain or branched C1 to C6 thiols (e.g., thiol methyl, hydroxyethyl, hydroxypropyl ... Thiols (ethyl, propyl, butyl, pentyl, and hexyl); halides (X), such as fluorides (F), chlorides (Cl), bromides (Br), and iodides (I); and "haloalkyl", such as straight-chain or branched C1 to C6 alkyl halides having one or more halogen atoms (e.g., iodomethyl, bromomethyl, chloromethyl, fluoromethyl, trifluoromethyl, 2-chloroethyl, 2-fluoroethyl, 2,2,2-trifluoroethyl, and pentafluoroethyl). The substituent itself can be substituted. For example, hydroxyalkyl is a substituted alkyl group in which the H atom on the alkyl group is replaced by an OH group.
[0045] As used herein, “radicalization” refers to the process of converting a stable precursor or reactant gas into radicals (highly reactive neutral substances with unpaired electrons) in a semiconductor deposition chamber environment, such as during plasma-enhanced atomic layer deposition (PE-ALD) or radical-enhanced atomic layer deposition (RE-ALD). These radicals can be generated by introducing an energy source (e.g., plasma, photons, thermal energy) that dissociates gaseous molecules into more reactive fragments. The radicalization process can occur within or near the deposition chamber and can be achieved through dedicated radical generation zones, plasma sources, radical injectors, or other field-generating components. By generating a controlled number of radicals, the radicalization process enhances reaction kinetics, improves overall chemical reactivity at the substrate surface, and enables more uniform, conformal, and efficient film deposition. These radicals can react with a variety of substrate surfaces, including silicon-based materials, metals, nitrides, oxides, and other semiconductor or dielectric materials, thereby promoting customized surface modification or layer formation. The radicalization process can be dynamically adjusted by controlling parameters such as gas flow, chamber pressure, plasma power, or residence time of precursor materials, thereby allowing for fine-tuning of film properties, improved process stability, and enhanced device performance in advanced semiconductor manufacturing environments.
[0046] Depending on the context, the article “a” or “an” refers to a substance or a genus that comprises multiple substances. Therefore, the terms “a / an,” “one or more,” and “at least one” are used interchangeably herein. It should also be noted that the terms “comprising,” “including,” and “having” are used interchangeably.
[0047] The term "approximately" typically refers to a range of numbers that are considered equivalent to the value (e.g., having the same function or result). In some cases, the term "approximately" may include a numerical value rounded to the nearest significant figure.
[0048] The term "basic" when applied to compositions, methods, or systems generally means that the addition of components does not substantially alter the properties and / or functions of the composition, method, or system.
[0049] The term "basic" applied to compositions, methods, or systems generally refers to a proportion of a value, property, characteristic, etc., or conversely, to the absence of such a value, i.e., at least about 70%, at least about 80%, at least about 90%, at least about 95%, at least about 97%, at least about 98%, at least about 99%, at least about 99.5%, at least about 99.9% or more, or any proportion between about 70% and about 100%. In some embodiments, the term "basic" means a proportion of about 90%, about 95%, about 97%, about 98%, about 99%, about 99.5%, or about 99.9%.
[0050] "At least one," "one or more," and "and / or" are open-ended expressions that are both conjunction and disjunctive in practice. For example, each of the expressions "at least one of A, B, and C," "at least one of A, B, or C," "one or more of A, B, and C," "one or more of A, B, or C," and "A, B, and / or C" represents A alone, B alone, C alone, A and B together, A and C together, B and C together, or A, B, and C together. When each of A, B, and C in the above expressions refers to an element (e.g., X, Y, and Z) or an element category (e.g., X1-X), the meaning is different. n Y1-Y m and Z1-Z o When used, this phrase is intended to refer to a single element selected from X, Y, and Z; a combination of elements selected from the same category (e.g., X1 and X2); and a combination of elements selected from two or more categories (e.g., Y1 and Z). o ).
[0051] It should be understood that every numerical range given in this disclosure is considered to include both an upper and lower endpoint, as well as every narrower numerical range falling within such a wider range, as such narrower numerical ranges are explicitly stated herein. For example, the phrase “about 2 to about 4” or “2 to 4” includes 2 and 4 and integer and / or integer ranges of about 2 to about 3, about 3 to about 4, and every possible range based on real numbers (e.g., irrational and / or rational numbers), such as about 2.1 to about 3.9, about 2.1 to about 3.4, etc.
[0052] This disclosure generally relates to methods for forming materials between gaps on a substrate using plasma-enhanced atomic layer deposition (PE-ALD) and apparatus for performing such methods, and particularly to using pulsed bottom RF power to reduce damage to underlying layers. More specifically, this disclosure generally relates to methods for forming films between gaps on a substrate using radical-enhanced atomic layer deposition (RE-ALD) and systems for performing such methods, and particularly to using pulsed bottom RF power to improve film uniformity. Various aspects of the methods and systems, and the benefits derived therefrom, will now be described.
[0053] The search for improved chemical precursors for ALD processes is an ongoing endeavor, driven by increasingly stringent material and process requirements for improving semiconductor devices. Typically, it is difficult to separately control plasma density and ion energy, as both are controlled by the same RF power. While using low ion energy at the substrate level to improve underlayer damage, there is a problem of reduced film density, leading to increased etch rates and decreased film density uniformity. In this regard, methods and systems for depositing films to improve underlayer damage at high film quality are disclosed herein. The methods and systems disclosed herein advantageously utilize pulsed bottom RF power to form material between gaps on the substrate. The disclosed methods can improve film uniformity and conformability while minimizing damage to the underlying liner. These and other advantages will be apparent from the various aspects, embodiments, and configurations disclosed herein.
[0054] Please refer to Figure 1 , Figure 1 This is a schematic diagram of a semiconductor processing apparatus 100 according to some embodiments of the present disclosure. The semiconductor processing apparatus 100 is an implementation of method 200, which will be combined with... Figure 2 Further discussion is needed. Therefore, the elements and / or components described herein can be associated with method 200.
[0055] A carrier gas is supplied from a carrier gas source 102 to the reaction chamber 120 via a gas manifold 101. The carrier gas flows into the reaction chamber 120 where a substrate (e.g., a wafer) 110 is placed. A precursor is also supplied in gaseous form from a precursor source 103 to the reaction chamber 120 via a gas manifold 101. The precursor may be evaporated and entrained in the carrier gas or pulsed into the carrier gas. A reactant is supplied in gaseous form from a reactant source 104 to the reaction chamber 120 via a gas manifold 101. That is, the precursor source 103 and the reactant source 104 are in fluid communication with the reaction chamber 120. In some embodiments, the reaction chamber 120 may form part of an ALD assembly and may be a single-wafer reactor, or it may comprise one or more multi-station deposition chambers. Alternatively, the reactor may be a batch reactor. The various steps of the method may be performed in a single reaction chamber, or they may be performed in multiple reaction chambers, such as the reaction chamber of a clustering tool. In some embodiments, the method is performed in a single reaction chamber of a clustering tool, but other preceding or subsequent fabrication steps of the structure or device are performed in a separate reaction chamber of the same clustering tool. Optionally, the components including the reaction chamber may be equipped with a heater to activate the reaction by raising the temperature of one or more of the substrate, reactants, precursors, and other gases. A spray-type reaction chamber, a cross-flow reaction chamber, or a combination thereof may be used to introduce the reactants, precursors, and other gases into the chamber.
[0056] The semiconductor processing apparatus 100 is also configured to allow the introduction of other gases into the reaction chamber 120, such as other reactants (reactive gases) and other gases (e.g., other carrier gases, precursor or reactive gases, carrier gas, diluent, process gas, feed gas, and / or purge gas). Therefore, the semiconductor processing apparatus 100 may include other sources (not shown). Unreacted gases and gaseous reaction byproducts exit the reaction chamber 120 via an exhaust line 112. The reaction chamber 120 may optionally be equipped with a purge line (not shown) and / or a pump line (not shown) connected to a vacuum pump (not shown), allowing the reaction chamber 120 to be purged between various reaction cycles.
[0057] A plasma source 105 is located above the reaction chamber 120 and configured to generate plasma. The plasma source 105 is activated to introduce plasma into the reaction chamber 120. In some embodiments, the plasma source 105 is an inductively coupled plasma source. However, this disclosure is not limited thereto. The semiconductor processing apparatus 100 may include a substrate support 111 located below the reaction chamber 120 and configured to support the substrate 110. An ion filter 109 is located between the plasma source 105 and the substrate support 111. In some embodiments, the ion filter 109 divides the reaction chamber 120 into an upper and lower portion. The ion filter 109 confines plasma from the plasma source 105 to the upper portion of the reaction chamber 120 above the ion filter 109. For example, an electrically grounded mesh plate can be used as the ion filter 109. In some embodiments, the mesh plate is a metal plate (e.g., aluminum) comprising hundreds of holes in a spray nozzle pattern that allow free radical material to pass through to the substrate 110 while capturing ions. For example, the stencil may include between about 1,000 and about 5,000 holes, each with a diameter between about 0.5 mm and about 2 mm. Adding an ion filter 109 advantageously reduces or even eliminates the interaction of electrons and ions with the surface of the substrate 110 by confining the first plasma to the upper part of the reaction chamber 120.
[0058] An RF power source 123 is connected to a substrate support 111 and configured to radially distribute plasma on the substrate 110. That is, the RF power source 123 allows the substrate support 111 to be biased relative to the ion filter 109. The semiconductor processing apparatus 100 also includes a controller 114 operatively connected to a first valve 115, a second valve 116, and a third valve 117, a plasma source 105, an RF power source 123, and other components (not shown). The controller 114 is configured and programmed to independently control (e.g., open and close) the supply of various gases (e.g., carrier gas, precursors, reactants and any diluents, process gas, feed gas, and / or purge gas, etc.), the plasma source 105, and the RF power source 123 as needed to deposit a film on the surface of the substrate 110. In some embodiments, the controller 114 is configured to control the first valve 115 to allow carrier gas to flow from a carrier gas source 102 into the reaction chamber 120. Controller 114 is further configured to open second valve 116 to allow precursors to flow from precursor source 103 into reaction chamber 120. After a set time period, controller 114 closes second valve 116 leading to precursor source 103 and opens third valve 117 to allow reactants to flow from reactant source 104 into reaction chamber 120 and activate plasma source 105 and RF power source 123. After a set time period, controller 114 closes third valve 117 leading to reactant source 104 and shuts down plasma source 105 and RF power source 123. Controller 114 is programmed to repeat various processing steps to grow a film on the surface of substrate 110. Controller 114 can be programmed to perform additional processing steps between these various steps.
[0059] The semiconductor processing apparatus or system disclosed herein may include Figure 1 Additional sources and components, not shown, such as those commonly found in semiconductor processing equipment. For example, semiconductor processing equipment 100 may be provided with one or more heaters and one or more temperature regulators to activate the reaction by raising the temperature of one or more of the substrate and / or gases entering the reaction chamber (e.g., carrier gas, precursor gas, reactant gas, etc.). Semiconductor processing equipment 100 may also be provided with a pumping system for purging the reaction chamber between various processing steps. The following will be combined with... Figure 2 and Figure 3 Further details on the operation of the semiconductor processing device 100 will be discussed.
[0060] Please refer to Figure 2 , Figure 2This is a schematic diagram of a method 200 for forming material between gaps on a substrate (e.g., substrate 110) according to some embodiments of the present disclosure. In step 202, method 200 includes introducing the substrate onto a substrate support in a reaction chamber. In some embodiments, substrate 110 is introduced onto a substrate support 111 in a reaction chamber 120. In step 204, method 200 includes introducing a precursor into the reaction chamber. In some embodiments, a precursor is introduced into reaction chamber 120. For example, the precursor includes silane, silane, propane, di(isopropylamino)silane, dichlorosilane, trichlorosilane, or monomethylsilane. However, the present disclosure is not limited thereto.
[0061] Next, in step 206, method 200 includes reacting the precursor with the surface of the substrate. In some embodiments, the precursor reacts with the surface (e.g., the upper surface) of the substrate 110. In some embodiments, the flow rate of the introduced precursor is greater than 0 and less than 3000 sccm, for example, about 500 sccm, about 1000 sccm, about 1500 sccm, about 2000 sccm, about 2500 sccm, etc. In step 208, method 200 includes purging the reaction chamber with an inert gas after the precursor reaction. In some embodiments, the reaction chamber 120 is purged with an inert gas after the reaction between the precursor and the surface of the substrate 110 has ended. It should be noted that in some embodiments, the purging step (e.g., step 208) is optional and may be omitted. In step 210, method 200 includes introducing a reactant gas into the reaction chamber after purging the reaction chamber (or, if step 208 is omitted, after the precursor reacts with the surface of the substrate 110). In some embodiments, after purging reaction chamber 120 (i.e., removing remaining precursors from reaction chamber 120), a reactant gas is introduced into reaction chamber 120. For example, the reactant gas includes oxygen or hydrogen peroxide. In some embodiments, the flow rate of the introduced reactant gas is greater than 0 and less than 3000 sccm, for example, about 500 sccm, about 1000 sccm, about 1500 sccm, about 2000 sccm, about 2500 sccm, etc. However, this disclosure is not limited thereto.
[0062] Then, in step 212, method 200 includes activating a plasma source to introduce plasma into the reaction chamber. In some embodiments, plasma source 105 is activated to introduce plasma into reaction chamber 120. In some embodiments, the power of plasma source 105 is greater than 0 and less than 6000W, such as about 500W, about 1000W, about 1500W, about 2000W, about 2500W, about 3000W, about 3500W, about 4000W, about 4500W, about 5000W, about 5500W, etc. However, this disclosure is not limited thereto. In step 214, method 200 includes pulsed connection to an RF power source of the substrate support. In some embodiments, pulsed (i.e. activated) an RF power source 123 connected to the substrate support 111. In some embodiments, the time period for introducing plasma into reaction chamber 120 is substantially the same as the time period for pulsed connection to the RF power source 123 of the substrate support 111. In some embodiments, the power of the RF power source 123 is higher than 0 and lower than 1000W, such as approximately 100W, approximately 200W, approximately 300W, approximately 400W, approximately 500W, approximately 600W, approximately 700W, approximately 800W, approximately 900W, etc. In some embodiments, the duty cycle of the RF power source is higher than 10% and lower than 90%, such as approximately 20%, approximately 30%, approximately 40%, approximately 50%, approximately 60%, approximately 70%, approximately 80%, etc. In some embodiments, the pulse frequency of the RF power is higher than 0 and lower than 100kHz, such as approximately 10kHz, approximately 20kHz, approximately 30kHz, approximately 40kHz, approximately 50kHz, approximately 60kHz, approximately 70kHz, approximately 80kHz, approximately 90kHz, etc. In some embodiments, the RF frequency of the RF power is higher than 13.56MHz and lower than 60MHz, such as approximately 15MHz, approximately 20MHz, approximately 30MHz, approximately 40MHz, approximately 50MHz, etc. However, this disclosure is not limited thereto.
[0063] In step 216, method 200 includes generating a reactive substance from the reactant gas while both the plasma source and the RF power source are activated. In some embodiments, the reactive substance is generated from the reactant gas when both the plasma source 105 and the RF power source 123 are activated. In step 218, method 200 includes reacting the reactive substance with a reactive precursor to form a material between the gaps (which will...) Figures 5A to 5C(as shown in the figure). In some embodiments, the process pressure for reacting the reactant gas with the precursor is higher than 1 Torr and lower than 9 Torr, for example, about 2 Torr, about 3 Torr, about 4 Torr, about 5 Torr, about 6 Torr, about 7 Torr, about 8 Torr, etc. In some embodiments, the process temperature for reacting the reactant gas with the precursor is higher than 0°C and lower than 1000°C, for example, about 100°C, about 200°C, about 300°C, about 400°C, about 500°C, about 600°C, about 700°C, about 800°C, about 900°C, etc. However, this disclosure is not limited thereto. In step 220, method 200 includes shutting down the plasma source when the pulse of the RF power source ends. In some embodiments, the plasma source 105 is shut down when the pulse of the RF power source 123 ends. In some embodiments, after the plasma source 105 is shut down, the reaction chamber 120 is purged with an inert gas. It should be noted that in some embodiments, the above purging step is optional and may be omitted.
[0064] It should be noted that multiple steps are provided in the specific order described above. However, this disclosure is not limited thereto. Those skilled in the art will be able to add, substitute, or repeat specific steps in method 200 to form material between gaps on substrate 110, and some of the steps described above may be performed simultaneously. These variations are also included within the scope of this disclosure and will not be listed individually below.
[0065] Figure 3 This is a timing diagram based on some embodiments of the present disclosure. Figure 3 As shown, in the feeding step, a precursor and an inert gas are introduced into the reaction chamber 120. Specifically, the precursor source 103 is activated and the second valve 116 is opened to allow the precursor to flow from the precursor source 103 into the reaction chamber 120. For example, the precursor includes silane, silane, propane, bis(isopropylamino)silane, dichlorosilane, trichlorosilane, or monomethylsilane. However, this disclosure is not limited thereto. Next, in the purging step, the second valve 116 is closed to cut off the flow of the precursor into the reaction chamber 120. The inert gas is still supplied to the reaction chamber 120 to purge the reaction chamber 120. It should be noted that in some embodiments, the purging step is optional and may be omitted.
[0066] Next, in the plasma step, after purging the reaction chamber 120, a reactant gas is introduced into the reaction chamber 120. In some embodiments, the reactant gas is introduced into the reaction chamber 120 by activating the reactant source 104 and opening the third valve 117. For example, the reactant gas includes oxygen or hydrogen peroxide. In some embodiments, the flow rate of the introduced reactant gas is higher than 0 and lower than 3000 sccm, for example, about 500 sccm, about 1000 sccm, about 1500 sccm, about 2000 sccm, about 2500 sccm, etc. However, this disclosure is not limited thereto. Simultaneously, in the plasma step, the plasma source 105 is activated to introduce plasma into the reaction chamber 120. In some embodiments, the power of the plasma source 105 is higher than 0 and lower than 6000W, such as about 500W, about 1000W, about 1500W, about 2000W, about 2500W, about 3000W, about 3500W, about 4000W, about 4500W, about 5000W, about 5500W, etc.
[0067] In the plasma step, a pulse (i.e., activation) is connected to an RF power source 123 on the substrate support 111. In some embodiments, the time period for introducing plasma into the reaction chamber 120 is substantially the same as the time period for pulsed RF power source 123. In some embodiments, the power of RF power source 123 is above 0 and below 1000W, such as about 100W, about 200W, about 300W, about 400W, about 500W, about 600W, about 700W, about 800W, about 900W, etc. In some embodiments, the duty cycle of RF power source is above 10% and below 90%, such as about 20%, about 30%, about 40%, about 50%, about 60%, about 70%, about 80%, etc. In some embodiments, the pulse frequency of RF power is above 0 and below 100kHz, such as about 10kHz, about 20kHz, about 30kHz, about 40kHz, about 50kHz, about 60kHz, about 70kHz, about 80kHz, about 90kHz, etc. In some embodiments, the RF frequency of the RF power is higher than 13.56 MHz and lower than 60 MHz, such as about 15 MHz, about 20 MHz, about 30 MHz, about 40 MHz, about 50 MHz, etc. However, this disclosure is not limited thereto.
[0068] During the plasma step, when both plasma source 105 and RF power source 123 are activated, reactive material is generated from the reactant gas. The reactive material reacts with the precursors of the reaction to form material between the gaps (this will...). Figures 5A to 5C(as shown in the figure). In some embodiments, the process pressure for reacting the reactant gas with the precursor is higher than 1 Torr and lower than 9 Torr, for example, about 2 Torr, about 3 Torr, about 4 Torr, about 5 Torr, about 6 Torr, about 7 Torr, about 8 Torr, etc. In some embodiments, the process temperature for reacting the reactant gas with the precursor is higher than 0°C and lower than 1000°C, for example, about 100°C, about 200°C, about 300°C, about 400°C, about 500°C, about 600°C, about 700°C, about 800°C, about 900°C, etc. However, this disclosure is not limited thereto.
[0069] Next, during the purging step, both plasma source 105 and RF power source 123 are deactivated, and the third valve 117 is closed to cut off the flow of reactant gas into reaction chamber 120. Inert gas is still supplied to reaction chamber 120 to purge it. It should be noted that this process is repeatable. Figure 3 The timing shown is for forming material between gaps on substrate 110. It should be noted that in some embodiments, the purging step is optional and may be omitted.
[0070] Figure 4A This is a schematic diagram of the surface of a substrate 110 according to some embodiments of the present disclosure. Figure 4B This is a diagram showing the thickness of the film on the surface of substrate 110 according to some embodiments of the present disclosure. For example... Figure 4A As shown, multiple measurement points are arranged on substrate 110. Substrate 110 is divided into a central region, an intermediate region, and an edge region, with the intermediate region sandwiched between the central region and the edge region. These measurement points are distributed in the central region, intermediate region, and edge region of substrate 110. In some embodiments, the distance between the center of substrate 110 and the central region can be in the range of 0 to about 49 mm. The distance between the center of substrate 110 and the intermediate region can be in the range of about 49 nm to about 98 mm. The distance between the center of substrate 110 and the edge region can be in the range of about 98 nm to about 147 mm. However, this disclosure is not limited thereto.
[0071] like Figure 4B As shown, when only plasma source 105 is used, the thickness of the deposited film is not uniform. For example, the film thickness deposited using plasma source 105 is only thicker at the edges of substrate 110. Conversely, when plasma source 105 and continuously activated RF power source 123 are used, the thickness of the deposited film is relatively uniform. However, the thickness of the deposited film is also relatively low, thus requiring more process time and cost. When plasma source 105 and pulsed RF power source 123 are used, the thickness of the deposited film is highly uniform and higher than in other processes. Therefore, depositing films using pulsed bottom RF power can improve film uniformity.
[0072] Figures 5A to 5CThese are cross-sectional views of semiconductor structures according to some embodiments of the present disclosure. Figure 5A As shown, the substrate 110 includes a plurality of fins 502 and a liner 504 formed on the fins 502. For example, the liner 504 includes SiN or other dielectric materials. Figure 5B and Figure 5C As shown, material 506 is formed on the liner 504 and between the fins 502. For example, the liner 504 comprises SiO or other dielectric material. It should be noted that... Figure 5B The deposition of material 506 using only plasma source 105 is shown, and Figure 5C The deposition of material 506 using plasma source 105 and pulsed RF power source 123 is shown. Therefore, deposition using plasma source 105 and pulsed RF power source 123 can cause less damage to the underlying liner 504 compared to using plasma source 105 alone. That is, the liner 504 is relatively thick after the deposition of material 506, which also improves film uniformity and quality.
[0073] The methods and systems disclosed herein can be used to deposit multiple films, such as, by way of non-limiting examples, silicon (Si) films and boron (B) films, as well as metal-containing films, metal oxide films, and metal nitride films, such as films containing aluminum (Al), molybdenum (Mo), titanium (Ti), hafnium (Hf), tungsten (W), magnesium (Mg), tantalum (Ta), strontium (Sr), etc. The methods and systems disclosed herein can be used to increase the reactivity of certain precursors, such as, by way of non-limiting examples, silicon-containing precursors, boron-containing precursors, and metal-containing precursors, such as those containing aluminum, molybdenum, titanium, hafnium, tungsten, magnesium, tantalum, strontium, etc. Precursors and the radicalized precursors formed therefrom may contain silicon, boron, and one or more metals selected from aluminum, molybdenum, titanium, hafnium, tungsten, magnesium, tantalum, and strontium. Suitable precursors may include those known to be usable in CVD processes. In some embodiments, the precursor may be used in a CVD-type deposition process, but may be non-reactive in an ALD-type deposition process. In this case, the radicalization of the precursor makes it reactive during ALD-type deposition.
[0074] In some embodiments, the reactive gas may be an oxygen-containing gas. For example, the oxygen-containing gas may be selected from one or more of the following: oxygen (O2), ozone (O3), water (H2O), hydrogen peroxide (H2O2), alcohols (ROH, where R is alkyl or aryl) (such as methanol (CH3OH) and ethanol (C2H5OH)), nitrogen dioxide (NO2), nitrous oxide (N2O), and oxygen atoms (O2) generated in plasma. *In some embodiments, the reactive gas may be a nitrogen-containing gas. For example, the nitrogen-containing gas may be selected from one or more of the following: ammonia (NH3), hydrazine (N2H4), nitric oxide (NO), reactive nitrogen (N2), reactive ammonia (NH3), and nitrogen atoms (N2) generated in the plasma. * In some embodiments, the reactive gas may be selected from hydrogen (H2) and hydrogen atoms (H2) generated in the plasma. * One or more of the following: O2, H2O, NH3, and H2. In some embodiments, the reactive gas includes one or more of O2, H2O, NH3, and H2. In some embodiments, the reactive gas may contain O2. * N * H * and their combinations.
[0075] The methods and systems disclosed herein can provide several benefits, including improved underlying layer damage and formation of materials with high quality and high deposition rates. The methods and systems disclosed herein advantageously utilize pulsed bottom RF power to form materials between gaps on a substrate. The disclosed methods can improve film uniformity and conformability while minimizing damage to the underlying liner. These and other advantages will become apparent from the various aspects, embodiments, and configurations disclosed herein.
[0076] Although embodiments of the present disclosure and their advantages have been described in detail, it should be understood that various changes, substitutions, and modifications may be made herein without departing from the spirit and scope of the disclosure as defined by the appended claims. For example, those skilled in the art will readily understand that many features, functions, processes, and materials described herein may vary while still remaining within the scope of the present disclosure. Furthermore, the scope of this application is not intended to be limited to the specific embodiments of the processes, machines, manufactures, compositions of matter, apparatuses, methods, and steps described in the specification. Those skilled in the art will readily understand from the disclosure of this publication that, according to this disclosure, existing or later-developed processes, machines, manufactures, compositions of matter, apparatuses, methods, or steps that perform substantially the same functions or achieve substantially the same results as the corresponding embodiments described herein can be utilized. Therefore, the appended claims are intended to include such processes, machines, manufactures, compositions of matter, apparatuses, methods, or steps within their scope. Additionally, the scope of this disclosure is defined by the scope of the appended claims. Furthermore, each scope of the claims is constructed as a separate embodiment, and various combinations of claims and combinations of embodiments are within the scope of this disclosure.
Claims
1. A method for forming a film between gaps on a substrate, comprising: The substrate is introduced onto a substrate support in the reaction chamber; The precursor is introduced into the reaction chamber; To cause the precursor to react with the surface of the substrate; The plasma is introduced from the plasma source into the reaction chamber; The reactant gas is introduced into the reaction chamber; The pulse is connected to the RF power source of the substrate support; When both the plasma source and the RF power source are activated, reactive substances are generated from the reactant gas; as well as The reactive substance reacts with the precursor on the surface to form a film on the substrate.
2. The method as described in claim 1, wherein, The precursors include silane, ethylsilane, propane, di(isopropylamino)silane, dichlorosilane, trichlorosilane, or monomethylsilane.
3. The method as described in claim 1, wherein, The reactant gas includes oxygen or hydrogen peroxide.
4. The method of claim 1, wherein, The time period for introducing the plasma into the reaction chamber is substantially the same as the time period for the RF power source pulsed to the substrate support.
5. The method of claim 1, further comprising a purging step after introducing the precursor into the reaction chamber and before introducing the reactant gas into the reaction chamber.
6. The method of claim 1, wherein, The flow rate of the introduced precursor is above 0 and below 3000 sccm.
7. The method of claim 1, wherein, The flow rate of the introduced reactant gas is above 0 and below 3000 sccm.
8. The method of claim 1, wherein, The power of the plasma source is higher than 0 and lower than 6000W.
9. The method of claim 1, wherein, The power of the RF power source is higher than 0 and lower than 1000W.
10. The method of claim 1, wherein, The duty cycle of the RF power source is higher than 10% and lower than 90%.
11. The method of claim 1, wherein, The pulse frequency of the RF power is higher than 0 and lower than 100kHz.
12. The method of claim 1, wherein, The RF frequency of the RF power is higher than 13.56MHz and lower than 60MHz.
13. The method of claim 1, wherein, The process pressure for reacting the reactant gas with the precursor is higher than 1 Torr and lower than 9 Torr.
14. The method of claim 1, wherein, The process temperature for reacting the reactant gas with the precursor is above 0°C and below 1000°C.
15. A method for forming material between gaps on a substrate, comprising: The substrate is introduced onto a substrate support in the reaction chamber; The precursor is introduced into the reaction chamber; To cause the precursor to react with the surface of the substrate; After the precursor reaction, the reaction chamber is purged with an inert gas; After purging the reaction chamber, the reactant gas is introduced into the reaction chamber; Activate the plasma source to introduce plasma into the reaction chamber; The pulse is connected to the RF power source of the substrate support; When both the plasma source and the RF power source are activated, reactive substances are generated from the reactant gas; The reactive substance reacts with the precursor of the reaction to form material in the interstitial space; as well as When the pulse from the RF power source ends, the plasma source is deactivated.
16. The method of claim 15, further comprising: While the precursor and reactant gases are introduced into the reaction chamber, the inert gas is also introduced into the reaction chamber.
17. The method of claim 16, further comprising: After the plasma source is shut down, the reaction chamber is purged with the inert gas.
18. A semiconductor processing apparatus, comprising: Reaction chamber; The plasma source is located at the top of the reaction chamber; A substrate support, located at the bottom of the reaction chamber, supports the substrate; An ion filter is located between the plasma source and the substrate support. An RF power source is connected to a substrate support and configured to radially distribute plasma on the substrate; as well as Precursor and reactant sources are in fluid communication with the reaction chamber.
19. The semiconductor processing apparatus of claim 18, further comprising a controller configured as follows: The precursor is introduced from the precursor source into the reaction chamber; The reaction chamber was purged after the precursor was introduced; The reactant gas is introduced from the reactant source into the reaction chamber; Activating the plasma source and pulsed the RF power source to form a film on the substrate by reacting the reactant gas with the precursor; and After the film is formed on the substrate, the reaction chamber is purged.
20. The semiconductor processing apparatus of claim 18, wherein, The plasma source is an inductively coupled plasma source.