A surface treatment method for Christmas stand accessories

By treating Christmas stand accessories with an electrophoresis process, the problems of short coating warranty period and high energy consumption have been solved, and the durability of the coating has been improved and energy consumption reduced.

CN123108701APending Publication Date: 2026-11-17JINHUA XIANGTAI IND & TRADE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611513434.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-28
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

The existing shot blasting and powder coating process for Christmas stand accessories has a short warranty period, making it difficult to meet customers' requirements for product durability, and it also consumes a lot of energy.

Method used

Electrophoresis is used to replace shot blasting. Through steps such as degreasing, water washing, film treatment, electrophoresis, ultrafiltration rinsing and paint curing, oil and impurities on the surface of the workpiece are gradually removed, and the coating is cured at high temperature to form a uniform electrophoretic coating.

Benefits of technology

It improves the adhesion and corrosion resistance of the coating, extends the product's shelf life, and reduces energy consumption during the processing.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a surface treatment method for Christmas stand accessories, belonging to the field of metal surface treatment technology. The method sequentially includes degreasing, a first water wash, a film treatment, a second water wash, a pure water wash, electrophoresis, ultrafiltration rinsing, a third pure water wash, dripping, paint curing, and cooling before unloading. By using electrophoresis instead of traditional shot blasting for surface treatment of Christmas stand accessories, it is beneficial to improve the adhesion and corrosion resistance of the workpiece surface coating, extend the product warranty period, and simultaneously reduce energy consumption during the processing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of metal surface treatment technology, and specifically discloses a surface treatment method for Christmas stand accessories. Background Technology

[0002] Christmas tree stand accessories are an important component of Christmas decorations, and the products are exported to Europe, America, and Southeast Asia. Currently, most Christmas tree stand accessories on the market undergo shot blasting and powder coating for surface treatment. Products treated with shot blasting and powder coating have a relatively short quality guarantee period for their surface coating, making it difficult to meet customers' requirements for product durability. Furthermore, shot blasting is an energy-intensive process, which is detrimental to production cost control. Summary of the Invention

[0003] The main technical problem this invention aims to solve is that the surface coating of Christmas stand accessories processed by existing shot blasting and powder coating processes has a short warranty period and cannot meet customers' requirements for product durability. Secondary technical problems include the high energy consumption during existing shot blasting processes.

[0004] To solve the above-mentioned technical problems, the present invention adopts the following technical solution:

[0005] A surface treatment method for Christmas stand accessories includes the following steps:

[0006] Step 1: Degrease the workpiece (immerse in ultrasonic heating for 3 minutes).

[0007] Step 2: Degrease the workpiece with a spray (spray rinse for 2 minutes).

[0008] Step 3: Perform a first water rinse on the degreased workpiece (soak for 1.5 minutes).

[0009] Step 4: After the first water wash and soaking (rinse with water spray for 1.5 minutes)

[0010] Step 5: Apply a coating treatment to the workpiece after the first water wash (soak the coating for 2.5 minutes).

[0011] Step 6: Perform a second water rinse on the workpiece after the coating treatment; (spray rinse for 1 minute)

[0012] Step 7: Rinse the workpiece with pure water after the second rinse (soak for 1 minute).

[0013] Step 8: After immersing the workpiece in pure water for the second time: (spray and rinse for 1 minute)

[0014] Step 9: Perform electrophoretic treatment on the workpiece after rinsing with pure water (electrophoresis for 2 minutes).

[0015] Step 10: Perform ultrafiltration rinsing on the electrophoretic workpiece; (spray rinse for 1 minute)

[0016] Step 11: Perform a third pure water rinse on the workpiece after ultrafiltration rinsing (soak for 2 minutes).

[0017] Step 12: Rinse the workpiece after the third pure water wash with water (spray rinsing).

[0018] Step 13: Perform a drip treatment on the workpiece after the third pure water wash;

[0019] Step 14: Curing the paint on the workpiece after the water dripping treatment; (curing time 50 minutes)

[0020] Step 15: Cool the workpiece after the paint has cured (15 minutes).

[0021] Furthermore, the degreasing process includes sequential soaking degreasing and spray degreasing.

[0022] Furthermore, the treatment temperature for both soaking degreasing and spray degreasing is 35–45°C.

[0023] Furthermore, the first water wash includes a soaking water wash and a spray water wash performed sequentially.

[0024] Furthermore, the coating treatment is an immersion coating treatment.

[0025] Furthermore, the second water wash includes a sequential spray water wash and a pure water wash.

[0026] Furthermore, the electrophoretic treatment temperature is 28–32°C.

[0027] Furthermore, the ultrafiltration rinsing includes sequential UF1 spraying and UF2 soaking, and UF3 soaking.

[0028] Furthermore, the curing temperature of the paint is 160–260°C.

[0029] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0030] 1. This application uses electrophoresis to replace the traditional shot blasting process for surface treatment of Christmas stand accessories. The electrophoretic coating can uniformly cover all parts of the workpiece surface, which is beneficial to improving the adhesion and corrosion resistance of the coating, thereby extending the product's warranty period.

[0031] 2. By sequentially setting pretreatment steps such as degreasing, first water washing, film treatment, second water washing and pure water washing before electrophoresis, this application can gradually remove oil and impurities from the surface of the workpiece and form a conversion film on the surface of the workpiece, which is beneficial to improving the adhesion and surface quality of the subsequent electrophoretic coating.

[0032] 3. By sequentially setting up post-treatment steps such as ultrafiltration rinsing, third pure water rinsing, water dripping, and paint curing after electrophoresis, this application can remove residual electrophoretic liquid on the workpiece surface and fully cure the coating at high temperature, which is beneficial to further improve the smoothness and durability of the product surface coating.

[0033] 4. Compared with the traditional shot blasting and powder coating process, the electrophoresis process does not require high-speed abrasive blasting, which helps to reduce energy consumption during the process. Detailed Implementation

[0034] The technical solutions in the embodiments of the present invention have been clearly and completely described. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of them. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0035] Furthermore, the use of terms such as "first" and "second" in this invention is for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. Additionally, the technical solutions of the various embodiments can be combined with each other, but only on the basis of being achievable by those skilled in the art. When the combination of technical solutions is contradictory or impossible to implement, such a combination of technical solutions should be considered non-existent and not within the scope of protection claimed by this invention.

[0036] The surface treatment method for Christmas stand accessories in this embodiment involves the following fifteen processes sequentially on a continuous production line:

[0037] Step 1: Immersion Degreasing. The Christmas stand parts to be treated are immersed in an immersion degreasing tank with an effective length of 6.0 meters and a treatment temperature of 35-45℃. Immersion degreasing can dissolve and remove most of the oil and dirt from the surface of the workpiece.

[0038] Step 2: Spray degreasing. The workpieces after soaking and degreasing are then sprayed for degreasing. The effective length of the spray degreasing tank is 3.0 meters, and the treatment temperature is 35-45℃. Spray degreasing further removes residual oil stains from the workpiece surface by utilizing the impact force of the liquid.

[0039] Step 3: Water washing and soaking. The workpieces after spray degreasing are then soaked in water. The effective length of the first water washing and soaking tank is 6 meters, and the treatment temperature is room temperature. This step is used to wash away any residual degreasing agent on the surface of the workpieces.

[0040] Step 4: Second water rinse. The workpieces, after soaking and rinsing, are then subjected to a second water rinse. The effective length of the first water rinse spray tank is 3 meters, and the treatment temperature is room temperature. This step is used to further rinse away any residual degreasing agent and impurities on the workpiece surface.

[0041] Step 5: Film Immersion. The washed workpieces undergo an immersion film treatment. The effective length of the immersion tank is 5.5 meters, and the treatment temperature is room temperature. This film treatment forms a conversion film on the workpiece surface, providing a good bonding substrate for subsequent electrophoretic coating.

[0042] Step Six: Three-Spray Water Wash. The workpieces after the coating treatment are washed with water spray. The effective length of the second water wash spray tank is 1.6 meters, and the treatment temperature is room temperature. This step is used to wash away the residual coating treatment solution on the surface of the workpieces.

[0043] Step Seven: Pure Water Rinse and Immersion. The workpieces, after being spray-washed, undergo an immersion rinse in pure water. The effective length of the first pure water immersion tank is 0.6 meters, and the processing temperature is room temperature. This step uses pure water to further clean the workpiece surface, preventing impurities from being carried into the electrophoresis tank.

[0044] Step 8: Pure water rinse with two sprays. The workpieces, after being immersed in pure water, undergo a second pure water rinse using a spray system. The effective length of the second pure water rinse tank is 1.6 meters, and the treatment temperature is room temperature. This step further ensures that the cleanliness of the workpiece surface meets the requirements for electrophoresis.

[0045] Step Nine: Electrophoresis. The workpieces, after being washed with pure water, undergo electrophoretic treatment. The effective length of the electrophoresis tank is 5.0 meters, and the treatment temperature is 28–38℃. Electrophoresis causes charged paint particles to migrate directionally under the influence of an electric field and deposit onto the workpiece surface, forming a uniform and continuous coating.

[0046] Step 10: UF1 spraying. The workpieces after electrophoresis are subjected to UF1 spraying. The effective length of the UF1 spraying device is 1.6 meters, and the processing temperature is room temperature. UF1 spraying uses ultrafiltration recovery liquid to rinse away residual paint on the surface of the workpieces.

[0047] Step 11: UF2 Immersion. The workpieces after UF1 spraying are immersed in UF2. The effective length of the UF2 immersion tank is 0.6 meters, and the treatment temperature is room temperature. UF2 immersion further removes residual electrophoretic solution from the surface and crevices of the workpieces.

[0048] Step 12: Pure water rinsing and spraying. The workpieces soaked in UF2 are subjected to a pure water rinsing spray. The effective length of the third pure water rinsing spray tank is 1.6 meters, and the treatment temperature is room temperature. This step ensures that there is no residual electrophoretic solution or impurities on the surface of the workpiece.

[0049] Step Thirteen: Drip Treatment. The workpieces, after being washed with pure water, undergo a drip treatment. The effective length of the drip area is 24.0 meters, and the treatment temperature is room temperature. The drip treatment allows the moisture on the workpiece surface to drip off naturally, reducing the amount of moisture brought into the curing oven.

[0050] Step Fourteen: Paint Curing. The workpiece after dripping water is then cured with paint. The effective length of the paint curing oven is 72.0 meters, and the processing temperature is 160–260℃. Paint curing allows the electrophoretic coating to undergo a cross-linking reaction at high temperature, fully curing it to form the final surface protective layer.

[0051] Step 15: Cooling and Unloading. The cured workpiece is cooled and unloaded. The effective length of the cooling and unloading zone is 24.0 meters, and the processing temperature is room temperature. After the workpiece cools to room temperature, it is removed from the production line, completing the entire surface treatment process.

[0052] The Christmas stand accessories processed through the above process have an improved surface coating quality compared to the traditional shot blasting and powder coating process, which helps to extend the product's warranty period and also helps to reduce energy consumption during the processing.

[0053] The above description represents the preferred embodiments of the present invention. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principles of the present invention, and these improvements and modifications are also considered to be within the scope of protection of the present invention.

Claims

1. A surface treatment method for a Christmas tree stand accessory, characterized in that, The steps are as follows: Degreasing treatment is performed on the workpiece; The degreased workpiece is then subjected to a first water wash; Apply a coating to the workpiece after the first water wash; The workpiece after the coating treatment is then rinsed a second time with water. The workpiece is then rinsed with pure water after the second water wash; Electrophoretic treatment is performed on the workpiece after it has been washed with pure water. The workpiece after electrophoresis is rinsed with ultrafiltration. The workpiece after ultrafiltration rinsing is then rinsed a third time with pure water. The workpiece after the third pure water wash is subjected to a drip treatment; the workpiece after the drip treatment is then cured with paint; the workpiece after the paint has cured is then cooled and removed from the machine.

2. The surface treatment method of a Christmas stand accessory according to claim 1, characterized in that, The degreasing process includes sequential soaking degreasing and spray degreasing.

3. The surface treatment method of a Christmas stand accessory according to claim 2, characterized in that, The treatment temperatures for both soaking degreasing and spray degreasing are 35–45°C.

4. The surface treatment method of a Christmas stand accessory according to claim 1, characterized in that, The first water wash includes a soaking water wash and a spray water wash performed sequentially.

5. The surface treatment method of a Christmas stand accessory according to claim 1, wherein The coating treatment is an immersion coating treatment.

6. The surface treatment method for Christmas stand accessories according to claim 1, characterized in that, The second water wash includes a sequential spray water wash and a pure water wash.

7. The surface treatment method of a Christmas stand accessory according to claim 1, wherein The electrophoretic treatment temperature is 28–38°C.

8. The surface treatment method of a Christmas stand accessory according to claim 1, wherein The ultrafiltration rinsing includes sequential UF1 spraying and UF2 soaking.

9. The surface treatment method of a Christmas stand accessory according to claim 1, wherein The curing temperature of the paint is 160–260°C.