Methods and systems for maintaining temporary prestress in precast concrete segmental beams in marine environments
By using a prestress retention system that combines a constant force energy storage compensator with threaded steel bars in a marine environment, the problem of temporary prestress retention in precast concrete segmental beams was solved, and the stability and long-term durability of joint compressive stress were improved.
Patent Information
- Application Number
- CN202611291546.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-25
- Publication Date
- 2026-11-17
AI Technical Summary
In marine environments, existing technologies struggle to effectively maintain the temporary prestress of precast concrete segmental beams, leading to a continuous attenuation of joint compressive stress during epoxy resin curing, which affects assembly quality and durability.
A prestress retention system combining a constant force energy storage compensator and threaded steel bars is adopted. By pre-drilling holes in the steel toothed sill and installing the constant force energy storage compensator, the mechanical energy storage and pressure release characteristics are used to automatically compensate for the shrinkage deformation of the precast concrete segmental beam and maintain the stability of the joint surface compressive stress.
It improves the shear, tensile, and impermeability properties of precast concrete segmental beam joints, reduces the number of manual tensioning operations, enhances long-term durability, and reduces construction risks.
Smart Images

Figure CN123109062A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of segmental beam assembly technology, and more specifically, relates to a method and system for maintaining temporary prestress in precast concrete segmental beams in a marine environment. Background Technology
[0002] In large-scale bridge projects such as cross-sea bridges, the assembly of precast concrete segmental beams is widely used due to its advantages such as high construction efficiency, controllable quality, and minimal impact on navigation and the environment. When assembling two adjacent precast concrete segmental beams, epoxy resin adhesive is applied to the joint surfaces to ensure good filling and tight interlocking. A temporary prestressing system is then used to establish a certain axial compressive stress between the joints. This axial compressive stress allows the epoxy resin adhesive to cure under pressure, thereby ensuring the shear, tensile, and impermeability properties of the joint. Whether the temporary prestress can be stably maintained during the epoxy resin curing process is one of the key factors determining the quality of the segmental beam assembly.
[0003] In existing technologies, temporary prestressed systems typically consist of prestressing tendons, anchoring devices, hydraulic jacks, support plates, and corresponding tensioning equipment. The prestressing tendons are mostly made of finely rolled threaded steel bars or steel strands. During construction, the prestressing tendons are first passed through pre-embedded ducts within the segmental beam. Hydraulic jacks are then used to tension the tendons according to the designed control stress, ensuring the joint surface of the segmental beam reaches the set axial compressive stress. Subsequently, the prestressing tendons are locked using anchors and clamps to maintain joint pressure. Simultaneously, to monitor the prestressing status, existing technologies often employ hydraulic gauge readings, pressure sensors, or displacement gauges for phased monitoring. Construction personnel periodically check and record data after tensioning, and manual tensioning is performed when a significant drop in compressive stress is observed. After the epoxy resin adhesive reaches its designed curing strength, the temporary prestressing device is removed or converted to a permanent prestressed system.
[0004] However, the marine environment is characterized by high salinity, high humidity, large diurnal and seasonal temperature differences, and frequent wind and wave loads. During construction, there are also disturbances such as equipment vibration and segmental beam assembly errors. Under the combined influence of these factors, prestressed tendons will experience stress relaxation, anchorages and wedges will retract or slip, and the concrete of the segmental beams and the epoxy resin at the joints will undergo shrinkage, creep, and flexural deformation. This causes the axial compressive stress to continuously decay during the epoxy resin curing period, and the decay process is often nonlinear and uncertain. Therefore, existing technologies cannot effectively solve the problem of maintaining temporary prestress under marine environments and complex construction conditions. Summary of the Invention
[0005] To address the aforementioned deficiencies or improvement needs of existing technologies, this invention provides a method and system for maintaining temporary prestress in precast concrete segmental beams in marine environments. By constructing a reliable system capable of adaptively maintaining joint compressive stress, it achieves higher reliability in harsh marine environments and reduces the number of manual tensioning attempts and subjective judgment errors. This forms a passive adaptive closed-loop maintenance capability, effectively reducing the risk of temporary prestress falling below the critical value and improving the shear, tensile, impermeability, and long-term durability of precast concrete segmental beam assembly joints.
[0006] To achieve the above objectives, the present invention provides a method for maintaining temporary prestress in precast concrete segmental beams in a marine environment, comprising the following steps: S1: Before assembling the precast concrete segmental beam, the upper limit of the equivalent stiffness of the constant force energy storage compensator is obtained based on the meteorological data of the construction sea area and the relevant data of the precast concrete segmental beam. S2: Anchor steel toothed brackets on the bottom and top plates of each adjacent precast concrete segment beam, and each steel toothed bracket has multiple reserved holes pre-drilled; apply epoxy resin adhesive to the matching surface of the precast concrete segment beam, and pass the threaded steel bars through the corresponding reserved holes of the adjacent steel toothed brackets. S3: At the tensioning end of the threaded steel bar, a constant force energy storage compensator that meets the upper limit of the equivalent stiffness is inserted into the threaded steel bar, so that the constant force energy storage compensator is clamped between the bearing surface of the steel toothed sill and the locking nut. S4: Use a jack to apply tension to the threaded steel bar to the corresponding tonnage, so that the compressive stress on the joint surface reaches the initial target compressive stress of the joint. At the same time, the constant force energy storage compensator is compressed to the designed energy storage stroke. After that, tighten the lock nut to lock it and remove the jack. S5: During the curing cycle of the epoxy resin adhesive, when the precast concrete segment beam shrinks and deforms, causing the threaded steel bars to show a tendency to relax, the constant force energy storage compensator in the state of compression energy storage automatically releases the rebound displacement to fill the shrinkage gap of the precast concrete segment beam, so that the actual compressive stress on the joint surface is not lower than the minimum allowable compressive stress of the joint. S6: After the longitudinal prestressed steel strands in the body are tensioned and the entire bridge system is converted, loosen the locking nut and remove the constant force energy storage compensator, threaded steel bars and steel toothed sill in sequence.
[0007] Furthermore, in step S1, the upper limit of the total equivalent stiffness of the joint surface is calculated as follows: ; In the formula, This represents the upper limit of the total equivalent stiffness of the joint surface. This refers to the cross-sectional area of the joint. The initial target compressive stress of the joint; This represents the minimum allowable compressive stress at the joint. The coefficient of linear expansion of precast concrete; It is the longitudinal equivalent length between the anchorage points of two adjacent precast concrete beam segments; For extreme theoretical temperature differences; This represents the extreme values of short-term shrinkage and creep of two adjacent precast concrete segment beams during the curing period.
[0008] Furthermore, in step S3, the constant force energy storage compensators arranged on the top and bottom plates of the precast concrete segment beams corresponding to the same joint surface have the following coordination relationship: ; ; In the formula, The equivalent stiffness of the constant force energy storage compensator on the top slab side of the precast concrete segmental beam; The equivalent stiffness of the constant force energy storage compensator on the bottom slab side of the precast concrete segmental beam; This is the vertical temperature gradient correction factor; This is the neutral axis height allocation coefficient; This represents the upper limit of the total equivalent stiffness of the joint surface. This refers to the cross-sectional area of the top slab of the precast concrete segmental beam. This refers to the cross-sectional area of the bottom slab of the precast concrete segmental beam. This refers to the total cross-sectional area of the web of the precast concrete segmental beam. This refers to the cross-sectional area of the joint of the precast concrete segmental beam.
[0009] Furthermore, in step S4, the minimum compensation displacement required by the constant force energy storage compensator is: ; In the formula, To compensate for the displacement; The coefficient of linear expansion of precast concrete; This refers to the total longitudinal length of the precast concrete segmental beam. To lock in the ambient temperature for the system; For extreme low temperature prediction; This represents the shrinkage deformation during the curing period.
[0010] Furthermore, in step S4, when applying tension force to the threaded steel bars, the threaded steel bars on the top and bottom plates of the precast concrete segmental beam are simultaneously and symmetrically tensioned. For the threaded steel bars on the top plate of the precast concrete segmental beam, symmetrical tensioning is performed in the order of first the middle and then the two sides.
[0011] Furthermore, in step S6, after the demolition is completed, one pre-reserved hole in the bottom plate is reserved for each precast concrete segment beam as a ventilation hole, and the remaining holes are sealed tightly by grouting.
[0012] The second aspect of the present invention provides a temporary prestress retention system for precast concrete segmental beams in a marine environment, which applies the retention method described above and is used for each precast concrete segmental beam that is connected to each other, and the joint surface between each precast concrete segmental beam is coated with epoxy resin adhesive. The system is characterized by comprising: steel toothed retainer, threaded steel bar, constant force energy storage compensator and locking nut. Several of the steel toothed brackets are respectively fixed to the top and bottom plates of each precast concrete segment beam; the steel toothed brackets are provided with multiple reserved holes; The same steel toothed sill serves as a common anchorage node between adjacent precast concrete segmental beams. Multiple independent threaded steel bars pass through multiple reserved holes of the steel toothed sill along the longitudinal direction of the bridge and extend to the corresponding steel toothed sill of the adjacent precast concrete segmental beams, forming a relay-type anchorage between adjacent precast concrete segmental beams. The constant force energy storage compensator is sleeved on the outer wall of the tensioning end of the threaded steel bar; The locking nut is screwed onto the end of the threaded steel bar; The constant force energy storage compensator is located between the bearing surface of the steel toothed sill and the locking nut, and the equivalent stiffness of the constant force energy storage compensator is not greater than the preset upper limit of the equivalent stiffness. It is used to maintain the compressive stress on the joint surface by utilizing the mechanical energy storage and pressure release characteristics when the precast concrete segmental beam undergoes volume deformation.
[0013] Furthermore, the specific arrangement of the steel toothed sills is based on the structural type of the precast concrete segmental beam. Specifically: when a steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; three steel toothed sills are arranged on the top plate of the precast concrete segmental beam, one of which is located in the middle of the top plate, and the other two are symmetrically arranged on both sides of the middle steel toothed sill about its longitudinal axis; when no steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; and four steel toothed sills are symmetrically arranged on the top plate of the precast concrete segmental beam about its longitudinal axis.
[0014] Furthermore, the diameter of each threaded steel bar arranged on the top slab of each precast concrete segment beam is 25-30mm, and the tension control force is 260-400kN; the diameter of each threaded steel bar arranged on the bottom slab is 30-35mm, and the tension control force is 400-600kN.
[0015] In summary, compared with the prior art, the above-described technical solutions conceived by this invention can achieve the following beneficial effects: 1. This invention constructs a reliable system that can adaptively maintain joint compressive stress, which is more reliable in harsh marine environments and can reduce the number of manual tensioning operations and subjective judgment errors. It forms a passive adaptive closed-loop maintenance capability, effectively reducing the risk of temporary prestress falling below the critical value, and improving the shear, tensile, impermeability and long-term durability of precast concrete segmental beam assembly joints.
[0016] 2. This invention transforms the abstract marine climate environment disturbance and the inherent rheological properties of materials into a quantified mechanical stiffness constraint, thereby scientifically guiding the selection of stiffness for constant force energy storage compensators, thus abandoning the previous practice of blindly trying and failing based on experience in engineering. Attached Figure Description
[0017] Figure 1 The following is a layout diagram of the system in an embodiment of the present invention, wherein A is a schematic diagram of the layout at the top slab of the precast concrete segmental beam; B is a schematic diagram of the layout at the bottom slab of the precast concrete segmental beam; and C is a corresponding sectional elevation view. Figure 2 This is a schematic diagram of the arrangement of steel toothed sills on the first type of precast concrete segmental beam according to an embodiment of the present invention; Figure 3 This is a schematic diagram of the arrangement of steel toothed supports on the second type of precast concrete segmental beam according to an embodiment of the present invention; Figure 4 This is a schematic diagram of the steps of the holding method in an embodiment of the present invention. Detailed Implementation
[0018] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention. Furthermore, the technical features involved in the various embodiments of this invention described below can be combined with each other as long as they do not conflict with each other.
[0019] Example 1 Please refer to Figures 1 to 3 This invention provides a temporary prestress retention system for precast concrete segmental beams in a marine environment, used for connecting precast concrete segmental beams, and the joint surfaces between precast concrete segmental beams are coated with epoxy resin adhesive, including: steel toothed retainers, threaded steel bars, constant force energy storage compensators and locking nuts. Several of the steel toothed brackets are respectively fixed to the top and bottom plates of each precast concrete segment beam; the steel toothed brackets are provided with multiple reserved holes; The same steel toothed sill serves as a common anchorage node between adjacent precast concrete segmental beams. Multiple independent threaded steel bars pass through multiple reserved holes of the steel toothed sill along the longitudinal direction of the bridge and extend to the corresponding steel toothed sill of the adjacent precast concrete segmental beams, forming a relay-type anchorage between adjacent precast concrete segmental beams. The constant force energy storage compensator is sleeved on the outer wall of the tensioning end of the threaded steel bar; The locking nut is screwed onto the end of the threaded steel bar; The constant force energy storage compensator is located between the bearing surface of the steel toothed sill and the locking nut, and the equivalent stiffness of the constant force energy storage compensator is not greater than the preset upper limit of the equivalent stiffness. It is used to maintain the compressive stress on the joint surface by utilizing the mechanical energy storage and pressure release characteristics when the precast concrete segmental beam undergoes volume deformation.
[0020] Understandably, during use, the constant force energy storage compensator is precisely positioned between the bearing surface of the steel toothed sill and the locking nut, and its equivalent stiffness is not greater than the preset upper limit of equivalent stiffness. This allows it to fully utilize its mechanical energy storage and pressure release characteristics to automatically absorb or release deformation energy when precast concrete segmental beams undergo volume deformation due to complex working conditions such as drastic diurnal temperature variations, tidal loads, and wave impacts in the marine environment. This ensures that the compressive stress on the joint surface is not lower than the minimum critical value required for the curing of the epoxy resin adhesive. Furthermore, compared to traditional rigid anchoring methods, this system fundamentally overcomes the problems of instantaneous loss and continuous attenuation of prestress caused by anchor retraction, concrete shrinkage and creep, and temperature deformation. It effectively avoids the initiation and propagation of micro-cracks inside the epoxy resin adhesive, ensuring dense interlocking and full filling of the joint surface. At the same time, the steel toothed retainer enhances the local bearing capacity and force transmission uniformity, and the constant force output characteristics of the constant force energy storage compensator eliminate the dependence on secondary tensioning, significantly reducing the difficulty and construction risk of high-altitude operations at sea. It significantly improves the mechanical properties, long-term durability, and overall structural safety reserve of the precast concrete segmental beam assembly joints of the cross-sea bridge, demonstrating outstanding engineering application value and technological advancement.
[0021] It should be noted that in this embodiment, the constant force energy storage compensator is a common constant force energy storage compensator in the prior art, such as a disc spring cluster. The disc spring cluster is arranged in a linear series along the axial direction of the threaded steel bar. In other embodiments, other types of constant force energy storage compensators can also be used, which are not specifically limited here.
[0022] In an optional embodiment, the specific arrangement of the steel toothed sills is determined according to the structural type of the precast concrete segmental beam. Specifically: when a steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; three steel toothed sills are arranged on the top plate of the precast concrete segmental beam, one located in the middle of the top plate, and the other two symmetrically arranged on either side of the middle steel toothed sill about its longitudinal axis; when no steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; and four steel toothed sills are symmetrically arranged on the top plate of the precast concrete segmental beam about its longitudinal axis.
[0023] Understandably, during use, the above design ensures the uniformity and reliability of the stress distribution on the joint surface under different structural forms, avoids local stress concentration, and significantly enhances the curing quality of the epoxy resin adhesive and the structural safety of the assembled joint.
[0024] In an optional embodiment, each threaded steel bar arranged on the top slab of each precast concrete segment beam has a diameter of 25-30mm and a tension control force of 260-400kN, while each threaded steel bar arranged on the bottom slab has a diameter of 30-35mm and a tension control force of 400-600kN. This is to ensure that the tension control force of the threaded steel bars is precisely matched with the stress requirements of the precast concrete segment beam, avoiding over-tensioning or under-tensioning, and ensuring uniform distribution of compressive stress on the joint surface.
[0025] Example 2 Please refer to Figures 1 to 4 This invention provides a method for maintaining temporary prestress in precast concrete segmental beams in a marine environment, comprising the following steps: S1: Before assembling the precast concrete segmental beam, the upper limit of the total equivalent stiffness of the joint surface is obtained based on the meteorological data of the construction sea area and the relevant data of the precast concrete segmental beam. Understandably, when assembling precast concrete segmental beams in a marine environment, the curing process of the epoxy resin adhesive at the joints typically takes tens of hours. During this curing period, the precast concrete segmental beams are inevitably affected by the sudden drop in nighttime temperature and the short-term creep of the material itself, resulting in volume shrinkage. This shrinkage leads to a reduction in the elongation of the anchored threaded steel bars, causing a significant loss of compressive stress at the joints. To address this issue, it is crucial to ensure that the decrease in tension of the constant force energy storage compensator during the release of rebound displacement (to fill the shrinkage gaps in the precast concrete segmental beams) is strictly less than the allowable compressive stress loss limit at the joint surface. Based on Hooke's Law and the principle of thermal expansion and contraction of solids, before the formal implementation of the precast concrete segmental beam assembly operation, it is necessary to obtain the upper limit of the total equivalent stiffness of the joint surface that meets the corresponding requirements, based on meteorological data of the construction sea area and the physical properties of the precast concrete segmental beams.
[0026] In an optional embodiment, the upper limit of the total equivalent stiffness of the joint surface is calculated as follows: ; In the formula, This represents the upper limit of the total equivalent stiffness of the joint surface. This refers to the cross-sectional area of the joint. The initial target compressive stress of the joint; This represents the minimum allowable compressive stress at the joint. The coefficient of linear expansion of precast concrete; It is the longitudinal equivalent length between the anchorage points of two adjacent precast concrete beam segments; For extreme theoretical temperature differences; This represents the extreme values of short-term shrinkage and creep of two adjacent precast concrete segment beams during the curing period.
[0027] It should be noted that, The total equivalent stiffness of all constant force energy storage compensators involved in the stress on this section. It is obtained from the design and construction drawings of precast concrete segmental beams, and the area of non-contact areas such as prestressed ducts and ventilation holes needs to be deducted. This refers to the benchmark compressive stress value specified in the temporary stress design code for bridge engineering. Epoxy resin adhesive manufacturers must clearly specify in their product manuals or material inspection reports the minimum compressive stress threshold required to maintain molecular chain crosslinking. The results are obtained from an authoritative report issued by a third-party laboratory after samples of the same batch of concrete mixtures were sent to the precast beam yard during the construction preparation stage for expansion testing under standard thermodynamic conditions. Obtained from the design structural drawings of precast concrete segmental beams. The extreme values of shrinkage monitoring are obtained by continuously collecting deformation data of precast concrete segmental beams of the same batch using dial gauges and strain gauges during the curing period of precast components in the precast beam yard.
[0028] S2: Anchor steel toothed brackets on the bottom and top plates of each adjacent precast concrete segment beam, and each steel toothed bracket has multiple reserved holes pre-drilled; apply epoxy resin adhesive to the matching surface of the precast concrete segment beam, and pass the threaded steel bars through the corresponding reserved holes of the adjacent steel toothed brackets. S3: At the tensioning end of the threaded steel bar, a constant force energy storage compensator that meets the upper limit of the equivalent stiffness is inserted into the threaded steel bar, so that the constant force energy storage compensator is clamped between the bearing surface of the steel toothed sill and the locking nut. Understandably, in the marine outdoor environment, precast concrete segmental beams are exposed to direct sunlight, resulting in extremely drastic temperature gradients and significant diurnal temperature variations in the top slab area. This leads to the most pronounced relative thermodynamic deformation (expansion or contraction) in the top slab. In contrast, the bottom slab is typically located in the shaded area of the box girder and is regulated by cold sea air and seawater evaporation, resulting in relatively gentler temperature changes and smaller deformation. If constant force energy storage compensators with the same equivalent stiffness are used for both the top and bottom slabs, it will inevitably lead to insufficient compensation stroke in the top slab area due to excessive deformation, or excessive compensation in the bottom slab area resulting in excessive initial tension loss. Therefore, a strict asymmetric stiffness matching relationship needs to be established between the constant force energy storage compensators arranged on the same joint surface of the precast concrete segmental beam's top and bottom slabs, allowing the top slab area to achieve a larger mechanical absorption stroke with lower stiffness. After clarifying the different stiffness parameters of the top and bottom slabs of the precast concrete segmental beam, a constant force energy storage compensator that meets the numerical requirements can be selected (such as a disc spring cluster with different numbers or thicknesses). The selected constant force energy storage compensator is then sequentially inserted into the outer wall of the tensioning end of the threaded steel bar that passes through the reserved hole in the steel toothed sill. After that, a lock nut is screwed into the outermost end of the threaded steel bar.
[0029] In an optional embodiment, the constant force energy storage compensators arranged on the top and bottom plates of the precast concrete segmental beams corresponding to the same joint surface have the following matching relationship: ; ; In the formula, The equivalent stiffness of the constant force energy storage compensator on the top slab side of the precast concrete segmental beam; The equivalent stiffness of the constant force energy storage compensator on the bottom slab side of the precast concrete segmental beam; This is the vertical temperature gradient correction factor; This is the neutral axis height allocation coefficient; This represents the upper limit of the total equivalent stiffness of the joint surface. This refers to the cross-sectional area of the top slab of the precast concrete segmental beam. This refers to the cross-sectional area of the bottom slab of the precast concrete segmental beam. This refers to the total cross-sectional area of the web of the precast concrete segmental beam. This refers to the cross-sectional area of the joint of the precast concrete segmental beam.
[0030] It should be noted that, To incorporate historical solar radiation intensity data provided by the local meteorological bureau in the construction area, the data was input into the finite element analysis simulation model of heat conduction in the precast concrete segmental beam. The dimensionless ratio was extracted after steady-state and transient thermodynamic solutions. Furthermore, the vertical temperature gradient correction coefficient ranged from 0.6 to 0.85, ensuring that the compensation stiffness of the top slab was less than that of the bottom slab, in order to achieve more flexible dynamic deformation absorption. , , , All were obtained from the design and construction drawings of precast concrete segmental beams, and met the requirements. . It is the ratio of the height above the centroidal principal axis of the cross section to the total height of the cross section, and is used to equivalently convert the web area to the top and bottom plates according to the stress area.
[0031] S4: Use a jack to apply tension to the threaded steel bar to the corresponding tonnage, so that the compressive stress on the joint surface reaches the initial target compressive stress of the joint. At the same time, the constant force energy storage compensator is compressed to the designed energy storage stroke. After that, tighten the lock nut to lock it and remove the jack. Understandably, existing mechanical constant-force energy storage compensators, such as disc spring assemblies, exhibit a period of mechanical nonlinearity during the initial compression stage due to the initial closure of the gaps between the springs and the dry friction of the contact surfaces. Directly and blindly tensioning to the target tonnage would cause the actual equivalent stiffness of the device to deviate significantly from the theoretical design value. Therefore, a calibration process is necessary. Specifically: an initial tension force is applied to the threaded steel bar using a jack. When the tension force reaches the nonlinearity elimination threshold force, the jack is stopped and pressure is maintained. Simultaneously, the initial compression displacement of the constant-force energy storage compensator at this point is recorded as the geometric zero point for eliminating nonlinear errors. Afterward, the jack is continued to be tensioned to the target tension force, and the actual linear working stroke is monitored.
[0032] Furthermore, due to the extreme temperature differences between day and night in the marine environment, the timing of the locking operation directly determines the thermodynamic deformation that the subsequent system needs to absorb. If locking is performed during the midday high temperature period, the temperature will only decrease afterward (causing volume shrinkage of the precast concrete segmental beams), requiring the constant force energy storage compensator to allow for a large rebound compensation stroke. Conversely, if locking is performed at the early morning low temperature, the precast concrete segmental beams will subsequently expand due to heat, not only eliminating the need for rebound compensation but also further compressing the device. Therefore, when tightening the locking nut, the constant force energy storage compensator needs to be adjusted forward based on the real-time meteorological parameters during the locking operation, i.e., allowing for corresponding compensation.
[0033] In an optional embodiment, the minimum compensation displacement required by the constant force energy storage compensator is: ; In the formula, To compensate for the displacement; The coefficient of linear expansion of precast concrete; This refers to the total longitudinal length of the precast concrete segmental beam. To lock in the ambient temperature for the system; For extreme low temperature prediction; This represents the shrinkage deformation during the curing period.
[0034] It should be noted that, During the on-site construction phase, temperature sensors placed on the surface of precast concrete segmental beams collect thermodynamic temperature values in real time. The data provided by the meteorological department shows the historical lowest temperature in the construction sea area for the current month. To monitor the extreme values of shrinkage and creep of precast concrete segmental beams of the same batch during the component curing period at the precast beam yard using a dial gauge.
[0035] In an optional embodiment, when applying tension to the threaded steel bars, the threaded steel bars on the top and bottom slabs of the precast concrete segmental beam are simultaneously and symmetrically tensioned. For the threaded steel bars on the top slab of the precast concrete segmental beam, symmetrical tensioning is performed in the order of first the middle and then the two sides. It can be understood that, during use, the above design effectively avoids eccentric stress and uneven stress at the joint surface, ensures uniform pressure curing of the epoxy resin adhesive, and improves the assembly accuracy and structural integrity of the concrete segmental beam.
[0036] S5: During the curing cycle of the epoxy resin adhesive, when the precast concrete segment beam shrinks and deforms, causing the threaded steel bars to show a tendency to relax, the constant force energy storage compensator in the state of compression energy storage automatically releases the rebound displacement to compensate for the amount of prestressed tendon retraction caused by the shrinkage of the precast concrete segment beam, so that the actual compressive stress on the joint surface is not lower than the minimum allowable compressive stress of the joint. S6: After the longitudinal prestressed steel strands in the body are tensioned and the entire bridge system is converted, loosen the locking nut and remove the constant force energy storage compensator, threaded steel bars and steel toothed sill in sequence.
[0037] In an optional embodiment, the threaded reinforcing bars must be removed after four precast concrete segment beams have been prestressed longitudinally; the threaded reinforcing bars at the precast concrete segment beams in the side spans and the last three cantilevered precast concrete segment beams in the middle span must be removed after the tensioning of the closure bundles. It is understood that, during use, this removal sequence ensures that the threaded reinforcing bars are removed after the longitudinal prestressing system has been fully established, avoiding sudden stress changes at the joint surfaces of the precast concrete segment beams; furthermore, the threaded reinforcing bars in the closure zones of the side spans and middle span are removed after the tensioning of the closure bundles, ensuring a smooth transition of the structural system and effectively maintaining the stress continuity and overall safety of the epoxy resin adhesive joints.
[0038] In an optional embodiment, after dismantling, one of the bolt holes reserved on the bottom plate of each precast concrete segment beam for installing the steel toothed sill is retained as a ventilation hole; the remaining bolt holes reserved for the steel toothed sill installation are sealed with grout. It is understood that, during use, the above design ensures air circulation within the box girder, prevents moisture accumulation and structural corrosion, and ensures the sealing and waterproofing of unused ducts, thus balancing the durability of the precast concrete segment beam with the controllability of the internal environment.
[0039] Other technical features are the same as in Embodiment 1 and can achieve the same technical effects, so they will not be described in detail here.
[0040] Example 3 This invention also provides a computer-readable storage medium storing a computer program that is executed by a processor to implement the various steps in the holding method described above. For details, please refer to the implementation methods provided for the various steps described above, which will not be repeated here.
[0041] It should be understood that although the steps in the flowcharts of the accompanying figures are shown sequentially as indicated by the arrows, these steps are not necessarily executed in the order indicated by the arrows. Unless explicitly stated herein, there is no strict order restriction on the execution of these steps, and they can be executed in other orders. Moreover, at least some steps in the flowcharts of the accompanying figures may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily completed at the same time, but can be executed at different times, and their execution order is not necessarily sequential, but can be performed alternately or in turn with other steps or at least some of the sub-steps or stages of other steps.
[0042] It should be noted that if the embodiments of the present invention involve directional indicators (such as up, down, left, right, front, back, etc.), the directional indicators are only used to explain the relative positional relationship and movement of the components in a certain specific posture (as shown in the figure). If the specific posture changes, the directional indicators will also change accordingly.
[0043] Furthermore, if the embodiments of this invention involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. If the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.
[0044] In this invention, the terms "comprising," "including," or any other variations thereof are intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitation, an element defined by the phrase "comprising..." does not exclude the presence of additional identical elements in the process, method, article, or apparatus that includes said element.
[0045] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit it; those skilled in the art will readily understand that the above descriptions are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A method for temporary prestress maintenance of a precast concrete segmental beam in a marine environment, characterized in that, Includes the following steps: S1: Before assembling the precast concrete segmental beam, the upper limit of the equivalent stiffness of the constant force energy storage compensator is obtained based on the meteorological data of the construction sea area and the relevant data of the precast concrete segmental beam. S2: Anchor steel toothed brackets on the bottom and top plates of each adjacent precast concrete segment beam, and each steel toothed bracket has multiple reserved holes pre-drilled; apply epoxy resin adhesive to the matching surface of the precast concrete segment beam, and pass the threaded steel bars through the corresponding reserved holes of the adjacent steel toothed brackets. S3: At the tensioning end of the threaded steel bar, a constant force energy storage compensator that meets the upper limit of the equivalent stiffness is inserted into the threaded steel bar, so that the constant force energy storage compensator is clamped between the bearing surface of the steel toothed sill and the locking nut. S4: Use a jack to apply tension to the threaded steel bar to the corresponding tonnage, so that the compressive stress on the joint surface reaches the initial target compressive stress of the joint. At the same time, the constant force energy storage compensator is compressed to the designed energy storage stroke. After that, tighten the lock nut to lock it and remove the jack. S5: During the curing cycle of the epoxy resin adhesive, when the precast concrete segment beam shrinks and deforms, causing the threaded steel bars to show a tendency to relax, the constant force energy storage compensator in the state of compression energy storage automatically releases the rebound displacement to fill the shrinkage gap of the precast concrete segment beam, so that the actual compressive stress on the joint surface is not lower than the minimum allowable compressive stress of the joint. S6: After the longitudinal prestressed steel strands in the body are tensioned and the entire bridge system is converted, loosen the locking nut and remove the constant force energy storage compensator, threaded steel bars and steel toothed sill in sequence.
2. The holding method according to claim 1, characterized by, In step S1, the calculation method for the upper limit of the total equivalent stiffness of the joint surface is as follows: ; wherein is the upper limit of the total equivalent stiffness of the joint surface; is the joint cross-sectional area; is the initial target compressive stress of the joint; is the minimum allowable compressive stress of the joint; is the linear expansion coefficient of the precast concrete; is the longitudinal equivalent length between the anchoring points of the adjacent two precast concrete segmental beams; is the extreme theoretical temperature difference; is the extreme short-term shrinkage and creep of the adjacent two precast concrete segmental beams within the curing period.
3. The holding method according to claim 1, characterized by, In step S3, the constant force energy storage compensators of the top and bottom slabs of the precast concrete segment beams arranged on the same joint surface have the following coordination relationship: ; ; In the formula, is the equivalent stiffness of the constant force and energy storage compensator on the top plate side of the precast concrete segmental beam; is the equivalent stiffness of the constant force and energy storage compensator on the bottom plate side of the precast concrete segmental beam; is the vertical temperature gradient correction coefficient; is the neutral axis height distribution coefficient; is the upper limit value of the total equivalent stiffness of the joint surface; is the cross-sectional area of the top plate of the precast concrete segmental beam; is the cross-sectional area of the bottom plate of the precast concrete segmental beam; is the total cross-sectional area of the web of the precast concrete segmental beam; is the joint cross-sectional area of the precast concrete segmental beam.
4. The holding method according to claim 1, characterized in that, In step S4, the minimum compensation displacement required by the constant force energy storage compensator is: ; In the formula, To compensate for the displacement; The coefficient of linear expansion of precast concrete; This refers to the total longitudinal length of the precast concrete segmental beam. To lock in the ambient temperature for the system; For extreme low temperature prediction; This represents the shrinkage deformation during the curing period.
5. The holding method according to claim 1, characterized in that, In step S4, when applying tension to the threaded steel bars, the threaded steel bars on the top and bottom slabs of the precast concrete segmental beam are simultaneously and symmetrically tensioned. For the threaded steel bars on the top slab of the precast concrete segmental beam, symmetrical tensioning is performed in the order of first the middle and then the two sides.
6. The holding method according to claim 1, characterized in that, In step S6, after the demolition is completed, one pre-reserved hole in the bottom plate is reserved for each precast concrete segment beam as a ventilation hole, and the remaining holes are sealed tightly by grouting.
7. A temporary prestress retention system for precast concrete segmental beams in a marine environment, employing the retention method as described in any one of claims 1-6, and used for each precast concrete segmental beam connected to each other, wherein the joint surfaces between each precast concrete segmental beam are coated with epoxy resin adhesive, characterized in that, include: Steel toothed retainer, threaded steel bar, constant force energy storage compensator and lock nut; Several of the steel toothed brackets are respectively fixed to the top and bottom plates of each precast concrete segment beam; the steel toothed brackets are provided with multiple reserved holes; The same steel toothed sill serves as a common anchorage node between adjacent precast concrete segmental beams. Multiple independent threaded steel bars pass through multiple reserved holes of the steel toothed sill along the longitudinal direction of the bridge and extend to the corresponding steel toothed sill of the adjacent precast concrete segmental beams, forming a relay-type anchorage between adjacent precast concrete segmental beams. The constant force energy storage compensator is sleeved on the outer wall of the tensioning end of the threaded steel bar; The locking nut is screwed onto the end of the threaded steel bar; The constant force energy storage compensator is located between the bearing surface of the steel toothed sill and the locking nut, and the equivalent stiffness of the constant force energy storage compensator is not greater than the preset upper limit of the equivalent stiffness. It is used to maintain the compressive stress on the joint surface by utilizing the mechanical energy storage and pressure release characteristics when the precast concrete segmental beam undergoes volume deformation.
8. The holding system according to claim 7, characterized in that, The specific arrangement of the steel toothed sills is based on the structural type of the precast concrete segmental beam. Specifically: when a steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; three steel toothed sills are arranged on the top plate of the precast concrete segmental beam, one of which is located in the middle of the top plate, and the other two are symmetrically arranged on both sides of the middle steel toothed sill about its longitudinal axis; when no steering block is arranged on the precast concrete segmental beam, two steel toothed sills are symmetrically arranged on the bottom plate of the precast concrete segmental beam about its longitudinal axis; and four steel toothed sills are symmetrically arranged on the top plate of the precast concrete segmental beam about its longitudinal axis.
9. The holding system according to claim 7, characterized in that, The diameter of each threaded steel bar arranged on the top slab of each precast concrete segment beam is 25-30mm, and the tension control force is 260-400kN. The diameter of each threaded steel bar arranged on the bottom slab is 30-35mm, and the tension control force is 400-600kN.