An adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove joint and its construction process

By introducing support components and sealing components into the flue system, combined with phase change ceramicized silicone rubber, the sealing failure problem caused by thermal expansion and contraction and load in traditional flue systems is solved. This achieves flexible crack resistance, odor prevention, and rigid fire protection in case of disasters, thereby improving the service life and waterproof performance of buildings.

CN123109362APending Publication Date: 2026-11-17NANNING ZHONGHAI HONGYANG REAL ESTATE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611374880.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-07
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional flue systems are prone to sealing failure due to factors such as thermal expansion and contraction, wind load, and foundation settlement. Furthermore, they have high requirements for the construction environment and are difficult to adapt to manufacturing errors and installation deviations, which affects the building's functionality and durability.

Method used

The system employs an adaptive flexible temperature-resistant sealing flue system with a non-unloading tongue-and-groove joint. By setting a support component between the bottom of the flue and the bottom of the concrete curb of the floor slab, combined with the sealing components and the temperature-resistant main body, a flexible isolation and labyrinth flow-blocking path are formed. The system utilizes phase-change ceramicized silicone rubber to form a rigid temperature-resistant layer at high temperatures, and combines it with a waterproof additional layer to solve the leakage problem.

Benefits of technology

It achieves flexible crack resistance and vibration isolation under normal conditions, preventing air leakage and odor transfer, and transforms into rigid fireproof and temperature-resistant properties during disasters, thereby improving the structural life and waterproof reliability of the flue system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123109362A_ABST
    Figure CN123109362A_ABST
Patent Text Reader

Abstract

This invention discloses an adaptive flexible temperature-resistant sealing flue system and construction process based on a non-unloading tongue-and-groove joint, comprising: a floor slab component, including a floor slab body, a bottom concrete curb integrally formed with the floor slab body, and a top floor slab tongue-and-groove joint; a flue, the bottom end of which is supported by the bottom concrete curb, and the top end of which passes through the top floor slab tongue-and-groove joint; a support component, which is disposed between the bottom end of the flue and the bottom concrete curb; the support component and the sealing component form a flexible isolation at the bottom and top of the flue, respectively, to cut off the rigid force transmission path between the flue and the floor slab component, and the bottom concrete curb provides vertical support for the flue; effectively cutting off the rigid force transmission path between the flue and the floor slab, avoiding local stress concentration and fatigue cracks caused by rigid collision.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue and groove joint, and more particularly to an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue and groove joint and its construction process. Background Technology

[0002] In modern building engineering, the flue system serves as a crucial channel for smoke and gas exhaust, and its sealing performance directly impacts the building's safety and service life. Currently, flues in residential and public buildings are mostly installed using prefabricated components assembled on-site. The treatment of joints between components becomes a critical aspect in ensuring the overall airtightness and structural stability of the system. Traditional construction techniques commonly employ polymer mortar for rigid sealing of flue interfaces, relying on the mortar's adhesive strength to achieve a sealed connection. However, with the increasing complexity of building service environments, this rigid connection method has gradually revealed significant technical shortcomings.

[0003] When a building experiences significant thermal expansion and contraction due to seasonal changes or diurnal temperature variations, the difference in linear expansion coefficients of different materials can cause uncoordinated deformation and displacement at the flue interface. Simultaneously, the periodic swaying of high-rise buildings under wind loads and the long-term micro-slippage caused by uneven foundation settlement can subject the originally rigid polymer mortar sealing layer to repeated tensile, compressive, and shear forces. Because polymer mortar lacks sufficient elastic deformation capacity, these external loads cannot be released through the material's flexible buffering mechanism; instead, they are directly transformed into localized stress concentrations at the interface. Over time, microcracks first appear in the stress concentration area, gradually expanding into penetrating cracks with load cycles, ultimately leading to flue seal failure, resulting in air leakage, odor transfer, and even structural damage, severely impacting the building's functionality and durability.

[0004] In addition, traditional mortar sealing technology has high requirements for the construction environment, long wet operation and maintenance cycle, and is difficult to adapt to irregular gaps caused by manufacturing errors or installation deviations in flue components, which further aggravates the uneven stress phenomenon on rigid contact surfaces. Summary of the Invention

[0005] This invention overcomes the shortcomings of the prior art and provides an adaptive flexible temperature-resistant sealing flue system and construction process based on unloading tongue and groove joints.

[0006] To achieve the above objectives, the technical solution adopted by this invention is: an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue-and-groove joint, comprising:

[0007] Floor slab components include the floor slab body, the bottom concrete curb integrally formed with the floor slab body, and the top floor slab tongue and groove joint.

[0008] The flue is supported at the bottom by a concrete curb and at the top by a tongue and groove joint in the top floor slab.

[0009] Support components, which are installed between the bottom end of the flue and the bottom concrete curb; and

[0010] A sealing component is installed in the annular gap formed between the outer wall of the flue and the tongue and groove joint of the top floor slab.

[0011] The sealing assembly includes a flow-blocking sealing part and a temperature-blocking body. The flow-blocking sealing part is used to form a non-straight labyrinth flow-blocking path in the annular gap. The temperature-blocking body is configured to maintain elastic deformation capability under normal temperature use and to form a rigid temperature-blocking sealing layer by ceramicization under high temperature.

[0012] The support and sealing components form flexible barriers at the bottom and top of the flue to cut off the rigid force transmission path between the flue and the floor slab components, and the bottom concrete curb provides vertical support for the flue.

[0013] In a preferred embodiment of the present invention, a bottom concrete curb is provided around the flue opening, and the outer periphery of the bottom concrete curb is adapted to the bottom inner cavity of the flue to position and vertically support the flue; the top floor slab tongue and groove is provided around the top periphery of the flue and together with the outer wall of the flue, defines an annular gap for accommodating the sealing component.

[0014] In a preferred embodiment of the present invention, the support is an L-shaped weather-resistant rubber shock-absorbing pad, which includes a horizontal pressure-bearing part and a vertical isolation part. The horizontal pressure-bearing part is sandwiched between the bottom end face of the flue and the support surface of the bottom concrete curb, and the vertical isolation part is disposed between the bottom side wall of the flue and the lateral positioning surface of the bottom concrete curb.

[0015] In a preferred embodiment of the present invention, the sealing component is a prefabricated annular seal, the flow-blocking sealing part is integrally formed with the temperature-blocking body, and the prefabricated annular seal is filled in the annular gap under radial pressure.

[0016] In a preferred embodiment of the present invention, the flow-blocking sealing part includes multiple flexible baffles spaced apart along the axial direction of the flue. The free ends of the multiple flexible baffles are inclined in the opposite direction to the flue gas escape direction, and after the sealing assembly is pressed into the annular gap, they are elastically fitted to the outer wall of the flue or the inner wall of the tongue and groove of the top floor slab to form a multi-stage throttling and pressure-reducing labyrinth flow-blocking cavity.

[0017] In a preferred embodiment of the present invention, the outer peripheral wall of the sealing component is provided with a self-locking texture, which includes at least one of circumferential ribs, reverse teeth, corrugations, or roughened textures. The self-locking texture is used to form a locking fit with the inner wall of the tongue and groove of the top floor slab after the sealing component is pressed into the annular gap.

[0018] In a preferred embodiment of the present invention, the temperature-resistant body is made of phase change ceramicized silicone rubber, which contains a silicone rubber matrix, low melting point glass powder and ceramic-forming additives, so that the temperature-resistant body undergoes micro-expansion in volume at high temperature and sinters to form an inorganic ceramic shell.

[0019] In a preferred embodiment of the present invention, the invention further includes a root waterproofing node, which includes an arc corner set at the junction of the bottom concrete curb and the flue, and a waterproofing additional layer covering the arc corner, wherein the radius of the arc corner is not less than 50mm.

[0020] A construction process for an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue-and-groove joint includes the following steps:

[0021] S1. During the main structure construction phase, the flue positioning mold and the floor slab reinforcement are positioned and fixed simultaneously, and when pouring the floor slab concrete, the floor slab body, the bottom concrete curb and the top floor slab tongue and groove are cast in one go.

[0022] S2. Lay the support component at the support position of the bottom concrete curb, so that the support component is located between the bottom end of the flue to be installed and the bottom concrete curb.

[0023] S3. Hoist the flue to the bottom concrete curb and make the top of the flue pass through the tongue and groove of the top floor slab to form an annular gap between the outer wall of the flue and the tongue and groove of the top floor slab.

[0024] S4. The prefabricated sealing component is fitted onto the outer periphery of the flue and pressed into the annular gap along the axial direction of the flue, so that the sealing component forms an elastic compression seal and a labyrinth flow obstruction path within the annular gap.

[0025] S5. Construct a rounded corner at the junction of the bottom concrete curb and the flue, and lay an additional waterproof layer at the rounded corner.

[0026] In a preferred embodiment of the present invention, in S4, when the sealing component is pressed in, the multiple flexible baffles of the sealing component form a reverse flow deflection fit along the flue gas escape direction, and the self-locking texture on the outer peripheral wall of the sealing component forms a backstop and limiting fit with the inner wall of the tongue and groove of the top floor slab; in S5, the radius of the arc corner is constructed to be not less than 50mm.

[0027] This invention addresses the shortcomings of the prior art and has the following beneficial effects:

[0028] (1) This invention provides an adaptive flexible temperature-resistant sealing flue system and construction process based on unloading tongue and groove. By setting a support between the bottom end of the flue and the bottom end of the concrete curb of the floor slab, the rigid force interface between the flue and the floor slab is changed. When the main body of the building expands and contracts due to temperature difference or vibrates due to wind load and uneven settlement, the support generates elastic deformation through radial compression or shear, which effectively cuts off the rigid force transmission path between the flue and the floor slab, avoiding local stress concentration and fatigue cracks caused by rigid collision. Compared with the traditional method of sealing with polymer mortar, this solution achieves flexible crack resistance and vibration isolation of the structural nodes in daily working conditions while satisfying reliable vertical support, thus extending the structural life of the flue system.

[0029] (2) This invention provides an adaptive flexible temperature-resistant sealing flue system and construction process based on unloading tongue and groove joint. By setting a sealing component including a flow-blocking sealing part and a temperature-resistant main body, and utilizing the structural constraint of the tongue and groove joint of the top floor slab, when the flue is in daily use, the sealing component uses a flexible tongue to form a multi-level labyrinth flow-blocking path. Through throttling, pressure reduction and direction change, the escape velocity of the oil fume gas is effectively reduced, and the flue gas is condensed in the labyrinth cavity to form an oil film to assist sealing. This not only improves the air tightness, but also avoids the failure mode of traditional mortar causing through cracks under long-term vibration, which leads to air leakage and odor leakage. It achieves long-term sealing stability under normal building service environment.

[0030] (3) This invention provides an adaptive flexible temperature-resistant sealing flue system and construction process based on unloading tongue and groove joint. The temperature-resistant body is made of phase change ceramicized silicone rubber, which is configured to undergo micro-expansion in volume and sinter to form an inorganic ceramic shell under fire or abnormal high temperature conditions. Under the structural constraint of the tongue and groove joint of the top floor slab, the expansion pressure is converted into a tight squeezing force on the outer wall of the flue and the inner wall of the tongue and groove joint, so that the sealing component is quickly converted into a rigid fire-resistant barrier structure. This temperature response mechanism completely blocks the path of high temperature flue gas and flames spreading along the floor slab joint, overcomes the contradiction that traditional flexible rubber materials are easy to soften and fail at high temperatures and inorganic mortar is easy to crack under daily vibration, and realizes the adaptive conversion and synergistic protection of daily flexible sealing and rigid fire protection during disasters.

[0031] (4) This invention provides an adaptive flexible temperature-resistant sealing flue system and construction process based on unloading tongue and groove joint. By setting a rounded corner at the root of the flue and laying a waterproof additional layer, and cooperating with the bottom concrete inverted wall and the floor slab body formed in one go, the construction gaps that may be generated by traditional secondary formwork are eliminated. The rounded corner provides a smooth corner base for the waterproof additional layer, effectively eliminating stress concentration at right angles. When the flue undergoes a small displacement, it can prevent the waterproof layer from becoming hollow, torn or punctured. A multi-level anti-seepage system composed of rigid structural inverted wall, flexible vibration isolation support and waterproof additional layer is constructed, which effectively solves the long-term leakage problem at the root of the flue in the water-contaminated area of ​​the building and significantly improves the overall waterproof reliability of the project. Attached Figure Description

[0032] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0033] Figure 1 This is a schematic cross-sectional view of an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue and groove joint, according to a preferred embodiment of the present invention.

[0034] Figure 2 This is a schematic diagram of the cooperation structure between the bottom concrete curb, the flue, and the support component in a preferred embodiment of the present invention.

[0035] Figure 3 This is a schematic diagram of the mating structure of the top floor slab tongue and groove, sealing components and outer wall of the flue in a preferred embodiment of the present invention;

[0036] Figure 4 This is a schematic cross-sectional view of the sealing assembly according to a preferred embodiment of the present invention;

[0037] Figure 5 This is a schematic diagram of the sealing assembly of a preferred embodiment of the present invention after high-temperature ceramization;

[0038] Figure 6 This is a schematic diagram of the construction process of an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue and groove joint, according to a preferred embodiment of the present invention.

[0039] In the diagram: 1. Floor slab component; 11. Floor slab body; 12. Bottom concrete curb; 121. Supporting surface; 122. Lateral positioning surface; 13. Top floor slab tongue and groove; 131. Tongue and groove inner wall; 14. Flue opening; 2. Flue; 21. Flue outer wall; 22. Flue bottom end face; 23. Flue top; 24. Flue inner cavity; 3. Supporting component; 31. Horizontal bearing part; 32. Vertical isolation part; 33. Transition rounded corner; 4. Sealing components; 41. Temperature-resistant body; 42. Flow-blocking seal; 421. Flexible tongue; 422. Tongue root; 423. Tongue free end; 43. Labyrinth flow-blocking cavity; 44. Self-locking texture; 441. Circumferential rib; 442. Reverse teeth; 443. Corrugated section; 45. Installation guide surface; 46. Segmented joint; 5. Annular gap; 6. Root waterproof node; 61. Rounded corner; 62. Waterproof additional layer; 7. Flue positioning mold. Detailed Implementation

[0040] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0041] Many specific details are set forth in the following description in order to provide a full understanding of the invention. However, the invention may also be practiced in other ways different from those described herein. Therefore, the scope of protection of the invention is not limited to the specific embodiments disclosed below.

[0042] In the description of this application, it should be understood that the terms center, longitudinal, transverse, up, down, front, back, left, right, vertical, horizontal, top, bottom, inner, and outer, indicating orientation or positional relationships, are based on the orientation or positional relationships shown in the accompanying drawings and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as limiting the scope of protection of this application. Furthermore, the terms first, second, etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Therefore, features defined with first, second, etc., may explicitly or implicitly include one or more of that feature. In the description of this invention, unless otherwise stated, multiple means two or more.

[0043] In the description of this application, it should be noted that, unless otherwise explicitly specified and limited, the terms installation, connection, and linking should be interpreted broadly. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to mechanical connections or electrical connections; they can refer to direct connections or indirect connections through an intermediate medium; and they can refer to the internal communication between two components. Those skilled in the art will understand the specific meaning of the above terms in this application based on the specific circumstances.

[0044] This invention provides an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue and groove joint, which includes: a floor slab component, the floor slab component including a floor slab body, a bottom concrete curb integrally formed with the floor slab body, and a top floor slab tongue and groove joint;

[0045] The flue is supported at the bottom by a concrete curb and at the top by a tongue and groove joint in the top floor slab.

[0046] Support component, which is installed between the bottom end of the flue and the bottom concrete curb;

[0047] And a sealing component, which is installed in the annular gap formed between the outer wall of the flue and the tongue and groove of the top floor slab;

[0048] The sealing assembly includes a flow-blocking seal and a temperature-blocking body. The flow-blocking seal is used to form a non-straight-through labyrinth flow-blocking path within the annular gap. The temperature-blocking body is configured to maintain elastic deformation capability under normal temperature use and to form a rigid temperature-blocking sealing layer by ceramicization under high temperature conditions. The support and sealing assembly form flexible isolation at the bottom and top of the flue, respectively, to cut off the rigid force transmission path between the flue and the floor slab components, and the bottom concrete curb provides vertical support for the flue.

[0049] Therefore, this invention couples vertical rigid support, bottom flexible vibration isolation, top labyrinth flow obstruction, and high-temperature ceramicized thermal insulation on a structural platform consisting of a single-cast concrete bottom curb and a tongue-and-groove joint in the top floor slab. It does not simply replace traditional mortar sealing with flexible sealing materials, nor does it rely solely on the concrete curb for flue support. By having the bottom concrete curb bear the vertical load of the flue, the flue can achieve stable support without additional steel reinforcement unloading components. The support component transforms the hard contact between the bottom of the flue and the concrete curb into a compressible and repositionable flexible contact. The sealing component at the tongue-and-groove joint in the top floor slab transforms the annular gap that could have formed a straight air leakage channel into a tortuous labyrinth flow obstruction path. The thermal insulation body makes the same sealing component a flexible crack-resistant component at normal temperature and a rigid fire-resistant barrier component under fire or abnormal high temperature conditions. Thus, this invention achieves flexible crack resistance, odor prevention, and vibration absorption in normal conditions, and rigid fire resistance, thermal insulation, and sealing in disaster conditions.

[0050] Furthermore, this invention repurposes the structural value of traditional cast-in-place reinforced concrete curbs and tongue-and-groove joints. Traditional cast-in-place reinforced concrete curbs are mainly used for waterproofing and support, while the top tongue-and-groove joint is mainly used for positioning and sealing. However, when the sealing material is still polymer mortar or other rigid or semi-rigid materials, floor slab deformation, flue thermal expansion and contraction, and building micro-vibrations will still concentrate on the joint, leading to fatigue cracks. In this invention, the bottom concrete curb no longer makes direct hard contact with the flue, but forms a mechanical buffer layer through the support component; the top floor slab tongue-and-groove joint is no longer a regular groove for mortar filling, but serves as a radial limiting cavity, a compression reaction surface, and a rigid constraint surface after high-temperature ceramicization of the sealing component. In other words, this invention transforms the cast-in-place concrete structure from a simple support and sealing platform into a flexible sealing component with synergistic functions of pressure bearing, positioning, limiting, and temperature resistance.

[0051] Example 1:

[0052] like Figures 1 to 4 As shown, this embodiment provides a basic non-unloading tongue-and-groove flexible sealing flue system, which is mainly used for the layered installation nodes of vertical flues in buildings such as residences, hotels, apartments, hospitals, and school dormitories. The flue system includes a floor slab component 1, a flue 2, a support component 3, and a sealing component 4. The floor slab component 1 serves as the structural foundation of the entire flue system, and includes a floor slab body 11, a bottom concrete curb 12, and a top floor slab tongue-and-groove joint 13. The bottom concrete curb 12 and the top floor slab tongue-and-groove joint 13 are cast in place with the floor slab body 11 during the main structure construction stage, thereby avoiding the formation of construction joints by secondary formwork, secondary pouring, or secondary chiseling in the later stage.

[0053] In this embodiment, a flue opening 14 is reserved on the floor slab body 11. The flue opening 14 is used for the vertical passage of the flue 2. The bottom concrete curb 12 is set around the flue opening 14 and protrudes upward from the upper surface of the floor slab body 11. The planar outline of the bottom concrete curb 12 can be rectangular, square, rounded rectangle or other annular outline that matches the shape of the inner cavity of the flue 2. When the flue 2 is a common rectangular thin-walled flue, the bottom concrete curb 12 is preferably a rectangular annular curb, whose outer circumference is slightly smaller than the bottom inner cavity size of the flue 2, so that the bottom concrete curb 12 can enter the bottom inner side of the flue 2 or form a nested positioning relationship with the bottom inner edge of the flue 2. This size relationship does not require the bottom concrete curb 12 to be completely tight-fitting with the flue 2, but allows there to be an installation space between them to accommodate the support 3.

[0054] Specifically, the bottom concrete curb 12 includes a support surface 121 on its upper part and a lateral positioning surface 122 on its outer or inner periphery. The support surface 121 is used to bear the vertical load transmitted from the flue 2, and the lateral positioning surface 122 is used to limit the horizontal displacement of the flue 2. In this embodiment, the support surface 121 can be a plane, or it can be provided with a shallow groove or roughened interface to facilitate the laying of the support component 3. The lateral positioning surface 122 can be a vertical surface or a slightly inclined guide surface so that the flue 2 can be naturally guided under the action of gravity when it is hoisted and placed. Through the above structure, the bottom concrete curb 12 provides both vertical support and participates in the horizontal positioning of the flue 2.

[0055] The top floor slab tongue and groove 13 is provided around the flue opening 14 and is formed at the upper or lower edge of the flue 2 where it passes through the floor slab. In this embodiment, the top floor slab tongue and groove 13 can be an annular step, an annular groove, or a tongue and groove structure with a stepped surface formed inward or downward around the periphery of the floor slab opening. An annular gap 5 is formed between the inner wall 131 of the top floor slab tongue and groove 13 and the outer wall 21 of the flue. This annular gap 5 is not a simple gap waiting to be filled with mortar in the traditional sense, but a functional cavity for accommodating the sealing component 4. Since the top floor slab tongue and groove 13 and the floor slab body 11 are cast in place at one time, its inner wall and stepped surface can provide a stable radial reaction force for the sealing component 4, so that the sealing component maintains a reliable elastic compression state after being pressed in.

[0056] The flue 2 can be a precast cement fiber flue, calcium silicate board flue, magnesium oxide board flue, composite inorganic board flue, or other finished thin-walled pipes for building smoke and exhaust. The flue 2 includes an outer wall 21, a bottom end face 22, a top end 23, and an inner cavity 24. When the flue 2 is installed, its bottom end face 22 is supported above the bottom concrete curb 12 and is separated from the bottom concrete curb 12 by the support 3. Its top end 23 passes through the tongue and groove 13 of the top floor slab, and an annular gap 5 is formed between the outer wall 21 and the inner wall 131 of the tongue and groove.

[0057] The support 3 is disposed between the bottom end of the flue 2 and the bottom concrete curb 12. Its function is not just to act as a leveling pad, but to transform the rigid stress interface between the flue 2 and the bottom concrete curb 12 into a flexible stress interface with elastic deformation capability. In this embodiment, the support 3 is preferably an L-shaped weather-resistant rubber damping pad. The L-shaped weather-resistant rubber damping pad includes a horizontal pressure-bearing part 31 and a vertical isolation part 32. The horizontal pressure-bearing part 31 is laid on the support surface 121 and sandwiched between the bottom end face 22 of the flue and the bottom concrete curb 12. The vertical isolation part 32 is disposed along the lateral positioning surface 122 of the bottom concrete curb 12 and is located between the bottom side wall of the flue 2 and the bottom concrete curb 12.

[0058] The horizontal pressure-bearing part 31 mainly undertakes the function of vertical load buffering. After the flue 2 is hoisted and placed, the self-weight of the flue 2 acts on the horizontal pressure-bearing part 31 through the bottom end face 22 of the flue. The horizontal pressure-bearing part 31 undergoes a certain elastic deformation under pressure, and disperses the concentrated hard contact force into surface contact force. Thus, even if there are local unevenness, rough edges or construction errors on the bottom end face 22 of the flue, it will not directly crush the edge of the anti-sill or the thin wall at the bottom of the flue. The vertical isolation part 32 mainly undertakes the functions of lateral isolation and vibration absorption. When the main body of the building experiences micro-vibration, thermal expansion and contraction or slight uneven settlement, the flue 2 may have a slight lateral displacement tendency relative to the bottom concrete anti-sill 12. At this time, the vertical isolation part 32 undergoes elastic deformation under radial compression or shear, avoiding direct collision between the thin wall of the flue 2 and the concrete anti-sill 12.

[0059] In a preferred embodiment, a transition rounded corner 33 is provided between the horizontal pressure-bearing part 31 and the vertical isolation part 32. The transition rounded corner 33 can avoid stress concentration at the inner corner of the L-shaped structure and make it easier to fit the corner area of ​​the bottom concrete curb 12 during construction and laying. The material of the support 3 can be weather-resistant rubber, EPDM rubber, silicone rubber, fluorosilicone rubber or other materials with aging resistance, temperature resistance and elastic recovery ability. The support 3 can be a continuous ring or it can be formed by splicing multiple strip gaskets end to end. When a multi-segment splicing structure is used, the joints between adjacent gaskets are preferably arranged by oblique joint, overlap or staggered joint to avoid forming a through air leakage seam.

[0060] The sealing component 4 is disposed in the annular gap 5 between the outer wall 21 of the flue and the tongue and groove joint 13 of the top floor slab. In this embodiment, the sealing component 4 is a prefabricated annular seal, which includes a heat-insulating body 41 and a flow-blocking sealing part 42. The heat-insulating body 41 constitutes the main skeleton of the sealing component 4. It is elastic and compressible at room temperature and can be ceramicized at high temperature to form a rigid heat-insulating sealing layer. The flow-blocking sealing part 42 is disposed on the side of the heat-insulating body 41 near the outer wall 21 of the flue, preferably integrally formed with the heat-insulating body 41. The flow-blocking sealing part 42 is used to form a non-straight labyrinth flow-blocking path in the annular gap 5, so that the airflow attempting to escape from the flue joint cannot pass in a straight line, but must go through multiple detours, expansions and throttling.

[0061] Specifically, the flow-blocking sealing part 42 includes multiple flexible baffles 421 spaced apart along the axial direction of the flue 2. Each flexible baffle 421 includes a baffle root 422 connected to the heat-insulating body 41 and a baffle free end 423 away from the baffle root 422. The baffle free end 423 is inclined in the opposite direction of the flue gas escape direction. In the common installation state, if the oil fumes or odorous gases in the flue tend to enter the annular gap 5 from bottom to top or from inside to outside, the free end of the flexible baffle 421 is preferably inclined downward or towards the airflow. When the airflow impacts the flexible baffle 421, it will cause the flexible baffle 421 to further adhere to the outer wall 21 of the flue or the inner wall 131 of the tongue and groove, rather than being lifted by the airflow. Thus, the flexible baffle 421 is not only a passive sealing lip, but also a dynamic sealing component that uses airflow pressure to achieve self-reinforcing sealing.

[0062] After multiple flexible baffles 421 are arranged at intervals along the axial direction, a labyrinthine flow-blocking cavity 43 is formed between adjacent flexible baffles 421. The labyrinthine flow-blocking cavity 43 can be manifested as multiple annular small cavities, zigzag channels, or bends. When a trace amount of gas enters the annular gap 5, it needs to pass through multiple flexible baffles 421 and multiple labyrinthine flow-blocking cavities 43 in sequence. Each time the gas passes through a flexible baffle 421, it will experience throttling, pressure reduction, and change of direction. Each time it enters a labyrinthine flow-blocking cavity 43, it will form a local vortex and a decrease in flow velocity. In this way, the oil fume gas that may have rushed up rapidly along the annular gap 5 is decomposed into multiple levels of low-speed turbulent airflow, and its ability to continue to escape is significantly reduced.

[0063] The outer peripheral wall of the sealing component 4 is provided with a self-locking texture 44. The self-locking texture 44 may include at least one of circumferential ribs 441, reverse teeth 442, corrugated segments 443 or roughened texture. In this embodiment, the self-locking texture 44 is preferably a plurality of circumferential ribs 441 arranged at intervals along the axial direction. The outer diameter of the circumferential ribs 441 is slightly larger than the radial width of the annular gap 5, so that when the sealing component 4 is pressed into the annular gap 5, the circumferential ribs 441 are squeezed by the tongue and groove inner wall 131 and generate elastic deformation.

[0064] After installation, the circumferential rib 441 presses against the inner wall 131 of the tongue and groove with the elastic restoring force of the temperature-resistant body 41, thereby providing anti-retraction friction force and radial sealing pressure. Furthermore, the circumferential rib 441 can be configured as a toothed structure with an inclined guide surface on the outside and an anti-retraction surface on the inside, so that it has less resistance when pressed downward, but greater resistance when it is pushed upward under the impact of airflow or thermal expansion and contraction.

[0065] During construction and use, in the main structure construction stage, the floor slab body 11, the bottom concrete curb 12, and the top floor slab tongue and groove 13 are cast in place at one time, forming a stable concrete support platform and sealing installation platform around the flue opening 14; before the flue 2 is hoisted, the support component 3 is laid on the bottom concrete curb 12; after the flue 2 is hoisted and positioned, its own weight is transferred to the bottom concrete curb 12 through the support component 3, the bottom concrete curb 12 bears the vertical load, and the support component 3 absorbs local unevenness and micro-displacement; subsequently, the sealing component 4 is pressed into the annular gap 5, the flow-blocking sealing part 42 adheres to the outer wall 21 of the flue under radial compression, and the self-locking texture 44 adheres to the inner wall 131 of the tongue and groove under radial compression, thereby forming a multi-level elastic seal at the top.

[0066] When the building is in daily use, hot flue gas and oily gas are present in the flue 2. The flue 2 will expand and contract slightly due to temperature changes. The main body of the high-rise building may also experience micro-vibrations due to wind load, elevator vibration, temperature stress or uneven settlement. If traditional mortar is used for sealing, a rigid connection will be formed between the flue 2 and the floor slab component 1. The above-mentioned micro-relative movements will cause tensile or shear cracks at the junction of the mortar and the outer wall of the flue. In this embodiment, the bottom end of the flue 2 is flexibly isolated by the support component 3, and the top end is flexibly constrained by the sealing component 4. The flue 2 and the floor slab component 1 no longer form a stress state with both ends rigidly connected. Therefore, when the flue 2 undergoes thermal expansion and contraction or slight displacement, the support component 3 and the sealing component 4 can release stress through compression, shearing or rebound, respectively, to avoid stress concentration at a single joint.

[0067] More importantly, the bottom concrete curb 12 does not lose its vertical support function due to the introduction of the support member 3. On the contrary, the bottom concrete curb 12 continues to provide reliable support through the support surface 121. The support member 3 only changes the way the force is transmitted, without canceling the support path. Thus, this embodiment simultaneously satisfies the two seemingly contradictory requirements of no unloading and flexible crack resistance. On the one hand, it can support the flue 2 without setting up a separate steel reinforcement unloading structure; on the other hand, it avoids a rigid collision between the flue 2 and the concrete curb 12. This is different from simply applying sealant to the outer perimeter of the flue, and also different from setting up a concrete curb separately. It establishes a stable but not rigid flue installation node through the combination of vertical rigid support and local flexible isolation.

[0068] When a trace amount of gas attempts to escape from the annular gap 5 between the outer wall 21 of the flue and the tongue and groove joint 13 of the top floor slab, the gas is first blocked by the innermost flexible baffle 421. Since the free end of the flexible baffle 421 is tilted towards the direction of the airflow, the airflow pressure will cause the flexible baffle 421 to press further against the outer wall 21 of the flue, thus forming a self-reinforcing sealing state with greater pressure and tighter fit. Even if there are extremely small gaps, the gas enters the labyrinth flow-blocking cavity 43 after passing through the first flexible baffle 421, where its speed decreases and local eddies are generated. Subsequently, the gas needs to continue to pass through the second and third flexible baffles 421. The multi-stage throttling and backflow cause the gas pressure to decrease step by step, making it difficult to form a perceptible air leak or odor. At the same time, the oil mist and water vapor in the flue gas are more likely to adhere and condense in the labyrinth flow-blocking cavity 43 due to the reduced flow velocity, forming a thin oil film or wet film. This oil film further fills the micro gaps, which in turn enhances the long-term airtightness.

[0069] As can be seen from the above structure and dynamic process, the bottom concrete inverted curb 12 provides vertical support, so that the flue 2 does not need to be unloaded by steel reinforcement; the support member 3 makes the support interface flexible, avoiding damage to the thin-walled flue due to hard contact; the top floor slab tongue and groove 13 provides a compression installation cavity and anti-reverse reaction force for the sealing component 4; the sealing component 4 blocks the direct gas passage path through the flexible baffle 421 and the labyrinth flow obstruction cavity 43. The above structures together form a synergistic system of lower support and vibration isolation, upper flexible flow obstruction, and overall no unloading, thereby solving the problems of traditional mortar sealing being prone to cracking in the long term and ordinary flexible materials being prone to aging and insufficient fire resistance.

[0070] Example 2:

[0071] This embodiment further explains the specific structure of the sealing component 4 based on embodiment 1. In embodiment 1, the sealing component 4 can be a continuous annular prefabricated seal. However, in actual construction, there may be differences in the outer wall dimensions of the flue 2, the construction deviation of the floor slab tongue and groove 13, and the on-site hoisting space. In order to improve the adaptability of the sealing component to different flue specifications and construction errors, this embodiment provides a sealing component 4.

[0072] In this embodiment, the sealing component 4 includes a temperature-resistant body 41, a flow-blocking sealing part 42, a labyrinth flow-blocking cavity 43, and a self-locking texture 44. The sealing component 4 can be configured as a segmented annular structure, that is, formed by two, three, or four arc-shaped sealing segments. Each arc-shaped sealing segment has segmented joints 46 at both ends. Adjacent arc-shaped sealing segments are spliced ​​together through segmented joints 46. The segmented joints 46 adopt a toothed overlapping structure with mutual staggered joints. With the segmented structure, the construction personnel do not need to put the sealing ring on the top of the flue 2 as a whole. Instead, after the flue 2 has been partially positioned, multiple arc-shaped sealing segments can be surrounded on the outer wall 21 of the flue from the side and then pressed into the annular gap 5 as a whole.

[0073] In this embodiment, to avoid the problem of weak air leakage paths at the joints of the segmented structure, the segmented joint 46 is configured as an axially staggered joint structure. Specifically, the end of the heat-insulating body 41 of one arc-shaped sealing section overlaps with the end of the heat-insulating body 41 of another arc-shaped sealing section in the axial direction, while the end of the flexible tongue 421 overlaps at another axial position, so that the body joint and the tongue joint are not in the same straight line or the same radial section. In this way, even if gas enters a certain joint area, it needs to go through at least one axial and radial deflection before it can continue to pass, thereby avoiding the segmented structure from weakening the labyrinth flow obstruction effect.

[0074] In a preferred embodiment, the sealing component 4 has a wedge-shaped cross-section, with its upper radial thickness being less than its lower radial thickness, forming an installation guide surface 45. The installation guide surface 45 is used to reduce the initial insertion force when the sealing component is pressed downward into the annular gap 5, and to allow the sealing component to gradually enter a radial compression state. The installation guide surface 45 can be set on one side near the inner wall 131 of the tongue and groove, or it can be set on both sides near the outer wall 21 of the flue and near the inner wall 131 of the tongue and groove. When the construction error causes the local width of the annular gap 5 to be too small, the wedge-shaped structure can guide the sealing component to enter the gap in a progressive compression manner, rather than causing flange turning, curling or local shearing damage at the inlet.

[0075] In this embodiment, the self-locking texture 44 is a combination of inverted teeth 442 and corrugated segments 443. The top of the inverted teeth 442 faces outward and abuts against the inner wall 131 of the tongue and groove. The upper side of the inverted teeth 442 can be a stop surface, and the lower side can be a guide slope. When the sealing component 4 is pressed down, the guide slope first contacts the inner wall 131 of the tongue and groove, causing the inverted teeth 442 to elastically deform inward. After the sealing component is pressed into place, the inverted teeth 442 rebound, the stop surface abuts against the inner wall 131 of the tongue and groove, and the corrugated segments 443 are set between adjacent inverted teeth 442 as a compressible deformation buffer. This combination structure allows the sealing component 4 to be pressed in smoothly and resist floating, rebounding and exiting, or loosening caused by airflow pulsation after installation.

[0076] In this embodiment, the flow-blocking sealing part 42 adopts a bidirectional flexible baffle structure. Specifically, among the multiple flexible baffles 421, the free ends of some flexible baffles 421 are inclined downwards, and the free ends of other flexible baffles 421 are inclined upwards. The two are arranged alternately. The downwardly inclined flexible baffles 421 mainly block the escape of oil fumes from bottom to top, while the upwardly inclined flexible baffles 421 mainly block the backflow of cold air, water vapor infiltration, or negative pressure backflow from top to bottom. The alternately arranged bidirectional flexible baffles 421 form a multi-level bidirectional labyrinth structure in the annular gap 5, so that the sealing component is not only suitable for unidirectional smoke exhaust conditions, but also suitable for high-rise buildings with significant wind pressure changes and multi-household shared flue environments.

[0077] Furthermore, the thickness of each flexible tongue 421 can gradually decrease from the root 422 to the free end 423. The root 422 is thicker, which can ensure sufficient connection strength between it and the heat-insulating body 41. The free end 423 is thinner, which can improve the fitting sensitivity and elastic deformation ability. When the flexible tongue 421 is pressed against the outer wall 21 of the flue, the thinner free end can adapt to the roughness, local warping or slight dimensional deviation of the outer wall 21 of the flue, forming a line seal or narrow surface seal. After multiple flexible tongues 421 form multiple sealing lines, even if one tongue is not completely fitted due to local impurities or construction deviations, the other tongues can still continue to play the role of flow obstruction and sealing.

[0078] During the dynamic installation process in this embodiment, the construction personnel first splice multiple arc-shaped sealing sections around the outer wall 21 of the flue to form a ring, so that the segmented joints 46 overlap each other; then, a pressing tool is used to apply force evenly along the circumference of the sealing component, so that the installation guide surface 45 first enters the annular gap 5; when pressing down, the reverse teeth 442 and the corrugated section 443 are compressed by the tongue and groove inner wall 131 in sequence, and the sealing component 4 as a whole generates radial elastic pre-tightening; after pressing into place, the reverse teeth 442 rebound and form a stop fit with the tongue and groove inner wall 131, while the flexible tongue 421 adheres to the outer wall 21 of the flue under radial pressure. At this time, the outer wall 21 of the flue, the flexible tongue 421, the labyrinth flow-blocking cavity 43, the temperature-insulating body 41 and the tongue and groove inner wall 131 together form a composite sealing path.

[0079] Therefore, compared with Example 1, this example improves on-site adaptability and anti-loosening ability. The segmented ring structure solves the problem that the integral sealing ring is not easy to fit in narrow construction space; the staggered segmented joint 46 avoids the risk of air leakage caused by segmentation; the wedge-shaped installation guide surface 45 reduces the difficulty of pressing in and reduces the risk of damage to the flue 2 caused by construction personnel forcibly knocking; the reverse teeth 442 and the corrugated section 443 enable the sealing component to maintain anti-retraction and pre-tightening under long-term thermal expansion and contraction and airflow pulsation. After the above features are combined with the single cast-in-place tongue and groove in Example 1, the tongue and groove 13 of the top floor slab is no longer just passively accommodating the sealing material, but becomes the reaction structure required for reverse tooth anti-retraction, corrugated compression and tongue fitting, thereby further enhancing the reliability of the overall node.

[0080] Example 3:

[0081] This embodiment is a functional optimization and extension based on Embodiment 1 or Embodiment 2, and describes the temperature-resistant main body 41. Although traditional flexible sealing materials can absorb deformation, they are prone to aging, softening, burning or losing sealing ability under high temperature, oil stains, corrosive gases or fire conditions in flues. If rigid fire-resistant materials such as inorganic mortar are used instead, they will crack under daily thermal expansion and contraction and micro-vibration of buildings. This embodiment uses phase change ceramic materials to make the sealing component 4 exhibit different mechanical and temperature-resistant properties under different temperature conditions, thereby solving the technical contradiction between flexible crack resistance and rigid fire resistance.

[0082] In this embodiment, the temperature-resistant body 41 is made of phase change ceramicized silicone rubber, which includes a silicone rubber matrix, low-melting-point glass powder, and ceramicizing additives. The silicone rubber matrix provides flexibility, elastic recovery capability, and weather resistance at room temperature. The low-melting-point glass powder softens or melts at high temperatures and forms a binding phase between the filler particles. The ceramicizing additives are used to promote the formation of a ceramicized skeleton at high temperatures, transforming the originally flexible sealing component into an inorganic ceramic shell with a certain strength. In an optional embodiment, inorganic refractory fillers, intumescent fillers, flame retardants, or reinforcing fibers can also be added to the phase change ceramicized silicone rubber to improve the integrity and crack resistance after ceramicization.

[0083] Within the range of ambient temperature and daily smoke exhaust temperature, the heat-insulating body 41 remains in an elastomeric state. At this time, the silicone rubber matrix allows the sealing component to maintain radial compression in the annular gap 5 and allows for slight relative displacement between the flue 2 and the floor slab component 1. Low-melting-point glass powder and ceramic-forming additives are dispersed in the silicone rubber matrix as fillers and do not cause the sealing component to exhibit a rigid mortar state. Therefore, in daily use, the heat-insulating body 41, together with the flexible baffle 421, can still absorb vibration, thermal expansion and contraction, and construction deviations, avoiding fatigue cracks at the joints.

[0084] When abnormal high temperature or fire occurs in the flue, the working state of the heat-insulating body 41 changes. As the temperature rises, the silicone rubber matrix gradually pyrolyzes and forms a silicon-containing residual skeleton; the low-melting-point glass powder softens and fills the gaps between particles; the ceramic-forming additive promotes the sintering of inorganic components, so that the heat-insulating body 41 gradually transforms from an elastomer into a ceramic shell. If the heat-insulating body 41 contains a micro-expansion component, the component can also generate micro-expansion in volume at high temperature, so that the ceramic shell further presses the outer wall 21 of the flue and the inner wall 131 of the tongue and groove. Thus, the sealing component originally used for flexible crack resistance is transformed into a rigid heat-insulating sealing structure in the event of a disaster.

[0085] The temperature response process is particularly important in conjunction with the structure of the tongue and groove joint 13 of the floor slab. If the phase change ceramic material exists alone in an open space, the micro-expansion at high temperature will cause the material to bulge or crack, and it will be unable to form a stable seal. In this embodiment, the heat-resistant body 41 is confined in the annular gap 5 between the outer wall 21 of the flue and the top floor slab tongue and groove joint 13. The inner wall 131 of the tongue and groove provides constraint on its outer side, and the outer wall 21 of the flue provides constraint on its inner side. When the heat-resistant body 41 expands and ceramicizes at high temperature, the annular gap 5 becomes the mold cavity for the ceramicized shell, so that the expansion trend of the material is transformed into radial compression force instead of disordered cracking. In this way, the high-temperature ceramicized layer can form a continuous or substantially continuous fire-resistant ring between the outer wall of the flue and the tongue and groove joint of the floor slab.

[0086] Furthermore, the flexible baffle 421 also participates in ceramic sealing under high temperature conditions. At room temperature, the flexible baffle 421 fits the outer wall 21 of the flue in the form of a thin lip, forming a multi-level labyrinth flow obstruction. At high temperature, the flexible baffle 421 heats up and ceramicizes faster due to its thinness. Multiple ceramic contact zones are formed at the contact point between its free end and the outer wall 21 of the flue. The multiple ceramic contact zones are distributed along the axial direction, which is equivalent to forming multiple fire-resistant baffle rings in the annular gap 5. Even if a baffle ring is partially damaged due to thermal shock, the other baffle rings and the heat-insulating body 41 can still continue to block the crossflow of flames, hot flue gas and high-temperature gas.

[0087] In this embodiment, a heat-resistant surface layer is provided on the side of the heat-resistant body 41 near the flue, and a reinforcing surface layer is provided on the side near the tongue and groove. The heat-resistant surface layer has a relatively high content of low-melting-point glass powder and ceramic-forming additives, so as to form a ceramic protective layer quickly under the impact of high-temperature flue gas. Fibrous inorganic fillers can be added to the reinforcing surface layer to improve the anti-peeling ability between the ceramicized surface and the inner wall 131 of the tongue and groove. Through the differentiated design of the inner and outer layers, the sealing component 4 can quickly form ceramics on the side near the heat source and maintain overall support on the side near the structure, thereby improving the integrity during disasters.

[0088] Thus, the heat-insulating body 41 works together with the bottom concrete curb 12, the support 3, the top floor slab tongue and groove 13, and the labyrinth flow-blocking cavity 43 in Example 1, instead of relying solely on the fire resistance performance of the materials to solve the problem. Under normal conditions, the support 3 and the heat-insulating body 41 jointly release structural stress and avoid rigid cracks. When there is a small amount of smoke leakage, the labyrinth flow-blocking cavity 43 reduces the airflow speed and temperature, slowing down the heat-insulating body 41 from being washed by oil fumes and thermal aging. Under fire conditions, the top floor slab tongue and groove 13 constrains the ceramic expansion of the heat-insulating body 41, transforming it into a stable fire-resistant ring. Thus, this embodiment realizes an adaptive heat-insulating mechanism with normal temperature flexibility, hot ceramic formation, tongue and groove constraint, and ring sealing. Its technical effect cannot be directly obtained by ordinary rubber seals or ordinary fireproof mortar.

[0089] Example 4:

[0090] This embodiment is a further optimization based on embodiments 1 to 3. In the traditional view, oil stains in fumes are usually regarded as adverse factors that lead to aging, contamination and failure of sealing materials. Therefore, conventional designs often try to discharge oil stains as soon as possible or avoid oil stains from contacting the seals. However, this embodiment utilizes the low-speed vortex region of the labyrinth flow-blocking cavity 43 to form a thin film of trace amounts of oil mist and water vapor in the local cavity, thereby transforming the originally unfavorable oil stain environment into an auxiliary sealing factor without affecting the normal exhaust of the flue.

[0091] In this embodiment, the flow-blocking sealing part 42 includes at least three flexible baffles 421, and at least two labyrinth flow-blocking cavities 43 are formed between adjacent flexible baffles 421. Each labyrinth flow-blocking cavity 43 is distributed at intervals along the axial direction of the flue 2, and its radial width is smaller than the original width of the annular gap 5. It is further separated by the inclined fitting state of the flexible baffles 421. The labyrinth flow-blocking cavity 43 is not a completely closed cavity, but forms a non-direct communication relationship through the small contact gap between the flexible baffles 421 and the outer wall 21 of the flue, the corner gap between the flexible baffles 421 and the heat-blocking body 41, and the compression interface between the sealing component and the tongue and groove inner wall 131.

[0092] When the gas pressure generated in the flue flue flues, a very small amount of oil fumes may enter the labyrinthine flow-blocking cavity 43 closest to the flue. Because this cavity has a larger local cross-sectional area and more return boundaries compared to the straight-through gap, the gas velocity decreases and forms a vortex after entering. Under the influence of vortex, collision and temperature difference, the oil mist particles in the oil fume are more likely to adhere to the surface of the flexible baffle 421, the surface of the flue outer wall 21 and the surface of the heat-insulating body 41. As the usage time increases, the adhered oil mist forms an extremely thin oil film. The oil film can fill the micro-rough gap between the flexible baffle 421 and the flue outer wall 21, and improve the continuity of the contact seal.

[0093] To avoid excessive oil film accumulation leading to pollution or blockage, in this embodiment, the flexible baffle 421 is configured to gradually decrease in height from the inside to the outside, or to have a structure with a longer inner baffle and a shorter outer baffle. The longer inner baffle is used to withstand the main oil fume impact and form the main oil film sealing area, while the shorter outer baffle is used to form a backup flow obstruction and odor prevention area. In this way, the oil film mainly stays in the labyrinth flow obstruction cavity 43 near the flue and is not easy to continue to spread to the outside of the floor tongue and groove 13. Furthermore, the surface of the flexible baffle 421 can be provided with fine textures or micro-grooves to improve the oil film adhesion stability, but the micro-grooves should not form a through exhaust channel.

[0094] In a preferred embodiment, the lower part of the labyrinth flow-blocking cavity 43 is provided with a micro-slope. This micro-slope can be naturally formed by the inclined surface of the flexible baffle 421 or by the partial molding of the inner wall of the heat-blocking body 41. The micro-slope causes excess condensate or oil to tend to flow back to the side near the outer wall 21 of the flue under the action of gravity, rather than seeping outward along the inner wall 131 of the tongue and groove. For vertical flues, after the oil flows back to the inner side of the flue, it can be gradually carried away or remain on the inner wall of the flue with the subsequent flue gas flow, and will not form pollution on the outside of the floor joint.

[0095] The labyrinth flow-blocking structure in this embodiment also has the function of reducing local thermal shock. If hot flue gas enters the annular gap 5 in a straight line, it will directly scour a local area of ​​the sealing material and accelerate the aging of the material. However, after passing through multiple flexible baffles 421, the hot flue gas continuously changes direction and mixes with the relatively stationary gas in each cavity, and its flow rate and thermal shock intensity are reduced. In this way, the thermal shock of the heat-blocking body 41 under normal high-temperature oil fume environment is weaker, and the material aging rate is reduced. Only under extreme high-temperature conditions such as fire, the heat-blocking body 41 enters the ceramic fire-resistant state.

[0096] During dynamic operation, the labyrinth flow-blocking cavity 43 acts as an airflow throttling cavity, reducing the pressure of the small amount of escaping airflow in multiple stages. It can also act as an oil mist condensation and adhesion cavity, allowing the oil mist to form an auxiliary oil film seal. It can also act as a thermal shock buffer cavity, allowing the hot flue gas to diffuse and slow down before entering the sealing body. These three functions are interconnected rather than isolated and superimposed. Because the airflow is slowed down, the oil mist has time to adhere. Due to the oil film adhesion, the tiny gaps are further reduced, making it more difficult for the airflow to pass through. Because the airflow is more difficult to pass through, the thermal shock is also further reduced. This cycle allows the labyrinth flow-blocking structure to exhibit an auxiliary sealing effect that becomes more and more fitted over long-term use, thus distinguishing it from the failure mode of traditional mortar where air leakage gradually worsens after cracking.

[0097] When this embodiment is combined with Embodiment 3, the oil film mainly serves as a micro-crack filler under normal conditions. When a fire occurs, a small amount of oil film near the high-temperature flue may be carbonized or ablated by the high temperature. However, at the same time, the temperature-resistant body 41 and the flexible tongue 421 begin to ceramicize. The micro-crack area where the original oil film is located is filled by ceramicized products and micro-expansion structures. In other words, the micro-crack filling function undertaken by the oil film under normal conditions is taken over by the ceramicized layer under high-temperature conditions. This temperature state conversion enables the sealing node to maintain its sealing ability under different working conditions.

[0098] Example 5:

[0099] This embodiment introduces a root waterproof node 6 based on the aforementioned embodiment to solve the problems of leakage and cracking of the waterproof layer in the root area of ​​the flue bottom. In the installation of building flues, the root of the flue is usually also a weak point in the waterproofing of water-contaminated areas such as kitchens and bathrooms. If there is a right angle intersection between the flue 2 and the bottom concrete curb 12, the subsequent additional waterproof layer 62 is prone to hollowing, cracking or being punctured by sharp corners at the corner. If only sealant or mortar is used for sealing, it is difficult to simultaneously take into account structural support, air tightness and waterproofing. Therefore, this embodiment combines the bottom concrete curb 12, the support 3, the sealing component 4 and the root waterproof node 6 into a three-in-one or multi-level protection system.

[0100] like Figure 2 As shown, the root waterproof node 6 includes a rounded corner 61 and a waterproof additional layer 62. The rounded corner 61 is set at the root of the junction between the bottom concrete curb 12 and the flue 2. Preferably, the radius of the rounded corner 61 is not less than 50mm. The rounded corner 61 can be made of waterproof mortar, polymer cement mortar or slope-finding material compatible with the subsequent waterproofing material. The function of the rounded corner 61 is not to bear the main vertical load of the flue 2, but to provide a continuous and smooth base layer for the waterproof additional layer 62, and to avoid stress concentration at right angles.

[0101] The additional waterproof layer 62 covers the rounded corner 61 and extends to the upper surface of the floor slab body 11 and the lower part of the outer wall 21 of the flue. The additional waterproof layer 62 can be a coating waterproof layer, a roll material additional layer, a polymer cement waterproof layer or other building waterproof materials. After the additional waterproof layer 62 is combined with the rounded corner 61, a smooth transition surface is formed at the root of the flue, so that water vapor or surface water is not easy to seep into the area around the floor slab opening 14 along the right-angle seam at the root of the flue. For kitchen or bathroom flues, this structure can reduce root leakage caused by ground water, cleaning water or condensation.

[0102] In this embodiment, the bottom concrete upstand 12 serves as the first layer of waterproofing and water-blocking. Since the bottom concrete upstand 12 and the floor slab body 11 are cast in one piece, there is no post-cast construction joint. This can prevent water on the floor slab surface from directly seeping down along the perimeter of the flue opening 14. The support member 3 serves as the second layer of flexible isolation. Its horizontal pressure-bearing part 31 and vertical isolation part 32 prevent hard contact cracking between the flue 2 and the bottom concrete upstand 12. The root waterproof node 6 serves as the third layer of surface waterproofing. Its rounded corner 61 and waterproof additional layer 62 allow the surface waterproofing to continuously cross the root of the flue. The sealing component 4 serves as the airtight and temperature-insulating function at the top floor slab tongue and groove joint 13, preventing the spread of smoke, odor and flame along the floor slab joint.

[0103] In this embodiment, the bottom concrete curb 12 is cast in place in one go, thus avoiding the construction joint between the bottom concrete curb 12 and the floor slab body 11, which may become a leakage path, as is the case with post-cast structures. Moreover, if the bottom of the flue 2 is directly pressed on the curb, thermal expansion and contraction and micro-vibration may cause the root waterproof layer to be repeatedly stretched. In this embodiment, the support 3 releases the micro-displacement of the flue 2, making the arc corner 61 and the additional waterproof layer 62 less likely to be repeatedly torn. If there is only bottom waterproofing and the top joint is leaking, odor may still be generated. In this embodiment, the sealing component 4 forms a labyrinth flow barrier at the top, which, together with the bottom waterproof node, forms an integrated node for waterproofing, odor prevention, and fire prevention.

[0104] During construction, the rounded corner 61 is preferably constructed after the flue 2 is installed and its verticality is adjusted. If the rounded corner 61 is constructed first and then the flue 2 is hoisted, the rounded corner 61 may be damaged due to collision during hoisting. If the additional waterproof layer 62 is laid before the flue 2 is stably positioned, the subsequent fine-tuning of the flue may crack the waterproof layer. Therefore, the preferred construction sequence in this embodiment is as follows: first, cast the bottom concrete curb 12 and the top floor slab tongue and groove 13 in one go; then lay the support component 3; then hoist the flue 2 and place it in position; then press in the sealing component 4; finally, smooth the rounded corner 61 at the root and lay the additional waterproof layer 62. This sequence allows the structural positioning, flexible sealing and waterproof finishing to be completed in sequence, reducing mutual interference.

[0105] Example 6

[0106] This embodiment provides a construction process for an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue-and-groove joint, which can be used to implement the flue system in any of the aforementioned embodiments.

[0107] During the main structure construction phase, the flue positioning mold 7 is positioned and fixed simultaneously with the floor slab reinforcement. The flue positioning mold 7 is used to define the position and shape of the flue opening 14, the bottom concrete curb 12, and the top floor slab tongue and groove 13. The flue positioning mold 7 may include an inner mold, an outer mold, and a tongue and groove forming mold. The inner mold is used to form the inner boundary of the flue opening 14, the outer mold is used to form the outer boundary of the bottom concrete curb 12, and the tongue and groove forming mold is used to form the step or groove structure of the top floor slab tongue and groove 13. After the flue positioning mold 7 is tied or temporarily fixed with the floor slab reinforcement, the floor slab body 11, the bottom concrete curb 12, and the top floor slab tongue and groove 13 are cast in place at one time when the floor slab concrete is poured.

[0108] In this way, the planar position, elevation, and cross-sectional dimensions of the anti-reflective curb and tongue-and-groove joint are controlled at the main structure stage, avoiding the eccentricity of the flue 2, uneven gaps, or inconsistent mortar thickness caused by positioning errors during the traditional secondary formwork. In particular, the inner wall 131 of the tongue-and-groove joint 13 of the top floor slab can form a relatively regular sealing installation surface under the constraint of the formwork, providing a reliable compression reaction surface for the subsequent sealing components 4. After the bottom concrete anti-reflective curb 12 and the floor slab body 11 are formed in one go, there is no construction joint between the old and new concrete at its root, reducing the risk of leakage from the source.

[0109] The support component 3 is laid at the support position of the bottom concrete inverted curb 12. Before laying, the laitance, sand and sharp protrusions on the support surface 121 are cleaned, and the local high points are ground to avoid sharp protrusions piercing the support component 3. The support component 3 is laid around the bottom concrete inverted curb 12, so that the horizontal bearing part 31 covers the support surface 121 and the vertical isolation part 32 is against the lateral positioning surface 122. If the support component 3 adopts a multi-segment splicing form, the adjacent segments are preferably staggered and overlapped, and the joints are avoided from the main stress corners of the flue 2.

[0110] The flue 2 is hoisted onto the bottom concrete curb 12, and the top end 23 of the flue is inserted into the tongue and groove joint 13 of the top floor slab. During hoisting, the flue 2 is lowered vertically by mechanical hoisting, so that the bottom end face 22 of the flue gradually presses against the horizontal bearing part 31. Since the support 3 has a certain elasticity, the flue 2 can be slightly buffered during the lowering process to avoid hard collision. After the flue 2 is lowered, it is horizontally limited by the lateral positioning surface 122 of the bottom concrete curb 12 and the vertical isolation part 32 of the support 3, and the verticality is corrected. An annular gap 5 for pressing the sealing component 4 should be formed between the outer wall 21 of the flue and the tongue and groove joint 13 of the top floor slab.

[0111] The prefabricated sealing component 4 is fitted or enclosed on the outer wall 21 of the flue and pressed into the annular gap 5 along the axial direction of the flue 2. If the sealing component 4 is an integral annular part, it can be fitted from the top or bottom before the flue 2 is fully in place. If it is a segmented annular part, it can be joined from the side after the flue 2 is in place. When pressing, a pressure plate, rubber hammer or special pressing tool can be used to apply force evenly in the circumference to avoid single-point knocking that may cause the sealing component to flip up or the flue 2 to break. During the pressing process, the installation guide surface 45 first enters the annular gap 5, the self-locking texture 44 is gradually deformed by pressure, and the flexible tongue 421 gradually fits into the outer wall 21 of the flue. After being pressed into place, the self-locking texture 44 and the tongue and groove inner wall 131 form a stop fit, and the flexible tongue 421 forms a multi-level labyrinth flow obstruction path in the gap.

[0112] At the junction of the bottom concrete curb 12 and the flue 2, construct an arc corner 61 and lay an additional waterproof layer 62. The radius of the arc corner 61 is preferably not less than 50mm. When constructing the arc corner 61, ensure that the transition between it and the floor slab body 11, the bottom concrete curb 12 and the outer wall 21 of the flue is smooth, and there should be no hollow areas, cracks or sharp corners. After the arc corner 61 meets the requirements of subsequent waterproofing construction, lay the additional waterproof layer 62 on its surface and extend the additional waterproof layer 62 to the floor slab body 11 and the outer wall 21 of the flue with a certain width to form a continuous waterproof seal.

[0113] Example 7:

[0114] When the flue 2 has a circular cross-section, the bottom concrete curb 12 can be set as an annular curb, the top floor slab tongue and groove 13 can be set as an annular tongue and groove, the sealing component 4 can be set as an annular seal, the flexible tongue 421 is continuously arranged along the circumference, and the labyrinth flow-blocking cavity 43 is manifested as multiple coaxial annular cavities. The advantage of the circular structure is that the radial compression is more uniform, and the circumferential force of the sealing component 4 is more consistent.

[0115] When the flue 2 has a rectangular or square cross section, the sealing component 4 can be provided with a thickened area or a rounded transition area at the corner. Since the corners of a rectangular flue are prone to stress concentration and uneven construction gaps, the thickened area at the corner can improve the compression and rebound capacity of the sealing component at the corner. The rounded transition area can prevent the flexible tongue 421 from breaking or turning over at the corner. For segmented sealing components, the segmented joint 46 is preferably set in the middle of the straight edge, avoiding the rectangular corner, to reduce the risk of air leakage at the corner.

[0116] When the floor height is high or the flue 2 is heavy, the height or width of the bottom concrete curb 12 can be appropriately increased to increase the vertical support area. The horizontal pressure-bearing part 31 of the support 3 can also be thickened or hardened accordingly so that it can maintain a reasonable amount of compression when bearing the weight of the flue. For lighter thin-walled flues, a softer support 3 can be used to improve the ability to isolate vibration and absorb construction errors. Regardless of how the specific parameters change, the common principle is that the bottom concrete curb 12 bears the main vertical load, the support 3 provides a flexible support interface, and the sealing component 4 provides flexible flow resistance and high-temperature ceramic barrier at the top.

[0117] For vertical flues installed continuously between floors, each floor slab can be equipped with the bottom concrete curb 12, the top floor slab tongue and groove 13, the support 3, and the sealing component 4 of this invention. In this way, each flue node forms an independent flexible vibration isolation and flow-blocking sealing unit. Even if a certain floor undergoes local deformation due to construction or use, it is not easy to transmit to the flue nodes of adjacent floors through rigid connection. Compared with the traditional multi-layer continuous rigid sealing structure, this embodiment can reduce the concentrated damage of a weak joint caused by cumulative deformation.

[0118] Example 8:

[0119] Under normal flue gas exhaust conditions, the hot flue gas in flue 2 flows vertically, the wall temperature of flue 2 rises and produces a slight expansion. Since the bottom end of flue 2 is not directly pressed against the bottom concrete curb 12, but contacts it through the support member 3, the slight displacement of the bottom end face 22 of the flue can be released by the compression and shearing of the horizontal bearing part 31. At the same time, the annular gap 5 at the top end 23 of the flue is filled by the sealing component 4. The heat-insulating body 41 and the flexible baffle 421 allow the outer wall 21 of the flue to undergo slight radial or axial displacement, without forming irreversible cracks like mortar.

[0120] Under micro-deformation conditions, such as when a high-rise building experiences slight inter-story displacement due to wind load, temperature changes, or uneven settlement, a relative displacement trend will occur between the floor slab component 1 and the flue 2. The bottom concrete curb 12 provides stable support to prevent the flue 2 from sinking as a whole; the support component 3 releases the bottom contact stress; and the sealing component 4 releases the top gap stress. Since neither the upper nor lower nodes are rigid and fully bonded structures, the displacement will not concentrate and tear a certain mortar sealing layer, but will be dispersed and absorbed by the flexible components.

[0121] Under negative pressure odor conditions, such as when the exhaust fan on a local floor in a public flue is started or when changes in external wind pressure cause pressure fluctuations in the flue, odorous gases enter the room along the floor slab joints. At this time, the flexible baffle 421 in the top annular gap 5 is first subjected to airflow pressure and adheres tightly to the outer wall 21 of the flue, forming a pressure-responsive seal. If the gas passes through the first baffle, it will slow down, eddy, and experience pressure attenuation in the labyrinth flow-blocking cavity 43. Subsequent flexible baffles 421 continue to block the gas, making it difficult for the gas to form a through flow. Compared with traditional single-layer adhesive or single-layer mortar, multiple flexible baffles 421 and labyrinth flow-blocking cavities 43 form a multi-level redundant seal.

[0122] In the case of a fire at high temperatures, the high-temperature flue gas or flames in the flue transfer heat to the floor joints. This invention achieves this by gradually ceramicizing and slightly expanding the heat-insulating body 41 at high temperatures, and the flexible baffle 421 is also transformed into multiple ceramic baffle rings. The top floor tongue and groove 13 restricts the expansion direction of the heat-insulating body 41, so that the expansion pressure is transformed into a pressing force on the outer wall 21 of the flue and the inner wall 131 of the tongue and groove. Finally, a ceramic heat-insulating sealing layer is formed in the annular gap 5, which blocks the spread of flames and high-temperature flue gas along the floor gap, and avoids the possibility of conventional flexible sealing materials softening, melting or burning, while rigid mortar may crack due to thermal shock.

[0123] In this way, it can release flexibly when there is slight movement at room temperature to cope with long-term crack resistance; when the air pressure fluctuates, the tongue can self-reinforce its fit to prevent odor from mixing; when the oil fumes are used for a long time, the labyrinth cavity forms an auxiliary oil film to ensure airtightness of the micro-seams; when the fire is at high temperature, the main body is ceramicized and forms a rigid fire-resistant ring under the constraint of the tongue and groove to cope with fire prevention and temperature resistance, thus forming a multi-state response mechanism.

[0124] Based on the preferred embodiments of the present invention described above, those skilled in the art can make various changes and modifications without departing from the inventive concept. The technical scope of this invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.

Claims

1. An adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove joints, characterized in that, include: The floor slab component includes a floor slab body, a bottom concrete curb integrally formed with the floor slab body, and a top floor slab tongue and groove joint. The flue has its bottom end supported by a bottom concrete curb and its top end inserted through the tongue and groove joint of the top floor slab. A support member, wherein the support member is disposed between the bottom end of the flue and the bottom end concrete curb; and A sealing assembly is disposed within the annular gap formed between the outer wall of the flue and the tongue and groove joint of the top floor slab; The sealing assembly includes a flow-blocking sealing part and a temperature-blocking body. The flow-blocking sealing part is used to form a non-straight labyrinth flow-blocking path in the annular gap. The temperature-blocking body is configured to maintain elastic deformation capability under normal temperature use and to form a rigid temperature-blocking sealing layer by ceramicization under high temperature. The support member and the sealing assembly form a flexible isolation at the bottom and top of the flue, respectively, to cut off the rigid force transmission path between the flue and the floor slab component, and the bottom concrete curb provides vertical support for the flue.

2. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: The bottom concrete curb is set around the flue opening, and the outer periphery of the bottom concrete curb is adapted to the bottom inner cavity of the flue to position and vertically support the flue; the top floor slab tongue and groove is set around the top periphery of the flue and together with the outer wall of the flue defines an annular gap for accommodating the sealing component.

3. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: The supporting component is an L-shaped weather-resistant rubber shock-absorbing pad, which includes a horizontal pressure-bearing part and a vertical isolation part. The horizontal pressure-bearing part is sandwiched between the bottom end face of the flue and the support surface of the bottom concrete curb, and the vertical isolation part is located between the bottom side wall of the flue and the lateral positioning surface of the bottom concrete curb.

4. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: The sealing assembly is a prefabricated annular seal, the flow-blocking seal is integrally formed with the temperature-blocking body, and the prefabricated annular seal is filled into the annular gap under radial pressure.

5. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: The flow-blocking sealing part includes multiple flexible baffles spaced apart along the axial direction of the flue. The free ends of the multiple flexible baffles are inclined in the opposite direction of the flue gas escape direction. After the sealing assembly is pressed into the annular gap, they elastically fit with the outer wall of the flue or the inner wall of the tongue and groove of the top floor slab to form a multi-stage throttling and pressure-reducing labyrinth flow-blocking cavity.

6. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 4, characterized in that: The outer peripheral wall of the sealing component is provided with a self-locking texture, which includes at least one of circumferential ribs, reverse teeth, corrugations, or roughened textures. The self-locking texture is used to form a locking fit with the inner wall of the tongue and groove of the top floor slab after the sealing component is pressed into the annular gap.

7. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: The temperature-resistant body is made of phase change ceramicized silicone rubber, which contains a silicone rubber matrix, low-melting-point glass powder and ceramic-forming additives, so that the temperature-resistant body undergoes micro-expansion in volume at high temperature and sintersects to form an inorganic ceramic shell.

8. The adaptive flexible temperature-resistant sealing flue system based on unloading tongue and groove as described in claim 1, characterized in that: It also includes a root waterproofing node, which includes a rounded corner set at the junction of the bottom concrete curb and the flue, and an additional waterproofing layer covering the rounded corner, wherein the radius of the rounded corner is not less than 50mm.

9. A construction process for an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue-and-groove joint, based on the flue system described in any one of claims 1-8, characterized in that, Includes the following steps: S1. During the main structure construction phase, the flue positioning mold and the floor slab reinforcement are positioned and fixed simultaneously, and when pouring the floor slab concrete, the floor slab body, the bottom concrete curb and the top floor slab tongue and groove are cast in one go. S2. Lay a support component at the support position of the bottom concrete curb, so that the support component is located between the bottom end of the flue to be installed and the bottom concrete curb. S3. Hoist the flue onto the bottom concrete curb and make the top of the flue pass through the tongue and groove of the top floor slab to form an annular gap between the outer wall of the flue and the tongue and groove of the top floor slab. S4. The prefabricated sealing assembly is fitted onto the outer periphery of the flue and pressed into the annular gap along the axial direction of the flue, so that the sealing assembly forms an elastic compression seal and a labyrinth flow obstruction path in the annular gap. S5. Construct a rounded corner at the junction of the bottom concrete curb and the flue, and lay an additional waterproof layer at the rounded corner.

10. The construction process of an adaptive flexible temperature-resistant sealing flue system based on a non-unloading tongue-and-groove joint according to claim 1, characterized in that: In step S4, when the sealing assembly is pressed in, the multiple flexible baffles of the sealing assembly form a reverse flow deflection fit along the flue gas escape direction, and the self-locking texture on the outer peripheral wall of the sealing assembly forms a backstop and limiting fit with the inner wall of the tongue and groove of the top floor slab; in step S5, the radius of the arc corner is constructed to be not less than 50mm.