An LDMOS device and its fabrication method
By constructing undulating epitaxial layers and doped regions in LDMOS devices and optimizing the electric field and doping distribution, the problem of increased on-resistance under high breakdown voltage was solved, achieving higher breakdown voltage and lower on-resistance, with good process compatibility.
Patent Information
- Application Number
- CN202611301843.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-26
- Publication Date
- 2026-11-17
AI Technical Summary
In pursuing higher breakdown voltages, existing LDMOS devices exhibit significantly increased characteristic on-resistance, leading to wasted chip area and increased manufacturing costs. Furthermore, conventional silicon-on-insulator substrates cannot optimize the lateral electric field distribution.
By forming grooves of different depths on the substrate and performing non-selective epitaxial growth, an undulating epitaxial layer is formed. Mask implantation is then performed within the epitaxial layer to form a doped region corresponding to the groove depth. Combined with chemical mechanical polishing and high-temperature annealing processes, a stepped buried oxide layer and doped region are constructed, optimizing the electric field and doping distribution.
Without increasing the lateral length of the device, the breakdown voltage is increased and the on-resistance is reduced, saving chip area, reducing manufacturing costs, and ensuring good compatibility with existing processes.
Smart Images

Figure CN123124379A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, and in particular to an LDMOS device and its fabrication method. Background Technology
[0002] Laterally diffused metal-oxide-semiconductor (LDMOS) is a type of power semiconductor device. Due to its high compatibility with complementary metal-oxide-semiconductor (CMOS) processes, ease of monolithic integration, and simple turn-on control, it has become a core component in the field of high-voltage power integrated circuits. In existing technologies, to further improve the electrical performance of these devices, a substrate structure with an insulating buried layer is typically used to fabricate LDMOS. This substrate structure can fully utilize the excellent isolation characteristics of the underlying insulating buried layer, improving the longitudinal breakdown voltage of the device and helping to reduce parasitic capacitance, thereby improving the switching speed of the device to some extent.
[0003] However, as high-voltage power integrated circuits continue to evolve towards higher voltage levels, smaller integration areas, and higher power densities, the existing traditional device structures based on silicon-on-insulator (SiS) substrates are gradually revealing their inherent limitations. On the other hand, the buried insulating layer in conventional SiS substrates is typically a flat and continuous planar structure. While this provides a basic vertical breakdown voltage, it cannot further modulate or optimize the lateral electric field distribution within the device. This physical limitation inevitably leads to a significant increase in characteristic on-resistance when pursuing higher breakdown voltages.
[0004] To compensate for the increased on-resistance, existing technologies often require increasing the lateral dimensions of devices, which not only directly leads to wasted chip area and increased manufacturing costs, but also severely restricts the improvement of the overall power density of power integrated circuits. Summary of the Invention
[0005] The main objective of this invention is to provide an LDMOS device and its fabrication method, which aims to improve the withstand voltage while reducing the on-resistance.
[0006] To achieve the above objectives, the present invention proposes a method for fabricating an LDMOS device, the method comprising:
[0007] A substrate is provided, the substrate including a first surface and a second surface disposed opposite to each other;
[0008] An oxide layer is formed on the first surface;
[0009] The buried oxide layer is etched using a mask to form multiple grooves of different depths. The groove with the largest depth is etched through the buried oxide layer to expose the substrate.
[0010] Non-selective epitaxial growth is performed on the exposed substrate to form an epitaxial layer covering the groove, the epitaxial layer having an undulating top surface morphology that varies with the depth of the groove;
[0011] Mask implantation is performed on the epitaxial layer to form doped regions within the epitaxial layer whose longitudinal positions correspond to the undulating top surface morphology.
[0012] In some embodiments of the present invention, the mask etching of the buried oxide layer includes: etching the buried oxide layer using a photoresist mask, performing photoresist thinning and retraction after etching and etching again, repeating the process to form multiple grooves with varying longitudinal depths.
[0013] In some embodiments of the present invention, the non-selective epitaxial growth of the exposed substrate includes: the temperature of the non-selective epitaxial growth process is 1000°C to 1200°C, and the gas source includes silicon source gas and chlorine source gas.
[0014] In some embodiments of the present invention, after forming doped regions of different depths in the epitaxial layer, the preparation method further includes: performing chemical mechanical polishing planarization on the epitaxial layer.
[0015] In some embodiments of the present invention, after performing chemical mechanical polishing planarization on the epitaxial layer, the preparation method further includes: injecting oxygen plasma into the second surface and performing a high-temperature annealing process to close the buried oxide layer in the region where the substrate is exposed.
[0016] In some embodiments of the present invention, the longitudinal cross-sectional profile formed by the plurality of grooves is centrally symmetrical in a stepped or sawtooth shape.
[0017] In some embodiments of the present invention, the fabrication method further includes forming a gate and a field plate covering the gate.
[0018] The present invention also discloses an LDMOS device, the LDMOS device comprising a substrate, a buried oxide layer and an epitaxial layer arranged sequentially from bottom to top, wherein the epitaxial layer has a doped region;
[0019] The buried oxide layer has steps of different depths on the side away from the substrate, and the epitaxial layer covers each of the steps;
[0020] The depth distribution of the doped region in the longitudinal section corresponds to the morphology of the step.
[0021] In some embodiments of the present invention, the longitudinal cross-sectional profile of the step is serrated or stepped.
[0022] In some embodiments of the present invention, the LDMOS device further includes a gate and a field plate located above the gate.
[0023] The technical solution of this invention utilizes a deeply undulating buried oxide layer structure, non-selective epitaxial lateral supergrowth, and mask implantation based on undulating morphology to achieve partitioned modulation of the electric field and spatial gradient distribution of doping within the device. Thick steps enhance longitudinal breakdown voltage, while thin steps smooth the lateral potential; simultaneously, the carrier conduction path is optimized by relying on doped regions that follow morphological changes. The fabrication process of this invention relies solely on photoresist retraction cycles and backside oxygen implantation to complete the core structure construction, exhibiting good compatibility with existing mainstream processes. It can simultaneously achieve an effective increase in breakdown voltage and a reduction in characteristic on-resistance without increasing the lateral length of the device, demonstrating significant industrial application value in saving chip area and reducing integrated circuit manufacturing costs. Attached Figure Description
[0024] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0025] Figure 1 This invention relates to a method for fabricating an LDMOS device.
[0026] Figures 2-10 This is a cross-sectional structural diagram of each step in the fabrication method of the LDMOS device of the present invention.
[0027] Figure 11 This is one of the schematic cross-sectional views of the LDMOS device of the present invention;
[0028] Figure 12 This is a second schematic cross-sectional view of the LDMOS device of the present invention;
[0029] Figure 13 This is the third schematic diagram of the cross-sectional structure of the LDMOS device of the present invention.
[0030] Figure label:
[0031] 100, Substrate; 200, Buried oxide layer; 300, Photoresist; 400, Epitaxial layer; 500, Doped region; 600, Gate; 700, Field plate;
[0032] The realization of the objective, functional features and advantages of the present invention will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0033] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0034] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative positional relationship and movement of each component in a certain specific posture (as shown in the figure). If the specific posture changes, the directional indication will also change accordingly.
[0035] Furthermore, the use of terms such as "first" and "second" in this invention is for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. Additionally, the technical solutions of the various embodiments can be combined with each other, but only on the basis of being achievable by those skilled in the art. When the combination of technical solutions is contradictory or impossible to implement, the user should consider such a combination of technical solutions to be non-existent and not within the scope of protection claimed by this invention.
[0036] See appendix Figure 1 This invention proposes a method for fabricating an LDMOS device, the method comprising:
[0037] S100: A substrate 100 is provided, the substrate 100 including a first surface and a second surface disposed opposite to each other;
[0038] S200: An oxide layer 200 is formed on the first surface;
[0039] S300: Mask etching is performed on the buried oxide layer 200 to form grooves of different depths. The groove with the largest depth is etched through the buried oxide layer 200 to expose the substrate 100.
[0040] S400: Non-selective epitaxial growth is performed on the exposed substrate 100 to form an epitaxial layer 400 covering the groove. The epitaxial layer 400 has a top surface morphology that varies with the depth of the groove.
[0041] S500: Mask implantation is performed on the epitaxial layer 400 to form a doped region 500 within the epitaxial layer 400, with a vertically distributed top surface morphology corresponding to the top surface undulation.
[0042] Understandably, this invention achieves zoned electric field modulation through the design of the stepped buried oxide layer 200. Thick steps enhance longitudinal breakdown voltage, while thin steps smooth the potential distribution, eliminating localized electric field concentration. Furthermore, the corresponding step morphology implantation based on the stepped epitaxial layer 400 makes the doping concentration distribution more reasonable in different regions, synergistically optimizing charge distribution. This solution improves breakdown voltage and reduces on-resistance without increasing the lateral length of the device, and has extremely high compatibility with existing process lines.
[0043] Below, in conjunction with the appendix Figures 2-10 The schematic cross-sectional structure of the LDMOS device shown in the diagram illustrates the fabrication process of this invention, providing a further detailed explanation of the fabrication method.
[0044] First, refer to the appendix Figure 2 Step S100 is performed, providing a substrate 100, which includes a first surface and a second surface disposed opposite to each other.
[0045] The substrate 100 can be made of any suitable substrate material known to those skilled in the art. This application uses a single-crystal silicon substrate 100 as an example for illustration. The first surface of the substrate 100 serves as the front side of the device and is used for subsequent thin film deposition and device fabrication; the second surface serves as the back side of the device and is used for subsequent thinning and back-side implantation processes.
[0046] Next, refer to Figure 3 Step S200 is performed to form a buried oxide layer 200 on the first surface.
[0047] First, the first surface of the substrate 100 is cleaned using conventional methods. Then, a buried oxide layer 200 is formed by thermal oxidation combined with wafer bonding, or by ion implantation combined with high-temperature annealing for oxygen implantation isolation. Optionally, the thickness of the initial buried oxide layer 200 can be controlled by adjusting the thermal oxidation time or the implantation dose.
[0048] Next, step S300 is performed to perform mask etching on the buried oxide layer 200 to form grooves of different depths. The groove with the largest depth is etched through the buried oxide layer 200 to expose the substrate 100.
[0049] See appendix Figures 4-6 This step involves multiple stages of cyclic etching operations. For details, refer to... Figure 4 First, a photoresist mask of 300 is coated on the surface of the buried oxide layer 200, and then exposed and developed to open the initial etching window. Next, refer to... Figure 5Dry etching is performed on the buried oxide layer 200 in the exposed area to a certain depth. After etching, oxygen plasma is used to isotropically thin and shrink the photoresist 300, thereby laterally expanding the opening window of the photoresist 300 and exposing the step edge formed by the previous etching. Subsequently, dry etching is performed again on the enlarged window area.
[0050] Preferably, the photoresist 300 thinning and re-etching process in this step is repeated multiple times, thereby forming multiple grooves with varying longitudinal depths within the buried oxide layer 200. Since the first window to open undergoes the most etching cycles, it has the greatest depth; the edge of the last opening undergoes the fewest etching cycles, thus having the shallowest depth. (Reference) Figure 6 During this cycle, the deepest groove needs to be etched through the entire buried oxide layer 200 so that the bottom monocrystalline silicon substrate 100 is exposed.
[0051] Optionally, the longitudinal cross-sectional profile of the formed groove is centrally symmetrical, either stepped or sawtooth. The sawtooth profile can further increase the diffusion path of the electric field at the interface when the subsequent device operates at high voltage, effectively reducing the electric field concentration phenomenon.
[0052] Next, see the appendix. Figure 7 Step S400 is executed to perform non-selective epitaxial growth on the exposed substrate 100 to form an epitaxial layer 400 covering the groove.
[0053] The etched wafer is placed in a chemical vapor deposition (CVD) reaction chamber, and a mixed gas containing silicon and chlorine source gases, such as dichlorosilane or trichlorosilane, and hydrogen chloride, is introduced. Preferably, the temperature inside the reaction chamber is controlled to be between 1000°C and 1200°C. The growth process begins in step S300 by exposing the bottom monocrystalline silicon region. Due to the difference in nucleation energy between the exposed bottom monocrystalline silicon window and the unetched area of the buried oxide layer 200 in silicon dioxide, silicon atoms preferentially nucleate on the monocrystalline silicon surface and grow upwards in a direction perpendicular to the surface of the substrate 100. To achieve lateral supergrowth of the covered groove, the concentration of the chlorine source gas in the mixed gas is controlled. By reducing the relative proportion of the chlorine source gas and combining it with a high-temperature environment, silicon atoms can obtain sufficient surface migration energy on the silicon dioxide surface. Under these process conditions, silicon atoms adsorbed on the stepped surface of the buried oxide layer 200 can overcome the nucleation barrier of the silicon dioxide surface and achieve lateral spreading on the silicon dioxide steps.
[0054] As the growth time increases, the laterally spread silicon epitaxial layer 400 and the vertically growing monocrystalline silicon epitaxial layer 400 at the window gradually merge, eventually covering the entire stepped groove.
[0055] It should be noted that since the growth of the epitaxial layer 400 is conformally covered along the physical morphology of the underlying buried oxide layer 200, the top surface of the grown epitaxial layer 400 exhibits an undulating top surface morphology that varies with the different depths of the bottom groove. This means that even if the same injection energy is used in subsequent steps, the physical penetration depth of doped impurities at different heights on the undulating surface will have a naturally corresponding spatial difference in the longitudinal direction.
[0056] Next, refer to Figure 8 In step S500, mask implantation is performed on the epitaxial layer 400 to form a doped region 500 within the epitaxial layer 400 whose vertical position distribution corresponds to the undulating top surface morphology.
[0057] A new photoresist mask 300 is coated on the undulating epitaxial layer 400, and a predetermined doping window region is opened. Subsequently, vertical doping is performed using an ion implanter with a single and uniform implantation energy.
[0058] Understandably, due to the undulations on the top surface of the epitaxial layer 400, the depth to which an ion beam of the same energy penetrates the epitaxial layer 400 at a higher step surface will necessarily differ from the absolute depth (i.e., the distance relative to the first surface of the substrate 100) it penetrates at a lower step surface. Therefore, through this mask implantation process, a doped region 500 with a vertical depth distribution that perfectly corresponds to the undulating morphology is ultimately formed within the epitaxial layer 400.
[0059] In this embodiment of the invention, the doped region 500 refers to the deep implanted region formed within epitaxial layers 400 of different thicknesses. It should be noted that this region can be specifically implemented as a deep N-type buried layer doped region 500 or a deep N-type drift region in conventional processes, depending on device performance requirements. However, the core of this invention lies not in the specific type of doping implantation, but in utilizing the stepped top surface of the epitaxial layer 400 to ensure that implanted impurities at the same implantation energy are necessarily at different depths in physical space. That is, the doped region 500 in the thick groove region is closer to the bottom, and the doped region 500 in the thin groove region is closer to the surface, thereby achieving a synergistically optimized distribution of electric field and charge in both the lateral and longitudinal directions.
[0060] For further details, please refer to the appendix. Figure 9 After forming the doped region 500, the preparation method also includes: performing chemical mechanical polishing planarization treatment on the epitaxial layer 400.
[0061] Chemical mechanical polishing (CMP) planarization is used to grind the front side of the doped epitaxial layer 400, removing surface irregularities and making the top surface of the epitaxial layer 400 nearly flat. Because the surface irregularities are smoothed out, the doped region 500 implanted in step S500 exhibits a gradient of absolute physical depth relative to the planarized device surface. This gradient depth, combined with the varying heights of the underlying buried oxide layer 200, allows for a more rational distribution of doping concentration across different regions.
[0062] For further details, please refer to the appendix. Figure 10 After completing the chemical mechanical polishing planarization process, the preparation method further includes: injecting oxygen plasma into the second surface and performing a high-temperature annealing process to close the buried oxide layer 200 in the area of the exposed substrate 100.
[0063] After planarization of the front side, the wafer is flipped. Preferably, the second surface of the wafer is first physically thinned to reduce the thickness of the silicon substrate that needs to be penetrated for subsequent energy implantation. Then, high-energy oxygen plasma is implanted from the back side with the second surface facing upwards. After implantation, a high-temperature annealing process is performed under inert gas protection. Driven by high temperature, the implanted oxygen ions combine with the silicon atoms at the bottom to form silicon dioxide. This causes the area in step S300 that etched through the buried oxide layer 200 and exposed the substrate 100 to be filled with newly generated silicon dioxide and insulated, thereby achieving physical and electrical closure of the buried oxide layer 200. Finally, the previously interconnected epitaxial layer 400 and the bottom substrate 100 are completely isolated by the complete stepped buried oxide layer 200, forming a silicon-on-insulator structure.
[0064] Furthermore, the fabrication method also includes forming a gate 600 and a field plate 700 covering the gate 600.
[0065] On the planarized front side of the device, a gate 600 is formed using conventional gate oxide growth, polysilicon deposition, and etching processes. A dielectric layer is then deposited above the gate 600, and a field plate 700 is formed through metal deposition and patterning processes. Preferably, the field plate 700 covers the gate 600, and its vertical position corresponds to the thicker step in the buried oxide layer 200. The combined synergistic voltage-dividing effect of the field plate 700 and the thick buried oxide layer 200 further disperses the electric field spikes in the off-state, ensuring the device's reliability under extremely high withstand voltages.
[0066] See appendix Figures 11-13 The present invention also discloses an LDMOS device, which includes a substrate 100, a buried oxide layer 200 and an epitaxial layer 400 arranged sequentially from bottom to top, and the epitaxial layer 400 has a doped region 500.
[0067] The buried oxide layer 200 has steps of different depths on the side away from the substrate 100, and the epitaxial layer 400 covers each step;
[0068] The depth distribution of the doped region 500 in the longitudinal section corresponds to the morphology of the step.
[0069] In this embodiment, the alternating thick and thin stepped buried oxide layer 200 design enables the regional modulation of the internal electric field of the device. The thicker stepped regions of the buried oxide layer 200 can enhance the longitudinal breakdown voltage of the device and effectively disperse the peak value of the interface electric field; the thinner stepped regions of the buried oxide layer 200 can smooth the lateral potential distribution, which helps to improve the breakdown voltage of the device; and through the synergy of gradient doping process and stepped structure, the physical burial depth distribution of the doped region 500 in the longitudinal direction is more reasonable, further optimizing the macroscopic charge distribution and reducing the on-resistance of the device.
[0070] Optionally, see Figure 11 and 12 The longitudinal cross-sectional profile of the step is centrally symmetrical, with a sawtooth or stepped shape. The sawtooth profile can further increase the diffusion path of the electric field at the interface when the subsequent device is operating at high voltage, effectively reducing the electric field concentration phenomenon.
[0071] Additionally, see Figure 13 The LDMOS device in this embodiment also includes a gate 600 and a field plate 700 located above the gate 600. Optionally, the field plate 700 corresponds vertically to the thicker step in the buried oxide layer 200. The field plate 700 and the thick buried oxide layer 200 can work together to form a multi-level electric field voltage reduction structure, further weakening the electric field spikes in the off state, thereby providing structural protection for improving the breakdown voltage.
[0072] In summary, in this embodiment of the invention, a stepped buried oxide layer 200 of different depths is constructed on a single-crystal silicon substrate 100 through silicon dioxide etching and non-selective epitaxial growth. The multiple right-angled ends of the stepped buried oxide layer 200 disperse and guide the electric field peak that was originally concentrated in one place, thereby avoiding excessive concentration of charge at the edge of the gate 600 and improving the device breakdown voltage. Simultaneously, the stepped structure better increases the conduction paths of charge carriers in both the lateral and longitudinal directions, resulting in a more uniform charge carrier distribution and optimizing the electric field distribution inside the device.
[0073] Furthermore, mask implantation is performed on the surface of the epitaxial layer 400 with its undulating top surface, thereby forming a gradient doped region 500 within the epitaxial layer 400 corresponding to the stepped undulation. It is particularly important to emphasize that the "gradient" here essentially reflects the spatial difference in the physical burial depth of the doped region 500. After penetration onto different undulating top surfaces using the same implantation energy, the subsequent chemical mechanical polishing process completely smooths the top surface of the epitaxial layer 400, ultimately resulting in a stepped distribution of the absolute depth of the doped region 500 from the flat surface. This gradient doping in vertical depth forms a physical synergy with the underlying stepped buried oxide layer 200: the doped region 500 above the thicker buried oxide layer 200 is relatively shallow, while the doped region 500 above the thinner buried oxide layer 200 is relatively deep. This precisely matches the zonal modulation of the electric field by the underlying buried oxide layer 200, allowing the depletion region to expand more smoothly and reasonably when the device is subjected to high voltage. By leveraging the deep synergy between the doping depth distribution and the stepped structure, the device achieves a significant optimization of charge distribution without increasing the lateral dimension, resulting in an effective increase in breakdown voltage and a significant reduction in characteristic on-resistance. Furthermore, it exhibits good process compatibility and is easy to mass-produce.
[0074] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
Claims
1. A method for fabricating an LDMOS device, characterized in that, The preparation method includes: A substrate is provided, the substrate including a first surface and a second surface disposed opposite to each other; An oxide layer is formed on the first surface; The buried oxide layer is etched using a mask to form multiple grooves of different depths. The groove with the largest depth is etched through the buried oxide layer to expose the substrate. Non-selective epitaxial growth is performed on the exposed substrate to form an epitaxial layer covering the groove, the epitaxial layer having an undulating top surface morphology that varies with the depth of the groove; Mask implantation is performed on the epitaxial layer to form doped regions within the epitaxial layer whose longitudinal positions correspond to the undulating top surface morphology; The longitudinal cross-sectional profile formed by the multiple grooves is centrally symmetrical, either stepped or serrated.
2. The method for fabricating an LDMOS device as described in claim 1, characterized in that, The mask etching of the buried oxide layer includes: etching the buried oxide layer using a photoresist mask, performing photoresist thinning and retraction after etching, and repeating the process to form multiple grooves with varying longitudinal depths.
3. The method for fabricating an LDMOS device as described in claim 1, characterized in that, The non-selective epitaxial growth of the exposed substrate includes: the temperature of the non-selective epitaxial growth process is 1000℃~1200℃, and the gas source includes silicon source gas and chlorine source gas.
4. The method for fabricating an LDMOS device according to any one of claims 1-3, characterized in that, After forming doped regions of different depths within the epitaxial layer, the preparation method further includes performing a chemical mechanical polishing planarization treatment on the epitaxial layer.
5. The method for fabricating an LDMOS device as described in claim 4, characterized in that, After performing chemical mechanical polishing planarization on the epitaxial layer, the preparation method further includes: injecting oxygen plasma into the second surface and performing a high-temperature annealing process to close the buried oxide layer in the area where the substrate is exposed.
6. The method for fabricating an LDMOS device according to any one of claims 1-3, characterized in that, The fabrication method further includes forming a gate and a field plate covering the gate.
7. An LDMOS device, characterized in that, The LDMOS device includes a substrate, a buried oxide layer, and an epitaxial layer arranged sequentially from bottom to top, and the epitaxial layer has a doped region. The buried oxide layer has steps of different depths on the side away from the substrate, and the epitaxial layer covers each of the steps; The depth distribution of the doped region in the longitudinal section corresponds to the morphology of the step; The longitudinal cross-sectional profile formed by the multiple grooves is centrally symmetrical, either stepped or serrated.
8. The LDMOS device as described in claim 7, characterized in that, The LDMOS device also includes a gate and a field plate located above the gate.