A stepped-doped superjunction trench gate SiC MOSFET device with a P-shielding layer and its fabrication method thereof.
By setting a locally high-concentration P-type shielding layer at the top of the P-type pillar region, the problem of easy breakdown of the gate oxide layer in traditional devices in high-frequency applications is solved, and optimization of high withstand voltage, low loss and long-term reliability is achieved.
Patent Information
- Application Number
- CN202611205487.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-10
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional trench-gate SiC MOSFET devices struggle to balance high voltage withstand and low conduction loss, exhibiting significant gate oxide reliability issues. In particular, the gate oxide layer is susceptible to early breakdown due to concentrated electric field in high-frequency applications.
A stepped-doped superjunction trench gate SiC MOSFET device with a P-type shielding layer is adopted. By setting a local high-concentration P-type shielding layer at the top of the P-type pillar region and short-circuiting it with the source metal, an electrostatic shielding effect is formed, reducing the electric field peak of the gate oxide layer. Furthermore, the electric field and capacitive coupling are optimized through the vertical stepped doping distribution.
It achieves a combination of high breakdown voltage, low on-resistance, and low switching loss, improving the static and dynamic characteristics of the device, ensuring the long-term reliability of the gate oxide layer, and has good process compatibility, making it easy to mass-produce.
Smart Images

Figure CN123124404A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of power semiconductor device technology, and in particular to a stepped-doped superjunction trench gate SiC MOSFET device with a P-shielding layer and its fabrication method. Background Technology
[0002] In the field of power electronics technology, the efficient conversion of high-frequency, high-voltage, and high-power electrical energy is a core research topic that continues to be tackled. Emerging applications, such as electric vehicle main inverters and renewable energy grid connection, place stringent demands on the voltage withstand capability, switching losses, and long-term reliability of power devices. Traditional silicon-based devices are unable to meet these requirements due to physical limitations. Wide-bandgap semiconductor silicon carbide (SiC) has become an ideal choice due to its advantages such as high critical breakdown electric field and high thermal conductivity. Among them, trench-gate SiC MOSFETs (Metal-Oxide-Semiconductor Field Effect Transistors) have become the mainstream technology for 1200V high-voltage switching due to their high channel density and low on-resistance.
[0003] Traditional trench-gate SiC MOSFET structures struggle to balance high breakdown voltage with low conduction losses. The inherent trade-off between breakdown voltage and specific on-resistance is constrained by the "silicon limit." The trench gate structure also results in high gate-drain capacitance and significant switching losses, limiting high-frequency applications. The core issue with gate oxide reliability in trench-gate SiC MOSFETs lies in the electric field concentration at the bottom corner of the trench. The difference in dielectric constant between SiC and SiO2 causes the gate oxide electric field to be more than 2.5 times that of the bulk material, easily leading to premature gate oxide breakdown. Industry requirements dictate that the peak gate oxide electric field be below 3 MV / cm, a standard often exceeded by traditional structures. To overcome this static trade-off, superjunction technology has been introduced into SiC MOSFETs. Through the charge balance effect of P / N pillars, the longitudinal electric field is transformed from a triangle to a quasi-rectangular shape, significantly increasing the doping concentration in the drift region. Uniformly doped superjunctions can increase the breakdown voltage by 21% and reduce the specific on-resistance by more than 75%, but the dynamic loss and gate oxide reliability of uniformly doped superjunctions have not been improved: the gate-drain capacitance remains high due to the high doping of P / N pillars, and the problem of electric field concentration at the bottom of the trench is still prominent.
[0004] Patent CN114927559A discloses a novel silicon carbide-based superjunction trench MOSFET and its fabrication method. The MOSFETs incorporate three p+ pillar regions and two n+ pillar regions beneath the p-type shielding layer and p-body region of the trench, forming a semi-superjunction structure. During forward conduction, current flows downward along the n-pillar regions. The presence of the n-pillar regions increases the carrier concentration in the current path, resulting in better forward conduction characteristics. During reverse blocking, the superjunction structure achieves basic charge balance, forming a near-intrinsic semiconductor with higher breakdown voltage. Furthermore, in localized regions, the triangular electric field transforms into a trapezoidal electric field. Under the same avalanche electric field, the breakdown voltage is higher than that of conventional structures. Therefore, this structure alleviates the electric field congestion effect at the corners of the p-type shielding layer, while simultaneously increasing the on-state current and reducing the on-state resistance. However, this scheme uses a P-type shielding layer structure at the bottom of the trench. On the one hand, it will form a JFET clamping effect on the N-type carrier path in the on-state, introducing additional on-resistance and partially offsetting the low resistance advantage of the superjunction. On the other hand, the shielding layer needs to be fabricated separately after the trench is etched, which has poor compatibility with the fabrication process of the superjunction pillar region. Summary of the Invention
[0005] The purpose of this invention is to provide a stepped-doped superjunction trench gate SiC MOSFET device with a P-shielding layer and its fabrication method, thereby achieving superior overall performance in terms of static, dynamic, and long-term reliability.
[0006] The objective of this invention can be achieved through the following technical solution: a stepped-doped superjunction trench gate SiC MOSFET device (SSD-SJ) with a P-shield, the cell structure of which includes: a trench gate region, a source metal, an N+ source region, a P-type base region, a P-type shielding layer, an N+ substrate, and a drain metal. Below the P-type base region is a stepped-doped superjunction P / N pillar drift region, which includes a P-type pillar region and an N-type pillar region. The trench gate region is in contact with the N+ type source region and the P type base region, and extends into the N type pillar region; The P-type shielding layer is located above the P-type column region and is connected to the source metal potential.
[0007] In this invention, the P-type shielding layer is short-circuited to the source metal, serving as a longitudinal extension of the source potential. Under the reverse blocking state, it forms a strong electrostatic shielding effect, thereby creating an electrostatic shielding structure for the gate oxide layer at the bottom of the trench gate region.
[0008] In this invention, the localized P-type shielding layer is located at the top of the P-type pillar region rather than at the bottom of the trench. In the reverse blocking state, this P-type shielding layer extends the source potential longitudinally into the device, forming a strong electrostatic shielding field: the high-voltage electric field lines from the drain are captured and deflected into the silicon carbide bulk material by the P-type shielding layer region before reaching the gate oxide layer at the bottom of the trench, thereby suppressing the gate oxide peak electric field below the long-term reliability safety threshold. Simultaneously, since the P-type shielding layer is located at the top of the P-type pillar region and does not occupy space at the bottom of the trench, it does not introduce additional JFET resistance in the on-state, thus fully preserving the low on-resistance advantage of the superjunction structure.
[0009] Preferably, the stepped-doped superjunction P / N pillar drift region includes alternating P-type pillar regions and N-type pillar regions, which extend along the longitudinal direction of the device, and the doping concentration of the two is distributed in a stepped non-uniform manner in the longitudinal direction, specifically with low doping at the top, medium doping in the middle, and high doping at the bottom.
[0010] In this invention, the doping concentration distribution of the P-type column region is symmetrical to that of the N-type column region.
[0011] In this invention, the longitudinal stepped doping distribution of the stepped-doped superjunction P / N pillar drift region is achieved by segmentally controlling the doping concentration of the P / N pillars, while maintaining a constant total charge. The top low-doped region widens the depletion layer width of the gate-drain overlap region, weakening the capacitive coupling between the gate and drain, thereby reducing reverse transfer capacitance and gate-drain charge; the middle high-doped region maintains a low-resistance conduction path; and the bottom high-doped region compensates for the charge loss caused by the top low-doping region. Through this design, the static and dynamic characteristics of the device are decoupled and optimized.
[0012] More preferably, the P-type pillar region includes a top low-doped P-pillar region, a middle uniformly doped P-pillar region, and a bottom high-doped P-pillar region arranged sequentially from top to bottom; The top low-doped P-pillar region is provided with a P-type shielding layer, and the bottom high-doped P-pillar region is provided with an N+ type substrate.
[0013] More preferably, the N-type pillar region includes a top low-doped N-pillar region, a middle uniformly doped N-pillar region, and a bottom high-doped N-pillar region arranged sequentially from top to bottom; The trench gate region extends into the top low-doped N-pillar region, and the bottom high-doped N-pillar region has an N+ type substrate at its bottom.
[0014] In this invention, the doping concentration of the top low-doped region of the N-type pillar region and the middle medium-doped region is lower than that of the middle medium-doped region, and the doping concentration of the bottom high-doped region is higher than that of the middle medium-doped region. In addition, the total vertical charge is equal to that of the uniformly doped superjunction to ensure overall charge balance.
[0015] Preferably, the P-type shielding layer and the trench gate region have an intersection in the longitudinal direction and are spaced apart in the lateral direction.
[0016] Preferably, the P-type shielding layer is located near the bottom region of the trench gate region and at the top of the P-pillar, with a longitudinal depth of 0.8~1.2 μm; in the transverse direction, a gap of 0.08~0.12 μm is maintained between the sidewall of the P-type shielding layer near the trench gate region and the sidewall of the trench gate region.
[0017] More preferably, the longitudinal depth of the P-type shielding layer is 1.0 μm, and in the transverse direction, a 0.1 μm gap is maintained between the sidewall of the P-type shielding layer near the trench gate region and the sidewall of the trench gate region.
[0018] Preferably, the depth of the P-type shielding layer is set such that it can cover the bottom corner region of the trench gate region, and the peak doping concentration is higher than the top doping concentration of the P-type pillar region.
[0019] More preferably, the doping concentration of the P-type shielding layer is (1.4~1.5)×10⁻⁶. 17 cm -3 The top doping concentration of the P-type column region is (6~8)×10 16 cm -3 .
[0020] In this invention, the P-type shielding layer is a locally high-concentration P-type shielding layer located at the top of the P-pillar region near the bottom of the trench gate region.
[0021] Preferably, the P-type shielding layer is formed by high-dose aluminum ion implantation.
[0022] Preferably, the trench gate region includes a polysilicon gate electrode and a gate oxide layer disposed around the polysilicon gate electrode.
[0023] More preferably, the gate electrode is heavily doped polycrystalline silicon.
[0024] More preferably, the gate oxide layer is silicon dioxide.
[0025] More preferably, the gate oxide layer has a thickness of 30~50nm to balance the requirements of threshold voltage, channel resistance and gate oxide electric field suppression.
[0026] Preferably, the source metal and drain metal are Al alloys, and the N+ type substrate is N-type 4H-SiC.
[0027] Preferably, the trench gate region is located below the source metal.
[0028] Preferably, the N+ type source region is surrounded by a source metal above, a P-type base phase below, and a P+ contact region on the outside.
[0029] Preferably, the N+ type substrate has a stepped-doped superjunction P / N pillar drift region above it and a drain metal below it, with the drain metal in contact with the N+ type substrate.
[0030] Preferably, the semiconductor material of the device is 4H-SiC, and all parts use the same material system.
[0031] A method for fabricating the above-mentioned stepped-doped superjunction trench gate SiC MOSFET device with a P-shielding layer includes the following steps: N-type drift regions were epitaxially grown multiple times on an N+ 4H-SiC substrate. During the multiple epitaxial growth cycles, the doping concentration of each N-type epitaxial layer was adjusted sequentially to form a vertically stepped distribution with low doping at the top, medium doping in the middle, and high doping at the bottom. After each epitaxial growth cycle, P-pillars were formed by ion implantation. During the multiple epitaxial growth cycles, the doping concentration of each P-type epitaxial layer was adjusted sequentially to form a vertically stepped distribution with low doping at the top, medium doping in the middle, and high doping at the bottom. In the last few cycles, an additional high-dose ion implantation was performed to form a local P-type shielding layer at the top of the P-pillars. After all epitaxy and implantation were completed, high-temperature activation annealing was performed. Trenching was etched to form trenches and sacrificial oxidation was performed. A silicon dioxide gate oxide layer was thermally grown and nitrided and annealed. Polysilicon was deposited and etched back to form the gate electrode. Interlayer dielectric was deposited and contact holes were etched. Metal was sputtered and annealed to form ohmic contacts.
[0032] To further optimize dynamic performance, the Step-Doped Superjunction SiCMOSFET (SD-SJ) utilizes a vertically non-uniform distribution of low doping at the top and high doping at the bottom to widen the depletion layer in the gate-drain overlap region, significantly reducing reverse transfer capacitance and gate-drain charge. However, the low doping at the top weakens the electrostatic shielding of the gate oxide layer, causing the peak gate oxide electric field to rise to 6.8 MV / cm, severely threatening device reliability. Existing gate oxide protection schemes (such as a P-type shielding layer at the bottom of the trench, dual trenches, etc.) often introduce additional JFET resistors, increase process complexity, and have poor compatibility with multi-epitaxy processes for superjunctions.
[0033] To address the aforementioned issues, this invention proposes a shielded step-doped superjunction SiC MOSFET (SSD-SJ) with a P-shielding layer. Its innovation lies in the high-concentration P-type shielding layer placed at the top of the P-pillars, near the bottom of the trench, serving as a vertical extension of the source potential and forming a strong electrostatic shield in the reverse blocking state, suppressing the peak gate oxide electric field to below 3 MV / cm. Simultaneously, this shielding layer is located at the top of the P-pillars rather than the bottom of the trench, thus not introducing JFET resistance. SSD-SJ can be achieved through multiple epitaxial growth steps followed by selective ion implantation, requiring only a high-dose step in the last 1-2 implantations, resulting in high process compatibility. This structure achieves three-dimensional synergistic optimization of static performance, dynamic loss, and gate oxide reliability.
[0034] In this invention, a stepped-doped superjunction and a localized P-type shielding layer work together: the low-doped top region of the stepped doping widens the depletion layer, providing a more favorable electric field modulation space for the P-type shielding layer, enabling the shielding layer to achieve effective electric field deflection with appropriate doping concentration and depth; simultaneously, the P-type shielding layer compensates for the risk of increased gate oxide electric field caused by the low doping at the top of the stepped doping layer. The synergistic effect of these two components simultaneously optimizes the device in terms of breakdown voltage, on-resistance, switching loss, and gate oxide reliability.
[0035] Compared with the prior art, the present invention has the following technical advantages: 1. In this invention, the stepped-doped superjunction and the localized P-type shielding layer work synergistically. The low-doped region at the top of the stepped-doped layer provides a more favorable electric field shielding environment for the P-type shielding layer, while the P-type shielding layer compensates for the risk of increased gate oxide electric field caused by stepped doping. Together, they enable the device to maintain high breakdown voltage and low on-resistance while keeping the peak gate oxide electric field within a safe range, and further reducing reverse transfer capacitance, achieving three-dimensional synergistic optimization of static performance, dynamic loss, and long-term reliability.
[0036] 2. Compared with traditional uniformly doped superjunction trench gate SiC MOSFETs, this invention introduces a vertical three-segment stepped doping distribution (low doping at the top, medium doping in the middle, and high doping at the bottom) in the N-type drift region. Without disrupting the superjunction charge balance, the low-doped top region widens the depletion layer width of the gate-drain overlap region, effectively weakening the capacitive coupling effect between the gate and drain. Thus, without sacrificing the breakdown voltage and specific on-resistance, the reverse transfer capacitance is significantly reduced, achieving decoupling optimization of static and dynamic characteristics.
[0037] 3. This invention utilizes a vertically non-uniform P / N pillar design with low top doping and high bottom doping to adaptively control the width of the depletion layer and the electric field distribution in the drift region while maintaining the superjunction charge balance and high breakdown voltage: the depletion layer naturally widens under low current and off-state conditions, effectively reducing gate-drain capacitance and dynamic losses; the high-doped region at the bottom maintains low on-resistance during high current conduction; and the depletion layer rapidly recovers and expands as the current density decreases during off-state. This adaptive carrier control achieves synergistic optimization of conduction characteristics and switching losses, overcoming the bottleneck of traditional uniform superjunctions where static and dynamic performance are difficult to balance.
[0038] 4. This invention employs a locally high-concentration P-type shielding layer at the top of the P-pillar, near the bottom of the trench, and short-circuit this shielding layer to the source metal, making it a longitudinal extension of the source potential. In the reverse blocking state, this shielding layer forms a strong electrostatic shielding field, capturing and deflecting the high-voltage electric field from the drain into the SiC bulk material before it reaches the gate oxide layer at the bottom of the trench, thereby suppressing the gate oxide peak electric field below the long-term reliability safety threshold. Compared with the traditional trench-bottom P-type shielding layer scheme, the P-type shielding layer in this invention is located at the top of the P-pillar rather than at the bottom of the trench, thus not occupying the trench bottom space and not introducing additional JFET resistance in the on-state. Therefore, while improving gate oxide reliability, it fully retains the low on-resistance advantage of the superjunction structure.
[0039] 5. The structure described in this invention is based on a process route combining multiple epitaxial growth and selective ion implantation, and is fully compatible with existing SiC superjunction device manufacturing platforms. The formation of the P-type shielding layer only requires adding a high-dose Al implantation in the last 1-2 epitaxial implantation cycles, without adding any additional core process steps; at the same time, this structure has good process tolerance to doping concentration deviations, and can still meet the breakdown voltage design target within the typical process deviation range, making it easy to engineer for mass production.
[0040] 6. The present invention can overcome the defects of trench gate SiC MOSFETs in the prior art, such as the inherent trade-off between specific on-resistance and breakdown voltage, high dynamic loss, and insufficient reliability caused by the electric field concentration of the gate oxide layer at the bottom of the trench, and obtain better overall static-dynamic-long-term reliability performance.
[0041] 7. This invention, through the synergistic design of a longitudinally stepped doped superjunction structure and local shielding at the top of the P-pillar, avoids the inherent shortcomings of traditional bottom shielding, such as compressing the carrier flow path and introducing additional on-resistance, compared to the bottom P-type shielding scheme of trenches. It can control the gate oxide electric field within a long-term reliable and safe range, and achieve a more balanced and comprehensive performance improvement in terms of conduction capability and device stability.
[0042] 8. This invention integrates the P-type shielding layer on the top of the P-pillar, without occupying the bottom space of the trench, without introducing additional JFET resistors, and is compatible with superjunction epitaxial implantation process. Attached Figure Description
[0043] Figure 1 This is a schematic diagram of the cell structure of a stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer according to the present invention.
[0044] Figure 2 This is a comparison of the blocking characteristic curves of the stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer of the present invention with those of UD-SJ and SD-SJ.
[0045] Figure 3 This is a comparison of the output characteristic curves of the stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer of the present invention with those of UD-SJ and SD-SJ.
[0046] Figure 4 This is a comparison of the capacitance characteristic curves of a stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer according to the present invention, and those of UD-SJ and SD-SJ.
[0047] Figure 5 This is a comparison diagram of the electric field distribution at the gate oxide of a stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer according to the present invention, and UD-SJ and SD-SJ.
[0048] In the figure: 1-Source metal, 2-Gate electrode, 3-Gate oxide layer, 4-P+ contact region, 5-N+ type source region, 6-P type base region, 7-P type shielding layer, 8-Top low-doped P-pillar region, 9-Middle uniformly doped P-pillar region, 10-Bottom high-doped P-pillar region, 11-N+ type substrate, 12-Drain metal, 13-Top low-doped N-pillar region, 14-Middle uniformly doped N-pillar region, 15-Bottom high-doped N-pillar region. Detailed Implementation
[0049] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments. These embodiments are based on the technical solution of the present invention and provide detailed implementation methods and specific operating procedures. However, the scope of protection of the present invention is not limited to the following embodiments.
[0050] like Figure 1As shown, the present invention provides a stepped-doped superjunction trench gate SiC MOSFET device (SSD-SJ) with a P-shielding layer. Its cell structure includes: a gate region, a source metal 1, an N+ type source region 5, a P+ contact region 4, a P-type base region 6, a stepped-doped superjunction P / N pillar drift region below the P-type base region 6, a locally high-concentration P-type shielding layer 7 at the top of the P pillar near the bottom of the trench, an N+ type substrate 11 below the stepped-doped superjunction, and a drain metal 12 in contact with the N+ type substrate 11.
[0051] The gate region is a trench gate structure. The trench gate region is in contact with the N+ type source region 5 and the P type base region 6, and extends into the N type pillar region of the stepped doped superjunction. The local P type shielding layer 7 is located at the top of the P pillar and is connected to the potential of the source metal 1, forming an electrostatic shielding structure for the gate oxide at the bottom of the trench.
[0052] The superjunction structure consists of alternating N-type and P-type pillar regions, extending longitudinally from below the P-type base region 6 to near the N+ substrate 11. The doping concentration of the N- and P-pillars exhibits a stepped, non-uniform distribution longitudinally, specifically a low-doped region at the top, a medium-doped region in the middle, and a high-doped region at the bottom. The N- and P-pillars have equal widths, forming a strict charge balance geometry. The low-doped region at the top widens the depletion layer width of the gate-drain overlap region, weakening the capacitive coupling between the gate and drain, and reducing reverse transfer capacitance and gate-drain charge. A higher doping concentration is maintained in the middle to ensure low resistance characteristics of the vertical conduction path, while the high-doped region at the bottom compensates for the longitudinal charge loss caused by the low doping at the top, maintaining overall charge balance.
[0053] A locally high-concentration P-type shielding layer 7 is provided at the top of the P-pillar and near the bottom of the trench. This P-type shielding layer 7 is short-circuited to the source metal 1, serving as a longitudinal extension of the source potential. The longitudinal depth of the P-type shielding layer 7 is such that it can cover the corner area at the bottom of the trench, and its doping concentration is significantly higher than that at the top of the P-pillar.
[0054] Specifically, the trench gate region extends deep into the N-type pillar region, with its bottom located within the top low-doped region of the superjunction structure. In reverse blocking mode, a high voltage is applied to the drain, and the P-type shielding layer 7 is at the same potential as the source, forming a strong electrostatic shielding field. According to Gauss's law for electrostatic fields, electric field lines are always perpendicular to the equipotential surface. Since the potential of the P-type shielding layer 7 is clamped at the low potential of the source, the high-voltage electric field lines from the drain are attracted to the P-type shielding layer 7 region before reaching the gate oxide interface at the bottom of the trench, and flow along the P-pillars towards the source. This mechanism significantly weakens the electric field peak that was originally concentrated at the corner of the bottom of the trench and transfers it into the SiC bulk material, thereby suppressing the electric field strength borne by the gate oxide layer below the long-term reliability safety threshold. Meanwhile, since the P-type shielding layer 7 is located at the top of the P-pillar rather than the bottom of the trench, in the forward conduction state, after electrons enter the N-type drift region from the N+ source region 5 through the inversion channel, they are mainly transported downward along the N-pillar. The P-type shielding layer 7 does not occupy the main flow path of the charge carriers, so no additional JFET resistance is introduced, and the low on-resistance advantage of the superjunction structure is fully preserved.
[0055] Specifically, the stepped-doped superjunction and the localized P-type shielding layer 7 work together to form a multi-dimensional synergistic electric field modulation mechanism. The low-doped top region of the stepped doping allows the depletion layer to be fully extended in both the vertical and horizontal directions, providing a more favorable electric field deflection space for the P-type shielding layer 7; while the P-type shielding layer 7 compensates for the risk of increased gate oxide electric field that may be caused by the low-doping top region of the stepped doping by actively capturing electric field lines. The synergistic effect of the two optimizes the device simultaneously in terms of breakdown voltage, on-resistance, switching loss, and gate oxide reliability.
[0056] Specifically, the gate oxide layer 3 is made of silicon dioxide. The polycrystalline silicon gate electrode 2 is n-type doped. The P-type base region 6 is a P-type region formed by aluminum ion implantation. The N+ source region 5 is a heavily doped region formed by nitrogen or phosphorus ion implantation. The N+ substrate 11 is made of 4H-silicon carbide. The source metal 1 and drain metal 12 are nickel / aluminum / titanium alloys.
[0057] Specifically, the back and front structures of the SSD-SJ device are not strictly aligned. The area directly above the local P-type shielding layer 7 can be the gate oxide layer at the bottom of the trench or the top area of the P-pillar. This non-aligned design reduces the alignment accuracy requirements of the photolithography process and improves the manufacturing yield.
[0058] Specifically, the semiconductor material of the SSD-SJ device is 4H-silicon carbide, and all parts use the same material system to ensure lattice matching and consistent thermal expansion coefficient.
[0059] Specifically, one method for fabricating the SSD-SJ device includes the following steps: epitaxially growing an N-type drift region multiple times on an N+ 4H-SiC substrate; forming a P-pillar by ion implantation after each epitaxy, and successively adjusting the implantation dose to achieve a vertical stepped distribution of the P-pillar doping concentration; performing an additional high-dose ion implantation in the last few cycles to form a local P-type shielding layer at the top of the P-pillar; performing high-temperature activation annealing after completing all epitaxy and implantation; etching to form trenches and performing sacrificial oxidation treatment; thermally growing a silicon dioxide gate oxide layer and performing nitriding annealing; depositing polysilicon and etching back to form the gate electrode; depositing interlayer dielectric and etching contact holes; sputtering metal and annealing to form ohmic contacts.
[0060] The following detailed description is provided with reference to specific embodiments: Example 1 A stepped-doped superjunction (SSD-SJ) trench-gate SiC MOSFET device with an integrated P-shielding layer, wherein the device has a cell pitch of 2 μm, a thickness of 12 μm, a drift region thickness of 11 μm, and a polysilicon gate electrode 2 of 1e20 cm. -3 The structure is N-type phosphorus ion doped, with a trench gate region depth of 0.8 μm, a gate oxide layer thickness of 40 nm, and a P-type base region doping concentration of 5e17cm. -3 The doping concentration of N+ source region 5 is 1e20 cm⁻¹ -3 The local high-concentration P-type shielding layer has a doping concentration of 1.45e17 cm⁻¹. -3 The top low-doped P / N pillar region has a doping concentration of 7e17 cm⁻¹. -3 The doping concentration of the uniformly doped P / N pillar region 9 / 14 in the middle is 9.5e16cm. -3 The doping concentration of the highly doped P / N pillar region at the bottom is 1.2e17 cm⁻¹. -3 .
[0061] In this embodiment, the P-type dopants are all aluminum, the N-type dopants are all nitrogen, the device material is all silicon carbide, and the dielectric layer is all silicon dioxide.
[0062] Comparative Example 1 A UD-SJ device is described, wherein the cell spacing is 2 μm, the thickness is 12 μm, the drift region thickness is 11 μm, and the polysilicon gate electrode 2 is 1e20 cm. -3 The structure is N-type phosphorus ion doped, with a trench gate region depth of 0.8 μm, a gate oxide layer thickness of 40 nm, and a P-type base region doping concentration of 5e17 cm⁻¹. -3 The doping concentration of N+ source region 5 is 1e20 cm⁻¹ -3The difference between it and the stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer of the present invention is that the UD-SJ does not have the locally high-concentration P-type shielding layer 7, the top low-doped P / N pillar region 8 / 13, the middle uniformly doped P / N pillar region 9 / 14, and the bottom high-doped P / N pillar region 10 / 15.
[0063] Comparative Example 2 An SD-SJ device is provided, wherein the cell spacing is 2 μm, the thickness is 12 μm, the drift region thickness is 11 μm, and the polysilicon gate electrode 2 is 1e20 cm. -3 The structure is N-type phosphorus ion doped, with a trench gate region depth of 0.8 μm, a gate oxide layer thickness of 40 nm, and a P-type base region doping concentration of 5e17 cm⁻¹. -3 The doping concentration of N+ source region 5 is 1e20 cm⁻¹ -3 The top low-doped P / N pillar region has a doping concentration of 7e17 cm⁻¹. -3 The doping concentration of the uniformly doped P / N pillar region 9 / 14 in the middle is 9.5e16 cm⁻¹. -3 The doping concentration of the highly doped P / N pillar region at the bottom is 1.2e17 cm⁻¹. -3 The difference between it and the stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with an integrated P-shielding layer of the present invention is that the SD-SJ does not have a locally high-concentration P-type shielding layer 7.
[0064] To verify the beneficial effects of the present invention, the following simulation comparison of Embodiment 1, Comparative Example 1, and Comparative Example 2 of the present invention was conducted using Sentaurus TCAD software. The performance results are as follows: Figures 2-5 As shown in Table 1.
[0065] Table 1 As shown in Table 1, the forward blocking voltages of Example 1, Comparative Example 1, and Comparative Example 2 are 1670 V, 1703 V, and 1703 V, respectively. When the voltage continues to increase, the device undergoes avalanche breakdown. The SSD-SJ drops slightly to 1670 V due to the local charge mismatch introduced by the P-shield layer. Figure 3 The output characteristics of the three devices are shown. The on-resistances of Example 1, Comparative Examples 1 and 2 are 0.84 mΩ·cm. 2 0.83 mΩ·cm 2 and 0.83 mΩ·cm 2 .
[0066] In terms of reverse transfer capacitance and maximum gate oxide electric field strength, Embodiment 1 of the present invention has achieved optimizations compared to Comparative Example 1 and Comparative Example 2. On the one hand, by widening the depletion layer width of the gate-drain overlap region through the low-doping design at the top of the drift region, the reverse transfer capacitance of the embodiment is reduced by 23% compared to Comparative Example 1 and by 14% compared to Comparative Example 2. On the other hand, the integrated local P-type shielding layer can deflect the electric field lines originally pointing to the gate oxide layer into the SiC bulk material, thereby reducing the peak gate oxide electric field to 2.9 MV / cm, successfully controlling it within the long-term reliability safety threshold of 3 MV / cm.
[0067] In summary, the stepped-doped superjunction (SSD-SJ) trench-gate SiC MOSFET device with an integrated P-type shielding layer described in this invention designs the drift region as an alternating P / N pillar superjunction structure, employing a vertically non-uniform doping distribution of "low doping at the top, medium doping in the middle, and high doping at the bottom." This design, while maintaining the total charge of the P / N pillars and preserving a high breakdown voltage, effectively reduces the gate-drain parasitic capacitance by widening the depletion layer through the low-doped region at the top, achieving decoupling optimization of static breakdown voltage and dynamic loss. A locally high-concentration P-type shielding layer is integrated in the region near the bottom of the gate trench at the top of the P-type pillars. This shielding layer is directly shorted to the source metal and maintains equipotential. In the reverse blocking state, the shielding layer forms a strong electrostatic shielding field, deflecting the electric field lines originally pointing towards the gate oxide layer into the SiC bulk material, thereby reducing the peak electric field of the gate oxide.
[0068] The present invention discloses a stepped-doped superjunction (SSD-SJ) trench gate SiC MOSFET device with a local P-shielding layer. Through a three-segment vertically stepped doped P / N pillar structure, the static and dynamic characteristics are decoupled and optimized. At the same time, by taking advantage of the electrostatic shielding effect of the local P-type shielding layer at the top of the P pillar, the peak gate oxide electric field is significantly reduced without introducing an additional JFET resistor, thereby achieving multi-dimensional synergistic optimization of device static performance, dynamic loss and gate oxide reliability.
[0069] The above description of the embodiments is provided to enable those skilled in the art to understand and use the invention. It will be apparent to those skilled in the art that various modifications can be made to these embodiments, and the general principles described herein can be applied to other embodiments without inventive effort. Therefore, the present invention is not limited to the above embodiments, and any improvements and modifications made by those skilled in the art based on the disclosure of the present invention without departing from the scope of the invention should be within the protection scope of the present invention.
Claims
1. A stepped doped super junction trench gate SiC MOSFET device with P shield layer, characterized in that, Its cellular structure includes: trench gate region, source metal (1), N+ type source region (5), P type base region (6), P type shielding layer (7), N+ type substrate (11) and drain metal (12). Below the P-type base region (6) is a stepped doped superjunction P / N pillar drift region, including a P-type pillar region and an N-type pillar region; The trench gate region is in contact with the N+ type source region (5) and the P type base region (6), and extends into the N type pillar region; The P-type shielding layer (7) is located above the P-type column region and is electrically connected to the source metal (1).
2. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 1, wherein, The stepped-doped superjunction P / N pillar drift region includes alternating P-type pillar regions and N-type pillar regions. The P-type pillar regions and N-type pillar regions extend along the longitudinal direction of the device, and their doping concentrations are distributed in a stepped, non-uniform manner in the longitudinal direction, specifically with low doping at the top, medium doping in the middle, and high doping at the bottom.
3. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 2, wherein, The P-type pillar region includes a top low-doped P-pillar region (8), a middle uniformly doped P-pillar region (9), and a bottom high-doped P-pillar region (10) arranged from top to bottom. The top low-doped P-pillar region (8) is provided with a P-type shielding layer (7), and the bottom high-doped P-pillar region (10) is provided with an N+ type substrate (11).
4. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 2, wherein, The N-type pillar region includes a top low-doped N-pillar region (13), a middle uniformly doped N-pillar region (14), and a bottom high-doped N-pillar region (15) arranged from top to bottom. The trench gate region extends into the top low-doped N-pillar region (13), and the bottom high-doped N-pillar region (15) has an N+ type substrate (11) at the bottom.
5. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 1, wherein, The P-type shielding layer (7) is located near the bottom region of the trench gate region. Its depth is set so that it can cover the bottom corner region of the trench gate region. The peak doping concentration is higher than the top doping concentration of the P-type pillar region.
6. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 1, wherein, The P-type shielding layer (7) is formed by high-dose injection of aluminum ions.
7. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 1, wherein, The trench gate region includes a polysilicon gate electrode (2) and a gate oxide layer (3) disposed around the polysilicon gate electrode (2).
8. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 7, wherein, The gate electrode (2) is heavily doped polycrystalline silicon, the gate oxide layer (3) is silicon dioxide, the source metal (1) and the drain metal (12) are Al alloys, and the N+ type substrate (11) is N-type 4H-SiC.
9. The stepped-doped super junction trench gate SiC MOSFET device with P shield layer of claim 1, wherein, The trench gate region is located below the source metal (1), the source metal (1) is above the N+ type source region (5), the P-type base region phase (6) is below, the P+ contact region (4) is on the outside, the N+ type substrate (11) is above the stepped doped superjunction P / N pillar drift region, and the drain metal (12) is below.
10. A method for fabricating a stepped-doped superjunction trench gate SiC MOSFET device with a P-shielding layer as described in any one of claims 1 to 9, characterized in that, Includes the following steps: N-type drift regions were epitaxially grown multiple times on an N+ 4H-SiC substrate. During the multiple epitaxial growth cycles, the doping concentration of each N-type epitaxial layer was adjusted sequentially to form a vertically stepped distribution with low doping at the top, medium doping in the middle, and high doping at the bottom. After each epitaxial growth cycle, P-pillars were formed by ion implantation. During the multiple epitaxial growth cycles, the doping concentration of each P-type epitaxial layer was adjusted sequentially to form a vertically stepped distribution with low doping at the top, medium doping in the middle, and high doping at the bottom. In the last few cycles, an additional high-dose ion implantation was performed to form a local P-type shielding layer at the top of the P-pillars. After all epitaxy and implantation were completed, high-temperature activation annealing was performed. Trenches were etched and then subjected to sacrificial oxidation. Thermal growth of silicon dioxide gate oxide layer followed by nitriding annealing; deposition of polysilicon followed by etching back to form gate electrode; deposition of interlayer dielectric followed by etching of contact holes; sputtering of metal followed by annealing to form ohmic contact.