A low-voltage, low-capacitance ESD device and its fabrication method

By designing a vertical series-parallel structure of a low-capacitance Schottky diode and a low-voltage TVS diode in an ESD device, the problems of complex fabrication process, high cost and large device size in the prior art are solved, and miniaturization and high response speed of ESD devices are realized.

CN123124448APending Publication Date: 2026-11-17YANGZHOU GUOYU ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611270752.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-20
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing low-voltage, low-capacitance ESD devices have complex fabrication processes, high costs, and large device sizes, making it difficult to meet the high-density and miniaturization requirements of modern electronic devices.

Method used

The structure design employs a lightly doped P-type substrate, heavily doped P-type and N-type epitaxial layers, dielectric layer, trench, oxide layer, polysilicon layer, and metal layer to form a vertical series-parallel structure of a low-capacitance Schottky diode and a low-voltage TVS diode. The miniaturization of the ESD device is achieved through four photolithography and etching processes and one implantation and annealing process.

Benefits of technology

This has enabled the miniaturization of ESD devices, reduced capacitance and production costs, improved response speed, and shortened production cycles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124448A_ABST
    Figure CN123124448A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of semiconductor manufacturing technology and provides a low-voltage, low-capacitance ESD device and its fabrication method. The device includes a lightly doped P-type substrate, a heavily doped P-type epitaxial layer, a heavily doped N-type epitaxial layer, and a dielectric layer arranged sequentially. Trenches are formed on the dielectric layer, penetrating the heavily doped N-type and P-type epitaxial layers and extending into the lightly doped P-type substrate. An oxide layer and a polysilicon layer are formed sequentially within the trenches. Windows are opened on the oxide dielectric layer between the trenches, one window for implanting ions into the heavily doped N-type epitaxial layer to form a heavily doped N-type region. A metal layer is disposed on the heavily doped N-type region and the other window, forming a barrier layer by contacting the gold half-shell of the heavily doped N-type epitaxial layer at the other window. This invention meets the miniaturization requirements of ESD chips by forming a vertical series connection between a low-capacitance Schottky diode D1 and a low-voltage TVS diode, followed by a parallel connection with a unidirectional low-capacitance TVS diode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor manufacturing technology, specifically to a low-voltage, low-capacitance ESD device and its fabrication method. Background Technology

[0002] Electrostatic discharge protection (ESD) devices, also known as ESD diodes or TVS arrays, are overvoltage protection devices designed specifically for high-speed data transmission I / O ports. They are mainly used to prevent electrostatic discharge (ESD) from damaging sensitive circuits such as HDMI, USB, and mobile communication ports.

[0003] As integrated circuit technology continues to shrink and high-speed interface data rates break through 10Gbps, ESD protection devices face multiple stringent requirements, including low operating voltage, low capacitance, and small size.

[0004] Existing low-voltage, low-capacitance ESD devices mainly suffer from the following problems: Traditional solutions typically integrate multiple discrete devices into a single package, requiring the fabrication of separate photomasks for different types of devices and the execution of their respective independent process flows. This approach not only leads to numerous process steps and significantly increases process complexity, but also results in high manufacturing costs due to the need for repetitive mask alignment, etching, and deposition. Furthermore, the multiple discrete devices themselves and their interconnections occupy additional physical space, resulting in a larger overall package size, which fails to meet the urgent needs of modern electronic devices for high-density, miniaturized chip integration. Summary of the Invention

[0005] To address the shortcomings of existing technologies, this invention provides a low-voltage, low-capacitance ESD device and its fabrication method, thereby promoting the miniaturization of ESD chips, reducing the parasitic capacitance of ESD devices, and simultaneously reducing production costs and production cycles.

[0006] In a first aspect, the present invention provides a low-voltage, low-capacitance ESD device, comprising: Lightly doped p-type substrate; A heavily doped P-type epitaxial layer is disposed on a lightly doped P-type substrate; A heavily doped N-type epitaxial layer is disposed on top of a heavily doped P-type epitaxial layer; A dielectric layer is disposed on top of a heavily doped N-type epitaxial layer; The trench is formed on the dielectric layer, penetrates the heavily doped N-type epitaxial layer and the heavily doped P-type epitaxial layer and extends into the lightly doped P-type substrate; An oxide layer is formed on the inner surface of the trench; A polycrystalline silicon layer is formed on the oxide layer and fills the trench; A window is formed on the oxide dielectric layer and located between the trenches; one of the windows is used to implant ions into the heavily doped N-type epitaxial layer to form an N-type heavily doped region. Metal layers are respectively disposed on the heavily doped N-type region and another window. The metal layers form a barrier layer in contact with the heavily doped N-type epitaxial gold half-layer in the other window.

[0007] As can be seen from the above technical solution, the low-voltage, low-capacitance ESD device provided by the present invention utilizes a small area of ​​gold-semiconductor contact between the metal layer and the N-type heavily doped epitaxial layer to generate a low-capacitance Schottky diode, while the metal layer and the N-type heavily doped region form an ohmic contact; finally, a vertical series connection is formed between the low-capacitance Schottky diode D1 and the low-voltage TVS diode, and then a parallel connection is formed with the unidirectional low-capacitance TVS diode, which meets the miniaturization requirements of ESD chips.

[0008] Optionally, the depth of the heavily doped N-type region is less than the depth of the trench. The heavily doped N-type region extends into the lightly doped P-type substrate, forming a unidirectional conducting low-capacitance TVS diode between the region and the lightly doped P-type substrate. After high-temperature annealing, the junction depth of the heavily doped N-type region is less than the trench depth. The trench isolates the low-capacitance TVS diode from the Schottky diode and the low-voltage TVS diode, thus realizing a large-size low-voltage TVS diode and a small-size unidirectional conducting low-capacitance TVS diode.

[0009] Optionally, the trench spacing on both sides of the N-type heavily doped region is 15~20µm, and the trench spacing on both sides of the barrier layer is 200~250µm.

[0010] Optionally, the length and width of the barrier layer are 10~15µm.

[0011] Optionally, the depth of the trench is 20~25µm and the width is 1~1.2µm.

[0012] Optionally, the oxide layer has a thickness of 4000 Å.

[0013] Optionally, the doping concentration of the lightly doped P-type substrate is 1e14~5e14; the doping concentration of the heavily doped P-type epitaxial layer is 1e17~3e17 and the thickness is 5~6µm; the doping concentration of the heavily doped N-type epitaxial layer is 5e16~9e16 and the thickness is 4~5µm.

[0014] Optionally, the N-type heavily doped region is formed by implanting phosphorus ions, with a doping concentration of 1e20~3e20.

[0015] Optionally, the metal layer is made of Al.

[0016] Secondly, the present invention provides a method for fabricating a low-voltage, low-capacitance ESD device, comprising: S1. Obtain a lightly doped P-type substrate, and form a heavily doped P-type epitaxial layer on the lightly doped P-type substrate; S2. Grow a heavily doped N-type epitaxial layer on a heavily doped P-type epitaxial layer; S3. A dielectric layer is formed on the heavily doped N-type epitaxial layer; S4. Trenches are etched on the dielectric layer by photolithography. The trenches penetrate the dielectric layer, the heavily doped N-type epitaxial layer, the heavily doped P-type epitaxial layer and extend into the lightly doped P-type substrate. An oxide layer is generated in the trenches by hydrogen-oxygen synthesis. Then, the trenches are filled with N-type polysilicon. S5. A window is formed on the dielectric layer and between the trenches by photolithography, one of which is used to implant ions into the heavily doped N-type epitaxial layer to form an N-type heavily doped region. S6. A metal layer is formed on the heavily doped N-type region and another window, and the metal layer on the other window forms a barrier layer in contact with the gold half of the heavily doped N-type epitaxial layer.

[0017] By adopting the above technical solution, this application has the following beneficial effects: The low-voltage, low-capacitance ESD device provided by this invention utilizes the gold-semiconductor contact between a metal layer and a heavily doped N-type epitaxial layer to generate a low-capacitance Schottky diode, while simultaneously forming an ohmic contact between the metal layer and the heavily doped N-type region. Based on this, a low-capacitance Schottky diode D1 is connected in series with a low-voltage TVS diode, while avoiding the formation of a Schottky contact between the metal layer and the heavily doped N-type region. This ultimately forms a vertical series connection between the low-capacitance Schottky diode D1 and the low-voltage TVS diode, followed by a parallel connection with a unidirectional low-capacitance TVS diode, thus meeting the miniaturization requirements of ESD chips. This invention introduces a vertical series structure of a low-capacitance Schottky diode D1 and a low-voltage TVS diode, which can significantly improve the response speed of the entire ESD device and effectively reduce the clamping voltage. The fabrication process provided by this invention can produce wafers with only 4 photolithography and etching processes and 1 implantation and annealing process, eliminating the need for multiple photolithography and etching, implantation and annealing processes in traditional low-voltage and low-capacitance ESD processes, which greatly reduces production costs and production cycle. Attached Figure Description

[0018] To more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the accompanying drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn to scale.

[0019] Figure 1 A schematic diagram of a low-voltage, low-capacitance ESD device provided in an embodiment of the present invention is shown; Figure 2Another schematic diagram of a low-voltage, low-capacitance ESD device provided in an embodiment of the present invention is shown; Figure 3 A schematic diagram of the N-type heavily doped region and barrier layer provided in an embodiment of the present invention is shown; Figure 4 A flowchart illustrating a method for fabricating a low-voltage, low-capacitance ESD device according to an embodiment of the present invention is shown; Figure 5a A schematic diagram of the product obtained by step S1 of the preparation method provided in the embodiment of the present invention is shown; Figure 5b A schematic diagram of the product obtained by step S2 of the preparation method provided in the embodiment of the present invention is shown; Figure 5c A schematic diagram of the product obtained in step S3 of the preparation method provided in the embodiment of the present invention is shown; Figure 5d A schematic diagram of the product obtained in step S4 of the preparation method provided in an embodiment of the present invention is shown; Figure 5e A schematic diagram of the product obtained by step S5 of the preparation method provided in the embodiment of the present invention is shown; Figure 5f A schematic diagram of the product obtained by step S6 of the preparation method provided in the embodiment of the present invention is shown; Figure 5g A schematic diagram of the product obtained by the preparation method provided in the embodiment of the present invention is shown.

[0020] Figure label: 1-Lightly doped P-type substrate; 2-Heavily doped P-type epitaxial layer; 3-Heavily doped N-type epitaxial layer; 4-Dielectric layer; 5-Trench; 6-Heavily doped N-type region; 7-Barrier layer; 8-Metal layer. Detailed Implementation

[0021] The embodiments of the technical solution of the present invention will now be described in detail with reference to the accompanying drawings. These embodiments are only used to more clearly illustrate the technical solution of the present invention and are therefore merely examples, and should not be construed as limiting the scope of protection of the present invention.

[0022] It should be noted that, unless otherwise stated, the technical or scientific terms used in this application should have the ordinary meaning as understood by one of ordinary skill in the art to which this invention pertains.

[0023] In one embodiment, such as Figure 1 As shown, a low-voltage, low-capacitance ESD device is provided, comprising: Lightly doped P-type substrate 1, with a doping concentration of 1e14~5e14; A heavily doped P-type epitaxial layer 2 is disposed on a lightly doped P-type substrate 1, with a doping concentration of 1e17~3e17 and a thickness of 5~6µm; A heavily doped N-type epitaxial layer 3 is disposed on top of a heavily doped P-type epitaxial layer 2, with a doping concentration of 5e16~9e16 and a thickness of 4~5µm; the heavily doped P-type epitaxial layer and the heavily doped N-type epitaxial layer are in contact to form a low-voltage TVS transistor. Dielectric layer 4 is disposed on top of the heavily doped N-type epitaxial layer; Trench 5 is formed on the dielectric layer, penetrates the heavily doped N-type epitaxial layer and the heavily doped P-type epitaxial layer and extends into the lightly doped P-type substrate; An oxide layer is formed on the inner surface of the trench; A polycrystalline silicon layer is formed on the oxide layer and fills the trench; A window is formed on the oxide dielectric layer and located between the trenches; one of the windows is used to implant ions into the heavily doped N-type epitaxial layer to form an N-type heavily doped region 6, and a unidirectional TVS tube is formed between the N-type heavily doped region and the lightly doped P-type substrate. Metal layer 9 is disposed on N-type heavily doped region 6 and another window respectively. The metal layer is in contact with the heavily doped N-type epitaxial gold half-layer in the other window to form barrier layer 7, thereby forming Schottky diode.

[0024] In one embodiment, the depth of the heavily doped N-type region 6 is less than the depth of the trench, the trench spacing on both sides of the heavily doped N-type region 6 is 15~20µm, and the doping concentration of the heavily doped N-type region 6 is 1e20~3e20. The doping concentration of the heavily doped N-type region 6 is much greater than 10. 19 cm -3 A unidirectional low-capacitance TVS is formed between the TVS and the lightly doped P-type substrate 1.

[0025] In one embodiment, the trench spacing on both sides of the barrier layer 7 is 200~250µm, and the length and width of the barrier layer 7 are 10~15µm. Due to its small size, it forms a small-sized, low-capacitance Schottky diode.

[0026] In one embodiment, the trench 5 has a depth of 20-25µm and a width of 1-1.2µm; the oxide layer has a thickness of 4000Å.

[0027] like Figure 2-3As shown, due to the small barrier region area of ​​the low-capacitance Schottky diode D1, with a maximum size of only 15µm × 15µm, its capacitance is much smaller than that of the large-size low-voltage TVS diode T1 formed by heavily doped P-type and heavily doped N-type epitaxial layers. Although the PN junction of the unidirectional low-capacitance TVS diode T2 is deep, its sidewalls are in contact with the trenches. Therefore, the area of ​​its PN junction is determined only by the planar junction. T2's PN junction area is very small due to the influence of the trench spacing (15~20µm), and its capacitance is directly proportional to the concentration of the lightly doped P-type substrate. Therefore, the capacitance of the unidirectional low-capacitance TVS diode T2 is also much smaller than that of TVS diode T1. In summary, the capacitance values ​​of both the low-capacitance Schottky diode D1 and the unidirectional low-capacitance TVS diode T2 in the entire ESD device are much smaller than that of TVS diode T1, significantly reducing the overall capacitance of the ESD device.

[0028] ; ; ; Among them, C D1 C is the junction capacitance of the low-capacitance Schottky diode D1; T1 C is the junction capacitance of the low-voltage TVS diode T1; T2 ρ is the junction capacitance of the unidirectional low-capacitance TVS transistor T2; C is the capacitance of the entire ESD device; S is the area of ​​the barrier region; A is the area of ​​the PN junction; q is the elementary charge. N is the dielectric constant; D Low doping concentration; V bi V is the built-in potential; V is the reverse bias voltage.

[0029] In one embodiment, the metal layer 8 is made of Al. A portion of the Al in the metal layer 8 contacts a small area of ​​gold semiconductor in the heavily doped N-type epitaxial layer to form a low-capacitance Schottky diode D1. Simultaneously, because the Al metal barrier is low and the doping concentration of the heavily doped N-type region is much greater than 10⁻⁶, this process also achieves a low capacitance. 19 cm -3 Electrons tunnel directly through the potential barrier, thus forming an ohmic contact between the metal layer and the heavily doped N-type region. Based on this, a low-capacitance Schottky diode D1 is connected in series with the low-voltage TVS diode, while avoiding the formation of a Schottky contact between the metal layer and the heavily doped N-type region. This results in a vertical series connection between the low-capacitance Schottky diode D1 and the low-voltage TVS diode, followed by a parallel connection with a unidirectional low-capacitance TVS diode, meeting the miniaturization requirements of ESD chips. Furthermore, this invention introduces a vertical series structure between the low-capacitance Schottky diode D1 and the low-voltage TVS diode, which significantly improves the response speed of the entire ESD device while effectively reducing the clamping voltage.

[0030] In one embodiment, such as Figure 4 As shown, a method for fabricating a low-voltage, low-capacitance ESD device is provided, comprising: S1. Obtain a lightly doped P-type substrate 1, and form a heavily doped P-type epitaxial layer 2 on the lightly doped P-type substrate 1, such as... Figure 5a As shown; S2. Grow a heavily doped N-type epitaxial layer 3 on the heavily doped P-type epitaxial layer 2, such as Figure 5b As shown, a low-voltage TVS diode is formed by the contact between the heavily doped P-type epitaxial layer 2 and the heavily doped N-type epitaxial layer 3. S3. A dielectric layer 4 is formed on the heavily doped N-type epitaxial layer 3. The dielectric layer 4 is a SiO2 layer with a thickness of 20000 Å. Figure 5c As shown; S4. A trench 5 is etched on the dielectric layer 4 by photolithography. The trench 5 penetrates the dielectric layer 4, the heavily doped N-type epitaxial layer 3, the heavily doped P-type epitaxial layer 2 and extends into the lightly doped P-type substrate 1. A 4000 Å oxide layer is generated in the trench 5 by hydrogen-oxygen synthesis. Then, the trench 5 is filled with N-type polysilicon.

[0031] like Figure 5d As shown, the trenches 5 are spaced 200~250µm and 15~20µm from left to right, respectively. The trenches extend into the lightly doped P-type substrate. The purpose is to isolate the low-capacitance Schottky diodes connected in series with the low-voltage TVS diodes and the unidirectional low-capacitance TVS diodes, while realizing both large-size low-voltage TVS diodes and small-size unidirectional low-capacitance TVS diodes.

[0032] S5. A window is formed on the dielectric layer 4 and between the trenches 5 by photolithography etching.

[0033] One window is used to implant phosphorus ions into the heavily doped N-type epitaxial layer 3 to form the heavily doped N-type region 5, such as Figure 5e As shown, the implantation dose and energy were 1e17~3e17 and 120keV, respectively. High-temperature annealing was then performed to form a heavily doped N-type region with a junction depth of 15-20µm and a doping concentration of 1e20~3e20, significantly greater than 10. 19 cm -3 A unidirectional low-capacitance TVS is formed between the TVS and the lightly doped P-type substrate 1.

[0034] S6. A 4µm thick metal layer is deposited on the heavily doped N-type region 6 and the other window, followed by alloying. Ultimately, the metal layer deposited on the other window contacts the heavily doped N-type epitaxial layer to form an AlSi barrier layer, creating a small-sized, low-capacitance Schottky diode, such as... Figure 5f As shown; the size of the barrier layer is affected by the size of another window, with a length and width of 10~15µm.

[0035] like Figure 5gAs shown, the interconnect structure of the MET metal layer is realized through photolithography and etching, which connects the surface metal on the low-capacitance Schottky diode and the surface metal on the unidirectional low-capacitance TVS diode, ultimately becoming a low-voltage, low-capacitance ESD device.

[0036] Based on the above steps, wafer fabrication can be achieved with only 4 photolithography and etching processes and 1 implantation and annealing process, eliminating the need for multiple photolithography and etching, implantation and annealing processes in traditional low-voltage, low-capacitance ESD processes, which greatly reduces production costs and production cycle.

[0037] The above embodiments are only used to provide a detailed description of the technical solutions of this application. However, the descriptions of the above embodiments are only for the purpose of helping to understand the methods of the embodiments of the present invention and should not be construed as limiting the embodiments of the present invention. Any variations or substitutions that can be easily conceived by those skilled in the art should be covered within the protection scope of the embodiments of the present invention.

Claims

1. A low voltage, low capacitance ESD device, characterized by, include: Lightly doped p-type substrate; A heavily doped P-type epitaxial layer is disposed on a lightly doped P-type substrate; A heavily doped N-type epitaxial layer is disposed on top of a heavily doped P-type epitaxial layer; A dielectric layer is disposed on top of a heavily doped N-type epitaxial layer; The trench is formed on the dielectric layer, penetrates the heavily doped N-type epitaxial layer and the heavily doped P-type epitaxial layer and extends into the lightly doped P-type substrate; An oxide layer is formed on the inner surface of the trench; A polycrystalline silicon layer is formed on the oxide layer and fills the trench; A window is formed on the oxide dielectric layer and located between the trenches; one of the windows is used to implant ions into the heavily doped N-type epitaxial layer to form an N-type heavily doped region. Metal layers are respectively disposed on the heavily doped N-type region and another window. The metal layer forms a barrier layer in contact with the heavily doped N-type epitaxial gold half-layer in the other window.

2. The low voltage low capacitance ESD device of claim 1, wherein, The depth of the N-type heavily doped region is less than the depth of the trench.

3. The low-voltage, low-capacitance ESD device according to claim 1, characterized in that, The trench spacing on both sides of the N-type heavily doped region is 15~20µm, and the trench spacing on both sides of the barrier layer is 200~250µm.

4. The low-voltage, low-capacitance ESD device according to claim 3, characterized in that, The length and width of the barrier layer are 10~15µm.

5. The low-voltage, low-capacitance ESD device according to claim 4, characterized in that, The trench has a depth of 20~25µm and a width of 1~1.2µm.

6. The low-voltage, low-capacitance ESD device according to claim 3, characterized in that, The thickness of the oxide layer is 4000 Å.

7. The low-voltage, low-capacitance ESD device according to claim 1, characterized in that, The doping concentration of the lightly doped P-type substrate is 1e14~5e14; the doping concentration of the heavily doped P-type epitaxial layer is 1e17~3e17 and the thickness is 5~6µm; the doping concentration of the heavily doped N-type epitaxial layer is 5e16~9e16 and the thickness is 4~5µm.

8. The low-voltage, low-capacitance ESD device according to claim 1, characterized in that, The N-type heavily doped region is formed by implanting phosphorus ions, with a doping concentration of 1e20~3e20.

9. The low-voltage, low-capacitance ESD device according to claim 1, characterized in that, The metal layer is made of Al.

10. A method for fabricating a low-voltage, low-capacitance ESD device, characterized in that, include: S1. Obtain a lightly doped P-type substrate, and form a heavily doped P-type epitaxial layer on the lightly doped P-type substrate; S2. Grow a heavily doped N-type epitaxial layer on a heavily doped P-type epitaxial layer; S3. A dielectric layer is formed on the heavily doped N-type epitaxial layer; S4. Trenches are etched on the dielectric layer by photolithography. The trenches penetrate the dielectric layer, the heavily doped N-type epitaxial layer, the heavily doped P-type epitaxial layer and extend into the lightly doped P-type substrate. An oxide layer is generated in the trenches by hydrogen-oxygen synthesis. Then, the trenches are filled with N-type polysilicon. S5. A window is formed by photolithography etching on the dielectric layer and between the trenches. One of the windows is used to implant ions into the heavily doped N-type epitaxial layer to form an N-type heavily doped region. A metal is deposited in contact with the heavily doped N-type epitaxial layer to form a barrier layer. S6. A metal layer is formed on the heavily doped N-type region and another window. The metal layer deposited on the other window contacts the heavily doped N-type epitaxial layer to form a barrier layer.