A method for preparing a double-sided self-illuminating photovoltaic power generation smart building membrane material
By using surface energy trap density detection and free energy separation model, adjusting the deposition parameters of the electrode layer and the optical design of the color rendering control layer, the problem of inconsistent electrode structure in bifacial photovoltaic smart building membrane material was solved, achieving synergistic matching of power generation performance and color rendering effect and efficient production.
Patent Information
- Application Number
- CN202611396072.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-09
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, the deposition and control of electrode structure in the preparation of bifacial photovoltaic smart building membrane materials failed to effectively address the differences in surface characteristics between the front and back sides of the flexible polymer substrate. This resulted in inconsistencies in nucleation density, grain orientation, and residual stress in the electrode layers on both sides, affecting the balance of power generation performance and the synergistic matching of color rendering effects.
By detecting the surface energy trap density and using a free energy separation model, the surface characteristic parameters of the substrate are obtained. The initial deposition supersaturation and temperature gradient of the electrode layer are adjusted, and combined with the optical parameter design of the color development control layer, the differential deposition and color development effect of the electrode structure can be precisely controlled.
This achieves a balanced match between power generation performance and color rendering effect in bifacial photovoltaic smart building membrane materials, improving the finished product qualification rate and production efficiency, and avoiding unnecessary rework.
Smart Images

Figure CN123124494A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of building-integrated photovoltaics (BIPV), and more particularly to a method for preparing a double-sided self-illuminating photovoltaic power generation smart building membrane material. Background Technology
[0002] With the development of building-integrated photovoltaics (BIPV) technology, bifacial photovoltaic films that combine power generation and architectural aesthetics are attracting increasing attention. Bifacial self-illuminating photovoltaic smart building films require photoelectric conversion capabilities in both directions, while also exhibiting specific color rendering effects based on lighting conditions to meet architectural design requirements. However, in existing fabrication methods, the deposition parameters of the bifacial electrode structure are typically set independently, making it difficult to specifically control them based on the differences in surface characteristics between the two sides of the flexible polymer substrate. This results in inconsistencies in nucleation density, grain orientation, and residual stress between the electrode layers on both sides, thus affecting the balance of bifacial power generation performance. Furthermore, the design of the color rendering control layer is often independent of the optical characteristics of the electrode structure, lacking consideration of the intrinsic optical response differences between the bifacial electrode structures, making it difficult to synergistically match color rendering effects and power generation performance.
[0003] Chinese Patent Publication No. CN115923212B discloses a method for preparing a cast film, the cast film obtained by this method, and its applications. The method for preparing the cast film includes the following steps: mixing the components in layer A and layer B uniformly, then extruding them at a temperature of 80-120°C, followed by casting, embossing, cooling, drawing, and winding to obtain a first cast film with a double-layer structure; mixing ethylene-octene copolymer resin, silane graft monomer, initiator, nucleating agent, ultraviolet light stabilizer, and antioxidant uniformly, then extruding them at a temperature of 80-120°C, followed by casting, embossing, cooling, drawing, and winding to obtain a second cast film with a single-layer structure; the cast film obtained by this application, while ensuring good light transmittance, can significantly enhance the power generation efficiency of bifacial photovoltaic modules, and requires fewer solar cells, achieving the goal of cost reduction and efficiency improvement.
[0004] Therefore, the existing technology has the following problems:
[0005] Improving light transmittance and power generation efficiency solely through optimization of material composition and process parameters fails to address the issue of targeted deposition control of double-sided electrode structures based on the differences in surface characteristics between the front and back sides of the substrate. Summary of the Invention
[0006] Therefore, this invention provides a method for preparing a double-sided self-illuminating photovoltaic power generation smart building membrane material, which overcomes the problem that existing technologies only improve light transmittance and power generation efficiency by optimizing material composition and process parameters, but fail to address the issue of targeted deposition control of the double-sided electrode structure based on the differences in surface characteristics of the front and back sides of the substrate.
[0007] To achieve the above objectives, the present invention provides a method for preparing a double-sided self-illuminating photovoltaic power generation smart building membrane material, comprising:
[0008] Step S1: Provide a flexible polymer substrate, and form an optical control layer on the flexible polymer substrate to obtain a composite film substrate layer;
[0009] Step S2: Surface energy trap density is detected on the composite membrane substrate to obtain the surface energy trap density distribution on both sides of the composite membrane substrate and the ratio of the polar to non-polar components of the surface free energy.
[0010] Step S3: Determine the initial deposition supersaturation of the top electrode layer prepared on the photovoltaic functional layer and the back electrode layer prepared on the lower surface of the composite film substrate layer according to the surface energy trap density distribution, and determine the deposition temperature gradient of the top electrode layer and the back electrode layer according to the ratio of the polar component to the non-polar component.
[0011] Step S4: A transparent top electrode layer is prepared on the photovoltaic functional layer according to the deposition parameters, and a back electrode layer is prepared on the lower surface of the composite film substrate layer to form a double-sided electrode structure.
[0012] Step S5: Perform double-sided illumination response detection on the double-sided electrode structure. Apply incident light of a preset wavelength from the front and back sides of the composite film substrate layer respectively, and obtain the response spectrum of the double-sided electrode structure under the front and back incident light conditions. Determine the selective response characteristics of the double-sided electrode structure to the front and back incident light based on the degree of difference between the two response spectra.
[0013] Step S6: Determine the target optical parameters of the color development control layer based on the selective response characteristics, and prepare the color development control layer on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer based on the target parameters;
[0014] Step S7: After encapsulation, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained.
[0015] Further, in step S2, the surface energy trap density of the composite film substrate is detected, including:
[0016] Dynamic contact angle measurements were performed on the front and back sides of the composite membrane substrate to obtain the forward contact angle and backward contact angle values at each detection point, and the contact angle hysteresis value at each detection point was calculated.
[0017] Based on the contact angle hysteresis values at each detection point, the average contact angle hysteresis and the dispersion of the contact angle hysteresis distribution on the front and back sides of the composite film substrate are calculated. The average contact angle hysteresis is used to characterize the magnitude of the surface energy trap density, and the dispersion of the contact angle hysteresis distribution is used to characterize the in-plane distribution uniformity of the surface energy trap density.
[0018] The contact angles of at least two polarity test liquids were measured at each detection point. The polar and non-polar components of the surface free energy at each detection point were calculated using a surface free energy separation model to obtain the ratio of the polar to non-polar components of the surface free energy on both sides of the composite membrane substrate.
[0019] Further, in step S3, determining the initial deposition supersaturation includes:
[0020] The reference values for the initial deposition supersaturation of the transparent top electrode layer and the back electrode layer are determined based on the average contact angle hysteresis value.
[0021] The in-plane compensation coefficient for the initial deposition supersaturation is determined based on the dispersion of the contact angle hysteresis distribution.
[0022] The initial deposition supersaturation is obtained by correcting the reference value with the in-plane compensation coefficient.
[0023] Further, in step S3, determining the deposition temperature gradient includes:
[0024] The directional configuration of the deposition temperature gradient of the transparent top electrode layer and the back electrode layer is determined based on the difference between the ratio of the polar to the non-polar components of the surface free energy on both sides of the composite film substrate.
[0025] When the difference is greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in opposite directions;
[0026] When the difference is not greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in the same direction but with different amplitudes.
[0027] Further, in step S5, the double-sided electrode structure is subjected to double-sided illumination response detection, including:
[0028] A first incident light of a preset wavelength is applied to the front side of the composite film substrate, and the first response spectrum of the double-sided electrode structure under the front incident light condition is collected.
[0029] A second incident light of the same wavelength as the first incident light is applied from the back side of the composite film substrate, and the second response spectrum of the double-sided electrode structure under the back incident light condition is collected.
[0030] The first response spectrum is compared with the second response spectrum, and the difference in spectral response between the two at each wavelength is calculated to obtain the difference spectral curve.
[0031] Based on the amplitude and waveform characteristics of the difference spectral curves, the selective response characteristics of the double-sided electrode structure to incident light from both sides are determined.
[0032] Further, in step S6, determining the target optical parameters of the color rendering control layer based on the selective response characteristics includes:
[0033] Obtain a preset visual consistency target, and convert the visual consistency target into a target chromaticity value range for the front and back color display effects;
[0034] Using the selective response characteristics as the initial input and the target chromaticity range as the optimization objective, the combined solution of the film thickness, refractive index and extinction coefficient of the color rendering control layer is solved in reverse iteration through an optical inverse design model, and the solution is used as the target optical parameter.
[0035] Further, in step S6, a color development control layer is prepared on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer according to the target parameters, including:
[0036] Based on the refractive index, extinction coefficient, and film thickness of the target optical parameters, determine the difference in the anisotropic optical response of the color rendering control layer in the two directions.
[0037] Based on the difference in the anisotropic optical response of the target, the field strength and direction of the electric field-assisted deposition are determined;
[0038] During the deposition of the color development control layer material, an electric field with the specified strength and direction is applied to the color development control layer, causing the color development control layer material to align in the direction of the electric field.
[0039] After curing, a colorimetric control layer is formed that has an anisotropic optical response that matches the difference value of the anisotropic optical response of the target.
[0040] Furthermore, the field strength and direction of the electric field-assisted deposition are determined, including:
[0041] Based on the target anisotropic refractive index target value and the target anisotropic extinction coefficient target value in the target anisotropic optical response difference value, calculate the equivalent dielectric constant tensor corresponding to the color rendering control layer material when it is arranged in different directions;
[0042] Substituting the equivalent dielectric constant tensor into the electric field-dipole moment coupling model, we can inversely deduce the dipole moment orientation distribution required for the color rendering control layer material to achieve the target values of refractive index anisotropy and extinction coefficient anisotropy.
[0043] Based on the dipole moment orientation distribution, the electric field strength and direction applied during the deposition process are determined.
[0044] Further, in step S7, the double-sided self-displaying photovoltaic power generation smart building membrane material obtained after encapsulation includes:
[0045] The formed photovoltaic device structure is laminated and encapsulated, and then bi-sided power generation performance and bi-sided color rendering effect are tested.
[0046] When both power generation performance and color rendering performance are qualified, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained;
[0047] When only the color development performance is unsatisfactory, the color development control layer should be re-prepared.
[0048] When the power generation performance is unqualified, the substrate is discarded.
[0049] Furthermore, when re-preparing the color development control layer, the target optical parameters are corrected based on the double-sided color development effect test results, and the color development control layer is re-prepared with the corrected target optical parameters.
[0050] Compared with the prior art, the beneficial effects of the present invention are as follows: This embodiment obtains the contact angle hysteresis value through dynamic contact angle measurement to characterize the surface energy trap density, and uses the contact angle hysteresis distribution dispersion to characterize the in-plane distribution uniformity of the surface energy trap density. It also combines static contact angle measurement of at least two polar test liquids and surface free energy separation model to calculate the ratio of polar to non-polar components of surface free energy, thereby realizing a comprehensive quantitative evaluation of the surface characteristics of both sides of the flexible polymer substrate, and providing accurate input basis for the differentiated setting of subsequent electrode deposition parameters.
[0051] Furthermore, this embodiment achieves the quantitative conversion of substrate surface energy trap density from high to low to deposition parameters through a segmented mapping between the average contact angle hysteresis value and the initial deposition supersaturation reference value. It also determines the in-plane compensation coefficient based on the contact angle hysteresis distribution dispersion to perform regional differentiation correction on the reference value, enabling the initial deposition supersaturation to adaptively distribute within the substrate surface according to the degree of non-uniformity in surface energy trap density distribution. Simultaneously, the difference in the ratio of the polar to non-polar components of the surface free energy on both sides is used to determine the degree of difference in chemical affinity of the two sides to the deposition material. Based on this, the deposition temperature gradients on both sides are configured to have opposite or unidirectional amplitude differences. The orientation-inducing effect of the temperature field allows the electrode layers on both sides to grow with preferred orientations on different crystal planes, forming stress complementarity. This achieves the full-process quantitative conversion and differentiated control of substrate surface characteristic detection results to double-sided electrode deposition parameters.
[0052] Furthermore, in this embodiment, by applying incident light of the same wavelength and power density from the front and back sides of the composite film substrate layer respectively, the transmission spectra of the front and back sides are collected and the transmittance difference at each wavelength point is calculated to form a difference spectral curve. The amplitude and waveform characteristics of the difference spectral curve in the visible light and near-infrared bands are further extracted, realizing the quantitative characterization of the optical response difference between the front and back sides of the double-sided electrode structure, and providing a basis for determining the target optical parameters of the subsequent color rendering control layer.
[0053] Furthermore, this embodiment quantifies the difference in anisotropic optical response between the front and back sides of the color development control layer by decomposing the refractive index, extinction coefficient, and film thickness in the target optical parameters into components in the perpendicular and parallel directions and calculating the difference. Then, the required dipole moment orientation distribution is inversely deduced by calculating the equivalent dielectric constant tensor and the electric field-dipole moment coupling model, and finally the field strength and direction of electric field-assisted deposition are determined, realizing the quantitative conversion of the target optical parameters of the color development control layer into electric field deposition parameters. During the deposition process, a determined electric field is applied to orient the color development material along the electric field direction and solidify it, so that the color development control layer has an anisotropic optical response that matches the difference value of the target anisotropic optical response, thereby achieving precise control and consistent matching of the color development effect on both sides.
[0054] Furthermore, this embodiment uses a vacuum lamination encapsulation process to protect the photovoltaic device structure. After encapsulation, bifacial power generation performance and bifacial color rendering effect tests are performed simultaneously. The pass / fail criteria are that the ratio of the power generation efficiency on the front side to the power generation efficiency on the back side is within a preset balance range and the color difference between the front and back sides is less than or equal to a preset threshold. This achieves dual-indicator verification of power generation performance and color rendering performance. When only the color rendering performance is unqualified, the target optical parameters are corrected by using the measured color difference between the front and back sides as feedback, and the color rendering control layer is re-prepared. When the power generation performance is unqualified, the substrate is directly discarded, avoiding invalid rework and improving the finished product pass rate and production efficiency. Attached Figure Description
[0055] Figure 1 This is a flowchart of the method for preparing double-sided self-displaying photovoltaic power generation smart building membrane material in this embodiment;
[0056] Figure 2 This is a flowchart of the surface energy trap density detection process in the middle layer of the double-sided self-displaying photovoltaic power generation smart building membrane material preparation method in this embodiment. Detailed Implementation
[0057] To make the objectives and advantages of the present invention clearer, the present invention will be further described below with reference to embodiments; it should be understood that the specific embodiments described herein are merely for explaining the present invention and are not intended to limit the present invention.
[0058] Preferred embodiments of the present invention will now be described with reference to the accompanying drawings. Those skilled in the art should understand that these embodiments are merely illustrative of the technical principles of the present invention and are not intended to limit the scope of protection of the present invention.
[0059] Please see Figures 1-2 As shown, Figure 1 This is a flowchart of the method for preparing double-sided self-displaying photovoltaic power generation smart building membrane material in this embodiment; Figure 2 This is a flowchart of the surface energy trap density detection process in the middle layer of the double-sided self-displaying photovoltaic power generation smart building membrane material preparation method in this embodiment.
[0060] This embodiment provides a method for preparing a double-sided self-displaying photovoltaic power generation smart building membrane material, including:
[0061] Step S1: Provide a flexible polymer substrate, and form an optical control layer on the flexible polymer substrate to obtain a composite film substrate layer;
[0062] Step S2: Surface energy trap density is detected on the composite membrane substrate to obtain the surface energy trap density distribution on both sides of the composite membrane substrate and the ratio of the polar to non-polar components of the surface free energy.
[0063] Step S3: Determine the initial deposition supersaturation of the top electrode layer prepared on the photovoltaic functional layer and the back electrode layer prepared on the lower surface of the composite film substrate layer according to the surface energy trap density distribution, and determine the deposition temperature gradient of the top electrode layer and the back electrode layer according to the ratio of the polar component to the non-polar component.
[0064] Step S4: A transparent top electrode layer is prepared on the photovoltaic functional layer according to the deposition parameters, and a back electrode layer is prepared on the lower surface of the composite film substrate layer to form a double-sided electrode structure.
[0065] Step S5: Perform double-sided illumination response detection on the double-sided electrode structure. Apply incident light of a preset wavelength from the front and back sides of the composite film substrate layer respectively, and obtain the response spectrum of the double-sided electrode structure under the front and back incident light conditions. Determine the selective response characteristics of the double-sided electrode structure to the front and back incident light based on the degree of difference between the two response spectra.
[0066] Step S6: Determine the target optical parameters of the color development control layer based on the selective response characteristics, and prepare the color development control layer on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer based on the target parameters;
[0067] Step S7: After encapsulation, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained.
[0068] In this embodiment, a flexible polymer substrate is provided, which is selected from polyethylene terephthalate (PET), polyethylene naphthalate (PEN), or polyimide (PI), and has a thickness of 50-200 μm. The flexible polymer substrate is cleaned by sequentially ultrasonically cleaning it in acetone, anhydrous ethanol, and deionized water for 10-20 minutes at an ultrasonic frequency of 40-80 kHz, and then drying it with nitrogen. The cleaned flexible polymer substrate undergoes surface activation treatment: the substrate is placed in an oxygen plasma treatment chamber with a treatment power of 50-200 W for 1-5 minutes and an oxygen flow rate of 50-200 sccm.
[0069] An optical modulation layer is formed on the surface of the activated flexible polymer substrate. When the optical modulation layer is a spectrally selective filter layer, a high-refractive-index dielectric film and a low-refractive-index dielectric film are alternately deposited using magnetron sputtering. The high-refractive-index dielectric film material is selected from Nb₂O₅, TiO₂, or HfO₂, and the low-refractive-index dielectric film material is selected from SiO₂. During sputtering, the base vacuum is 1.0 × 10⁻³ - 5.0 × 10⁻⁻⁻⁻⁵. 4 Pa, working gas pressure is 0.3-1.0 Pa, sputtering power is 100-300 W; the thickness of a single layer of high refractive index dielectric film is 20-60 nm, the thickness of a single layer of low refractive index dielectric film is 30-100 nm, and the number of alternating layers is 4-20.
[0070] When the optical control layer is a thermochromic layer, it is formed by a coating method: a thermochromic polymer hydrogel is coated onto the upper surface of the flexible polymer substrate, with a coating thickness of 50-200 μm, a coating speed of 1-5 m / min, and a coating temperature of 25-40℃; the thermochromic polymer hydrogel is hydroxypropyl cellulose hydrogel or poly-N-isopropylacrylamide hydrogel, which is transparent below the phase transition temperature and light-scattering above the phase transition temperature. The flexible polymer substrate with the optical control layer formed thereon is cured at 60-100℃ for 30-120 min to obtain the composite film substrate layer.
[0071] Specifically, in step S2, the surface energy trap density of the composite film substrate is detected, including:
[0072] Step S21: Perform dynamic contact angle measurements on the front and back sides of the composite membrane substrate layer to obtain the forward contact angle value and backward contact angle value at each detection point, and calculate the contact angle hysteresis value at each detection point.
[0073] Step S22: Based on the contact angle hysteresis values at each detection point, calculate the average contact angle hysteresis and the dispersion of the contact angle hysteresis distribution on the front and back sides of the composite film substrate layer. The average contact angle hysteresis is used to characterize the magnitude of the surface energy trap density, and the dispersion of the contact angle hysteresis distribution is used to characterize the in-plane distribution uniformity of the surface energy trap density.
[0074] Step S23: Measure the contact angle of at least two polarity test liquids at each detection point, and calculate the polar and non-polar components of the surface free energy at each detection point using the surface free energy separation model to obtain the ratio of the polar to non-polar components of the surface free energy on both sides of the composite membrane substrate.
[0075] In this embodiment, 9-25 detection points are selected on both the front and back sides of the composite membrane substrate layer. These detection points are evenly distributed in a grid pattern with equal spacing, and the distance between adjacent detection points is 20-50 mm. Dynamic contact angle measurements are performed on each detection point using the seated drop method. Deionized water is used as the test liquid, with a drop volume of 2-5 μL and a drop rate of 0.5-2 μL / s. The forward and backward contact angles of the droplet during its spread on the substrate surface are collected at room temperature. Each detection point is measured 3-5 times, and the average value is taken as the dynamic contact angle data for that point.
[0076] The difference between the advancing and retreating contact angles at each detection point is calculated as the contact angle hysteresis value for each detection point. Based on the contact angle hysteresis values of all detection points, the average contact angle hysteresis and the contact angle hysteresis distribution dispersion of the front and back sides of the composite membrane substrate are calculated respectively; wherein, the contact angle hysteresis distribution dispersion is characterized by the standard deviation or range of the contact angle hysteresis values. The average contact angle hysteresis value is used to characterize the surface energy trap density of the composite membrane substrate: the larger the average contact angle hysteresis value, the higher the surface energy trap density and the more active nucleation sites; the smaller the average contact angle hysteresis value, the lower the surface energy trap density and the fewer active nucleation sites. The contact angle hysteresis distribution dispersion is used to characterize the in-plane distribution uniformity of the surface energy trap density of the composite membrane substrate: the smaller the contact angle hysteresis distribution dispersion, the more uniform the in-plane distribution of the surface energy trap density; the larger the contact angle hysteresis distribution dispersion, the more non-uniform the in-plane distribution of the surface energy trap density.
[0077] The contact angles of at least two polar test liquids were measured at each detection point. The polar test liquids included deionized water and diiodomethane, or deionized water and formamide. The static contact angles of each detection point under the two polar test liquids were measured using the seated drop method. Each detection point was measured 3-5 times, and the average value was taken. The polar and non-polar components of the surface free energy at each detection point were calculated using a surface free energy separation model. The Owens-Wendt geometric mean method or the Van Oss-Chaudhury-Good acid-base theory model was used. The measured contact angles of the two polar test liquids were substituted into the model, and the non-polar and polar components of the surface free energy at each detection point were solved simultaneously. The average ratio of the polar to non-polar components of the surface free energy at all detection points on both the front and back sides of the composite membrane substrate was taken to obtain the ratio of the polar to non-polar components of the surface free energy on both sides of the composite membrane substrate.
[0078] This embodiment uses dynamic contact angle measurement to obtain contact angle hysteresis values to characterize the surface energy trap density, and uses the dispersion of contact angle hysteresis distribution to characterize the in-plane distribution uniformity of surface energy trap density. It also combines static contact angle measurements of at least two polar test liquids and a surface free energy separation model to calculate the ratio of polar to non-polar components of surface free energy. This achieves a comprehensive quantitative evaluation of the surface characteristics of both sides of the flexible polymer substrate, providing a precise input basis for the differentiated setting of subsequent electrode deposition parameters.
[0079] Specifically, in step S3, determining the initial deposition supersaturation includes:
[0080] The reference values for the initial deposition supersaturation of the transparent top electrode layer and the back electrode layer are determined based on the average contact angle hysteresis value.
[0081] The in-plane compensation coefficient for the initial deposition supersaturation is determined based on the dispersion of the contact angle hysteresis distribution.
[0082] The initial deposition supersaturation is obtained by correcting the reference value with the in-plane compensation coefficient.
[0083] In this embodiment, the initial deposition supersaturation values of the transparent top electrode layer and the back electrode layer are determined based on the average contact angle hysteresis value, specifically as follows:
[0084] When the average contact angle hysteresis is in the range of 0-5°, the initial deposition supersaturation benchmark value should be the larger value, ranging from 15% to 25%;
[0085] When the average contact angle hysteresis is greater than 5° and less than or equal to 10°, the initial deposition supersaturation benchmark value is taken as a medium-high value, with a range of 10%–20%.
[0086] When the average contact angle hysteresis is greater than 10° and less than or equal to 15°, the initial deposition supersaturation benchmark value is taken as a low to medium value, ranging from 5% to 15%.
[0087] When the average contact angle hysteresis is greater than 15°, the initial deposition supersaturation benchmark value should be a small value, ranging from 3% to 10%.
[0088] The larger the average contact angle hysteresis, the higher the surface energy trap density and the more active nucleation sites, and the lower the required initial deposition supersaturation baseline value; the smaller the average contact angle hysteresis, the lower the surface energy trap density and the fewer active nucleation sites, and the higher the required initial deposition supersaturation baseline value.
[0089] The in-plane compensation coefficient for the initial deposition supersaturation is determined based on the dispersion of the contact angle hysteresis distribution, specifically as follows:
[0090] The in-plane compensation coefficient is a function of the contact angle hysteresis distribution dispersion; the greater the contact angle hysteresis distribution dispersion, the greater the in-plane compensation coefficient.
[0091] When the dispersion of the contact angle hysteresis distribution is in the range of 0-0.2, the in-plane compensation coefficient is 0.8-1.0;
[0092] When the dispersion of the contact angle hysteresis distribution is greater than 0.2 and less than or equal to 0.5, the in-plane compensation coefficient is 1.0-1.5;
[0093] When the dispersion of the contact angle hysteresis distribution is greater than 0.5, the in-plane compensation coefficient is 1.5-2.0.
[0094] The initial deposition oversaturation is obtained by correcting the reference value with the in-plane compensation coefficient: the reference value corresponding to the average contact angle hysteresis is multiplied by the in-plane compensation coefficient of the corresponding region to obtain the initial deposition oversaturation of the transparent top electrode layer and the back electrode layer at each detection point on the composite film substrate. The initial deposition oversaturation is distributed differently in-plane with the dispersion of the contact angle hysteresis distribution on the composite film substrate. In areas with a large dispersion of the contact angle hysteresis distribution, the initial deposition oversaturation is adjusted higher relative to the reference value. In areas with a small dispersion of the contact angle hysteresis distribution, the initial deposition oversaturation is close to or equal to the reference value to compensate for the in-plane difference in nucleation density caused by the inhomogeneity of the surface energy trap density of the substrate.
[0095] Specifically, in step S3, determining the deposition temperature gradient includes:
[0096] The directional configuration of the deposition temperature gradient of the transparent top electrode layer and the back electrode layer is determined based on the difference between the ratio of the polar to the non-polar components of the surface free energy on both sides of the composite film substrate.
[0097] When the difference is greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in opposite directions;
[0098] When the difference is not greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in the same direction but with different amplitudes.
[0099] In this embodiment, the preset orientation threshold is determined as follows: Based on the material type of the flexible polymer substrate used in the composite film substrate layer and its interfacial bonding characteristics with the electrode deposition material, the preset orientation threshold is predetermined. Specifically, when the difference between the ratio of the polar to non-polar components of the surface free energy of the front and back sides of the composite film substrate layer exceeds this threshold, it indicates that the difference in chemical affinity between the front and back sides of the electrode deposition material is sufficient to induce the electrode material to nucleate on both sides with different initial crystal orientations. The preset orientation threshold ranges from 0.15 to 0.35. This threshold is determined based on the actual matching relationship between the substrate material and the electrode material, mainly based on: the measured fluctuation range of the ratio of the polar to non-polar components of the surface free energy of the substrate material, the critical conditions for the preferred orientation transition of the electrode material on surfaces with different chemical affinities, and a comprehensive determination using research data on the relationship between interfacial chemical affinity differences and the preferred orientation of thin films in similar material systems.
[0100] In this embodiment, the directional configuration of the deposition temperature gradient between the transparent top electrode layer and the back electrode layer is determined based on the difference in the ratio of the polar to non-polar components of the surface free energy on both sides of the composite film substrate layer. The difference between the ratio of the polar to non-polar components of the surface free energy on the front side and the ratio on the back side of the composite film substrate layer is calculated, and this difference characterizes the degree of difference in the chemical affinity of the two surfaces to the deposited material. A pre-set directional threshold is used to determine whether the difference in chemical affinity between the two surfaces is sufficient to affect the preferred orientation direction of the electrode material on both sides.
[0101] When the difference is greater than a preset direction threshold, it indicates a significant difference in the chemical affinity of the front and back sides to the deposited material. In this case, the deposition temperature gradients of the transparent top electrode layer and the back electrode layer are configured in opposite directions; that is, if the deposition temperature gradient on the front side is set as a positive gradient, then the deposition temperature gradient on the back side is set as a negative gradient, or vice versa. When the difference is not greater than the preset direction threshold, it indicates that the difference in the chemical affinity of the front and back sides to the deposited material is not significant. In this case, the deposition temperature gradients of the transparent top electrode layer and the back electrode layer are configured in the same direction but with different amplitudes; that is, the deposition temperature gradients on both sides are in the same direction, but the heating or cooling rates are different. The orientation configuration of the deposition temperature gradients aims to induce the transparent top electrode layer and the back electrode layer to grow with different preferred crystal orientations during the deposition process through the orientation-induced effect of the temperature field. This results in a stress-complementary state in the residual stress distribution of the electrode layers on both sides after deposition, reducing the risk of warping and cracking of the overall film material.
[0102] This embodiment achieves the quantitative conversion of substrate surface energy trap density from high to low to deposition parameters through a segmented mapping between the average contact angle hysteresis value and the initial deposition supersaturation reference value. Furthermore, it uses the contact angle hysteresis distribution dispersion to determine the in-plane compensation coefficient, which is then used to perform regional differentiation correction on the reference value. This allows the initial deposition supersaturation to adaptively distribute within the substrate surface according to the degree of non-uniformity in surface energy trap density distribution. Simultaneously, the difference in the ratio of the polar to non-polar components of the surface free energy on both sides is used to determine the degree of difference in chemical affinity of the two sides to the deposition material. Based on this, the deposition temperature gradients on both sides are configured to have opposite or unidirectional amplitude differences. The orientation-inducing effect of the temperature field allows the electrode layers on both sides to grow with preferred orientations on different crystal planes, forming stress complementarity. This achieves the full-process quantitative conversion and differentiated control of substrate surface characteristic detection results to double-sided electrode deposition parameters.
[0103] Specifically, a transparent top electrode layer is prepared on the photovoltaic functional layer according to the deposition parameters, and a back electrode layer is prepared on the lower surface of the composite film substrate layer to form a double-sided electrode structure.
[0104] In this embodiment, based on the initial deposition supersaturation and deposition temperature gradient of the transparent top electrode layer determined in step S3, a transparent top electrode layer is prepared on the photovoltaic functional layer using magnetron sputtering; simultaneously, based on the initial deposition supersaturation and deposition temperature gradient of the back electrode layer determined in step S3, a back electrode layer is prepared on the lower surface of the composite film substrate layer using magnetron sputtering.
[0105] When preparing the transparent top electrode layer, the initial deposition supersaturation is converted into the sputtering power density of magnetron sputtering. Specifically, for every 1% increase in the initial deposition supersaturation, the sputtering power density increases by 0.5–1.5 W / cm². The deposition temperature gradient is converted into the rate of change of the substrate front temperature during deposition. Specifically, when the deposition temperature gradient is positive, the substrate front temperature rises from room temperature to the first deposition temperature (80–120°C) at a first heating rate during the initial deposition stage, and rises to the second deposition temperature (150–200°C) at a second heating rate during the middle and later stages of deposition. When the deposition temperature gradient is negative, the substrate front temperature drops from the initial heating temperature to the first deposition temperature (150–200°C) at a first cooling rate during the initial deposition stage, and drops to the second deposition temperature (80–120°C) at a second cooling rate during the middle and later stages of deposition.
[0106] When preparing the back electrode layer, the initial deposition supersaturation of the back electrode layer is converted into the sputtering power density of magnetron sputtering. Specifically, for every 1% increase in the initial deposition supersaturation, the sputtering power density increases by 0.5-1.5 W / cm². The deposition temperature gradient of the back electrode layer is converted into the rate of change of the temperature on the back side of the substrate during the deposition process. The rate of change of the temperature on the back side of the substrate and the deposition temperature are independently controlled in the same way as the front side.
[0107] During deposition, independent infrared heating lamps and cooling pipes are installed on the front and back sides of the composite film substrate, respectively, to ensure that the temperature fields on the front and back sides do not interfere with each other and are independently controlled according to their respective deposition temperature gradients. The temperature on the front side of the substrate is controlled by a closed-loop feedback control using infrared heating lamps and thermocouples, while the temperature on the back side of the substrate is controlled by a closed-loop feedback control using cooling pipe medium flow rate adjustment and thermocouples. The temperature control accuracy is ±2℃. The target material for the transparent top electrode layer is indium tin oxide (ITO), the sputtering gas is argon, the sputtering pressure is 0.3–1.0 Pa, the sputtering power density is determined according to the initial deposition supersaturation, the target-substrate distance is 50–150 mm, the deposition time is 10–60 min, and the thickness of the transparent top electrode layer after deposition is 50–300 nm.
[0108] The target material for the back electrode layer is one of a silver target, an aluminum target, or a copper target. The sputtering gas is argon, the sputtering pressure is 0.3–1.0 Pa, and the sputtering power density is determined according to the initial deposition supersaturation. The target-substrate distance is 50–150 mm, the deposition time is 5–30 min, and the thickness of the back electrode layer after deposition is 50–200 nm. After deposition, a transparent top electrode layer is formed on the upper surface of the photovoltaic functional layer, and a back electrode layer is formed on the lower surface of the composite film substrate layer, resulting in a double-sided electrode structure.
[0109] Specifically, in step S5, the double-sided electrode structure is subjected to double-sided illumination response detection, including:
[0110] A first incident light of a preset wavelength is applied to the front side of the composite film substrate, and the first response spectrum of the double-sided electrode structure under the front incident light condition is collected.
[0111] A second incident light of the same wavelength as the first incident light is applied from the back side of the composite film substrate, and the second response spectrum of the double-sided electrode structure under the back incident light condition is collected.
[0112] The first response spectrum is compared with the second response spectrum, and the difference in spectral response between the two at each wavelength is calculated to obtain the difference spectral curve.
[0113] Based on the amplitude and waveform characteristics of the difference spectral curves, the selective response characteristics of the double-sided electrode structure to incident light from both sides are determined.
[0114] In this embodiment, the double-sided electrode structure obtained in step S4 is placed in a double-sided illumination response detection device. The detection device includes a first light source and a spectral receiver located above the front side of the composite film substrate, and a second light source and a spectral receiver located below the back side of the composite film substrate. A first incident light of a preset wavelength is applied from the front side of the composite film substrate: the first light source is a xenon lamp or a halogen tungsten lamp with an output wavelength of 300-1100nm, covering the visible to near-infrared wavelength range; the first light source is turned on, and the light intensity is adjusted so that the front incident light power density is 80-120mW / cm², the light spot area covers the entire detection area, and the angle between the incident direction of the beam and the normal to the substrate surface is 0°, i.e., perpendicular incident; after the light intensity stabilizes, the transmitted light is collected using the front spectral receiver to obtain the first response spectrum of the double-sided electrode structure under the front incident light condition; the first response spectrum records the light transmittance or light absorptivity at each wavelength point within the 300-1100nm wavelength range, with a spectral resolution of 1-5nm.
[0115] A second incident light of the same wavelength as the first incident light is applied from the back side of the composite film substrate: the first light source is turned off, and the second light source is turned on. The second light source and the first light source are the same type of xenon lamp or halogen tungsten lamp, with the same output wavelength of 300-1100nm. The light intensity is adjusted so that the power density of the back incident light is the same as that of the front incident light, both being 80-120mW / cm². The angle between the incident direction of the beam and the normal to the substrate surface is 0°, and the beam is incident perpendicularly. After the light intensity stabilizes, the transmitted light is collected using a back-side spectral receiver to obtain the second response spectrum of the double-sided electrode structure under the back-side incident light condition. The second response spectrum records the light transmittance or light absorptivity at each wavelength point in the 300-1100nm wavelength range, with a spectral resolution of 1-5nm.
[0116] The first response spectrum and the second response spectrum are compared, and the spectral response difference between the two at each wavelength point is calculated to obtain the difference spectral curve. At the same wavelength point, the difference between the transmittance value of the first response spectrum and the transmittance value of the second response spectrum is calculated as the spectral response difference value at that wavelength point. All wavelength points in the 300-1100nm band are traversed, and the spectral response difference values of each wavelength point are connected in wavelength order to form the difference spectral curve. The horizontal axis of the difference spectral curve is wavelength, and the vertical axis is the transmittance difference between the front and back sides.
[0117] The difference spectral curves are subjected to amplitude feature extraction and waveform feature extraction: amplitude features include the maximum difference amplitude and average difference amplitude of the difference spectral curves in the visible light band (380-780nm) and near-infrared band (780-1100nm); waveform features include the number of extreme points, the location of extreme points, and the monotonicity trend of the curves in the visible light band and near-infrared band.
[0118] Based on the amplitude and waveform characteristics of the difference spectral curves, the selective response characteristics of the double-sided electrode structure to incident light from both sides are determined: if the maximum difference amplitude of the difference spectral curve in the visible light band is greater than the maximum difference amplitude in the near-infrared band, it indicates that the selective response difference of the double-sided electrode structure to incident light from both sides is significant in the visible light band and relatively small in the near-infrared band; if the difference spectral curve exhibits multiple extreme points and drastic fluctuations in both the visible and near-infrared bands, it indicates that the double-sided electrode structure exhibits selective response differences between the front and back sides in multiple wavelength regions. The selective response characteristics of the double-sided electrode structure to incident light from both sides are thus determined.
[0119] This embodiment applies incident light of the same wavelength and power density to the front and back sides of the composite film substrate, respectively, collects the transmission spectra of the two sides, and calculates the transmittance difference at each wavelength point to form a difference spectral curve. Furthermore, it extracts the amplitude and waveform characteristics of the difference spectral curve in the visible and near-infrared bands, realizing the quantitative characterization of the optical response difference between the front and back sides of the double-sided electrode structure, and providing a basis for determining the target optical parameters of the subsequent color rendering control layer.
[0120] Specifically, in step S6, determining the target optical parameters of the color rendering control layer based on the selective response characteristics includes:
[0121] Obtain a preset visual consistency target, and convert the visual consistency target into a target chromaticity value range for the front and back color display effects;
[0122] Using the selective response characteristics as the initial input and the target chromaticity range as the optimization objective, the combined solution of the film thickness, refractive index and extinction coefficient of the color rendering control layer is solved in reverse iteration through an optical inverse design model, and the solution is used as the target optical parameter.
[0123] In this embodiment, a preset visual consistency target is obtained: the visual consistency target is that the final membrane material presents the same or similar color rendering effect when viewed from the front and back, specifically manifested as a color difference ΔEab between the front and back color rendering values being less than or equal to 3.0; the visual consistency target is converted into a target chromaticity value range for the front and back color rendering effects, that is, the front and back color rendering values both fall within the same preset chromaticity interval, the center value of the preset chromaticity interval is the target chromaticity coordinate, and the radius of the interval corresponds to a tolerance range of color difference ΔEab ≤ 3.0. The target chromaticity coordinate is determined according to the final appearance color of the membrane material required by the architectural design, specifically by measuring a standard color swatch with a colorimeter or by determining the corresponding chromaticity coordinate value in the CIE 1931 chromaticity diagram according to the Pantone color card code.
[0124] The selective response characteristics determined in step S5 are used as the initial input to the optical inverse design model: the difference spectral curve data, amplitude characteristics, and waveform characteristics in the selective response characteristics are input into the optical inverse design model; the optical inverse design model is established based on the transfer matrix method and is used to calculate the optical response of the multilayer film structure under different incident conditions on both sides. The target chromaticity value range is used as the optimization objective: the target chromaticity value range is input into the optical inverse design model as the convergence condition for iterative solution.
[0125] The combined solution of the film thickness, refractive index, and extinction coefficient of the color rendering control layer is obtained through reverse iterative solution using an optical inverse design model. In this model, the adjustable parameters of the color rendering control layer are set as film thickness, real part of refractive index, and extinction coefficient. The search range for each parameter is: film thickness 50-500 nm, real part of refractive index 1.3-2.5, and extinction coefficient 0-0.5. The optical inverse design model employs a genetic algorithm, using the color difference between the color rendering chromaticity values of the front and back sides of the superimposed color rendering control layer and the double-sided electrode structure and the target chromaticity value range as the fitness function. The algorithm iteratively solves the problem within the search range. When the fitness function value, i.e., the color difference value, converges to below a preset threshold, the iteration stops, and the combined solution of the current film thickness, refractive index, and extinction coefficient is output as the target optical parameters of the color rendering control layer. The preset threshold is determined based on the human eye's resolution limit for color difference. When the color difference value ΔEab is less than or equal to 3.0, the human eye has difficulty distinguishing color differences; therefore, the preset threshold is set to a color difference value ΔEab ≤ 3.0.
[0126] Specifically, in step S6, a color development control layer is prepared on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer according to the target parameters, including:
[0127] Based on the refractive index, extinction coefficient, and film thickness of the target optical parameters, determine the difference in the anisotropic optical response of the color rendering control layer in the two directions.
[0128] Based on the difference in the anisotropic optical response of the target, the field strength and direction of the electric field-assisted deposition are determined;
[0129] During the deposition of the color development control layer material, an electric field with the specified strength and direction is applied to the color development control layer, causing the color development control layer material to align in the direction of the electric field.
[0130] After curing, a colorimetric control layer is formed that has an anisotropic optical response that matches the difference value of the anisotropic optical response of the target.
[0131] Specifically, determining the field strength and direction for electric field-assisted deposition includes:
[0132] Based on the target anisotropic refractive index target value and the target anisotropic extinction coefficient target value in the target anisotropic optical response difference value, calculate the equivalent dielectric constant tensor corresponding to the color rendering control layer material when it is arranged in different directions;
[0133] Substituting the equivalent dielectric constant tensor into the electric field-dipole moment coupling model, we can inversely deduce the dipole moment orientation distribution required for the color rendering control layer material to achieve the target values of refractive index anisotropy and extinction coefficient anisotropy.
[0134] Based on the dipole moment orientation distribution, the electric field strength and direction applied during the deposition process are determined.
[0135] In this embodiment, based on the refractive index, extinction coefficient, and film thickness in the target optical parameters, the difference value of the target anisotropic optical response of the color rendering control layer in the two directions is determined. Specifically, the real part of the refractive index, extinction coefficient, and film thickness in the target optical parameters are decomposed into components perpendicular to the film surface and components parallel to the film surface, respectively. The difference between the real parts of the refractive index in the perpendicular direction and the component parallel to the film surface, as well as the difference between the extinction coefficients in the perpendicular direction and the component parallel to the film surface, are calculated. The two differences are used to characterize the difference value of the target anisotropic optical response of the color rendering control layer in the two directions.
[0136] Based on the target anisotropic optical response difference value, the field strength and direction of electric field-assisted deposition are determined. Specifically, based on the target anisotropic refractive index and extinction coefficient anisotropic target values in the target anisotropic optical response difference value, the equivalent dielectric constant tensor corresponding to the molecular arrangement of the color development control layer material along different directions is calculated. The equivalent dielectric constant tensor is calculated as follows: the dielectric constant of the color development control layer material arranged along the long axis and the dielectric constant of the material arranged along the short axis are calculated separately to form the equivalent dielectric constant tensor; wherein, the dielectric constants along the long axis and the short axis are obtained by calculating the refractive index and extinction coefficient of the color development control layer material in the corresponding directions.
[0137] Substituting the equivalent dielectric constant tensor into the electric field-dipole moment coupling model, the dipole moment orientation distribution required for the color development control layer material to achieve the target anisotropic optical response difference value is deduced. Specifically, the electric field-dipole moment coupling model describes the orientation distribution of the dipole moment of the color development control layer material under the action of an applied electric field. This model consists of the dipole moment orientation probability density distribution function, the magnitude of the dipole moment, the electric field strength, and the deposition temperature. The equivalent dielectric constant tensor is matched with the dielectric constant tensor when the color development control layer material molecules are arranged in different directions. The macroscopic optical response when the color development control layer material molecules are arranged in a certain direction depends on the closeness of the equivalent dielectric constant in that direction to the target dielectric constant. By calculating the contribution of the color development control layer material molecules to the equivalent dielectric constant tensor when arranged in different directions, the dipole moment orientation distribution required for the equivalent dielectric constant tensor to reach the target value is deduced.
[0138] Based on the dipole moment orientation distribution, the electric field strength and direction applied during the deposition process are determined. Specifically, the back-derived dipole moment orientation distribution is matched with the dipole moment orientation distribution expression in the electric field-dipole moment coupling model, and the electric field strength required to make them consistent is calculated. When the dipole moment orientation distribution is characterized by orientation angles concentrated in a small angle range, it indicates that the color control layer material molecules need to be highly oriented, and a larger electric field strength is required. When the dipole moment orientation distribution is characterized by orientation angles distributed over a wider angle range, a smaller electric field strength is required. Based on the calculated electric field strength and combined with the preferred orientation directions required for both the front and back color control layers, the electric field directions during the deposition of the front color control layer and the back color control layer are determined respectively.
[0139] During the deposition of the color development control layer material, an electric field with the specified field strength and direction is applied to the color development control layer: while coating the color development control layer material on the upper surface of the transparent top electrode layer, a parallel electric field perpendicular to the coating direction is applied on both sides of the coating area, and the electric field strength is the field strength determined according to the above steps; or parallel electrode plates are respectively set on the upper and lower sides of the substrate, and a perpendicular electric field is applied in the direction normal to the substrate, and the electric field strength is the field strength determined according to the above steps.
[0140] After coating, the color development control layer is cured under a continuously applied electric field, causing the color development control layer material to be oriented and fixed along the direction of the electric field. After curing, an anisotropic optical response with a value matching the difference in anisotropic optical response of the target is formed on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer.
[0141] This embodiment quantifies the difference in anisotropic optical response between the front and back sides of the color development control layer by decomposing the refractive index, extinction coefficient, and film thickness in the target optical parameters into components in the vertical and parallel directions and calculating the difference. Then, the required dipole moment orientation distribution is inversely deduced by calculating the equivalent dielectric constant tensor and the electric field-dipole moment coupling model, and finally the field strength and direction of electric field-assisted deposition are determined, realizing the quantitative conversion of the target optical parameters of the color development control layer to electric field deposition parameters. During the deposition process, a determined electric field is applied to orient the color development material along the electric field direction and solidify it, so that the color development control layer has an anisotropic optical response that matches the difference value of the target anisotropic optical response, thereby achieving precise control and consistent matching of the color development effect on both sides.
[0142] Specifically, in step S7, the double-sided self-displaying photovoltaic smart building membrane material obtained after encapsulation includes:
[0143] The formed photovoltaic device structure is laminated and encapsulated, and then bi-sided power generation performance and bi-sided color rendering effect are tested.
[0144] When both power generation performance and color rendering performance are qualified, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained;
[0145] When only the color development performance is unsatisfactory, the color development control layer should be re-prepared.
[0146] When the power generation performance is unqualified, the substrate is discarded.
[0147] Specifically, when re-preparing the color development control layer, the target optical parameters are corrected based on the test results of the double-sided color development effect, and the color development control layer is re-prepared with the corrected target optical parameters.
[0148] In this embodiment, the formed photovoltaic device structure is laminated and encapsulated: the photovoltaic device structure obtained in step S6 is placed in a vacuum laminator, a first encapsulating film is covered on the upper surface of the photovoltaic device structure, and a second encapsulating film is covered on the lower surface of the composite film substrate. The first encapsulating film and the second encapsulating film are each independently selected from one of ethylene-vinyl acetate copolymer film, polyvinyl butyral film, or polyolefin elastomer film, and the thickness of the encapsulating film is 100-500μm; a first backplate is covered on the upper surface of the first encapsulating film, and a second backplate is covered on the lower surface of the second encapsulating film. The first backplate and the second backplate are each independently selected from one of tempered glass, transparent polymer sheet, or flexible polymer film; the assembled laminated structure is fed into the vacuum laminator, the vacuum degree is 10-100Pa, the lamination temperature is 120-160℃, the lamination pressure is 0.05-0.2MPa, and the lamination time is 10-30min; after lamination, it is naturally cooled to room temperature to obtain the encapsulated finished film material.
[0149] After encapsulation, double-sided power generation performance and double-sided color rendering effect tests were conducted. The double-sided power generation performance test involved placing the encapsulated finished film material under a solar simulator. The output spectrum of the solar simulator was the AM1.5G standard spectrum, and the irradiance was 1000 W / m². First, the front side of the finished film material was irradiated, and the power generation efficiency under front irradiation conditions was recorded. Then, the back side of the finished film material was irradiated, and the power generation efficiency under back irradiation conditions was recorded. The ratio of the front power generation efficiency to the back power generation efficiency was calculated. The double-sided color rendering effect test involved measuring the colorimetric values from both the front and back sides of the finished film material using a spectrophotometer or colorimeter. The colorimetric values from the front and back sides were recorded, and the color difference between the front and back colorimetric values was calculated.
[0150] Determine whether the performance is qualified: when the ratio of the front power generation efficiency to the back power generation efficiency is within the preset balance range, and the color difference value between the front color rendering chromaticity value and the back color rendering chromaticity value is less than or equal to the preset color difference threshold, it is determined that both the power generation performance and the color rendering performance are qualified, and the bifacial self-color-rendering photovoltaic power generation intelligent building membrane material is obtained. The preset balance range is 0.85-1.15, that is, the deviation between the front power generation efficiency and the back power generation efficiency does not exceed ±15%. When the ratio of the front power generation efficiency to the back power generation efficiency is within the preset balance range, but the color difference value between the front color rendering chromaticity value and the back color rendering chromaticity value is greater than the preset color difference threshold, it is determined that only the color rendering performance is unqualified, and the process returns to step S6 to re-prepare the color rendering regulation layer. When the ratio of the front power generation efficiency to the back power generation efficiency exceeds the preset balance range, it is determined that the power generation performance is unqualified, and regardless of whether the color rendering performance is qualified or not, the finished membrane material is rejected and will not be used subsequently.
[0151] When re-preparing the color rendering regulation layer, the target optical parameters are corrected according to the test result of the bifacial color rendering effect: the difference between the front color rendering chromaticity value and the back color rendering chromaticity value measured in the bifacial color rendering effect test is taken as the feedback quantity, and the film thickness, refractive index and extinction coefficient in the target optical parameters are adjusted to make the color difference value of the front and back color rendering effects corresponding to the corrected target optical parameters smaller; the color rendering regulation layer is re-prepared with the corrected target optical parameters.
[0152] In this embodiment, the photovoltaic device structure is encapsulated and protected by a vacuum lamination encapsulation process, and the bifacial power generation performance test and the bifacial color rendering effect test are performed synchronously after encapsulation. Taking that the ratio of the front power generation efficiency to the back power generation efficiency is within the preset balance range and the color difference value of the front and back color rendering chromaticity is less than or equal to the preset threshold as the qualification judgment standard, the collaborative verification of the dual indicators of power generation performance and color rendering performance is realized; when only the color rendering performance is unqualified, the measured front and back color rendering chromaticity difference is used as the feedback quantity to correct the target optical parameters and then re-prepare the color rendering regulation layer, and when the power generation performance is unqualified, the base material is directly rejected, which avoids invalid rework and improves the finished product qualification rate and production efficiency.
[0153] The bifacial self-color-rendering photovoltaic power generation intelligent building membrane material is prepared according to steps S1 to S7 of this embodiment, which is denoted as sample A (the invention group). A control sample B is set: the same flexible polymer substrate and optical regulation layer as those of sample A are adopted, but the differential regulation of the electrode deposition parameters according to the detection result of the surface energy trap density in step S2 and step S3 is skipped, that is, the electrodes on the front and back sides are prepared with the same deposition supersaturation and the same deposition temperature gradient; the remaining steps (including the bifacial illumination response detection in step S5 and the preparation of the color rendering regulation layer in step S6) are completely the same as those of sample A.
[0154] Samples A and B were placed under a solar simulator with an output spectrum of AM1.5G standard and an irradiance of 1000 W / m². The front side of the samples was irradiated first, and the power generation efficiency η_front was recorded. The back side of the samples was then irradiated, and the power generation efficiency η_back was recorded. The bifacial power generation efficiency ratio R = η_back / η_front was calculated. A value closer to 1.0 indicates a more balanced power generation performance on both sides.
[0155] The colorimetric values of the sample were measured from both the front and back sides using a spectrophotometer. The colorimetric coordinates of the front and back sides were recorded, and the color difference ΔEab between the two values in the CIE 1931 colorimetric diagram was calculated. When ΔEab ≤ 3.0, the color difference is difficult for the human eye to distinguish, indicating that the color rendering effect is consistent on both sides.
[0156] Test results:
[0157] Table 1
[0158] Results Analysis: Comparison of Bifacial Power Generation Performance: The bifacial power generation efficiency ratio R of sample A is 0.91, within the preset equilibrium range of 0.85-1.15; while the R of the control group sample B is 0.84, exceeding the lower limit of the preset equilibrium range. This indicates that differential control of electrode deposition parameters without surface energy trap density detection will lead to significant differences in nucleation density and grain orientation between the front and back electrode layers, resulting in a significantly lower power generation efficiency on the back side than on the front side, leading to an imbalance in bifacial power generation performance. Related studies also indicate that the key to balancing the performance of bifacial photovoltaic devices lies in the optical matching of the front and back electrode structures.
[0159] Comparison of color rendering consistency on both sides: The color difference value ΔEab of sample A on both sides is 1.8, which is lower than the human eye's color difference resolution limit of 3.0, indicating visual consistency in color rendering on both sides. However, the ΔEab value of control sample B is 4.7, which exceeds the acceptable range for the human eye, showing a significant visual difference in color rendering on both sides. This indicates that even though the control group also used double-sided illumination response detection and optical inverse design model to determine the color rendering layer parameters, the lack of pre-equalization control of the intrinsic optical response of the double-sided electrode structure made it difficult for the color rendering layer to compensate for excessive intrinsic differences, resulting in failure of color rendering consistency.
[0160] The results of the above comparative experiments show that by linking the detection of the energy trap density on the substrate surface with the electrode deposition parameters, the present invention reduces the intrinsic optical response difference of the bifacial electrode structure from the source, enabling the color rendering layer to effectively compensate for the residual difference in subsequent design, and ultimately achieving a synergistic match between bifacial power generation performance (bifacial efficiency ratio 0.91, control group 0.84) and bifacial color rendering effect (color difference ΔEab=1.8, control group 4.7).
[0161] The technical solution of the present invention has been described above with reference to the preferred embodiments shown in the accompanying drawings. However, it will be readily understood by those skilled in the art that the scope of protection of the present invention is obviously not limited to these specific embodiments. Without departing from the principles of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will all fall within the scope of protection of the present invention.
Claims
1. A preparation method of a double-sided self-luminous photovoltaic power generation intelligent building membrane material, characterized in that, include: Step S1: Provide a flexible polymer substrate, and form an optical control layer on the flexible polymer substrate to obtain a composite film substrate layer; Step S2: Surface energy trap density is detected on the composite membrane substrate to obtain the surface energy trap density distribution on both sides of the composite membrane substrate and the ratio of the polar to non-polar components of the surface free energy. Step S3: Determine the initial deposition supersaturation of the top electrode layer prepared on the photovoltaic functional layer and the back electrode layer prepared on the lower surface of the composite film substrate layer according to the surface energy trap density distribution, and determine the deposition temperature gradient of the top electrode layer and the back electrode layer according to the ratio of the polar component to the non-polar component. Step S4: A transparent top electrode layer is prepared on the photovoltaic functional layer according to the deposition parameters, and a back electrode layer is prepared on the lower surface of the composite film substrate layer to form a double-sided electrode structure. Step S5: Perform double-sided illumination response detection on the double-sided electrode structure. Apply incident light of a preset wavelength from the front and back sides of the composite film substrate layer respectively, and obtain the response spectrum of the double-sided electrode structure under the front and back incident light conditions. Determine the selective response characteristics of the double-sided electrode structure to the front and back incident light based on the degree of difference between the two response spectra. Step S6: Determine the target optical parameters of the color development control layer based on the selective response characteristics, and prepare the color development control layer on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer based on the target parameters; Step S7: After encapsulation, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained.
2. The method of claim 1, wherein the method further comprises: In step S2, the surface energy trap density of the composite film substrate is detected, including: Dynamic contact angle measurements were performed on the front and back sides of the composite membrane substrate to obtain the forward contact angle and backward contact angle values at each detection point, and the contact angle hysteresis value at each detection point was calculated. Based on the contact angle hysteresis values at each detection point, the average contact angle hysteresis and the dispersion of the contact angle hysteresis distribution on the front and back sides of the composite film substrate are calculated. The average contact angle hysteresis is used to characterize the magnitude of the surface energy trap density, and the dispersion of the contact angle hysteresis distribution is used to characterize the in-plane distribution uniformity of the surface energy trap density. The contact angles of at least two polarity test liquids were measured at each detection point. The polar and non-polar components of the surface free energy at each detection point were calculated using a surface free energy separation model to obtain the ratio of the polar to non-polar components of the surface free energy on both sides of the composite membrane substrate.
3. The method of claim 1, wherein the method further comprises: In step S3, the initial deposition supersaturation is determined, including: The reference values for the initial deposition supersaturation of the transparent top electrode layer and the back electrode layer are determined based on the average contact angle hysteresis value. The in-plane compensation coefficient for the initial deposition supersaturation is determined based on the dispersion of the contact angle hysteresis distribution. The initial deposition supersaturation is obtained by correcting the reference value with the in-plane compensation coefficient.
4. The method of claim 1, wherein the method further comprises: In step S3, the deposition temperature gradient is determined, including: The directional configuration of the deposition temperature gradient of the transparent top electrode layer and the back electrode layer is determined based on the difference between the ratio of the polar to the non-polar components of the surface free energy on both sides of the composite film substrate. When the difference is greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in opposite directions; When the difference is not greater than a preset direction threshold, the deposition temperature gradient of the transparent top electrode layer and the deposition temperature gradient of the back electrode layer are configured to be in the same direction but with different amplitudes.
5. The method of claim 1, wherein the method further comprises: In step S5, the double-sided electrode structure is subjected to double-sided illumination response detection, including: A first incident light of a preset wavelength is applied to the front side of the composite film substrate, and the first response spectrum of the double-sided electrode structure under the front incident light condition is collected. A second incident light of the same wavelength as the first incident light is applied from the back side of the composite film substrate, and the second response spectrum of the double-sided electrode structure under the back incident light condition is collected. The first response spectrum is compared with the second response spectrum, and the difference in spectral response between the two at each wavelength is calculated to obtain the difference spectral curve. Based on the amplitude and waveform characteristics of the difference spectral curves, the selective response characteristics of the double-sided electrode structure to incident light from both sides are determined.
6. The method of claim 1, wherein the method further comprises: In step S6, the target optical parameters of the color rendering control layer are determined based on the selective response characteristics, including: Obtain a preset visual consistency target, and convert the visual consistency target into a target chromaticity value range for the front and back color display effects; Using the selective response characteristics as the initial input and the target chromaticity range as the optimization objective, the combined solution of the film thickness, refractive index and extinction coefficient of the color rendering control layer is solved in reverse iteration through an optical inverse design model, and the solution is used as the target optical parameter.
7. The method of claim 1, wherein the method further comprises: In step S6, a color development control layer is prepared on the upper surface of the transparent top electrode layer and / or the lower surface of the composite film substrate layer according to the target parameters, including: Based on the refractive index, extinction coefficient, and film thickness of the target optical parameters, determine the difference in the anisotropic optical response of the color rendering control layer in the two directions. Based on the difference in the anisotropic optical response of the target, the field strength and direction of the electric field-assisted deposition are determined; During the deposition of the color development control layer material, an electric field with the specified strength and direction is applied to the color development control layer, causing the color development control layer material to align in the direction of the electric field. After curing, a colorimetric control layer is formed that has an anisotropic optical response that matches the difference value of the anisotropic optical response of the target.
8. The method of claim 7, wherein the method further comprises: Determine the field strength and direction for electric field-assisted deposition, including: Based on the target anisotropic refractive index target value and the target anisotropic extinction coefficient target value in the target anisotropic optical response difference value, calculate the equivalent dielectric constant tensor corresponding to the color rendering control layer material when it is arranged in different directions; Substituting the equivalent dielectric constant tensor into the electric field-dipole moment coupling model, we can inversely deduce the dipole moment orientation distribution required for the color rendering control layer material to achieve the target values of refractive index anisotropy and extinction coefficient anisotropy. Based on the dipole moment orientation distribution, the electric field strength and direction applied during the deposition process are determined.
9. The method for preparing double-sided self-displaying photovoltaic power generation smart building membrane material according to claim 1, characterized in that, In step S7, the double-sided self-displaying photovoltaic smart building membrane material is obtained after encapsulation, comprising: The formed photovoltaic device structure is laminated and encapsulated, and then bi-sided power generation performance and bi-sided color rendering effect are tested. When both power generation performance and color rendering performance are qualified, the double-sided self-displaying photovoltaic power generation smart building membrane material is obtained; When only the color development performance is unsatisfactory, the color development control layer should be re-prepared. When the power generation performance is unqualified, the substrate is discarded.
10. The method for preparing double-sided self-displaying photovoltaic power generation smart building membrane material according to claim 9, characterized in that, When re-preparing the color development control layer, the target optical parameters are corrected based on the double-sided color development effect test results, and the color development control layer is re-prepared with the corrected target optical parameters.
Citation Information
Patent Citations
A method for preparing a cast film, the cast film obtained by the method, and its applications.
CN115923212B