Display panel and method for manufacturing a mother panel thereof

By creating multi-level stepped sections in the cutting area of ​​the display panel and utilizing the difference in light transmittance of the mask, the problems of inorganic film layer crack risk and high cost and complexity are solved, thereby improving the reliability and production capacity of the display panel.

CN123124603APending Publication Date: 2026-11-17BOE TECHNOLOGY GROUP CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611517497.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-28
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the existing technology, during the manufacturing process of display panels, the inorganic film layer extends from the module cutting channel to the module cutting channel, which makes it easy for cracks to occur during laser cutting. In addition, the existing process is complex and the material cost is high, which restricts production capacity.

Method used

By employing a multiple exposure and development method, multi-level steps are formed in the inorganic layer of the cutting zone. Utilizing the difference in light transmittance of the photomask, multi-level etching is achieved through a single photomask, reducing the number of exposure and development cycles, avoiding inorganic layer residue and cracks, and simplifying the process flow.

Benefits of technology

This effectively prevents laser cutting stress from extending to the display area, improving the reliability of the display panel, reducing material costs, simplifying the process, and increasing production capacity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124603A_ABST
    Figure CN123124603A_ABST
Patent Text Reader

Abstract

The application relates to the technical field of display, and particularly provides a display panel and a preparation method of a mother board thereof. The method comprises the following steps: forming at least one display panel area and a cutting channel area surrounding the display panel area on a substrate of the mother board, the display panel area comprising a display area and an edge area surrounding the display area, and the cutting channel area comprising an inorganic layer arranged in the same layer as the display panel area; and forming M step parts in the inorganic layer on the side of the cutting line of the cutting channel area facing the edge area through N times of exposure and development, wherein N < M, and a mask plate used at least once in the N times of exposure and development comprises a plurality of opening areas arranged from inside to outside, and the light transmittance of an inside opening area in adjacent opening areas is smaller than that of an outside opening area. The application can reduce the number of times of exposure and development, reduce the number of mask plates used, simplify the process flow, and improve the production capacity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of display technology. More specifically, it relates to a method for manufacturing a display panel and its motherboard. Background Technology

[0002] Currently, during the manufacturing process of display products, the inorganic film layer formed by chemical vapor deposition extends from the module display area to the module dicing line (MDL). The inorganic film layer formed on the module dicing line is prone to cracking during subsequent laser cutting.

[0003] To mitigate this risk, the inorganic layer inside the cutting line is typically formed with multiple steps. Related technologies require an exposure and development process for each step, resulting in high material costs and a complex process, which limits production capacity. Summary of the Invention

[0004] The purpose of this invention is to provide a method for preparing a motherboard for a display panel and a method for preparing a display panel, so as to solve at least one of the problems existing in the prior art.

[0005] To achieve the above objectives, the present invention adopts the following technical solution: The first aspect of the present invention provides a method for preparing a motherboard for a display panel, comprising: At least one display panel area and a cleaving channel area surrounding the display panel area are formed on the substrate of the motherboard. The display panel area includes a display area and an edge area surrounding the display area. The cleaving channel area includes an inorganic layer disposed in the same layer as the display panel area. M stepped portions are formed in the inorganic layer on the side of the cutting line towards the edge region by N exposures and developments, where N < M. The mask used at least once in the N exposures and developments includes multiple opening regions arranged from the inside to the outside, and the light transmittance of the inner opening region among adjacent opening regions is less than that of the outer opening region.

[0006] Optionally, in adjacent opening areas, the light transmittance of the material in the inner opening area is less than that in the outer opening area.

[0007] Optionally, the opening area includes an array of opening patterns, wherein the total opening area of ​​the opening patterns in the inner opening area is smaller than that in the outer opening area among adjacent opening areas.

[0008] Optionally, the inorganic layer includes a first inorganic encapsulation layer, a second inorganic encapsulation layer, and a touch insulating layer stacked on the substrate.

[0009] Optionally, after N exposures and developments, the substrate at the dicing line is exposed by the inorganic layer.

[0010] Optionally, forming three stepped portions in the inorganic layer on the side of the cutting line towards the edge region by two exposures and development includes: Two stepped portions are formed in the inorganic layer on the side of the dicing line towards the edge region during the first exposure and development. The mask used in the first exposure and development includes a first opening region and a second opening region arranged from the edge region towards the dicing region. The mask used in the first exposure and development simultaneously performs the first etching and the second etching. The second opening region corresponds to the common etching region of the first and second etching processes, and the first opening region corresponds to the first etching process. Afterwards... A second exposure and development is performed using a mask that performs the third etching, forming three stepped sections in the inorganic layer on the side of the cutting line in the cutting zone facing the edge region.

[0011] Optionally, forming three stepped portions in the inorganic layer on the side of the cutting line towards the edge region by two exposures and development includes: Two stepped portions are formed in the inorganic layer on the side of the dicing line towards the edge region during the first exposure and development. The mask used in the first exposure and development includes a third opening region and a fourth opening region arranged from the edge region towards the dicing region. The mask used in the first exposure and development simultaneously performs the first etching and the third etching. The fourth opening region corresponds to the common etching region of the first and third etching processes, and the third opening region corresponds to the first etching process. Afterwards... A second exposure and development is performed using a mask that performs the second etching, forming three stepped sections in the inorganic layer on the side of the cutting line in the cutting zone facing the edge region.

[0012] Optionally, the etching range of the second etching is larger than the etching range of the third etching.

[0013] Optionally, forming three stepped portions in the inorganic layer on the side of the cutting line towards the edge region by a single exposure and development includes: The first etching, second etching, and third etching are performed simultaneously using a mask plate, wherein the mask plate includes a fifth opening area, a sixth opening area, and a seventh opening area arranged from the edge area toward the cutting channel area; the seventh opening area corresponds to the common etching area for the first etching, the second etching, and the third etching, the sixth opening area corresponds to the second etching, and the fifth opening area corresponds to the first etching.

[0014] A second aspect of the present invention provides a method for preparing a display panel, comprising: forming a mother plate using the preparation method provided in the first aspect of the present invention; and cutting along a cutting line in a cutting channel area to obtain a display panel.

[0015] The beneficial effects of this invention are as follows: In the method for preparing the motherboard of the display panel provided in this application, the light transmittance of the inner opening area of ​​the mask is less than that of the outer opening area. A step is formed in the inorganic layer on the side of the cutting line facing the edge area in the cutting channel area. The step reduces the overall slope angle of the inorganic layer, avoids the residue of the inorganic layer near the cutting line, and further avoids the extension of laser cutting stress to the display area, thereby improving the reliability of the display panel. By utilizing the light transmittance difference of multiple opening areas of the mask, a multi-level etching step is formed by a single exposure and development, so that the number of exposure and development times N is less than the number of step sections M. In other words, this application can reproduce multiple etching effects that require multiple mask stacks in the prior art by using a single mask. This reduces the number of masks used, thereby reducing material costs, simplifying the process flow, and increasing production capacity. Attached Figure Description

[0016] The specific embodiments of the present invention will be described in further detail below with reference to the accompanying drawings.

[0017] Figure 1 A flowchart illustrating a method for preparing a motherboard for a display panel according to an embodiment of the present invention is shown.

[0018] Figure 2 A plan view of the motherboard of the display panel provided in Embodiment 1 of the present invention is shown; Figure 3 for Figure 2 Cross-sectional view of region F within the Chinese square frame; Figure 4 This diagram shows the structure of the mask used in the first exposure and development of Embodiment 1 of the present invention. Figure 5 This diagram illustrates a structural schematic of the opening pattern of the mask plate in Embodiment 1 of the present invention. Figure 6 This diagram illustrates another structural schematic of the opening pattern of the mask plate in Embodiment 1 of the present invention; Figures 7 to 8 The diagram shows cross-sectional schematics of each stage in the fabrication process of the motherboard for the display panel provided in Embodiment 1 of the present invention. Figure 9 This diagram shows the structure of the mask used in the first exposure and development of Embodiment 2 of the present invention. Figures 10 to 11 The diagram shows cross-sectional schematics of each stage in the fabrication process of the motherboard for the display panel provided in Embodiment 2 of the present invention. Figure 12 This diagram shows a schematic of the structure of the mask used in the exposure and development process of Embodiment 3 of the present invention. Figure 13 This diagram shows a cross-sectional view of the motherboard of the display panel provided in Embodiment 3 of the present invention during its fabrication process. Detailed Implementation

[0019] In this invention, "on," "formed on," and "set on" can mean that one layer is directly formed or set on another layer, or that one layer is indirectly formed or set on another layer, meaning that there are other layers between the two layers.

[0020] It should be noted that although the terms "first," "second," etc., may be used herein to describe various components, members, elements, regions, layers, and / or portions, these components, members, elements, regions, layers, and / or portions should not be limited by these terms. Rather, these terms are used to distinguish one component, member, element, region, layer, and / or portion from another. Thus, for example, the first component, first member, first element, first region, first layer, and / or first portion discussed below may be referred to as a second component, second member, second element, second region, second layer, and / or second portion without departing from the teachings of the invention.

[0021] In related technologies, for extremely small display products, such as OLED (Organic Light-Emitting Diode) products smaller than 1 inch, when forming inorganic films using chemical vapor deposition (CVD), a window for forming the inorganic film needs to be defined by photolithography. This window is the CVD opening. If a conventional CVD opening design is used, the boundary of the CVD opening is essentially aligned with the boundary of the module display area, resulting in a small CVD opening size, leading to a thin inorganic film and poor film quality. Therefore, the design employs an outward expansion of the CVD opening, extending the inorganic film from the display area to the module dicing line (MDL), increasing the CVD opening size to ensure the thickness and quality of the inorganic film. After the CVD opening is expanded, an inorganic film will form on the module dicing line. During subsequent laser cutting, the inorganic film is prone to cracking, and these cracks extending further into the display area can affect the reliability of the display product.

[0022] Therefore, to avoid the risk of cracks caused by laser cutting, it is necessary to remove the inorganic film layer on the module cutting track. For example, the inorganic film layer on the module cutting track includes a stacked first inorganic film layer, a second inorganic film layer, and a third inorganic film layer. The steps for removing the inorganic film layer on the module cutting track include: performing a first etching process on the third inorganic film layer and a portion of the second inorganic film layer using a first mask to remove the third inorganic film layer and a portion of the second inorganic film layer; performing a second etching process on a portion of the second inorganic film layer and a portion of the first inorganic film layer using a second mask to remove the second inorganic film layer and a portion of the first inorganic film layer; and performing a second etching process on the first inorganic film layer using a third mask to remove the first inorganic film layer. It is evident that for different inorganic film layers, each etching requirement necessitates a separate etching process using a dedicated mask. This results in high material costs and a complex process flow, limiting production capacity.

[0023] In view of this, embodiments of the present invention provide a method for preparing a motherboard for a display panel, referring to... Figure 1 ,include: S1: At least one display panel area and a cleaving channel area surrounding the display panel area are formed on the substrate of the motherboard. The display panel area includes a display area and an edge area surrounding the display area. The cleaving channel area includes an inorganic layer disposed in the same layer as the display panel area. S2: M stepped portions are formed in the inorganic layer on the side of the cutting line towards the edge region by N exposures and developments, wherein N < M, and the mask used at least once in the N exposures and developments includes multiple opening regions arranged from the inside to the outside, and the light transmittance of the inner opening region among adjacent opening regions is less than that of the outer opening region.

[0024] In this embodiment, the transmittance of the inner opening area of ​​the mask is less than that of the outer opening area. A step is formed in the inorganic layer on the side of the cutting line facing the edge area in the cutting channel area. The step reduces the overall slope angle of the inorganic layer, avoids the residue of the inorganic layer near the cutting line, and further avoids the extension of laser cutting stress to the display area, thereby improving the reliability of the display panel. By utilizing the transmittance difference of multiple opening areas of the mask, a multi-level etching step is formed in a single exposure and development, so that the number of exposure and development N is less than the number of step M. In other words, this application can reproduce various etching effects that require multiple mask stacks in the prior art by using a single mask. This reduces the number of masks used, thereby reducing material costs, simplifying the process flow, and increasing production capacity.

[0025] It should be noted that the mask includes multiple opening areas arranged from the inside out, meaning that the multiple opening areas of the mask are arranged from the side near the edge area to the side near the dicing area; the light transmittance of the inner opening area among adjacent opening areas is less than that of the outer opening area, so that the light transmittance of the mask near the edge area is less than that of the mask near the dicing area. After exposure and development, the etching range of the inorganic layer near the edge area is smaller than that of the inorganic layer near the dicing area, so that a stepped portion is formed in the inorganic layer on the side of the dicing line facing the edge area, and M stepped portions are arranged from the dicing line towards the edge area.

[0026] The process of forming the inorganic layer in the dicing area and the display panel area includes chemical vapor deposition. The dicing area including the inorganic layer disposed in the same layer as the display panel area means that, during the formation of the inorganic layer, the inorganic layer extends from the display area through the edge area to the dicing area.

[0027] In one embodiment, after N exposures and developments, the substrate at the dicing line is exposed by the inorganic layer. During subsequent laser cutting along the dicing line, the laser energy acts on the substrate rather than the inorganic layer, preventing laser cutting stress from causing cracks in the inorganic layer.

[0028] In one embodiment, among adjacent opening areas, the material transmittance of the inner opening area is less than that of the outer opening area. That is, the material transmittance of the opening area on the side of the mask closer to the edge area is less than that of the opening area on the side closer to the cutting channel area.

[0029] In another embodiment, the opening region includes an array of opening patterns, wherein the total opening area of ​​the opening patterns in the inner opening region is smaller than that in the outer opening region. That is, the total opening area of ​​the opening patterns in the opening region near the edge of the mask is smaller than the total opening area of ​​the opening patterns in the opening region near the cutting channel region.

[0030] The method for preparing the motherboard of the display panel also includes: forming a touch metal layer on the inorganic layer of the display area; and forming an organic insulating layer on the touch metal layer.

[0031] The process sequence of forming the touch metal layer and the M steps on the inorganic layer of the display area can be adjusted according to actual needs. The step of forming the touch metal layer on the inorganic layer of the display area can be performed after forming the M steps or during forming the M steps. After forming the touch metal layer and the M steps on the inorganic layer of the display area, an organic insulating layer is formed on the touch metal layer.

[0032] The following describes the preparation method of the motherboard and the preparation method of the display panel provided in the embodiments of the present invention through several specific examples.

[0033] Example 1 Example 1 provides a method for preparing a motherboard for a display panel. For example... Figure 2 As shown, a display panel area A and a dicing area B surrounding the display panel area A are formed on the substrate of the motherboard. In this embodiment, the number of display panel areas A on the substrate of the motherboard is not limited, and can be 3 or 5. Figure 3 for Figure 2 The cross-sectional view of the frame region F shows that the dicing area B on the substrate 300 includes an inorganic layer 100 disposed on the same layer as the edge region C of the display panel region A.

[0034] In this embodiment, N is 2 and M is 3. The formation of three stepped portions in the inorganic layer 100 on the side of the cutting line towards the edge region C through two exposures and development includes: During the first exposure and development, two stepped portions are formed in the inorganic layer 100 on the side of the cutting line in the cutting zone B toward the edge zone C. (Referencing...) Figure 4 The mask 200 used in the first exposure and development includes a first opening region 220 and a second opening region 230 arranged from the edge region C toward the cutting track region B; the mask 200 used in the first exposure and development simultaneously performs the first etching and the second etching; the second opening region 230 corresponds to the common etching region of the first etching and the second etching, and the first opening region 220 corresponds to the first etching; subsequently, A second exposure and development is performed using a mask that performs the third etching, forming three stepped portions in the inorganic layer 100 on the side of the cutting line in the cutting zone B facing the edge zone C.

[0035] Specifically, the transmittance of the first opening region 220 is less than that of the second opening region 230; after the first exposure and development, the etching range of the inorganic layer 100 corresponding to the first opening region 220 is less than the etching range of the inorganic layer 100 corresponding to the first light-shielding region 210. The mask used for the second exposure and development performs a third etching at the common etching region corresponding to the second opening region 230, further removing the inorganic layer 100 in that region until the inorganic layer 100 exposes the substrate 300, forming three stepped portions on the inorganic layer 100 on the side of the cutting line in the dicing region B facing the edge region C.

[0036] In one embodiment, continue to refer to Figure 4 The mask 200 further includes: a first light-shielding area 210, with multiple opening areas located outside the first light-shielding area 210; and a second light-shielding area 240 located outside the multiple opening areas. In this embodiment, the first opening area 220 is located outside the first light-shielding area 210, and the second light-shielding area 240 is located outside the second opening area 230. This avoids etching of the film layer of other surrounding display panel areas A, improving the production yield of the display panel.

[0037] In one embodiment, the method for preparing the motherboard of the display panel further includes: forming a photoresist layer on the side of the inorganic layer 100 facing away from the substrate 300; exposing and developing the photoresist layer through a mask 200 to form a patterned photoresist layer on the side of the inorganic layer 100 facing away from the substrate 300; and etching the inorganic layer 100 using the patterned photoresist layer as a mask to form a step portion in the inorganic layer 100.

[0038] It should be noted that a photoresist layer needs to be formed on the side of the inorganic layer 100 facing away from the substrate 300 before each exposure and development. Utilizing the transmittance gradient of multiple opening regions on a single photomask, the residual thickness of various photoresist layers can be obtained in a single exposure and development. After the first exposure and development, the residual thickness of the photoresist layer corresponding to the second opening region 230 is less than the residual thickness of the photoresist layer corresponding to the first opening region 220, resulting in a larger etching range for the inorganic layer 100 corresponding to the second opening region 230 compared to the inorganic layer 100 corresponding to the first opening region 220.

[0039] In one embodiment, the material transmittance of the first opening region 220 is less than that of the second opening region 230, and the material transmittance of the first shading region 210 and the second shading region 240 is 0. For example, the mask 200 includes a halftone mask.

[0040] In another embodiment, the total opening area of ​​the opening pattern in the first opening region 220 is smaller than the total opening area of ​​the opening pattern in the second opening region 230, and the first light-shielding region 210 and the second light-shielding region 240 are not provided with opening patterns. For example, the mask 200 includes a grayscale mask.

[0041] In one embodiment, the size of the opening pattern of the second opening area 230 is smaller than the minimum resolution size of the exposure machine, which can achieve the effect that the exposure light partially passes through the mask and does not form an actual pattern on the inorganic layer 100. By adjusting the size of the opening pattern of the second opening area 230, the energy of the transmitted exposure light is controlled to achieve grayscale exposure.

[0042] In one embodiment, reference Figure 5 The opening pattern 400 is a strip-shaped opening pattern; for reference. Figure 6 The opening pattern 400 is a hole-shaped opening pattern. In other embodiments, the shape of the opening pattern is not limited.

[0043] It is known that the mask 200 includes a transparent substrate and a light-shielding film located on one side of the transparent substrate.

[0044] In this embodiment, the transmittance of the first light-shielding area 210 is 0. For a halftone mask, the material of the light-shielding film in the first light-shielding area 210 is chromium; for a grayscale mask, the light-shielding film in the first light-shielding area 210 has no opening pattern. After the first exposure and development, the photoresist layer corresponding to the first light-shielding area 210 is completely retained, and correspondingly, the inorganic layer 100 corresponding to the first light-shielding area 210 is also retained.

[0045] In other embodiments, the transmittance of the first light-shielding area 210 can also be a small non-zero value, so that the inorganic layer corresponding to the first light-shielding area 210 is etched in very small amounts, as long as the integrity of the inorganic layer in the edge area C is not affected.

[0046] In this embodiment, the transmittance of the second opening region 230 is 100%. That is, the second opening region 230 is a fully transparent area. For a halftone mask, the second opening region 230 only includes the transparent substrate and does not have a light-shielding film; for a grayscale mask, the opening pattern of the light-shielding film in the second opening region 230 is an overall opening, exposing the transparent substrate of the second opening region 230. After the first exposure and development, the photoresist layer corresponding to the second opening region 230 is completely removed, and correspondingly, the etching depth of the inorganic layer 100 corresponding to the second opening region 230 is the maximum.

[0047] In other embodiments, the transmittance of the second opening region 230 may also be a large value close to 100%, such as 99%, 98% or 97%.

[0048] In one embodiment, the transmittance of the first opening region 220 is between 0 and 100%, for example, 30%, 50%, or 80%. Exemplarily, the first opening region 220 is a semi-transparent region. For a halftone mask, the material of the light-shielding film of the first opening region 220 is chromium oxide or molybdenum oxide; for a grayscale mask, the light-shielding film of the first opening region 220 has a partially open pattern. After the first exposure and development, the photoresist layer corresponding to the first opening region 220 is partially removed, and correspondingly, the etching depth of the inorganic layer 100 corresponding to the first opening region 220 is then increased.

[0049] In other embodiments, the light transmittance of the first opening region 220 and the second opening region 230 are not limited, as long as the light transmittance of the first opening region 220 is less than that of the second opening region 230. The light transmittance of each opening region can be adjusted by adjusting the material of the light-shielding film and the total opening area of ​​the opening pattern.

[0050] In one embodiment, reference Figure 3The inorganic layer 100 includes a first inorganic encapsulation layer 110, a second inorganic encapsulation layer 120, and a touch insulating layer 130 stacked on the substrate. Specifically, the first inorganic encapsulation layer 110 extends from the display area through the edge area C to the cut-out area B, the second inorganic encapsulation layer 120 extends from the display area through the edge area C to the cut-out area B, and the touch insulating layer 130 extends from the display area through the edge area C to the cut-out area B.

[0051] The edge area of ​​the display panel area also includes: a barrier dam 500 located between the first inorganic encapsulation layer 110 and the substrate 300; and an organic encapsulation layer 600 located between the first inorganic encapsulation layer 110 and the second inorganic encapsulation layer 120, and located on the side of the barrier dam 500 facing the display area. The barrier dam 500 is used to block the flow of the organic encapsulation layer 600 during the formation of the organic encapsulation layer 600, preventing material of the organic encapsulation layer 600 from overflowing to the side of the barrier dam 500 away from the display area, thereby reducing the probability of encapsulation failure.

[0052] In one embodiment, the barrier 500 includes a first barrier 510 and a second barrier 520, with the second barrier 520 located on the side of the first barrier 510 facing the display area.

[0053] It is known that the first inorganic encapsulation layer 110, the second inorganic encapsulation layer 120, and the touch insulation layer 130 are stacked on the edge area C on the side of the barrier dam 500 away from the display area to the cutting channel area B.

[0054] In this embodiment, three stepped portions are formed between the first inorganic encapsulation layer 110, the second inorganic encapsulation layer 120, and the touch insulating layer 130 between the cutting line and the barrier dam 500 in the cutting channel area B. Exemplarily, the first etching removes the touch insulating layer 130 and a portion of the second inorganic encapsulation layer 120, forming a stepped portion between the touch insulating layer 130 and the second inorganic encapsulation layer 120. During the first etching, a portion of the second inorganic encapsulation layer 120 below the touch insulating layer 130 is over-etched to ensure the overlap between the touch layer in the display area and the source / drain metal layer, improving touch reliability. The second etching, after the first etching, removes a portion of the second inorganic encapsulation layer 120 and a portion of the first inorganic encapsulation layer 110. A step is formed between the mechanical packaging layer 120 and the first inorganic packaging layer 110. During the second etching, the portion of the first inorganic packaging layer 110 below the second inorganic packaging layer 120 is over-etched, reducing the subsequent etching time for the thicker first inorganic packaging layer 110 and ensuring uniform etching of the second and subsequent third etching. After the second etching, the third etching removes the remaining first inorganic packaging layer 110 until the substrate 300 is exposed, forming a step between the first inorganic packaging layer 110 and the substrate 300. Therefore, compared to the prior art which requires three masks to perform three etchings separately, this application utilizes the three opening areas of one mask 200 to simultaneously perform the first and second etchings through the first exposure and development, and uses another mask to perform the third etching through the second exposure and development. That is, three step portions can be formed by using two masks and two exposures and developments, reducing the use of one mask, shortening the process flow, and reducing material costs.

[0055] In one embodiment, the etching range of the second etching is greater than the etching range of the third etching. The etching range refers to the etching depth of the inorganic layer 100 and the etching width along the direction from the edge region C to the dicing region. Specifically, the etching widths of the second inorganic encapsulation layer 120 and the first inorganic encapsulation layer 110 removed after the second etching are both greater than the etching widths of the second inorganic encapsulation layer 120 and the first inorganic encapsulation layer 110 removed after the third etching, and the etching depth of the second inorganic encapsulation layer 120 and the first inorganic encapsulation layer 110 removed after the second etching is greater than the etching depth of the second inorganic encapsulation layer 120 and the first inorganic encapsulation layer 110 removed after the third etching.

[0056] refer to Figure 7 and Figure 8 This embodiment details the fabrication process of forming three stepped portions in the inorganic layer 100 on the side of the cutting line towards the edge region through two exposures and developments. The illustration is illustrated by the first light-shielding region 210 having a transmittance of 0%, the second opening region 230 having a transmittance of 100%, and the first opening region 220 having a transmittance between 0 and 100%.

[0057] refer to Figure 7 Two stepped portions are formed in the inorganic layer 100 on the side of the cutting line towards the edge B in the cutting zone C by the first exposure and development. Since the transmittance of the first light-shielding area 210 is 0, the inorganic layer 100 corresponding to the first light-shielding area 210 is retained, that is, the first inorganic encapsulation layer 110, the second inorganic encapsulation layer 120, and the touch insulating layer 130 corresponding to the first light-shielding area 210 are not etched; since the transmittance of the second opening area 230 is 100%, the etching depth of the inorganic layer 100 corresponding to the second opening area 230 is the largest, and the touch insulating layer 130, the second inorganic encapsulation layer 120, and part of the first inorganic encapsulation layer 110 corresponding to the second opening area 230 are etched away; since the transmittance of the first opening area 220 is between 0 and 100%, the etching depth of the inorganic layer 100 corresponding to the first opening area 220 is the second largest, and the touch insulating layer 130 and part of the second inorganic encapsulation layer 120 corresponding to the first opening area 220 are etched away.

[0058] refer to Figure 8 A second exposure and development is performed using a mask that performs the third etching, forming three stepped portions in the inorganic layer 100 on the side of the dicing line facing the edge region C in the dicing zone B. Specifically, the remaining first inorganic encapsulation layer 110 on the dicing line is removed using a mask that performs the third etching until the substrate 300 is exposed.

[0059] Example 2 Example 2 provides a method for preparing a motherboard for a display panel, which differs from Example 1 in that: (Referring to the reference...) Figure 9 , Figure 10 and Figure 11 The inorganic layer in the cutting area B, facing the edge area C, is formed by two exposures and development, resulting in three stepped sections: During the first exposure and development, two stepped portions are formed in the inorganic layer 100 on the side of the cutting line in the dicing area B facing the edge area C. The mask 700 used in the first exposure and development includes a third opening area 720 and a fourth opening area 730 arranged from the edge area C towards the dicing area. The mask 700 used in the first exposure and development simultaneously performs the first etching and the third etching. The fourth opening area 730 corresponds to the common etching area of ​​the first and third etching processes, and the third opening area 720 corresponds to the area where the first etching is performed. Afterwards... A second exposure and development is performed using a mask that performs the second etching, forming three stepped sections in the inorganic layer on the side of the cutting line in the cutting zone facing the edge region.

[0060] Specifically, the transmittance of the third opening region 720 is less than that of the fourth opening region 730. After the first exposure and development, the residual thickness of the photoresist layer corresponding to the fourth opening region 730 is less than that corresponding to the third opening region 720. Consequently, the etching range of the inorganic layer 100 corresponding to the fourth opening region 730 is greater than that corresponding to the third opening region 720. During the second exposure and development, the mask performs a third etching at the common etching region corresponding to the fourth opening region 730, further removing the inorganic layer 100 in that region until the inorganic layer 100 exposes the substrate 300. Three steps are formed in the inorganic layer 100 on the side of the dicing line in the dicing region B facing the edge region C.

[0061] In one embodiment, continue to refer to Figure 9 The mask 200 further includes: a first light-shielding area 710, with multiple opening areas located outside the first light-shielding area 710; and a second light-shielding area 740 located outside the multiple opening areas. In this embodiment, a third opening area 720 is located outside the first light-shielding area 710, and the second light-shielding area 740 is located outside the fourth opening area 730. This avoids etching the film layer of other surrounding display panel areas A, improving the production yield of the display panel.

[0062] In one embodiment, the material transmittance of the third opening region 720 is less than that of the fourth opening region 730, and the material transmittance of the first shading region 710 and the second shading region 740 is 0. For example, the mask 700 includes a halftone mask.

[0063] In another embodiment, the total opening area of ​​the opening pattern in the third opening region 720 is smaller than the total opening area of ​​the opening pattern in the fourth opening region 730, and the first light-shielding region 710 and the second light-shielding region 740 are not provided with opening patterns. For example, the mask 700 includes a grayscale mask.

[0064] In one embodiment, the size of the opening pattern of the fourth opening region 730 is smaller than the minimum resolution size of the exposure machine, which can achieve the effect that the exposure light partially passes through the mask and does not form an actual pattern on the inorganic layer 100. By adjusting the size of the opening pattern of the fourth opening region 730, the energy of the transmitted exposure light is controlled to achieve grayscale exposure.

[0065] In this embodiment, the transmittance of the first light-shielding area 710 is 0. For a halftone mask, the material of the light-shielding film in the first light-shielding area 710 is chromium; for a grayscale mask, the light-shielding film in the first light-shielding area 710 has no opening pattern. After the first exposure and development, the photoresist layer corresponding to the first light-shielding area 710 is completely retained, and correspondingly, the inorganic layer 100 corresponding to the first light-shielding area 710 is also retained.

[0066] In other embodiments, the transmittance of the first light-shielding area can also be a small non-zero value, so that the inorganic layer corresponding to the first light-shielding area is etched by a very small amount, as long as the integrity of the inorganic layer in the edge area is not affected.

[0067] In this embodiment, the transmittance of the fourth opening region 730 is 100%. That is, the fourth opening region 730 is a fully transparent area. For a halftone mask, the fourth opening region 730 only includes the transparent substrate and does not have a light-shielding film; for a grayscale mask, the opening pattern of the light-shielding film in the fourth opening region 730 is a complete opening, exposing the transparent substrate of the fourth opening region 730. After the first exposure and development, the photoresist layer corresponding to the fourth opening region 730 is completely removed, and correspondingly, the etching depth of the inorganic layer 100 corresponding to the fourth opening region 730 is the maximum.

[0068] In other embodiments, the transmittance of the fourth opening region may also be a large value close to 100%, such as 99%, 98% or 97%.

[0069] In one embodiment, the transmittance of the third opening region 720 is between 0 and 100%, for example, 30%, 50%, or 80%. That is, the third opening region 720 is a semi-transparent region. For a halftone mask, the material of the light-shielding film in the third opening region 720 is chromium oxide or molybdenum oxide; for a grayscale mask, the light-shielding film in the third opening region 720 has a partially open pattern. After the first exposure and development, the photoresist layer corresponding to the third opening region 720 is partially removed, and correspondingly, the etching depth of the inorganic layer 100 corresponding to the third opening region 720 is then increased.

[0070] In other embodiments, the light transmittance of the third opening region 720 and the fourth opening region 730 are not limited, as long as the light transmittance of the third opening region 720 is less than that of the fourth opening region 730. The light transmittance of each opening region can be adjusted by adjusting the material of the light-shielding film and the total opening area of ​​the opening pattern.

[0071] In one embodiment, the etching range of the second etching is larger than the etching range of the third etching. Accordingly, the size of the third opening region 720 of the mask in this embodiment is smaller than the size of the first opening region 220 of the mask in Embodiment 1, and the size of the fourth opening region 730 of the mask in this embodiment is larger than the size of the second opening region 230 of the mask in Embodiment 1.

[0072] refer to Figure 10 and Figure 11 This embodiment details the fabrication process of forming three stepped portions in the inorganic layer 100 on the side of the cutting line towards the edge region through two exposures and developments. The first light-shielding region 710 has a transmittance of 0%, the fourth opening region 730 has a transmittance of 100%, and the third opening region 720 has a transmittance between 0 and 100% as an illustration.

[0073] refer to Figure 10 Two stepped portions are formed in the inorganic layer 100 on the side of the cutting line towards the edge B in the cutting zone C by the first exposure and development. Since the transmittance of the first light-shielding area 710 is 0, the inorganic layer 100 corresponding to the first light-shielding area 710 is retained, that is, the first inorganic encapsulation layer 110, the second inorganic encapsulation layer 120, and the touch insulating layer 130 corresponding to the first light-shielding area 710 are not etched; since the transmittance of the fourth opening area 730 is 100%, the etching depth of the inorganic layer 100 corresponding to the fourth opening area 730 is the largest, and the touch insulating layer 130, the second inorganic encapsulation layer 120, and part of the first inorganic encapsulation layer 110 corresponding to the fourth opening area 730 are etched away; since the transmittance of the third opening area 720 is between 0 and 100%, the etching depth of the inorganic layer 100 corresponding to the third opening area 720 is the second largest, and the touch insulating layer 130 and part of the second inorganic encapsulation layer 120 corresponding to the third opening area 720 are etched away.

[0074] refer to Figure 11 A second exposure and development is performed using a mask that performs the second etching, forming three stepped portions in the inorganic layer 100 on the side of the dicing line facing the edge region C in the dicing zone B. Specifically, the remaining portion of the second inorganic encapsulation layer 120 and the first inorganic encapsulation layer 110 on the dicing line is removed using a mask that performs the second etching until the substrate 300 is exposed.

[0075] Example 3 Example 3 provides a method for preparing a motherboard for a display panel, which differs from Examples 1 and 2 in that: Reference Figure 12 and Figure 13 The inorganic layer formed by a single exposure and development on the side of the cutting line in the cutting zone B toward the edge zone C comprises three stepped sections: This invention utilizes a mask 800 to simultaneously perform the first, second, and third etching processes. The mask 800 includes a fifth opening region 820, a sixth opening region 830, and a seventh opening region 840 arranged from the edge region C towards the cutting channel region B. The seventh opening region 840 corresponds to the common etching area for the first, second, and third etching processes; the sixth opening region 830 corresponds to the second etching process; and the fifth opening region 820 corresponds to the first etching process. Compared to the prior art which requires three masks to perform three etching processes separately, this application utilizes the four opening regions of a single mask 800 to simultaneously achieve the first, second, and third etching processes in a single exposure and development. In other words, three stepped sections can be formed with a single mask in one exposure and development, reducing the use of two masks, shortening the process flow, and lowering material costs.

[0076] Specifically, the transmittance of the fifth opening region 820 is less than that of the sixth opening region 830, and the transmittance of the sixth opening region 830 is less than that of the seventh opening region 840. After one exposure and development, the residual thickness of the photoresist layer corresponding to the seventh opening region 840 is less than that corresponding to the sixth opening region 830. Correspondingly, the etching range of the inorganic layer 100 corresponding to the seventh opening region 840 is greater than that corresponding to the sixth opening region 830. The residual thickness of the photoresist layer corresponding to the sixth opening region 830 is less than that corresponding to the fifth opening region 820. Correspondingly, the etching range of the inorganic layer 100 corresponding to the sixth opening region 830 is greater than that corresponding to the fifth opening region 820. The first, second and third etching processes are performed simultaneously by the mask 800 used in the single exposure development, and the inorganic layer 100 corresponding to the seventh opening region 840 exposes the substrate 300. Three stepped portions are formed in the inorganic layer 100 on the side of the cutting line in the dicing region B facing the edge region C.

[0077] In one embodiment, continue to refer to Figure 12 The mask 200 further includes: a first light-shielding area 810, with a plurality of opening areas located outside the first light-shielding area 810; and a second light-shielding area 850 located outside the plurality of opening areas. In this embodiment, the fifth opening area 820 is located outside the first light-shielding area 810, and the second light-shielding area 850 is located outside the seventh opening area 840. This avoids etching of the film layer of other surrounding display panel areas A, improving the production yield of the display panel.

[0078] In one embodiment, the material transmittance of the fifth opening region 820 is less than that of the sixth opening region 830, the material transmittance of the sixth opening region 830 is less than that of the seventh opening region 840, and the material transmittance of the first shading region 810 and the second shading region 850 is 0. For example, the mask 800 includes a halftone mask.

[0079] In another embodiment, the total opening area of ​​the opening pattern in the fifth opening region 820 is smaller than the total opening area of ​​the opening pattern in the sixth opening region 830, the total opening area of ​​the opening pattern in the sixth opening region 830 is smaller than the total opening area of ​​the opening pattern in the seventh opening region 840, and the first light-shielding region 810 and the second light-shielding region 850 are not provided with opening patterns. For example, the mask 800 includes a grayscale mask.

[0080] In one embodiment, the size of the opening pattern of the seventh opening region 840 is smaller than the minimum resolution size of the exposure machine, which can achieve the effect that the exposure light partially passes through the mask and does not form an actual pattern on the inorganic layer 100. By adjusting the size of the opening pattern of the seventh opening region 840, the energy of the transmitted exposure light is controlled to achieve grayscale exposure.

[0081] In this embodiment, the transmittance of the first light-shielding area 810 is 0. For a halftone mask, the material of the light-shielding film in the first light-shielding area 810 is chromium; for a grayscale mask, the light-shielding film in the first light-shielding area 810 has no opening pattern. After the first exposure and development, the photoresist layer corresponding to the first light-shielding area 810 is completely retained, and correspondingly, the inorganic layer 100 corresponding to the first light-shielding area 810 is also retained.

[0082] In this embodiment, the transmittance of the seventh opening region 840 is 100%. That is, the seventh opening region 840 is a fully transparent area. For a halftone mask, the seventh opening region 840 only includes the transparent substrate and does not have a light-shielding film; for a grayscale mask, the opening pattern of the light-shielding film in the seventh opening region 840 is a complete opening, exposing the transparent substrate of the seventh opening region 840. After the first exposure and development, the photoresist layer corresponding to the seventh opening region 840 is completely removed, and correspondingly, the etching depth of the inorganic layer 100 corresponding to the seventh opening region 840 is the maximum.

[0083] In one embodiment, the light transmittance of the fifth opening region 820 and the sixth opening region 830 is between 0 and 100%. For example, the light transmittance of the fifth opening region 820 is 30% and the light transmittance of the sixth opening region 830 is 50%, or the light transmittance of the fifth opening region 820 is 50% and the light transmittance of the sixth opening region 830 is 80%. There is no restriction on the light transmittance of the fifth opening region 820 and the sixth opening region 830, as long as the light transmittance of the fifth opening region 820 is less than the light transmittance of the sixth opening region 830.

[0084] Both the fifth opening area 820 and the sixth opening area 830 are semi-transparent areas. For the halftone mask, the material of the light-shielding film in both the fifth opening area 820 and the sixth opening area 830 is chromium oxide or molybdenum oxide. The thickness of the light-shielding film in the fifth opening area 820 is greater than that in the sixth opening area 830. For the grayscale mask, both the fifth opening area 820 and the sixth opening area 830 have partial opening patterns. The total opening area of ​​the light-shielding film pattern in the fifth opening area 820 is smaller than that in the sixth opening area 830. After the first exposure and development, the residual thickness of the photoresist layer corresponding to the fifth opening region 820 is greater than the residual thickness of the photoresist layer corresponding to the sixth opening region 830. Correspondingly, the etching depth of the inorganic layer 100 corresponding to the fifth opening region 820 is less than the etching depth of the inorganic layer 100 corresponding to the sixth opening region 830, and less than the etching depth of the inorganic layer 100 corresponding to the seventh opening region 840.

[0085] In other embodiments, the light transmittance of the fifth opening region 820, the sixth opening region 830, and the seventh opening region 840 are not limited, as long as the light transmittance of the fifth opening region 820 is less than that of the sixth opening region 830, and the light transmittance of the sixth opening region 830 is less than that of the seventh opening region 840. The light transmittance of each opening region can be adjusted by adjusting the material of the light-shielding film and the total opening area of ​​the opening pattern.

[0086] refer to Figure 13 This embodiment details the fabrication process of forming three stepped portions in the inorganic layer 100 on the side of the cutting line towards the edge region through a single exposure and development. The illustration is illustrated by the following: the transmittance of the first light-shielding region 810 is 0; the transmittance of the seventh opening region 840 is 100%; and the transmittances of the fifth opening region 820 and the sixth opening region 830 are between 0 and 100%, with the transmittance of the fifth opening region 820 being less than that of the sixth opening region 830.

[0087] refer to Figure 13In the first exposure and development, three stepped portions are formed in the inorganic layer 100 on the side of the cutting line towards the edge B in the cutting area C. Since the transmittance of the first light-shielding area 810 is 0, the inorganic layer 100 corresponding to the first light-shielding area 810 is retained; that is, the first inorganic encapsulation layer 110, the second inorganic encapsulation layer 120, and the touch insulating layer 130 corresponding to the first light-shielding area 810 are not etched. Since the transmittance of the seventh opening area 840 is 100%, the etching depth of the inorganic layer 100 corresponding to the seventh opening area 840 is the largest. The touch insulating layer 130, the second inorganic encapsulation layer 120, and the first inorganic encapsulation layer 110 corresponding to the seventh opening area 840 are all etched away, exposing the substrate 300. Based on the fifth opening... The light transmittance of region 820 and the sixth opening region 830 is between 0 and 100%, and the light transmittance of the fifth opening region 820 is less than that of the sixth opening region 830. The etching depth of the inorganic layer 100 corresponding to the sixth opening region 830 is the second deep. The touch insulating layer 130, the second inorganic encapsulation layer 120 and part of the first inorganic encapsulation layer 110 corresponding to the sixth opening region 830 are etched away. The etching depth of the inorganic layer 100 corresponding to the fifth opening region 820 is the smallest. The touch insulating layer 130 and part of the second inorganic encapsulation layer 120 corresponding to the fifth opening region 820 are etched away.

[0088] Another embodiment of the present invention provides a method for manufacturing a display panel, comprising: forming a mother plate according to the method for manufacturing a mother plate of a display panel according to the above embodiment of the present invention; and cutting along a cutting line in a cutting channel area B to obtain a display panel.

[0089] In this embodiment, since the inorganic layer in the edge area of ​​the cut display panel has a stepped portion, the gentle slope structure of the stepped portion can avoid the residue of the inorganic layer near the cutting line, reduce the stress concentration of the inorganic layer at the cutting line, reduce the possibility of cracks in the inorganic layer during the cutting process and subsequent use, thereby preventing stress from extending to the display area and improving the reliability of the display panel.

[0090] In one embodiment, the display panel includes an OLED (Organic Light-Emitting Diode) display panel.

[0091] Another embodiment of the present invention provides a display device including the above-described display panel. The display device can be any product or component with display function, such as a mobile phone, tablet computer, television, monitor, laptop computer, digital photo frame, or navigator; this embodiment does not limit this.

[0092] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation of the present invention. For those skilled in the art, other variations or modifications can be made based on the above description. It is impossible to exhaustively list all the implementation methods here. All obvious variations or modifications derived from the technical solutions of the present invention are still within the protection scope of the present invention.

Claims

1. A method of manufacturing a mother panel of a display panel, characterized by, include: At least one display panel area and a cleaving channel area surrounding the display panel area are formed on the substrate of the motherboard. The display panel area includes a display area and an edge area surrounding the display area. The cleaving channel area includes an inorganic layer disposed in the same layer as the display panel area. M stepped portions are formed in the inorganic layer on the side of the cutting line towards the edge region by N exposures and developments, where N < M. The mask used at least once in the N exposures and developments includes multiple opening regions arranged from the inside to the outside, and the light transmittance of the inner opening region among adjacent opening regions is less than that of the outer opening region.

2. The method of manufacturing a mother panel for a display panel according to claim 1, wherein In adjacent opening areas, the light transmittance of the material in the inner opening area is less than that in the outer opening area.

3. The method of manufacturing a mother panel for a display panel according to claim 1, wherein The opening area includes an array of opening patterns, and among adjacent opening areas, the total opening area of ​​the opening patterns in the inner opening area is smaller than that in the outer opening area.

4. The method of manufacturing a mother panel for a display panel according to claim 1, wherein The inorganic layer includes a first inorganic encapsulation layer, a second inorganic encapsulation layer, and a touch insulating layer stacked on the substrate.

5. The method of manufacturing a mother panel for a display panel according to claim 1, wherein After N exposures and developments, the substrate at the dicing line is exposed by the inorganic layer.

6. The method of manufacturing a mother panel for a display panel according to any one of claims 1 to 5, wherein Three stepped sections are formed in the inorganic layer on the side of the cutting line towards the edge area by two exposures and development, including: Two stepped portions are formed in the inorganic layer on the side of the dicing line towards the edge region during the first exposure and development. The mask used in the first exposure and development includes a first opening region and a second opening region arranged from the edge region towards the dicing region. The mask used in the first exposure and development simultaneously performs the first etching and the second etching. The second opening region corresponds to the common etching region of the first and second etching processes, and the first opening region corresponds to the first etching process. Afterwards... A second exposure and development is performed using a mask that performs the third etching, forming three stepped sections in the inorganic layer on the side of the cutting line in the cutting zone facing the edge region.

7. The method of manufacturing a mother panel for a display panel according to any one of claims 1 to 5, wherein Three stepped sections are formed in the inorganic layer on the side of the cutting line towards the edge area by two exposures and development, including: Two stepped portions are formed in the inorganic layer on the side of the dicing line towards the edge region during the first exposure and development. The mask used in the first exposure and development includes a third opening region and a fourth opening region arranged from the edge region towards the dicing region. The mask used in the first exposure and development simultaneously performs the first etching and the third etching. The fourth opening region corresponds to the common etching region of the first and third etching processes, and the third opening region corresponds to the first etching process. Afterwards... A second exposure and development is performed using a mask that performs the second etching, forming three stepped portions in the inorganic layer on the side of the cutting line in the cutting zone facing the edge region.

8. The method of producing a display panel according to claim 6 or 7, wherein The etching range of the second etching is larger than that of the third etching.

9. The method of manufacturing a mother panel for a display panel according to any one of claims 1 to 5, wherein Three stepped sections are formed in the inorganic layer on the side of the cutting line towards the edge region by a single exposure development, including: The first etching, second etching, and third etching are performed simultaneously using a mask plate, wherein the mask plate includes a fifth opening area, a sixth opening area, and a seventh opening area arranged from the edge area toward the cutting channel area; the seventh opening area corresponds to the common etching area for the first etching, the second etching, and the third etching, the sixth opening area corresponds to the second etching, and the fifth opening area corresponds to the first etching.

10. A method for manufacturing a display panel, characterized by, include: The preparation method according to any one of claims 1-9 forms a master plate; The display panel is obtained by cutting along the cutting line in the cutting channel area.