Resistive memory structure and fabrication method
By forming conductive elements through a double exposure technique, the problem of incomplete contact between the upper electrode and the conductive element in resistive memory is solved, achieving complete contact between the conductive element and the upper electrode, and improving the compatibility and reliability of the resistive memory manufacturing process.
Patent Information
- Application Number
- CN202510615750.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-14
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies cannot ensure effective contact between the upper electrode of resistive memory and conductive elements, leading to problems such as incomplete or no contact.
The conductive element is formed by using a double exposure technique. By superimposing the conductive pad pattern and the conductive plug pattern, complete contact between the conductive element and the upper electrode is ensured. The conductive element pattern is used as a template to etch the dielectric layer and fill in the metal layer to form the conductive element.
This achieves complete contact between the electrodes and conductive elements on resistive memory, improving the compatibility and reliability of resistive memory manufacturing processes.
Smart Images

Figure CN123124667A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a resistive memory structure and its fabrication method, and particularly to a method for fabricating conductive elements on top of a resistive memory using double exposure. Background Technology
[0002] As modern electronic devices increasingly demand higher storage density, speed, and low power consumption, traditional memory technologies such as Dynamic Random Access Memory (DRAM) and Flash Memory are gradually facing performance and energy efficiency bottlenecks. To address these challenges, Resistive Random Access Memory (RRAM), as an emerging non-volatile memory technology, has gradually attracted attention. RRAM utilizes changes in the resistivity of materials to store data; by applying a voltage to change the cell resistance, information can be read and written.
[0003] RRAM boasts fast write speeds, low power consumption, and high data durability. Unlike traditional charge storage methods, RRAM relies on resistance changes to store data, giving it advantages in terms of simple structure and strong compatibility with manufacturing processes. Its non-volatile nature means that data is retained even when power is off, making RRAM a promising candidate for applications in embedded systems, mobile devices, and high-performance computing. Summary of the Invention
[0004] In view of this, the present invention provides a manufacturing process for fabricating a conductive element above a resistive memory, so as to ensure that the upper electrode of the resistive memory can reliably contact the conductive element above the upper electrode.
[0005] According to a preferred embodiment of the present invention, a resistive memory structure includes a first dielectric layer, a second dielectric layer covering the first dielectric layer, a resistive memory embedded in the first dielectric layer, and the resistive memory including a lower electrode, a resistive switching layer and an upper electrode stacked sequentially from bottom to top. A conductive element is embedded in the second dielectric layer, and the conductive element includes a conductive plug and a conductive pad. The conductive plug contacts the upper electrode, and the conductive pad contacts the conductive plug and is located above the conductive plug. A first direction is defined as from the upper electrode toward the lower electrode. Viewed along the first direction, the conductive plug is offset from the center of the conductive pad.
[0006] According to another preferred embodiment of the present invention, a method for fabricating a resistive memory structure includes providing a first dielectric layer, a second dielectric layer, and a resistive memory, wherein the second dielectric layer covers the first dielectric layer, the resistive memory is embedded in the first dielectric layer, and the resistive memory includes a bottom electrode, a resistive switching layer, and a top electrode stacked sequentially from bottom to top. Then, a first mask layer and a second mask layer are formed to cover the second dielectric layer from bottom to top. Subsequently, the second mask layer and the first mask layer are etched to form a conductive pad pattern in the second mask layer and the first mask layer. Following this, a third mask layer is formed to cover the first dielectric layer. Two mask layers are used to fill the conductive pad pattern. Then, a third mask layer, a first mask layer, and a second dielectric layer are etched to form a conductive plug pattern in the conductive pad pattern. A first direction is defined as from the upper electrode to the lower electrode. When viewed along the first direction, the conductive plug pattern is off-center from the center of the conductive pad pattern. After the conductive plug pattern is formed, the third mask layer is completely removed. Then, using the second mask layer and the first mask layer as masks, the second dielectric layer is etched to form a conductive element trench, and the upper electrode is exposed from the conductive element trench. Finally, a metal layer is formed to fill the conductive element trench to form a conductive element.
[0007] To make the above-mentioned objects, features, and advantages of the present invention more apparent and understandable, preferred embodiments are described below in detail with reference to the accompanying drawings. However, the following preferred embodiments and drawings are for reference and illustration only and are not intended to limit the present invention. Attached Figure Description
[0008] Figure 1 , Figure 2 , Figure 3 , Figure 4 and Figure 5 A schematic diagram illustrating a method for fabricating a resistive memory structure according to a first preferred embodiment of the present invention;
[0009] Figure 6 , Figure 7 and Figure 8 A schematic diagram illustrating a method for fabricating a resistive memory structure according to a second preferred embodiment of the present invention;
[0010] Figure 9 , Figure 10 , Figure 11 , Figure 12 and Figure 13 A schematic diagram illustrating a method for fabricating a resistive memory structure according to a third preferred embodiment of the present invention;
[0011] Figure 14 , Figure 15 and Figure 16 This is a schematic diagram illustrating a method for manufacturing a resistive memory structure according to a fourth preferred embodiment of the present invention;
[0012] Figure 17 The diagram shows a top view of a conductive element and a resistive memory according to the first to fourth preferred embodiments of the present invention.
[0013] Symbol explanation:
[0014] 1: Top view
[0015] 2: Top view
[0016] 3: Top view
[0017] 4: Top view
[0018] 5: Top view
[0019] 6: Top view
[0020] 7: Top View
[0021] 8: Top View
[0022] 10: First dielectric layer
[0023] 12: Conductive plug
[0024] 14: Stepped outline
[0025] 20: Second dielectric layer
[0026] 20a: Dielectric layer
[0027] 20b: Dielectric layer
[0028] 30a: First mask layer
[0029] 30b: Second mask layer
[0030] 30c: Third mask layer
[0031] 40: Conductive element pattern
[0032] 40a: Conductive pad pattern
[0033] 40b: Conductive plug pattern
[0034] 50: Conductive element trench
[0035] 50a: Lower trench
[0036] 50b: Upper Groove
[0037] 52: Metal layer
[0038] 60: Conductive element
[0039] 60a: Conductive plug
[0040] 60b: Conductive pad
[0041] 70: Protruding part
[0042] 100: Resistive Memory Structure
[0043] 200: Resistive Memory Structure
[0044] 300: Resistive Memory Structure
[0045] 400: Resistive Memory Structure
[0046] B: Lower electrode
[0047] C1: Center
[0048] C2: Center
[0049] C3: Center
[0050] C4: Center
[0051] C5: Center
[0052] E1: First Exposure
[0053] E2: Second Exposure
[0054] R: Resistive memory
[0055] O1: Opening
[0056] O2: Opening
[0057] PR1: Photoresist
[0058] PR2: Photoresist
[0059] S: Resistor conversion layer
[0060] T: Upper electrode
[0061] W1: First lateral wall
[0062] W2: Second sidewall
[0063] W3: Third lateral wall
[0064] X: Second direction
[0065] Y: First direction Detailed Implementation
[0066] Figures 1 to 5 This is a method for fabricating a resistive memory structure according to a first preferred embodiment of the present invention.
[0067] like Figure 1As shown, a first dielectric layer 10 is provided, and a resistive memory R is embedded in the first dielectric layer 10. The resistive memory R includes a lower electrode B, a resistive switching layer S, and an upper electrode T stacked sequentially from bottom to top. A conductive plug 12 is embedded in the first dielectric layer 10 and contacts the lower electrode B of the resistive memory R. A second dielectric layer 20 covers the first dielectric layer 10. The second dielectric layer 20 may include multiple dielectric materials, such as dielectric layer 20a and dielectric layer 20b. In addition, a first mask layer 30a, a second mask layer 30b, and a photoresist PR1 sequentially cover the second dielectric layer 20 from bottom to top. The first mask layer 30a and the second mask layer 30b each contain titanium nitride, silicon nitride, silicon oxide, or silicon oxynitride. According to a preferred embodiment of the present invention, the first mask layer 30a is titanium nitride, and the second mask layer 30b is silicon oxide. The first exposure E1 in the secondary exposure is used to form an opening O1 on the photoresist PR1. The opening O1 defines the position of the conductive pad pattern to be formed subsequently. A second direction X is defined as parallel to the upper surface of the first dielectric layer 10. Along the second direction X, the width of the opening O1 is greater than the width T of the upper electrode.
[0068] like Figure 2 As shown, a second mask layer 30b and a first mask layer 30a are etched using photoresist PR1 as a mask to form a conductive pad pattern 40a in the second mask layer 30b and the first mask layer 30a. Along the second direction X, the width of the conductive pad pattern 40a is greater than the width of the upper electrode T. Furthermore, the first mask layer 30a is not etched through during the etching of the second mask layer 30b and the first mask layer 30a. Figure 3 As shown, the photoresist PR1 is first removed, then a third mask layer 30c is formed to cover the second mask layer 30b and fill the conductive pad pattern 40a. The third mask layer 30c is preferably a bottom anti-reflective coating. Next, a photoresist PR2 is formed to cover the third mask layer 30c. Then, a second exposure E2 is performed in the secondary exposure process to form an opening O2 on the photoresist PR2. The opening O2 defines the position of the conductive plug pattern to be formed subsequently. Then, using the photoresist PR2 as a mask, the third mask layer 30c, the first mask layer 30a, and the dielectric layer 20b in the second dielectric layer 20 are etched to form a conductive plug pattern 40b in the conductive pad pattern 40a. A first direction Y is defined as from the upper electrode T towards the lower electrode B. Viewed along the first direction Y, as from top view... Figure 1As shown, the conductive plug pattern 40b is offset from the center C1 of the conductive pad pattern 40a. Specifically, the center C2 of the conductive plug pattern 40b is offset from the center C1 of the conductive pad pattern 40a, but the conductive plug pattern 40b does not exceed the range of the conductive pad pattern 40a. The area of the conductive plug pattern 40b is smaller than the area of the conductive pad pattern 40a. When the conductive pad pattern 40a is rectangular, the center C1 of the conductive pad pattern 40a is defined as the intersection of the diagonals of the conductive pad pattern 40a; when the conductive plug pattern 40b is rectangular, the center C2 of the conductive plug pattern 40b is defined as the intersection of the diagonals of the conductive plug pattern 40b. Furthermore, as seen from the side view, the width of the conductive plug pattern 40b is smaller than the width of the conductive pad pattern 40a. Therefore, when etching the third mask layer 30c, the first mask layer 30a, and the second dielectric layer 20 to form the conductive plug pattern 40b, the second mask layer 30b is not etched. In addition, the conductive plug pattern 40b is defined by the dielectric layer 20b in the first mask layer 30a and the second dielectric layer 20. Therefore, there is no conductive plug pattern 40b in the dielectric layer 20a. The conductive pad pattern 40a and the conductive plug pattern 40b together form a conductive element pattern 40.
[0069] Please also refer to Figure 3 and Figure 4 The photoresist PR2 and the third mask layer 30c are completely removed. Then, using the second mask layer 30b and the first mask layer 30a as masks, the first mask layer 30a and the second dielectric layer 20 (including dielectric layer 20a and dielectric layer 20b) are etched to form a conductive element trench 50, and the upper electrode T is exposed from the conductive element trench 50. Specifically, the conductive element trench 50 includes an upper trench 50b and a lower trench 50a. The width of the upper trench 50b is greater than that of the lower trench 50a. The upper trench 50b is only buried in the dielectric layer 20b, and the lower trench 50a is only buried in the dielectric layer 20a. The upper electrode T is exposed from the lower trench 50a. During the etching process, the second mask layer 30b and the first mask layer 30a may be completely removed. Figure 5 As shown, a metal layer 52 is formed and filled into the conductive element trench 50 to form a conductive element 60. Thus, the resistive memory structure 100 of the first preferred embodiment of the present invention has been completed.
[0070] Figures 6 to 8 The second preferred embodiment of the present invention illustrates a method for manufacturing a resistive memory structure, wherein elements having the same function and location will use the element symbols in the first preferred embodiment.
[0071] The difference between the second preferred embodiment and the first preferred embodiment is that in the second preferred embodiment, the conductive plug pattern 40b is located at the center C1 of the conductive pad pattern 40a, and the center C2 of the conductive plug pattern 40b overlaps with the center C1 of the conductive pad pattern 40a. All other manufacturing process steps are the same as in the first preferred embodiment. In the second preferred embodiment, the following... Figure 2 ,like Figure 6 As shown, a third mask layer 30c is formed to cover the second mask layer 30b and fill the conductive pad pattern 40a. Then, a photoresist PR2 is formed to cover the third mask layer 30c. The opening O2 on the photoresist PR2 defines the position of the conductive plug pattern to be formed subsequently. Next, using the photoresist PR2 as a mask, the third mask layer 30c, the first mask layer 30a, and the dielectric layer 20b in the second dielectric layer 20 are etched to form the conductive plug pattern 40b in the conductive pad pattern 40a. Viewed along the first direction Y, as shown in top view... Figure 2 As shown, the conductive plug pattern 40b is located at the center C1 of the conductive pad pattern 40a. That is, the center C2 of the conductive plug pattern 40b overlaps with the center C1 of the conductive pad pattern 40a. The area of the conductive plug pattern 40b is smaller than the area of the conductive pad pattern 40a. Furthermore, as seen from the side view, the width of the conductive plug pattern 40b is smaller than the width of the conductive pad pattern 40a. At this point, the conductive pad pattern 40a and the conductive plug pattern 40b together form a conductive element pattern 40.
[0072] like Figure 7 As shown, using the second mask layer 30b and the first mask layer 30a as masks, the first mask layer 30a and the second dielectric layer 20 are etched to form a conductive element trench 50, following the contour of the conductive element pattern 40, and the upper electrode T is exposed through the conductive element trench 50. Figure 8 As shown, a metal layer 52 is formed and filled into the conductive element trench 50 to form a conductive element 60. Thus, the resistive memory structure 200 of the second preferred embodiment of the present invention has been completed.
[0073] Figures 9 to 13 The present invention provides a method for fabricating a resistive memory structure according to a third preferred embodiment, wherein elements having the same function and location will use the element symbols in the first preferred embodiment.
[0074] like Figure 9As shown, a first dielectric layer 10 is provided, and a resistive memory R is embedded in the first dielectric layer 10. The resistive memory R includes a lower electrode B, a resistive switching layer S, and an upper electrode T stacked sequentially from bottom to top. A conductive plug 12 is embedded in the first dielectric layer 10 and contacts the lower electrode B of the resistive memory R. A second dielectric layer 20 covers the first dielectric layer 10. The second dielectric layer 20 may include multiple dielectric materials, such as dielectric layer 20a and dielectric layer 20b. A first mask layer 30a, a second mask layer 30b, and a photoresist PR1 are sequentially covered by the second dielectric layer 20 from bottom to top. Then, a first exposure E1 is performed in a secondary exposure to form an opening O1 on the photoresist PR1. The opening O1 defines the position of the conductive pad pattern to be formed subsequently. A second direction X is defined as parallel to the upper surface of the first dielectric layer 10. Along the second direction X, the width of the opening O1 is not greater than the width of the upper electrode T. According to a preferred embodiment of the present invention, the width of the opening O1 is equal to the width of the upper electrode T.
[0075] like Figure 10 As shown, a second mask layer 30b and a first mask layer 30a are etched using photoresist PR1 as a mask to form a conductive pad pattern 40a in the second mask layer 30b and the first mask layer 30a. Along the second direction X, the width of the conductive pad pattern 40a is not greater than the width of the upper electrode T, and preferably equal to the width of the upper electrode T. Furthermore, during the etching of the second mask layer 30b and the first mask layer 30a, the first mask layer 30a is not etched through. Figure 11 As shown, photoresist PR1 is removed, then a third mask layer 30c is formed to cover the second mask layer 30b and fill the conductive pad pattern 40a. Next, photoresist PR2 is formed to cover the third mask layer 30c. Then, a second exposure E2 is performed in the secondary exposure process to form an opening O2 on the photoresist PR2. The opening O2 defines the position of the conductive plug pattern to be formed subsequently. Since the width of the conductive pad pattern 40a in the third preferred embodiment is smaller than that in the first preferred embodiment, when the opening O2 deviates from the center C1 of the conductive pad pattern 40a, it can easily extend beyond the range of the conductive pad pattern 40a. In the third preferred embodiment, this is the case where the opening O2 extends beyond the range of the conductive pad pattern 40a.
[0076] The subsequent etching step involves etching the third mask layer 30c, the second mask layer 30b, the first mask layer 30a, and the dielectric layer 20b of the second dielectric layer 20 using photoresist PR2 as a mask to form a conductive plug pattern 40b in the conductive pad pattern 40a. A first direction Y is defined as from the upper electrode T toward the lower electrode E. Viewed along the first direction Y, as from top view... Figure 3As shown, the conductive plug pattern 40b is offset from the center C1 of the conductive pad pattern 40a. Specifically, the center C2 of the conductive plug pattern 40b is offset from the center C1 of the conductive pad pattern 40a, and the conductive plug pattern 40b extends beyond the range of the conductive pad pattern 40a. The area of the conductive plug pattern 40b is smaller than the area of the conductive pad pattern 40a. In addition, as seen from the side view, the width of the conductive plug pattern 40b is smaller than the width of the conductive pad pattern 40a. Furthermore, since the etchant used in the etching step has a lower etching rate on the second mask layer 30b but a higher etching rate on the third mask layer 30c, the depth of the O2 transfer into the second mask layer 30b, the first mask layer 30a, and the dielectric layer 20b is inconsistent. This results in the conductive plug pattern 40b being deeper within the conductive pad pattern 40a and shallower outside the conductive pad pattern 40a. Specifically, the conductive plug pattern 40b within the conductive pad pattern 40a has the second dielectric layer 20b as its bottom, while the conductive plug pattern 40b outside the conductive pad pattern 40a has the second mask layer 30b as its bottom. At this time, the conductive pad pattern 40a and the conductive plug pattern 40b together form a conductive element pattern 40.
[0077] like Figure 12 As shown, using the second mask layer 30b and the first mask layer 30a as masks, and following the contour of the conductive element pattern 40, the second mask layer 30b, the first mask layer 30a, and the second dielectric layer 20 are etched to form a conductive element trench 50, and the upper electrode T is exposed by the conductive element trench 50. The conductive element trench 50 includes an upper trench 50b and a lower trench 50a. The width of the upper trench 50b is greater than the width of the lower trench 50a. The upper trench 50b is only embedded in the dielectric layer 20b, and the lower trench 50a is only embedded in the dielectric layer 20a. It is worth noting that the sidewall of the upper trench 20b includes a stepped contour 14, and the sidewall of the lower trench 50a is flush with the sidewall of the resistive memory R. Figure 13 As shown, a metal layer 52 is formed and filled into the conductive element trench 50 to form a conductive element 60. Thus, the resistive memory structure 300 of the third preferred embodiment of the present invention has been completed.
[0078] Figures 14 to 16 The present invention illustrates a method for manufacturing a resistive memory structure according to a fourth preferred embodiment, wherein elements having the same function and location will use the element symbols in the third preferred embodiment.
[0079] The difference between the fourth preferred embodiment and the third preferred embodiment is that in the fourth preferred embodiment, the conductive plug pattern 50a is located at the center of the conductive pad pattern 50b, but the conductive plug pattern 50a does not exceed the range of the conductive pad pattern 50b. The other manufacturing process steps are the same as those in the third preferred embodiment.
[0080] In the fourth preferred embodiment, the continuation Figure 10 ,like Figure 14 As shown, a third mask layer 30c is formed to cover the second mask layer 30b and fill the conductive pad pattern 40a. Then, a photoresist PR2 is formed to cover the third mask layer 30c. Next, a second exposure E2 is performed in a secondary exposure process to form an opening O2 on the photoresist PR2. The opening O2 defines the position of the conductive plug pattern to be formed subsequently. Then, using the photoresist PR2 as a mask, the third mask layer 30c and the dielectric layer 20b of the second dielectric layer 20 are etched to form the conductive plug pattern 40b in the conductive pad pattern 40a. In the fourth preferred embodiment, when etching the third mask layer 30c, the first mask layer 30a, and the second dielectric layer 20 to form the conductive plug pattern 40b, the second mask layer 30b is not etched. At this time, viewed along the first direction Y, such as from above... Figure 4 As shown, the conductive plug pattern 40b is located at the center C1 of the conductive pad pattern 40a. The center C2 of the conductive plug pattern 40b overlaps with the center C1 of the conductive pad pattern 40a. The area of the conductive plug pattern 40b is smaller than the area of the conductive pad pattern 40a. Furthermore, as seen from the side view, the width of the conductive plug pattern 40b is smaller than the width of the conductive pad pattern 40a. At this time, the conductive pad pattern 40a and the conductive plug pattern 40b together form a conductive element pattern 40.
[0081] like Figure 15 As shown, using the second mask layer 30b and the first mask layer 30a as masks, and following the contour of the conductive element pattern 40, the first mask layer 30a and the second dielectric layer 20 are etched to form a conductive element trench 50. The conductive element trench 50 includes an upper trench 50b and a lower trench 50a. The upper trench 50b is only embedded in the dielectric layer 20b, and the lower trench 50a is only embedded in the dielectric layer 20a. The upper electrode T is exposed by the conductive element trench 50. Figure 16 As shown, a metal layer 52 is formed and filled into the conductive element trench 50 to form a conductive element 60. Thus, the resistive memory structure 400 of the fourth preferred embodiment of the present invention has been completed.
[0082] Figure 5 A resistive memory structure is illustrated according to a first preferred embodiment of the present invention. Figure 8 This is a resistive memory structure illustrated according to a second preferred embodiment of the present invention. Figure 13 A resistive memory structure is illustrated according to a third preferred embodiment of the present invention. Figure 16 This is a resistive memory structure illustrated according to a fourth preferred embodiment of the present invention. Figure 17 This is a top view illustrating a conductive element and a resistive memory according to the first to fourth preferred embodiments of the present invention. Wherein... Figure 8 , Figure 13 , Figure 16 and Figure 17 Components with the same function and location will use and Figure 5 Same component designation.
[0083] Please also refer to Figure 5 and Figure 17 A resistive memory structure 100 fabricated according to a first preferred embodiment of the present invention includes a first dielectric layer 10, a second dielectric layer 20 covering the first dielectric layer 10, and the second dielectric layer 20 including a dielectric layer 20a and a dielectric layer 20b, with the dielectric layer 20b located above the dielectric layer 20a. The dielectric layers 20a and 20b each comprise insulating materials such as silicon oxide, silicon nitride, and silicon oxynitride. The dielectric layer 20b is preferably silicon oxide, and the dielectric layer 20a is preferably silicon nitride. The dielectric layers 20b and 20a must be made of different materials. The first dielectric layer 10 is preferably silicon oxide.
[0084] A resistive memory R is embedded in a first dielectric layer 10. The resistive memory R includes a lower electrode B, a resistive conversion layer S, and an upper electrode T stacked sequentially from bottom to top. A conductive element 60 is embedded in a second dielectric layer 20. The conductive element 60 includes a conductive plug 60a and a conductive pad 60b. The conductive element 60 is integrally formed. For clear identification, the conductive plug 60a and the conductive pad 60b are separated by a dashed line. The conductive pad 60b refers to the portion of the conductive element 60 embedded in the dielectric layer 20b, and the conductive plug 60a refers to the portion of the conductive element 60 embedded in the dielectric layer 20a. The conductive plug 60a contacts the upper electrode T, and the conductive pad 60b contacts the conductive plug 60a and is located above the conductive plug 60a. A first direction Y is defined as from the upper electrode T toward the lower electrode B. Figure 17 A bird's-eye view Figure 5As shown, viewed along the first direction Y, the conductive plug 60a is offset from the center C3 of the conductive pad 60b and also from the center C4 of the resistive memory. Specifically, the center C5 of the conductive plug 60a is offset from both the center C3 of the conductive pad 60b and the center C4 of the resistive memory. When the conductive pad 60b, the resistive memory R, and the conductive plug 60a are rectangular, the center C3 of the conductive pad 60b is defined as the intersection of its diagonals, the center C4 of the resistive memory R is defined as the intersection of its diagonals, and the center C5 of the conductive plug 60a is defined as the intersection of its diagonals. The conductive plug 60a is completely located within the conductive pad 60b. Furthermore, the area of the conductive pad 60b is larger than the area of the conductive plug 60a, and the area of the conductive pad 60b is also larger than the area of the resistive memory R. Furthermore, a second direction X is defined as parallel to the upper surface of the first dielectric layer 10. Along the second direction X, the width of the conductive pad 60b is greater than the width of the upper electrode T, and the width of the conductive pad 60b is greater than the width of the conductive plug 60a. Additionally, along the first direction Y, the thickness of the conductive pad 60b is 5 to 10 times the thickness of the conductive plug 60a. Moreover, the conductive pad 60b does not contact the resistive memory R at all.
[0085] The upper electrode T and the lower electrode B may each contain titanium nitride, tantalum nitride, tungsten, copper, aluminum, gold, silver, platinum, titanium, or other conductive materials. The resistive conversion layer S may contain aluminum oxide, tantalum oxide, titanium oxide, hafnium oxide, or other metal oxides. The conductive pad 60b and the conductive plug 60a are made of copper, aluminum, nickel, tungsten, titanium, tantalum, or other conductive materials.
[0086] Please also refer to Figure 8 and Figure 17 The difference between the resistive memory structure 200 of the second preferred embodiment and the resistive memory structure 100 of the first preferred embodiment is as follows: Figure 17 A bird's-eye view Figure 6 As shown, viewed along the first direction Y, the conductive plug 60a is located at the center C3 of the conductive pad 60b and also at the center C4 of the resistive memory R. The center C5 of the conductive plug 60a overlaps with the center C3 of the conductive pad 60b and the center C4 of the resistive memory R. Other components are the same as in the first preferred embodiment and will not be described again here.
[0087] Please also refer to Figure 13 and Figure 17The difference between the resistive memory structure 300 of the third preferred embodiment and the resistive memory structure 100 of the first preferred embodiment is that, along the second direction X, the width of the conductive pad 60b is not greater than the width of the upper electrode T. According to a preferred embodiment of the present invention, the width of the conductive pad 60b is equal to the width of the upper electrode T. Furthermore, the conductive pad 60b includes a first sidewall W1, the conductive plug 60a includes a second sidewall W2, and the resistive memory R includes a third sidewall W3. The first sidewall W1, the second sidewall W2, and the third sidewall W3 are flush with each other. Additionally, a protrusion 70 protrudes from the first sidewall W1 along the second direction X. The upper surface of the protrusion 70 is flush with the upper surface of the conductive pad 60b. The conductive element 60 includes the conductive plug 60a, the conductive pad 60b, and the protrusion 70. The conductive element 60 is integrally formed. To clearly identify the element, the conductive plug 60a, the conductive pad 60b, and the protrusion 70 are separated by dashed lines. Figure 13 and Figure 17 A bird's-eye view Figure 7 As shown, viewed along the first direction Y, the area of the conductive pad 60b coincides with the area of the resistive memory R. The protrusion 70 extends outside the area of the conductive pad 60b, and the center C5 of the conductive plug 60a not only deviates from the center C3 of the conductive pad 60b, but also, viewed along the first direction Y, the conductive plug 60a and the protrusion 70 can form a complete rectangle. Other components are the same as in the first preferred embodiment and will not be described again here.
[0088] Please also refer to Figure 16 and Figure 17 The difference between the resistive memory structure 400 of the fourth preferred embodiment and the resistive memory structure 100 of the first preferred embodiment is as follows: Figure 17 A bird's-eye view Figure 8 As shown, viewed along the first direction Y, the conductive plug 60a is located at the center C3 of the conductive pad 60b and also at the center C4 of the resistive memory R. The center of the conductive plug 60a, the center C3 of the conductive pad 60b, and the center C4 of the resistive memory R overlap, and the area of the conductive pad 60b coincides with the area of the resistive memory R. Other components are the same as in the first preferred embodiment, and will not be described again here.
[0089] The manufacturing process of the conductive element of the present invention involves using a conductive pad pattern superimposed with a conductive plug pattern to form a conductive element pattern on a mask. After etching the second dielectric layer using the conductive element pattern as a template, a metal layer is filled in to form the conductive element. If the conductive pad pattern is used alone as a template to form the conductive element, there may be cases where the conductive element and the upper electrode do not make complete contact or do not make any contact at all. However, using a conductive pad pattern superimposed with a conductive plug pattern can ensure that the conductive element formed at the overlapping position can make complete contact with the upper electrode.
[0090] The above description is only a preferred embodiment of the present invention. All equivalent changes and modifications made in accordance with the claims of the present invention should be included within the scope of the present invention.
Claims
1. A resistive memory structure, comprising: First dielectric layer; A second dielectric layer covers the first dielectric layer; A resistive memory, with the first dielectric layer embedded therein, wherein the resistive memory includes a lower electrode, a resistive conversion layer and an upper electrode stacked sequentially from bottom to top; A conductive element is embedded in the second dielectric layer, wherein the conductive element comprises: A conductive plug that contacts the upper electrode; A conductive pad contacts the conductive plug and is positioned above the conductive plug; as well as The first direction is defined as the direction from the upper electrode toward the lower electrode, along which the conductive plug is offset from the center of the conductive pad.
2. The resistive memory structure as claimed in claim 1, wherein the second direction is defined as parallel to the upper surface of the first dielectric layer, and along the second direction, the width of the conductive pad is greater than the width of the upper electrode.
3. The resistive memory structure as claimed in claim 1, wherein the second direction is defined as parallel to the upper surface of the first dielectric layer, and along the second direction, the width of the conductive pad is not greater than the width of the upper electrode.
4. The resistive memory structure of claim 3, wherein the conductive pad includes a first sidewall, the conductive plug includes a second sidewall, the resistive memory includes a third sidewall, and the first sidewall, the second sidewall, and the third sidewall are flush with each other.
5. The resistive memory structure of claim 4 further includes a protrusion that protrudes from the first sidewall along a second direction, and the upper surface of the protrusion is flush with the upper surface of the conductive pad.
6. The resistive memory structure of claim 1, wherein the second direction is defined as parallel to the upper surface of the first dielectric layer, and along the second direction, the width of the conductive pad is greater than the width of the conductive plug.
7. The resistive memory structure of claim 1, wherein along the first direction, the thickness of the conductive pad is 5 to 10 times the thickness of the conductive plug.
8. The resistive memory structure as claimed in claim 1, wherein the conductive pad does not contact the resistive memory at all.
9. A method for fabricating a resistive memory structure, comprising: A first dielectric layer, a second dielectric layer, and a resistive memory are provided, wherein the second dielectric layer covers the first dielectric layer, the resistive memory is embedded in the first dielectric layer, and the resistive memory includes a lower electrode, a resistive switching layer, and an upper electrode stacked sequentially from bottom to top. A first mask layer and a second mask layer are formed to cover the second dielectric layer from bottom to top; The second mask layer and the first mask layer are etched to form a conductive pad pattern in the second mask layer and the first mask layer; A third mask layer is formed to cover the second mask layer and fill the conductive pad pattern; The third mask layer, the first mask layer, and the second dielectric layer are etched to form a conductive plug pattern in the conductive pad pattern, wherein the first direction is defined as from the upper electrode toward the lower electrode, and the conductive plug pattern is offset from the center of the conductive pad pattern when viewed along the first direction. After the conductive plug pattern is formed, the third mask layer is completely removed; Using the second mask layer and the first mask layer as masks, the second dielectric layer is etched to form a conductive element trench, and the upper electrode is exposed by the conductive element trench; as well as A metal layer is formed to fill the trench of the conductive element to form the conductive element.
10. The method for fabricating a resistive memory structure as claimed in claim 9, wherein the second direction is defined as parallel to the upper surface of the first dielectric layer, and along the second direction, the width of the conductive pad pattern is greater than the width of the upper electrode.
11. The method of manufacturing a resistive memory structure as claimed in claim 10, wherein, viewed along the first direction, the conductive plug pattern is completely located within the conductive pad pattern.
12. The method for fabricating a resistive memory structure as claimed in claim 10, wherein the second mask layer is not etched when etching the third mask layer, the first mask layer and the second dielectric layer to form the conductive plug pattern.
13. The method for fabricating a resistive memory structure as claimed in claim 9, wherein the second dielectric layer is not penetrated when etching the third mask layer, the first mask layer, and the second dielectric layer to form the conductive plug pattern.
14. The method for fabricating a resistive memory structure as claimed in claim 9, wherein the second mask layer is not penetrated when etching the second mask layer and the first mask layer to form the conductive pad pattern.
15. The method for fabricating a resistive memory structure as claimed in claim 9, wherein the second direction is defined as parallel to the upper surface of the first dielectric layer, and along the second direction, the width of the conductive pad pattern is not greater than the width of the upper electrode.
16. The method of manufacturing a resistive memory structure as claimed in claim 15, wherein, viewed along the first direction, the conductive plug pattern portion is located outside the conductive pad pattern.
17. The method of fabricating a resistive memory structure as claimed in claim 16, wherein when etching the third mask layer, the first mask layer and the second dielectric layer to form the conductive plug pattern, the second mask layer outside the conductive pad pattern is etched.
18. The method for fabricating a resistive memory structure as described in claim 15, wherein the conductive element comprises: A conductive plug that contacts the upper electrode; and A conductive pad contacts and is positioned above the conductive plug, wherein the conductive pad includes a first sidewall, the conductive plug includes a second sidewall, and the resistive memory includes a third sidewall, the first sidewall, the second sidewall, and the third sidewall are flush with each other.
19. The method of manufacturing a resistive memory structure as claimed in claim 18, wherein the conductive element further includes a protrusion that protrudes from the first sidewall along a second direction, and the upper surface of the protrusion is flush with the upper surface of the conductive pad.