A method for fabricating mercury cadmium telluride devices via high-energy ion low-damage implantation
By forming a double-layer mask structure of thin film and photoresist on the surface of mercury cadmium telluride device, combined with wet etching process, the damage problem caused by high-energy ion implantation is solved, and low-damage high-energy ion implantation is achieved, which improves the electrical performance and yield of the device.
Patent Information
- Application Number
- CN202611324841.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-28
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the high-energy ion implantation process damages mercury cadmium telluride materials, leading to leakage current on the device surface. Furthermore, the mask is difficult to remove completely, affecting device performance and yield.
A dual-layer mask structure consisting of a thin film and photoresist is adopted, combined with a wet etching process. The mask is formed on the surface of mercury cadmium telluride material through photolithography and wet chemical etching, which reduces the complexity of mask removal and minimizes injection damage.
It effectively reduces implantation damage on the surface of P-on-N type mercury cadmium telluride devices, lowers surface leakage current, optimizes the high-energy ion implantation process, and improves the electrical performance and yield of the devices.
Smart Images

Figure CN123124685A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor device fabrication technology, and in particular to a method for fabricating mercury cadmium telluride devices by high-energy ion implantation with low damage. Background Technology
[0002] Based on device structure, mercury cadmium telluride (HCdTe) infrared focal plane array devices include N-on-P structure devices and P-on-N structure devices. In existing technologies, N-on-P technology has achieved stable process technology, reliable device performance, and large-scale production capabilities. However, with the increasing demands on the performance of HCdTe detectors, some inherent defects of N-on-P technology are becoming increasingly apparent, limiting its further development. First, as a narrow bandgap semiconductor device, the N-on-P homojunction HCdTe detector results in a higher probability of direct tunneling due to its narrow bandgap, leading to a larger direct tunneling current. Second, in N-on-P ion-implanted planar junction devices, the P-type absorber layer is achieved through Hg vacancy defect doping, but the Hg vacancy concentration is difficult to control precisely, and Hg vacancies themselves easily form recombination defect centers, increasing dark current. Therefore, it is difficult to obtain high-performance P-type HgCdTe materials based on Hg vacancy doping. Value N-on-P planar junction device.
[0003] P-on-N structure devices benefit from significantly reduced dark current, The significant improvement in charge density and longer minority carrier lifetime have made cadmium telluride (HCTM) infrared focal plane array (PFLAG) devices a key trend in their development. Ion implantation is the primary process for forming pn junctions in HCTM infrared PFLAG devices, using photolithography to create photoresist mask patterns to define the implantation region. However, the high-energy ion implantation process inevitably causes implantation damage to the mercury cadmium telluride material, resulting in surface leakage in the device, which affects the electrical performance and yield of the device. Existing technologies are unable to effectively reduce implantation damage. Furthermore, the mask may deform or crack during the high-energy ion implantation process, making it difficult to remove the mask completely and degrading the device performance. Summary of the Invention
[0004] To address the shortcomings of the existing technology, this invention provides a method for fabricating a mercury cadmium telluride device using high-energy ion implantation with low damage, employing the following technical solution: A method for fabricating a mercury cadmium telluride device via high-energy ion implantation with low damage is provided, comprising: Thin films were prepared on the surface of mercury cadmium telluride devices; A photolithography process is performed on the surface of the thin film to form a photoresist mask pattern in the injection area, thus forming a two-layer mask structure of thin film and photoresist. The thin film in the implantation area is removed by using an etching solution, exposing the implantation area that needs to be implanted with high-energy ions; A high-energy ion implantation process is performed in the implantation region to form a P-on-N type mercury cadmium telluride device; The P-on-N type mercury cadmium telluride device was de-adhesive-treated using acetone solution; The remaining film is removed from the P-on-N type mercury cadmium telluride device after the adhesive removal process is completed using the etching solution; Cleaning completes the process.
[0005] This application has the following beneficial effects: This application proposes a dual-layer mask structure of thin film + photoresist by combining wet etching process, successfully obtaining a planar structure that is simple to fabricate, has minimal implantation damage, and is easy to remove. The photomask pattern is transferred onto a thin film using photolithography and wet chemical etching techniques, thus forming a dual-layer mask structure of thin film + photoresist on the surface of HgCdTe material. This reduces the complexity of mask removal, effectively reduces implantation damage on the surface of P-on-N type HgCdTe devices, thereby reducing the surface leakage current of the P-type implantation region, optimizing the high-energy ion implantation process, and improving the electrical performance and product yield of the device. Attached Figure Description
[0006] Figure 1 A schematic flowchart illustrating a method for fabricating a mercury cadmium telluride device using high-energy ion low-damage implantation, as provided in an embodiment of this application. Figure 2 An effect diagram of a dual-layer mask layer provided in an embodiment of this application; Figure 3 A damage effect diagram of a single-layer mask high-energy ion implantation provided for an embodiment of this application; Figure 4 This image shows a comparison of the injection results of a double-layer mask layer (ZnS thin film + photoresist) and a single-layer photoresist mask layer, as provided in an embodiment of this application. Detailed Implementation
[0007] To further illustrate the technical means and effects adopted by the present invention to achieve its intended purpose, the technical solutions in the embodiments of this application are clearly described. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art are within the scope of protection of this application.
[0008] The terms "first," "second," etc., used in the specification and claims of this application are used to distinguish similar objects and not to describe a specific order or sequence. It should be understood that such terms can be used interchangeably where appropriate so that embodiments of this application can be implemented in orders other than those illustrated or described herein, and the objects distinguished by "first," "second," etc., are generally of the same class and the number of objects is not limited; for example, a first object can be one or more. Furthermore, in the specification, "and / or" indicates at least one of the connected objects, and the character " / " generally indicates that the preceding and following objects are in an "or" relationship.
[0009] The steps described in this application and the flowcharts in the accompanying drawings are not necessarily strictly executed according to the step numbers; the execution order of the steps can be changed. Furthermore, certain steps can be omitted, multiple steps can be combined into one step, and / or one step can be broken down into multiple steps.
[0010] This specification provides a method for fabricating a mercury cadmium telluride device using high-energy ion implantation with low damage. The following detailed description is provided in conjunction with the accompanying drawings and preferred embodiments.
[0011] Please see Figure 1-4 This application provides a method for fabricating a mercury cadmium telluride device using high-energy ion low-damage implantation, comprising: Step S1: Prepare a thin film on the surface of the mercury cadmium telluride device; Step S2: Perform photolithography on the surface of the thin film to form a photoresist mask pattern in the injection area, thus forming a double-layer mask structure of thin film and photoresist. Step S3: Use an etching solution to etch and remove the thin film in the implantation area, exposing the implantation area that needs to be implanted with high-energy ions; Step S4: Perform a high-energy ion implantation process in the implantation region to form a P-on-N type mercury cadmium telluride device; Step S5: Use acetone solution to remove the adhesive from the P-on-N type mercury cadmium telluride device; Step S6: Use the etching solution to remove the remaining film from the P-on-N type mercury cadmium telluride device after the adhesive removal is completed; Step S7: Cleaning, process complete.
[0012] This application proposes a dual-layer mask structure of thin film + photoresist by combining wet etching process, successfully obtaining a planar structure that is simple to fabricate, has minimal implantation damage, and is easy to remove. The photomask pattern is transferred onto a thin film using photolithography and wet chemical etching techniques, thus forming a dual-layer mask structure of thin film + photoresist on the surface of HgCdTe material. This reduces the complexity of mask removal, effectively reduces implantation damage on the surface of P-on-N type HgCdTe devices, thereby reducing the surface leakage current of the P-type implantation region, optimizing the high-energy ion implantation process, and improving the electrical performance and product yield of the device.
[0013] Furthermore, the thin film material is ZnS, CdTe or graphene.
[0014] Furthermore, the thin film preparation on the surface of the mercury cadmium telluride device includes a coating method comprising magnetron sputtering, ion beam deposition, thermal evaporation, or PECVD.
[0015] Furthermore, the film thickness is 1–10000 nm.
[0016] Furthermore, the corrosive solution includes HCl, , , One or more of the following mixed solutions.
[0017] Furthermore, the thin film in the injection area is removed by etching with an etching solution. The etching process is carried out at an ice water temperature and the etching time is 1 second to 5 minutes.
[0018] Furthermore, during ion implantation, the substrate temperature is controlled within the range of 0–50°C, the implantation angle is 7°, the implantation energy range is 10–600 keV, and the implantation dose range is 1E13–1E16. .
[0019] Further, step S5, which involves removing the adhesive from the P-on-N type mercury cadmium telluride device using an acetone solution, includes: The P-on-N type mercury cadmium telluride device is immersed in acetone solution to remove photoresist, then immersed in ethanol solution to remove residual acetone solution, and finally rinsed with deionized water to remove ethanol solution.
[0020] Furthermore, the remaining film of the P-on-N type mercury cadmium telluride device after the adhesive removal is completed is removed using the etching solution. The etching process is carried out at room temperature and the etching time is 5 to 20 minutes.
[0021] Furthermore, the cleaning includes: The device surface is then cleaned with acetone and ethanol solutions after being immersed in a trichloroethylene solution to remove the thermally conductive coolant (derived from the ion implantation process).
[0022] For example, the following provides a specific implementation process: Step S101: Prepare a thin film with a thickness ranging from 10 to 10000 nm on the surface of a P-on-N type mercury cadmium telluride device; Step S102: Using photolithography, a photoresist mask pattern for the injection region is formed on the surface of the P-on-N type mercury cadmium telluride device; Step S103: Use an etching solution to etch the thin film on the surface of the implantation area. Place the P-on-N type mercury cadmium telluride device into the fixture, and then immerse the fixture in an etching solution at the temperature of an ice-water mixture for wet etching. During the etching process, the etching solution should be stirred continuously to ensure that the etching solution is evenly distributed throughout the chip. The etching time is 1s to 5min, exposing the implantation area that needs to be implanted with high-energy ions. Step S104: High-energy ion implantation is performed on the processed device using an ion implanter. During the implantation process, the substrate temperature is controlled at -10~50℃, the implantation angle is 0-15°, the implantation energy range is 10~800keV, and the implantation dose range is 1E13~1E16. ; Step S105: Take out the P-on-N type mercury cadmium telluride device after implantation and immerse it in acetone solution to remove the photoresist on the patterned surface. Then immerse it in ethanol solution to remove the residual acetone solution. Finally, rinse the ethanol solution with deionized water. Step S106: Take out the injected P-on-N type mercury cadmium telluride device and place it in the fixture. Then place the fixture into the hydrochloric acid etching solution at room temperature for wet etching. During the etching process, the etching solution should be stirred continuously to ensure that the etching solution is evenly distributed throughout the chip. The etching time is 1 min to 20 min to fully etch away the ZnS on the surface of the device. Step S107: Immerse the P-on-N type mercury cadmium telluride device after wet etching in trichloroethylene solution to remove lipid residues, then clean the P-on-N type mercury cadmium telluride device with acetone and ethanol, and finally rinse the ethanol solution with deionized water to complete the process.
[0023] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or apparatus. Without further limitations, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or apparatus that includes that element. Furthermore, it should be noted that the scope of the methods and apparatuses in the embodiments of this application is not limited to performing functions in the order shown or discussed, but may also include performing functions substantially simultaneously or in the reverse order, depending on the functions involved. For example, the described methods may be performed in a different order than described, and various steps may be added, omitted, or combined. Additionally, features described with reference to certain examples may be combined in other examples.
[0024] It is understood that the embodiments of this application have been described above in conjunction with the accompanying drawings. However, this application is not limited to the specific embodiments described above. The specific embodiments described above are merely illustrative and not restrictive. As those skilled in the art will know, various changes or equivalent substitutions can be made to these features and embodiments without departing from the spirit and scope of the invention. Furthermore, those skilled in the art, under the guidance or instruction of this application, can modify these features and embodiments to adapt to specific situations and materials without departing from the spirit and scope of the invention. Therefore, this invention is not limited to the specific embodiments disclosed herein, and all embodiments falling within the scope of the claims of this application are within the protection scope of this invention.
Claims
1. A method for preparing a high-energy ion low-damage implanted mercury cadmium telluride device, the method comprising: include: Thin films were prepared on the surface of mercury cadmium telluride devices; A photolithography process is performed on the surface of the thin film to form a photoresist mask pattern in the injection area, thus forming a two-layer mask structure of thin film and photoresist. The thin film in the implantation area is removed by using an etching solution, exposing the implantation area that needs to be implanted with high-energy ions; A high-energy ion implantation process is performed in the implantation region to form a P-on-N type mercury cadmium telluride device; The P-on-N type mercury cadmium telluride device was de-adhesive-treated using acetone solution; The remaining film is removed from the P-on-N type mercury cadmium telluride device after the adhesive removal process is completed using the etching solution; Cleaning completes the process.
2. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The thin film material is ZnS, CdTe or graphene.
3. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The method for preparing a thin film on the surface of a mercury cadmium telluride device includes magnetron sputtering, ion beam deposition, thermal evaporation, or PECVD.
4. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The film thickness ranges from 1 to 10,000 nm.
5. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The aforementioned method involves using an etching solution to remove the thin film in the injection area. The etching process is carried out at an ice water temperature and takes 1 second to 5 minutes.
6. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The remaining film of the P-on-N type mercury cadmium telluride device after the adhesive removal is completed is removed using the etching solution. The etching process is carried out at room temperature and the etching time is 5 to 20 minutes.
7. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The etching solution includes a mixture of one or more of HCl, , , .
8. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The process of removing the adhesive from the P-on-N type mercury cadmium telluride device using acetone solution includes: The P-on-N type mercury cadmium telluride device is immersed in acetone solution to remove photoresist, then immersed in ethanol solution to remove residual acetone solution, and finally rinsed with deionized water to remove ethanol solution.
9. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The cleaning includes: The device surface is then cleaned with acetone and ethanol solutions after being immersed in a trichloroethylene solution to remove the thermally conductive coolant (derived from the ion implantation process).
10. The method for fabricating a mercury cadmium telluride device by high-energy ion low-damage implantation according to claim 1, characterized in that, The substrate temperature during ion implantation is controlled in the range of 0-50°C, the implantation angle is 7°, the implantation energy range is 10-600 KeV, and the implantation dose range is 1E13-1E16 .