A rapid detection method for glass substrate structure and glass through-hole sputtering seed layer
By setting test key areas on the glass substrate and forming current paths using laser cutting, the problem of cumbersome and time-consuming testing in the prior art is solved, enabling rapid and non-destructive testing of the seed layer thickness of the glass substrate and realizing online monitoring during mass production.
Patent Information
- Application Number
- CN202611206395.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-10
- Publication Date
- 2026-11-17
AI Technical Summary
In the existing technology, the method for detecting the thickness of the through-hole metal seed layer in glass substrates is cumbersome, time-consuming, and destructive, and cannot achieve online monitoring during mass production.
Test key areas are set on a glass substrate, and current paths are formed by laser cutting. The thickness of the seed layer on the sidewall is measured by resistance measurement, achieving non-destructive and rapid detection.
It enables rapid, non-destructive testing of the seed layer thickness on glass substrates, avoiding material waste and allowing online monitoring of seed layer coverage quality during mass production.
Smart Images

Figure CN123124753A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor packaging inspection, and more specifically, to a rapid inspection method for glass substrate structure and glass through-hole sputtering seed layer. Background Technology
[0002] Through-glass via (TGV) technology has significant application prospects in 5G communications, optoelectronics, and advanced packaging due to its advantages such as high frequency, low loss, high insulation, and thermal stability. Large-size TGV glass substrates are key carriers for realizing high-density interconnects and high-speed signal transmission, and play a driving role in upgrading computing power in fields such as AI chips and data centers.
[0003] One of the core processes of TGV technology is through-hole metallization, which involves depositing a continuous metal seed layer on the inner wall of a TGV via using sputtering to provide a conductive substrate for subsequent electroplating. During sputtering, an RF bias is typically applied to the substrate stage to form a plasma sheath, accelerating ionized metal target particles and depositing them on the via sidewalls. The quality of the seed layer deposition is usually measured by step coverage, which is the ratio of the seed layer thickness in the middle of the via sidewall to the seed layer thickness on the outer side of the via opening. Since the middle of the via is furthest from the sputtering source during double-sided sputtering, the seed layer thickness at this location is the thinnest, making it the weakest point in the overall seed layer coverage.
[0004] Currently, the main method for assessing the seed layer thickness within TGV vias is to cleave the glass substrate and observe the cross-section using a scanning electron microscope or focused ion beam to directly measure the sidewall seed layer thickness. This method has the following problems: it is cumbersome, time-consuming, and has high equipment costs; cleaving is a destructive test, meaning the tested substrate cannot be reused in production, resulting in waste; and it only allows for sampling inspection, making daily monitoring of substrates during mass production impossible. Summary of the Invention
[0005] In order to overcome the shortcomings of the prior art, the technical problem to be solved by the present invention is to propose a glass substrate structure and a rapid detection method for sputtered seed layer in glass through-holes, which can quickly detect the thickness of the metal seed layer on the sidewall of the through-hole without damaging the glass substrate, and realize online monitoring of the seed layer coverage quality during mass production.
[0006] To achieve this objective, the present invention adopts the following technical solution:
[0007] The present invention also provides a glass substrate structure, including a glass substrate structure for detecting glass through-hole sputtering seed layers, wherein at least one test key area is provided thereon, and the test key area has at least two sets of glass through-holes; the upper surface, lower surface and sidewalls of each glass through-hole of the glass substrate structure for detecting glass through-hole sputtering seed layers are covered with metal seed layers; on the upper or lower surface of the glass substrate structure for detecting glass through-hole sputtering seed layers, the metal seed layers between each set of glass through-holes are cut to form isolation grooves to expose the glass substrate, thereby disconnecting the metal seed layers of each set of glass through-holes on that surface.
[0008] This invention also provides a method for rapid detection of sputtered seed layers in glass vias of glass substrates, comprising the following steps:
[0009] At least one test key area is provided on the glass substrate, and the test key area has at least two sets of glass through holes;
[0010] The glass substrate is sputtered to form a metal seed layer on the upper surface, lower surface and sidewalls of each glass via.
[0011] On the upper or lower surface of the glass substrate, the metal seed layer between each group of glass vias in the same test key area is cut open until the glass substrate is exposed, so that the metal seed layers of each group of glass vias on this surface are disconnected from each other.
[0012] The resistance between the metal seed layer on the surface of any two sets of glass vias within the same test key area is measured, and the magnitude of the resistance characterizes the thickness of the metal seed layer on the sidewall of the glass via.
[0013] In a preferred embodiment of the present invention, the cutting method is laser cutting.
[0014] In a preferred embodiment of the present invention, the test key area has at least three sets of glass through holes, and the resistance between any two sets is measured and the average value is taken, with the average value representing the thickness.
[0015] In a preferred embodiment of the present invention, the metal seed layer is formed by stacking a Ti layer and a Cu layer, wherein the Ti layer is located between the glass substrate and the Cu layer.
[0016] In a preferred embodiment of the present invention, the sputtering is magnetron sputtering.
[0017] In a preferred embodiment of the present invention, the resistance is compared with a preset threshold. If the resistance is greater than the preset threshold, the thickness is determined to be unsatisfactory.
[0018] In a preferred embodiment of the present invention, the preset threshold is obtained by performing the steps on a calibration substrate.
[0019] In a preferred embodiment of the present invention, the thickness of the metal seed layer in the middle of the glass through-hole sidewall is less than the thickness of the metal seed layer at both ends of the glass through-hole sidewall.
[0020] In a preferred embodiment of the present invention, the number of through holes in each group of glass through holes within the same test key area is equal.
[0021] The beneficial effects of this invention are as follows:
[0022] This invention provides a special pipe connector for the inverted method of large-diameter well pipes, which can quickly connect and fix two vertically oriented pipes. By pre-setting a test key area on a glass substrate, and cutting the metal seed layer between each group of glass vias within the same test key area after sputtering, the groups are disconnected on one surface of the substrate, thus forming a current path from that surface through the sidewalls of each group of vias to the other surface of the substrate and back. Based on this, by simply measuring the resistance between the metal seed layers of any two groups of glass vias on that surface, the thickness of the metal seed layer on the sidewall of the via can be characterized by the resistance; a higher resistance indicates a thinner sidewall seed layer and poorer coverage quality. The entire testing process does not require dicing the substrate, thus avoiding damage to the substrate structure. The tested substrate can continue to be used in subsequent production processes, fundamentally avoiding the material waste caused by existing dicing methods. Furthermore, this application only requires two steps—cutting and resistance measurement—on the same surface, without flipping or double-sided contact, making operation convenient and testing fast. Compared with existing scanning electron microscopes or focused ion beam cross-sectional observation methods, it significantly shortens the time required for a single test. Furthermore, this application allows for the flexible setting of one or more test key areas on the same glass substrate, enabling random sampling and testing after the sputtering process, thus truly achieving online monitoring of seed layer coverage quality during mass production. When three or more sets of glass vias are set within the same test key area, the resistance between any two sets can be measured separately and averaged, effectively reducing the interference of occasional defects in a single via on the measurement results and further improving the reliability of the test. Attached Figure Description
[0023] Figure 1 This is a cross-sectional schematic diagram of the glass through-hole according to a specific embodiment of the present invention;
[0024] Figure 2 This is a schematic diagram of the structure of the metal seed layer cutting the glass substrate in a specific embodiment of the present invention;
[0025] Figure 3 yes Figure 2 Schematic diagram of the cross-section at point A;
[0026] Figure 4A schematic diagram for measuring the resistance between two sets of glass vias.
[0027] Figure 5 This is a schematic diagram of the glass substrate structure according to a specific embodiment of the present invention;
[0028] Figure 6 for Figure 5 Enlarged structural diagram at point B;
[0029] Figure 7 This is a schematic diagram of the structure of a glass substrate after sputtering deposition, according to a specific embodiment of the present invention.
[0030] Figure 8 for Figure 7 Enlarged structural diagram at point C;
[0031] Figure 9 This is a schematic diagram of the structure of three sets of glass through holes according to a specific embodiment of the present invention;
[0032] Figure 10 for Figure 9 A schematic diagram of the glass through-hole cross-section measurement structure.
[0033] In the picture:
[0034] 1. Glass substrate; 2. Glass via; 3. Metal seed layer; 31. Outside of via opening; 32. Middle sidewall of via; 33. Opening of metal seed layer; 4. Test key area; 51. Impedance test meter; 52. Meter needle. Detailed Implementation
[0035] The technical solution of the present invention will be further described below with reference to the accompanying drawings and specific embodiments.
[0036] like Figure 1 As shown, the technical principle of this invention will first be briefly explained. In the glass through-hole sputtering process, since the center of the through-hole is farthest from the sputtering target, the deposition thickness of the metal seed layer 3 is smallest in the center of the through-hole sidewall. Taking a typical specification with an aspect ratio of 10:1 as an example, the thickness of the metal seed layer 3 in the center of the through-hole sidewall is only about 3% of the thickness of the metal seed layer 3 on the substrate surface. This location is a weak point in the seed layer coverage and is also the key to evaluating the step coverage capability. This invention utilizes this physical characteristic to construct a current path with the metal seed layer 3 on the through-hole sidewall as the dominant resistance, transforming the sidewall thickness, which is difficult to measure directly, into an easily measurable resistance value, thereby achieving rapid and non-destructive online detection.
[0037] like Figures 1-8As shown, the detection method provided by this invention firstly involves setting at least one test bonding region 4 on a glass substrate 1, with at least two sets of glass vias 2 within the test bonding region 4. A glass substrate 1 is provided, with dimensions of 510mm × 515mm and a thickness of 500μm. One or more test bonding regions 4 are set at the center or edge of the glass substrate 1, with a side length of 2mm to 10mm. The via specifications of each set of glass vias 2 within the test bonding region 4 are consistent with the specifications of glass vias 2 in the remaining functional areas of the substrate, ensuring that the detection results of the test bonding region 4 can represent the seed layer coverage of the entire board. The diameter of the glass vias 2 can be from 10μm to 100μm; taking a via diameter of 50μm as an example, the corresponding aspect ratio is approximately 10:1. The number of vias in each set of glass vias 2 within the same test bonding region 4 is equal, with each set containing 5 to 100 vias.
[0038] After the test key area 4 is set up, sputtering is performed on the glass substrate 1. The sputtering method is magnetron sputtering, forming a continuous metal seed layer 3 on the upper and lower surfaces of the glass substrate 1, as well as on the sidewalls of each glass via 2. The metal seed layer 3 is formed by stacking Ti and Cu layers. The Ti layer is located between the glass substrate 1 and the Cu layer, acting as a bonding layer, while the Cu layer acts as a conductive layer. Due to the characteristics of the sputtering process, the metal seed layer 3 is deposited throughout the entire depth of the via sidewall, from the opening through the middle of the sidewall to the opening on the other surface, forming a continuous sidewall seed layer. The thickness of the metal seed layer 3 is greatest at the outer side 31 of the via opening; extending towards the middle of the via sidewall, the thickness of the metal seed layer 3 gradually decreases, reaching its minimum at the middle of the via sidewall; continuing towards the other surface, the thickness of the metal seed layer 3 gradually increases again. Therefore, the thickness of the metal seed layer 3 in the middle of the via sidewall is less than the thickness of the metal seed layer 3 at both ends of the via sidewall.
[0039] After sputtering, the metal seed layer 3 between each group of glass vias 2 within the same test bond area 4 is cut on the upper or lower surface of the glass substrate 1. The cutting method is laser cutting, and the cutting depth must penetrate the metal seed layer 3 until the glass substrate 1 is exposed, thus breaking the metal seed layer 3 between each group of glass vias 2 on that surface, forming a metal seed layer opening 33 at the cut. The other surface of the glass substrate 1 does not require cutting, and the metal seed layer 3 on it remains in its original continuous, full-surface coverage state.
[0040] Taking two groups of glass vias 2, A and B, within the same test key area 4 as an example, after cutting, the metal seed layer 3 of group A and group B on this surface are completely disconnected, and the two are no longer connected on this surface. However, a continuous metal seed layer 3 is deposited on the sidewall of each glass via 2 in group A. This sidewall seed layer extends from this surface to the other surface of the substrate and communicates with the metal seed layer 3 on the other surface of the substrate. The metal seed layer 3 on the other surface of the substrate is a continuous coverage, with one end communicating with the metal seed layer 3 on the sidewall of each via in group A and the other end communicating with the metal seed layer 3 on the sidewall of each via in group B. The metal seed layer 3 on the sidewall of each via in group B extends back from the other surface of the substrate to this surface. Therefore, starting from the metal seed layer 3 on the surface of group A, the path extends through the metal seed layers 3 on the sidewalls of each via of group A to the metal seed layer 3 on the other surface of the substrate. It then moves laterally along the metal seed layer 3 on that other surface to the corresponding positions on the sidewalls of each via of group B, and finally returns through the metal seed layers 3 on the sidewalls of each via of group B to the metal seed layer 3 on the surface of group B, forming a complete electrical connection path. Since the thickness of the metal seed layer 3 in the middle of the via sidewall is much smaller than the thickness of the metal seed layer 3 on the substrate surface, the resistance of the metal seed layer 3 on the via sidewall is much greater than the resistance of the metal seed layer 3 on the substrate surface. Within the small space of the test key area 4, which is only a few millimeters square, the resistance of the metal seed layers 3 on the operating surface and the other surface can be ignored. The resistance of the entire electrical connection path is mainly contributed by the series connection of the resistances of the metal seed layers 3 on the sidewalls of each via of group A and the metal seed layers 3 on the sidewalls of each via of group B.
[0041] Within group A, each glass via 2 can be considered an independent resistive element, the resistance of which is the resistance of the metal seed layer 3 on the sidewall of that via. Since the top of all vias in the group is connected to the metal seed layer 3 on that surface of group A, and the bottom is connected to the metal seed layer 3 on the other surface of the substrate, the sidewall resistances of each via within the group are in parallel. The total sidewall resistance Ra of group A is the parallel equivalent value of the sidewall resistances R1a, R2a, ..., Rna of each via within the group, i.e., Ra = 1 / (1 / R1a + 1 / R2a + ... + 1 / Rna), where n is the number of glass vias 2 in group A. Similarly, the total sidewall resistance Rb of group B = 1 / (1 / R1b + 1 / R2b + ... + 1 / Rnb). In the electrical connection path, the sidewall resistances of group A and group B are in series, and the total resistance R is equal to the sum of the two, i.e., R = Ra + Rb.
[0042] Based on the electrical connection path formed after the single-sided cutting, using an impedance meter 51, the two probes 52 are respectively brought into contact with the metal seed layer 3 on the surface of any two sets of glass vias 2 within the same test key area 4, with the probes 52 avoiding the openings 33 of the metal seed layer. The resistance between the two sets can then be measured. Taking groups A and B as examples, the measured resistance is R = Ra + Rb. The magnitude of this resistance characterizes the thickness of the metal seed layer 3 on the sidewall of the via. Specifically, given the substrate specifications, via specifications, and sputtering process conditions, the thinner the metal seed layer 3 on the sidewall of the via, the greater the resistance, and the larger the measured resistance value. Therefore, the measured resistance can be compared with a preset threshold. If the resistance is greater than the preset threshold, the thickness is determined to be insufficient. The preset threshold is obtained by performing all the above steps on a calibration substrate.
[0043] like Figures 9-10 As shown, when there are at least three sets of glass vias 2 within the same test key area 4, the resistance between any two sets is measured and the average value is taken. The average value is used to characterize the thickness of the metal seed layer 3 on the sidewall of the via. Taking three sets of glass vias 2 as an example, they are denoted as group A, group B, and group C, respectively. The number of vias in each group within the same test key area 4 is equal. After laser cutting, the metal seed layers 3 of groups A, B, and C on this surface are disconnected from each other. During measurement, the resistance between group A and group B, Rab = Ra + Rb, the resistance between group A and group C, Rac = Ra + Rc, and the resistance between group B and group C, Rbc = Rb + Rc are measured respectively, and the arithmetic mean of the three resistance values is taken. Extending this further, if there are n sets of glass vias 2 within the test key area 4 and n≥3, any two sets can be selected for pairing, resulting in n×(n-1) / 2 sets of resistance measurement data. The average value of all data is taken as the judgment criterion. Taking the average of multiple sets can effectively reduce the interference of occasional defects in a single through hole on the measurement results, making the test results more reflective of the true level of seed layer coverage in the test key area 4.
[0044] This invention also provides a glass substrate 1 structure for the above-described detection method, comprising a glass substrate structure for glass through-hole sputtering seed layer detection, wherein at least one test key region 4 is provided, and the test key region 4 has at least two sets of glass through-holes 2. The upper surface, lower surface, and sidewalls of each glass through-hole 2 of the glass substrate structure for glass through-hole sputtering seed layer detection are all covered with a metal seed layer 3. On the upper or lower surface of the glass substrate structure for glass through-hole sputtering seed layer detection, the metal seed layer 3 between each set of glass through-holes 2 is cut to form an isolation groove, exposing the glass substrate 1, thus disconnecting the metal seed layer 3 of each set of glass through-holes 2 from each other on that surface. This glass substrate 1 structure, through a single-sided cut isolation construction, establishes a series detection path with the seed layer on the sidewall of the through-hole as the dominant resistance, providing a structural basis for the aforementioned detection method. Other techniques in this embodiment adopt existing technologies. This invention has been described through preferred embodiments; those skilled in the art will understand that various changes or equivalent substitutions can be made to these features and embodiments without departing from the spirit and scope of the invention. This invention is not limited to the specific embodiments disclosed herein, and other embodiments falling within the scope of the claims of this application are also within the protection scope of this invention.
Claims
1. A glass substrate structure, characterized in that, A glass substrate structure including a glass substrate (1) for glass through-hole sputtering seed layer detection, wherein at least one test key area (4) is provided thereon, and the test key area (4) has at least two sets of glass through-holes (2); the upper surface, lower surface and sidewalls of each glass through-hole (2) of the glass substrate structure for glass through-hole sputtering seed layer detection are covered with metal seed layers (3); on the upper or lower surface of the glass substrate structure for glass through-hole sputtering seed layer detection, the metal seed layers (3) between each set of glass through-holes (2) are cut to form isolation grooves and expose the glass substrate (1), so that the metal seed layers (3) of each set of glass through-holes (2) on this surface are disconnected from each other.
2. A rapid detection method for sputtered seed layers in glass through-holes, used to detect the glass substrate structure as described in claim 1, characterized in that, Includes the following steps: At least one test key area (4) is provided on the glass substrate (1), and the test key area (4) has at least two sets of glass through holes (2). Sputtering is performed on the glass substrate (1) to form a metal seed layer (3) on the upper surface, lower surface and sidewalls of each glass through hole (2). On the upper or lower surface of the glass substrate (1), the metal seed layer (3) between each group of glass through holes (2) in the same test key area (4) is cut open until the glass substrate (1) is exposed, so that the metal seed layer (3) of each group of glass through holes (2) on this surface is disconnected from each other. Measure the resistance between any two sets of glass vias (2) in the same test key area (4) and the metal seed layer (3) on the surface. The magnitude of the resistance characterizes the thickness of the metal seed layer (3) on the sidewall of the glass via (2).
3. The rapid detection method for glass through-hole sputtered seed layer according to claim 2, characterized in that, The cutting method is laser cutting.
4. The rapid detection method for glass through-hole sputtered seed layer according to claim 2, characterized in that, The test key area (4) has at least three sets of glass through holes (2). The resistance between any two sets is measured and the average value is taken to characterize the thickness.
5. The rapid detection method for glass through-hole sputtered seed layer according to claim 2, characterized in that, The metal seed layer (3) is formed by stacking a Ti layer and a Cu layer, with the Ti layer located between the glass substrate (1) and the Cu layer.
6. The rapid detection method for glass through-hole sputtered seed layer according to claim 2, characterized in that, The sputtering is magnetron sputtering.
7. The rapid detection method for glass through-hole sputtered seed layer according to claim 2, characterized in that, The resistance is compared with a preset threshold. If the resistance is greater than the preset threshold, the thickness is determined to be unacceptable.
8. The rapid detection method for glass through-hole sputtered seed layer according to claim 7, characterized in that, The preset threshold is obtained by performing the steps on a calibration substrate.
9. The rapid detection method for glass through-hole sputtered seed layer according to claim 1, characterized in that, The thickness of the metal seed layer (3) in the middle of the sidewall of the glass through hole (2) is less than the thickness of the metal seed layer (3) at both ends of the sidewall of the glass through hole (2).
10. The rapid detection method for glass through-hole sputtered seed layer according to claim 1, characterized in that, The number of through holes in each group of glass through holes (2) in the same test key area (4) is equal.