A packaging method based on extended TMV process

By using the extended TMV process, the problem of the limited capability of the TMV process in extremely small apertures was solved, realizing high aspect ratio interconnects and double-sided electrical interconnects of thick chips, simplifying the process flow and improving reliability.

CN123124849APending Publication Date: 2026-11-17NANJING RES INST OF ELECTRONICS TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610493574.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-04-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing TMV technology has limited capabilities in extremely small hole diameters, making it difficult to achieve high aspect ratio and high-quality drilling, and the TMV process for high aspect ratio requirements is complex.

Method used

The process employs an extended TMV process, which includes steps such as chip and adapter board mounting, ball placement, encapsulation, separation, rewiring, thinning and polishing, and ball placement. By using laser and mechanical methods, the TMV interconnect length is extended to achieve double-sided interconnection.

Benefits of technology

It effectively extends the TMV interconnect length, making it suitable for thick chip packaging, simplifying the process flow, and improving integration and interconnect reliability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124849A_ABST
    Figure CN123124849A_ABST
Patent Text Reader

Abstract

This invention discloses a packaging method based on extended TMV process, belonging to integrated circuit packaging technology. The specific method includes: mounting a chip and an adapter board onto a temporary carrier board; performing ball bonding on the pads of the adapter board; molding the chip and the adapter board to form a molding compound; separating the molding compound from the temporary carrier board; performing redistribution on the lower surface of the molding compound; thinning and polishing the upper surface of the molding compound until the ball bonding metal bumps on the upper surface of the adapter board are exposed; and performing ball bonding on the ball bonding metal bumps on the upper surface of the molding compound and the redistribution areas on the lower surface. This method can effectively extend the TMV interconnect length, which is beneficial for the molding interconnect of thick chips.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to integrated circuit packaging technology, specifically a packaging method based on extended TMV process. Background Technology

[0002] Through Molding Via (TMV) is a vertical interconnect structure formed within molding compound to achieve electrical connections between layers. TMV has relatively low manufacturing costs, a short process flow, and relatively low technical difficulty. Through-holes can be directly formed through laser ablation, and then conductive materials are filled into the through-holes via sputtering and electroplating to achieve interlayer interconnection. As a vertical interconnect technology, TMV has certain advantages in the field of microelectronic packaging, especially in terms of cost and process complexity. Using nanosecond or microsecond lasers with process optimization, through-holes with steep sidewalls (angles approaching 88°) and high aspect ratios can be fabricated. However, this method has relatively limited capabilities for extremely small apertures (e.g., less than 50 μm). Using picosecond and femtosecond lasers, their "cold processing" characteristics can effectively reduce thermal effects, theoretically enabling drilling of smaller apertures, higher aspect ratios, and higher quality holes. GHz femtosecond laser technology holds even greater promise for overcoming the taper problem of traditional laser-based hole formation, fabricating through-holes with high aspect ratios and no taper.

[0003] For TMV (Through Molding Via) with high aspect ratio requirements, alloy balls can be implanted first, followed by plastic sealing. Then, the surface of the alloy balls is exposed by laser or mechanical drilling. Finally, a second implantation of alloy balls is performed and the material is reflowed. A high aspect ratio TMV can be achieved through multiple drilling and ball implantation operations, which is a relatively complex process. Summary of the Invention

[0004] To effectively extend the interconnect length of TMV, this invention provides a packaging method based on extended TMV technology. This invention can effectively extend the interconnect depth of TMV, is compatible with applications of embedding thick chips, and can achieve double-sided interconnection of plastic-encapsulated substrates, thereby improving integration.

[0005] A packaging method based on extended TMV process, comprising: (1) Mount the chip and adapter board onto the temporary carrier board; (2) Perform ball-planting treatment on the pads of the adapter board; (3) The chip and the adapter board are encapsulated to form a plastic-encapsulated board; (4) Separate the plastic sealing plate from the temporary carrier plate; (5) Redecorate the lower surface of the plastic sealing board; (6) Thin and polish the upper surface of the plastic sealant until the metal bumps for ball placement on the upper surface of the adapter are exposed; (7) Perform ball-planting treatment on the metal bumps on the upper surface of the plastic sealant and the redistribution area on the lower surface.

[0006] Furthermore, the temporary carrier is covered with a temporary bonding film or temporary bonding adhesive.

[0007] Furthermore, in step (2), solder balls are welded onto the surface of the adapter plate using an automatic ball-mounting machine to form metal interconnect bumps.

[0008] Furthermore, the molding compound is thermocured from epoxy molding compound.

[0009] Furthermore, the debonding process in step (4) can be performed using heating, laser, or mechanical debonding methods.

[0010] Furthermore, the rewiring process electrically interconnects the chip interconnect pins and the adapter board interconnect pins.

[0011] Furthermore, the thinning polishing is mechanical grinding and polishing.

[0012] Furthermore, the ball-planting process in step (7) employs either reflux or laser ball-planting.

[0013] Compared with the prior art, the present invention has the following beneficial effects: (1) The present invention can effectively extend the TMV interconnect length, which is of great benefit to the plastic encapsulation interconnect of thick chips.

[0014] (2) The packaging method of the present invention is simple and reliable. Attached Figure Description

[0015] Figure 1 This is a cross-sectional view of the chip and adapter board after they have been mounted onto a wafer-level temporary carrier board, according to an embodiment of the present invention.

[0016] Figure 2 This is a cross-sectional view of the adapter board pads after ball placement in an embodiment of the present invention.

[0017] Figure 3 This is a cross-sectional schematic diagram of the process in which the chip and the adapter board are mounted onto a wafer-level temporary carrier board and then encapsulated to form a plastic encapsulation board in an embodiment of the present invention.

[0018] Figure 4 This is a cross-sectional schematic diagram of the plastic sealing plate and the temporary carrier plate after separation in an embodiment of the present invention.

[0019] Figure 5 This is a cross-sectional view of the lower surface of the plastic sealing plate after redistribution processing according to an embodiment of the present invention.

[0020] Figure 6 This is a cross-sectional schematic diagram of the upper surface of the plastic sealant plate after thinning and polishing according to an embodiment of the present invention.

[0021] Figure 7 This is a cross-sectional schematic diagram showing the upper and lower surfaces of the plastic sealing plate after ball-planting treatment according to an embodiment of the present invention.

[0022] The reference numerals in the figures include: 1. Chip, 2. Adapter board, 3. Temporary bonding film, 4. Temporary carrier board, 5. TIV (Through Interposer Via), 6. I / O pin, 7. First alloy ball, 8. Molding board, 9. Epoxy resin, 10. Rewiring interconnect layer, 11. Rewiring passivation layer, 12. UBM (Under Bump Metal), 13. Second alloy ball, 14. Third alloy ball. Detailed Implementation

[0023] The specific embodiments of the present invention will be further described below with reference to the accompanying drawings. It should be noted that the accompanying drawings are for illustrative purposes only and are not actual drawings, and should not be construed as limiting the present invention; in order to clearly illustrate the scope of the present invention, various components in the drawings may be omitted, enlarged, or reduced, and do not represent the actual product dimensions, so as to facilitate understanding by those skilled in the art.

[0024] In the description of this invention, it should be understood that the terms indicating orientation or positional relationship are based on the orientation or positional relationship shown in the drawings and are only for the convenience of describing the invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention.

[0025] This invention provides a packaging method based on extended TMV process, such as... Figures 1 to 7 As shown, it includes the following steps: S110: Mounts the chip and adapter board onto the wafer-level temporary carrier board, such as... Figure 1 As shown; S120: Perform ball-planting treatment on the pads of the adapter board, such as... Figure 2 As shown; S130: The chip, the adapter board, and the wafer-level temporary carrier board are encapsulated to form a molding compound, such as... Figure 3 As shown; S140: Separate the plastic sealing plate from the temporary carrier plate, such as... Figure 4 As shown; S150: Perform rewiring on the lower surface of the molding compound, such as... Figure 5 As shown; S160: Thin and polish the upper surface of the plastic-sealed board, such as... Figure 6 As shown; S170: Perform ball-planting treatment on the upper and lower surfaces of the molding compound, such as... Figure 7 As shown; The above is the specific process flow of the packaging method based on the extended TMV process. The following is a detailed description of the process flow.

[0026] In step S110, chip 1 and adapter board 2 are mounted onto a wafer-level temporary carrier board 4. The wafer-level temporary carrier board 4 is typically a silicon wafer, glass sheet, or metal sheet, with a temporary bonding film 3, such as a thermal release sheet, covering its surface. At room temperature, this thermal release sheet 3 is adhesive on both sides. Following certain rules, an automatic pick-and-place machine mounts chip 1 and adapter board 2 onto the wafer-level temporary carrier board 4 covered with the thermal release sheet 3, using one side of the I / O pins 6. TIV 5 is the interconnect via of the adapter board, primarily serving as an electrical interconnect.

[0027] In step S120, ball-planting is performed on the pads of the adapter board 2. A laser ball-planting machine or similar equipment is used to plant the first alloy balls 7 onto the pads of the adapter board 2. Here, the adapter board pads refer to the pads on the other surface not covered by the pyrolysis film 3. The alloy balls are generally made of tin-lead, tin-silver, or tin-silver-copper alloys.

[0028] In step S130, the chip 1 and the adapter board 2 are encapsulated to form a molded board 8. This process uses wafer-level encapsulation equipment to encapsulate the temporary carrier board 4, on which the chip 1 and the adapter board 2 are mounted, to form the molded board 8. The wafer-level encapsulation adopts a compression molding process, using thermosetting epoxy resin 9 to wrap the chip and the adapter board, and under certain temperature and molding pressure conditions, a molded board 8 of a certain shape is formed.

[0029] In step S140, the molding compound 8 is separated from the temporary carrier plate 4. First, according to the process parameters of the pyrolysis film 3, the molding compound 8 is heated to separate it from the pyrolysis film 3. Then, according to the process parameters of the thermosetting epoxy resin, the molding compound 8 is post-cured.

[0030] In step S150, the lower surface of the molding compound 8 is subjected to redistribution processing. Here, the lower surface refers to the lower surface of the molding compound 8, i.e., the surface bonded to the pyrolytic film 3. This step uses a redistribution process to electrically interconnect the chip 1 and the adapter board 2. The redistribution process is also called the RDL process. RDL stands for Redistribution Layer, and metal wiring is generally completed through processes such as sputtering, photolithography, electroplating, and etching. Depending on the design requirements, UBM 12 is selectively fabricated, generally located at the pads where alloy balls need to be implanted. Before the redistribution process on the molding compound 8, the surface of the molding compound 8 should be polished according to the product design requirements and redistribution process requirements. Figure 5In the process, the rewiring interconnect layer 10 is generally made of metals such as titanium and copper, the rewiring passivation layer 11 is generally made of insulating materials such as polyimide (PI) and benzocyclobutene (BCB), and UBM12 is generally made of metals such as titanium, copper, nickel, and gold.

[0031] In step S160, the upper surface of the molding compound 8 is thinned and polished. Here, the upper surface refers to the upper surface of the molding compound 8, that is, the surface that has not been bonded to the pyrolytic film 3. The upper surface of the molding compound 8 is thinned and polished so that one end of the first alloy ball 7 near this side is flush with the upper surface of the molding compound 8, forming an extended TMV structure.

[0032] In step S170, ball-mounting is performed on the upper and lower surfaces of the molding compound 8. Here, the upper surface of the molding compound 8 refers to the side with the first alloy ball, and the lower surface refers to the side with the I / O pin 6 of the chip 1. Flux is applied to the upper surface of the molding compound 8, especially at the location of the first alloy ball 7. Then, an automatic ball-mounting machine is used to place the second alloy ball 13 on the surface of the first alloy ball 7. The first alloy ball 7 and the second alloy ball 13 are heated and melted together by a reflow soldering process. Finally, a flux cleaning process is performed. In this step, rosin-based flux is generally used. The automatic ball-mounting machine can place the pre-made alloy balls in the required positions through a nozzle. The first alloy ball 7 and the second alloy ball 13 are made of the same alloy material.

[0033] In step S170, after completing the ball-mounting process on the upper surface of the molding compound 8, ball-mounting processing will be performed on the lower surface of the molding compound 8. Here, a laser ball-mounting process is used to mount the third alloy balls 14 onto the surface of the UBM pads, thereby forming reliable interconnect alloy bumps.

[0034] The method of this invention can effectively extend the interconnect length of TMV, meet the application requirements of high aspect ratio TMV, and at the same time, the method can effectively package thick chips and achieve double-sided electrical interconnection effect of plastic-encapsulated boards.

[0035] The above-described embodiments merely illustrate preferred embodiments of the present invention, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of the invention. It should be noted that those skilled in the art should understand that various modifications, substitutions, and changes can be made without departing from the technical principles of the present invention, and these changes should also be considered within the scope of protection of this application. Therefore, the scope of protection of the present invention should be determined by the scope of the claims.

Claims

1. A packaging method based on extended TMV process, characterized in that, include: (1) Mount the chip and adapter board onto the temporary carrier board; (2) Perform ball-planting treatment on the pads of the adapter board; (3) The chip and the adapter board are encapsulated to form a plastic-encapsulated board; (4) Separate the plastic sealing plate from the temporary carrier plate; (5) Redecorate the lower surface of the plastic sealing board; (6) Thin and polish the upper surface of the plastic sealant until the metal bumps for ball placement on the upper surface of the adapter are exposed; (7) Perform ball-planting treatment on the metal bumps on the upper surface of the plastic sealant and the redistribution area on the lower surface.

2. The packaging method based on extended TMV process according to claim 1, characterized in that, The temporary carrier is covered with a temporary bonding film or temporary bonding adhesive.

3. The packaging method based on extended TMV process according to claim 1, characterized in that, Step (2) Solder balls are welded onto the surface of the adapter plate using an automatic ball-mounting machine to form metal interconnect bumps.

4. The packaging method based on extended TMV process according to claim 1, characterized in that, The molding compound is made of epoxy molding compound that has been thermocured.

5. The packaging method based on extended TMV process according to claim 1, characterized in that, The debonding process in step (4) can be performed using heating, laser, or mechanical debonding methods.

6. The packaging method based on extended TMV process according to claim 1, characterized in that, The rewiring process electrically interconnects the chip interconnect pins and the adapter board interconnect pins.

7. The packaging method based on extended TMV process according to claim 1, characterized in that, The thinning polishing is mechanical grinding and polishing.

8. The packaging method based on extended TMV process according to claim 1, characterized in that, Step (7) involves ball planting using either reflux or laser ball planting.