A method for fabricating a POP packaging structure and the POP packaging structure.

By pre-enlarging the package size and substrate spacing to form an annular dispensing gap, combined with whole-board ball placement and copper pillar connection, the problem of glue overflow pollution in POP packaging is solved, improving production efficiency and packaging quality.

CN123124853APending Publication Date: 2026-11-17SHANDONG XINTONG MICROELECTRONICS TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611557060.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-09
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

During the POP packaging process, adhesive can easily overflow onto the side of the package during the dispensing process, contaminating the subsequent ball-mounting area. This can cause the solder balls to fail to adhere properly or have poor reflow, affecting the packaging quality and efficiency.

Method used

By pre-enlarging the size of the first package and the spacing between the second substrate panels, an annular dispensing gap is formed. After sealing, balls are placed on the entire board, and copper pillars are used to achieve electrical connection, ensuring that the glue fills the gap without overflowing. The entire board is then cut to form the final package.

Benefits of technology

It effectively avoids glue overflow problems, improves ball placement efficiency and consistency, is suitable for mass production, and ensures that the sides of the package are flush and the electrical connection is stable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124853A_ABST
    Figure CN123124853A_ABST
Patent Text Reader

Abstract

This invention belongs to the field of POP packaging technology, specifically relating to a method for preparing a POP packaging structure and the POP packaging structure itself. The method involves providing a first substrate to fabricate a first package and cut it into individual pieces, the size of each piece being larger than the final finished product size; providing a second substrate to fabricate a second package, with the width of the cutting channel between adjacent second packages set to a preset value; aligning and sealing the individual first packages with the entire second package to form a sealed structure; filling the dispensing gaps between the first packages in the sealed structure with adhesive; performing full-board solder ball placement on the second packages in the sealed structure to form a solder ball array; and cutting the sealed structure along the cutting channel of the final finished product size to obtain multiple final packages. This method, by pre-enlarging the size of the first package and increasing the width of the cutting channel on the second substrate, creates sufficient dispensing gaps after sealing, effectively preventing adhesive from overflowing to the sides of the package. The full-board solder ball placement and subsequent cutting process improve production efficiency and meet the needs of mass production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of POP packaging technology, specifically relating to a method for preparing a POP packaging structure and the POP packaging structure itself. Background Technology

[0002] POP is an abbreviation for "Package on Package," a packaging technology that involves stacking two or more independent semiconductor packages vertically and electrically connecting them using interconnect structures such as solder balls. Typically, the lower and upper packages are individually molded and ball-mounted, then reflow soldering connects the solder balls to form a single unit. POP effectively saves substrate area and shortens signal transmission distances between chips, making it suitable for applications such as smartphones and portable devices where high integration and performance are required.

[0003] In POP (Position-on-Package) stacking, the vertical gap between the upper and lower packages is determined by the solder ball height, typically ranging from 0.15 to 0.25 mm. During the dispensing process, adhesive is squeezed into the extremely narrow gap from the side, easily overflowing onto the sidewalls and bottom of the second package. This overflow not only affects the appearance but also contaminates the pads in the subsequent solder ball placement area, causing solder balls to fail to adhere properly or resulting in poor reflow. Summary of the Invention

[0004] This invention provides a method for preparing a POP packaging structure. By pre-enlarging the size of the first package and the spacing of the second substrate panels, a dispensing gap is formed after sealing to avoid glue overflow contamination. After the entire second package is sealed with a single first package, the entire board is then used for ball placement, improving ball placement efficiency and consistency.

[0005] Includes the following steps: S1: Provide a first substrate, fabricate a first package on the first substrate, and cut the first package into individual pieces along a preset first cutting path, wherein the size of each individual piece of the first package is smaller than the size of the final packaged product. S2: Provide a second substrate, and fabricate a second package on the second substrate. The size of the second package is equal to the size of the final packaged product. The width of the cut channel between adjacent second packages on the second substrate is set to a preset value so that after subsequent sealing, an annular gap for dispensing is formed between the side of the first package and the side of the adjacent second package. S3: Align and seal the single first package obtained in step S1 with the entire second package obtained in step S2, so that the first package is centered above the corresponding second package to form a sealing structure, and the dispensing gap is formed between the side of the first package and the side of the adjacent second package. S4: In the sealing structure obtained in step S3, glue is applied in the glue application gap between the side of the first package and the side of the adjacent second package, so that the glue fills the gap between the first package and the second package. S5: Perform full-board solder ball mounting on the second package body in the sealing structure after the adhesive is cured in step S4, forming a solder ball array on each package unit of the second package body; S6: Cut the encapsulation structure after ball placement in step S5 along the cutting path of the final packaged product size to obtain multiple final packages with the final package size.

[0006] According to another embodiment of this application, a POP encapsulation structure is provided. Before dispensing and curing, the POP encapsulation structure includes two encapsulation bodies stacked on top of each other, with the upper layer being a smaller first encapsulation body and the lower layer being a larger second encapsulation body. The first package is disposed above the second package, and the size of the first package is smaller than the size of the second package; The first package is placed in the center within the actual size range of the POP package structure, and an annular gap for dispensing is left between the four edges of the first package and the edge of the second package. The second package contains a copper pillar embedded inside. The copper pillar penetrates the second package vertically, with the upper end face of the copper pillar flush with or exposed to the upper surface of the second package, and the lower end face flush with the lower surface of the second package. The top of the copper pillar is connected to the solder ball on the bottom surface of the first package, and a metallurgical connection is formed by reflow soldering to achieve electrical conduction between the first package and the second package; the bottom of the copper pillar is connected to the ball pad on the lower surface of the second package, and then connected to the external circuit board through the solder ball.

[0007] As can be seen from the above technical solutions, the present invention has the following advantages: In this invention, the first package is smaller than the second package, naturally forming a regular annular gap after encapsulation. The width of the dicing groove between adjacent package units on the second substrate is preset, and SMT optical alignment marks are made on the edge of the second substrate. The pick-and-place machine uses these marks as a global reference to center-mount each first package onto each package unit on the second substrate, forming a uniform annular gap between the four sides of the first and second packages. A dispensing needle extends into the annular gap, expels adhesive along the gap, and, under gravity and capillary action, falls into the dispensing gap, spreading over the area between the side of the first package and the top surface of the second package, filling the gap between them. The adhesive completely fills the gap without overflowing. The entire encapsulation structure is directly ball-mounted, covering the bottom pads of all second package units in one go. Finally, the encapsulation structure is cut along the preset final finished size dicing groove on the second substrate, separating the encapsulation structure into independent final packages, improving production efficiency and meeting the requirements of mass production. Attached Figure Description

[0008] To more clearly illustrate the technical solution of the present invention, the accompanying drawings used in the description will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0009] Figure 1 This is a schematic diagram of a POP package structure; Figure 2 This is a layout diagram of a POP stacked package structure; Figure 3 This is a flowchart illustrating the fabrication method of the POP packaging structure. Detailed Implementation

[0010] Combination Figure 1 and Figure 2 As shown in the accompanying drawings, the specific embodiments of the present invention will be described in detail below.

[0011] In this embodiment of the invention, the POP packaging structure includes two packages stacked one on top of the other. The upper layer is a first package 11, the size of which is smaller than the final packaged product size; the lower layer is a second package 12, the size of which is equal to the final packaged product size. The second package 12 exists in the form of a whole substrate, on which multiple second packaging units are arranged in an array, and a cutting channel of a preset width is provided between adjacent second packaging units.

[0012] The first package 11 is mounted on top of the second package 12, and within the horizontal projection range of the first package 11, all four sides of the first package 11 are located within the corresponding sides of the second package 12 below. That is, the first package 11 is recessed relative to the second package 12, so that a continuous annular gap is formed between the four sidewalls of the first package 11 and the upper surface of the second package 12. This annular gap is located inside the same packaging unit.

[0013] A copper pillar 13 is embedded inside the second package 12. The copper pillar 13 vertically penetrates the molding compound of the second package 12. The upper end face of the copper pillar 13 is flush with or slightly exposed to the upper surface of the second package 12, and the lower end face is flush with or slightly exposed to the lower surface of the second package 12. The top of the copper pillar 13 is mated with the solder ball 14 on the bottom surface of the first package 11, and the two are connected by reflow soldering to form a metallurgical connection, realizing electrical conduction between the upper and lower packages. The bottom of the copper pillar 13 is used to connect to the ball pads on the lower surface of the second package 12, and then connects to the external circuit board through the solder ball.

[0014] The annular gap and the linear channel are spatially interconnected, together forming a cavity whose bottom is occupied by the top of the copper pillar 13 and the solder ball 14, and whose sides are open. The area in the cavity not filled by the copper pillar 13 and the solder ball 14 is the dispensing gap 15, which is specifically used for subsequent dispensing processes.

[0015] The dispensing needle enters the linear channel from the side of the sealing structure, moves along the channel, and injects glue into the dispensing gap 15. The glue fills the gap between the first package 11 and the second package 12, and wraps around the copper pillar 13 and the solder ball 14, which serves to reinforce and prevent moisture.

[0016] The copper pillar 13 ensures that a stable electrical connection has been established between the first package 11 and the second package 12 before dispensing, through the solder balls 14 and the copper pillar 13. The dispensing process only provides mechanical reinforcement and environmental protection and does not participate in signal transmission.

[0017] Furthermore, after a single first package 11 is sealed with the entire second substrate, a linear channel with both ends extending through is formed directly above the cut channel between two adjacent first packages 11, that is, between two adjacent second package units. The bottom of the linear channel is the upper surface of the second package 12, that is, the cut channel area, and the two sides are the opposite sidewalls of the adjacent first packages 11.

[0018] The annular gap and the linear channel are spatially connected, together forming a cavity area that allows the dispensing needle to enter and move. Functionally, this cavity area serves the dispensing process and is called the dispensing gap.

[0019] Specifically, the dispensing needle enters the linear channel from the side or end of the sealing structure, moves along the linear channel, and the glue is squeezed out from the needle to first fill the linear channel, then spread to the annular gaps on both sides, and finally fills all the gaps.

[0020] In this embodiment, the width Wgap of the cut channel between adjacent second packaging units on the second substrate is preferably 3 mm. The single-side dimension of the first package 11 is 0.5 mm smaller than the final packaged product size, i.e., the inward shrinkage δ = 0.5 mm, and the size of the second package 12 is equal to the final packaged product size.

[0021] After sealing, the linear channel width between adjacent first package bodies 11 is Waccess = Wgap - 2δ = 3mm - 1mm = 2mm. This 2mm gap is sufficient to allow a dispensing needle with an outer diameter of 0.6mm to freely enter and move.

[0022] Figure 1 The diagram shows a POP package structure, in which the first package 11 is placed in the center above the second package 12, with an annular gap around it. Figure 2 The diagram shows the layout after sealing, with the cutting width of 3mm, the single-sided inward shrinkage of 0.5mm, and the dispensing gap of 2mm between adjacent first packages marked.

[0023] During the manufacturing process, the first package 11 is first aligned and sealed with the entire second package 12, using SMT optical alignment marks on the edge of the second substrate to achieve high-precision mounting. After sealing, the aforementioned dispensing gap is formed. Next, a dispensing needle is inserted into this gap and expels adhesive, filling the annular gap. After curing, the bottom surface of the second substrate in the entire sealed structure is ball-mounted. Finally, the package is cut along the cutting path of the final package size, removing the excess material of the first package 11 and the excess material on both sides of the second substrate cutting path, resulting in a final package with flush sidewalls.

[0024] The following are embodiments of the preparation method of the POP packaging structure provided in this disclosure. This method and the POP packaging structure in the above embodiments belong to the same inventive concept. For details not described in detail in the embodiments of the preparation method of the POP packaging structure, please refer to the embodiments of the POP packaging structure above.

[0025] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0026] Please see Figure 3 The diagram shows a flowchart of a method for fabricating a POP packaging structure in a specific embodiment. The method includes: S1: Provide a first substrate, fabricate a first package on the first substrate, and cut the first package into individual pieces along a preset first cutting path, wherein the size of each individual piece of the first package is smaller than the size of the final packaged product. S2: Provide a second substrate, and fabricate a second package on the second substrate. The size of the second package is equal to the size of the final packaged product. The width of the cut channel between adjacent second packages on the second substrate is set to a preset value so that after subsequent sealing, an annular gap for dispensing is formed between the side of the first package and the side of the adjacent second package.

[0027] S3: Align and seal the single first package obtained in step S1 with the entire second package obtained in step S2, so that the first package is centered above the corresponding second package to form a sealed structure, and the dispensing gap is formed between the side of the first package and the side of the adjacent second package.

[0028] S4: In the sealing structure obtained in step S3, glue is applied to the glue application gap between the side of the first package and the side of the adjacent second package, so that the glue fills the gap between the first package and the second package.

[0029] S5: Perform full-board solder ball mounting on the second package body in the sealing structure after the adhesive is cured in step S4, forming a solder ball array on each package unit of the second package body; S6: Cut the encapsulation structure after ball placement in step S5 along the cutting path of the final packaged product size to obtain multiple final packages with the final package size.

[0030] This method, by pre-enlarging the width of the second substrate cutting channel and combining it with a design where the size of the first package is smaller than the finished product size, automatically forms a spacious annular dispensing gap after encapsulation. This solves the problem of adhesive overflow onto the sides of the package in POP packaging, reducing the defect rate. When encapsulating a single first package with the entire second package, high-precision alignment can be achieved using optical alignment marks on the second substrate, reducing the encapsulation misalignment rate and improving yield. Whole-board ball placement of the entire second package is more efficient and accurate than single-ball placement. Final cutting ensures that all package sidewalls are cut with the same blade, resulting in good dimensional consistency and suitability for mass production.

[0031] In one embodiment of the present invention, based on step S1, the following will provide a possible embodiment and describe its specific implementation in a non-limiting manner.

[0032] S11: Provide a first substrate, and sequentially perform substrate baking, SMT placement, AOI inspection, pre-core baking, core mounting, post-core baking, plasma cleaning, wire bonding, three-light inspection, pre-encapsulation cleaning, encapsulation, PMC post-curing, and grinding on the first substrate to form a first package on the first substrate. S12: Based on the ball placement on the surface of the first package, solder balls are formed on the pad array on the bottom surface of the first package; S13: Cut the first package body after ball implantation into individual pieces along the preset first cutting channel. The first cutting channel is located inside the outline of the final packaged product size, so that the size of each individual piece of the first package body is smaller than the size of the final packaged product, and each side is shrunken inward by a preset amount.

[0033] In some embodiments, the first substrate is placed in an oven to remove moisture adsorbed inside the substrate. The baked first substrate is then fed into an SMT placement line, where solder paste is printed onto the substrate pads using a solder paste printer. A pick-and-place machine picks up passive components and places them onto the corresponding pads. A reflow oven heats the solder paste to melt it and metallurgically bond it to the pads. An AOI (Optical Inspection) device scans the substrate surface, comparing component placement coordinates, polarity, and solder joint appearance to remove misaligned, missing, or reversed defective components.

[0034] The inspected and qualified substrates are sent to the pre-bonding baking station for baking to further reduce the substrate moisture content. The wafer dicing machine's vacuum nozzle picks up the diced chips, applies conductive adhesive, and then adheres the chips to the chip carrier area of ​​the substrate. The conductive adhesive cures at a certain temperature to form a mechanical connection between the chip and the substrate. An argon-oxygen mixed gas is introduced into the plasma cleaning equipment, and plasma is generated under the excitation of a radio frequency electric field to bombard the substrate surface, removing organic residues and oxide layers. A wire bonding machine uses gold or copper wires as interconnecting conductors to connect the chip pads to the substrate pins one by one through thermo-ultrasonic bonding, forming an electrical path. Then, three-light inspection, pre-encapsulation cleaning, encapsulation, PMC post-curing, and polishing are performed to form the first package on the first substrate. Pre-encapsulation cleaning removes surface particles to prevent foreign matter from being trapped inside the package; PMC post-curing fully cross-links the molecular chains of the encapsulation material, improving mechanical strength and resistance to damp heat.

[0035] Further, the ground first package is placed in the ball-mounting station, and a ball-mounting stencil covers the bottom surface of the first package, with the openings of the stencil corresponding one-to-one with the bottom surface pad array. Flux is evenly applied to the pads, with the flux thickness controlled to 1 / 4 to 1 / 3 of the solder ball diameter. The ball-mounting fixture vacuum-picks up the solder balls and transfers them above the flux-coated pads. The vacuum switch is released, and the solder balls adhere to the pads under the adhesive effect of the flux. The first package after ball mounting is sent to a reflow oven, where it is heated to above the melting point of the solder balls in a nitrogen atmosphere. The solder balls melt and wet and diffuse with the pads under the action of surface tension, forming a hemispherical solder ball array after cooling.

[0036] Furthermore, the size of a single first package is larger than the final package size. After sealing, a second cut is made along the outline of the final package size to align the sides of the first and second packages. This eliminates the shape misalignment problem caused by the misalignment of the upper and lower packages during PoP sealing. The preset outward expansion is evenly extended along each side to ensure that each side of the first package has sufficient allowance during the second cut after sealing. After cutting, the sides of the upper and lower packages are coplanar.

[0037] In one embodiment of the present invention, based on step S2, the specific steps include the following: S21: Provide a second substrate, and sequentially perform substrate baking, SMT placement, AOI inspection, pre-core baking, core mounting, post-core baking, plasma cleaning, wire bonding, three-light inspection, pre-encapsulation cleaning, encapsulation, PMC post-curing, and grinding on the second substrate to form a second package body on the second substrate. The external dimensions of the second package body are equal to the dimensions of the final packaged product. S22: A cleaving channel is provided between adjacent second packages on the second substrate. The width of the cleaving channel is calculated and determined based on the preset outward expansion amount and the width requirement of the dispensing gap, so that the width of the cleaving channel is greater than the width of a conventional package cleaving channel. S23: An SMT optical alignment mark is set on the edge of the panel of the second substrate, and the positional relationship between the SMT optical alignment mark and the second package meets the visual recognition requirements of the SMT pick and place machine. S24: Retain the second package in the panelized state of the second substrate, do not perform the cut-off operation, and allow the second package to enter the subsequent sealing process in the form of a whole strip.

[0038] In some embodiments, during the panel layout design of the second substrate, a cutting channel is reserved between adjacent second packages, and the width of the cutting channel is determined according to the following method: The width of the cutting channel is equal to the sum of the preset outward expansion of each of the two adjacent second packages plus the dispensing gap width. Taking a preset outward expansion of 0.5mm on one side and a dispensing gap width of 2.0mm as an example, the cutting channel width is 0.5mm + 0.5mm + 2.0mm = 3.0mm. The cutting channel width is adjusted within the range of 2.0mm to 5.0mm according to the actual package size and dispensing equipment parameters. The cutting channels are evenly distributed horizontally and vertically in the panel layout, forming multiple second package units arranged in a matrix. Each second package unit is surrounded by the cutting channels. After subsequent sealing, the cutting channels form the dispensing gap between the side of the first package and the side of the adjacent second package.

[0039] It should be noted that the width of the cutting track is greater than that of conventional packaging cutting tracks, which are typically 0.3mm to 0.5mm wide. This application expands the cutting track width to 2.0mm to 5.0mm, providing ample space for dispensing operations after encapsulation. The dispensing gap width is greater than 2.0mm, allowing the dispensing needle to smoothly enter the gap and avoiding collisions between the needle and the side of the package, supporting automated high-speed dispensing. The cutting track is determined during the panel design stage, requiring no subsequent processing adjustments. The matrix arrangement of the second package unit enables whole-board encapsulation, whole-board dispensing, and whole-board ball mounting, improving production efficiency.

[0040] Furthermore, the SMT optical alignment mark serves as the defining reference for the panel, with its center coordinates defined with high-precision values ​​in the panel design file. The SMT pick-and-place machine's vision system identifies the deviation between the actual and designed positions of the mark, establishing a mapping between the actual and designed coordinate systems to correct the placement coordinates. The precise relative positional relationship between the mark and the center of the second package allows the pick-and-place machine to accurately place the first package directly above the second package. In this way, the SMT optical alignment mark enables the entire second package on the board to be directly recognized by the SMT pick-and-place machine, replacing the method of using dedicated fixtures for fixing in PoP (PoP) packaging and improving alignment accuracy.

[0041] Furthermore, in step S24, the second packaged components, after grinding, remain on the panel of the second substrate without undergoing any cutting or separation operations. The second packages are arranged in a matrix on the panel, with adjacent second packages separated by the cutting channels. The entire panel is fixed to the platform of an SMT placement machine, with the platform using vacuum adsorption to fix the bottom surface of the panel. The SMT placement machine picks up individual first packages one by one, and sequentially mounts the first packages onto the corresponding second packages according to the position order of the second package units in the panel layout. After mounting, the entire encapsulation structure enters the dispensing process, where dispensing is performed point by point within the dispensing gaps between each first package and the adjacent second package. After dispensing curing, the entire encapsulation structure enters the ball-mounting process, where balls are uniformly mounted on each package unit on the bottom surface of the second packages. After ball mounting, the entire encapsulation structure is cut along the cutting channels of the final package size, separating it into multiple final packages.

[0042] In one embodiment of the present invention, the first package is output as a single unit smaller than the finished product size, and the second package is output as a whole strip equal to the finished product size with the cut width pre-enlarged. This provides an alignment basis for the sealing process in step S3. When the single first package is aligned and sealed with the whole second package in step S3, since the size of the first package is smaller than that of the second package and the cut width of the second substrate has been enlarged, an annular dispensing gap is naturally formed between the side of the first package and the side of the adjacent second package after sealing. The formation of this gap does not require additional machining or structural adjustment, allowing the dispensing process to be carried out in a spacious and controllable space, solving the problem of glue overflow in traditional POP packaging.

[0043] Specifically, step S3 includes the following steps: S31: Place the entire second package onto the worktable of the mounting platform, use vacuum adsorption to fix the four corners and edges of the second substrate, turn on the optical alignment system of the mounting machine, and identify the SMT optical alignment marks at the corners of the second substrate.

[0044] S32: Pick up a single first package from the tray, flip the first package so that the chip side is facing down, move the mounting head above the second substrate, align the solder ball array at the bottom of the first package with the pad array on the upper surface of the corresponding second package unit on the second substrate, and adjust the mounting head so that the alignment deviation is less than the set threshold.

[0045] S33: The placement head is lowered so that the solder balls at the bottom of the first package contact the flux on the surface of the pads on the second substrate. A set pressure is applied and maintained to pre-fit the solder balls with the pads. The placement head temperature is raised to the reflow temperature so that the solder balls melt and wet the pads. After cooling, a metallurgical connection is formed, resulting in a one-to-one encapsulation structure where each first package corresponds to a second package on the entire second substrate.

[0046] In this way, each chip is mounted to the entire strip, and all units are sealed in one reflow, improving sealing efficiency.

[0047] After the sealing process in step S3, the single first package and the entire second package form an integrated sealing structure. Since the size of the first package in step S1 meets the final package size, and the cutting width between adjacent units of the second substrate in step S2 is pre-enlarged, the sealing structure forms a controllable annular dispensing gap between the side of the first package and the side of the adjacent second package.

[0048] In traditional POP packaging, the upper and lower packages are of equal size and cut into single pieces, resulting in only a very narrow lateral gap after sealing. During dispensing, adhesive easily overflows to the sides of the package, contaminating the subsequent ball-mounting area. This embodiment, through the aforementioned differentiated size design and whole-line retention strategy, obtains an open dispensing channel after sealing, changing the operating conditions of the dispensing process. Based on this, step S4 utilizes this annular dispensing gap to perform the dispensing operation. Under gravity and capillary action, the adhesive fills the gap between the first and second packages, ensuring uniform and complete filling.

[0049] In one embodiment of the present invention, step S4 includes the following: S41: Fix the obtained sealing structure on the dispensing machine worktable. The sealing structure maintains its whole shape, with the dispensing gap between the first package and the adjacent first package facing upward.

[0050] S42: The visual positioning system of the dispensing machine captures images of the edge of the first package and the surface of the second package, identifies the boundary position of the dispensing gap, and calculates the starting and ending coordinates of the dispensing trajectory.

[0051] S43: The dispensing needle of the dispensing machine moves above the dispensing gap and moves longitudinally or laterally along the dispensing gap. The dispensing needle expels liquid glue at a set speed. The glue falls into the dispensing gap and spreads in the angled area between the side of the first package and the top surface of the second package.

[0052] S44: The dispensing machine dispenses adhesive into all the dispensing gaps on the sealing structure one by one. After dispensing, the sealing structure enters the curing oven and is heated to cross-link and cure the adhesive, forming a cured adhesive layer that fills the gap between the first package and the second package.

[0053] In step S42 of some embodiments, the visual positioning system of the dispensing machine captures images of the edge contour of the first package and the surface of the second package using a CCD camera. The image processing software identifies the boundary line between the first package and the second package, extracts the longitudinal and transverse boundaries of the dispensing gap, calculates the center line of the dispensing gap as the dispensing trajectory, and determines the starting coordinates and ending coordinates of the dispensing trajectory. The starting coordinates are located at one end of the dispensing gap, and the ending coordinates are located at the other end of the dispensing gap.

[0054] Further, in step S43, the dispensing needle of the dispensing machine moves above the dispensing gap according to the starting point coordinates. The diameter of the dispensing needle is 0.3mm to 0.6mm, and the vertical distance between the dispensing needle and the surface of the sealing structure is 0.1mm to 0.3mm. The dispensing machine moves longitudinally or laterally along the centerline of the dispensing gap at a set speed, and expels liquid epoxy resin adhesive at a set flow rate. The adhesive flows out from the end of the dispensing needle and falls into the dispensing gap under gravity and capillary action, spreading in the area between the side of the first package and the top surface of the second package, filling the gap between the first package and the second package. Here, capillary action allows the adhesive to spread and fill automatically without additional pressure. The dispensing speed and flow rate parameters can be adjusted according to the adhesive viscosity and gap width.

[0055] Sequential dispensing ensures uniform filling of all gaps, while alternating directions reduce needle travel. The curing oven provides the temperature required for the cross-linking reaction. The epoxy groups in the liquid epoxy resin react chemically with the curing agent to form a network structure, transforming the adhesive from a fluid state to a solid state. The cured adhesive layer forms a mechanical bond between the first and second encapsulations. The cured adhesive layer enhances the physical stability between the first and second encapsulations, preventing delamination during processing and use.

[0056] After the adhesive curing process is completed in step S4, the sealed structure does not require individual cutting or disassembly; instead, it remains in its entirety and flows to the next process. Because the adhesive gaps formed in step S4 effectively accommodate the adhesive, the second encapsulation area on the bottom surface of the sealed structure remains flat and uncontaminated by adhesive after curing. This provides a physical basis for the subsequent whole-board ball-planting process. Based on this, the ball-planting process in step S5 is performed on the sealed structure, which maintains its entirety, and specifically includes the following steps: S51: Fix the sealed structure after dispensing and curing onto the ball-mounting machine workbench. The sealed structure maintains its whole shape, with the pad array on the bottom surface of the second package facing upwards.

[0057] S52: The stencil of the ball-mounting machine covers the bottom surface of the second package, the openings on the stencil are aligned with the pad array on the bottom surface of the second package, and the squeegee applies solder paste to the surface of the stencil, and the solder paste is printed onto the surface of the pads through the openings.

[0058] S53: Remove the stencil, and place the solder balls one by one onto the solder paste on the surface of the pad. The solder balls are in contact with the solder paste. The solder balls are picked up by vacuum suction or mechanical clamping and placed in the corresponding pad position.

[0059] S54: After the solder balls are printed, the encapsulation structure enters the reflow oven, where it is heated to melt the solder paste and form a metallurgical bond with the solder balls and the pads. After cooling, an array of solder balls is formed on each encapsulation unit on the bottom surface of the second package.

[0060] As can be seen, after the stencil is removed, the ball-planting head of the ball-planting machine moves above the solder ball feeder. The ball-planting head picks up a single solder ball through a vacuum nozzle or clamps the solder ball in a mechanical gripper. The ball-planting head moves above the target pad, releases the vacuum or opens the gripper to allow the solder ball to fall onto the solder paste on the surface of the pad. The solder ball is in physical contact with the solder paste. The ball-planting head places the solder balls one by one into all the pad positions in a preset order. The solder balls are solder balls or tin-silver-copper alloy balls.

[0061] The solder ball pick-up head picks up solder balls via vacuum suction or mechanical clamping. The vacuum nozzle uses negative pressure to adsorb the solder balls, while the mechanical clamping jaws hold them in place with elasticity. After the ball pick-up head moves to the target position, it releases the solder balls, which fall onto the solder paste surface. The viscosity of the solder paste keeps the solder balls in place and prevents them from rolling. The ball pick-up head places the solder balls one by one according to the arrangement of the pad array until all pads are covered. The reflow oven temperature profile controls the heating process of the solder paste and solder balls. The preheating section evaporates the solvent in the solder paste, the heat preservation section activates the flux, the reflow section melts the solder paste and forms a metallurgical bond with the solder balls and pads, and the cooling section solidifies to form solder joints. An intermetallic compound layer grows at the interface between the solder balls and pads, providing strength support and electrical connection. After the solder ball array is formed, it serves as the connection interface between the final package and the external circuit board.

[0062] After completing the ball placement and forming of the solder ball array in step S5, the encapsulated structure retains its integral shape and requires no individual ball separation or disassembly process between ball placement and cutting. Based on the cutting allowance reserved in the pre-enlarged size design in the steps, the solder ball array on the bottom surface of the encapsulated body and the reserved cutting paths between adjacent units do not interfere with each other spatially, thus allowing the cutting operation to be performed directly in the integral state. Based on this, the final cutting and forming process of step S6 is directly performed on the encapsulated structure that maintains its integral shape, specifically including the following sub-steps: S61: Fix the sealing structure after ball planting in step S5 onto the cutting machine workbench. The sealing structure maintains its whole shape. Plan the longitudinal cutting path and the transverse cutting path. The longitudinal cutting path and the transverse cutting path intersect to form a grid-like cutting path.

[0063] S62: The cutting machine makes a longitudinal cut along the longitudinal cutting path, which is located at the reserved cutting allowance boundary of the first package, cutting through the molding body of the first package, the first substrate, the molding body of the second package, and the second substrate. The longitudinal cut removes the reserved cutting allowance on both sides of the longitudinal direction of the first package.

[0064] S63: The cutting machine performs a transverse cut along the transverse cutting path, which is located at the boundary of the reserved cutting allowance of the first package. It cuts through the molding body, the first substrate, the molding body and the second substrate of the first package. The transverse cut removes the reserved cutting allowance on both sides of the first package. The longitudinal cut and the transverse cut separate the encapsulation structure into multiple final packages with the final package size.

[0065] It can be seen that the fixed sealing structure of the cutting machine worktable prevents displacement during the cutting process. The cutting path planning is determined based on the final package size and the reserved cutting allowance. The reserved cutting allowance is the portion of the first package that expands outward by 0.3mm to 0.8mm on one side based on the final package size. The cutting path is located at the boundary of the reserved cutting allowance, which means that the cutting line passes through the outward expansion portion of the first package. The intersection of the longitudinal cutting path and the transverse cutting path divides the entire sealing structure into multiple independent final package units.

[0066] The horizontal cutting removes the reserved cutting allowance on both sides of the first package body, restoring the horizontal dimension of the first package body to the final packaged product size. The intersection of the vertical and horizontal cutting separates the whole board into multiple independent final packages. Each final package body has a uniform final package size. The four sides of the first package body and the second package body are flush, forming a package shape with consistent four sides.

[0067] It should be understood that the sequence number of each step in the above embodiments does not imply the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present invention.

[0068] In the description of this invention, it should be noted that the terms "upper," "lower," "inner," "outer," "front end," "rear end," "both ends," "one end," and "the other end," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this invention and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance.

[0069] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installed," "equipped with," "connected," etc., should be interpreted broadly. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be a connection within two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

[0070] The above description of the disclosed embodiments enables those skilled in the art to make or use the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for preparing a POP packaging structure, characterized in that, Includes the following steps: S1: Provide a first substrate, fabricate a first package on the first substrate, and cut the first package into individual pieces along a preset first cutting path, wherein the size of each individual piece of the first package is smaller than the size of the final packaged product. S2: Provide a second substrate, and fabricate a second package on the second substrate. The size of the second package is equal to the size of the final packaged product. The width of the cut channel between adjacent second packages on the second substrate is set to a preset value so that after subsequent sealing, an annular gap for dispensing is formed between the side of the first package and the side of the adjacent second package. S3: Align and seal the single first package obtained in step S1 with the entire second package obtained in step S2, so that the first package is centered above the corresponding second package to form a sealing structure, and the dispensing gap is formed between the side of the first package and the side of the adjacent second package. S4: In the sealing structure obtained in step S3, glue is applied in the glue application gap between the side of the first package and the side of the adjacent second package, so that the glue fills the gap between the first package and the second package. S5: Perform full-board solder ball mounting on the second package body in the sealing structure after the adhesive is cured in step S4, forming a solder ball array on each package unit of the second package body; S6: Cut the encapsulation structure after ball placement in step S5 along the cutting path of the final packaged product size to obtain multiple final packages with the final package size.

2. The method for preparing the POP packaging structure according to claim 1, characterized in that, S1 includes the following steps: S11: Provide a first substrate, and perform the following steps sequentially on the first substrate: substrate baking, SMT placement, AOI inspection, pre-core baking, core mounting, post-core baking, plasma cleaning, wire bonding, three-light inspection, pre-encapsulation cleaning, encapsulation, PMC post-curing, and grinding to form a first package on the first substrate. S12: Based on the ball placement on the surface of the first package, solder balls are formed on the pad array on the bottom surface of the first package; S13: Cut the first package body after ball implantation into individual pieces along the preset first cutting channel. The first cutting channel is located inside the outline of the final packaged product size, so that the size of each individual piece of the first package body is smaller than the size of the final packaged product, and each side is shrunken inward by a preset amount.

3. The method for preparing the POP packaging structure according to claim 1, characterized in that, S2 includes the following steps: S21: Provide a second substrate, and perform the following steps on the second substrate in sequence: substrate baking, SMT placement, AOI inspection, pre-core baking, core mounting, post-core baking, plasma cleaning, wire bonding, three-light inspection, pre-encapsulation cleaning, encapsulation, PMC post-curing, and grinding to form a second package on the second substrate. The external dimensions of the second package are equal to the dimensions of the final packaged product. S22: A cleaving channel is provided between adjacent second packages on the second substrate. The width of the cleaving channel is calculated and determined based on the preset outward expansion amount and the width requirement of the dispensing gap, so that the width of the cleaving channel is greater than the width of a conventional package cleaving channel. S23: An SMT optical alignment mark is set on the edge of the panel of the second substrate, and the positional relationship between the SMT optical alignment mark and the second package meets the visual recognition requirements of the SMT pick and place machine. S24: Retain the second package in the panelized state of the second substrate, do not perform the cut-off operation, and allow the second package to enter the subsequent sealing process in the form of a whole strip.

4. The method for preparing the POP packaging structure according to claim 1, characterized in that, S3 includes the following steps: S31: Place the entire second package on the worktable of the mounting platform, use vacuum adsorption to fix the four corners and edges of the second substrate, turn on the optical alignment system of the mounting machine, and identify the SMT optical alignment marks at the corners of the second substrate. S32: Pick up a single first package from the tray, flip the first package so that the chip side is facing down, move the mounting head above the second substrate, align the solder ball array at the bottom of the first package with the solder pad array on the upper surface of the corresponding second package unit on the second substrate, and adjust the mounting head so that the alignment deviation is less than the set threshold. S33: The placement head is lowered so that the solder balls at the bottom of the first package contact the flux on the surface of the pads on the second substrate. A set pressure is applied and maintained to pre-fit the solder balls with the pads. The placement head temperature is raised to the reflow temperature so that the solder balls melt and wet the pads. After cooling, a metallurgical connection is formed, resulting in a one-to-one encapsulation structure where each first package corresponds to a second package on the entire second substrate.

5. The method for preparing the POP packaging structure according to claim 1, characterized in that, S4 includes the following steps: S41: Fix the obtained sealing structure on the dispensing machine worktable. The sealing structure maintains its whole shape, with the dispensing gap between the first package and the adjacent first package facing upward. S42: The visual positioning system of the dispensing machine captures images of the edge of the first package and the surface of the second package, identifies the boundary position of the dispensing gap, and calculates the starting and ending coordinates of the dispensing trajectory. S43: The dispensing needle of the dispensing machine moves to the top of the dispensing gap and moves longitudinally or laterally along the dispensing gap. The dispensing needle squeezes out liquid glue at a set speed. The glue falls into the dispensing gap and spreads in the angled area between the side of the first package and the top surface of the second package. S44: The dispensing machine dispenses adhesive into all the dispensing gaps on the sealing structure one by one. After dispensing, the sealing structure enters the curing oven and is heated to cross-link and cure the adhesive, forming a cured adhesive layer that fills the gap between the first package and the second package.

6. The method for preparing the POP packaging structure according to claim 1, characterized in that, S5 includes the following steps: S51: Fix the sealed structure after dispensing and curing to the ball-mounting machine workbench. The sealed structure should maintain its whole shape, with the pad array on the bottom surface of the second package facing upwards. S52: The stencil of the ball-mounting machine covers the bottom surface of the second package, the openings on the stencil are aligned with the pad array on the bottom surface of the second package, and the squeegee applies solder paste to the surface of the stencil, and the solder paste is printed onto the surface of the pads through the openings; S53: Remove the stencil, and place the solder balls one by one on the solder paste on the surface of the pad. The solder balls are in contact with the solder paste. The solder balls are picked up by vacuum suction or mechanical clamping and placed in the corresponding pad position. S54: After the solder balls are printed, the encapsulation structure enters the reflow oven, where it is heated to melt the solder paste and form a metallurgical bond with the solder balls and the pads. After cooling, an array of solder balls is formed on each encapsulation unit on the bottom surface of the second package.

7. The method for preparing the POP packaging structure according to claim 1, characterized in that, S6 includes the following steps: S61: Fix the sealing structure after ball planting in step S5 onto the cutting machine workbench. The sealing structure maintains its whole shape. Plan the longitudinal cutting path and the transverse cutting path. The longitudinal cutting path and the transverse cutting path intersect to form a grid-like cutting path. S62: The cutting machine makes a longitudinal cut along the longitudinal cutting path, the longitudinal cutting path being located at the reserved cutting allowance boundary of the first package, cutting through the molding body of the first package, the first substrate, the molding body of the second package, and the second substrate, the longitudinal cut removing the reserved cutting allowance on both sides of the longitudinal direction of the first package; S63: The cutting machine performs a transverse cut along the transverse cutting path, which is located at the boundary of the reserved cutting allowance of the first package. It cuts through the molding body, the first substrate, the molding body and the second substrate of the first package. The transverse cut removes the reserved cutting allowance on both sides of the first package. The longitudinal cut and the transverse cut separate the encapsulation structure into multiple final packages with the final package size.

8. A POP packaging structure in the preparation method according to any one of claims 1 to 4, characterized in that, Before the adhesive is cured, the POP encapsulation structure includes two encapsulation bodies stacked on top of each other, with the upper layer being a smaller first encapsulation body (11) and the lower layer being a larger second encapsulation body (12). The first package (11) is disposed above the second package (12), and the size of the first package (11) is smaller than the size of the second package (12); The first package (11) is placed in the center within the actual size range of the POP package structure, and an annular gap for dispensing is left between the four edges of the first package (11) and the edge of the second package (12). The second package (12) has a copper pillar (13) embedded inside. The copper pillar (13) penetrates vertically through the second package (12). The upper end face of the copper pillar (13) is flush with or exposed to the upper surface of the second package (12), and the lower end face is flush with the lower surface of the second package (12). The top of the copper pillar (13) is connected to the solder ball (14) on the bottom surface of the first package (11), and a metallurgical connection is formed by reflow soldering to realize the electrical conduction between the first package (11) and the second package (12); the bottom of the copper pillar (13) is connected to the ball pad on the lower surface of the second package (12), and then connected to the external circuit board through the solder ball.

9. The POP packaging structure according to claim 8, characterized in that, The annular gap and the linear channel between the two adjacent first encapsulation bodies (11) are spatially connected, together forming a dispensing gap for the dispensing needle to enter and move. The linear channel is located directly above the cut channel between two adjacent second packaging units. The bottom of the linear channel is the upper surface of the second package (12), and the two sides of the linear channel are the opposite sidewalls of the adjacent first package (11).

10. The POP packaging structure according to claim 8, characterized in that, The width Wgap of the cut channel between adjacent second packaging units on the second substrate is 3mm. The single-side dimension of the first package (11) is 0.5mm smaller than the final packaged product size, i.e., the shrinkage δ=0.5mm; the linear channel width between adjacent first packages (11) after sealing. Waccess = Wgap - 2δ, and Waccess = 2mm.