Temperature-controllable polymer spline die cutting device
By using a combination of thermal insulation layer, temperature-controlled heating plate and isostatically pressed high-purity graphite plate in the polymer spline die-cutting device, uniform temperature control of the polymer material and continuity of the cutting process are achieved, solving the existing technical problems It improves the accuracy and efficiency of mechanical property testing by eliminating the problems of long time consumption and structural inconsistency.
Patent Information
- Application Number
- CN202420162706.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-23
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2034-01-23
Smart Images

Figure CN221834502U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a polymer material die-cutting device, in particular to a temperature-controllable polymer strip die-cutting device. Background Art
[0002] The existing die-cutting method for polymer materials usually adopts the traditional process of first pressing the polymer plate, film or sheet, and then cutting the sample strips individually with a die cutter. The device matched with this method has the defects of being time-consuming and inefficient. Summary of the invention
[0003] The invention of the utility model aims to overcome the shortcomings of the prior art and provide a device capable of realizing the continuity of the temperature control process and the die cutting process of the polymer spline.
[0004] The utility model adopts the following technical solutions:
[0005] A temperature-controllable polymer spline die-cutting device, comprising a base and a die cutter, characterized in that: a heat-insulating layer is embedded in the base, a temperature-controlled heating plate is embedded in the heat-insulating layer, an isostatically pressed high-purity graphite plate is embedded in the temperature-controlled heating plate, a shallow groove structure is arranged in the isostatically pressed high-purity graphite plate, the shallow groove structure is arranged correspondingly to the die cutter up and down, and a polymer plate is placed in the shallow groove structure;
[0006] The cutting die is connected to the power device through a metal pressing plate and a high-strength magnet;
[0007] The metal pressing plate is connected to the base through a column, and an adjustable limiting device is installed at the bottom of the column.
[0008] Compared with the prior art, the utility model adopting the above technical solution can perform uniform and accurate temperature control on the polymer material, ensure that several specimens cut at the same time have the same heating history and the consistency of the internal structure of the cut specimens, greatly improve the uniformity of the results of subsequent mechanical properties tests of the polymer specimens, and improve the accuracy of the performance test results.
[0009] The utility model adopts the following preferred solution:
[0010] Furthermore, the adjustable limiting device adopts an adjusting nut or a limiting block.
[0011] Furthermore, a top plate is installed on the upper part of the column.
[0012] Furthermore, the top plate is threadedly connected to the upper part of the column.
[0013] Furthermore, the power device adopts a cylinder, a piston rod at one end of the cylinder is connected to the high-strength magnet, and a piston rod at the other end of the cylinder is equipped with a stroke-adjustable nut.
[0014] Furthermore, the length of the knife die which is perpendicular to the metal pressing plate and is placed outside the metal pressing plate is equal to the sum of the height of the adjustable limiting device and the height of the shallow groove structure.
[0015] Furthermore, an embedding groove is provided at the lower part of the metal pressing plate, a metal embedded plate is installed in the embedding groove, the lower surface of the metal embedded plate is arranged flush with the lower surface of the metal pressing plate, a shallow groove structure is provided on the metal embedded plate, and the knife die is installed in the shallow groove structure.
[0016] Furthermore, a shallow groove structure is provided on the lower surface of the metal pressing plate, the cutting die is installed in the shallow groove structure, and a high-strength magnet is installed on the upper surface of the metal pressing plate, and the high-strength magnet is arranged corresponding to the upper and lower parts of the cutting die.
[0017] Furthermore, the length of the knife die which is perpendicular to the metal inner panel and is placed outside the metal inner panel is equal to the sum of the height of the adjustable limiting device and the height of the shallow groove structure.
[0018] Furthermore, the temperature-controlled heating plate is externally connected to a heating control element and a cooling control element. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of the first embodiment of the utility model.
[0020] Figure 2 yes Figure 1 Schematic diagram of the lower surface structure of the middle metal pressure plate.
[0021] Figure 3 yes Figure 1 Top view of the inner layer of the middle base.
[0022] Figure 4 It is a structural diagram of the second embodiment.
[0023] Figure 5 yes Figure 4 Schematic diagram of the structure of the lower surface of the metal pressure plate.
[0024] Figure 6 yes Figure 4 AA section view in. DETAILED DESCRIPTION
[0025] The utility model is described in detail below with reference to the accompanying drawings and embodiments: Embodiment 1:
[0026] A temperature-controlled polymer strip die-cutting device, see attached Figure 1 To Attachment Figure 3The structure shown in the figure comprises a base 1, an insulation layer 2, a temperature-controlled heating plate 3, an isostatically pressed high-purity graphite plate 4, a cooling control element 5, a metal pressure plate 6, a column 7, a high-strength magnet 8, a cylinder 9, a stroke-adjustable nut 10, a piston rod 1 11, a piston rod 2 12, a cutting die 13, a top plate 14, a polymer sheet 15, a heating control element 16, a limit block 17, a shallow groove structure 18, and a shallow groove structure 19.
[0027] In this embodiment, the base 1 is embedded with an insulation layer 2, the insulation layer 2 is embedded with a temperature-controlled heating plate 3, the temperature-controlled heating plate 3 is embedded with an isostatically pressed high-purity graphite plate 4, the isostatically pressed high-purity graphite plate 4 is provided with a shallow groove structure 19, the shallow groove structure 19 is arranged corresponding to the knife die 13 up and down, and a polymer plate 15 is placed in the shallow groove structure 19.
[0028] The cutting die 13 is connected to the power device through the metal pressing plate 6 and the high-strength magnet 8 in sequence.
[0029] The metal pressing plate 6 is connected to the base 1 through a column 7, and an adjustable limit device is installed at the bottom of the column 7.
[0030] like Figure 1 As shown in , the adjustable limiting device adopts a limiting block 17, and can also be replaced by an adjustable nut.
[0031] A top plate 14 is mounted on the upper portion of the column 7 .
[0032] The top plate 14 is connected to the upper part of the column 7 via threads; that is, the upper end of the column 7 is provided with a threaded structure.
[0033] The power device adopts a cylinder 9, a piston rod 2 12 at one end of the cylinder 9 is connected to the high-strength magnet 8, and a piston rod 11 at the other end of the cylinder 9 is equipped with a stroke-adjustable nut 10.
[0034] The cutting die 13 is perpendicular to the metal pressing plate 6 and the length of the portion outside the metal pressing plate 6 is equal to the sum of the height of the limiting block 17 and the height of the shallow groove structure 19 .
[0035] The four upright posts 7 are respectively placed near the four corners of the metal pressure plate 6 with a rectangular structure, and are symmetrically arranged in pairs at the front and back and in pairs at the left and right.
[0036] A shallow groove structure 18 is provided on the lower surface of the metal pressing plate 6 , and the cutting die 13 is installed in the shallow groove structure 18 . A high-strength magnet 8 is installed on the upper surface of the metal pressing plate 6 , and the high-strength magnet 8 is arranged correspondingly to the upper and lower parts of the cutting die 13 .
[0037] The cutting dies 13 are evenly distributed in the shallow groove structure 18 on the lower surface of the metal pressing plate 6; and the number of the cutting dies 13 is five.
[0038] The temperature control heating plate 3 is externally connected to a heating control element 16 and a cooling control element 5 .
[0039] There is a stopper 17 at each connection between the four columns 7 and the base 1. The stopper 17 is detachable. The stopper 17 of different heights is selected according to the height of the cutter die, so that the blade at the bottom of the cutter die 13 just contacts the bottom of the inner groove structure of the isostatically pressed high-purity graphite plate 4, avoiding hard contact between the cutter die 13 and the isostatically pressed high-purity graphite plate 4 and damaging the blade of the cutter die 13; the cutter die 13 can be selected as a rectangular cutter die 13, a dumbbell-shaped cutter die 13 or a cutter die 13 of other specifications according to the type of polymer spline test method. Of course, at this time, the shallow groove structure 18 on the lower surface of the metal pressure plate also needs to be changed in shape accordingly. Or: The upper shape of the dumbbell-shaped cutter die 13 is the same as the existing Figure 2 The shallow groove structure 18 shown in FIG.
[0040] The polymer sheet used for die-cutting in the device can be first pressed and formed by a hot press, a flat vulcanizer, etc., with a thickness of 1 to 5 mm, and a length and width not greater than the length and width of the shallow groove structure 19 of the isostatically pressed high-purity graphite plate 4.
[0041] The isostatically pressed high-purity graphite plate 4 is embedded in a temperature-controlled heating plate 3 with grooves. The temperature-controlled heating plate 3 is made of metal. The temperature-controlled heating plate 3 is externally connected to a heating control element 16 and a cooling control element 5 .
[0042] The isostatically pressed high-purity graphite plate 4 has good thermal conductivity and can uniformly heat the polymer plate 15 placed in the shallow groove structure 19 of the isostatically pressed high-purity graphite plate 4. The depth of the shallow groove structure 19 is 1-5 mm, and the polymer plate 15 placed therein can be in the form of a sheet or a film.
[0043] The temperature control heating plate 3 can control the heating and cooling speed, isothermal time, etc.; the temperature control heating plate 3 is located in the insulating layer 2 with grooves, and the insulating layer 2 is made of polytetrafluoroethylene, and can also be made of other insulating and hard materials; the insulating layer 2 is located in the base 1 with grooves, and the base is made of metal.
[0044] When the piston rod 12 moves downward to the lowest position, the cutting die 13 embedded in the shallow groove structure 18 of the metal pressing plate 6 cuts the polymer sheet 15 in the groove of the isostatically pressed high-purity graphite plate 4 into strips.
[0045] The temperature-controlled heating plate 3 heats the isostatically pressed high-purity graphite plate 4. The isostatically pressed high-purity graphite plate 4 has high thermal conductivity and can be quickly and accurately temperature-controlled under the action of the temperature-controlled heating plate 3. The temperature at each position inside the shallow groove structure 19 of the isostatically pressed high-purity graphite plate 4 is uniform, and the polymer sheet 15 placed in the shallow groove structure 19 of the isostatically pressed high-purity graphite plate 4 is heated evenly, and the structure and performance of the finally cut strips are consistent.
[0046] Action process:
[0047] The cylinder 9 drives the piston rod 11 and the piston rod 2 12 to move up and down, and the cylinder 9 is connected to an air compressor; the stroke adjustable nut 10 installed on the top of the piston rod 11 can adjust the maximum stroke of the piston rod 11 and the piston rod 2 12. The piston rod 11 and the piston rod 2 12 share the same piston to achieve up and down displacement through the cylinder 9; the piston rod 11 and the piston rod 2 12 share a piston, which is actually a mounting rod at both ends of a piston, and the piston rod 11 and the piston rod 2 12 have the same length.
[0048] The piston rod 12 drives the high-strength magnet 8 and the metal pressure plate 6 to move up and down synchronously, and the top plate 14 limits the highest moving position of the piston rod 12 pull rod.
[0049] The limit block 17 limits the lowest moving position of the piston rod 12, and the limit block 17 is detachable. The limit blocks 17 of different heights can be selected according to the height of the cutting die 13, so that when the cutting die 13 is at the lowest position, the blade just contacts the bottom end face of the groove of the shallow groove structure 19 of the isostatically pressed high-purity graphite plate 4, avoiding hard contact between the cutting die 13 and the isostatically pressed high-purity graphite plate 4.
[0050] The cutting die 13 is embedded in the shallow groove structure 18 on the bottom end face of the metal pressing plate 6 and fixed by the high-strength magnet 8; there is a through hole at each of the four right angles of the metal pressing plate 6, and the hole diameter fits the diameter of the four columns 7, so that the metal pressing plate 6 can slide up and down along the columns 7.
[0051] Four columns 7 are fixed on the base; the base 1 has a groove, in which a thermal insulation layer 2 is nested; the thermal insulation layer 2 has a groove, in which a temperature-controlled heating plate 3 is nested; the temperature-controlled heating plate 3 has a groove, and an external heating control element 16 and a cooling control element 5 are connected, which can accurately control the heating and cooling speed, temperature, isothermal time, etc.
[0052] Work Case:
[0053] (1) For polymer materials with a very slow crystallization rate, such as polylactic acid, the device can be used to set the temperature and isothermal time of the temperature-controlled heating plate 3, so that the polylactic acid can be crystallized under isothermal conditions, and its crystallinity can be regulated. After that, die-cutting is performed, and the die-cut specimens are then subjected to tensile, impact or bending performance tests. In this way, the relationship between the crystallinity of polylactic acid and mechanical properties such as tensile properties, impact strength, and bending strength can be explored.
[0054] (2) The polymer sheet 15 can be annealed. Taking polylactic acid as an example, polylactic acid is not fully crystallized during the hot pressing process and has a low degree of crystallinity, which affects its mechanical strength. The temperature and isothermal time of the temperature-controlled heating plate 3 can be set by the device to anneal the polylactic acid. After annealing, die-cutting is performed. The obtained die-cut specimens are subjected to tensile, impact or bending performance tests to explore the effects of different annealing temperatures and annealing times on the mechanical properties of polylactic acid.
[0055] (3) The temperature-controlled heating plate 3 of the device can adjust the heating and cooling rates. It can heat the polymer sheet 15 to near the melting point and then cool it to room temperature at different cooling rates. The different cooling rates lead to different crystalline structures and crystallinity of the polymer, which in turn affects its mechanical properties. Therefore, the relationship between the cooling rate and the polymer crystallinity, crystalline structure and mechanical properties can be explored.
[0056] (4) The isostatically pressed high-purity graphite plate 4 in the device has good thermal conductivity and high strength. The temperature inside the shallow groove structure 19 is uniform, and the temperature at each location of the polymer sheet 15 can be accurately controlled, eliminating the differences in the thermal history of the splines cut at different positions of the polymer sheet 15. The splines have the same thermal history and the structure tends to be uniform. In this way, the error of the subsequent spline mechanical property test results can be reduced.
[0057] The device can realize continuous operation of the in-situ temperature control process and the die-cutting process of the polymer sheet 15, and can cut multiple specimens at one time. The number of specimens required for subsequent mechanical property testing can be prepared in one operation, replacing the time-consuming and inefficient process of first pressing the polymer sheet 15 and then cutting the specimens individually with a die cutter 13 in the traditional process.
[0058] At the same time, the device adopts isostatically pressed high-purity graphite plate 4 with high thermal conductivity and high strength, which can perform uniform and accurate temperature control on the polymer sheet 15, ensuring that several specimens cut at the same time have the same heating history, ensuring the consistency of the internal structure of the specimens cut at the same time, greatly improving the consistency of the results of the polymer specimens in subsequent mechanical properties tests, and improving the accuracy of the performance test results. Embodiment 2:
[0059] The difference from the first embodiment is that, see the attached Figure 4-6 In the figure, the added reference numerals are: metal embedded plate 20, mounting member 21, embedding groove 22.
[0060] The metal pressing plate 6 is provided with an embedding groove 22 at the bottom, and a metal embedded plate 20 is installed in the embedding groove 22. The lower surface of the metal embedded plate 20 is flush with the lower surface of the metal pressing plate 6. A shallow groove structure 18 is provided on the metal embedded plate 20, and the knife die 13 is installed in the shallow groove structure 18.
[0061] The length of the knife die 13 which is perpendicular to the metal inner panel 20 and is located outside the metal inner panel 20 is equal to the sum of the height of the adjustable limiting device and the height of the shallow groove structure 19 .
[0062] The metal inner plate 20 is connected to the metal pressing plate 6 via a mounting member 21. When a different cutting die 13 needs to be replaced, or when the cutting die 13 needs to be replaced due to wear, the metal inner plate 20 can be removed from the metal pressing plate 6 via the mounting member 21, which is convenient for replacement. The mounting member 21 preferably adopts a countersunk screw, or a countersunk hole is provided on the metal inner plate.
[0063] This device can be used for in-situ temperature control experiments on polymers. The heating and cooling rates, temperature, and isothermal time are all controllable. It can be used to prepare polymer strips with different crystalline structures caused by isothermal and non-isothermal processes, and used for subsequent mechanical properties tests.
[0064] The present invention is not limited to the above-mentioned ones, and all equivalent substitutions made within the protection scope of the present invention are deemed to be within the protection scope of the present invention.
Claims
1. A temperature-controllable polymer spline die-cutting device, comprising a base and a die cutter, characterized in that: The base is embedded with an insulation layer, the insulation layer is embedded with a temperature control heating plate, the temperature control heating plate is embedded with an isostatically pressed high-purity graphite plate, the isostatically pressed high-purity graphite plate is provided with a shallow groove structure, the shallow groove structure is arranged corresponding to the upper and lower parts of the knife die, and a polymer plate is placed in the shallow groove structure; The cutting die is connected to the power device through a metal pressing plate and a high-strength magnet; The metal pressing plate is connected to the base through a column, and an adjustable limiting device is installed at the bottom of the column.
2. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: The adjustable limiting device adopts an adjusting nut or a limiting block.
3. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: A top plate is arranged on the upper part of the column.
4. The temperature-controllable polymer spline die-cutting device according to claim 3, characterized in that: The top plate is threadedly connected to the upper part of the column.
5. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: The power device adopts a cylinder, a piston rod at one end of the cylinder is connected to the high-strength magnet, and a piston rod at the other end of the cylinder is equipped with a stroke-adjustable nut.
6. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: The length of the knife die which is perpendicular to the metal pressing plate and is placed outside the metal pressing plate is equal to the sum of the height of the adjustable limiting device and the height of the shallow groove structure.
7. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: The lower part of the metal pressing plate is provided with an embedding groove, in which a metal embedded plate is installed, the lower surface of the metal embedded plate is arranged flush with the lower surface of the metal pressing plate, the metal embedded plate is provided with a shallow groove structure, in which the knife die is installed.
8. The temperature-controllable polymer spline die-cutting device according to claim 1, characterized in that: The lower surface of the metal pressing plate is provided with a shallow groove structure, the cutting die is installed in the shallow groove structure, and the upper surface of the metal pressing plate is provided with a high-strength magnet, and the high-strength magnet is arranged corresponding to the upper and lower parts of the cutting die.
9. The temperature-controllable polymer spline die-cutting device according to claim 7, characterized in that: The length of the knife die which is perpendicular to the metal inner panel and is located outside the metal inner panel is equal to the sum of the height of the adjustable limiting device and the height of the shallow groove structure.