Swab

By setting a specific thickness of the water-based glue layer and a latex-like glue structure, it ensures that the villi fibers are evenly embedded and firmly fixed in the swab, solving the problem of uneven villi embedding and falling off in traditional swabs, improving sampling and release efficiency, and enhancing The stability and detection accuracy of the swab are improved.

CN221844797UInactive Publication Date: 2024-10-18SHENZHEN KANGDAAN BIOLOGICAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322910292.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-27
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The thickness and fixation method of glue in traditional swabs may cause uneven embedding of villi, affecting sampling and sample release efficiency, and may react with samples or reagents, affecting analytical accuracy.

Method used

Design a swab with a water-based glue layer with a dry thickness ranging from 0.15mm to 0.3mm, ensuring that the fluff fibers are vertically inserted and firmly fixed, using a latex-like glue and cortex structure, combined with a polystyrene stem and a hydrophilic or hydrophobic fibers to improve sampling and release efficiency.

Benefits of technology

It ensures that the fluff fibers are firmly fixed during the sampling process and is not easy to fall off, improves sampling efficiency and sample release efficiency, enhances the structural stability and durability of the swab, reduces the amount of glue used, and ensures the accuracy of detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221844797U_ABST
    Figure CN221844797U_ABST
Patent Text Reader

Abstract

The utility model provides a swab which comprises a rod part and a sampling head, the swab comprises a water-based glue layer and a fluff layer, one end of the rod part is coated with the water-based glue layer, and the fluff layer is formed by vertically planting a plurality of fluff fibers on the water-based glue layer; wherein the thickness of the dried water-based glue layer ranges from 0.15 mm to 0.3 mm. According to the provided swab, the thickness range of the dried water-based glue layer is set to be 0.15 mm-0. 3 mm, the thickness range provides enough depth for the fluff, it is ensured that the fluff is firmly fixed and is not prone to falling off in the sampling process, and the structural stability of the swab is enhanced. And in the specific thickness range, the fluff fibers can be uniformly and completely embedded into the glue layer. Therefore, each fluff fiber can be in contact with the surface to be detected, so that the sampling efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of medical equipment, and in particular to a swab. Background Art

[0002] As a basic tool in medical and laboratory, swabs are widely used in many diagnostic and sample collection applications. Traditional swab designs vary, and the main considerations include sampling efficiency, material biocompatibility, and sample release ability.

[0003] In the evolution of swab design, the transplantation and fixation of villi has become a core consideration. In order to maximize sampling efficiency and sample release, the villi usually need to be firmly fixed to the swab rod. Traditional technical solutions usually use various glues or adhesives to fix the villi to the swab rod. However, the thickness, type and fixation method of these glues may affect the sampling and release efficiency of the villi.

[0004] Although existing technologies provide certain solutions for the transplantation of villi, there are still some key defects. For example, some glues may not completely fix the villi, resulting in the loss of villi during sampling. In addition, inconsistent thickness of the glue layer may cause the villi to be embedded unevenly, thus affecting the efficiency of sample collection and release. Moreover, some glues may react with specific samples or reagents, further affecting the accuracy of analysis. These defects highlight the need to develop a new swab with optimized glue thickness and ensure vertical implantation of villus fibers. Utility Model Content

[0005] In view of this, it is necessary to provide a swab that is convenient for vertical implantation of villi to solve the above problems.

[0006] An embodiment of the present application provides a swab, comprising:

[0007] Rod;

[0008] The sampling head comprises a water-based glue layer and a fluff layer, wherein the water-based glue layer is coated on one end of the rod, and the fluff layer comprises a plurality of fluff fibers vertically planted on the water-based glue layer;

[0009] Wherein, the thickness of the aqueous glue layer after drying is in the range of 0.15mm-0.3mm.

[0010] In at least one embodiment of the present application, the thickness of the aqueous glue layer after drying is 0.2 mm.

[0011] In at least one embodiment of the present application, the aqueous glue layer includes a glue layer and a skin layer attached to the glue layer, and a plurality of fluff fibers are vertically inserted into the glue layer through the skin layer.

[0012] In at least one embodiment of the present application, the adhesive layer is latex glue.

[0013] In at least one embodiment of the present application, the villi layer is hydrophilic nylon villi, which is used for collecting human body sample fluid.

[0014] In at least one embodiment of the present application, the fluff layer is one of hydrophobic polypropylene or polyester, which is used to improve the elution rate of the swab during detection.

[0015] In at least one embodiment of the present application, the rod is a polystyrene rod.

[0016] In at least one embodiment of the present application, the rod portion includes a testing portion and a handle portion that is breakably connected to the testing portion, and the water-based glue layer is coated on the testing portion.

[0017] In at least one embodiment of the present application, the rod portion further includes a breaking portion, and opposite ends of the breaking portion are respectively provided on the testing portion and the handle portion, for breaking along the breaking portion.

[0018] In at least one embodiment of the present application, the breaking portion is provided with a fold for breaking the swab at the fold.

[0019] The swab provided above sets the thickness of the aqueous glue layer after drying to 0.15mm-0.3mm. This thickness range provides sufficient depth for the villi, ensuring that they are firmly fixed during the sampling process and are not easy to fall off, thereby enhancing the structural stability of the swab. In this specific thickness range, the villi fibers can be evenly and completely embedded in the glue layer. This ensures that each villi fiber can contact the surface to be tested, thereby improving the sampling efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a three-dimensional diagram of a swab in one embodiment of the present application.

[0021] Figure 2 for Figure 1 A cross-sectional view of the swab is shown.

[0022] Main component symbols

[0023] 100, swab; 10, rod; 11, testing part; 12, handle; 13, breaking part; 131, crease; 20, sampling head; 21, water-based glue layer; 211, bonding layer; 212, cortex; 22, villi layer. DETAILED DESCRIPTION

[0024] The embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all the embodiments.

[0025] It should be noted that when a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be a central component at the same time. When a component is considered to be "located on" another component, it may be directly located on the other component or there may be a central component at the same time. The terms "top", "bottom", "upper", "lower", "left", "right", "front", "back", and similar expressions used herein are for illustrative purposes only.

[0026] An embodiment of the present application provides a swab, comprising:

[0027] Rod;

[0028] The sampling head comprises a water-based glue layer and a fluff layer, wherein the water-based glue layer is coated on one end of the rod, and the fluff layer comprises a plurality of fluff fibers vertically planted on the water-based glue layer;

[0029] Wherein, the thickness of the aqueous glue layer after drying is in the range of 0.15mm-0.3mm.

[0030] The swab provided above sets the thickness of the aqueous glue layer after drying to 0.15mm-0.3mm. This thickness range provides sufficient depth for the villi, ensuring that they are firmly fixed during the sampling process and are not easy to fall off, thereby enhancing the structural stability of the swab. In this specific thickness range, the villi fibers can be evenly and completely embedded in the glue layer. This ensures that each villi fiber can contact the surface to be tested, thereby improving the sampling efficiency.

[0031] Some embodiments of the present application are described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the following embodiments and features in the embodiments can be combined with each other.

[0032] See also Figure 1-Figure 2 , an embodiment of the present application provides a swab 100, comprising:

[0033] Rod 10;

[0034] The sampling head 20 includes a water-based glue layer 21 and a fluff layer 22. The water-based glue layer 21 is coated on one end of the rod 10. The fluff layer 22 includes a plurality of fluff fibers vertically planted on the water-based glue layer 21.

[0035] The thickness of the aqueous glue layer 21 after drying is in the range of 0.15 mm to 0.3 mm.

[0036] Specifically, the rod portion 10 provides the main structure of the swab 100 , which facilitates the user to grasp and operate the swab 100 for sampling, enhances the mechanical strength and stability of the swab 100 , and provides a convenient hand-held portion.

[0037] Furthermore, the sampling head 20 is the part of the swab 100 that contacts the sampled object, plays the role of actual sampling, provides the swab 100 with the functional part of actual sampling, and is the core component of the swab 100.

[0038] Furthermore, the aqueous glue layer 21 is used to fix and support the villi layer 22, ensuring that the villi fibers are vertically inserted and firmly secured, making the villi fibers evenly distributed, stable and not easy to fall off, thereby enhancing the sampling effect and the durability of the swab 100. The specific thickness range ensures uniform implantation of the villi fibers and efficient sample release.

[0039] Furthermore, the fluff layer 22 is in actual contact with the sampled object, adsorbs and retains the sample, thereby improving the sampling efficiency and maintaining the stability of the sample.

[0040] When sampling in the above scheme, the user operates the swab 100 through the rod 10 to make the villi layer 22 of the sampling head 20 contact the sample. Since the villi fibers are perpendicular to the aqueous glue layer 21, this ensures sufficient contact with the sample, thereby obtaining a higher sampling efficiency. The vertical arrangement of the villi fibers also increases the contact area between the villi fibers and the sample, thereby increasing the adsorption amount of the sample. The aqueous glue layer 21 provides sufficient support within a specific thickness range to ensure that the villi fibers do not fall off during the sampling process.

[0041] It should be noted that, in the manufacturing process of the swab 100, the following steps are used:

[0042] Pretreatment: First, a layer of adhesive, usually water-based glue, is coated on the head of the swab 100. This glue acts as a binding agent to allow the fibers to be fixed thereon.

[0043] Electrostatic flocking: The flock fibers are placed in a container with an electrostatic field. The fibers become charged due to electrostatic forces and they are attracted to the surface of the sticky object.

[0044] Insertion and fixation: Due to the electrostatic force, the pile fibers are inserted into the adhesive base layer in a nearly vertical manner. This ensures that they are firmly fixed and will not fall off easily in actual application.

[0045] Drying and curing: The glue then needs to be dried and cured to ensure the fibers are firmly fixed in their position. This may be accelerated by natural drying or the use of heat.

[0046] Inspection and trimming: After flocking, the swab 100 is inspected to ensure that the fibers are evenly distributed and properly fixed. If necessary, trimming is performed, such as cutting off excessively long fibers.

[0047] Through this process, the head of the swab 100 will be evenly covered with fluff fibers, which helps to improve the efficiency of sample collection and release.

[0048] However, in the manufacturing process of the above-mentioned swab 100, the villi need to be inserted and cured in the aqueous glue layer 21. The insertion angle and the thickness of the aqueous glue will lead to the stability of the villi insertion, as follows: In order to ensure that the villi fibers can be completely and vertically inserted into the glue layer, the glue needs to have a certain thickness. This thickness should be enough to accommodate most of the length of the villi to ensure that they are firmly fixed and will not fall off easily during the sampling process. And a sufficiently thick glue layer may provide better protection and sustainability. In practical applications, the swab 100 may be subjected to some friction and pressure, and a thicker glue layer can increase its durability and ensure that the villi fibers will not fall off easily. Further, a thicker glue layer may form a more uniform and stable structure when solidified, which helps to maintain the position of the villi fibers and ensure their effect during the sampling process, and a sufficiently thick glue layer helps to increase the collection and release of samples. The villi fibers can better absorb and release samples in the glue layer, improving the accuracy of the detection.

[0049] The present application conducted experiments by setting the water-based glue layer 21 to different thicknesses after drying, and obtained the conclusions as shown in the following table:

[0050]

[0051] From the above experimental data, it can be seen that in order to ensure the proportion of the villi to extract a sufficient amount of sample liquid and to save the amount of water-based glue, the thickness of the water-based glue layer 21 after drying is selected to be between 0.15mm and 0.3mm, which can not only extract enough sample liquid but also greatly reduce the amount of water-based glue used.

[0052] In a specific embodiment, when the thickness of the water-based glue layer 21 after drying is 0.2 mm, the proportion of the fluff present after sampling is 90%, the sample liquid is sufficient for testing and the amount of water-based glue used is relatively small, which saves material costs and ensures the accuracy of sampling.

[0053] The effect of controlling the thickness of the water-based glue layer 21 and vertically inserting the fluff into the water-based glue layer 21 is explained as follows:

[0054] Insertion depth of the fluff fibers: The fluff fibers of the swab 100 need to be stably inserted into the glue layer. The thickness of the glue must be sufficient so that the fluff fibers can be inserted evenly and vertically. If the glue layer is too thin, the fluff may not be fully inserted, which will affect its efficiency and stability when collecting and releasing samples.

[0055] Physical stability of the glue: A moderate thickness means that the glue layer can provide sufficient mechanical strength after curing. This ensures that during the sampling process, even if the swab 100 is subjected to friction or pressure, the glue layer will not be easily broken or damaged.

[0056] Adsorption and release of samples: The thickness of the glue can affect the interaction between the fluff fibers and the sample to be tested. A suitable thickness can ensure that the fluff fibers have enough space to fully contact the sample, thereby improving the adsorption and release efficiency of the sample.

[0057] Uniformity of glue curing process: The curing process of glue takes time and may require certain conditions (such as temperature). If the glue layer is too thick, the curing rate inside and outside may be different, resulting in unevenness. The thickness of 0.2mm may be an empirical balance point to ensure that the glue can be cured evenly and quickly.

[0058] Cost and manufacturing efficiency: From an economic and production perspective, choosing an appropriate glue thickness can balance raw material costs and production efficiency. Too thick a glue layer may increase costs and prolong curing time, while too thin a glue layer may sacrifice product quality.

[0059] The following reasons should be considered for vertically inserting the fluff into the aqueous glue layer 21:

[0060] Maximize surface contact: When the villi are inserted vertically into the glue layer, their effective surface area is maximized. This means that more villi fibers are exposed to the outside and can fully contact with the sampled material, thereby improving sampling efficiency.

[0061] Enhanced stability of the fluff: vertical insertion ensures deeper contact and fixation of the fluff with the glue layer. This helps to make the fluff more stable during sampling and reduce fiber shedding due to friction or other reasons.

[0062] Improving sample release efficiency: The vertical villi structure forms many tiny "channels" or "holes" that facilitate liquid flow and sample release when the swab 100 is inserted into the test fluid.

[0063] Uniform sampling: Since the fluff fibers are evenly and vertically distributed in the glue layer, this ensures that the sampling effect is consistent throughout the head of the swab 100.

[0064] Prevent adhesion between fluff fibers: If the fluff is not inserted vertically but distributed randomly or obliquely, the fibers may stick to each other or get entangled. This will reduce sampling efficiency and may cause damage or shedding of the fibers.

[0065] Manufacturing and Quality Control: From a production perspective, ensuring that the fluff fibers are inserted vertically allows for a more standardized manufacturing process, easier quality control, and ensures consistency and reliability for every swab 100.

[0066] In one embodiment, the aqueous glue layer 21 includes a glue layer 211 and a skin layer 212 attached to the glue layer 211 , and a plurality of fluff fibers are vertically inserted into the glue layer 211 through the skin layer 212 .

[0067] Specifically, the aqueous glue layer 21 provides a stable and elastic base, into which the fluff fibers can be inserted and fixed, for providing an adhesive medium that is environmentally friendly and has good compatibility with the human body and microorganisms.

[0068] Furthermore, the adhesive layer 211 serves as a main adhesive medium to provide a stable insertion and fixing position for the fluff fibers, so as to ensure the stability of the swab 100 during the sampling process and prevent the fluff fibers from falling off easily.

[0069] Furthermore, the skin layer 212 covers the outside of the glue layer 211 to provide a protective layer for the insertion of the fluff fibers, and also to increase the firmness of the structure, so as to further enhance the durability and stability of the swab 100 , and also to help keep the swab 100 clean.

[0070] When the above scheme is implemented, the operation process is as follows:

[0071] When sample collection is required, the swab 100 is used to contact and collect the sample. Due to the vertical insertion design of the villi fibers, they can fully contact the sample to be tested, thereby ensuring efficient adsorption of the sample. The swab 100 is then placed in the test liquid. The design of the villi fibers allows the sample to be efficiently released from the fibers into the liquid. Finally, the liquid is analyzed by various detection methods to obtain the desired results.

[0072] In one embodiment, the adhesive layer 211 is latex glue.

[0073] In a specific embodiment, the villi layer 22 is hydrophilic nylon villi, which is used for collecting human body sample fluids, such as body fluids or human oral or nasal mucosal fluids.

[0074] In another specific embodiment, the villi layer 22 is made of hydrophobic polypropylene or polyester, which is used to improve the elution rate of the swab 100 during detection, such as for antigen detection.

[0075] In a specific embodiment, the rod 10 is a polystyrene rod.

[0076] In one embodiment, the rod portion 10 includes a testing portion 11 and a handle portion 12 that is breakably connected to the breaking portion 13 , and the water-based glue layer 21 is coated on the testing portion 11 .

[0077] It should be noted that the test part 11, as the part covered by the water-supplying glue layer 21 and the villi layer 22, is inserted into the oral cavity or nasal cavity of the human body when in use, so as to support the villi for testing. The handle 12 is a handle for a person to hold and insert the test part 11 into the oral cavity and nasal cavity of the human body. Specifically, it is a long rod-shaped structure, so that a person can hold the test part 11 and insert it into a deeper cavity of the human body to extract body fluids.

[0078] Furthermore, in order to facilitate breaking the test portion 11 and the handle portion 12 , in a specific embodiment, the rod portion 10 also includes a breaking portion 13 , and the opposite ends of the breaking portion 13 are respectively arranged on the test portion 11 and the handle portion 12 , for breaking along the breaking portion 13 .

[0079] It should be noted that the breaking portion 13 is disposed between the test portion 11 and the handle portion 12, and is used to connect the test portion 11 and the handle portion 12. After the test portion 11 extracts body fluids from the human body, the test portion 11 is broken into a collection tube through the breaking portion 13, thereby avoiding the problem of difficulty in breaking after the medical staff completes the extraction of body fluids.

[0080] In a specific embodiment, the testing portion 11 , the breaking portion 13 and the handle portion 12 are integrally provided in a rod-shaped structure.

[0081] In a specific embodiment, the breaking portion 13 is provided with a fold 131, which is used to break the swab 100 from the fold 131. Preferably, the fold 131 is an unbroken fold 131 provided on the breaking portion 13, which is part of the prior art and will not be described in detail here.

[0082] The swab 100 provided above sets the thickness of the aqueous glue layer 21 after drying to 0.15 mm-0.3 mm. This thickness range provides sufficient depth for the villi, ensuring that they are firmly fixed during the sampling process and are not easy to fall off, thereby enhancing the structural stability of the swab 100. In this specific thickness range, the villi fibers can be evenly and completely embedded in the glue layer. This ensures that each villi fiber can contact the surface to be tested, thereby improving the sampling efficiency.

[0083] The above is only an implementation method of the present application. It should be pointed out that a person skilled in the art can make improvements without departing from the inventive concept of the present application, but these improvements are within the scope of protection of the present application.

Claims

1. A swab, characterized in that: include: Rod; The sampling head comprises a water-based glue layer and a fluff layer, wherein the water-based glue layer is coated on one end of the rod, and the fluff layer comprises a plurality of fluff fibers vertically planted on the water-based glue layer; Wherein, the thickness of the aqueous glue layer after drying is in the range of 0.15mm-0.3mm.

2. The swab according to claim 1, characterized in that: The thickness of the aqueous glue layer after drying is 0.2 mm.

3. The swab according to claim 1, characterized in that: The water-based glue layer comprises a glue layer and a skin layer attached to the glue layer, and a plurality of fluff fibers are vertically inserted into the glue layer through the skin layer.

4. The swab according to claim 3, characterized in that: The adhesive layer is latex glue.

5. The swab according to claim 1, characterized in that: The villi layer is hydrophilic nylon villi and is used for collecting human body sample fluid.

6. The swab according to claim 1, characterized in that: The villi layer is one of hydrophobic polypropylene or polyester, and is used to improve the elution rate of the swab during detection.

7. The swab according to claim 1, characterized in that: The rod part is a polystyrene rod.

8. The swab according to claim 1, characterized in that: The rod portion comprises a testing portion and a handle portion which is breakably connected to the testing portion, and the water-based glue layer is coated on the testing portion.

9. The swab according to claim 8, characterized in that The rod portion further comprises a breaking portion, and opposite ends of the breaking portion are respectively arranged on the testing portion and the handle portion, and are used for breaking along the breaking portion.

10. The swab according to claim 9, characterized in that The breaking portion is provided with a fold, and is used to break the swab at the fold.