Die-casting feeding barrel
By designing a detachable die-casting feed barrel combination and an insulation ring plate, the problems of difficulty in cleaning wear debris and lack of insulation in traditional die-casting feed barrels are solved, achieving efficient maintenance and heat preservation of molten metal, and improving the quality of die-casting parts. and production efficiency.
Patent Information
- Application Number
- CN202420419571.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-05
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-03-05
AI Technical Summary
The traditional die-casting feed barrel is difficult to clean wear debris and lacks a heat preservation device, resulting in reduced quality of die-casting parts and low production efficiency.
A die-casting feed barrel including a first barrel and a second barrel is designed. Through the combination of seals and insulation ring plates, rapid disassembly and cleaning are achieved, and the metal melt is heated through the insulation ring plates to reduce heat. Lost.
It simplifies the maintenance process, improves work efficiency, avoids debris from being mixed into the molten metal, ensures the quality of die castings, and reduces the heat loss of the molten metal.
Smart Images

Figure CN221870223U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of die casting machines, and in particular to a die casting feed barrel. Background Art
[0002] Die casting machine is a machine used for pressure casting, including hot press chamber and cold press chamber, which are divided into vertical and horizontal types. The die casting machine hydraulically injects molten metal into the mold under pressure to cool and form. After the mold is opened, solid metal castings can be obtained.
[0003] In the die-casting industry, the die-casting feed barrel, as a key component, plays a vital role in the transportation of molten metal and the die-casting molding process. However, after long-term use, traditional die-casting feed barrels often have problems such as inner wall wear and blockage. The die-casting machine feed barrels on the market usually adopt an integrated design, and the disassembly and assembly process is complicated. It is difficult to efficiently clean the wear debris, resulting in a decrease in the quality of die-castings and reduced production efficiency. In addition, during the transportation of the molten metal in the feed pipe, due to the lack of a heat preservation device, some heat will be dissipated, affecting the production quality of die-castings.
[0004] With respect to the above-mentioned related technologies, the inventor believes that the die-casting barrel has the defects of being difficult to clean the wear debris and difficult to keep the molten metal warm, which leads to the low quality of the die-casting parts;
[0005] The above information disclosed in the background technology is only used to increase the understanding of the background technology of the present application, and therefore, it may include information that does not constitute the prior art known to ordinary technicians in the field. Utility Model Content
[0006] In order to solve the problem that it is difficult to clean the wear debris from the die-casting feed barrel and it is difficult to keep the molten metal warm, resulting in poor quality of die-casting parts, the present application provides a die-casting feed barrel.
[0007] The present application provides a die-casting feed barrel adopting the following technical solution:
[0008] A die-casting barrel comprises a first barrel, a sealing member is fixedly connected to the side surface of the first barrel, a second barrel is snap-connected to the side surface of the first barrel on the outside of the sealing member, and the second barrel is tightly attached to the side surface of the sealing member, a filling groove is provided on the outer surface of the second barrel, a flange joint is fixedly connected to the outer surface of the first barrel, and an insulation ring plate is snap-connected to the outer surfaces of the first barrel and the second barrel.
[0009] Preferably, a plurality of first limiting grooves are formed on the side surface of the first barrel, a plurality of limiting blocks are fixedly connected to the side surface of the second barrel opposite to the first barrel, and the plurality of limiting blocks can penetrate the sealing member and engage with the inner walls of the plurality of first limiting grooves.
[0010] Preferably, a first groove is formed on the side surface of the limit block, a first clamping groove is formed on the inner wall of the first limit groove, the inner wall of the first clamping groove is elastically slidably connected to a first clamping block via a spring, and the first clamping block can be engaged with the inner wall of the first groove.
[0011] Preferably, a second limiting groove is formed on the inner wall of the insulation ring plate, a limiting ring is integrally formed on the outer surface of the first barrel, and the limiting ring can be engaged with the inner wall of the second limiting groove.
[0012] Preferably, a second groove is formed on the outer surface of the second barrel, a second clamping groove is formed on the inner wall of the insulation ring plate, the inner wall of the second clamping groove is elastically slidably connected to a second clamping block via a spring, and the second clamping block can be engaged with the inner wall of the second groove.
[0013] In summary, this application includes the following beneficial technical effects:
[0014] 1. The first barrel is quickly separated from the second barrel by sliding the heat-insulating ring plate to remove it, and then sliding the second barrel, so as to clean the inner walls of the first barrel and the second barrel to prevent the device from being blocked, and to prevent the worn debris from being mixed in the molten metal, resulting in poor quality of the die casting, simplifying the maintenance process and improving work efficiency; compared with the prior art, it is easy to clean the debris;
[0015] 2. By setting up the insulation ring plate, the outer surfaces of the first barrel and the second barrel can be heated to keep the molten metal warm, thereby reducing the heat loss of the molten metal during the die-casting process and ensuring the quality of the die-casting parts; compared with the existing technology, it has the effect of keeping the molten metal warm. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is an overall schematic diagram of an embodiment of the application;
[0017] Figure 2 It is a cross-sectional structural diagram of the insulation ring plate;
[0018] Figure 3 It is a schematic diagram of the cross-sectional structure of the material tube;
[0019] Figure 4 yes Figure 3 A magnified schematic diagram;
[0020] Figure 5 yes Figure 3 Enlarged schematic diagram of point B.
[0021] Explanation of the reference numerals: 1. first barrel; 2. sealing element; 3. second barrel; 4. injection slot; 5. flange joint; 6. insulation ring plate; 7. first limiting slot; 8. limiting block; 9. first groove; 10. first clamping slot; 11. first clamping block; 12. second limiting slot; 13. limiting ring; 14. second groove; 15. second clamping slot; 16. second clamping block. DETAILED DESCRIPTION
[0022] The following is combined with Figure 1-5 This application is described in further detail.
[0023] The present application embodiment discloses a die casting feed barrel. Figure 1 , Figure 2 , Figure 3 A die-casting barrel comprises a tubular first barrel 1, an annular sealing member 2 is fixedly connected to the side surface of the first barrel 1, and a tubular second barrel 3 is snap-connected to the side surface of the first barrel 1 on the outside of the sealing member 2, and the second barrel 3 is in close contact with the side surface of the sealing member 2, so that the first barrel 1 and the second barrel 3 can be quickly disassembled, and the inner walls of the first barrel 1 and the second barrel 3 can be cleaned after long-term use, so as to avoid the worn debris from mixing in the metal melt, resulting in low quality of the die-casting, and can prevent the device from being blocked, simplifying the maintenance process, improving work efficiency, and through the sealing member 2 to The sealing of the module connection is ensured, the leakage of molten metal is effectively prevented, and the stability of the die-casting process is ensured. Secondly, a square groove-shaped injection groove 4 is opened on the outer surface of the second barrel 3, which is convenient for injecting molten metal from here for subsequent die-casting operations. An annular flange joint 5 is fixedly connected to the outer surface of the first barrel 1, and an annular insulation ring plate 6 is snap-connected to the outer surfaces of the first barrel 1 and the second barrel 3. The outer surfaces of the first barrel 1 and the second barrel 3 are heated by the insulation ring plate 6 to insulate the molten metal, reduce the heat loss of the molten metal during the die-casting process, and ensure the quality of the die-casting parts.
[0024] Reference Figure 3 A second annular groove-shaped limiting groove 12 is provided on the inner wall of the insulation ring plate 6, and an arc-shaped limiting ring 13 is integrally formed on the outer surface of the first barrel 1, and the limiting ring 13 can be engaged with the inner wall of the second limiting groove 12, so that after the second barrel 3 is stably installed on the side surface of the first barrel 1, the insulation ring plate 6 is slid from the outer surface of the second barrel 3 to the first barrel 1, so that the limiting ring 13 is engaged with the inner wall of the second limiting groove 12, thereby preliminarily limiting the insulation ring plate 6.
[0025] Reference Figure 4, a plurality of square groove-shaped first limiting grooves 7 are opened on the side surface of the first barrel 1, and a plurality of rectangular parallelepiped limiting blocks 8 are fixedly connected to the side surface of the second barrel 3 opposite to the first barrel 1, and the plurality of limiting blocks 8 can penetrate the sealing member 2 and engage with the inner walls of the plurality of first limiting grooves 7, so as to accurately align and connect the second barrel 3 with the first barrel 1;
[0026] Secondly, an arc-shaped first groove 9 is provided on the side surface of the limit block 8, and a columnar first clamping groove 10 is provided on the inner wall of the first limit groove 7. The inner wall of the first clamping groove 10 is elastically and slidably connected with a block-shaped first clamping block 11 through a spring, and the first clamping block 11 can be engaged with the inner wall of the first groove 9. After the limit block 8 is engaged with the inner wall of the first limit groove 7, the first clamping block 11 is engaged with the inner wall of the first groove 9 under the resetting action of the spring, so as to reinforce the stability of the connection between the second barrel 3 and the first barrel 1 and ensure the circulation of the molten metal.
[0027] Reference Figure 5 An arc-shaped second groove 14 is provided on the outer surface of the second barrel 3, and a columnar second clamping groove 15 is provided on the inner side wall of the insulation ring plate 6. The inner wall of the second clamping groove 15 is elastically slidably connected with a block-shaped second clamping block 16 through a spring, and the second clamping block 16 can be engaged with the inner wall of the second groove 14. When the limiting ring 13 is engaged with the inner wall of the second limiting groove 12, the second clamping block 16 is engaged with the inner wall of the second groove 14 under the resetting action of the spring, so as to stably fix the insulation ring plate 6.
[0028] The implementation principle of a die-casting barrel in an embodiment of the present application is as follows: by setting a heat-insulating ring plate 6, the outer surfaces of the first barrel 1 and the second barrel 3 can be heated so as to keep the molten metal warm, thereby reducing the heat loss of the molten metal during the die-casting process and ensuring the quality of the die-casting. After the device has been used for a period of time, the second clamping block 16 is pressed to make the second clamping block 16 slide out from the inner wall of the second groove 14, and then the heat-insulating ring plate 6 is slid to disassemble it, and then the first clamping block 11 is pressed to make the first clamping block 11 slide out from the inner wall of the first groove 9, and then the second barrel 3 is slid so that the limit block 8 slides out from the inner wall of the first limit groove 7, thereby quickly separating the first barrel 1 from the second barrel 3, so as to clean the inner walls of the first barrel 1 and the second barrel 3, and avoid the worn debris of the inner wall from mixing in the molten metal, resulting in poor quality of the die-casting, and can prevent the device from being blocked, simplifying the maintenance process and improving work efficiency.
[0029] Finally, a few points should be explained: First, in the description of this application, it should be noted that, unless otherwise specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, which may refer to mechanical connection or electrical connection, or internal communication between two components, or direct connection. "upper", "lower", "left", "right", etc. are only used to indicate relative positional relationships. When the absolute position of the object being described changes, the relative positional relationship may change;
[0030] Secondly: In the drawings of the embodiments disclosed in the present utility model, only the structures related to the embodiments disclosed in the present utility model are involved, and other structures can refer to the general design. In the absence of conflict, the same embodiment and different embodiments of the present utility model can be combined with each other;
[0031] Finally: The above description is only a preferred embodiment of the present utility model and is not intended to limit the present utility model. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present utility model should be included in the protection scope of the present utility model.
[0032] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A die-casting barrel, comprising a first barrel (1), Features: The side surface of the first barrel (1) is fixedly connected to a sealing member (2); the side surface of the first barrel (1) is located on the outer side of the sealing member (2) and is snap-connected to a second barrel (3), and the second barrel (3) is tightly attached to the side surface of the sealing member (2); an injection groove (4) is provided on the outer surface of the second barrel (3); a flange joint (5) is fixedly connected to the outer surface of the first barrel (1); and an insulation ring plate (6) is snap-connected to the outer surfaces of the first barrel (1) and the second barrel (3).
2. A die-casting feed barrel according to claim 1, Features: The side surface of the first barrel (1) is provided with a plurality of first limiting grooves (7), and the side surface of the second barrel (3) opposite to the first barrel (1) is fixedly connected with a plurality of limiting blocks (8), and the plurality of limiting blocks (8) can penetrate the sealing member (2) and engage with the inner walls of the plurality of first limiting grooves (7).
3. A die-casting feed barrel according to claim 2, Features: The side surface of the limiting block (8) is provided with a first groove (9), the inner wall of the first limiting groove (7) is provided with a first clamping groove (10), the inner wall of the first clamping groove (10) is elastically slidably connected to a first clamping block (11) via a spring, and the first clamping block (11) can be clamped on the inner wall of the first groove (9).
4. A die-casting feed barrel according to claim 1, Features: The inner wall of the heat-insulating ring plate (6) is provided with a second limiting groove (12), and the outer surface of the first barrel (1) is integrally formed with a limiting ring (13), and the limiting ring (13) can be engaged with the inner wall of the second limiting groove (12).
5. A die-casting feed barrel according to claim 1, Features: The outer surface of the second barrel (3) is provided with a second groove (14), the inner wall of the heat-insulating ring plate (6) is provided with a second clamping groove (15), the inner wall of the second clamping groove (15) is elastically slidably connected to a second clamping block (16) via a spring, and the second clamping block (16) can be engaged with the inner wall of the second groove (14).