Reinforced pier based on sulphoaluminate cement-based repair material

By strengthening the bridge piers based on a combination of sulfoaluminate cement-based repair materials and FRP materials, the problems of long time, poor corrosion resistance and poor bonding ability of the existing bridge pier reinforcement methods are solved, achieving higher compression resistance and Structural safety, suitable for bridge structure repair in harsh environments.

CN221877728UActive Publication Date: 2024-10-22HEBEI SHENGKAI HIGHWAY ENGINEERING CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420446926.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-08
Publication Date
2024-10-22
Estimated Expiration
2034-03-08

AI Technical Summary

Technical Problem

Existing bridge pier reinforcement methods have problems such as long repair time, poor corrosion resistance, high carbon emissions, and poor bonding ability. Especially in harsh environments, the compressive resistance of the bridge pier structure is insufficient, which affects bridge safety.

Method used

The bridge piers are reinforced with repair materials based on sulfoaluminate cement. The first layer of sulfoaluminate cement-based material is sprayed, wrapped with FRP mesh cloth, and the second layer of sulfoaluminate cement-based material is sprayed on the outside and covered with glass fiber. Reinforced resin composite sleeve, combined with fastening straps and stainless steel nail fixation, using epoxy resin sealant and interface agent to improve bonding strength.

Benefits of technology

It significantly improves the anti-seepage, anti-freeze, and anti-compression properties of the bridge pier, extends the service life of the structure, and improves the overall mechanical properties. The reinforcement process is short and time-consuming, and is suitable for bridge emergency repair and reinforcement projects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221877728U_ABST
    Figure CN221877728U_ABST
Patent Text Reader

Abstract

The utility model relates to a reinforcing bridge pier based on sulphoaluminate cement-based repairing materials, which comprises a bridge pier, a first layer of sulphoaluminate cement-based repairing materials is sprayed on the outer surface of the bridge pier, FRP (fiber reinforced plastic) gridding cloth is wound on the outer side of the first layer of sulphoaluminate cement-based repairing materials, and a second layer of sulphoaluminate cement-based repairing materials is wound on the outer side of the FRP gridding cloth. A second layer of sulphoaluminate cement-based repair material is sprayed outside the FRP gridding cloth, and the outer side of the second layer of sulphoaluminate cement-based repair material is sleeved with an FRP sleeve. The FRP material and the sulphoaluminate cement-based material are compounded to reinforce the pier, so that the pier has higher impermeability, frost resistance, corrosion resistance and compression resistance, the service life of the structure is prolonged, the overall mechanical property of the structure is improved, the reinforcing process is short in time consumption, construction is facilitated, and the pier is suitable for bridge repair and reinforcing engineering.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of civil engineering, in particular to a reinforced bridge pier based on sulphoaluminate cement-based repairing material. Background Art

[0002] As the service life of bridge structures increases, the durability of the structures within their design service life becomes more and more prominent. As the most important substructure of bridges, most bridge piers are components that are frequently exposed to rain or water level fluctuations. For cold and severe regions, the environment in which bridge piers are located is mostly a freeze-thaw environment.

[0003] For bridges that have been in operation for a long time, especially those with relatively harsh environments or pier structures with insufficient concrete cover thickness, the pier concrete and internal steel bars are damaged to varying degrees. The rust and expansion of local steel bars may also cause external concrete damage, cracking, and even steel bar exposure. The occurrence of such situations seriously weakens the ability of the pier to resist external loads, and the mechanical properties of the pier will drop sharply, endangering the overall safety of the bridge structure. Therefore, it is urgent to propose reasonable reinforcement measures to improve the overall performance of the pier, especially the compressive performance, so as to ensure the safety of the bridge within the designed service life.

[0004] At present, common methods for reinforcing reinforced concrete piers include increasing the cross-sectional area, pasting reinforcing materials, and painting reinforcing materials, but these methods all have certain limitations. For example, the method of using silicate cement to repair piers has a series of disadvantages such as long repair time, poor corrosion resistance, and high carbon emissions; the method of wrapping the piers with fiber-reinforced polymer materials has problems such as poor bonding with the piers and easy falling off. Utility Model Content

[0005] The utility model aims to solve the deficiencies of the prior art and provides a reinforced bridge pier based on sulphoaluminate cement-based repairing material.

[0006] In order to achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a reinforced bridge pier based on sulphoaluminate cement-based repair material, comprising: a bridge pier, the outer surface of which is sprayed with a first layer of sulphoaluminate cement-based repair material, the outer side of the first layer of sulphoaluminate cement-based repair material is wrapped with FRP mesh cloth, the outer side of the FRP mesh cloth is sprayed with a second layer of sulphoaluminate cement-based repair material, and the outer side of the second layer of sulphoaluminate cement-based repair material is covered with an FRP sleeve.

[0007] Furthermore, a plurality of fastening belts are provided on the outside of the FRP sleeve.

[0008] Furthermore, the FRP sleeve is fixedly connected to the bridge pier via a plurality of stainless steel nails, and the plurality of stainless steel nails are evenly arranged along the vertical direction of the bridge pier.

[0009] Furthermore, epoxy resin sealant is coated between the upper and lower ends of the FRP sleeve and the bridge pier.

[0010] Furthermore, the thickness of the second layer of sulphoaluminate cement-based repair material is greater than the thickness of the FRP mesh cloth.

[0011] Furthermore, the FRP mesh cloth is a basalt fiber reinforced resin composite material mesh cloth.

[0012] Furthermore, the FRP sleeve is a glass fiber reinforced resin composite material sleeve.

[0013] Furthermore, an interface agent is coated between the second layer of sulphoaluminate cement-based repair material and the FRP sleeve, and the interface agent is epoxy resin glue.

[0014] The beneficial effects of the utility model are as follows: the utility model compositely uses FRP material and sulphoaluminate cement-based material to reinforce the bridge pier, has higher anti-seepage performance, anti-freeze performance, corrosion resistance and compressive resistance, extends the service life of the structure, improves the overall mechanical properties of the structure, and the reinforcement process is time-saving and conducive to construction, and is suitable for bridge emergency repair and reinforcement projects. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the structure of the utility model;

[0016] Figure 2 It is a schematic diagram of the internal structure of the utility model;

[0017] Figure 3 It is a cross-sectional view of the utility model;

[0018] In the figure: 1-epoxy resin sealant; 2-bridge pier; 3-first layer of sulphoaluminate cement-based repair material; 4-FRP mesh cloth; 5-second layer of sulphoaluminate cement-based repair material; 6-FRP sleeve; 7-fastening belt; 8-stainless steel nails;

[0019] The drawings in this utility model are all schematic diagrams, and their sizes do not represent actual sizes;

[0020] The following is a detailed description of the embodiments of the present invention with reference to the accompanying drawings. DETAILED DESCRIPTION

[0021] The utility model is further described below in conjunction with the accompanying drawings and embodiments:

[0022] like Figure 1 to Figure 3As shown, a reinforced bridge pier based on sulphoaluminate cement-based repair material comprises: a bridge pier 2, the outer surface of which is sprayed with a first layer of sulphoaluminate cement-based repair material 3, the outer side of the first layer of sulphoaluminate cement-based repair material 3 is wrapped with an FRP mesh cloth 4, the outer side of the FRP mesh cloth 4 is sprayed with a second layer of sulphoaluminate cement-based repair material 5, and the outer side of the second layer of sulphoaluminate cement-based repair material 5 is sleeved with an FRP sleeve 6.

[0023] A plurality of fastening belts 7 are provided on the outer side of the FRP sleeve 6 .

[0024] The FRP sleeve 6 is fixedly connected to the pier 2 by a plurality of stainless steel nails 8, and the plurality of stainless steel nails 8 are evenly arranged along the vertical direction of the pier 2. The length of the stainless steel nails 8 extending below the outer surface of the FRP sleeve 6 is greater than the thickness of the FRP sleeve 6, so that the FRP sleeve 6 and the pier 2 form an integral structure.

[0025] Epoxy resin sealant 1 is coated between the upper and lower ends of the FRP sleeve 6 and the bridge pier 2 to prevent corrosive and harmful substances in the environment from entering the material along the upper and lower ends of the bridge pier reinforcement layer.

[0026] The thickness of the second layer of sulphoaluminate cement-based repair material 5 is greater than the thickness of the FRP mesh cloth 4 .

[0027] The FRP mesh cloth 4 is a basalt fiber reinforced resin composite material mesh cloth, and its longitudinal and transverse tensile strengths are both greater than 1500 MPa.

[0028] The FRP sleeve 6 is a glass fiber reinforced resin composite material sleeve, the wall thickness of which should be no less than 3 mm and the hoop tensile strength of which should be no less than 450 MPa.

[0029] An interface agent is applied between the second layer of sulphoaluminate cement-based repair material 5 and the FRP sleeve 6. The interface agent is epoxy resin glue. The epoxy resin glue is applied to the surface where the second layer of sulphoaluminate cement-based repair material 5 and the FRP sleeve 6 need to be pasted by roller coating. The bonding strength of the epoxy resin glue is greater than 2.0 MPa.

[0030] The construction method of the utility model is as follows: firstly, a first layer of sulphoaluminate cement-based repair material 3 is sprayed on the outer surface of the pier 2, and the FRP mesh cloth 4 is wound around the first layer of sulphoaluminate cement-based repair material 3 before the initial setting, and the second layer of sulphoaluminate cement-based repair material 5 is sprayed immediately after the FRP mesh cloth 4 is wound, and the thickness of the second layer of sulphoaluminate cement-based repair material 5 is greater than the thickness of the FRP mesh cloth 4. The final setting time of the first layer of sulphoaluminate cement-based repair material 3 and the second layer of sulphoaluminate cement-based repair material 5 is less than two hours, which can quickly complete the repair and reduce carbon emissions, and make the pier 2 as a whole have better mechanical properties and durability.

[0031] The utility model is described above by way of example in conjunction with the accompanying drawings. It is obvious that the specific implementation of the utility model is not limited to the above-mentioned method. As long as various improvements are made using the method concept and technical solution of the utility model, or are directly applied to other occasions without improvement, they are all within the protection scope of the utility model.

Claims

1. A reinforced bridge pier based on sulphoaluminate cement-based repair material, characterized in that: include: A bridge pier (2), wherein a first layer of sulphoaluminate cement-based repair material (3) is sprayed on the outer surface of the bridge pier (2), an FRP mesh cloth (4) is wrapped around the outer side of the first layer of sulphoaluminate cement-based repair material (3), a second layer of sulphoaluminate cement-based repair material (5) is sprayed on the outer side of the FRP mesh cloth (4), and an FRP sleeve (6) is sleeved on the outer side of the second layer of sulphoaluminate cement-based repair material (5).

2. A reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 1, characterized in that: A plurality of fastening belts (7) are provided on the outside of the FRP sleeve (6).

3. A reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 2, characterized in that: The FRP sleeve (6) is fixedly connected to the bridge pier (2) via a plurality of stainless steel nails (8), and the plurality of stainless steel nails (8) are evenly arranged along the vertical direction of the bridge pier (2).

4. A reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 3, characterized in that: Epoxy resin sealant (1) is coated between the upper and lower ends of the FRP sleeve (6) and the bridge pier (2).

5. The reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 1, characterized in that: The thickness of the second layer of sulphoaluminate cement-based repair material (5) is greater than the thickness of the FRP mesh cloth (4).

6. The reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 1, characterized in that: The FRP mesh cloth (4) is a basalt fiber reinforced resin composite material mesh cloth.

7. The reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 1, characterized in that: The FRP sleeve (6) is a glass fiber reinforced resin composite material sleeve.

8. The reinforced bridge pier based on sulphoaluminate cement-based repair material according to claim 1, characterized in that: An interface agent is coated between the second layer of sulphoaluminate cement-based repair material (5) and the FRP sleeve (6), and the interface agent is epoxy resin glue.

Citation Information

Cited By

  • Anti-freezing reinforcing pier performance test system

    CN120369470A