Crack corrosion test device for bimetallic composite material
Through the crevice corrosion test device that controls the temperature and humidity in the reaction box, the problem that the existing technology cannot study the impact of temperature and humidity on the corrosion degree of composite metal materials is solved, and the in-depth study of the corrosion mechanism and the reliability of the experimental results are achieved. sex and safety.
Patent Information
- Application Number
- CN202420360007.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-27
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-02-27
AI Technical Summary
The existing technology cannot directly test the effect of temperature or humidity on the corrosion degree of composite metal materials, resulting in the inability to effectively study the mechanism of crevice corrosion.
A crevice corrosion test device for bimetal composite materials is designed. By controlling the temperature and humidity level in the reaction box, and using heating elements, moving mechanisms, humidifying mechanisms and blocking components, the corrosion conditions of metal materials can be finely controlled and controlled. test.
By controlling variables, the relationship between the degree of corrosion and temperature and humidity is obtained, which improves the accuracy and reliability of experimental results, prevents accidental contact of heating elements, and ensures experimental safety and accuracy of results.
Smart Images

Figure CN221883413U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of bimetallic composite materials, in particular to a crevice corrosion test device for bimetallic composite materials. Background Art
[0002] Carbon steel / stainless steel bimetallic composite materials use carbon steel base and stainless steel coating. This composite material has both the corrosion resistance of stainless steel and the high strength and toughness of carbon steel. The production process mainly includes heating process, plastic deformation process and mechanical processing process, which has less pollution to the environment and belongs to green and environmentally friendly production process. At the same time, since the thickness of the stainless steel layer of the composite material is generally 0.2-0.4mm, compared with the integral stainless steel material, the cost of corrosion-resistant materials is greatly reduced, and its comprehensive cost performance is very high.
[0003] However, due to the existence of crevice corrosion, crevice corrosion is prone to occur between metal and metal, metal and non-metal, and almost all media can experience crevice corrosion. Carbon steel / stainless steel bimetallic composites cannot avoid the occurrence of crevice corrosion.
[0004] Under the existing technology, it is impossible to directly test the effect of temperature or humidity on the corrosion degree of composite metal materials. Utility Model Content
[0005] The purpose of the utility model is to address the problems existing in the background technology and to propose a crevice corrosion test device for bimetallic composite materials, which corrodes composite metal materials by controlling the temperature or humidity in a reaction box and obtains the relationship between the corrosion of the composite metal materials and the temperature and humidity by controlling variables.
[0006] The technical solution of the utility model is: a crevice corrosion test device for bimetallic composite materials, comprising:
[0007] A reaction box, wherein a plurality of second vent holes are arranged inside the reaction box;
[0008] A placement plate is slidably disposed in the reaction box and is provided with a plurality of first ventilation holes;
[0009] A moving mechanism is rotatably disposed in the reaction box and is used to drive the placement plate to move;
[0010] A heating element is arranged in the reaction box and below the placement plate;
[0011] A wetting mechanism is arranged in the reaction box;
[0012] The blocking component is rotatably arranged on the reaction box and is engaged with the reaction box in a detachable manner.
[0013] Preferably, the moving mechanism includes a driving motor arranged on the reaction box, a screw connected to the output end of the driving motor and rotatably arranged in the reaction box, and a guide rail arranged in the reaction box; the screw is threadedly connected to the placement plate; and the guide rail is slidably connected to the placement plate.
[0014] Preferably, the wetting mechanism includes a water pump arranged on the reaction box, an input pipe having one end connected to the input end of the water pump, an output pipe having one end connected to the output end of the water pump, and a spray head connected to the other end of the output pipe.
[0015] Preferably, the blocking assembly includes a rotating shaft rotatably arranged on the reaction box, and a blocking door arranged on the rotating shaft; the blocking door is engaged with the reaction box and is detachably connected.
[0016] Preferably, a latch is provided on the blocking door; a latch hole is provided on the reaction box; a plurality of latches and latch holes are provided; the latch is embedded in the latch hole, and the blocking door is snap-connected with the reaction box.
[0017] Preferably, a placement slot is provided on the placement plate; a plurality of placement slots are provided.
[0018] Preferably, a working frame is provided at the lower end of the reaction box.
[0019] Compared with the prior art, the utility model has the following beneficial technical effects:
[0020] In the utility model, the temperature inside the reaction box is maintained within a constant range. After a period of time, the corrosion degree of the material is observed, and then a group of metal materials are re-prepared to test the corrosion degree at another temperature. By controlling the variables, the relationship between the corrosion degree and the temperature can be obtained; by testing the corrosion degrees of multiple groups of metals in different humidity environments, the influence of humidity on metal corrosion can be obtained; the reason for testing multiple groups of metal materials at one time is that multiple materials are tested at the same time and the average value is obtained, so that the experimental results are true and reliable; the heating element is arranged in the reaction box to prevent the staff from accidentally touching the heating element to prevent injuries; when the placement plate is removed from the reaction box, the blocking door can also serve as a support plate for the placement plate to provide support for the placement plate; the reaction box is closed by the blocking door to prevent the external environment from affecting the reaction box, so that the experimental results are accurate. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a structural front view of an embodiment of the utility model;
[0022] Figure 2 It is a structural cross-sectional view of an embodiment of the utility model;
[0023] Figure 3 for Figure 2 A schematic diagram of the local enlarged structure at point A in the middle;
[0024] Figure 4 It is a structural rear view of an embodiment of the present utility model.
[0025] Figure numerals: 1. working frame; 2. moving mechanism; 201. driving motor; 202. screw rod; 203. guide rail; 3. placement plate; 4. first air vent; 5. heating element; 6. second air vent; 7. wetting mechanism; 701. water pump; 702. input pipe; 703. output pipe; 704. sprinkler head; 8. reaction box; 9. rotating shaft; 10. blocking door; 11. latch; 12. latch hole; 13. placement slot. DETAILED DESCRIPTION
[0026] Embodiment 1
[0027] like Figure 1-Figure 4 As shown, the present invention proposes a crevice corrosion test device for a bimetallic composite material, comprising a moving mechanism 2, a placement plate 3, a heating element 5, a wetting mechanism 7, a reaction box 8 and a plugging assembly; a plurality of second vents 6 are arranged inside the reaction box 8; the second vents 6 can protect the heating element 5 without affecting the normal dissipation of the heat, prevent the heating element 5 from being touched and damaged, and avoid contact with the heating element 5 during operation, resulting in accidents such as burns; the placement plate 3 is slidably arranged in the reaction box 8, and a plurality of first vents 4 are arranged on it; the hot air under the placement plate 3 can move to the top of the placement plate 3 through the first vents 4, which can speed up the temperature control in the reaction box 8; the moving mechanism 2 is rotatably arranged in the reaction box 8, and is used to drive the placement plate 3 to move; the heating element 5 is arranged in the reaction box 8, and is located below the placement plate 3; the wetting mechanism 7 is arranged in the reaction box 8; the plugging assembly is rotatably arranged on the reaction box 8, and is engaged with the reaction box 8, and is detachably connected. A placement groove 13 is arranged on the placement plate 3; and a plurality of placement grooves 13 are arranged. A working frame 1 is provided at the lower end of the reaction box 8 .
[0028] In this embodiment, when detecting the crevice corrosion effect of the metal composite material, the reaction box 8 is first opened, and then the moving mechanism 2 is started. The moving mechanism 2 drives the placement plate 3 to move so that the placement plate 3 moves to the outside of the reaction box 8 to facilitate the placement of the metal material. Then, multiple metal materials are placed on the placement groove 13 on the placement plate 3, and then the same amount of corrosive liquid is dripped at the gaps of multiple composite metal materials. After the dripping is completed, the moving mechanism 2 is started, and the moving mechanism 2 moves the placement plate 3 back into the reaction box 8. The reaction box 8 is closed and the preparation work is completed; the effect of temperature on the degree of material corrosion is tested at different temperatures, and the heating element 5 is connected to the power supply. The heating element 5 emits heat, and the heat is transferred to the inside of the reaction box 8 through the first vent 4 and the second vent 6. Then, the temperature inside the reaction box 8 is maintained within a constant range. After a period of time, the corrosion degree of the material is observed. Then, a new group of metal materials is prepared and the corrosion degree at another temperature is tested. By controlling the variables, the relationship between the corrosion degree and the temperature can be obtained. The influence of the wetness on the metal corrosion degree is tested, and the wetting mechanism 7 is started. The wetting mechanism 7 changes the wet environment in the reaction box 8. By testing the corrosion degrees of multiple groups of metals in different wet environments, the influence of the wetness on the metal corrosion can be obtained. The reason for testing multiple groups of metal materials at one time is that multiple materials are tested at the same time and the average value is obtained, so that the experimental results are true and reliable. The heating element 5 is arranged in the reaction box 8 to prevent the staff from accidentally touching the heating element 5 and preventing them from being injured.
[0029] Embodiment 2
[0030] like Figure 1-Figure 4 As shown, the utility model proposes a crevice corrosion test device for a bimetallic composite material. Compared with the first embodiment, the moving mechanism 2 in this embodiment includes a driving motor 201 arranged on the reaction box 8, a screw rod 202 connected to the output end of the driving motor 201 and rotatably arranged in the reaction box 8, and a guide rail 203 arranged in the reaction box 8; the screw rod 202 is threadedly connected to the placement plate 3; the guide rail 203 is slidably connected to the placement plate 3.
[0031] In this embodiment, when placing the composite metal material, the drive motor 201 is started, and the drive motor 201 drives the screw rod 202 to rotate, and the screw rod 202 drives the placement plate 3 to move on the guide rail 203, so that the guide rail 203 is removed from the reaction box 8, making it convenient for the staff to place the composite metal material on the placement plate 3.
[0032] Embodiment 3
[0033] like Figure 1-Figure 4As shown, the utility model proposes a crevice corrosion test device for a bimetallic composite material. Compared with the first or second embodiment, the wetting mechanism 7 in this embodiment includes a water pump 701 arranged on a reaction box 8, an input pipe 702 with one end connected to the input end of the water pump 701, an output pipe 703 with one end connected to the output end of the water pump 701, and a spray head 704 connected to the other end of the output pipe 703.
[0034] In this embodiment, when experimenting with the effect of wetness on metal corrosion, a group of metal materials are first placed on the placement plate 3, then the reaction box 8 is closed, and the water pump 701 is started. The water pump 701 absorbs water through the input pipe 702 and outputs it through the output pipe 703. The water flow is sprayed into the reaction box 8 through the sprinkler head 704. The wet environment in the reaction box 8 is regulated by the wetting mechanism 7, and then the corrosion degree of the metal material is observed. Multiple experiments are carried out to obtain the effect of the wetness on metal corrosion.
[0035] Embodiment 4
[0036] like Figure 1-Figure 4 As shown, the utility model proposes a crevice corrosion test device for a bimetallic composite material. Compared with the first embodiment, the second embodiment or the third embodiment, the sealing assembly in this embodiment includes a rotating shaft 9 rotatably arranged on the reaction box 8, and a sealing door 10 arranged on the rotating shaft 9; the sealing door 10 is clamped with the reaction box 8 and is detachably connected.
[0037] The blocking door 10 is provided with a latch 11 ; the reaction box 8 is provided with a latch hole 12 ; there are multiple latches 11 and latch holes 12 ; the latch 11 is embedded in the latch hole 12 , and the blocking door 10 is engaged with the reaction box 8 .
[0038] In this embodiment, when the reaction box 8 is opened, the latch 11 is pulled out from the latch hole 12 to contact the blocking door 10 and the reaction box 8, and then the blocking door 10 is flipped over so that the blocking door 10 is in contact with the work frame 1. Then, when the placement plate 3 is moved out of the reaction box 8, the blocking door 10 can also serve as a support plate for the placement plate 3 to provide support for the placement plate 3. The reaction box 8 is closed by the blocking door 10 to prevent the external environment from affecting the reaction box 8, thereby ensuring accurate experimental results.
[0039] The implementation modes of the present invention are described in detail above in conjunction with the accompanying drawings, but the present invention is not limited thereto, and various changes can be made within the knowledge scope of technicians in the relevant technical field without departing from the purpose of the present invention.
Claims
1. A crevice corrosion test device for a bimetallic composite material, characterized in that: include: A reaction box (8) having a plurality of second vent holes (6) disposed therein; A placement plate (3) is slidably disposed in the reaction box (8) and is provided with a plurality of first ventilation holes (4); A moving mechanism (2) is rotatably disposed in the reaction box (8) and is used to drive the placement plate (3) to move; A heating element (5) is arranged in the reaction box (8) and is located below the placement plate (3); A wetting mechanism (7) is arranged in a reaction box (8); The blocking component is rotatably arranged on the reaction box (8) and is engaged with the reaction box (8) in a detachable manner.
2. A crevice corrosion test device for a bimetallic composite material according to claim 1, characterized in that: The moving mechanism (2) comprises a driving motor (201) arranged on a reaction box (8), a screw rod (202) connected to the output end of the driving motor (201) and rotatably arranged in the reaction box (8), and a guide rail (203) arranged in the reaction box (8); the screw rod (202) is threadedly connected to the placement plate (3); and the guide rail (203) is slidably connected to the placement plate (3).
3. The crevice corrosion test device of a bimetallic composite material according to claim 1, characterized in that: The wetting mechanism (7) comprises a water pump (701) arranged on the reaction box (8), an input pipe (702) having one end connected to the input end of the water pump (701), an output pipe (703) having one end connected to the output end of the water pump (701), and a spray head (704) connected to the other end of the output pipe (703).
4. The crevice corrosion testing device of a bimetallic composite material according to claim 1, characterized in that: The blocking component comprises a rotating shaft (9) rotatably arranged on a reaction box (8), and a blocking door (10) arranged on the rotating shaft (9); the blocking door (10) is engaged with the reaction box (8) in a detachable manner.
5. The crevice corrosion testing device of a bimetallic composite material according to claim 4, characterized in that: The blocking door (10) is provided with a latch (11); the reaction box (8) is provided with a latch hole (12); a plurality of latches (11) and latch holes (12) are provided; the latch (11) is embedded in the latch hole (12), and the blocking door (10) is engaged with the reaction box (8).
6. The crevice corrosion testing device of a bimetallic composite material according to claim 1, characterized in that: A placement groove (13) is provided on the placement plate (3); a plurality of placement grooves (13) are provided.