Electroplating roughening liquid regeneration system
By using unbalanced electrolysis and filtration devices in the electroplating roughening solution regeneration system, the problem of oxidation of hexavalent chromium into trivalent chromium is solved, the roughening effect and the binding force of the electroplating layer are improved, and environmental pollution is reduced.
Patent Information
- Application Number
- CN202323232969.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2033-11-29
AI Technical Summary
In the plastic electroplating process, the hexavalent chromium in the roughening solution is oxidized into trivalent chromium, which leads to a decrease in oxidation ability and affects the roughening effect and the binding force of the electroplated layer. Moreover, the chromic anhydride and sulfuric acid in the scrap solution are seriously polluted.
A regeneration system for electroplating roughening liquid is designed, including a roughening tank and an electrolysis device. It uses two electrolytic porcelain bladders and detachable electrode sheets to reduce the trivalent chromium content through unbalanced electrolysis, and sets up a filter at the liquid inlet. Device to initially filter metal particle impurities.
It effectively reduces the trivalent chromium content in the roughening liquid, extends the service life of the roughening liquid, avoids environmental pollution, and simplifies the maintenance and replacement process of electrode sheets.
Smart Images

Figure CN221918315U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of electroplating, in particular to an electroplating roughening liquid regeneration system. Background Art
[0002] The plastic electroplating process includes a roughening process, which mainly uses the roughening liquid to etch the plastic surface to form honeycomb-shaped pores on the plastic surface, thereby improving the bonding between the plastic and the electroplated layer generated by the subsequent electroplating process. The roughening liquid mainly includes chromic anhydride acid and sulfuric acid. During the roughening process, the hexavalent chromic acid in the roughening liquid reacts with the product to produce trivalent chromium and organic matter. During the roughening process, hexavalent chromium will become trivalent chromium. As the content of trivalent chromium increases, the oxidation ability of the roughening liquid will be weakened, resulting in a decrease in the roughening effect. Due to poor roughening, the bonding strength between the plastic workpiece and the electroplated layer will also be significantly reduced. When the concentration of trivalent chromium rises to 30g / L, it will seriously affect the roughening quality and cause the roughening liquid to be scrapped. The waste roughening liquid contains a large amount of chromic anhydride and sulfuric acid, which will seriously pollute the environment if directly discharged. Utility Model Content
[0003] The utility model provides an electroplating roughening liquid regeneration system for solving the technical problems raised in the background technology.
[0004] The technical solution adopted by the utility model to solve the above technical problems is:
[0005] The electroplating roughening liquid regeneration system is characterized by comprising:
[0006] A roughening tank, wherein the roughening tank has a receiving cavity in the middle, and at least two electrolytic porcelain tanks are arranged in the receiving cavity, the electrolytic porcelain tank contains electrolyte, the receiving cavity contains roughening liquid, and the liquid level of the roughening liquid is lower than the top surface of the electrolytic porcelain tank; the top of one side wall of the roughening tank is a liquid inlet, the liquid inlet is a detachable structure and a filtering device is arranged inside, the bottom of the roughening tank is a liquid outlet, and the roughening liquid flows from the liquid inlet to the liquid outlet;
[0007] The electrolysis device comprises an electrolysis anode, an electrolysis cathode and a connector; the connector is divided into an anode connector and a cathode connector, both of which are arranged on the top of the accommodating cavity; the electrolysis anode is electrically connected to the positive electrode of the power supply, one end of which is fixed on the anode connector, and the other end of which extends into the accommodating cavity and is immersed in the roughening liquid; the electrolysis cathode is connected to the negative electrode of the power supply, one end of which is fixed on the cathode connector, and the other end of which extends into the electrolytic porcelain tank and is immersed in the electrolyte.
[0008] As a further preferred embodiment of the present invention, the anode connector and the cathode connector are made of copper, are transversely arranged at the opening of the accommodating cavity, and are fixed to the roughening tank at both ends.
[0009] As a further preferred embodiment of the present invention, there are n electrolytic cathodes, the tops of which are bent to one side to form a hooking portion, and the hooking portion is hooked on the cathode connector; wherein n≥2.
[0010] As a further preferred embodiment of the present invention, the number of the electrolytic anodes is n+1, and the tops are bent to one side to form a hooking portion, and the hooking portion is hooked to the anode connector; wherein n≥2.
[0011] As a further preferred embodiment of the present invention, an electrolysis cathode is disposed between two adjacent electrolysis anodes.
[0012] As a further preferred embodiment of the present invention, the thickness of the electrolysis anode and the electrolysis cathode is 3 to 6 mm.
[0013] As a further preferred embodiment of the present invention, the liquid inlet is an inverted right triangle structure with an opening at the top, the vertical surface of which is a connecting surface connected to the side wall of the roughening tank, and the inclined surface of which is a liquid outlet surface.
[0014] As a further preferred embodiment of the present invention, a filter screen is provided on the liquid outlet surface.
[0015] As a further preferred embodiment of the present invention, a hanging portion protruding upward is provided on the side wall of the roughening tank, a hanging interface is provided at a corresponding position of the connecting surface, and the liquid inlet is connected to the roughening tank by hanging.
[0016] As a further preference of the utility model, a roughening tank is further included, wherein the liquid outlet at the bottom of the roughening tank is connected to the roughening tank via a first pipeline, and the liquid outlet at the bottom of the roughening tank is connected to the roughening tank via a second pipeline, and a one-way circulation pump is provided on the second pipeline.
[0017] Compared with the prior art, the utility model has the following advantages or technical effects:
[0018] 1. Two porcelain tanks are set in the roughening pool. The porcelain tanks contain electrolyte and are provided with electrolytic cathodes, forming two independent cathode chambers. This avoids the problem that the anode and cathode in the traditional electrolytic regeneration tank are openly placed in the same space, resulting in a small local anode and cathode area and poor electrolysis efficiency. 2. An electrolytic cathode is set in each porcelain tank, and electrolytic anodes are set on both sides of the outside of the porcelain tank. During the electrolysis process, the actual effective area of the cathode is smaller than the actual effective area of the anode, thereby performing unbalanced electrolysis on the roughening liquid to greatly reduce the content of trivalent chromium in the roughening liquid to be electrolyzed. 3. Both the electrolytic anode and the electrolytic cathode are fixed to the connector in a hooking manner. This method is a detachable structure, which is convenient for repairing or replacing scrapped or aged electrode sheets. 4. The liquid inlet is designed as an inverted right triangle, and the liquid outlet surface is an inclined surface to form a buffer zone to prevent the coarsening liquid from splashing to the outside. The liquid inlet is a detachable structure with a filter screen inside to perform preliminary filtration on the coarsening liquid to remove most of the metal particle impurities in the liquid to avoid reaction with the electrode sheet during the electrolysis process to affect the electrolysis effect. The detachable structure is convenient for operators to clean the liquid inlet. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The present invention and its features, appearance and advantages will become more apparent by reading the detailed description of non-limiting embodiments with reference to the following drawings. The same reference numerals indicate the same parts in all the drawings. The drawings are not drawn to scale, but the emphasis is on illustrating the subject matter of the present invention.
[0020] Figure 1 It is a structural schematic diagram of the electroplating roughening solution regeneration system;
[0021] Figure 2 is a schematic diagram of the structure of the electrolytic cathode;
[0022] Figure 3 is a schematic diagram of the structure of the electrolytic anode;
[0023] Figure 4 It is a schematic diagram of the connection between the electrode sheet and the connecting piece;
[0024] Figure 5 It is an enlarged schematic diagram of the connection between the liquid inlet and the roughening tank;
[0025] In the figure, 1, roughening tank, 11, accommodating chamber, 12, electrolytic porcelain tank, 13, liquid inlet, 131, connecting surface, 132, liquid outlet, 133, filter screen, 134, hanging interface, 135, hanging part, 14, liquid outlet, 2, electrolytic anode, 21, hooking part (anode) 3, electrolytic cathode, 31, hooking part (cathode), 41, anode connector, 42, cathode connector, 5, roughening tank, 6, first pipeline, 7, second pipeline, 8, one-way circulation pump. DETAILED DESCRIPTION
[0026] The technical solutions in the embodiments of the present invention are described below in conjunction with the drawings in the embodiments of the present invention. It is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the utility model claimed for protection, but merely represents the selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative work belong to the protection scope of the present invention. Example
[0027] Please refer to the attached Figure 1 The utility model provides a regeneration system for electroplating roughening liquid, including a roughening tank 1 and an electrolytic device. The roughening tank 1 has a receiving chamber 11 in the middle, and two electrolytic porcelain gallbladders 12 are arranged in the receiving chamber 11. The electrolytic porcelain gallbladders 12 contain electrolyte, and the receiving chamber 11 contains roughening liquid, and the liquid level of the roughening liquid is lower than the top surface of the electrolytic porcelain gallbladders 12; the top of one side wall of the roughening tank 1 is a liquid inlet 13, and the liquid inlet 13 is a detachable structure and a filtering device is arranged inside. The bottom of the roughening tank 1 is a liquid outlet 14, and the roughening liquid flows from the liquid inlet 13 to the liquid outlet 14. The electrolysis device includes an electrolytic anode 2, an electrolytic cathode 3 and a connector. The connector is divided into an anode connector 41 and a cathode connector 42, both of which are arranged on the top of the accommodating chamber 11. The electrolytic anode 2 is electrically connected to the positive electrode of the power supply, one end of which is fixed on the anode connector 41, and the other end of which extends into the accommodating chamber 11 and is immersed in the roughening liquid. The electrolytic cathode 3 is connected to the negative electrode of the power supply, one end of which is fixed on the cathode connector 42, and the other end of which extends into the electrolytic porcelain tank 12 and is immersed in the electrolyte.
[0028] Further explanation, the anode connector 41 and the cathode connector 42 are made of copper, are horizontally arranged at the opening of the accommodating cavity 11, and are fixed to the roughening tank 1 at both ends. Among them, the anode connector 41 is electrically connected to the positive pole of the power supply, and the cathode connector 42 is electrically connected to the negative pole of the power supply.
[0029] Further explanation, there are two electrolytic cathodes 3, each of which is provided with an electrolytic cathode 3 in the two electrolytic porcelain vessels 12, and three electrolytic anodes 2 are provided. Figure 1 As shown, an electrolytic cathode 3 is provided between two adjacent electrolytic anodes 2. Since the cathode performs a reduction reaction and the anode performs an oxidation reaction, and the water permeability of the porcelain chamber is poor, the electrolytic efficiency of the cathode in the porcelain chamber is poor. Anodes are provided on both sides of the porcelain chamber, so that during the electrolysis process, the actual effective area of the cathode is smaller than the actual effective area of the anode, thereby performing unbalanced electrolysis on the roughening solution to greatly reduce the content of trivalent chromium in the roughening solution to be electrolyzed.
[0030] like Figure 2-Figure 4 As shown, the top of the electrolytic cathode 3 is bent to one side to form a hooking portion 31, and the hooking portion 31 is hooked on the cathode connector 42. Similarly, the top of the electrolytic anode 2 is bent to one side to form a hooking portion 21, and the hooking portion 21 is hooked on the anode connector 41. This method is a detachable structure, which is convenient for repairing or replacing scrapped or aged electrode sheets. It is also possible to move the electrode sheets or increase or decrease the number of electrode sheets before the experiment starts according to actual conditions. The thickness of the electrolytic anode 2 and the electrolytic cathode 3 is 6mm, which has a certain thickness and can prevent the electrode sheets from being deformed or damaged during the hooking process.
[0031] like Figure 5 As shown, the liquid inlet 13 is an inverted right triangle structure with an opening at the top, the vertical surface of which is a connecting surface 131, and the inclined surface is a liquid outlet surface 132. An upwardly protruding hanging portion 135 is provided on the side wall of the roughening tank 1, and a hanging port 134 is provided at the corresponding position of the connecting surface 131. The liquid inlet 13 is connected to the roughening tank 1 by hanging. The liquid outlet surface 132 is an inclined surface to form a buffer zone to prevent the roughening liquid from splashing to the outside. A filter screen 133 is attached to the liquid outlet surface 132, which can perform preliminary filtration on the roughening liquid to remove most of the metal particle impurities in the liquid to avoid reactions with the electrode sheet during the electrolysis process that affect the electrolysis effect. The detachable structure of the liquid inlet 13 is convenient for the operator to clean it.
[0032] like Figure 1 As shown, a roughening tank 5 is also provided to form a plating roughening liquid circulation system. Specifically, the liquid outlet 14 at the bottom of the roughening tank 1 is connected to the roughening tank 5 via a first pipeline 6, and the liquid outlet at the bottom of the roughening tank 5 is connected to the roughening tank 1 via a second pipeline 7. A one-way circulation pump 8 is provided on the second pipeline 7 to prevent the roughening liquid from flowing back.
[0033] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structural transformation made using the contents of the specification and drawings of the present invention, or directly or indirectly applied in other related technical fields, is also included in the patent protection scope of the present invention.
Claims
1. Electroplating roughening solution regeneration system, It is characterized in that include: A roughening tank (1), wherein the roughening tank (1) has a receiving chamber (11) in the middle, wherein at least two electrolytic porcelain vessels (12) are arranged in the receiving chamber (11), wherein the electrolytic porcelain vessel (12) contains electrolyte, and wherein the receiving chamber (11) contains roughening liquid, wherein the liquid level of the roughening liquid is lower than the top surface of the electrolytic porcelain vessel (12); wherein the top of one side wall of the roughening tank (1) is a liquid inlet (13), wherein the liquid inlet (13) is a detachable structure and a filtering device is arranged inside; and wherein the bottom of the roughening tank (1) is a liquid outlet (14), wherein the roughening liquid flows from the liquid inlet (13) to the liquid outlet (14); An electrolysis device comprises an electrolysis anode (2), an electrolysis cathode (3) and a connector; the connector is divided into an anode connector (41) and a cathode connector (42), both of which are arranged on the top of the accommodating chamber (11); the electrolysis anode (2) is electrically connected to the positive electrode of a power supply, one end of which is fixed to the anode connector (41), and the other end of which extends into the accommodating chamber (11) and is immersed in a roughening solution; the electrolysis cathode (3) is connected to the negative electrode of the power supply, one end of which is fixed to the cathode connector (42), and the other end of which extends into the electrolytic porcelain tank (12) and is immersed in the electrolyte.
2. The electroplating roughening solution regeneration system according to claim 1, It is characterized in that The anode connector (41) and the cathode connector (42) are made of copper and are arranged transversely at the opening of the accommodating cavity (11), with both ends being fixed to the roughening tank (1).
3. The electroplating roughening solution regeneration system according to claim 2, It is characterized in that The electrolytic cathodes (3) are provided in n numbers, the tops of which are bent to one side to form a hooking portion, and the hooking portion is hooked onto the cathode connecting piece (42); wherein n≥2.
4. The electroplating roughening solution regeneration system according to claim 3, It is characterized in that The electrolysis anodes (2) are provided with n+1 pieces, the tops of which are bent to one side to form a hooking portion, and the hooking portion is hooked onto the anode connector (41); wherein n≥2.
5. The electroplating roughening solution regeneration system according to claim 4, It is characterized in that An electrolysis cathode (3) is arranged between two adjacent electrolysis anodes (2).
6. The electroplating roughening solution regeneration system according to claim 5, It is characterized in that The thickness of the electrolysis anode (2) and the electrolysis cathode (3) is 3 to 6 mm.
7. The electroplating roughening solution regeneration system according to claim 1, It is characterized in that The liquid inlet (13) is an inverted right triangle structure with an opening at the top, its vertical surface is a connecting surface (131) connected to the side wall of the roughening tank (1), and its inclined surface is a liquid outlet surface (132).
8. The electroplating roughening solution regeneration system according to claim 7, It is characterized in that A filter screen (133) is provided on the liquid outlet surface (132).
9. The electroplating roughening solution regeneration system according to claim 8, It is characterized in that An upwardly protruding hanging portion (135) is provided on the side wall of the roughening tank (1), a hanging port (134) is provided at a corresponding position of the connecting surface (131), and the liquid inlet (13) is connected to the roughening tank (1) by hanging.
10. The electroplating roughening solution regeneration system according to any one of claims 1 to 9, It is characterized in that It also comprises a roughening tank (5), wherein a liquid outlet (14) at the bottom of the roughening tank (1) is connected to the roughening tank (5) via a first pipeline (6), and a liquid outlet at the bottom of the roughening tank (5) is connected to the roughening tank (1) via a second pipeline (7), wherein a one-way circulation pump (8) is provided on the second pipeline (7).