Ceramic copper-clad substrate structure convenient for peel strength detection

By using laser cutting and fixing the copper sheet structure on the ceramic copper-clad substrate, peeling strength testing is directly performed, which solves the problems of low efficiency and inaccurate testing of traditional methods, and achieves more efficient and accurate testing results.

CN221926079UActive Publication Date: 2024-10-29JIANGSU HANSIRUI SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420194999.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-26
Publication Date
2024-10-29
Estimated Expiration
2034-01-26

AI Technical Summary

Technical Problem

The traditional peel strength testing method of ceramic copper-clad substrates is inefficient, the bonding quality affects the test results, and the milling process can easily damage the ceramic and joint surfaces, resulting in inaccurate test results.

Method used

It adopts a structure including a ceramic sheet, a fixing copper sheet and a detection copper sheet. The 90° peeling test is performed directly after being cut by a laser cutting machine, eliminating the bonding and milling steps. The fixing copper sheet is used to fix the detection copper sheet. Peel strength testing.

Benefits of technology

It improves detection efficiency and accuracy, reduces costs, avoids interference of bonding quality on test results, and reduces damage to ceramics and bonding layers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221926079U_ABST
    Figure CN221926079U_ABST
Patent Text Reader

Abstract

The utility model discloses a ceramic copper-clad substrate structure convenient for peel strength detection. The ceramic copper-clad substrate structure comprises a ceramic sheet, a copper sheet for fixation and a copper sheet for detection, a U-shaped copper sheet for fixing is arranged on the front surface of the ceramic chip along the length direction of the ceramic chip, and the opening end of the copper sheet for fixing is arranged rightwards along the length direction of the ceramic chip; a detection copper sheet is arranged on the front surface of the ceramic sheet relative to the interior of the fixing copper sheet along the length direction, and the right end of the detection copper sheet extends out of the opening end side of the fixing copper sheet to form a short end for detection; a laser cutting machine is used for cutting the front side and the back side of the ceramic wafer relative to the short end part, after the short end part is separated from the ceramic wafer, the short end part is bent upwards by 90 degrees towards the inner side direction through a standard 90-degree peeling testing machine, and then the peeling strength of the ceramic wafer can be detected by vertically lifting the short end part. And in the process, a copper sheet for fixing is used for fixing. According to the utility model, the interference of bonding quality on the accuracy of a test result is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of ceramic copper-clad substrates, in particular to a ceramic copper-clad substrate structure which is convenient for detecting peeling strength. Background Art

[0002] With the continuous advancement of electronic technology, in the packaging application of power electronic components, the heat dissipation substrate not only undertakes the functions of electrical connection and mechanical support, but also is an important channel for heat transmission. Ceramic substrate is a commonly used material in power modules. It has special thermal, mechanical and electrical properties and is an ideal choice for demanding power electronic applications. Currently, common types of ceramic substrates include HTCC, LTCC, TFC, DBC, DBA, DPC, etc.

[0003] In practical applications, the failure form of ceramic substrates is related to many factors such as substrate material, interface strength, residual stress in the manufacturing process, process defects, and the load borne. The normal stress perpendicular to the ceramic substrate interface is usually defined as peeling stress, and the surface force acting on the ceramic substrate interface is defined as shear force. The corresponding strengths are called peeling strength and shear strength, respectively, which are used as parameters to evaluate the strength of ceramic substrates.

[0004] For ceramic copper-clad substrates, the industry often uses peel strength as the evaluation standard for its production quality. Specifically, under the test conditions of an ambient temperature of 25°C and an ambient humidity of 65%, the ceramic copper-clad substrate samples are subjected to peel tests, the sample width is 5mm, and the displacement application rate is 50mm / min. The traditional test method in the industry is: the test sample needs to be bonded to the iron plate with an adhesive, and then the metal bottom pattern is milled with a blade, and finally the milled metal pattern is clamped with a chuck for a 90° peel test. However, if the above test method is used, each batch of samples needs to be repeatedly bonded multiple times, resulting in low efficiency. At the same time, the quality of bonding will greatly affect the test results of the peel strength. In the process of milling the metal bottom pattern, it is also easy to cause damage to the ceramic and the joint surface, thereby affecting the test results. Therefore, the above problems need to be solved urgently. Summary of the invention

[0005] The technical problem to be solved by the utility model is to provide a ceramic copper-clad substrate structure which is convenient for testing peel strength, thereby eliminating the step of separately bonding each sample to an iron plate with an adhesive during traditional testing of peel strength of ceramic copper-clad substrates. The structure of the utility model can be directly cut by a laser cutting machine before testing, thereby avoiding interference of bonding quality on the accuracy of test results, saving time and effort, reducing test costs, and improving test efficiency and test accuracy.

[0006] In order to solve the above technical problems, the utility model adopts the following technical solutions: the utility model is a ceramic copper-clad substrate structure that is convenient for detecting peeling strength, and its innovation lies in: comprising a ceramic sheet, a fixing copper sheet and a detecting copper sheet; a fixing copper sheet is arranged in the middle position of the front side of the horizontally arranged ceramic sheet along its length direction, the fixing copper sheet is U-shaped, and its open end is arranged horizontally to the right along the length direction of the ceramic sheet; a rectangular detecting copper sheet matching with the fixing copper sheet is also arranged in the opening groove on the front side of the ceramic sheet relative to the fixing copper sheet along its length direction. The detection copper sheet and the fixing copper sheet are arranged at equal intervals, and the right end thereof extends horizontally and vertically out of the open end side of the fixing copper sheet, thereby forming a short end for detection; the front and back sides of the ceramic sheet are cut relative to the short end of the detection copper sheet by a laser cutting machine, and after the short end is separated from the ceramic sheet, the short end is bent vertically upward 90° along the cutting line inwardly by a standard 90° peeling tester, and the peeling strength test can be carried out by vertically pulling the short end, and it is fixed by the fixing copper sheet in the process.

[0007] Preferably, the fixing copper sheet and the detecting copper sheet are both formed synchronously by sequentially undergoing film lamination, exposure, development, etching solution immersion and film stripping.

[0008] Preferably, the ceramic sheet is made of alumina ceramic, and has a thickness of 0.38 mm and a size of 138*190 mm.

[0009] Preferably, the copper layer thickness of the fixing copper sheet is 0.3 mm, and the width of both side edges of the fixing copper sheet is 9 mm.

[0010] Preferably, the copper layer of the detection copper sheet has a thickness of 0.3 mm and a width of 5 mm.

[0011] Preferably, the distance between the portion of the testing copper sheet located inside the fixing copper sheet and the fixing copper sheet is consistent, so that during the peel strength test of the testing copper sheet, the fixing copper sheet is used to fix it.

[0012] Preferably, the short end of the copper sheet for testing needs to be long enough to ensure that after being bent 90°, it can be directly clamped by the chuck of a standard 90° peel tester for peel strength testing.

[0013] Preferably, the vertical pulling speed is 50 mm / min, and the peeling length must be ensured to be no less than 75 mm.

[0014] Beneficial effects of the utility model:

[0015] (1) The utility model eliminates the need to use adhesive to bond each sample to an iron plate during the traditional ceramic copper-clad substrate peel strength test. The test can be directly performed after the structure of the utility model is cut by a laser cutting machine, thereby avoiding the interference of the bonding quality on the accuracy of the test results, saving time and effort, reducing the test cost, and improving the test efficiency and test accuracy.

[0016] (2) The utility model eliminates the need to mill the metal pattern at the bottom of the traditional ceramic copper-clad substrate during peel strength testing, thereby avoiding possible damage to the ceramic and bonding layer, greatly saving time and improving test accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0018] Figure 1 The utility model is a structural schematic diagram of a ceramic copper-clad substrate structure that is convenient for testing peel strength.

[0019] Figure 2 It is a schematic diagram of the bending state of the copper sheet for detection of the utility model.

[0020] Among them, 1-ceramic sheet; 2-copper sheet for fixing; 3-copper sheet for detection. DETAILED DESCRIPTION

[0021] The technical solution of the utility model will be clearly and completely described below through specific implementation methods.

[0022] The utility model discloses a ceramic copper-clad substrate structure which is convenient for testing peel strength, comprising a ceramic sheet 1, a fixing copper sheet 2 and a testing copper sheet 3; the specific structure is as follows Figure 1 , Figure 2 As shown, the ceramic sheet 1 is made of alumina ceramic, and its thickness is 0.38mm, and its size is 138*190mm; a fixing copper sheet 2 is provided in the middle position of the front side of the horizontally arranged ceramic sheet 1 along its length direction, and the fixing copper sheet 2 is U-shaped, and its open end is arranged horizontally to the right along the length direction of the ceramic sheet 1; wherein, the copper layer thickness of the fixing copper sheet 2 is 0.3mm, and the width of both side edges of the fixing copper sheet 2 is 9mm.

[0023] The utility model also provides a rectangular copper sheet 3 for detection that matches the ceramic sheet 1 in the opening groove of the fixing copper sheet 2 along its length direction. Figure 1, Figure 2 As shown, the detection copper sheet 3 and the fixing copper sheet 2 are arranged at equal intervals, and the right end thereof extends horizontally and vertically out of the open end side of the fixing copper sheet 2, thereby forming a short end for detection; wherein, the fixing copper sheet 2 and the detection copper sheet 3 are both formed synchronously after film pasting, exposure, development, etching solution immersion and film stripping.

[0024] like Figure 1 , Figure 2 As shown, the copper layer thickness of the detection copper sheet 3 is 0.3 mm, and its width is 5 mm; the portion of the detection copper sheet 3 located inside the fixing copper sheet 2 is consistent with the spacing between the fixing copper sheet 2, and thus during the peel strength test of the detection copper sheet 3, it is fixed by the fixing copper sheet 2.

[0025] The utility model uses a laser cutting machine to cut the front and back sides of the ceramic sheet 1 relative to the short end portion of the detection copper sheet 3. After the short end portion is separated from the ceramic sheet 1, the short end portion is bent vertically upward 90° along the cutting line inwardly through a standard 90° peeling tester, and the peeling strength test can be carried out by vertically pulling the short end portion, and the copper sheet 2 is used to fix it in the process; wherein, the vertical pulling speed is 50mm / min, and the peeling length must be ensured to be not less than 75mm; the length of the short end of the detection copper sheet 3 of the utility model must ensure that after it is bent 90°, it is convenient to be directly clamped by the chuck of the standard 90° peeling tester for peeling strength test.

[0026] When testing the peel strength of the utility model, the short end of the copper sheet 3 for testing is first directly clamped by the chuck of a standard 90° peel tester, and then vertically pulled at a speed of 50 mm / min, and the maximum and minimum values ​​of the peel force within a peel length of at least 75 mm are recorded, and the corresponding peel strength is calculated.

[0027] Beneficial effects of the utility model:

[0028] (1) The utility model eliminates the need to use adhesive to bond each sample to an iron plate during the traditional ceramic copper-clad substrate peel strength test. The test can be directly performed after the structure of the utility model is cut by a laser cutting machine, thereby avoiding the interference of the bonding quality on the accuracy of the test results, saving time and effort, reducing the test cost, and improving the test efficiency and test accuracy.

[0029] (2) The utility model eliminates the need to mill the metal pattern at the bottom of the traditional ceramic copper-clad substrate during peel strength testing, thereby avoiding possible damage to the ceramic and bonding layer, greatly saving time and improving test accuracy.

[0030] The embodiments described above are merely descriptions of preferred implementation modes of the present invention, and are not intended to limit the concept and scope of the present invention. Without departing from the design concept of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary engineering and technical personnel in the field should fall within the protection scope of the present invention. The technical contents for which protection is sought in the present invention have been fully recorded in the technical requirements.

Claims

1. A ceramic copper-clad substrate structure that is convenient for testing peel strength, characterized in that: It includes a ceramic sheet, a fixing copper sheet and a detection copper sheet; a fixing copper sheet is provided in the middle position of the front side of the horizontally arranged ceramic sheet along its length direction, the fixing copper sheet is U-shaped, and its open end is arranged horizontally to the right along the length direction of the ceramic sheet; a matching rectangular detection copper sheet is also provided in the opening groove on the front side of the ceramic sheet relative to the fixing copper sheet along its length direction, the detection copper sheet and the fixing copper sheet are arranged at equal intervals, and the right end thereof extends horizontally and vertically out of the open end side of the fixing copper sheet to form a short end for detection; a laser cutting machine is used to cut the front and back sides of the ceramic sheet relative to the short end of the detection copper sheet, and after the short end is separated from the ceramic sheet, a standard 90° peeling tester is used to bend the short end vertically upward 90° along the cutting line toward the inside, and the short end can be vertically pulled up to test its peeling strength, and in the process it is fixed by the fixing copper sheet.

2. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The fixing copper sheet and the detection copper sheet are both formed synchronously after film lamination, exposure, development, etching solution immersion and film stripping.

3. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The ceramic sheet is made of alumina ceramic, has a thickness of 0.38 mm, and has a size of 138*190 mm.

4. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The copper layer thickness of the fixing copper sheet is 0.3 mm, and the width of both sides of the fixing copper sheet is 9 mm.

5. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The copper layer thickness of the detection copper sheet is 0.3 mm, and the width is 5 mm.

6. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The distance between the portion of the testing copper sheet located inside the fixing copper sheet and the fixing copper sheet is consistent, so that during the peeling strength test of the testing copper sheet, the fixing copper sheet is used to fix it.

7. A ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The length of the short end of the copper sheet for testing needs to ensure that after being bent 90°, it can be directly clamped by the chuck of a standard 90° peel tester for peel strength testing.

8. The ceramic copper-clad substrate structure that is convenient for testing peel strength according to claim 1, characterized in that: The vertical pulling speed is 50mm / min, and the peeling length must be ensured to be no less than 75mm.