Cathode material melting furnace method coating equipment
By connecting equipment such as solution barrels and mixers, and improving the stirring mechanism, the problems of continuous automation and uniform absorption of the negative electrode material furnace method coating equipment are solved, and the coating quality and automation level are improved.
Patent Information
- Application Number
- CN202420292942.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-18
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-02-18
AI Technical Summary
The existing anode material furnace method coating equipment cannot achieve continuous automated processing, and the coating agent solution cannot quickly move down to the lower part of the mixer, resulting in uneven absorption of the anode material.
By connecting the solution barrel, mixer, high-temperature kettle and cooling kettle to the delivery pump, the mixing mechanism of the mixer is improved, and the hollow stirring shaft and stirring paddle, liquid suction pipe and discharge pipe are used, combined with the floating unit and the piston unit, to realize the package Full contact and even distribution of coating solution.
It achieves continuous automatic coating of negative electrode materials, improves the uniformity of contact between the coating agent and the negative electrode material and the coating quality, and improves the degree of automation.
Smart Images

Figure CN221928135U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of negative electrode material processing, in particular to a negative electrode material melting furnace coating device. Background Art
[0002] The negative electrode material melting furnace coating is commonly used in the preparation process of negative electrode materials for lithium-ion batteries. This method improves the performance and stability of the battery by forming a protective coating layer on the surface of the negative electrode material.
[0003] The specific steps of furnace cladding are as follows:
[0004] Prepare negative electrode materials: Prepare the negative electrode materials. Commonly used negative electrode materials include graphite, silicon, etc.
[0005] Pretreatment: The negative electrode material needs to undergo some pretreatment steps before being put into the furnace, such as grinding, screening, etc., to obtain a uniform particle size.
[0006] Preparation of coating agent solution: Prepare a coating agent solution of a certain concentration. The coating agent is usually a polymer or carbon material that can form a stable coating layer at high temperature.
[0007] Coating agent coating: Soak the negative electrode material in the coating agent solution to allow it to fully absorb the coating agent. Then, put the soaked negative electrode material into the furnace.
[0008] Furnace treatment: The furnace is heated to a certain temperature, usually the pyrolysis temperature of the coating agent. At high temperature, the coating agent begins to decompose, producing a carbide or graphitized protective layer covering the surface of the negative electrode material.
[0009] Cooling and collection: Cool the materials in the furnace to room temperature, and then collect the coated negative electrode materials.
[0010] The furnace coating method can improve the conductivity, structural stability and durability of the negative electrode material, and increase the cycle life and energy density of the battery. This method is widely used in the preparation of energy storage devices such as lithium-ion batteries.
[0011] However, the existing equipment used for coating negative electrode materials by furnace method has the following technical problems:
[0012] 1. The existing coating equipment cannot carry out continuous processing and production, and the degree of automation is low;
[0013] 2. After the powdered negative electrode material is loaded into the mixer, when the coating agent solution is input, the coating agent solution cannot be quickly transferred from the upper part to the lower part of the mixer, resulting in the negative electrode material being unable to fully and evenly absorb the coating agent, resulting in problems such as slow absorption speed. Utility Model Content
[0014] In view of the above problems, the utility model provides a negative electrode material furnace coating equipment, which realizes continuous and automatic coating furnace preparation of negative electrode materials by connecting the solution barrel, mixer, high-temperature kettle and cooling kettle with a delivery pump through pipelines, and by improving the mixer, the coating agent can be fully in contact with the negative electrode material, so that the negative electrode material can completely absorb the coating agent, thereby improving the coating quality of the negative electrode material by the coating agent.
[0015] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0016] A negative electrode material melting furnace coating device, comprising:
[0017] Solution tank, mixer, high temperature kettle and cooling kettle;
[0018] The solution barrel is used to carry the coating agent solution;
[0019] The feed port at the top of the mixer is connected to the solution barrel through a pipeline, and the negative electrode material is input into the mixer through the feed port;
[0020] The input port at the top of the high-temperature kettle is connected to the discharge port at the bottom of the mixer, and the high-temperature kettle is heated to decompose the coating agent solution;
[0021] The cooling kettle is installed below the high-temperature kettle. The feed inlet at the top of the cooling kettle is connected to the output port at the bottom of the high-temperature kettle, and a discharge port is provided at the bottom of the cooling kettle.
[0022] As an improvement, an expansion joint is provided on the connecting pipe between the high-temperature kettle and the cooling kettle.
[0023] As an improvement, the top of the high-temperature kettle is connected to a tail gas processor, which processes the waste gas discharged from the high-temperature kettle.
[0024] As an improvement, the mixer is provided with a stirring mechanism, which includes a stirring driver, a stirring shaft, a stirring paddle, a floating unit and a piston unit;
[0025] The stirring driver is arranged on the top of the mixer, and the stirring driver drives the stirring mechanism to operate;
[0026] The stirring shaft is vertically rotatably installed in the mixing chamber of the mixer, and the interior of the stirring shaft is hollow;
[0027] The stirring paddles are arranged in a circular array around the stirring shaft, the stirring paddles are connected to the stirring shaft, and the interior of the stirring paddles is hollow and connected to the cavity of the stirring shaft, the stirring paddles include a liquid suction pipe and a liquid discharge pipe, the liquid suction pipe is located at the top of the stirring paddles, the liquid discharge pipe is located below the liquid suction pipe, and a liquid discharge hole is opened on the side wall of the liquid discharge pipe, and a one-way valve is provided in the liquid suction pipe and the cavity of the stirring shaft;
[0028] The floating unit is arranged at the liquid inlet of the liquid pumping tube, and the floating unit controls the liquid inlet switch;
[0029] The piston unit is arranged on the top of the stirring shaft. When the piston unit is in operation, the coating agent solution is extracted through the liquid extraction pipe and discharged from the liquid discharge pipe.
[0030] As an improvement, the floating unit includes a floating head and a floating ball;
[0031] The floating head is slidably mounted at the liquid inlet, a plurality of liquid inlet holes are provided on the side wall of the floating head, and a limit plate is provided at the lower end of the floating head, and a flange is provided at the liquid inlet for contacting and limiting the limit plate;
[0032] The floating ball is arranged on the top of the floating head, the density of the floating ball is less than the density of the coating agent solution, and the diameter of the floating ball is greater than the diameter of the liquid inlet hole.
[0033] As an improvement, the piston unit comprises a piston, an inner magnetic ring, an outer magnetic ring, a rotating disk and a spring member;
[0034] The piston is slidably disposed in the cavity of the stirring shaft;
[0035] The inner magnetic ring is sleeved on the piston;
[0036] The outer magnetic ring is sleeved on the outside of the stirring shaft, the outer magnetic ring is arranged corresponding to the inner magnetic ring, and a protrusion is provided on the lower end of the outer magnetic ring;
[0037] The turntable is installed on the stirring shaft, the turntable rotates synchronously with the stirring shaft, and the turntable is located below the outer magnetic ring. A lifting block is protruded on the turntable, and the lifting block cooperates with the protrusion to lift the outer magnetic ring;
[0038] The spring member is sleeved on the stirring shaft, and the spring member abuts between the rotating disk and the top plate of the mixer.
[0039] The beneficial effects of the utility model are:
[0040] (1) The utility model realizes continuous and automatic coating furnace preparation of negative electrode materials by connecting a solution barrel, a mixer, a high-temperature kettle and a cooling kettle through a pipeline and a delivery pump, and by improving the mixer, the coating agent can fully contact with the negative electrode material, so that the negative electrode material can fully absorb the coating agent, thereby improving the coating quality of the negative electrode material by the coating agent;
[0041] (2) The utility model improves the mixer by setting the stirring shaft and stirring paddle in the mixer hollow, so that a suction pipe and a discharge pipe are formed on the stirring shaft and stirring paddle, and the coating agent input into the upper part of the mixer is sucked and transferred to the lower part of the mixer for discharge in coordination with the setting of the piston unit, thereby avoiding the coating agent from being unable to penetrate the obstruction of the negative electrode material to reach the lower part of the mixer, so that the coating agent is evenly distributed inside the mixer, so that the coating agent can fully coat the negative electrode material;
[0042] (3) The utility model provides a floating unit at the liquid inlet of the liquid extraction tube, and uses the floating unit to control the opening and closing of the liquid inlet, so that the liquid inlet is closed when the negative electrode material is input, and when the coating agent solution is input, the liquid inlet is automatically opened by the buoyancy of the coating agent solution, so that the piston unit can suck and transfer the coating agent solution.
[0043] In summary, the utility model has the advantages of high automation, good coating effect in preparing negative electrode materials, uniform mixing of coating agent and negative electrode material, etc., and is particularly suitable for the technical field of negative electrode material furnace coating equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 This is a schematic diagram of the distribution structure of the utility model;
[0045] Figure 2 This is a schematic diagram of the three-dimensional structure of the practical stirring mechanism;
[0046] Figure 3 This is a cross-sectional structural diagram of the practical stirring mechanism;
[0047] Figure 4 for Figure 3 A schematic diagram of the structure enlargement in the middle;
[0048] Figure 5 This is a schematic diagram of the three-dimensional structure of the floating head of the utility model;
[0049] Figure 6 This is a schematic diagram of the cross-sectional structure of the piston of the utility model;
[0050] Figure 7 This is a schematic diagram of the three-dimensional structure of the outer magnetic ring of the utility model;
[0051] Figure 8It is a schematic diagram of the three-dimensional structure of the turntable of the utility model. DETAILED DESCRIPTION
[0052] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0053] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0054] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present utility model, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0055] Example:
[0056] like Figures 1 to 8 As shown, a negative electrode material melting furnace coating device comprises:
[0057] Solution tank 1, mixer 2, high temperature kettle 3 and cooling kettle 4;
[0058] The solution barrel 1 is used to carry the coating agent solution;
[0059] The feed port 21 at the top of the mixer 2 is connected to the solution barrel 1 through a pipeline, and the negative electrode material is input into the mixer 2 through the feed port 21;
[0060] The input port 31 at the top of the high temperature kettle 3 is connected to the discharge port 22 at the bottom of the mixer 2, and the high temperature kettle 3 is heated to decompose the coating agent solution;
[0061] The cooling kettle 4 is installed below the high temperature kettle 3 , the inlet 41 arranged at the top of the cooling kettle 4 is connected to the outlet 32 at the bottom of the high temperature kettle 3 , and the bottom of the cooling kettle 4 is provided with a discharge port 42 .
[0062] Wherein, an expansion joint 5 is provided on the connecting pipe between the high temperature kettle 3 and the cooling kettle 4 .
[0063] Furthermore, a tail gas processor 6 is connected to the top of the high temperature kettle 3 , and the tail gas processor 6 processes the waste gas discharged from the high temperature kettle 3 .
[0064] Specifically, the coating agent solution contained in the solution barrel 1 is transported to the mixer 2 through a pipeline and a delivery pump. The powdered negative electrode material has been pre-delivered into the mixer 2. The coating agent solution covers the top of the negative electrode material, and then the coating agent solution and the negative electrode material are mixed by stirring the mixer 2. When the negative electrode material and the coating agent solution are evenly mixed, the mixture is transported to the high-temperature kettle 3 by a screw pump. The high temperature of the high-temperature kettle 3 is used to heat the coating agent solution to form a furnace treatment, so that the coating agent solution is thermally decomposed to produce a carbide or graphitized protective layer, which covers the surface of the negative electrode material. When the negative electrode material completes the furnace treatment, the negative electrode material is cooled by the cooling kettle 4, and the coated negative electrode material is collected.
[0065] It should be noted that when the high-temperature reactor 3 performs furnace treatment on the negative electrode material, the waste gas generated is discharged to the outside after being subjected to environmental protection treatment by the tail gas processor 6 .
[0066] It is further explained that an expansion joint 5 is provided on the connecting pipe between the cooling kettle 4 and the high temperature kettle 3 , and the expansion joint 5 is used to compensate for the deformation of the connecting pipe between the cooling kettle 4 and the high temperature kettle 3 during the cold-heat conversion.
[0067] As a preferred embodiment, the mixer 2 is provided with a stirring mechanism 7, and the stirring mechanism 7 includes a stirring driver 71, a stirring shaft 72, a stirring paddle 73, a floating unit 74 and a piston unit 75;
[0068] The stirring driver 71 is disposed on the top of the mixer 2, and the stirring driver 71 drives the stirring mechanism 7 to operate;
[0069] The stirring shaft 72 is vertically rotatably installed in the mixing chamber of the mixer 2, and the interior of the stirring shaft 72 is hollow;
[0070] The stirring paddles 73 are arranged in a circular array around the stirring shaft 72. The stirring paddles 73 are connected to the stirring shaft 72, and the interior of the stirring paddles 73 is hollow and connected to the cavity of the stirring shaft 72. The stirring paddles 73 include a liquid suction pipe 731 and a liquid discharge pipe 732. The liquid suction pipe 731 is located at the top of the stirring paddle 73, and the liquid discharge pipe 732 is located below the liquid suction pipe 731. A liquid discharge hole 733 is opened on the side wall of the liquid discharge pipe 732. A one-way valve 730 is provided in the cavity of the liquid suction pipe 731 and the stirring shaft 72. The one-way valve 730 in the stirring shaft 72 is used to control the connection between the stirring shaft 72 and the liquid discharge pipe 732. The one-way valve 730 is a conventional spring-type one-way valve, so its specific structure is not described in detail.
[0071] The floating unit 74 is disposed at the liquid inlet 734 of the liquid extraction tube 731 , and the floating unit 74 controls the opening and closing of the liquid inlet 734 ;
[0072] The piston unit 75 is disposed on the top of the stirring shaft 72 . When the piston unit 75 operates, the coating agent solution is extracted through the extraction pipe 731 and discharged from the discharge pipe 732 .
[0073] The floating unit 74 includes a floating head 741 and a floating ball 742;
[0074] The floating head 741 is slidably mounted at the liquid inlet 734. A plurality of liquid inlet holes 743 are provided on the side wall of the floating head 741. A limit plate 744 is provided at the lower end of the floating head 741. A flange 735 is provided at the liquid inlet 734 to limit the limit plate 744.
[0075] The floating ball 742 is disposed on the top of the floating head 741 . The density of the floating ball 742 is less than the density of the coating agent solution, and the diameter of the floating ball 742 is greater than the diameter of the liquid inlet hole 743 .
[0076] Furthermore, the piston unit 75 includes a piston 751, an inner magnetic ring 752, an outer magnetic ring 753, a rotating disk 754 and a spring member 755;
[0077] The piston 751 is slidably disposed in the cavity of the stirring shaft 72;
[0078] The inner magnetic ring 752 is sleeved on the piston 751;
[0079] The outer magnetic ring 753 is sleeved on the outside of the stirring shaft 72, and the outer magnetic ring 753 is arranged corresponding to the inner magnetic ring 752, and a protrusion 756 is provided on the lower end of the outer magnetic ring 753, and a guide rod is provided on the outer magnetic ring 753, and the guide rod penetrates the top plate of the mixer upward;
[0080] The turntable 754 is installed on the stirring shaft 72, and the turntable 754 rotates synchronously with the stirring shaft 72. The turntable 754 is located below the outer magnetic ring 753. A lifting block 757 is protruded on the turntable 754, and the lifting block 757 cooperates with the protrusion 756 to lift the outer magnetic ring 753.
[0081] The spring member 755 is sleeved on the stirring shaft 72 , and the spring member 755 abuts between the rotating disk 754 and the top plate of the mixer 2 .
[0082] It should be noted that when the mixer 2 mixes and stirs the coating agent solution and the negative electrode material, the powdered negative electrode material is first input into the mixing chamber of the mixer 2, and then the coating agent solution is transported into the mixing chamber. Since the negative electrode materials graphite and silicon are both in fine powder form, it is difficult for the coating agent solution to sink through the powdered negative electrode material after being input into the mixing chamber, and it is also difficult to reach the lower layer of the mixing chamber, making it impossible to evenly mix the negative electrode material and the coating agent solution.
[0083] Based on this problem, the present application improves the stirring mechanism 7 of the mixer 2, improves the stirring shaft 72 and the stirring paddle 73 to form a hollow setting, forms a suction pipe 731 and a discharge pipe 732 on the stirring member 73, and the suction pipe 731 and the discharge pipe 732 are both connected to the hollow interior of the stirring shaft 72. When the stirring shaft 72 rotates, the piston unit 75 works in conjunction with the suction pipe 731 to suck the coating solution at the top of the mixing chamber, so that the coating solution is sucked into the hollow interior of the stirring shaft 72, and then the piston unit 75 is squeezed to discharge the coating solution through the discharge pipe 732. Since the discharge pipe 732 is always stirring the negative electrode material, the coating solution is conveniently discharged into the negative electrode material for mixing, so that the coating solution and the negative electrode material are fully mixed and absorbed.
[0084] Among them, the working principle of the floating unit 74 is that the floating ball 742 in the floating unit 74 will float up after being affected by the buoyancy of the coating solution, driving the floating head 741 to move upward, so that the liquid inlet hole 743 on the floating head 741 is connected with the liquid extraction tube 731, and the coating solution enters the liquid extraction tube 731 through the liquid inlet hole 743. When the coating solution is not input, the floating ball 742 is not affected by the buoyancy and will not float up. The liquid inlet hole 743 is located in the liquid extraction tube 731, and the negative electrode material will not enter the liquid extraction tube 731.
[0085] It is further explained that the working principle of the piston unit 75 is that when the stirring driver 71 drives the stirring shaft 72 to rotate, the turntable 754 rotates synchronously with the stirring shaft 72. As the turntable 754 rotates, the outer magnetic ring 753 is repeatedly lifted up and down through the cooperation of the lifting block 757 and the protrusion 756. The piston 751 moves up and down in the hollow stirring shaft 71 through the cooperation of the outer magnetic ring 753 and the inner magnetic ring 752. When the piston 751 moves upward, the one-way valve 730 located in the suction pipe 731 is opened, and the one-way valve 730 located in the stirring shaft 72 is closed. The piston 751 forms a negative pressure in the stirring shaft 71, and the coating agent solution is sucked through the suction pipe 731. After that, when the piston 751 moves downward, the suction pipe 731 and the one-way valve 730 in the stirring shaft 72 are adjusted in the opposite direction, and the piston 751 discharges the coating agent solution in the stirring shaft 71 through the discharge pipe 732.
[0086] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A negative electrode material melting furnace coating device, characterized in that: include: Solution barrel (1), mixer (2), high temperature kettle (3) and cooling kettle (4); The solution barrel (1) is used to carry the coating agent solution; The feed port (21) at the top of the mixer (2) is connected to the solution barrel (1) through a pipeline, and negative electrode material is input into the mixer (2) through the feed port (21); The input port (31) at the top of the high-temperature kettle (3) is connected to the discharge port (22) at the bottom of the mixer (2), and the high-temperature kettle (3) heats and decomposes the coating agent solution; The cooling kettle (4) is installed below the high-temperature kettle (3); an inlet (41) provided at the top of the cooling kettle (4) is connected to an outlet (32) at the bottom of the high-temperature kettle (3); and a discharge port (42) is provided at the bottom of the cooling kettle (4).
2. The negative electrode material melting furnace coating equipment according to claim 1, characterized in that: An expansion joint (5) is provided on the connecting pipe between the high-temperature kettle (3) and the cooling kettle (4).
3. The negative electrode material melting furnace coating equipment according to claim 1, characterized in that: The top of the high-temperature kettle (3) is connected to a tail gas processor (6), and the tail gas processor (6) processes the waste gas discharged from the high-temperature kettle (3).
4. The negative electrode material melting furnace coating equipment according to claim 1, characterized in that: The mixer (2) is provided with a stirring mechanism (7), the stirring mechanism (7) comprising a stirring driver (71), a stirring shaft (72), a stirring paddle (73), a floating unit (74) and a piston unit (75); The stirring driver (71) is arranged on the top of the mixer (2), and the stirring driver (71) drives the stirring mechanism (7) to operate; The stirring shaft (72) is vertically rotatably mounted in the mixing chamber of the mixer (2), and the interior of the stirring shaft (72) is hollow; The stirring paddles (73) are arranged in a circular array around the stirring shaft (72); the stirring paddles (73) are connected to the stirring shaft (72); the interior of the stirring paddles (73) is hollow and is connected to the cavity of the stirring shaft (72); the stirring paddles (73) include a liquid extraction pipe (731) and a liquid discharge pipe (732); the liquid extraction pipe (731) is located at the top of the stirring paddle (73); the liquid discharge pipe (732) is located below the liquid extraction pipe (731); a liquid discharge hole (733) is provided on the side wall of the liquid discharge pipe (732); and a one-way valve (730) is provided in the cavity of the liquid extraction pipe (731) and the stirring shaft (72); The floating unit (74) is arranged at the liquid inlet (734) of the liquid extraction tube (731), and the floating unit (74) controls the switch of the liquid inlet (734); The piston unit (75) is disposed at the top of the stirring shaft (72). When the piston unit (75) operates, the coating agent solution is extracted through the liquid extraction pipe (731) and discharged from the liquid discharge pipe (732).
5. The negative electrode material melting furnace coating equipment according to claim 4, characterized in that: The floating unit (74) comprises a floating head (741) and a floating ball (742); The floating head (741) is slidably mounted at the liquid inlet (734); a plurality of liquid inlet holes (743) are provided on the side wall of the floating head (741); a limit plate (744) is provided at the lower end of the floating head (741); and a flange (735) is provided at the liquid inlet (734) for contacting and limiting the limit plate (744); The floating ball (742) is arranged on the top of the floating head (741), the density of the floating ball (742) is less than the density of the coating agent solution, and the diameter of the floating ball (742) is greater than the diameter of the liquid inlet hole (743).
6. The negative electrode material melting furnace coating equipment according to claim 4, characterized in that: The piston unit (75) comprises a piston (751), an inner magnetic ring (752), an outer magnetic ring (753), a rotating disk (754) and a spring member (755); The piston (751) is slidably disposed in the cavity of the stirring shaft (72); The inner magnetic ring (752) is sleeved on the piston (751); The outer magnetic ring (753) is sleeved on the outside of the stirring shaft (72), the outer magnetic ring (753) is arranged corresponding to the inner magnetic ring (752), and a protrusion (756) is provided on the lower end of the outer magnetic ring (753); The turntable (754) is mounted on the stirring shaft (72), the turntable (754) rotates synchronously with the stirring shaft (72), and the turntable (754) is located below the outer magnetic ring (753). A lifting block (757) is provided on the turntable (754), and the lifting block (757) cooperates with the protrusion (756) to lift the outer magnetic ring (753); The spring member (755) is sleeved on the stirring shaft (72), and the spring member (755) abuts between the rotating disk (754) and the top plate of the mixer (2).