Novel continuous casting tundish
By designing a detachable buffer slag stop groove and multi-layer lining structure in the continuous casting intermediate tank, the problems of inconvenient disassembly and assembly and poor protection effects are solved, efficient filtration and safety monitoring of molten steel are achieved, and the purity of molten steel is improved. and the service life of the intermediate tank.
Patent Information
- Application Number
- CN202420262796.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-03
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2034-02-03
AI Technical Summary
The buffer plates and slag-retaining weirs of the existing continuous cast intermediate tanks are inconvenient to disassemble and install, have poor buffer protection effect, low safety performance, and impurities generated during injection of molten steel affect the performance and quality of the steel.
Design a new type of continuous casting intermediate tank with a built-in removable buffer slag stop groove, which includes inner linings of thermal insulation layer, support layer, refractory layer, connecting layer, indicator layer and wear-resistant refractory layer, and filters the steel water through the slag stop holes. Improve the contact area and protection effect, and judge the lining status through the indicator layer to ensure safety.
The disassembly and assembly and maintenance of buffer slag stop grooves is simplified, the purity and quality of the molten steel is improved, the service life of the intermediate tank is extended, and the lining status is timely judged through the indicator layer, which improves the safety of use.
Smart Images

Figure CN221935364U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of metallurgical equipment, relates to the field of continuous casting equipment, and specifically relates to a novel continuous casting intermediate tank. Background Art
[0002] The continuous casting intermediate tank is a device used to receive, distribute and transport molten steel in the continuous steel casting process. When the molten steel is filled into the continuous casting intermediate tank, the molten steel directly contacts the intermediate tank, which will scour the tank wall of the intermediate tank, causing friction damage to the tank wall and shortening its service life. Therefore, a buffer plate is usually placed at the steel receiving level of the intermediate tank to reduce the scouring and wear of the molten steel on the intermediate tank. However, the buffer plate is usually a plate-like structure with a single material, and its contact area with the molten steel is limited. The splashing of the molten steel will scour the side wall of the tank body, resulting in poor buffer protection effect. Moreover, when the buffer plate is used, it is impossible to determine its use status and whether it has been burned through, so it is impossible to make a disposal plan in time, affecting the safety of use. At the same time, when the molten steel is injected into the intermediate tank, impurities and oxides are usually inevitably generated, which will affect the performance and quality of the steel. Therefore, a slag weir is often set at the steel receiving level of the intermediate tank to intercept impurities in the molten steel and ensure the purity and quality of the molten steel.
[0003] The buffer plate and slag weir installed in the current continuous casting tundish are usually split structures, so they need to be disassembled and maintained separately, which is inconvenient to operate and affects production efficiency. Utility Model Content
[0004] The utility model is to solve the technical problems that the buffer plate and the slag retaining weir are inconvenient to disassemble and maintain, the buffer plate has poor buffering protection effect, and the use safety performance is low, and provides a new type of continuous casting intermediate tank. The liner is placed in the buffer slag retaining groove to receive the molten steel, which is easy to disassemble and maintain, and increases the contact area with the molten steel, improves the buffering protection effect, and the indication signal emitted by the indication layer determines the use status of the liner, thereby improving the use safety.
[0005] The technical solution adopted by the utility model is: to provide a new type of continuous casting intermediate tank, including an intermediate tank, a buffer slag retaining groove is detachably installed in the intermediate tank, an inner liner is fitted and inserted in the buffer slag retaining groove, and the inner liner and the buffer slag retaining groove are detachably installed and matched, the outer wall of the buffer slag retaining groove and the outer wall of the inner liner are both provided with slag retaining holes, the positions and numbers of the slag retaining holes are matched, and the slag retaining holes are all facing the inside of the intermediate tank; the buffer slag retaining groove is sequentially provided with an insulating layer, a supporting layer and a refractory layer from the inside to the outside; the inner liner is sequentially provided with a connecting layer, an indicating layer and a wear-resistant and refractory layer from the outside to the inside.
[0006] After the buffer slag retaining trough is assembled at the molten steel level of the intermediate tank, the liner is inserted into the buffer slag retaining trough, and then the molten steel is injected into the liner. After the molten steel is filtered through the slag retaining holes on the liner and the buffer slag retaining trough, the residue is intercepted in the liner, and the filtered molten steel is injected into the intermediate tank and diverted thereto to ensure the purity of the molten steel. The liner and the buffer slag retaining trough receive and buffer the molten steel to prevent the intermediate tank from being damaged by the molten steel. The buffer slag retaining trough supports the thermal insulation layer and the refractory layer through the supporting layer to maintain their shape. The refractory layer and the molten steel in the intermediate tank are The contact is stable and the supporting layer is prevented from being damaged, while the heat-insulating layer is fitted with the lining to support the lining. The heat-insulating layer reduces the conduction of heat on the lining to avoid thermal damage to the supporting layer and insulates the lining to improve the reliability of molten steel holding. The lining supports the indicating layer and the wear-resistant and refractory layer through the connecting layer, so that the wear-resistant and refractory layer on the inner side of the lining can hold the molten steel and extend its service life. After the wear-resistant and refractory layer is worn and burned through with use, the indicating layer sends an indicating signal to dispose of the lining in time and improve production safety.
[0007] To further optimize the technical solution, a support ring is provided on the top wall of the buffer slag retaining groove, the support ring is fixedly connected to the support layer of the buffer slag retaining groove, and the side wall of the support ring protrudes from the refractory layer of the buffer slag retaining groove and abuts against the outer wall of the intermediate tank; the top wall of the support ring is provided with docking holes along the circumferential direction.
[0008] When the buffer slag stop groove is inserted into the intermediate tank, the support ring on the top wall of the buffer slag stop groove abuts against the top of the intermediate tank, so that the support ring supports the buffer slag stop groove, and the side wall of the support ring protrudes from the refractory layer of the outer layer of the buffer slag stop groove, so that the support ring and the intermediate tank abut smoothly and the support is stable. The docking holes arranged along the circumference of the top wall of the support ring are threadedly connected to the intermediate tank by inserting bolts to lock and fix the buffer slag stop groove to avoid arbitrary displacement, thereby improving the reliability of use, facilitating disassembly and maintenance, and being flexible to use.
[0009] To further optimize the technical solution, the support layer is a carbon steel layer, and the thickness of the carbon steel layer is 30-40 mm.
[0010] Carbon steel has low cost and is easy to process. The carbon element in carbon steel reacts with the iron element in steel to form iron carbide on the surface of carbon steel under high temperature environment. The crystal structure of iron carbide is very stable and the interaction force between its internal atoms is very strong, which makes it difficult for iron carbide to decompose or change phases at high temperatures, so that it can maintain its original structure and properties under high temperature environment, thereby enhancing the strength and hardness of carbon steel. Secondly, the carbon element and iron element in iron carbide are covalently bonded to form a stable Fe-C chemical bond. This chemical bond reduces the ability of carbon element to react with other elements in steel, so that carbon steel maintains stability. In addition, the surface tension of iron carbide formed on the surface of carbon steel is small, and a flat and smooth protective layer is formed on the surface of carbon steel, which can prevent further contact between oxygen and iron carbide, prevent carbon steel from being oxidized, and improve the stability of use.
[0011] To further optimize the technical solution, the refractory layer is a silicon carbide casting layer, and the silicon carbide casting layer is 180-250mm.
[0012] Silicon carbide is composed of carbon and silicon elements combined in the form of covalent bonds to form a stable crystal structure. There are many covalent bonds in the crystal structure of silicon carbide, which remain stable in the solid state, making the crystal structure of silicon carbide stable. At the same time, silicon carbide has a high melting point, so that silicon carbide can still remain in a solid state at extremely high temperatures, so that it will not melt or deform when it comes into contact with molten steel. Silicon carbide has a low thermal expansion coefficient, so that silicon carbide is not easy to break or deform due to rapid changes in temperature. Secondly, silicon carbide has a high thermal conductivity. When the heat of molten steel is transferred to the silicon carbide casting layer, the silicon carbide casting layer quickly transfers the heat to the surrounding medium, thereby reducing the local temperature and preventing the silicon carbide casting layer from burning through due to heat concentration. In addition, the Mohs hardness of silicon carbide is about 9.25, which makes it have good wear resistance and impact resistance, can resist the erosion of molten steel, and enhance the protection effect on the supporting layer.
[0013] To further optimize the technical solution, the thermal insulation layer is a perlite layer, and the thickness of the perlite layer is 60-80 mm.
[0014] Perlite is a porous inorganic non-metallic material. The porous structure of perlite allows for a large number of pores to exist inside the perlite, which can store air. When the perlite is heated, the air in its pores absorbs heat, causing the temperature to rise. Since the porosity of perlite is high, air diffuses and exchanges quickly in the pores, so it can absorb and release heat faster, thereby slowing down the rate of temperature rise during the heating process of the perlite. At the same time, perlite has a low thermal conductivity, which slows down the transfer of heat, giving perlite good thermal insulation and heat-insulating effects, thereby reducing heat conduction to the support layer, slowing down damage to carbon steel, and reducing heat conduction to the refractory layer, accelerating heat loss, and improving the insulation effect of the lining.
[0015] To further optimize the technical solution, the connecting layer is a low alloy steel layer, and the low alloy steel layer is 20-30 mm.
[0016] Low alloy steel usually contains a small amount of alloying elements, which refine the microstructure of the steel, improve the strength and toughness of the steel, make it less likely to crack and break, and be able to withstand large deformation and chip force, making it convenient to process the supporting layer. The small amount of alloying elements contained in low alloy steel can form stable carbides with the carbon elements in the steel, thereby improving the corrosion resistance of the steel. At the same time, the small amount of alloying elements in low alloy steel can improve the tempering stability and creep resistance of the steel, so that it can maintain good stability in high temperature environments, thereby improving its stability and reliability in use.
[0017] To further optimize the technical solution, the indicator layer is a chromium oxide green layer, and the thickness of the chromium oxide green layer is 3-5 mm.
[0018] At normal temperature, the chromium element in chromium oxide green exists in the +3 valence state, and combines with oxygen to form a stable oxide, showing green. As the temperature rises, part of the chromium element in chromium oxide green will change its valence state from +3 to +4, resulting in changes in the electron configuration and the generation of electron transitions. This electron transition causes changes in the absorption spectrum, increasing the absorption of green light and reducing the absorption of yellow light, causing the chromium oxide green to change color as the temperature rises. This is used to indicate the temperature increase. By observing the color change of chromium oxide green, the temperature increase trend and the risk of burn-through can be judged, so that corresponding measures can be taken to prevent accidents. In addition, in a high temperature environment, chromium oxide green can react with oxygen to form a dense oxide film, which protects chromium oxide green from the influence of oxidation, allowing it to maintain its stability and oxidation resistance in high temperature and corrosive environments, and is stable in use.
[0019] To further optimize the technical solution, the wear-resistant and fire-resistant layer is a mullite layer, and the mullite layer is 200-250 mm.
[0020] Mullite is a high-temperature refractory material, which is mainly composed of aluminum, silicon and oxygen elements. Its chemical bonds are stable, making it difficult for mullite to react with other substances at high temperatures. At the same time, the crystal structure of mullite is arranged regularly and the interaction between atoms is strong, which can maintain the stability of its structure and performance in a high temperature environment, ensuring that the lining is not easily deformed or damaged at high temperatures. The high hardness of mullite material gives it excellent wear resistance, which can resist the wear of the lining caused by the flow and friction of molten steel and extend the service life of the lining. Secondly, mullite material also has good thermal shock resistance and erosion resistance. Under rapid temperature changes, it can quickly adapt to temperature changes and reduce the stress caused by thermal expansion and contraction, so that it maintains structural stability to resist the erosion of molten steel.
[0021] The beneficial effects of the utility model are:
[0022] 1. The buffer slag retaining groove is easy to assemble with the intermediate tank through the connecting ring. After the liner is placed in the buffer slag retaining groove and the molten steel is injected into the liner, the slag retaining hole intercepts the impurities in the molten steel to ensure the purity and quality of the molten steel flowing into the intermediate tank. The liner and the buffer slag retaining groove are detachable, which is convenient for taking them out and cleaning the intercepted impurities, and is flexible to use.
[0023] 2. When molten steel is injected into the lining, it is prevented from contacting the lining with the tank wall, and the molten steel is prevented from scouring and wearing the lining. The mullite layer on the inner side of the lining receives the molten steel, and its performance is stable and reliable. The use status of the mullite layer can be judged by the color change of the chromium oxide green layer of the lining, so that it can be handled in time after burning through, thereby improving the safety of use;
[0024] 3. When the lining is placed in the buffer slag retaining trough, the perlite layer fits with the lining and supports it. The porous structure of the perlite gives it a good thermal insulation effect, which insulates the lining and reduces the temperature loss of the molten steel in the lining. When the molten steel flows into the intermediate tank, the silicon carbide casting layer on the outside of the buffer slag retaining trough contacts with the molten steel. Its fire-resistant and high-temperature resistant properties prevent the buffer slag retaining trough from being damaged, making it safe and reliable to use. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 This is a schematic structural diagram of the continuous casting tundish of this embodiment;
[0026] Figure 2 This is a schematic diagram of the structure of the buffer slag retaining groove of this embodiment;
[0027] Figure 3 is a schematic structural diagram of the liner of this embodiment;
[0028] Figure 4 Schematic diagram of the cross-sectional structure of the buffer slag retaining groove of this embodiment;
[0029] Figure 5 Schematic diagram of the cross-sectional structure of the liner of this embodiment.
[0030] In the figure, 1. intermediate tank; 2. buffer slag retaining groove; 201. support ring; 2011. docking hole; 202. thermal insulation layer; 203. support layer; 204. refractory layer; 3. lining; 301. connection layer; 302. indication layer; 303. wear-resistant refractory layer; 4. slag retaining hole. DETAILED DESCRIPTION
[0031] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0032] Please see attached Figure 1, Attachment Figure 2 , Attachment Figure 4 A novel continuous casting intermediate tank comprises an intermediate tank 1, which is a "T"-shaped structure. A buffer slag retaining groove 2 is detachably installed in the intermediate tank 1. A support ring 201 is provided on the top wall of the buffer slag retaining groove 2. The buffer slag retaining groove 2 is assembled with the intermediate tank 1 through the support ring 201. The buffer slag retaining groove 2 is provided with an insulating layer 202, a support layer 203 and a refractory layer 204 from the inside to the outside. The support ring 201 is fixedly connected to the support layer 203 of the buffer slag retaining groove 2, and the side wall of the support ring 201 protrudes from the refractory layer 204 on the outside of the buffer slag retaining groove 2, so that the support ring 201 abuts against the top wall of the intermediate tank 1 to support the buffer slag retaining groove 2. A docking hole 2011 is provided on the outer wall of the support ring 201 along the circumferential direction. By inserting bolts into the docking hole 2011 and threadedly connecting it with the intermediate tank 1, it is fixed on the intermediate tank 1, thereby improving the firmness of the buffer slag retaining groove 2, and facilitating its disassembly and making it flexible to use.
[0033] The supporting layer 203 of the buffer slag retaining trough 2 is a carbon steel layer. The carbon steel layer can be made of conventional carbon steel material purchased from the market and cast into a carbon steel layer of specific specifications through a carbon steel casting process. The preferred thickness of the carbon steel layer is 35 mm. The heat insulating layer 202 of the inner wall and the refractory layer 204 of the outer wall of the buffer slag retaining trough 2 are both attached to the carbon steel layer, and the carbon steel layer supports them. The price of carbon steel is relatively low, which can reduce its production and use costs. In addition, the carbon element in carbon steel forms iron carbide on the surface of carbon steel with the iron element in steel under high temperature conditions. The crystal structure of iron carbide is very stable, and the interaction force between its internal atoms is very strong. Very strong, so that iron carbide is not easy to decompose or phase change at high temperature, so that it can maintain its original structure and properties in high temperature environment, thereby enhancing the strength and hardness of carbon steel. Secondly, the carbon element and iron element of iron carbide are covalently bonded to form a stable Fe-C chemical bond. This chemical bond reduces the ability of carbon element to react with other elements in steel, so that carbon steel maintains stability. In addition, the surface tension of iron carbide formed on the surface of carbon steel is small, and a flat and smooth protective layer is formed on the surface of carbon steel, which can prevent further contact between oxygen and iron carbide and prevent carbon steel from being oxidized. It is stable and reliable to use.
[0034] The refractory layer 204 on the outside of the support layer 203 is a silicon carbide casting layer. The silicon carbide casting layer can be made of silicon carbide powder produced by Beijing Gaoke New Material Technology Co., Ltd., and after mixing with an adhesive, it is cast on the outside of the support layer 203. The preferred casting thickness of the silicon carbide casting layer is 200mm. Silicon carbide is formed by combining carbon and silicon elements in the form of covalent bonds to form a stable crystal structure. There are many covalent bonds in the crystal structure of silicon carbide. These covalent bonds remain stable in the solid state, so that the crystal structure of silicon carbide remains stable. When the temperature rises, although the atoms begin to do thermal motion, the covalent bonds require very high temperatures to be destroyed, so that the melting point of silicon carbide is very high, reaching 2830°C, which means that silicon carbide can still remain in a solid state at extremely high temperatures, so that when it comes into contact with molten steel , no melting or deformation will occur. At the same time, the crystal structure of silicon carbide is a hexagonal crystal with a small lattice constant and close atomic spacing, which makes the interaction between atoms stronger and makes silicon carbide less likely to deform when the temperature changes, that is, the thermal expansion coefficient is low, which means that silicon carbide is not easy to break or deform due to a sharp change in temperature. Secondly, silicon carbide has a high thermal conductivity. When the heat of molten steel is transferred to the silicon carbide casting layer, the silicon carbide casting layer quickly transfers the heat to the surrounding medium, thereby reducing the local temperature and preventing the silicon carbide casting layer from burning through due to heat concentration. In addition, the crystal structure of silicon carbide is similar to that of diamond, and its Mohs hardness is about 9.25, which makes it have good wear resistance and impact resistance, can resist the erosion of molten steel, and enhance the protection effect on the support layer 203;
[0035] The heat insulating layer 202 inside the support layer 203 is a perlite layer. The perlite layer can be made of perlite produced by Hebei Shanfang Mining Co., Ltd., and after being mixed with a binder, it is laid on the inner wall of the support layer 203. The preferred laying thickness is 70 mm. Perlite is a porous inorganic non-metallic material. Its main components are silicate minerals such as feldspar, quartz and mica. It does not contain combustible substances. In addition, the porous structure of perlite causes a large number of pores to exist inside the perlite. A large amount of air can be stored in the pores. When the perlite is heated, the air in the pores will absorb heat, causing the temperature to rise. High, because the porosity of perlite is high, the air diffuses and exchanges quickly in the pores, so it can absorb and release heat faster, so that the temperature rise rate can be slowed down during the heating process of perlite. At the same time, the thermal conductivity of perlite is between 0.035 and 0.055 W / (m·K), which has a low thermal conductivity, slows down the heat transfer rate, and makes perlite have good thermal insulation and heat insulation effects, thereby reducing the heat conduction to the support layer 203, slowing down the damage to the carbon steel, and reducing the heat conduction to the refractory layer 204, accelerating the heat loss, and improving the thermal insulation effect of the lining 3;
[0036] Please see attached Figure 1 , Attachment Figure 3 , Attachment Figure 5 The top wall of the buffer slag retaining groove 2 is provided with a support ring 201, which abuts against the outer wall of the intermediate tank 1 to support the buffer slag retaining groove 2. The support ring 201 is fixedly connected to the support layer 203 of the buffer slag retaining groove 2, that is, fixedly connected to the carbon steel layer. The outer ring wall of the support ring 201 protrudes from the refractory layer 204 of the buffer slag retaining groove 2, so that the diameter of the support ring 201 is larger than the diameter of the buffer slag retaining groove 2, which is convenient for the intermediate tank 1 to support the buffer slag retaining groove 2 through the support ring 201. The top wall of the ring 201 is provided with a docking hole 2011 along the circumferential direction. After the bolts are inserted into the docking hole 2011 and the docking hole 2011 is threadedly connected with the intermediate tank 1, the buffer slag retaining groove 2 is fixed on the intermediate tank 1 to improve the firmness of use. The buffer slag retaining groove 2 is fitted with an inner liner 3. The inner liner 3 and the buffer slag retaining groove 2 can be detachably installed. The buffer slag retaining groove 2 receives molten steel through the inner liner 3. The inner liner 3 is provided with a connecting layer 301, an indicating layer 302 and a wear-resistant and fire-resistant layer 303204 from the outside to the inside.
[0037] The connecting layer 301 of the lining 3 is a low-alloy steel layer, the low-alloy steel layer is bonded to the perlite layer of the buffer slag retaining groove 2, and the perlite layer supports the low-alloy steel layer. The low-alloy steel layer is processed into a shape by using a low-alloy steel plate commonly used on the market, and its preferred processing thickness is 25 mm. Low-alloy steel usually contains a small amount of alloy elements, which refines the microstructure of the steel, improves the strength and toughness of the steel, makes it less likely to crack and break, and can withstand a large deformation and chip force, making it convenient to process the support layer 203. The small amount of alloy elements contained in the low-alloy steel can form stable carbides with the carbon elements in the steel, thereby improving the corrosion resistance of the steel. At the same time, the small amount of alloy elements in the low-alloy steel improves the tempering stability and creep resistance of the steel, so that it can maintain good stability in a high temperature environment, making it stable in use;
[0038] The indicator layer 302 of the lining 3 is a chromium oxide green layer. The chromium oxide green layer adopts chromium oxide green powder produced by Beijing Gaoke New Material Technology Co., Ltd., and after mixing with an adhesive, a proper amount of water is added to make a slurry, which is brushed or sprayed on the connecting layer 301 of the lining 3. The preferred brushing thickness of chromium oxide green is 3mm. Under normal temperature, the chromium element in chromium oxide green exists in a +3 valence state, which combines with oxygen to form a stable oxide, showing green. As the temperature rises, part of the chromium element in chromium oxide green will change its valence state from +3 to +4, resulting in changes in the electron configuration and electron hopping. The generation of electron transition causes the absorption spectrum to change, the absorption of green light increases, while the absorption of yellow light decreases, so that the color of chromium oxide green changes with the increase of temperature, which is used to indicate the temperature increase. By observing the color change of chromium oxide green, the temperature increase trend and the risk of burn-through can be judged, so that corresponding measures can be taken to prevent accidents. In addition, in a high temperature environment, chromium oxide green can react with oxygen to form a dense oxide film, which protects chromium oxide green from oxidation, so that it can maintain its stability and oxidation resistance in high temperature and corrosive environment, making it stable in use.
[0039] The wear-resistant and fire-resistant layer 303204 of the lining 3 is a mullite layer. The mullite layer can be made of mullite powder produced by Beijing Gaoke New Material Technology Co., Ltd. and made into a slurry and applied on the indicator layer 302. The preferred coating thickness of the mullite is 200mm. When the molten steel is injected into the lining 3, the mullite layer receives the molten steel. Mullite is a high-temperature refractory material, which is mainly composed of aluminum, silicon, and oxygen elements. Its chemical bonds are stable, so that the mullite material is not easy to react with other substances at high temperatures. At the same time, the crystal structure of the mullite material is arranged The material law, the interaction force between atoms is strong, and it can maintain the stability of its structure and performance in a high temperature environment, ensuring that the lining 3 is not easily deformed or damaged at high temperatures. The mullite material has high hardness, which makes it have excellent wear resistance, and can resist the wear of the lining 3 caused by the flow and friction of molten steel, thereby extending the service life of the lining 3. Secondly, the mullite material also has good thermal shock resistance and erosion resistance. Under rapid temperature changes, it can quickly adapt to temperature changes, reduce the stress caused by thermal expansion and contraction, and keep its structure stable to resist the erosion of molten steel.
[0040] Please see attached Figure 2 , Attachment Figure 3 The outer wall of the buffer slag retaining groove 2 and the outer wall of the inner lining 3 are both provided with slag retaining holes 4, the positions and numbers of the slag retaining holes 4 are matched, and the slag retaining holes 4 are all facing the middle tank 1. After the molten steel is injected into the inner lining 3, the molten steel flows into the middle tank 1 along the slag retaining holes 4 on the inner lining 3 and the buffer slag retaining groove 2. The slag retaining holes 4 filter the residue in the molten steel and intercept it in the inner lining 3 to maintain the purity and quality of the molten steel.
[0041] The working principle of the novel continuous casting intermediate tank is as follows: insert the buffer slag retaining groove 2 into the intermediate tank 1 to receive the molten steel level, the support ring 201 on the top wall of the buffer slag retaining groove 2 abuts against the top wall of the intermediate tank 1 to support the buffer slag retaining groove 2, and after the bolts are passed through the docking holes 2011 on the support ring 201, the bolts are connected with the threads of the intermediate tank 1 to fix the buffer slag retaining groove 2 on the intermediate tank 1, and then the liner 3 is inserted into the buffer slag retaining groove 2, the low alloy steel layer on the outer wall of the liner 3 fits with the heat insulation layer 202 on the inner wall of the buffer slag retaining groove 2, after the molten steel is injected into the mullite layer of the liner 3, the liner 3 and the slag retaining holes 4 on the buffer slag retaining groove 2 filter the molten steel, so that the residue in the molten steel is intercepted in the liner 3, to ensure the purity and quality of the molten steel, and after the molten steel flows into the intermediate tank 1, it can be diverted and the like, and it is easy to use;
[0042] The mullite layer of the lining 3 receives and buffers the molten steel, preventing the molten steel from directly scouring the intermediate tank 1 and causing damage, thereby extending the service life of the intermediate tank 1. The mullite layer is wear-resistant and high-temperature-resistant, thereby improving the stability of the lining 3. As the mullite layer is worn away by the molten steel and its thickness decreases, the heat conduction temperature of the mullite layer to the chromium oxide green layer gradually increases, causing the chromium oxide green layer to change color. The service life of the mullite layer can be determined by the color change. After the mullite layer is burned through by the molten steel, the molten steel contacts the chromium oxide green layer and the chromium oxide green layer is oxidized. The chromium oxide in the chrome green reacts with the carbon and iron in the molten steel to reduce, consume the chromium oxide green, generate bubbles in the molten steel, and cause boiling, so that the surface mullite layer is burned through so as to react in time. When the mullite layer is burned through, the low alloy steel layer receives the molten steel, which is stable at high temperatures and avoids leakage of the molten steel, further improving the safety of use. After the lining 3 is burned by the molten steel, it is taken out of the buffer slag retaining tank 2 so that it can be disassembled and replaced to continue the continuous casting operation. The operation is simple and flexible.
[0043] When the lining 3 holds molten steel, the porous structure of the perlite layer on the inner wall of the buffer slag retaining trough 2 provides good thermal insulation for the lining 3, reduces heat conduction to the carbon steel layer and silicon carbide casting layer of the buffer slag retaining trough 2, and alleviates thermal damage to the carbon steel layer. When the molten steel is injected into the intermediate tank 1 through the slag retaining hole, the molten steel contacts the silicon carbide casting layer, and the silicon carbide casting layer can remain solid at extremely high temperatures, so that it will not melt or deform when in contact with the molten steel, and can resist the erosion of the molten steel, thereby enhancing the protective effect on the carbon steel layer.
Claims
1. A novel continuous casting tundish, comprising a tundish (1), characterized in that: The intermediate tank (1) is provided with a detachable buffer slag retaining groove (2), an inner lining (3) is inserted into the buffer slag retaining groove (2), and the inner lining (3) and the buffer slag retaining groove (2) are detachably mounted and matched, and the outer wall of the buffer slag retaining groove (2) and the outer wall of the inner lining (3) are both provided with slag retaining holes (4), the positions and numbers of the slag retaining holes (4) are matched, and the slag retaining holes (4) are all facing the inside of the intermediate tank (1); the buffer slag retaining groove (2) is provided with a heat insulation layer (202), a support layer (203) and a refractory layer (204) in sequence from the inside to the outside; the inner lining (3) is provided with a connecting layer (301), an indication layer (302) and a wear-resistant and refractory layer (303) (204) in sequence from the outside to the inside.
2. A novel continuous casting intermediate tank according to claim 1, characterized in that: The top wall of the buffer slag retaining groove (2) is provided with a support ring (201), the support ring (201) is fixedly connected to the support layer (203) of the buffer slag retaining groove (2), and the side wall of the support ring (201) protrudes from the refractory layer (204) of the buffer slag retaining groove (2) and abuts against the outer wall of the intermediate tank (1); the top wall of the support ring (201) is provided with a docking hole (2011) along the circumferential direction.
3. A novel continuous casting tundish according to claim 2, characterized in that: The support layer (203) is a carbon steel layer, and the thickness of the carbon steel layer is 30-40 mm.
4. A novel continuous casting tundish according to claim 2, characterized in that: The refractory layer (204) is a silicon carbide casting layer, and the thickness of the silicon carbide casting layer is 180-250 mm.
5. The novel continuous casting intermediate tank according to claim 1 is characterized in that: The heat insulation layer (202) is a perlite layer, and the thickness of the perlite layer is 60-80 mm.
6. The novel continuous casting intermediate tank according to claim 1 is characterized in that: The connecting layer (301) is a low alloy steel layer, and the low alloy steel layer is 20-30 mm thick.
7. The novel continuous casting tundish according to claim 1 is characterized by: The indicating layer (302) is a chromium oxide green layer, and the thickness of the chromium oxide green layer is 3-5 mm.
8. The novel continuous casting tundish according to claim 1 is characterized by: The wear-resistant and fire-resistant layer (303) (204) is a mullite layer, and the thickness of the mullite layer is 200-250 mm.