Welding preheating device

By designing a welding preheating device including a support frame, a curved adjustment frame and an electric heating sheet, the problems of uneven preheating and slow speed in the prior art are solved, more efficient welding preheating is achieved, and welding is improved Quality and construction efficiency.

CN221935750UActive Publication Date: 2024-11-01ZHONGHAI FULU HEAVY IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323608737.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-11-01
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

When the existing welding preheating device is welded with pipes, the preheating heating rate is low and the temperature is uneven, which affects the welding quality and construction efficiency.

Method used

A welding preheating device is designed, including a support frame, a curved adjustment frame, an electric heating sheet, a telescopic rod and a locking member. By adjusting the angle and position of the electric heating sheet, it is fitted to the outer periphery of the pipe and increasing the heating area. , achieve more even and fast preheating.

Benefits of technology

Improve the uniformity and speed of pipeline preheating temperature, improve welding quality and construction efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221935750U_ABST
    Figure CN221935750U_ABST
Patent Text Reader

Abstract

The utility model discloses a welding preheating device which comprises a supporting frame, an arc-shaped adjusting frame, an electric heating piece, a first telescopic rod, an adjusting rod, a second telescopic rod, a first locking piece and a second locking piece, and the electric heating piece is laid and fixedly connected to the concave side of the arc-shaped adjusting frame; the first end of the first telescopic rod is horizontally and telescopically connected to the first end of the supporting frame, and the second end of the first telescopic rod is fixedly connected to the first end of the arc-shaped adjusting frame. The first end of the adjusting rod is rotatably connected to the second end of the supporting frame, the first end of the second telescopic rod is telescopically connected to the second end of the adjusting rod, and the second end of the second telescopic rod is rotatably connected to the second end of the arc-shaped adjusting frame. According to the preheating device, the angle of the electric heating piece can be adjusted, so that the electric heating piece is well attached to the periphery of the pipeline to be welded, the heated contact area of a pipeline groove can be increased, the pipeline preheating temperature is more uniform, preheating is faster, the preheating efficiency is higher, and the welding quality and the construction efficiency can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of welding, in particular to a welding preheating device. Background Art

[0002] In the fields of petrochemicals, offshore platforms, etc., metal pipes are often used to transport a variety of media such as oil, gas, and water. The quality requirements for pipes are extremely strict, so the welding of pipes is particularly important. When welding carbon steel pipes, in order to ensure the welding quality and prevent welding defects such as pores and hydrogen-induced delayed cracks, preheating before welding is an important factor in the design of welding technology and welding quality control. Preheating the parent material before welding can not only ensure that the moisture in the parent material is fully removed and avoid the formation of pores in the weld, but also reduce the cooling rate of the weld, ensure that the temperature fluctuation range of the parent material is small, and avoid reducing the performance of the welded joint due to excessive cooling. The preheating methods in the prior art include flame torch heating and electric heating, but when welding the circumferential seam of the pipe extension, there are problems such as low preheating temperature rise rate, inadequate preheating, and uneven preheating temperature, which affect the welding quality and construction efficiency. Utility Model Content

[0003] In order to overcome the deficiencies of the prior art, the purpose of the utility model is to provide a welding preheating device, which can make the pipeline preheating temperature rise faster, the preheating temperature more uniform, and improve the welding quality and construction efficiency.

[0004] To solve the above problems, the technical solution adopted by the utility model is as follows: a welding preheating device, comprising a support frame, an arc-shaped adjustment frame, an electric heating plate, a first telescopic rod, an adjustment rod, a second telescopic rod, a first locking piece and a second locking piece, the electric heating plate being laid and fixedly connected to the concave side of the arc-shaped adjustment frame; the first end of the first telescopic rod being horizontally telescopically connected to the first end of the support frame, and the second end of the first telescopic rod being fixedly connected to the first end of the arc-shaped adjustment frame; the first end of the adjusting rod being rotatably connected to the second end of the support frame, the first end of the second telescopic rod being telescopically connected to the second end of the adjusting rod, and the second end of the second telescopic rod being rotatably connected to the second end of the arc-shaped adjustment frame, the first locking piece being used to lock and fix the adjusting rod and the support frame, and the second locking piece being used to lock and fix the adjusting rod and the second telescopic rod.

[0005] Compared with the prior art, the beneficial effect of the utility model is that: when in use, the preheating device is placed on the side of the groove of the pipe to be welded, and the electric heating plate is laid on the concave side of the arc-shaped adjustment frame to form a curved sheet structure, which can wrap the groove of the pipe, and then the electric heating plate is adjusted in the up and down and front and back directions by the extension and contraction of the first telescopic rod and the second telescopic rod and the rotation of the adjustment rod, so that the electric heating plate can be well fitted on the outer periphery of the pipe to be welded, and then the first locking member is used to lock and fix the adjustment rod and the support frame, and the second locking member is used to lock and fix the adjustment rod and the second telescopic rod, and the electric heating plate is energized, and the pipe can be preheated by rotating the pipe at a uniform speed. Compared with the traditional preheating device, the preheating device can adjust the angle of the electric heating plate, so that the electric heating plate is well fitted on the outer periphery of the pipe to be welded, and the heat contact area of ​​the pipe groove can be increased, so that the preheating temperature of the pipe is more uniform, the preheating is faster, and the efficiency is higher, thereby improving the welding quality and construction efficiency.

[0006] In the above-mentioned welding preheating device, a handle is provided on the arc-shaped adjustment frame, and the first end and the second end of the handle are fixedly connected to the first end and the second end of the arc-shaped adjustment frame respectively.

[0007] In the above-mentioned welding preheating device, the second end of the first telescopic rod is fixedly connected to a connecting sleeve, and the first end of the handle is inserted into the connecting sleeve.

[0008] The above-mentioned welding preheating device, the support frame includes a fixed rod, the adjusting rod includes a first rotating sleeve and an oblique support sleeve fixedly connected in a "T" shape, the first rotating sleeve is rotatably sleeved on the outer periphery of the fixed rod, the first end of the second telescopic rod is telescopically inserted into the oblique support sleeve, the first locking piece is used to lock and fix the fixed rod and the first rotating sleeve, and the second locking piece is used to lock and fix the oblique support sleeve and the second telescopic rod.

[0009] The above-mentioned welding preheating device, the support frame includes four columns, four first supporting rods connected to the upper ends of the columns and four second supporting rods connected to the lower ends of the columns, one first supporting rod and one second supporting rod are connected between each two adjacent columns, and the two ends of the fixing rod are respectively connected to the two columns away from the arc-shaped adjustment frame.

[0010] In the above-mentioned welding preheating device, two first telescopic rods are provided, and the two first telescopic rods are respectively telescopically connected to two first supporting tie rods perpendicular to the fixing rod.

[0011] In the above-mentioned welding preheating device, the arc-shaped adjustment frame includes two arc-shaped connecting rods and a mounting rod connected between the two arc-shaped connecting rods, and a plurality of the mounting rods are distributed along the length direction of the arc-shaped connecting rods.

[0012] In the above-mentioned welding preheating device, the second end of the second telescopic rod is fixedly connected with a second rotating sleeve, and the second rotating sleeve is rotatably sleeved on one of the mounting rods.

[0013] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a schematic diagram of the overall structure of the welding preheating device according to an embodiment of the utility model;

[0015] Figure 2 This is a front view of a welding preheating device according to an embodiment of the present utility model.

[0016] Description of the accompanying drawings: 100 support frame, 110 fixing rod, 120 column, 130 first supporting tie rod, 140 second supporting tie rod, 200 arc-shaped adjustment frame, 210 arc-shaped connecting rod, 220 installation rod, 300 first telescopic rod, 310 connecting sleeve, 400 adjusting rod, 410 first rotating sleeve, 420 oblique supporting sleeve, 500 second telescopic rod, 510 second rotating sleeve, 600 first locking piece, 700 second locking piece, 800 handle. DETAILED DESCRIPTION

[0017] The embodiments of the present invention are described in detail below. Figure 1 and Figure 2 The embodiment of the utility model provides a welding preheating device, including a support frame 100, an arc-shaped adjustment frame 200, an electric heating plate, a first telescopic rod 300, an adjustment rod 400, a second telescopic rod 500, a first locking member 600 and a second locking member 700, the electric heating plate is laid and fixedly connected to the concave side of the arc-shaped adjustment frame 200; the first end of the first telescopic rod 300 is horizontally telescopically connected to the first end of the support frame 100, and the second end of the first telescopic rod 300 is fixedly connected to the first end of the arc-shaped adjustment frame 200; the first end of the adjustment rod 400 is rotatably connected to the second end of the support frame 100, the first end of the second telescopic rod 500 is telescopically connected to the second end of the adjustment rod 400, and the second end of the second telescopic rod 500 is rotatably connected to the second end of the arc-shaped adjustment frame 200, the first locking member 600 is used to lock and fix the adjustment rod 400 and the support frame 100, and the second locking member 700 is used to lock and fix the adjustment rod 400 and the second telescopic rod 500.

[0018] When in use, the preheating device is placed on the side of the groove of the pipe to be welded, and the electric heating sheet is laid on the concave side of the arc-shaped adjustment frame 200 to form a curved sheet structure, which can wrap the groove of the pipe, and then the electric heating sheet is adjusted in the up and down and front and back directions by the extension of the first telescopic rod 300 and the second telescopic rod 500 and the rotation of the adjustment rod 400, so that the electric heating sheet can be well fitted on the outer periphery of the pipe to be welded, and the first locking member 600 is used to lock and fix the adjustment rod 400 and the support frame 100, and then the second locking member 700 is used to lock and fix the adjustment rod 400 and the second telescopic rod 500, and the electric heating sheet is energized, and the pipe can be preheated by rotating the pipe at a uniform speed. Compared with the traditional preheating device, the preheating device can adjust the angle of the electric heating sheet, so that the electric heating sheet is well fitted on the outer periphery of the pipe to be welded, and the heat contact area of ​​the pipe groove can be increased, so that the preheating temperature of the pipe is more uniform, the preheating is faster, and the efficiency is higher, thereby improving the welding quality and construction efficiency.

[0019] Further, refer to Figure 1 The support frame 100 includes four columns 120, four first support ties 130 connected to the upper ends of the columns 120, and four second support ties 140 connected to the lower ends of the columns 120. A first support ties 130 and a second support ties 140 are connected between each two adjacent columns 120, so that the four columns 120, the four first support ties 130, and the four second support ties 140 can form a spatial square frame structure to increase the strength and support stability of the support frame 100. The four columns 120, the four first support ties 130, and the four second support ties 140 can be welded and formed using steel materials on the construction site.

[0020] Furthermore, the support frame 100 further includes a fixed rod 110, and the two ends of the fixed rod 110 are respectively connected to two upright posts 120 away from the arc-shaped adjustment frame 200. The adjustment rod 400 includes a first rotating sleeve 410 and an oblique support sleeve 420 that are fixedly connected in a "T" shape, the first rotating sleeve 410 is rotatably sleeved on the outer periphery of the fixed rod 110, the first end of the second telescopic rod 500 is telescopically inserted into the oblique support sleeve 420, the first locking member 600 is used to lock and fix the fixed rod 110 and the first rotating sleeve 410, and the second locking member 700 is used to lock and fix the oblique support sleeve 420 and the second telescopic rod 500. Further, the first locking member 600 is threadedly connected to a side of the first rotating sleeve 410 away from the oblique support sleeve 420, and the first locking member 600 can be screwed in or out relative to the first rotating sleeve 410 to connect or disconnect the first locking member 600 with the fixed rod 110, and the second locking member 700 can be screwed in or out relative to the oblique support sleeve 420 to connect or disconnect the second locking member 700 with the second telescopic rod 500. When the angle of the lower end of the arc adjustment frame 200 needs to be adjusted, the first locking member 600 is screwed out to allow the first rotating sleeve 410 to rotate relative to the fixed rod 110, and the second locking member 700 is screwed out to allow the second telescopic rod 500 to telescopically move along the oblique support sleeve 420. Then push the arc adjustment frame 200 forward or backward to make the second telescopic rod 500 telescopically move along the oblique support sleeve 420, and at the same time, the first rotating sleeve 410 rotates around the fixed rod 110. After being adjusted to the right position, screw in the first locking member 600 and the second locking member 700 to lock and connect the first rotating sleeve 410 and the fixed rod 110, and lock and connect the oblique support sleeve 420 and the second telescopic rod 500. In some embodiments, the first locking member 600 and the second locking member 700 can be threaded members such as bolts with larger sizes. When the first locking member 600 is screwed in, the inner end of the first locking member 600 abuts against the fixed rod 110, thereby locking and fixing the first rotating sleeve 410 and the fixed rod 110. When the second locking member 700 is screwed in, the inner end of the second locking member 700 abuts against the second telescopic rod 500, thereby locking and fixing the second telescopic rod 500 and the oblique support sleeve 420. In addition, the first locking member 600 and the second locking member 700 can also be structures such as spiral valves, as long as they can achieve locking and loosening between the first rotating sleeve 410 and the fixed rod 110, and locking and loosening between the inclined support sleeve 420 and the second telescopic rod 500.

[0021] Further, continue to refer to Figure 1, there are two first telescopic rods 300, and the two first telescopic rods 300 are respectively telescopically connected to two first support ties 130 perpendicular to the fixed rod 110, and the first support ties 130 connected to the first telescopic rod 300 are hollow tubular structures to facilitate the telescopic movement of the first telescopic rod 300. The other first support ties 130, the second support ties 140 and the column 120 can adopt a solid rod structure to ensure the strength and stability of the support frame 100. Further, the arc adjustment frame 200 is provided with a handle 800, and the handle 800 is U-shaped. The first end and the second end of the handle 800 are respectively fixedly connected to the first end and the second end of the arc adjustment frame 200, and the second end of the first telescopic rod 300 is fixedly connected to the connecting sleeve 310, and the first end of the handle 800 passes through the connecting sleeve 310 and then connected to the first end of the arc adjustment frame 200. When the angle of the arc adjustment frame 200 needs to be adjusted, the arc adjustment frame 200 can be pushed forward or pulled backward by holding the handle 800. Further, the arc adjustment frame 200 includes two arc connecting rods 210 and a mounting rod 220 connected between the two arc connecting rods 210. There are multiple mounting rods 220 distributed along the length direction of the arc connecting rods 210. The arc connecting rods 210 can provide a connection function for the mounting rods 220, and can also make the arc adjustment frame 200 present an arc shape, so as to facilitate welding of the electric heating plate, so that the electric heating plate forms an arc-shaped structure. The second end of the second telescopic rod 500 is fixedly connected with a second rotating sleeve 510, and the second rotating sleeve 510 can be rotatably sleeved with one of the mounting rods 220. When the second telescopic rod 500 is telescopically moved, the first rotating sleeve 410 rotates around the fixed rod 110, and the second rotating sleeve 510 rotates around the mounting rod 220, so that the adjustment rod 400 can smoothly adjust the angle of the arc adjustment frame 200.

[0022] It should be noted that in the description of the present invention, if there are any orientation descriptions, such as up, down, front, back, left, right, etc., the orientations or positional relationships indicated are all based on the orientations or positional relationships shown in the drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed or operated in a specific orientation, and cannot be understood as a limitation on the present invention.

[0023] In the description of the present utility model, "several" means one or more, "more" means two or more, "greater than", "less than", "exceed" etc. are understood to exclude the number itself, and "above", "below", "within" etc. are understood to include the number itself. If there is a description of "first" or "second", it is only used to distinguish the technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.

[0024] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.

[0025] The above-mentioned implementation modes are only preferred implementation modes of the present invention, and cannot be used to limit the protection scope of the present invention. Any non-substantial changes and substitutions made by technicians in this field on the basis of the present invention shall fall within the scope of protection required by the present invention.

Claims

1. A welding preheating device, characterized in that: It comprises a support frame (100), an arc-shaped adjustment frame (200), an electric heating plate, a first telescopic rod (300), an adjustment rod (400), a second telescopic rod (500), a first locking member (600) and a second locking member (700), wherein the electric heating plate is laid and fixedly connected to the concave side of the arc-shaped adjustment frame (200); The first end of the first telescopic rod (300) is horizontally telescopically connected to the first end of the support frame (100), and the second end of the first telescopic rod (300) is fixedly connected to the first end of the arc-shaped adjustment frame (200); The first end of the adjusting rod (400) is rotatably connected to the second end of the supporting frame (100), the first end of the second telescopic rod (500) is telescopically connected to the second end of the adjusting rod (400), the second end of the second telescopic rod (500) is rotatably connected to the second end of the arc-shaped adjusting frame (200), the first locking member (600) is used to lock and fix the adjusting rod (400) and the supporting frame (100), and the second locking member (700) is used to lock and fix the adjusting rod (400) and the second telescopic rod (500).

2. The welding preheating device according to claim 1, characterized in that: The arc-shaped adjustment frame (200) is provided with a handle (800), and the first end and the second end of the handle (800) are respectively fixedly connected to the first end and the second end of the arc-shaped adjustment frame (200).

3. The welding preheating device according to claim 2, characterized in that: The second end of the first telescopic rod (300) is fixedly connected to a connecting sleeve (310), and the first end of the handle (800) is inserted into the connecting sleeve (310).

4. The welding preheating device according to claim 1, characterized in that: The support frame (100) comprises a fixed rod (110), and the adjustment rod (400) comprises a first rotating sleeve (410) and an oblique support sleeve (420) which are fixedly connected in a "T" shape, the first rotating sleeve (410) being rotatably sleeved on the outer periphery of the fixed rod (110), the first end of the second telescopic rod (500) being telescopically plugged into the oblique support sleeve (420), the first locking member (600) being used to lock and fix the fixed rod (110) and the first rotating sleeve (410), and the second locking member (700) being used to lock and fix the oblique support sleeve (420) and the second telescopic rod (500).

5. The welding preheating device according to claim 4, characterized in that: The support frame (100) comprises four columns (120), four first support ties (130) connected to the upper ends of the columns (120), and four second support ties (140) connected to the lower ends of the columns (120), one first support ties (130) and one second support ties (140) are connected between each two adjacent columns (120), and both ends of the fixing rod (110) are respectively connected to two of the columns (120) away from the arc-shaped adjustment frame (200).

6. The welding preheating device according to claim 5, characterized in that: Two first telescopic rods (300) are provided, and the two first telescopic rods (300) are respectively telescopically connected to two first supporting tie rods (130) perpendicular to the fixing rod (110).

7. The welding preheating device according to claim 1, characterized in that: The arc-shaped adjustment frame (200) comprises two arc-shaped connecting rods (210) and a mounting rod (220) connected between the two arc-shaped connecting rods (210), and a plurality of the mounting rods (220) are distributed along the length direction of the arc-shaped connecting rods (210).

8. The welding preheating device according to claim 7, characterized in that: The second end of the second telescopic rod (500) is fixedly connected to a second rotating sleeve (510), and the second rotating sleeve (510) is rotatably sleeved on one of the installation rods (220).