Novel micro-concave graphite boat for TopCon coating process

By designing the snap point assembly and the micro-concave square area of ​​the micro-concave graphite boat in the TopCon coating process, the problems of yellowing of the edges of the silicon wafer and gas deposition on the reverse side are solved, and higher fit and coating uniformity are achieved, reducing the Cleaning costs and adverse phenomena in production.

CN221940620UActive Publication Date: 2024-11-01CHUZHOU YIJING PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420200630.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-26
Publication Date
2024-11-01
Estimated Expiration
2034-01-26

AI Technical Summary

Technical Problem

In the TopCon coating process, after the number of times of use of graphite boats increases, the edges of the silicon wafer are prone to yellowing, resulting in groups deposited on the back of the silicon wafer after gas ionization, causing yellowing and winding, affecting the coating effect.

Method used

Design a new micro-concave graphite boat for TopCon coating process, with a snap point assembly and a micro-concave square area on the boat leaf to ensure that the silicon wafer is tightly attached and prevent gas from depositing on the reverse side of the silicon wafer. By setting a jack on the boat leaf In the dot assembly and the microconcave square area, the silicon wafer only deposits gas at the front edge to reduce winding and plating.

Benefits of technology

It effectively reduces the possibility of gas depositing on the reverse side of the silicon wafer, reduces cleaning costs and adverse phenomena in production, improves the uniformity and quality of the coating, and extends the service life of the graphite boat.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221940620U_ABST
    Figure CN221940620U_ABST
Patent Text Reader

Abstract

The utility model discloses a novel micro-concave graphite boat for a TopCon coating process, which comprises a boat blade on which silicon wafers can be arranged in an array; the clamping point assembly is arranged on the boat blade, and the clamping point assembly is used for clamping a silicon wafer; the boat blade is provided with a square area around the sticking point assembly, and a slightly concave square area is formed in the sticking point assembly; the boat blade is located in the middle of the micro-concave square area and is hollow, the clamping point assembly is arranged on the boat blade, a silicon wafer can be conveniently placed on the clamping point assembly, the silicon wafer is tightly attached to the boat blade, the square area and the micro-concave square area are formed around the clamping point assembly, gas deposition can only appear on the side edge and the edge of the front face of the silicon wafer, and the gas deposition efficiency is improved. And gas can be effectively prevented from depositing on the other surface of the silicon wafer after ionization. During continuous production of a production line, compared with an existing graphite boat, the possibility of gas deposition winding plating is reduced from the source, the number and degree of winding plating can be effectively reduced, and the cleaning cost is low.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of solar cells, in particular to a novel micro-concave graphite boat used in a TopCon coating process. Background Art

[0002] Solar cells are semiconductor devices that convert solar energy directly into electrical energy. The core component is the solar cell, also known as the solar cell chip. The preparation process of solar cells mainly includes the steps of cutting silicon ingots, cleaning silicon wafers, coating silicon wafers, diffusion of silicon wafers, etching of silicon wafers, and electrode production of silicon wafers. Among them, the coating of silicon wafers is a key process that affects the performance of solar cells. Its purpose is to form a thin film with high transmittance and low reflectivity on the surface of the silicon wafer to improve the photoelectric conversion efficiency of solar cells.

[0003] In the TopCon process, the graphite boat is a graphite product used to carry silicon wafers. Its structure is similar to a small boat, consisting of multiple graphite boats with a certain interval. There is a narrow gap between each graphite boat for placing silicon wafers. The function of the graphite boat is to form positive and negative electrodes between adjacent graphite boats by applying AC voltage during the coating process, thereby generating glow discharge between the graphite boats, decomposing molecules such as silicon hydride and ammonia in the gas, forming silicon and nitrogen ions, which are deposited on the surface of the silicon wafer to form a TopCon film. The material, structure and size of the graphite boat directly affect the coating effect and conversion efficiency of the silicon wafer. Therefore, the design and manufacture of the graphite boat is an important part of the TopCon process.

[0004] At present, the TopCon process has become the main process for the preparation of photovoltaic solar cells. The graphite boat is an indispensable silicon wafer carrier in the coating stage of the TopCon process. With the increase in the number of times the graphite boat is used, various defects are prone to occur in the appearance after coating, among which the yellowing defect of the silicon wafer edge is more frequent. At present, the number of times the graphite boat is used is generally set at 60-70 times. After the number of uses is reached, the graphite boat will be offline for cleaning. However, after the graphite boat is used multiple times within the specified number of times, the boat leaves will undergo slight deformation, causing the silicon wafer to be unable to fit tightly with the boat leaves, resulting in the deposition of radicals after gas ionization on the B side of the silicon wafer (target A side) during the process, causing yellowing around the plating phenomenon.

[0005] To this end, we propose a new micro-dimpled graphite boat for TopCon coating process. Utility Model Content

[0006] The purpose of the utility model is to provide a new type of micro-dimpled graphite boat for TopCon coating process to solve the problems raised in the above background technology. To achieve the above purpose, the utility model provides the following technical solutions: a new type of micro-dimpled graphite boat for TopCon coating process, comprising:

[0007] A boat blade, on which silicon wafers can be placed in an array;

[0008] A clamping point assembly, the clamping point assembly is arranged on the boat blade, and the clamping point assembly is used to clamp the silicon wafer;

[0009] The boat blade is provided with a square area around the clamping point assembly, and a slightly concave square area is formed in the clamping point assembly;

[0010] The boat blade is located in the middle of the slightly concave square area and is hollow.

[0011] Preferably, the square area sinks by 140 μm, and the slightly concave square area is 184 mm*184 mm.

[0012] Preferably, the boat blade is located in a square area of ​​the card point assembly of 189mm*189mm.

[0013] Preferably, the clamping point assembly further includes a lower clamping point, a side clamping point one and a side clamping point two, and the lengths of the lower clamping point, the side clamping point one and the side clamping point two are between 5.6 mm and 4.3 mm.

[0014] Preferably, the clamping point assembly also includes a lower clamping point, side clamping point one and side clamping point two, all of which are provided with grooves, and the clamping point assembly also includes a lower clamping point, side clamping point one and side clamping point two, which are located in the groove and have a smooth part, a sliding part and a clamping part respectively.

[0015] Preferably, the cross-sectional shapes of the lower clamping point and the side clamping point 1 are circular, the cross-sectional shapes of the side clamping point 2 are elliptical, and the clamping point assembly also includes the lower clamping point, the side clamping point 1 and the side clamping point 2 are all embedded in the boat blade.

[0016] The utility model has at least the following beneficial effects: by setting a card point assembly on the boat blade, it is convenient to place the silicon wafer on the card point assembly, and the silicon wafer is closely attached to the boat blade, and a square area and a slightly concave square area are opened around the card point assembly, so that gas deposition can only occur on the side and the front edge of the silicon wafer, which can effectively prevent the gas from being ionized and deposited on the other side of the silicon wafer. When the production line is in continuous production, compared with the existing graphite boat, the possibility of gas deposition plating is reduced from the source, the number and degree of plating can be effectively reduced, and the cleaning cost is low. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0018] Figure 2 This is a schematic diagram of the boat-blade structure of the utility model;

[0019] Figure 3 This is a schematic diagram of the structure of the practical card point component;

[0020] Figure 4 This is a schematic diagram of the card point structure for this practical application;

[0021] Figure 5 This is a schematic diagram of the structure of the second side card point of this utility model;

[0022] In the figure: 1, boat blade; 2, clamping point assembly; 21, lower clamping point; 22, side clamping point one; 23, side clamping point two; 31, groove; 32, smooth part; 33, sliding part; 34, clamping part. DETAILED DESCRIPTION

[0023] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0024] See also Figure 1-5 The utility model provides a technical solution: a new type of micro-dimpled graphite boat for TopCon coating process, comprising:

[0025] A boat blade 1, on which silicon wafers can be placed in an array;

[0026] A clamping point assembly 2, wherein the clamping point assembly 2 is arranged on the boat blade 1, and the clamping point assembly 2 is used to clamp the silicon wafer;

[0027] The boat blade 1 is provided with a square area around the card point component 2, and a slightly concave square area is formed in the card point component 2. The boat blade 1 is hollow in the middle of the slightly concave square area. By providing the card point component 2 on the boat blade 1, it is convenient to place the silicon wafer on the card point component 2, and the silicon wafer is closely attached to the boat blade. The square area and the slightly concave square area are provided around the card point component 2, so that gas deposition only occurs on the side and the front edge of the silicon wafer, which can effectively prevent the gas from being ionized and deposited on the other side of the silicon wafer. When the production line is in continuous production, compared with the existing graphite boat, the possibility of gas deposition plating is reduced from the source, which can effectively reduce the number and degree of plating, and the cleaning cost is low.

[0028] The square area sinks 140μm, and the micro-concave square area is 184mm*184mm. By setting the square area sinking 140μm and the micro-concave square area 184mm*184mm on the boat blade 1, such a design can also form a tiny depression between the central part of the silicon wafer and the central part of the graphite boat, thereby increasing the contact area between the central part of the silicon wafer and the central part of the graphite boat, thereby improving the fit between the silicon wafer and the graphite boat, reducing the movement or warping of the silicon wafer during the coating process, and improving the coating uniformity and quality of the silicon wafer. Such a design can also adapt to the current mainstream silicon wafer size of 182~184, improve the versatility and adaptability of the graphite boat, and reduce the production cost and replacement frequency of the graphite boat.

[0029] The boat blade 1 is located in the card point component 2, and the square area is 189mm*189mm. The boat blade 1 is located in the card point component 2, and the square area is 189mm*189mm. Such a design can form a tiny gap between the edge of the silicon wafer and the edge of the graphite boat, thereby avoiding arc discharge between the edge of the silicon wafer and the edge of the graphite boat, resulting in the deposition of ionized gas radicals on the B side of the silicon wafer, causing yellowing plating phenomenon.

[0030] The clamping point assembly 2 also includes a lower clamping point 21, a side clamping point 1 22 and a side clamping point 23. The lengths of the lower clamping point 21, the side clamping point 1 22 and the side clamping point 23 are between 5.6 mm and 4.3 mm to strengthen the prevention of silicon wafers from falling off when a mechanical arm fails.

[0031] The clamping point assembly 2 also includes a lower clamping point 21, a side clamping point 1 22 and a side clamping point 23, all of which are provided with grooves 31. The clamping point assembly 2 also includes a lower clamping point 21, a side clamping point 1 22 and a side clamping point 23, which are located in the groove 31 and have a smooth portion 32, a sliding portion 33 and a clamping portion 34 in sequence. The design of the smooth portion 32 can prevent the silicon wafer from entering the groove 31 and being scratched or causing the silicon wafer to break. The design of the sliding portion 33 facilitates the stable sliding of the silicon wafer while increasing the depth of the groove 31, which can effectively prevent the silicon wafer from escaping from the groove 31 during the movement of the graphite boat. The design of the clamping portion 34 can cooperate with the inner wall of the boat blade 1 to clamp the edge of the silicon wafer.

[0032] The cross-sectional shapes of the lower clamping point 21 and the side clamping point 1 22 are circular, and the side clamping point 23 is elliptical. The clamping point assembly 2 also includes the lower clamping point 21, the side clamping point 1 22 and the side clamping point 23, all of which are embedded in the boat blade 1. When the specifications of the silicon wafer are small, the angle of the side clamping point 23 can be adjusted so that the groove 31 on the side clamping point 23 is close to the silicon wafer, so that the side clamping point 23 cooperates with the lower clamping point 21 and the side clamping point 1 22 to clamp the silicon wafer, thereby preventing the silicon wafer from escaping from the groove 31 during the movement of the graphite boat.

[0033] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0034] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A novel micro-dimpled graphite boat for TopCon coating process, characterized in that: include: A boat blade (1), on which silicon wafers can be placed in an array; A clamping point assembly (2), the clamping point assembly (2) being arranged on the boat blade (1), and the clamping point assembly (2) being used to clamp the silicon wafer; The boat blade (1) is provided with a square area around the clamping point assembly (2), and a slightly concave square area is formed in the clamping point assembly (2); The boat blade (1) is located in the middle of the slightly concave square area and is hollow.

2. The novel micro-dimpled graphite boat for TopCon coating process according to claim 1, characterized in that: The square area is sunken by 140 μm, and the slightly concave square area is 184 mm*184 mm.

3. The novel micro-dimpled graphite boat for TopCon coating process according to claim 2, characterized in that: The square area where the boat blade (1) is located at the clamping point assembly (2) is 189 mm*189 mm.

4. The novel micro-dimpled graphite boat for TopCon coating process according to claim 1, characterized in that: The clamping point assembly (2) further comprises a lower clamping point (21), a first side clamping point (22) and a second side clamping point (23); the lengths of the lower clamping point (21), the first side clamping point (22) and the second side clamping point (23) are between 5.6 mm and 4.3 mm.

5. The novel micro-dimpled graphite boat for TopCon coating process according to claim 4, characterized in that: The clamping point assembly (2) further comprises a lower clamping point (21), a first side clamping point (22) and a second side clamping point (23), each of which is provided with a groove (31); the clamping point assembly (2) further comprises a lower clamping point (21), a first side clamping point (22) and a second side clamping point (23), which are located in the groove (31) and have a smooth portion (32), a sliding portion (33) and a clamping portion (34) in sequence.

6. The novel micro-dimpled graphite boat for TopCon coating process according to claim 5, characterized in that: The cross-sectional shapes of the lower clamping point (21) and the side clamping point one (22) are circular, and the side clamping point two (23) is elliptical. The clamping point assembly (2) further comprises the lower clamping point (21), the side clamping point one (22) and the side clamping point two (23), all of which are embedded in the boat blade (1).