Combined brick for rotary kiln
By using wedge-shaped composite bricks in the rotary kiln and filling the low-thermal conductivity nanoplate at their connections, the problems of short life and high heat consumption of refractory masonry are solved, and temperature reduction and life extension are achieved, achieving energy-saving and environmentally friendly effects.
Patent Information
- Application Number
- CN202323329420.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-07
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-07
AI Technical Summary
The rotary kiln refractory masonry has a short life and high heat consumption, so it is difficult for the prior art to effectively reduce the surface temperature of the cylinder and extend the service life.
A wedge-shaped composite brick is designed, using low-thermal conductivity nanoplate as the insulation layer, and the connection between the refractory brick and the pad is filled with low-thermal conductivity thermal insulation material to form an integral brick body, reducing heat conduction and enhancing the strength of the brick body.
It greatly reduces the surface temperature of the rotary kiln barrel, extends the service life of refractory materials, saves fuel consumption, and achieves energy saving, carbon reduction and pollution reduction.
Smart Images

Figure CN221944902U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the application field of rotary kilns, in particular to a combined brick for rotary kilns. Background Art
[0002] The utility model is to leave a gap on the side of the heavy refractory brick close to the rotary kiln shell, and embed a thin nano-plate heat insulation material during masonry to form a combined brick. Under the premise of not reducing the strength and service life of the heavy brick, the heat insulation effect can be enhanced, the surface temperature of the shell can be greatly reduced, the heat dissipation loss can be reduced, the fuel consumption can be saved, and the energy-saving and environmentally friendly effects can be achieved.
[0003] The biggest disadvantage of rotary kiln is the high surface temperature of the cylinder, large heat dissipation, high energy consumption and short service life of refractory masonry. The reason is determined by the characteristics of rotary kiln: the cylinder of rotary kiln is always in a rotating state when working, which requires the internal refractory lining to have a certain strength and firmness, and must be seamless and close to the cylinder. In order to prevent the refractory lining from loosening and falling and extend the service life, the refractory lining is built with heavy bricks or heavy high-strength castables + lightweight insulation castables. The thickness is generally thinner than other industrial kilns, and ceramic fibers, calcium silicate boards and other refractory materials with good insulation performance and low compressive strength cannot be used. Despite this, the use of heavy bricks often causes the bricks to crack and peel off due to excessive internal thermal stress, which eventually leads to the loosening and falling of heavy bricks. The refractory masonry needs to be repaired after about 2 years of use; the use of heavy high-strength castables + lightweight insulation castables can reach a service life of more than 3 years, but it is difficult to dismantle during overhaul and the construction period is long.
[0004] Later, a composite brick masonry method emerged: the working layer still uses heavy bricks made of magnesium-aluminum spinel and high-aluminum materials; the non-working layer close to the cylinder uses materials with lower thermal conductivity, and the two materials are pressed together to form an integral composite brick. The use of this composite brick has extended the service life of the refractory masonry to a certain extent and reduced the surface temperature of the cylinder, but the cylinder temperature is still between 250-350℃.
[0005] The utility model is a new type of combined brick for a rotary kiln designed in view of the current situation, which solves the two major problems of short life of the refractory masonry of the rotary kiln and high heat consumption. Utility Model Content
[0006] The purpose of the utility model is to provide a composite brick for a rotary kiln in view of the above problems.
[0007] The purpose of the utility model is achieved as follows: a combination brick for a rotary kiln, the combination brick is a wedge-shaped brick, the wedge-shaped brick is a quadrangular platform as a whole, the top width of the quadrangular platform is 90-120mm, the length is 200-400mm, the bottom width of the quadrangular platform is 100-130mm, the length is 200-400mm, the height of the quadrangular platform is 230-260mm, the side length of the quadrangular platform slope is 1.5-3m, the left and right sides below the quadrangular platform are provided with pads, the pad width is 35-45mm, the pad height is 5-10mm, and a heat insulation layer is provided at the contact surface between the combination brick and the inner wall of the rotary kiln.
[0008] The heat insulation layer is a nano plate with low thermal conductivity.
[0009] A low thermal conductivity nanoplate is arranged at the connection between the quadrangular platform of the combined brick and the cushion block.
[0010] The beneficial effects of the utility model are as follows: (1) the surface temperature of the rotary kiln cylinder is greatly reduced, the average temperature is reduced from 280°C to below 170°C, and the heat dissipation loss is reduced by about 45%. (2) The service life of the rotary kiln refractory masonry is extended, and the overhaul cycle is extended from 2 years to more than 4 years. (3) Local maintenance and overhaul are convenient, and the refractory bricks are easy to remove during overhaul. (4) It is suitable for refractory bricks of different materials in the high temperature section, medium temperature section and low temperature section of rotary kilns for any purpose. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The utility model is further described below in conjunction with the accompanying drawings.
[0012] Figure 1 It is a side view of the utility model.
[0013] Figure 2 It is the front view of the utility model.
[0014] Figure 3 It is the longitudinal section diagram of the combined brick masonry: it shows the cross-sectional shape of the combined brick masonry along the length direction of the kiln chamber.
[0015] Figure 4 It is a cross-sectional view of combined brick masonry: it shows the cross-sectional shape of the combined brick masonry in the cross section of the kiln chamber.
[0016] Among them: 1. Working layer, 2. Inner wall of rotary kiln, 3. Insulation layer, 4. Combined bricks. Implementation
[0017] The utility model is suitable for rotary kilns of any purpose, such as cement rotary kilns, lime rotary kilns, dolomite rotary kilns, sintering rotary kilns, drying rotary kilns, high-temperature magnesia-calcium sand rotary kilns, etc., and refractory composite bricks and masonry of various materials are used in the kilns.
[0018] The utility model solves two major problems of the rotary kiln at the same time.
[0019] (1) Extending the service life of refractory masonry: Refractory bricks of different materials are selected for the high temperature section, medium temperature section and low temperature section according to the different temperatures of each section, but the entire thickness from the shell to the working layer is built with a whole brick, which is equivalent to only one layer, which is dense and firm with good integrity.
[0020] (2) Reduce the surface temperature of the cylinder and save energy and reduce consumption: Low thermal conductivity nanoplate insulation material is used as an insulation layer to significantly reduce the heat conducted to the shell, lower the shell temperature, reduce heat dissipation losses, save fuel consumption, and achieve energy conservation, carbon reduction, and pollution reduction.
[0021] Solving these two problems is equivalent to solving the two major shortcomings of the rotary kiln.
[0022] The technical solution of the utility model is as follows.
[0023] (1) Design of refractory brick dimensions: As shown in the figure, the refractory brick is a wedge-shaped brick with the outer dimension A larger than the inner dimension B, and the arc radius R is determined according to the cylinder diameter; dimension C refers to the length of the brick, dimension D refers to the thickness of the brick, and dimension E is designed according to the material, compressive strength and production requirements of the brick. It is as small as possible under the condition of meeting the heat load, so as to increase dimension F accordingly; dimension G is calculated according to the kiln chamber temperature, the thermal conductivity of the material, the thickness of the brick, and the shell surface temperature. In principle, it is as small as possible to enhance the strength of the refractory brick. The materials of the composite bricks are different according to the use temperature and environment: corundum mullite bricks, magnesia bricks, magnesia-alumina spinel bricks, high-alumina bricks, clay bricks, etc. The insulation layer is a low thermal conductivity nanoplate. The joint between the four-sided platform of the composite brick and the pad is filled with low thermal conductivity insulation materials and low thermal conductivity nanoplates, which can also be high-efficiency composite insulation coatings.
[0024] The gap A×F×G left by the refractory bricks is used to fill the low thermal conductivity insulation material during masonry. The size design of the refractory bricks is very important. It should not affect the overall strength of the bricks, but also increase the insulation layer area as much as possible to minimize heat loss.
[0025] (2) Refractory brick masonry: Figure 3 and Figure 4 Shown are the longitudinal section and cross section of the combined brick masonry, respectively. First, fill the gap left by each refractory brick with the low thermal conductivity insulation board, and then, in the same way as normal masonry, the refractory bricks are connected to the insulation board and laid at the same time.
[0026] Taking a 1000 t / d lime rotary kiln as an example, the dimensions of the combined bricks are as shown in the following table.
[0027]
[0028] After the combination of bricks and low thermal conductivity nano-plates was used, the average surface temperature of the cylinder was reduced from 280°C to 170°C, which directly brought about beneficial effects of energy saving and environmental protection: (1) Energy saving: The average surface temperature of the cylinder was reduced from 280°C to 170°C, and the heat dissipation per unit area was reduced from 5199 W / m 2 Reduced to 3001W / m 2 . Shell area is about 1002m 2 , reduce heat loss: (5199-3001) × 1002 × 10 -3 ≈2242kW≈1.931×10 6 kCal / h, equivalent to about 276kg / h of standard coal. Based on an annual working time of 330 days, about 2,186 tons of standard coal can be saved each year. (2) Environmental protection: Reducing the combustion consumption of 2,186 tons of standard coal each year can reduce carbon dioxide emissions by about 5,686 tons, and can also reduce sulfur dioxide and nitrogen oxide emissions.
[0029] The above description is only a specific embodiment of the present invention, but the structural features of the protection scope of the present invention are not limited thereto. Any changes or modifications made by any technician in the field of the present invention are included in the patent scope of the present invention.
Claims
1. A combined brick for a rotary kiln, characterized in that: The combined brick is a wedge-shaped brick, which is a quadrangular platform as a whole. The top width of the quadrangular platform is 90-120mm, the length is 200-400mm, the bottom width of the quadrangular platform is 100-130mm, the length is 200-400mm, the height of the quadrangular platform is 230-260mm, the side length of the inclined surface of the quadrangular platform is 1.5-3m, and pads are arranged on both sides of the bottom of the quadrangular platform. The pads are 35-45mm wide and 5-10mm high. A heat insulation layer is arranged at the contact surface between the combined brick and the inner wall of the rotary kiln.
2. The combined brick for rotary kiln according to claim 1, characterized in that: The heat insulation layer is a nano plate with low thermal conductivity.
3. The combined brick for rotary kiln according to claim 1, characterized in that: A low thermal conductivity nanoplate is arranged at the connection between the quadrangular platform of the combined brick and the cushion block.