Combined mark structure for improving laser dry etching precision of silver paste

By setting cross-combination alignment marks on the film sheet, the combined marking method between ITO and silver paste is realized, which solves the problem of large tolerance between silver paste and ITO during the ITO screen printing process, and improves the accuracy and recognition accuracy of silver paste laser drying.

CN221967044UActive Publication Date: 2024-11-08TRULY OPTO ELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323408394.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-13
Publication Date
2024-11-08
Estimated Expiration
2033-12-13

AI Technical Summary

Technical Problem

During the ITO screen printing process, the tolerance between silver paste and ITO is large, resulting in a deviation in the drying moment. The existing technology reduces the tolerance by grasping the ITO mark, but this will cause the tolerance of the silver paste block to become larger, affecting the laser drying Engraving accuracy.

Method used

Design a combination mark structure, by setting cross-combination marks on the film sheet, the horizontal mark and the vertical mark form a "cross" shape, and use the horizontal mark or vertical mark as marks as needed to achieve ITO and silver paste Combining the standard method reduces tolerances and improves laser drying accuracy.

Benefits of technology

By combining the standard structure, the up and down directions of the laser dry etching line are controlled to prevent the ITO from being biased, the tolerance is reduced, and the accuracy of the laser dry etching line on the silver paste block is improved, so as to achieve higher recognition accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221967044U_ABST
    Figure CN221967044U_ABST
Patent Text Reader

Abstract

A combination mark structure for improving silver paste laser dry etching precision comprises a film which comprises a film sheet; an electrode is arranged on one side of the film, a silver paste electrode is arranged on the side, close to the film, of the electrode and located on the front face of the film, and two cross-shaped combination alignment marks are arranged on the film. According to the combined mark structure capable of improving the silver paste laser dry etching precision, a simple silver paste mark grabbing mode or an ITO mark grabbing mode is changed into a combined mark grabbing mode of a transverse silver paste mark and a vertical ITO mark, so that transverse ITO control ensures that ITO cannot be etched in the vertical direction of a laser dry etching line, the laser dry etching line has only one tolerance relative to the ITO at the moment, and therefore the precision of the silver paste laser dry etching is improved. And the vertical silver paste strengthens and controls the precision of the laser dry etching line relative to the silver paste in the left-right direction during laser dry etching, and at the moment, the laser dry etching line has only one tolerance relative to the silver paste block.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of films, in particular to a combined mark structure for improving the precision of silver paste laser dry engraving. Background Art

[0002] At present, for the current film, for ITO routing, the binding position uses a whole piece of silver paste for silk screen printing and dry engraving. There are generally two ways to grab the mark: 1. Make a silver paste mark and grab the silver paste mark during laser dry engraving; 2. Make an ITO mark and grab the ITO mark during laser dry engraving. ITO is the first to be silk-screened on the film. Because the silver paste has a tolerance relative to ITO when silk-screen printing, if the silver paste silk-screen mark is grabbed during dry engraving, the tolerance of the dry engraved line relative to ITO will be larger (equal to the silk-screen tolerance of the silver paste relative to ITO plus the tolerance of the dry engraved line relative to the silver paste, two cumulative tolerances). Therefore, we usually dry-etch the silver paste by grabbing the ITO mark, so that there is only one dry engraved line with a tolerance relative to ITO, which avoids the dry engraved line from damaging the ITO. However, grabbing the ITO mark alone will cause the tolerance of the dry engraved line relative to the silver paste block to become larger. Because the ITO mark is used as the benchmark, the dry engraved line relative to the silver paste needs to be added with the silk screen tolerance of the silver paste relative to ITO. Therefore, in order to reduce the tolerance, a combined mark structure is designed to improve the accuracy of silver paste laser dry engraving. The mark is grasped by combining the ITO mark and the silver paste table, thereby reducing the tolerance. Utility Model Content

[0003] The utility model aims to overcome the shortcomings of the prior art and provide a combined mark structure for improving the precision of silver paste laser dry engraving.

[0004] The purpose of this utility model is achieved through the following technical solutions:

[0005] A combined mark structure for improving the accuracy of silver paste laser dry engraving includes: a film, wherein the film includes a film sheet; an electrode is arranged on one side of the film sheet, a silver paste electrode is arranged on one side of the film sheet close to the electrode and located on the front side of the film sheet, and two cross combined alignment marks are arranged on the film sheet.

[0006] In one of the embodiments, silver paste is disposed in the center of the film, the front surface of the silver paste is circular in shape, and the silver paste electrodes are all located in the inner diameter of the silver paste.

[0007] In one of the embodiments, the front side of the film is in a square shape, and the diameter of the silver paste is adapted to the length of the film.

[0008] In one embodiment, two cross combination alignment marks are respectively designed on the left side of the top of the front side of the film and on the right side of the bottom of the front side, and the cross combination alignment mark includes a horizontal mark and a vertical mark.

[0009] In one embodiment, the horizontal mark and the vertical mark are perpendicular to each other to form a "cross" shape, and when the horizontal mark is a silver paste mark, the vertical mark is an ITO mark, and when the horizontal mark is an ITO mark, the vertical mark is a silver paste mark.

[0010] In one embodiment, the electrode is located at the center of the left side of the film, and the electrode is electrically connected to one side of the silver paste electrode.

[0011] In one embodiment, the silver paste electrode and the silver paste are formed at one time by laser dry etching of silver paste.

[0012] In one embodiment, the width of the horizontal mark and the vertical mark is between 0.02 mm and 0.08 mm.

[0013] In one embodiment, the cross combination alignment mark and the silver paste electrode are located at the same horizontal plane.

[0014] In one of the embodiments, the side of the front surface of the silver paste electrode away from the electrode is an irregular ring.

[0015] Compared with the prior art, the utility model has at least the following advantages:

[0016] The utility model improves the precision of silver paste laser dry engraving by changing the simple silver paste mark or ITO mark to a combination mark method of grabbing horizontal silver paste mark (or ITO mark) and vertical ITO mark (or silver paste mark) (the simple silver paste mark or ITO mark is changed to a combination mark method of grabbing horizontal silver paste mark (or ITO mark) and vertical ITO mark (or silver paste mark), with the manual attached Figure 1 For example, because we need to ensure the upper and lower widths of ITO at the binding position, we need to control the dry engraving lines in the upper and lower directions of ITO, so the horizontal direction is the ITO mark). Therefore, the horizontal ITO control ensures that the laser dry engraving line will not deviate from the ITO in the upper and lower directions. At this time, the laser dry engraving line has only one tolerance relative to ITO, and the vertical silver paste strengthens the control of the laser dry engraving. The accuracy of the laser dry engraving line in the left and right directions relative to the silver paste. At this time, the laser dry engraving line has only one tolerance relative to the silver paste block, so that the combined mark structure that improves the accuracy of silver paste laser dry engraving achieves the purpose of reducing tolerance and improving recognition accuracy. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.

[0018] Figure 1 It is a schematic diagram of the overall structure of the front side of the utility model. DETAILED DESCRIPTION

[0019] In order to facilitate the understanding of the present invention, the present invention will be described more comprehensively with reference to the relevant drawings. The drawings provide preferred embodiments of the present invention. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly and comprehensively understood.

[0020] In the description of the present application, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0021] Unless otherwise clearly stipulated and limited, terms such as "installed", "connected", "connected", "fixed", etc. should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements.

[0022] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0023] like Figure 1 As shown, a combined mark structure for improving the precision of silver paste laser dry engraving includes: film 1, film 1 includes film sheet 11; an electrode 13 is arranged on one side of film sheet 11, a silver paste electrode 15 is arranged on one side of electrode 13 close to film sheet 11 and located on the front of film sheet 11, and two cross combined alignment marks 12 are arranged on film sheet 11. It should be noted that this technical solution controls the horizontal and vertical precision of the binding position through horizontal silver paste mark (or ITO mark) and vertical ITO mark (or silver paste mark), and proposes the concept of combined mark, so as to improve the precision.

[0024] like Figure 1As shown, in one embodiment, a silver paste 14 is disposed in the center of the film 11, the front of the silver paste 14 is circular, and the silver paste electrodes 15 are all located in the inner diameter of the silver paste 14. The silver paste electrodes 15 and the silver paste 14 are formed at one time by laser dry etching of the silver paste. The side of the front of the silver paste electrode 15 away from the electrode 13 is an irregular ring.

[0025] like Figure 1 As shown, in one embodiment, the front side of the film 11 is in a square shape, and the diameter of the silver paste 14 matches the length of the film 11. It should be noted that this design allows the silver paste 14 to occupy the entire area of ​​the film 11.

[0026] like Figure 1 As shown, in one embodiment, two cross combination alignment marks 12 are respectively designed on the left side of the top of the front side of the film 11 and on the right side of the bottom of the front side, and the cross combination alignment mark 12 includes a horizontal mark 121 and a vertical mark 122. The horizontal mark 121 and the vertical mark 122 are perpendicular to each other to form a "cross" shape. When the horizontal mark 121 is a silver paste mark, the vertical mark 122 is an ITO mark. When the horizontal mark 121 is an ITO mark, the vertical mark 122 is a silver paste mark. It should be noted that whether the horizontal mark is an ITO mark or the vertical mark is an ITO mark depends on the placement of the product drawing, that is, the control of the dry engraving line, as shown in the attached manual. Figure 1 Because we need to ensure the upper and lower widths of the ITO at the binding position, we need to control the dry lines in the upper and lower directions of the ITO, so the horizontal direction is the ITO mark.

[0027] like Figure 1 As shown, in one embodiment, the electrode 13 is located at the center of the left side of the film 11, and the electrode 13 is electrically connected to one side of the silver paste electrode 15. It should be noted that the electrode 13 is also electrically connected to the silver paste 14.

[0028] like Figure 1 As shown, in one embodiment, the width of the horizontal mark 121 and the vertical mark 122 is between 0.02 mm and 0.08 mm.

[0029] like Figure 1 As shown in one embodiment, the cross combination alignment mark 12 and the silver paste electrode 15 are located at the same horizontal plane. It should be noted that when laser dry engraving is performed on the silver paste electrode 15, the cross combination alignment mark 12 needs to be grasped for alignment first.

[0030] The above-mentioned embodiments only express several implementation methods of the utility model, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the utility model patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the utility model, which all belong to the protection scope of the utility model. Therefore, the protection scope of the utility model patent shall be based on the attached claims.

Claims

1. A combined mark structure for improving the accuracy of silver paste laser dry engraving. It is characterized in that include: Film (1), wherein the film (1) comprises a film sheet (11); An electrode (13) is provided on one side of the film sheet (11), a silver paste electrode (15) is provided on one side of the electrode (13) close to the film sheet (11) and located on the front side of the film sheet (11), and two cross combination alignment marks (12) are provided on the film sheet (11).

2. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 1, It is characterized in that A silver paste (14) is arranged at the center of the film (11); the front of the silver paste (14) is circular in shape, and the silver paste electrodes (15) are all located in the inner diameter of the silver paste (14).

3. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 2, It is characterized in that The front side of the film sheet (11) is in a square shape, and the diameter of the silver paste (14) is adapted to the length of the film sheet (11).

4. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 1, It is characterized in that The two cross combination alignment marks (12) are respectively designed on the left side of the top of the front side of the film sheet (11) and on the right side of the bottom of the front side. The cross combination alignment mark (12) comprises a horizontal mark (121) and a vertical mark (122).

5. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 4, It is characterized in that The horizontal mark (121) and the vertical mark (122) are perpendicular to each other to form a "cross" shape. When the horizontal mark (121) is a silver paste mark, the vertical mark (122) is an ITO mark, and when the horizontal mark (121) is an ITO mark, the vertical mark (122) is a silver paste mark.

6. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 1, It is characterized in that The electrode (13) is located at the center of the left side of the film (11), and the electrode (13) is electrically connected to one side of the silver paste electrode (15).

7. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 2, It is characterized in that The silver paste electrode (15) and the silver paste (14) are formed at one time by laser dry etching of silver paste.

8. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 4, It is characterized in that The width of the horizontal mark (121) and the vertical mark (122) is between 0.02 mm and 0.08 mm.

9. The combined marking structure for improving the precision of silver paste laser dry engraving according to claim 1, It is characterized in that The cross combination alignment mark (12) and the silver paste electrode (15) are located on the same horizontal plane.

10. The combined mark structure for improving the precision of silver paste laser dry engraving according to claim 1, It is characterized in that The front side of the silver paste electrode (15) away from the electrode (13) is in an irregular ring shape.