Cover plate assembly for single battery and single battery

By designing multiple through holes and annular dissolving membranes on the cover plate of the single-cell battery, ensuring uniform sharing of electrolyte and gas, the problems of different performance of single-cell batteries and low reliability of shared pipeline components in large-capacity batteries are solved, and the problem of low reliability of shared pipeline components is improved. Battery performance and production efficiency.

CN221978066UActive Publication Date: 2024-11-08D AUS ENERGY STORAGE TECH (XIAN) CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323340963.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-08
Publication Date
2024-11-08
Estimated Expiration
2033-12-08

AI Technical Summary

Technical Problem

The performance differences in single cells in existing large-capacity batteries lead to limited overall capacity and cycle times, and the reliability of shared pipeline components is low, affecting battery performance.

Method used

Design a cover plate assembly for single-cell batteries, including at least two through holes and a sealing assembly, and removes the sealing assembly or forms a through hole through holes through external force or electrolyte to ensure the communication between the single-cell and the shared pipeline assembly, and adopts annular shape. Dissolve the membrane and protective membrane for sealing and fixing, improving shared effects and production efficiency.

Benefits of technology

The electrolyte and gas uniformity between single cells is improved, the cycle life and production efficiency of large-capacity batteries is enhanced, and manufacturing costs are reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221978066U_ABST
    Figure CN221978066U_ABST
Patent Text Reader

Abstract

The utility model aims to provide a cover plate assembly for a single battery and the single battery. And the problem of low sharing reliability of the existing high-capacity battery is solved. The cover plate assembly comprises a cover plate and a sealing assembly; at least two through holes are formed in the cover plate; the sealing assembly is fixed on the cover plate and seals the through hole; through external force or external electrolyte, the sealing assembly can fall off from the cover plate or an opening penetrating through the through hole is formed in the sealing assembly. According to the utility model, at least two through holes are formed in the cover plate, when one through hole cannot be opened, the rest through holes can be opened, so that the inner cavities of the single batteries are communicated with the inner cavity of the shared pipeline assembly, and the sharing success rate is improved; besides, when all the through holes are opened, compared with a structure which is shared only through one through hole, the electrolyte and / or gas in the inner cavity of the single battery can be fully and uniformly mixed with the electrolyte and / or gas in the inner cavity of the shared pipeline assembly, so that a better sharing effect is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the field of batteries, in particular to a cover plate assembly for a single cell battery and a single cell battery. Background Art

[0002] Currently, many single cells are connected in parallel or in series on the market to form large-capacity batteries (also called battery modules or battery packs).

[0003] However, the individual cells in existing large-capacity batteries are different from each other. Due to the existence of the barrel effect, they are often affected by the cell with the worst performance, which greatly limits the capacity limit and cycle times of the entire large-capacity battery. Therefore, how to improve the uniformity of each cell in a large-capacity battery has become the focus and difficulty of research in this field.

[0004] In order to solve the above problems, Chinese patent CN219892382U discloses a large-capacity battery, such as Figure 1 As shown, the electrolyte areas of all single cells 03 are connected by a first hollow component 01 fixed at the bottom of each single cell, and the gas areas of all single cells 03 are connected by a second hollow component 02 fixed at the top of each single cell. The first hollow component 01 can place each single cell 03 in a uniform electrolyte environment, thereby ensuring the uniformity of the electrolyte in each single cell 03. The second hollow component 02 achieves gas balance in each single cell 03, thereby improving the performance and charge and discharge cycle life of large-capacity batteries.

[0005] Usually, the first hollow member 01 can be connected to the electrolyte area of ​​all the single cells by opening the sealing assembly sealed at the through hole of the lower cover plate of the single cell 03. The second hollow member 02 can be connected to the gas area of ​​all the single cells by opening the sealing assembly sealed at the through hole of the upper cover plate of the single cell 03.

[0006] Based on the functions of the first hollow member and the second hollow member, they can be collectively referred to as a shared pipeline assembly. Because the first hollow member is connected to the electrolyte area of ​​all the single cells, it can be further referred to as an electrolyte shared pipeline assembly, and correspondingly, the second hollow member can be referred to as a gas shared pipeline assembly.

[0007] The above patent only provides one through hole in the single cell cover. During the unpacking process, if the sealing assembly sealed on the through hole cannot be opened due to misoperation or other factors, the inner cavity of the single cell will be unable to communicate with the shared pipeline assembly, and the electrolyte or gas environment of the single cell cannot be guaranteed to be consistent with that of other single cells, affecting the sharing effect and ultimately affecting the performance of the large-capacity battery. Utility Model Content

[0008] The purpose of the utility model is to provide a cover plate assembly for a single cell battery and a single cell battery, so as to overcome the problem of low reliability of existing large-capacity battery sharing.

[0009] The technical solution of the utility model is to provide a cover plate assembly for a single cell, which is special in that it comprises a cover plate and a sealing assembly;

[0010] The cover plate is provided with at least two through holes;

[0011] The sealing assembly is fixed on the cover plate and seals the through hole;

[0012] The sealing component can be detached from the cover plate or an opening through the through hole can be formed in the sealing component by external force or external electrolyte.

[0013] The utility model has at least two through holes on the cover plate. When one of the through holes cannot be opened, the remaining through holes can be opened to allow the inner cavity of the single cell and the inner cavity of the shared pipeline assembly to be connected, thereby improving the sharing success rate. In addition, when all the through holes of the utility model are opened, compared with a structure that shares through only one through hole, the electrolyte and / or gas in the inner cavity of the single cell can be fully mixed with the electrolyte and / or gas in the inner cavity of the shared pipeline assembly, thereby achieving a better sharing effect.

[0014] Furthermore, there are two through holes, which are symmetrically arranged on the cover plate along the length direction of the cover plate, which can not only ensure the overall strength of the cover plate before opening the package, but also improve the sharing effect of each single battery after opening the package.

[0015] Furthermore, the sealing assembly includes a protective film and a dissolving film; the protective film is in sheet form and covers the through hole; the dissolving film is in ring form and is fixed to the outer surface area of ​​the cover plate around the edge of the protective film and the through hole, and the protective film is fixed to the cover plate;

[0016] The material of the dissolving film is a material soluble in the electrolyte, and the material of the protective film is a material insoluble in the electrolyte.

[0017] The protective film is fixed on the battery shell by an annular dissolving film, and the dissolving film can well seal the gap between the protective film and the shell area around the through hole; at the same time, the electrolyte in the inner cavity of the single battery shell is in direct contact with the protective film, but cannot contact the dissolving film located on the outer surface of the shell, so that during the assembly process of the large-capacity battery (before unpacking), the through-hole parts of each single battery have good sealing performance; during the unpacking process, the electrolyte is injected into the shared pipeline assembly, and under the action of the electrolyte, the dissolving film melts, and the protective film falls off from the single battery shell, thereby connecting the inner cavity of each single battery shell with the inner cavity of the shared pipeline assembly. Because the utility model adopts an annular dissolving film, under the condition of the same outer diameter, the annular dissolving film has a smaller area than the circular dissolving film (the dissolving film in the background technology), therefore, compared with the dissolving film in the background technology, the dissolving time of the utility model is shorter, which can shorten the preparation time of the large-capacity battery and improve the production efficiency. In addition, the dissolving film of the utility model serves as a sealing component and a fixing mechanism at the same time, and there is no need to introduce an additional fixing mechanism of the sealing component, so that the overall structure of the sealing component is simple and the manufacturing cost is low.

[0018] Furthermore, the dissolving film is fixed on the outer surface area of ​​the cover plate around the edge of the protective film and the through hole by casting. Generally, a hot-melt slurry soluble in electrolyte can be cast on the outer surface area of ​​the cover plate around the edge of the protective film and the through hole, and after cooling, a dissolving film can be formed, which can achieve sealing and fix the protective film on the cover plate.

[0019] Furthermore, the material of the dissolving film is PS (polystyrene), PMMA (polymethyl methacrylate), SMMA (styrene dimethyl methacrylate copolymer), TPU (thermoplastic polyurethane), ABS (acrylonitrile / butadiene / styrene copolymer), POM (polyoxymethylene), PA6 (nylon 6), PA12 (nylon 12) or PVC (polyvinyl chloride).

[0020] Furthermore, the material of the protective film is aluminum, copper, zinc, nickel, silver, epoxy resin, PE (polyethylene), PP (polypropylene), polytetrafluoroethylene or EPDM rubber.

[0021] Further, the through hole is a stepped through hole, and the large hole is located on the outer surface of the cover plate;

[0022] The protective film is located in the macropore, and a second step structure is provided at the edge of the protective film along its circumference, so that the dissolving film can be fixed to it by means of stopper matching, which can improve the bonding strength between the two and further improve the sealing reliability of this part. A dissolving film installation space is formed between the protective film, the step surface of the step through hole and the wall of the macropore; the dissolving film is fixed in the dissolving film installation space. Through such an arrangement, the outer surface of the cover plate assembly of the single cell can be made into the same plane, thereby improving the structural regularity of the single cell.

[0023] Furthermore, when the thickness of the cover plate is relatively thin, a protrusion may be provided on the inner surface of the cover plate, and a stepped through hole penetrating the cover plate may be provided on the protrusion as the through hole.

[0024] Furthermore, a plurality of blind holes are provided on the step surface along its circumference. When hot melt slurry is poured at this position, columns can be formed in the blind holes, thereby further improving the bonding strength between the dissolving film and the cover plate.

[0025] The utility model also provides a single cell battery, comprising a lower cover plate, the special feature of which is that the lower cover plate is the cover plate assembly for the single cell battery.

[0026] The beneficial effects of the utility model are:

[0027] The utility model has at least two through holes on the cover plate. When one of the through holes cannot be opened, the remaining through holes can be opened to allow the inner cavity of the single cell and the inner cavity of the shared pipeline assembly to be connected, thereby improving the sharing success rate. In addition, when all the through holes of the utility model are opened, compared with a structure that shares through only one through hole, the electrolyte and / or gas in the inner cavity of the single cell can be fully mixed with the electrolyte and / or gas in the inner cavity of the shared pipeline assembly, thereby achieving a better sharing effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a structural schematic diagram of a large-capacity battery in the background technology;

[0029] Figure 2 This is a schematic structural diagram of the cover plate assembly of Example 1;

[0030] Figure 3 This is an exploded schematic diagram of the cover plate assembly in Example 1;

[0031] Figure 4 is a schematic structural diagram of the cover plate in Example 2;

[0032] Figure 5 is a cross-sectional view of the cover plate in Example 2;

[0033] Figure 6 is a partial cross-sectional view of the cover plate assembly of Example 2;

[0034] Figure 7 is a schematic diagram of the structure of the protective film in Example 2;

[0035] Figure 8 This is a schematic diagram of the cover plate structure provided with a protective film in Example 2;

[0036] Fig. 9 is a schematic structural diagram of the sealing assembly in Example 2;

[0037] Fig.10 This is an exploded schematic diagram of the sealing assembly in Example 2;

[0038] Fig.11 is a cross-sectional view of the sealing assembly in Example 2;

[0039] Fig.12 This is a schematic diagram of the assembly process of the cover plate assembly in Example 2;

[0040] Fig.13 This is a schematic diagram of the structure of a single cell of Example 3;

[0041] Fig.14 This is a schematic diagram of the structure of another single cell of Example 3;

[0042] Fig.15 This is a structural schematic diagram of a cover plate assembly in Example 4;

[0043] Fig.16 This is a schematic structural diagram of another cover plate assembly in Example 4;

[0044] The accompanying drawings in the figure are marked as follows:

[0045] 01. first hollow member; 02. second hollow member; 03. single cell;

[0046] 1. Cover plate; 11. Through hole; 12. Blind hole; 2. Sealing assembly; 3. Outer surface of cover plate; 4. Protrusion; 5. Sealing assembly installation space; 6. Protective film; 7. Dissolving film; 8. Step surface; 9. Step structure; 10. Dissolving film installation space; 13. Sealing part; 14. Fixing part; 15. Pole. DETAILED DESCRIPTION

[0047] In order to make the above-mentioned purposes, features and advantages of the utility model more obvious and easy to understand, the specific implementation methods of the utility model are described in detail below in conjunction with the drawings of the specification. Obviously, the described embodiments are part of the embodiments of the utility model, but not all of them. Based on the embodiments of the utility model, all other embodiments obtained by ordinary persons in the field without creative work should fall within the scope of protection of the utility model.

[0048] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0049] In the description of the present invention, it should be noted that the orientation or positional relationship indicated by the terms "upper, lower" etc. is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0050] The utility model provides a cover plate assembly for a single cell, comprising a cover plate, wherein at least two through holes are formed on the cover plate, and sealing components are arranged at the through holes for sealing the through holes. Such sealing components can fall off from the cover plate by external force or external electrolyte or form openings penetrating the through holes in the sealing components.

[0051] It should be noted here that the above-mentioned external electrolyte refers to the electrolyte located outside the single cell housing, rather than the electrolyte in the inner cavity of the single cell. That is to say, the above-mentioned sealing component cannot be opened through the electrolyte in the inner cavity of the single cell.

[0052] The single cell battery described here is a square shell battery, which includes an upper cover plate, a lower cover plate, a cylinder, a battery cell assembly and an electrolyte; the battery cell assembly described here can be called an electrode assembly, which is arranged in sequence by a positive electrode, a separator and a negative electrode and assembled by a lamination or winding process.

[0053] The cover plate assembly of the utility model can be used as a lower cover plate or an upper cover plate. When used as an upper cover plate, unlike the lower cover plate, a corresponding pole needs to be added. The specific selection can be made according to actual needs.

[0054] The utility model also provides a single cell with the above-mentioned cover plate assembly. As described in the background technology, such single cells are mainly used to construct large-capacity batteries (also known as battery packs or battery modules). Such large-capacity batteries include multiple single cells arranged side by side and at least one shared pipeline assembly; the shared pipeline assembly is connected to the inner cavity of the single cell through the single cell through hole.

[0055] If the cover plate assembly serves as the lower cover plate, the shared pipeline assembly is an electrolyte shared pipeline. The sealing assembly sealed on the through hole of the lower cover plate of each single cell is opened by external force. The electrolyte in the inner cavity of each single cell is connected through the electrolyte shared pipeline, so that the electrolyte of all single cells is in the same system, reducing the difference between the electrolytes of each single cell, improving the consistency between each single cell to a certain extent, thereby improving the cycle life of the large-capacity battery to a certain extent.

[0056] If the cover plate assembly serves as the upper cover plate, the shared pipeline assembly serves as the gas sharing pipeline. External force is used to open the sealing assembly sealed on the through hole of the upper cover plate of each single cell. The gas in the inner cavity of each single cell is connected through the gas sharing pipeline, so that the gas in the inner cavity of the entire large-capacity battery is balanced, thereby improving the cycle life of the large-capacity battery to a certain extent.

[0057] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0058] Example 1

[0059] This embodiment is mainly described by taking the cover plate assembly as the lower cover plate of a single cell as an example.

[0060] like Figure 2 and Figure 3 , which is a schematic diagram of the structure of the cover plate assembly of this embodiment. As can be seen from the figure, the cover plate assembly of this embodiment includes a cover plate 1 and a sealing assembly 2 fixed on the cover plate 1.

[0061] For the convenience of description, the length direction of the cover plate 1 may be defined as the x direction, the width direction may be defined as the y direction, and the thickness direction may be defined as the z direction.

[0062] In this embodiment, the cover plate 1 is a rectangular plate, and its area can be slightly larger than the area of ​​the open end of the cylinder, and it can be fixed to the open end of the cylinder by welding. It can also be fixed by setting a first step structure around the cover plate 1 by welding, and the step surface of the first step structure can also be used as a positioning surface. The positioning surface can be used to first position the cover plate 1 at the open end of the cylinder, and then fix it by welding. The area of ​​the cover plate 1 can also be slightly smaller than the area of ​​the open end of the cylinder, and it can be fixed to the open end of the cylinder by embedding welding.

[0063] In some other embodiments, the cover plate 1 and the cylinder body are an integral piece.

[0064] Two through holes 11 are provided on the cover plate 1. The two through holes 11 are arranged along the x direction and are symmetrical to each other. As can be seen from the figure, the two through holes 11 are provided near the edge in the width direction of the cover plate 1. When the battery cell inside the single cell adopts a winding core formed by winding, there is a large space between the side wall in the width direction of the single cell shell and the winding core. When the through hole 11 is provided near the edge in the width direction of the cover plate 1, firstly, when the through hole is provided, the internal battery cell structure is not affected. Secondly, after the sealing component at this part is opened, the electrolyte in the inner cavity of the shared pipeline can better enter the inner cavity of the single cell.

[0065] The size of the through hole 11 needs to meet the following conditions:

[0066] 1. The through hole 11 cannot be too large to ensure that the entire cover plate 1 has a certain strength, so as to avoid the single battery being scrapped due to poor strength of the cover plate 1 before the sealing component 2 at the through hole 11 is opened;

[0067] 2. The through hole 11 cannot be too small to ensure that after the sealing component 2 at the through hole 11 is opened, the electrolyte area of ​​each single battery cavity and the cavity of the shared pipeline component are smoothly connected to ensure a good sharing effect.

[0068] In some other embodiments, at least three through holes 11 may be provided on the cover plate 1, and the through holes 11 may be evenly distributed on the cover plate 1. The size of the through holes 11 still needs to meet the above two conditions.

[0069] In this embodiment, the sealing component 2 may adopt the sealing film disclosed in Chinese patent CN 218525645 U; the patent discloses two types of sealing films, one type of sealing film can be dissolved when encountering electrolyte; the other type of sealing film can be opened under the action of external force.

[0070] When a sealing film that is soluble in electrolyte is used, a protective film that is insoluble in electrolyte is generally provided on the side of the sealing film that faces the inside of the single battery housing. When the sealing film is dissolved in the electrolyte, the protective film falls off.

[0071] When this type of sealing film is used, the liquid circuit can be opened through the following process:

[0072] After the assembly of the large-capacity battery is completed, the electrolyte is injected into the electrolyte sharing pipeline, and the sealing films at the two through holes 11 can be automatically dissolved from the outside; because the protective film and the cover plate are not fixed in any way, when the sealing film is dissolved, the protective film will automatically fall off the cover plate, thereby making the electrolyte sharing pipeline and the inner cavity of the single battery connected, so that the electrolyte of all single batteries is in the same system, achieving the electrolyte sharing effect. In this embodiment, during the unpacking process, even if the sealing film at one through hole 11 is not completely dissolved, the electrolyte sharing effect can be achieved through the other through hole 11 (the sealing film of the through hole 11 is dissolved).

[0073] A sealing film that can be opened under the action of an external force is used. Generally, a traction ring can be provided on the sealing film. The traction ring is pulled by an external force to form an opening at the sealing film.

[0074] The liquid circuit can be opened through the following process:

[0075] After the assembly of the large-capacity battery is completed, the traction ring is pulled by a traction tool, and each sealing film is torn or falls off from the through hole 11, so that the electrolyte sharing pipeline is connected with the inner cavity of the single battery, so that the electrolyte of all single batteries is in the same system, achieving the electrolyte sharing effect. During the unpacking process, even if the sealing film at one through hole 11 is not torn or falls off, it can also pass through another through hole 11 (the sealing film of the through hole 11 is torn or completely falls off) to achieve the electrolyte sharing effect.

[0076] Example 2

[0077] Different from the first embodiment, this embodiment adopts a different sealing assembly 2 , and in order to cooperate with the sealing assembly 2 , the structure of the through hole 11 is also adjusted.

[0078] like Figure 4 and Figure 5 As shown, the through hole 11 of this embodiment is a circular step through hole, and the large hole of the step through hole is opened near the outer surface 3 of the cover plate, and the surface of the cover plate 1 away from the electrode assembly is defined as the outer surface. When the thickness of the cover plate 1 is thin, a protrusion 4 can be set on the inner surface of the cover plate 1, and a step through hole can be opened on the protrusion 4 as the through hole 11. When the thickness of the cover plate 1 is thick, the step through hole can be directly opened. The large hole of the step through hole serves as the sealing component installation space 5. When the sealing component 2 is fixed in the large hole, the flatness of the outer surface 3 of the cover plate can be ensured.

[0079] In some other embodiments, the through hole 11 can be a circular straight through hole 11, but relative to this embodiment, when the sealing assembly 2 is fixed at the position of the through hole 11, the protective film 6 and the dissolving film 7 will protrude from the outer surface 3 of the cover plate, making it difficult to ensure the flatness of the outer surface 3 of the cover plate.

[0080] In order to improve the stability of the sealing component 2 at the position of the through hole 11, the present embodiment further provides a plurality of fastening structures on the step surface 8 of the step through hole, through which the sealing component 2 can be firmly fixed on the cover plate 1. The fastening structure of the present embodiment is a plurality of blind holes 12 (see FIG. Figure 4 ), a plurality of blind holes 12 are evenly arranged along the circumference of the step surface 8. In some other embodiments, an annular groove may be provided on the step surface 8 along its circumference as a fastening structure.

[0081] like Figure 6 As shown, the sealing assembly 2 of this embodiment includes a protective film 6 and a dissolving film 7 .

[0082] The structure of the protective film 6 is as follows: Figure 7As shown, it is a sheet structure, and its shape is adapted to the shape of the through hole 11, and is circular, and the edge is fixed on the step surface 8 of the step through hole through the dissolving film 7 to seal the through hole 11. The material of the protective film 6 is a material that is insoluble in the electrolyte and has a certain strength to avoid the protective film 6 from being damaged due to the pressure of the electrolyte inside the single cell due to poor strength before the sealing component 2 at the through hole 11 is opened, resulting in the scrapping of the single cell. Generally, aluminum, copper, zinc, nickel, silver, epoxy resin, PE, PP, polytetrafluoroethylene or EPDM rubber can be selected.

[0083] In order to improve the bonding strength between the dissolving film 7 and the protective film 6, Figure 7 and Figure 8 It can be seen that in this embodiment, a second step structure 9 is provided at the edge of the protective film 6 along the circumference thereof, and a dissolving film installation space 10 is formed between the second step structure 9, the step surface 8 of the step through hole and the large hole wall of the step through hole.

[0084] In this embodiment, the dissolving membrane 7 is annular and fixed in the dissolving membrane installation space 10 , with its inner ring pressed against the edge of the protective membrane 6 and its outer ring fixed on the shell, thereby fixing the protective membrane 6 on the step surface 8 .

[0085] In this embodiment, the dissolving film 7 is fixed in the dissolving film installation space 10 by casting. Generally, a hot-melt slurry soluble in electrolyte can be cast in the dissolving film installation space 10, and after cooling, the dissolving film 7 can be formed, and the protective film 6 can be fixed on the single battery housing while achieving sealing. The material of the dissolving film 7 is at least one of PS, PMMA, SMMA, TPU, ABS, POM, PA6, PA12, and PVC.

[0086] In some other embodiments, a sealant that is soluble in the electrolyte may be poured into the dissolving film installation space 10 and, after solidification, the dissolving film 7 may be formed.

[0087] The sealing component 2 is isolated from the cover plate 1, and its structure is as follows Figures 9 to 11 As shown, for the convenience of description, the dissolving film 7 is divided into a sealing portion 13 and a fixing portion 14 according to different functions. The sealing portion 13 is annular, the inner ring surface cooperates with the stopper of the protective film 6, and the outer ring surface is used to fix with the inner wall of the through hole 11. The fixing portion 14 is a column adapted to the blind hole 12, which is used to strengthen the bonding strength between the sealing component 2 and the cover plate 1. Figure 8It can be seen that in this embodiment, there are multiple blind holes 12, which are evenly distributed on the step surface 8. In some other embodiments, there may be one blind hole 12, which is simpler in structure than in this embodiment, but the bonding strength between the sealing component 2 and the cover plate 1 is weaker. When there is a slight pressure in the inner cavity of the single cell, the entire sealing component 2 may fall off the cover plate 1, or cracks may be formed between the dissolving film 7 and the protective film 6, thereby damaging the performance of the single cell.

[0088] Reference Fig.12 In this embodiment, the sealing assembly 2 can be fixed on the cover plate 1 by the following process:

[0089] First, the protective film 6 is covered on the through hole 11;

[0090] Secondly, hot melt material is poured into the dissolving film installation space 10 , and after the hot melt material is cooled, a dissolving film 7 is formed, which achieves sealing and fixes the protective film 6 on the cover plate 1 at the same time.

[0091] The liquid circuit can be opened through the following process:

[0092] After the assembly of the large-capacity battery is completed, the electrolyte is injected into the electrolyte sharing pipeline to automatically dissolve the dissolving film 7 from the outside. Since the protective film 6 and the cover plate 1 are not fixed in any way, when the dissolving film 7 is dissolved, the protective film 6 will automatically fall off the cover plate 1, thereby making the electrolyte sharing pipeline and the inner cavity of the single battery connected, so that the electrolyte of all single batteries is in the same system.

[0093] This embodiment uses an annular dissolving membrane 7 instead of the solid sheet-shaped sealing membrane (soluble in electrolyte, also referred to as a dissolving membrane) used in Embodiment 1, which has at least the following advantages:

[0094] 1. The sealing component 2 has high installation reliability;

[0095] The utility model uses an annular dissolving film 7 to fix the protective film 6 on the battery housing. The annular dissolving film 7 can make the edge of the protective film 6 firmly combined with the single battery housing. Before the dissolving film 7 is dissolved, the protective film 6 is not easy to fall off, so that the installation reliability of the entire sealing assembly 2 is high.

[0096] 2. The sealing component 2 has good sealing performance;

[0097] The dissolving film 7 can well seal the gap between the protective film 6 and the shell area around the opening. At the same time, the electrolyte in the inner cavity of the single battery shell is in direct contact with the protective film 6, but cannot contact with the dissolving film 7 located on the outer surface of the shell. Therefore, during the assembly process of the large-capacity battery (before unpacking), the opening part of each single battery has good sealing performance.

[0098] 3. The sealing component 2 is easy to open;

[0099] During the unpacking process, electrolyte is injected into the shared pipe assembly. Under the action of the electrolyte, the dissolving film 7 is dissolved, and the protective film 6 falls off from the single battery shell, thereby connecting the inner cavity of each single battery shell with the inner cavity of the shared pipe assembly. Because the utility model adopts an annular dissolving film 7, when the outer diameter is the same, the annular dissolving film 7 has a smaller area than the solid dissolving film (sealing film in Example 1). Therefore, compared with Example 1, the dissolving time of the utility model is shorter, and the protective film 6 can fall off in a short time, which can shorten the preparation time of large-capacity batteries and improve production efficiency.

[0100] Example 3

[0101] like Fig.13 and Fig.14 As shown, this embodiment is a single cell, and its lower cover plate adopts the cover plate assembly in embodiment 1 and embodiment 2 respectively.

[0102] Example 4

[0103] like Fig.15 and Fig.16 As shown, what is different from the first and second embodiments is that the cover plate assembly of this embodiment serves as an upper cover plate of a single battery, and what is different from the lower cover plate is that a corresponding pole 15 needs to be added.

[0104] Fig.15 The two through holes are opened near the middle of the cover plate 1. Fig.16 In the embodiment, two through holes are opened near the edge of the cover plate 1 in the width direction. When the battery cell inside the single battery adopts a winding core, there is a large space between the side wall of the single battery shell in the width direction and the winding core. When the through holes are opened near the edge of the cover plate 1 in the width direction, firstly, when the through holes are opened, there is no influence on the internal battery cell structure. Secondly, after opening the sealing component at this part, the electrolyte in the inner cavity of the shared pipeline can better enter the inner cavity of the single battery.

Claims

1. A cover plate assembly for a single cell, characterized in that: It comprises a cover plate (1) and a sealing assembly (2); The cover plate (1) is provided with at least two through holes (11); The sealing assembly (2) is fixed on the cover plate (1) and seals the through hole (11); The sealing component (2) can be detached from the cover plate (1) or an opening through the through hole (11) can be formed in the sealing component (2) by external force or external electrolyte.

2. The cover plate assembly for a single cell according to claim 1, characterized in that: There are two through holes (11), which are symmetrically arranged on the cover plate (1) along the length direction of the cover plate (1).

3. The cover plate assembly for a single cell according to claim 2, characterized in that: The sealing component (2) comprises a protective film (6) and a dissolving film (7); the protective film (6) is in sheet form and covers the through hole (11); the dissolving film (7) is in annular form and is fixed to the outer surface (3) of the cover plate at the edge of the protective film (6) and the periphery of the through hole (11), thereby fixing the protective film (6) on the cover plate (1); The material of the dissolving film (7) is a material soluble in the electrolyte, and the material of the protective film (6) is a material insoluble in the electrolyte.

4. The cover plate assembly for a single cell according to claim 3, characterized in that: The dissolving film (7) is fixed on the edge of the protective film (6) and the outer surface (3) of the cover plate around the through hole (11) by casting.

5. The cover plate assembly for a single cell according to any one of claims 1 to 4, characterized in that: The material of the dissolving film (7) is PS, PMMA, SMMA, TPU, ABS, POM, PA6, PA12 or PVC.

6. The cover plate assembly for a single cell according to any one of claims 1 to 4, characterized in that: The material of the protective film (6) is aluminum, copper, zinc, nickel, silver, epoxy resin, PE, PP, polytetrafluoroethylene or EPDM rubber.

7. The cover plate assembly for a single cell according to claim 4, characterized in that: The through hole (11) is a stepped through hole, and the large hole is located on the outer surface (3) of the cover plate; The protective film (6) is located in the macropore, and a second step structure (9) is provided on the edge of the protective film (6) along its circumference, and a dissolving film installation space (10) is formed between the protective film (6), the step surface (8) of the step through hole, and the macropore wall; The dissolving membrane (7) is fixed in the dissolving membrane installation space (10).

8. The cover plate assembly for a single cell according to claim 7, characterized in that: A protrusion (4) is provided on the inner surface of the cover plate (1), and a stepped through hole penetrating the cover plate (1) is provided on the protrusion (4), and the stepped through hole serves as the through hole (11).

9. The cover plate assembly for a single cell according to claim 8, characterized in that: A plurality of blind holes (12) are arranged on the step surface (8) along its circumference.

10. A single cell battery, comprising a lower cover plate, characterized in that: The lower cover plate is the cover plate assembly for a single cell according to any one of claims 1 to 9.

Citation Information

Cited By

  • Sealing assembly, cover plate assembly, cylinder, battery cell casing member, and battery cell

    WO2025119193A1