Chromium plating tool clamp for CrMo cast iron piston ring

By adopting a ring-shaped pictogram anode and insulating structure that matches the shape of the CrMo cast iron bulb, the uneven coating thickness problem caused by the mismatch between the anode and the part during the chrome plating process is solved, the accuracy and efficiency of the chrome plating process are improved, and the product is ensured. Processing quality.

CN222008138UActive Publication Date: 2024-11-15STATE-OWNED CHANGJIANG POWER MASCH FACTORY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323356483.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-08
Publication Date
2024-11-15
Estimated Expiration
2033-12-08

AI Technical Summary

Technical Problem

During the chrome plating process, the anode and the part do not match the shape of the plating layer, resulting in uneven thickness, which is prone to chromium collapse and loose hole defects, affecting the product processing quality and progress.

Method used

A ring-shaped pictogram anode that matches the shape of the bulb-type parts is adopted, combined with the cathode clamping ring and the lining ring, and an insulating layer and rod part are installed to ensure uniform current density and prevent uneven coating thickness and inaccurate current.

Benefits of technology

It effectively avoids the problem of poor unevenness of the coating thickness, improves the accuracy and efficiency of the chrome plating process, reduces the chrome plating time and electricity consumption, and ensures the processing quality of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222008138U_ABST
    Figure CN222008138U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of chromium plating work fixtures, and discloses a chromium plating work fixture of a CrMo cast iron piston ring, which comprises an anode, a cathode clamping ring and a lining ring, and the end part of the anode is of an annular structure; the inner side of the cathode clamping ring is used for placing a CrMo cast iron piston ring, and one end part of the cathode clamping ring is provided with a necking towards the inner side along the radial direction; the outer wall of the CrMo cast iron piston ring is attached to the inner wall of the cathode clamping ring, and one end face of the CrMo cast iron piston ring is attached to the necking opening. The lining ring is arranged in the cathode clamping ring, the CrMo cast iron piston ring is located between the lining ring and the cathode clamping ring, and the outer wall of the lining ring is attached to the inner wall of the CrMo cast iron piston ring. According to the utility model, the anode adopts the annular pictographic anode matched with the piston ring part in shape, so that the problem of non-uniform current density at each part is solved, and the problem of poor thickness uniformity of a plating layer caused by mismatching of the anode and the piston ring in appearance when a common anode is used for chromium plating is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of chrome-plated fixtures and clamps, and discloses a chrome-plated fixture for a CrMo cast iron expansion ring. Background Art

[0002] CrMo cast iron is a loose and porous material. In order to increase the wear resistance of CrMo cast iron expansion rings, the surface is generally chrome-plated by electroplating loose chromium to reduce the surface friction coefficient and improve wear resistance. However, once the chrome plating layer is defective, due to the loose and porous material characteristics of CrMo cast iron, it is very easy to make the chromium layer difficult to deposit normally during repair, resulting in uneven plating thickness and chromium layer falling off on the working surface of the expansion ring.

[0003] In addition, in the prior art, when CrMo cast iron expansion rings are chrome-plated in batches, ordinary anodes are used for chrome plating, which often results in poor plating uniformity and rough chromium layer on the entire tank parts. Chromium chipping and loose hole defects are prone to occur during grinding, affecting the product processing quality and progress, and even scrapping parts. Utility Model Content

[0004] The utility model aims to provide a chrome-plating fixture for a CrMo cast iron expansion ring, which can avoid the problem of poor uniformity of coating thickness caused by mismatch between the anode and the expansion ring when chrome plating is performed using a common anode.

[0005] In order to achieve the above technical effects, the technical solution adopted by the utility model is:

[0006] A chrome-plated fixture for a CrMo cast iron expansion ring, comprising:

[0007] An anode, the anode is used to provide plating metal ions into the electroplating solution, and the end of the anode is a ring structure;

[0008] A cathode clamping ring, wherein the inner side of the cathode clamping ring is used to place a CrMo cast iron expansion ring, and one end of the cathode clamping ring is provided with a shrinkage opening radially inwardly; the outer wall of the CrMo cast iron expansion ring is fitted with the inner wall of the cathode clamping ring, and one end face of the CrMo cast iron expansion ring is fitted with the shrinkage opening;

[0009] An inner lining ring is arranged in a cathode clamping ring, the CrMo cast iron expansion ring is located between the inner lining ring and the cathode clamping ring, and the outer wall of the inner lining ring is in contact with the inner wall of the CrMo cast iron expansion ring.

[0010] Furthermore, the outer wall of the cathode clamping ring is provided with a first insulating layer.

[0011] Furthermore, a second insulating layer is provided at the contact position between the inner liner ring and the CrMo cast iron expansion ring.

[0012] Furthermore, the outer diameter of the inner liner ring is larger than the inner diameter of the CrMo cast iron expansion ring, and a notch is provided on the inner liner ring.

[0013] Furthermore, the inner diameter of the necking is smaller than the outer diameter of the inner liner ring.

[0014] Furthermore, the outer diameter of the anode of the annular structure is less than or equal to the outer diameter of the cathode clamping ring.

[0015] Furthermore, the anode and cathode clamping rings are both provided with a rod portion, and the rod portion is used to be connected to a wire.

[0016] Furthermore, a third insulating layer is provided on the outer wall of the rod portion of the cathode clamping ring.

[0017] Compared with the prior art, the utility model has the following beneficial effects: the anode in the utility model adopts a ring-shaped anode that matches the shape of the expansion ring-type parts, which improves the problem of uneven current density in various parts of the parts and avoids the problem of poor uniformity of coating thickness caused by the mismatch between the anode and the expansion ring shape when using ordinary anodes for chrome plating. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 Schematic diagram of the anode structure of the chrome-plated fixture of the CrMo cast iron expansion ring in the embodiment;

[0019] Figure 2 It is a schematic diagram of the three-dimensional structure of the cathode clamping ring, the CrMo cast iron expansion ring and the liner ring in the embodiment;

[0020] Figure 3 This is a schematic diagram of the installation of the cathode clamping ring, the CrMo cast iron expansion ring and the liner ring in the embodiment;

[0021] Among them, 1. anode; 2. cathode clamping ring; 3. CrMo cast iron expansion ring; 4. shrinkage; 5. liner ring; 6. first insulating layer; 7. second insulating layer; 8. rod; 9. third insulating layer. DETAILED DESCRIPTION

[0022] The present invention is further described in detail below in conjunction with the embodiments and drawings. However, this should not be understood as the scope of the above subject matter of the present invention being limited to the following embodiments, and all technologies realized based on the content of the present invention belong to the scope of the present invention.

[0023] Example

[0024] See also Figure 1-Figure 3 , a chrome-plated fixture for a CrMo cast iron expansion ring, comprising:

[0025] Anode 1, the anode 1 is used to provide plating metal ions into the electroplating solution, and the end of the anode 1 is a ring structure;

[0026] A cathode clamping ring 2, wherein the inner side of the cathode clamping ring 2 is used to place a CrMo cast iron expansion ring 3, and one end of the cathode clamping ring 2 is provided with a necking 4 radially inwardly; the outer wall of the CrMo cast iron expansion ring 3 is fitted with the inner wall of the cathode clamping ring 2, and one end face of the CrMo cast iron expansion ring 3 is fitted with the necking 4;

[0027] The inner lining ring 5 is arranged in the cathode clamping ring 2, the CrMo cast iron expansion ring 3 is located between the inner lining ring 5 and the cathode clamping ring 2, and the outer wall of the inner lining ring 5 is in contact with the inner wall of the CrMo cast iron expansion ring 3.

[0028] In this embodiment, the chrome plating of the CrMo cast iron expansion ring 3 is generally performed on one end face of the expansion ring. Before chrome plating, the CrMo cast iron expansion ring 3 is first placed in the cathode clamping ring 2, so that the outer wall of the CrMo cast iron expansion ring 3 contacts the inner wall of the cathode clamping ring 2, the end face that does not need chrome plating contacts the necking 4, and the inner wall of the CrMo cast iron expansion ring 3 fits the outer wall of the inner liner ring 5, so that the end face that does not need chrome plating, as well as the outer wall and inner wall are blocked to prevent the deposition of plating on these parts. Then the cathode clamping ring 2 and the anode 1 are placed in the electroplating solution, so that the end face that needs chrome plating is exposed to the electroplating solution, and then the power is turned on for chrome plating; because the anode 1 in this embodiment uses a ring-shaped anode 1 that matches the shape of the CrMo cast iron expansion ring 3 part, the problem of uneven current density at various parts of the part is improved, and the problem of poor uniformity of plating thickness caused by the mismatch between the anode 1 and the expansion ring shape when using an ordinary anode 1 for chrome plating is avoided.

[0029] In the present embodiment, the outer wall of the cathode clamping ring 2 is provided with a first insulating layer 6. The provision of the first insulating layer 6 can ensure that the contact portion between the cathode clamping ring 2 and the electroplating solution has a good insulating effect, so that the current absorbed by the cathode clamping ring 2 during the electroplating process is significantly reduced, thereby ensuring the accuracy of the current on the chrome-plated surface and greatly reducing the chrome plating time; avoiding the problem that the cathode clamping ring 2 absorbs more current due to inadequate and non-standard insulation, the chrome-plated surface current of the part is small and inaccurate, the chromium layer is deposited slowly, the electroplating takes a long time, and the power consumption is high.

[0030] In this embodiment, a second insulating layer 7 is provided at the contact position between the inner lining ring 5 and the CrMo cast iron expansion ring 3, which can further avoid the problem that when the inner lining ring 5 is a metal ring, the inner lining ring 5 absorbs current, resulting in small and inaccurate current on the chrome-plated surface of the part, slow deposition of the chromium layer, long electroplating time and high power consumption.

[0031] The outer diameter of the inner liner ring 5 is larger than the inner diameter of the CrMo cast iron expansion ring 3, and a notch is provided on the inner liner ring 5. The notch is provided on the inner liner ring 5 of the annular structure in this embodiment, so that the inner liner ring 5 has a certain elasticity, and the outer diameter of the inner liner ring 5 is larger than the inner diameter of the CrMo cast iron expansion ring 3, and the inner liner ring 5 can be compressed and stuck on the inner wall of the CrMo cast iron expansion ring 3, so that the outer wall of the CrMo cast iron expansion ring 3 is tightly fitted with the inner wall of the cathode clamping ring 2, and the inner wall of the CrMo cast iron expansion ring 3 is tightly fitted with the outer wall of the inner liner ring 5, thereby avoiding the problem of the CrMo cast iron expansion ring 3 coming out of the cathode clamping ring 2 during the electroplating process.

[0032] In this embodiment, the inner diameter of the necking 4 is smaller than the outer diameter of the inner lining ring 5, which can ensure that the end face of the necking 4 fits well with the end face of the CrMo cast iron expansion ring 3 that is not electroplated, thereby playing a better protective role; and the necking 4 can also play a certain supporting and limiting role for the inner lining ring 5, avoiding the problem of the inner lining ring 5 easily falling out of the CrMo cast iron expansion ring 3.

[0033] The outer diameter of the annular anode 1 is less than or equal to the outer diameter of the cathode clamping ring 2, which can avoid the problem of uneven coating thickness caused by large difference in current density at different parts of the same CrMo cast iron expansion ring 3 due to the mismatch between the shape of the ordinary anode 1 and the CrMo cast iron expansion ring 3.

[0034] The anode 1 and the cathode clamping ring 2 are both provided with a rod 8, and the rod 8 is used to connect with a wire, so that the cathode clamping ring 2 and the anode 1 can be electrically connected with a power source. In this embodiment, the outer wall of the rod 8 of the cathode clamping ring 2 is provided with a third insulating layer 9 to avoid the problem that the rod 8 of the cathode clamping ring 2 absorbs current after being charged, thereby affecting the current of the chrome-plated surface.

[0035] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A chrome-plated fixture for a CrMo cast iron expansion ring, characterized in that: include: An anode (1), the anode (1) being used to provide plating metal ions into the electroplating solution, and the end of the anode (1) being a ring-shaped structure; A cathode clamping ring (2), wherein the inner side of the cathode clamping ring (2) is used to place a CrMo cast iron expansion ring (3), and one end of the cathode clamping ring (2) is provided with a necking (4) radially inwardly; the outer wall of the CrMo cast iron expansion ring (3) is in contact with the inner wall of the cathode clamping ring (2), and one end face of the CrMo cast iron expansion ring (3) is in contact with the necking (4); An inner lining ring (5) is arranged in a cathode clamping ring (2), the CrMo cast iron expansion ring (3) is located between the inner lining ring (5) and the cathode clamping ring (2), and the outer wall of the inner lining ring (5) is in contact with the inner wall of the CrMo cast iron expansion ring (3).

2. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 1, characterized in that: The outer wall of the cathode clamping ring (2) is provided with a first insulating layer (6).

3. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 1, characterized in that: A second insulating layer (7) is provided at the contact position between the inner lining ring (5) and the CrMo cast iron expansion ring (3).

4. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 1, characterized in that: The outer diameter of the inner lining ring (5) is greater than the inner diameter of the CrMo cast iron expansion ring (3), and a notch is provided on the inner lining ring (5).

5. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 4, characterized in that: The inner diameter of the necking (4) is smaller than the outer diameter of the inner lining ring (5).

6. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 1, characterized in that: The outer diameter of the anode (1) of the annular structure is less than or equal to the outer diameter of the cathode clamping ring (2).

7. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 1, characterized in that: The anode (1) and the cathode clamping ring (2) are both provided with a rod portion (8), and the rod portion (8) is used to be connected to a conducting wire.

8. The chrome-plated fixture for the CrMo cast iron expansion ring according to claim 7, characterized in that: The outer wall of the rod portion (8) of the cathode clamping ring (2) is provided with a third insulating layer (9).