Novel electroplating system for enhancing thickness uniformity of metal film coating
By setting up multiple insoluble anode and square resistance detection devices connected by independent power supply in the electroplating system, the problem of uneven coating thickness is solved, and the uniformity of coating and production quality is improved.
Patent Information
- Application Number
- CN202420281696.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-05
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-02-05
AI Technical Summary
In the existing metal film electroplating process, due to the uneven distribution of insoluble anode, the thickness of the plating layer is uneven in the width direction, and the edge plating layer is thin, which affects the production quality.
A new electroplating system is designed, including multiple uniformly distributed insoluble anodes, each anodes are connected to a different power supply, and are equipped with a square resistance detection device and a supplementary plating device to ensure uniformity of the plating layer by independently controlling the current and detecting the plating thickness.
By independently controlling the current of each insoluble anode, the uniformity of the plating thickness is ensured, the production quality is improved, and the coating defects are compensated through the plating replenishment device, which improves the uniformity and integrity of the plating layer.
Smart Images

Figure CN222008155U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of coating equipment, and more specifically to a novel electroplating system for enhancing the uniformity of the thickness of a metal film coating. Background Art
[0002] The electroplating process is to pass an electrolyte over a metal film with a certain metal layer, and under the action of an electric current, the copper ions in the electrolyte are plated on the metal film. The current process mainly uses a conductive roller as the cathode and an insoluble anode in the electroplating tank as the anode. Under the action of the electric current, the copper ions leave the insoluble anode and are deposited on the metal film.
[0003] The existing insoluble anode is usually a whole titanium plate and titanium mesh, and the insoluble anode is connected to a power source. During electroplating, the electric lines of force between the cathode and the anode in the width direction of the metal film are uneven, which makes the coating of the metal film uneven in the width direction. Generally, the electric lines at the edge are sparse, and the electric lines in the middle are dense, resulting in a thinner coating at the edge of the metal film and a thicker coating in the middle.
[0004] The above shortcomings need to be improved. Summary of the invention
[0005] In order to solve the problem of uneven coating thickness during metal film electroplating, the utility model provides a novel electroplating system which enhances the uniformity of the metal film coating thickness.
[0006] The technical solution of the utility model is as follows:
[0007] A novel electroplating system for enhancing the uniformity of the thickness of a metal film coating comprises an electroplating tank in which a plurality of insoluble anodes are arranged, the plurality of insoluble anodes are evenly distributed along the width direction of the film, the insoluble anodes are arranged at intervals, and the insoluble anodes are respectively connected to different power supplies.
[0008] Furthermore, a square resistance detection device is provided on the electroplating tank, and the square resistance detection device is used to detect the square resistance of the film in sections in the width direction of the film.
[0009] Furthermore, the square resistance detection device includes a detection roller rotatably arranged on the electroplating tank, and a plurality of square resistance detection members are evenly arranged on the surface of the detection roller along the axial direction, and each of the square resistance detection members is used to detect the square resistance of each section position in the width direction of the film.
[0010] Furthermore, a supplementary plating device for supplementary coating of the thin film is arranged behind the electroplating tank.
[0011] Furthermore, the repair plating device includes a repair plating tank, in which a first spray pipe is arranged, the first spray pipes are arranged in pairs, each pair of the first spray pipes is located on two sides of the film respectively, and the first spray pipes are used to spray plating solution onto the film.
[0012] Furthermore, a second spray pipe is arranged behind the first spray pipe, and the second spray pipe is used for spraying cleaning liquid onto the film.
[0013] Furthermore, an insulating container is provided in the electroplating tank, and a grid is provided in the insulating container. The grid divides the insulating container into a plurality of accommodating spaces, and each of the insoluble anodes is respectively located in each of the accommodating spaces.
[0014] Furthermore, the grid is movably connected to the insulating container.
[0015] Furthermore, the grid comprises a transverse partition and a longitudinal partition, and the transverse partition and the longitudinal partition are detachably connected.
[0016] Furthermore, a plurality of first card slots are evenly formed on one of the long sides of the transverse partition, a plurality of second card slots are evenly formed on one of the long sides of the longitudinal partition, and the transverse partition and the longitudinal partition are cross-engaged through the first card slots and the second card slots.
[0017] According to the above-mentioned solution, the utility model has the beneficial effect that, by connecting each insoluble anode to a different power source, each insoluble anode is controlled by an independent power source, and the current on each insoluble anode can be accurately adjusted, thereby ensuring that the thickness of the coating deposited on the metal film is uniform, thereby improving the production quality. Since the insoluble anodes are arranged at intervals, the insoluble anodes will not contact each other, and the current will not flow randomly between the insoluble anodes, thereby enhancing the stability of the current and facilitating the uniformity of the coating thickness. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0019] Figure 1 It is a schematic diagram of the structure of the utility model;
[0020] Figure 2 This is a schematic diagram of the structure of the central resistance detection device in the utility model;
[0021] Figure 3It is a structural schematic diagram of the plating repair device in the utility model;
[0022] Figure 4 It is a structural schematic diagram of the insulating container in the utility model;
[0023] Figure 5 It is a schematic diagram of the structure of the transverse partition and the longitudinal partition in the utility model.
[0024] Among them, the figure marks in the figure are: 1, electroplating tank; 2, insoluble anode; 3, square resistance detection device; 301, detection roller; 302, square resistance detection member; 4, repair plating device; 401, repair plating tank; 402, first spray pipe; 403, second spray pipe; 5, insulating container; 501, grid; 502, accommodating space; 503, horizontal partition; 504, longitudinal partition; 505, first card slot; 506, second card slot; 6, conductive roller; 7, passing roller; 8, tension roller; 9, unwinding device; 10, winding device. DETAILED DESCRIPTION
[0025] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0026] It should be noted that when a component is referred to as being "fixed" or "set" or "connected" to another component, it may be located directly or indirectly on the other component. The directions or positions indicated by the terms "upper", "lower", "left", "right", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc. are based on the directions or positions shown in the accompanying drawings and are only for the convenience of description and should not be construed as limitations on the present technical solution. The terms "first", "second", etc. are only used for the convenience of description and should not be construed as indicating or implying relative importance or implicitly indicating the number of technical features. "Multiple" means two or more, unless otherwise clearly and specifically defined. "Several" means one or more, unless otherwise clearly and specifically defined.
[0027] like Figure 1 and Figure 4 As shown, a new electroplating system for enhancing the uniformity of the thickness of a metal thin film coating described in one embodiment of the utility model includes an electroplating tank 1, in which a plurality of insoluble anodes 2 are arranged, the plurality of insoluble anodes 2 are evenly distributed along the width direction of the film, the insoluble anodes 2 are arranged at intervals, and the respective insoluble anodes 2 are connected to different power sources respectively.
[0028] In this embodiment, a reeling device 9 is provided in front of the electroplating tank 1, and a reeling device 10 is provided behind the electroplating tank 1. The electroplating tank 1 is provided with multiple sections. By providing multiple sections of the electroplating tank 1, different plating processes of multiple metals or the same metal can be realized to meet diversified production needs. The number, configuration and order of the electroplating tanks 1 can be adjusted according to actual production needs to adapt to different electroplating process requirements. The electroplating tank 1 is provided with a plating solution, and the electroplating tank 1 is provided with a conductive roller 6, a passing roller 7 and a tension roller 8. The passing roller 7 and the tension roller 8 respectively ensure the stability of the transmission and the constancy of the tension, thereby ensuring the stability of the electroplating quality and the uniformity of the plating layer. During operation, the metal film is released through the reeling device 9, and the conductive roller 6 serves as the cathode. Driven by the conductive roller 6, the metal film passes through each section of the electroplating tank 1, and the metal film is transferred to the conductive roller 6 through the passing roller 7, and the conductive roller 6 contacts the metal film. The metal film acts as a cathode in the electroplating tank 1, and the insoluble anode 2 acts as an anode. When the cathode and the anode are energized, the insoluble anode 2 precipitates metal ions, which are deposited on the surface of the metal film to form a coating. The tension roller 8 is used to control the tension of the metal film to ensure its flatness and stability during the electroplating process. The electroplated metal film is rolled up by the winding device 10 to prepare for the next step of processing.
[0029] By connecting each insoluble anode 2 to a different power source, each insoluble anode 2 is controlled by an independent power source, and the current on each insoluble anode 2 can be accurately adjusted, so that the electric lines of force of the anode and the cathode on the film width are relatively uniform, thereby ensuring that the thickness of the coating deposited on the metal film is uniform, thereby improving production quality. Since the insoluble anodes 2 are arranged at intervals, the insoluble anodes 2 will not contact each other, and the current will not flow randomly between the insoluble anodes 2, which enhances the stability of the current and is conducive to the uniformity of the coating thickness.
[0030] like Figure 2 As shown, in a preferred embodiment, a square resistance detection device 3 is provided on the electroplating tank 1. In the width direction of the film, the square resistance detection device 3 is used to detect the square resistance of the film in sections.
[0031] The square resistance detection device 3 comprises a detection roller 301 rotatably arranged on the electroplating tank 1 , and a plurality of square resistance detection members 302 are evenly arranged on the surface of the detection roller 301 along the axial direction, and each square resistance detection member 302 is used to detect the square resistance of each section in the width direction of the film.
[0032] The resistance value per square area is called sheet resistance, which is an important quality indicator of conductive film. After the conductive film is produced, it needs to be tested for sheet resistance. Sheet resistance, also known as film resistance, has the same resistance measurement value for squares of any size. The size of the sheet resistance is related to the thickness of the conductive film. Therefore, the measurement of sheet resistance is widely used to detect the thickness of the conductive film and monitor the uniformity of the film thickness during the production process of the conductive film.
[0033] Since a plurality of square resistance detection members 302 are provided on the detection roller 301, the square resistance can be detected in sections in the film width direction, which helps to understand the resistance value of the conductive film in different areas, thereby evaluating its thickness distribution. Through continuous rotation and detection, the square resistance value of the conductive film can be obtained in real time, providing real-time production feedback to the operator. When the square resistance value of a certain area is found to be abnormal, it can be adjusted in time to ensure the overall quality and uniformity.
[0034] like Figure 1 and Figure 3 As shown, in a preferred embodiment, a supplementary plating device 4 for supplementary coating of the thin film is provided behind the electroplating tank 1 .
[0035] The plating device 4 includes a plating tank 401, in which a first spray pipe 402 is arranged. The first spray pipes 402 are arranged in pairs, and each pair of first spray pipes 402 is located on both sides of the film. The first spray pipes 402 are used to spray the plating solution onto the film. The first spray pipes 402 are titanium tubes, which are connected to a power supply as an anode.
[0036] After the film passes through the electroplating tank 1 and completes the preliminary electroplating, it enters the supplementary plating device 4. Each pair of first spray pipes 402 is located on both sides of the film, and the plating solution is sprayed on both sides of the film through the first spray pipes 402, and the film is supplementarily plated according to the detection result of the square resistance detection device 3.
[0037] Since the film may have uneven thickness in the length direction or some areas may not be completely covered during the electroplating process, the re-plating device 4 can be used to re-plating these areas, which can make up for the defects that may occur during the electroplating process, ensure the uniformity and integrity of the film, and thus improve the quality of the coating. Since the first spray pipe 402 is arranged in pairs on both sides of the film, the front and back sides can be re-plated at the same time, which improves the efficiency and speed of the operation. By spraying, the film does not need to be immersed in the plating solution, which can reduce the use of the plating solution and reduce costs.
[0038] like Figure 3 As shown, in a preferred embodiment, multiple pairs of first spray pipes 402 are provided, and a second spray pipe 403 is provided behind each first spray pipe 402. The second spray pipe 403 is used to spray a cleaning liquid onto the film, and the cleaning liquid is pure water. The second spray pipes 403 are provided in pairs, and each pair of two second spray pipes 403 are respectively located on the two sides of the film.
[0039] After the film is sprayed with the plating solution through the first spray pipe 402, it enters the area of the second spray pipe 403. Each pair of second spray pipes 403 is also located on both sides of the film, spraying cleaning solution on both sides of the film to clean the film and remove excess plating solution and other impurities.
[0040] By providing the second spray pipe 403 for cleaning, it is ensured that the surface of the film is clean and free of residue after the additional coating. By cleaning with pure water, impurities and excess plating solution on the surface of the film can be removed, thereby improving its surface quality. Each pair of second spray pipes 403 is located on both sides of the film, ensuring that both the front and back sides can obtain a uniform cleaning effect, further improving the uniformity of the coating.
[0041] like Figure 4 As shown, in a preferred embodiment, an insulating container 5 is provided in the electroplating tank 1, and a grid 501 is provided in the insulating container 5. The grid 501 divides the insulating container 5 into a plurality of accommodating spaces 502, and each insoluble anode 2 is respectively located in each accommodating space 502.
[0042] The grid 501 is movably connected to the insulating container 5 .
[0043] In this embodiment, the grid 501 in the insulating container 5 separates each insoluble anode 2, and the insulating container 5 is non-conductive, so that the insoluble anodes 2 will not contact each other, so that the current will not flow randomly in the insoluble anodes 2. By setting up the grid 501 to isolate each insoluble anode 2, the current density on each anode can be accurately controlled, thereby ensuring that the thickness of the coating deposited on the film is more uniform. Due to the isolation of the grid 501, even if an insoluble anode 2 fails or is abnormal during operation, it will not affect other anodes, thereby avoiding short circuits. The grid 501 is movably connected to the insulating container 5, and the grid 501 can be replaced as needed to adjust the position or number of the insoluble anodes 2, thereby increasing the flexibility and adaptability of the system.
[0044] like Figure 5 As shown, in a preferred embodiment, the grid 501 includes a transverse partition 503 and a longitudinal partition 504, and the transverse partition 503 and the longitudinal partition 504 are detachably connected.
[0045] A plurality of first slots 505 are evenly formed on one long side of the transverse partition 503 , a plurality of second slots 506 are evenly formed on one long side of the longitudinal partition 504 , and the transverse partition 503 and the longitudinal partition 504 are cross-engaged through the first slots 505 and the second slots 506 .
[0046] During installation, the first slot 505 on one long side of the transverse partition 503 is cross-engaged with the second slot 506 on one long side of the longitudinal partition 504. By setting a suitable number of transverse partitions 503 and longitudinal partitions 504, the spacing of the accommodating space 502 is controlled. Through the engagement of the first slot 505 and the second slot 506, the transverse partition 503 and the longitudinal partition 504 can be fixed at a specific position as required, ensuring the stability and accuracy of the grid 501.
[0047] Since the transverse partition 503 and the longitudinal partition 504 are detachably connected, the assembly and disassembly of the grid 501 becomes simple, and it is convenient for adjustment and maintenance. Through the cross-engagement of the first card slot 505 and the second card slot 506, the precise position of the grid 501 in the insulating container 5 can be ensured, thereby ensuring the accurate placement of the insoluble anode 2. Through the snap connection, the structure of the grid 501 is more stable, ensuring the stability of production.
[0048] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A novel electroplating system for enhancing the uniformity of metal film coating thickness, characterized in that: The electroplating tank comprises a plurality of insoluble anodes which are evenly distributed along the width direction of the film, each of the insoluble anodes is arranged at intervals, and each of the insoluble anodes is connected to a different power source.
2. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to claim 1, characterized in that: The electroplating tank is provided with a square resistance detection device, and in the width direction of the film, the square resistance detection device is used to detect the square resistance of the film in sections.
3. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to claim 2, characterized in that: The square resistance detection device comprises a detection roller rotatably arranged on the electroplating tank, and a plurality of square resistance detection members are evenly arranged on the surface of the detection roller along the axial direction, and each of the square resistance detection members is used to detect the square resistance of each section position in the width direction of the film.
4. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to claim 1, characterized in that: A supplementary plating device for supplementary coating of the thin film is arranged behind the electroplating tank.
5. A novel electroplating system for enhancing the uniformity of the thickness of the metal thin film coating according to claim 4, characterized in that: The plating repair device comprises a plating repair tank, in which a first spray pipe is arranged. The first spray pipes are arranged in pairs, and each pair of the first spray pipes is located on two sides of the film respectively. The first spray pipes are used to spray plating solution onto the film.
6. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to claim 5, characterized in that: A second spray pipe is arranged behind the first spray pipe, and the second spray pipe is used for spraying cleaning liquid onto the film.
7. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to any one of claims 1 to 6, characterized in that: An insulating container is arranged in the electroplating tank, and a grid is arranged in the insulating container. The grid divides the insulating container into a plurality of accommodating spaces, and each of the insoluble anodes is respectively located in each of the accommodating spaces.
8. A novel electroplating system for enhancing the uniformity of the thickness of the metal thin film coating according to claim 7, characterized in that: The grid is movably connected to the insulating container.
9. A novel electroplating system for enhancing the uniformity of the thickness of the metal thin film coating according to claim 7, characterized in that: The grid comprises a transverse partition and a longitudinal partition, and the transverse partition and the longitudinal partition are detachably connected.
10. A novel electroplating system for enhancing the uniformity of metal film coating thickness according to claim 9, characterized in that: A plurality of first card slots are evenly formed on one of the long sides of the transverse partition, a plurality of second card slots are evenly formed on one of the long sides of the longitudinal partition, and the transverse partition and the longitudinal partition are cross-engaged through the first card slots and the second card slots.