Equipment for testing performance of adhesive containing nano calcium carbonate
By introducing ventilation fans and electric heating tubes into the nano-cadherent carbonate performance testing equipment, the problem of the equipment lacking drying auxiliary components is solved, efficient drying of the adhesive is achieved, and testing efficiency is improved.
Patent Information
- Application Number
- CN202420481780.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-13
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-03-13
AI Technical Summary
The existing nanocadherent carbonate performance testing equipment lacks drying auxiliary components, which makes it impossible to effectively dry the adhesive after being stuck, affecting the testing efficiency.
A test equipment containing a ventilation fan, an electric heating tube and a ventilation hole was designed. The external control components were used to transport electric energy to the ventilation fan and an electric heating tube to realize air circulation and heat conduction, and complete the drying of the adhesive.
Through air circulation and heat conduction, the drying efficiency of nano-cadherent carbonate is significantly improved and the working efficiency of performance testing equipment is improved.
Smart Images

Figure CN222013942U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of calcium carbonate adhesive performance testing, in particular to a performance testing device for an adhesive containing nano calcium carbonate. Background Art
[0002] Nano calcium carbonate adhesive is a commonly used adhesive component in modern times. Its main function is to adhere objects. After the existing nano calcium carbonate adhesive is produced, it is often necessary to perform a performance test on the nano calcium carbonate adhesive to confirm the quality of the nano calcium carbonate adhesive. However, the existing nano calcium carbonate adhesive performance testing equipment lacks drying auxiliary components. After the nano calcium carbonate adhesive is used to adhere objects, the nano calcium carbonate adhesive cannot be dried, which affects the working efficiency of the nano calcium carbonate adhesive performance testing equipment.
[0003] Compared with the existing nano calcium carbonate adhesive performance testing equipment, the utility model adds a drying auxiliary component. After the nano calcium carbonate adhesive is adhered to the article, the nano calcium carbonate adhesive can be dried, thereby improving the working efficiency of the nano calcium carbonate adhesive performance testing equipment. Utility Model Content
[0004] The utility model aims to provide a performance testing device for an adhesive containing nano-calcium carbonate to solve the problems raised in the above-mentioned background technology.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solution: comprising a fixed shell and a box door, wherein two sets of box doors are installed on the front side of the fixed shell through hinges;
[0006] Two groups of ventilation shells are installed through the top of the fixed shell, a ventilation fan is installed inside the ventilation shell, an electric heating pipe is arranged inside the bottom inner wall of the fixed shell, and a plurality of ventilation holes are opened through the back of the fixed shell.
[0007] Preferably, two sets of cabinet doors are installed on the front side of the fixed shell through hinges, and a viewing window is inlaid on the front side of the cabinet doors.
[0008] Preferably, a password lock is installed on the front of the door, and the password lock is located on one side of the viewing window.
[0009] Preferably, a lock bolt is installed on the front of the door, the lock bolt is located on the other side of the viewing window, and the lock bolt is engaged with the password lock.
[0010] Preferably, electric telescopic rods are installed on both sides of the fixed shell, and the tail ends of the electric telescopic rods extend to the inner side of the fixed shell.
[0011] Preferably, a fixing frame is installed at the tail end of the electric telescopic rod, and a clamping piece is connected to the top of the fixing frame by bolts.
[0012] Preferably, a cylinder is installed through the top of the fixed shell, and the cylinder is located on the inner side of the ventilation shell, and a pressure detector is installed at the tail end of the cylinder.
[0013] Compared with the prior art, the beneficial effects of the utility model are:
[0014] 1. The utility model is equipped with a ventilation fan, an electric heating tube and a ventilation hole, and transmits electric energy to the inside of the ventilation fan through an external control component. At this time, the ventilation fan generates suction for the air in the external environment and transmits the air to the inside of the fixed shell. The resistance wire inside the electric heating tube transmits heat to the inside of the fixed shell through the electric heating effect, and dries the nano calcium carbonate adhesive inside the fixed shell. The ventilation hole transmits the air to the external environment, thereby completing the drainage of the air inside the fixed shell. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 A schematic diagram of the structure of a performance testing device for an adhesive containing nano-calcium carbonate is provided in the utility model;
[0016] Figure 2 A schematic diagram of the back structure of a performance testing device for an adhesive containing nano-calcium carbonate is provided in the utility model;
[0017] Figure 3 for Figure 1 Schematic diagram of the fixed shell cross-section connection part structure.
[0018] Figure numerals: 1. fixed shell; 2. box door; 3. ventilation shell; 4. ventilation fan; 5. electric heating tube; 6. ventilation hole; 7. inspection window; 8. password lock; 9. lock bolt; 10. electric telescopic rod; 11. fixed frame; 12. clamping plate; 13. cylinder; 14. pressure detector. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0020] Embodiment 1
[0021] like Figure 1 , Figure 2 and Figure 3As shown, the utility model proposes a performance testing device containing nano calcium carbonate adhesive, comprising a fixed shell 1 and a door 2. Two sets of doors 2 are installed on the front of the fixed shell 1 through hinges. The fixed shell 1 provides fixing points for the door 2, ventilation shell 3, electric heating tube 5, ventilation hole 6, electric telescopic rod 10 and cylinder 13 installed on its outer surface, and also provides bonding space for the nano calcium carbonate adhesive inside. The door 2 is installed to the front of the fixed shell 1 through hinges, providing space for the user to open the door 2 by external force; the front of the door 2 is inlaid with a viewing window 7, which is inlaid on the front of the door 2 for the user to check the parts adhered by the nano calcium carbonate adhesive. A viewing space is provided, a combination lock 8 is installed on the front of the box door 2, and the combination lock 8 is located on one side of the viewing window 7, and the combination lock 8 is connected with the lock bolt 9 to complete the fixing of the box door 2. When the box door 2 needs to be opened, the password can be transmitted to the inside of the combination lock 8 by external force. At this time, the engaging rod inside the combination lock 8 is separated from the lock bolt 9, and the driving user can open the box door 2 by external force. A lock bolt 9 is installed on the front of the box door 2, and the lock bolt 9 is located on the other side of the viewing window 7, and the lock bolt 9 is connected with the combination lock 8. The lock bolt 9 is connected with the combination lock 8 to complete the fixing of the box door 2. Electric telescopic rods 10 are installed on both sides of the fixed shell 1, and the tail end of the electric telescopic rod 10 extends to the fixed shell 1, when it is necessary to adjust the fixing range of the fixing component, the electric energy can be transmitted to the inside of the electric telescopic rod 10 through the external control component, and the electric telescopic rod 10 moves inwardly at this time, driving the fixing component to move inwardly, which is suitable for fixing the fixing components to each other. The tail end of the electric telescopic rod 10 is installed with a fixing frame 11, and the fixing frame 11 is installed to the tail end of the electric telescopic rod 10, providing a connection point for a clamping piece 12 connected to the top of the fixing frame 11 by bolts. Before using the device, the connecting component after bonding is moved to the top of the fixing frame 11, and the top of the fixing frame 11 is connected with the clamping piece 12 by bolts. When the adhesive part needs to be fixed, the screw can be turned by external force. The bolt drives the clamping piece 12 to move inward to complete the fixation of the adhesive. A cylinder 13 is installed through the top of the fixed shell 1, and the cylinder 13 is located on the inner side of the ventilation shell 3. When the adhesive component needs to be tested, the external gas can be delivered to the inside of the cylinder 13 through the external control component. At this time, the cylinder 13 drives the pressure detector 14 installed at its tail end to move downward, generating pressure on the adhesive. A pressure detector 14 is installed at the tail end of the cylinder 13. The pressure detector 14 moves downward under the drive of the cylinder 13 to detect the pressure on the adhesive, and transmits the detection data to the inside of the external display component, thereby completing the performance test of the calcium carbonate adhesive.
[0022] The working principle of a performance testing device containing nano-calcium carbonate adhesive based on Example 1 is: first, the nano-calcium carbonate adhesive is moved to the inner side of the adhesive component to complete the mutual fixation of the adhesive component, and then the bolt is rotated by external force to drive the clamping plate 12 to move inward to complete the fixation of the adhesive component. After the adhesive component is fixed, the external gas is transported to the inside of the cylinder 13 through the external control component. At this time, the cylinder 13 drives the pressure detector 14 installed at its tail end to move downward, generating pressure on the adhesive component. The pressure detector 14 moves downward under the drive of the cylinder 13, detects the pressure on the adhesive component, and transmits the detection data to the inside of the external display component, thereby completing the performance test of the calcium carbonate adhesive.
[0023] Embodiment 2
[0024] like Figure 1 , Figure 2 and Figure 3 As shown, the utility model proposes a performance testing device containing nano calcium carbonate adhesive. Compared with the first embodiment, the present embodiment further includes: a fixed shell 1 and a ventilation shell 3. Two sets of ventilation shells 3 are installed through the top of the fixed shell 1. The ventilation shell 3 is installed through the top of the fixed shell 1 to provide a fixing point for the ventilation fan 4 installed inside the fixed shell 1. The ventilation fan 4 is installed on the inner side of the ventilation shell 3. When the air inside the fixed shell 1 needs to be guided out, the electric energy can be transmitted to the inside of the ventilation fan 4 through the external control component. At this time, the ventilation fan 4 generates suction to the air in the external environment and transmits the air to the inside of the fixed shell 1, thereby improving the fixed shell 1. The air flow rate inside the nano-calcium carbonate adhesive in the shell 1, the inner wall of the bottom of the fixed shell 1 is arranged with an electric heating tube 5. When it is necessary to dry the nano-calcium carbonate adhesive inside the fixed shell 1, the electric energy can be transmitted to the inside of the electric heating tube 5 through the external control component. At this time, the resistance wire inside the electric heating tube 5 conducts the heat to the inside of the fixed shell 1 through the electrothermal effect, and the nano-calcium carbonate adhesive inside the fixed shell 1 is dried. A plurality of ventilation holes 6 are opened on the back of the fixed shell 1. When air is continuously transported to the inside of the fixed shell 1, the ventilation holes 6 transport the air to the external environment, thereby completing the drainage of the air inside the fixed shell 1.
[0025] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A performance testing device for an adhesive containing nano-calcium carbonate, comprising a fixed shell (1) and a door (2), characterized in that: The front side of the fixed shell (1) is provided with two sets of cabinet doors (2) via hinges; Two groups of ventilation shells (3) are installed through the top of the fixed shell (1), a ventilation fan (4) is installed inside the ventilation shell (3), an electric heating pipe (5) is arranged inside the bottom inner wall of the fixed shell (1), and a plurality of ventilation holes (6) are opened through the back of the fixed shell (1).
2. A nano-calcium carbonate-containing adhesive performance testing device according to claim 1, characterized in that: Two sets of cabinet doors (2) are installed on the front of the fixed shell (1) via hinges, and a viewing window (7) is inlaid on the front of the cabinet door (2).
3. A nano-calcium carbonate-containing adhesive performance testing device according to claim 1, characterized in that: A password lock (8) is installed on the front of the box door (2), and the password lock (8) is located on one side of the viewing window (7).
4. A nano-calcium carbonate-containing adhesive performance testing device according to claim 1, characterized in that: A lock bolt (9) is installed on the front of the box door (2), the lock bolt (9) is located on the other side of the viewing window (7), and the lock bolt (9) is engaged with the password lock (8).
5. A nano-calcium carbonate-containing adhesive performance testing device according to claim 1, characterized in that: Electric telescopic rods (10) are installed on both sides of the fixed shell (1), and the tail ends of the electric telescopic rods (10) extend to the inner side of the fixed shell (1).
6. A nano-calcium carbonate-containing adhesive performance testing device according to claim 5, characterized in that: A fixing frame (11) is installed at the rear end of the electric telescopic rod (10), and a clamping piece (12) is connected to the top of the fixing frame (11) via bolts.
7. A nano-calcium carbonate-containing adhesive performance testing device according to claim 1, characterized in that: A cylinder (13) is installed through the top of the fixed shell (1), and the cylinder (13) is located inside the ventilation shell (3). A pressure detector (14) is installed at the tail end of the cylinder (13).