Biosensor

CN222014054UActive Publication Date: 2024-11-15SOUTHEAST UNIV NANJING INST OF BIOMATERIALS & MEDICAL DEVICES
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202322657652.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Priority Date
2023-09-26
Filing Date
2023-09-28
Publication Date
2024-11-15
Estimated Expiration
2033-09-28

AI Technical Summary

Technical Problem

In the detection of organoid live organoids, the current switching ratio is relatively low, which affects the sensitivity and is difficult to process, resulting in low repeatability of micromachining preparation and reduced biomolecular adsorption capacity.

Method used

Design a vertical field effect VGFET structure including an ionic gel layer, a graphene layer, an organic layer and an electrode. Using fullerene C60 as an organic layer, a larger surface area and low processing difficulty can be achieved through the graphene/organic vertical structure. Combined with the sealing layer to increase the current switching ratio.

Benefits of technology

Fast and high-sensitivity organoid activity without marks is achieved, real-time electrochemical detection of labels is reduced, the probability of structural damage is improved, and the yield rate and current switching ratio are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222014054U_ABST
    Figure CN222014054U_ABST
Patent Text Reader

Abstract

The biosensor comprises an ionic gel layer, a graphene layer, a first organic layer, a first electrode, a second organic layer and a second electrode, wherein the graphene layer is arranged on the surface of the ionic gel layer; the first organic layer and the first electrode are arranged on the surface of the graphene layer; the second organic layer is arranged on the surface of the first organic layer; the biosensor provided by the utility model is provided with a graphene vertical field effect VGFET structure, when the biosensor is connected into an electric field through the first electrode and the second electrode, current flows in the direction of the first electrode, the graphene layer, the first organic layer, the second organic layer and the second electrode, namely, the channel direction is vertical to the graphene layer, the graphene layer has a large surface area, and the graphene layer has a large surface area. The processing difficulty is low, the current switch ratio is large, and rapid and high-sensitivity unmarked real-time electrochemical detection of the organoid activity can be realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of sensors, and in particular relates to a biosensor. Background Art

[0002] In recent years, organoid technology has gained popularity due to its advantages such as low cost, short time, and higher physiological relevance. As an in vitro model, organoids can simulate the genetic and epigenetic characteristics of the target tissue or organ to a large extent, and have broad application prospects in many directions such as disease mechanism, new target discovery, exploration of new diagnosis and treatment strategies, drug sensitivity testing, new drug development, and regenerative medicine. However, organoid detection methods are very scarce. In vivo observations are mainly focused on morphological observations, and breakpoint observations are focused on the detection of various indicators based on fluorescence. Optical, electrochemical and other means that can detect various indicators of organoids in real time in vivo are still relatively lacking.

[0003] Graphene has a single atomic layer structure and unique energy levels. Its carrier transport characteristics are affected by the surface chemical state. Its conductivity or field effect conductivity has a strong surface adsorption sensitivity. Traditional graphene biosensors are based on the lateral field effect transistor (LGFET) structure, and various biosensor structures are designed using the easy processing characteristics of graphene. The basic principle is: the sample solution to be tested is located on the graphene surface. When the biological molecules are non-covalently adsorbed on the graphene surface, their charged groups can interact with the free charges on the graphene surface. When the free charges are bound, they will affect the carrier distribution in the graphene, thereby generating electrostatic doping. The graphene surface potential and electrostatic doping will affect the conductivity of graphene, which is correlated with the concentration of the molecules to be tested in the solution.

[0004] In the application of LGFET in the study of high-sensitivity biomolecule detection, the current switching ratio is an important factor affecting the sensor signal amplification. The current switching ratio of the traditional graphene lateral field effect structure is low, which is not conducive to improving the sensitivity of label-free real-time detection of organoid activity. Reducing the width and size of graphene nanoribbons by photolithography and other methods can further improve the device current switching ratio, but the processing difficulty increases, the repeatability of microfabrication of nanoribbons is low, and the reduction in surface area also means a decrease in the adsorption capacity of biomolecules. Summary of the invention

[0005] The utility model aims to overcome the deficiencies in the prior art and to provide a biosensor with a large current switching ratio, which can realize fast and highly sensitive label-free real-time electrochemical detection of organoid activity.

[0006] The utility model provides the following technical solutions:

[0007] A biosensor comprises an ion gel layer, a graphene layer arranged on the surface of the ion gel layer, a first organic layer and a first electrode arranged on the surface of the graphene layer, a second organic layer arranged on the surface of the first organic layer, and a second electrode arranged on the surface of the second organic layer.

[0008] Furthermore, it also includes a sealing layer, which is coated on the outside of the ion gel layer, the graphene layer, the first organic layer, the second organic layer, the first electrode and the second electrode.

[0009] Furthermore, the first electrode and the second electrode are connected with leads extending out of the sealing layer.

[0010] Furthermore, the first organic layer and the second organic layer are both fullerene C 60 layer.

[0011] Furthermore, the first electrode is a gold electrode, and the second electrode is an aluminum electrode.

[0012] Furthermore, the thickness of the first electrode is 50 nm, and the thickness of the second electrode is 100 nm.

[0013] Furthermore, the thickness of the first organic layer and the second organic layer are both 100 nm.

[0014] Compared with the prior art, the beneficial effects of the utility model are:

[0015] (1) The biosensor provided by the utility model includes an ion gel layer, a graphene layer disposed on the surface of the ion gel layer, a first organic layer disposed on the surface of the graphene layer, and a second organic layer disposed on the surface of the first organic layer, forming a graphene vertical field effect VGFET structure. When the biosensor is connected to an electric field through a first electrode and a second electrode, current flows in the direction of the first electrode, the graphene layer, the first organic layer, the second organic layer, and the second electrode, that is, the current direction (channel direction) is perpendicular to the graphene layer, and the current switching ratio is large. Compared with the LGFET structure in the prior art, the graphene layer of the utility model can be designed to have a larger surface area, with low processing difficulty and a large current switching ratio, which is conducive to realizing fast and highly sensitive label-free real-time electrochemical detection of organoid activity.

[0016] (2) The biosensor provided by the utility model uses an ion gel layer as a structural support and dielectric layer of the biosensor. The ion gel layer is a flexible material, which is conducive to the effective transfer of the graphene / organic vertical structure layer to the planar substrate and reduces the probability of structural damage during the separation process from the glass substrate, and has a high yield rate; BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of the structure of the biosensor in the embodiment of the utility model;

[0018] Figure 2 This is a schematic diagram of the process of preparing a VGFET structure in an embodiment of the utility model;

[0019] Figure 3 This is a schematic diagram of the process of preparing a sample hole in an embodiment of the utility model;

[0020] Figure 4 This is a schematic diagram of the process of sealing and assembling the biosensor in the embodiment of the utility model;

[0021] Figure 5 Schematic diagram of the ion gel membrane prepared in the embodiment of the utility model;

[0022] Figure 6 This is a schematic diagram of the ion gel membrane capacitance detection structure in the embodiment of the utility model;

[0023] Figure 7 It is a schematic diagram of the evaporated gold electrode in the embodiment of the utility model;

[0024] Figure 8 This is a Raman spectrum of graphene on the surface of the ion gel membrane in the embodiment of the utility model;

[0025] Fig. 9 It is the fullerene C in the embodiment of the utility model 60 Raman spectrum of

[0026] Fig.10 The graphene SEM images of the ion gel membrane surface in the embodiment of the utility model are as follows: (a) the surface of the ion gel membrane without graphene transfer; (b) the surface of the ion gel membrane after graphene transfer;

[0027] Fig.11 The graphene surface SEM images of the present invention are as follows: (a) without evaporation of C 60 Graphene surface; (b) Evaporation of C 60 The graphene surface after

[0028] Fig.12 In the present utility model, C 60 Through TEM imaging: (a) high-resolution image; (b) electron diffraction image;

[0029] Fig.13 is a schematic diagram of a VGFET structure enclosed by a sealing layer in an embodiment of the utility model;

[0030] Fig.14 This is a schematic diagram of electrical detection of a VGFET structure with an ion gel gate dielectric in an embodiment of the utility model;

[0031] Fig.15The transfer characteristic curve of the VGFET structure enclosed by the enclosed layer at room temperature in the embodiment of the utility model: the left side is the curve after logarithmic processing, and the right side is the original data curve;

[0032] Fig.16 is the output characteristic curve of the VGFET structure with the sealing layer closed at room temperature in the embodiment of the utility model;

[0033] Fig.17 It is a plan view of the sample hole of the biosensor in the embodiment of the utility model;

[0034] Fig.18 Schematic diagram of the principle of applying the biosensor in the embodiment of the utility model to real-time electrochemical detection of organoid activity;

[0035] Fig.19 is a graph of the rate of change of organoid activity after intervention with different drugs in an embodiment of the present utility model;

[0036] Markings in the figure are: 1, ion gel layer; 2, graphene layer; 3, first organic layer; 4, first electrode; 5, second organic layer; 6, second electrode. DETAILED DESCRIPTION

[0037] The utility model is further described below in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the utility model, and cannot be used to limit the protection scope of the utility model.

[0038] Example 1

[0039] like Figure 1 As shown, this embodiment provides a biosensor, including an ion gel layer 1, a graphene layer 2 arranged on the surface of the ion gel layer 1, a first organic layer 3 and a first electrode 4 arranged on the surface of the graphene layer 2, a second organic layer 5 arranged on the surface of the first organic layer 3, and a second electrode 6 arranged on the surface of the second organic layer 5.

[0040] This embodiment provides a biosensor, further comprising a sealing layer, wherein the sealing layer is coated on the outside of the ion gel layer 1, the graphene layer 2, the first organic layer 3, the second organic layer 5, the first electrode 4 and the second electrode 6, and the first electrode 4 and the second electrode 6 are connected with leads extending out of the sealing layer.

[0041] In this embodiment, the first organic layer 3 and the second organic layer 5 are both fullerene C 60 , the first electrode 4 is a gold electrode, and the second electrode 6 is an aluminum electrode.

[0042] In this embodiment, the vapor-deposited thickness of the first electrode 4 is 50 nm, and the vapor-deposited thickness of the second electrode 6 is 100 nm; the vapor-deposited thickness of the first organic layer 3 and the second organic layer 5 are both 100 nm.

[0043] In the biosensor provided in this embodiment, the ion gel layer 1, the first organic layer 3 and the second organic layer 5 constitute a graphene vertical field effect VGFET structure. When the biosensor is connected to the electric field through the first electrode 4 and the second electrode 6, the current flows in the direction of the first electrode 4, the graphene layer 2, the first organic layer 3, the second organic layer 5 and the second electrode 6, that is, the current direction (channel direction) is perpendicular to the graphene layer 2, and the current switching ratio is large; and compared with the LGFET structure in the prior art, the graphene layer 2 of the utility model can be designed to have a larger surface area, low processing difficulty, and a large current switching ratio, which is conducive to the realization of fast and highly sensitive label-free real-time electrochemical detection of organoid activity. In addition, the biosensor provided by the utility model uses the ion gel layer 1 as the structural support and dielectric layer of the biosensor. The ion gel layer 1 is a flexible material, which is conducive to the effective transfer of the graphene / organic vertical structure layer to the flat substrate and the reduction of the probability of structural damage during the separation process from the glass substrate, and the yield rate is high.

[0044] Example 2

[0045] This embodiment provides a method for preparing a biosensor, the steps are as follows:

[0046] Step 1: Prepare ion gel membrane.

[0047] (1) Preparation of ion gel solution: Weigh PVDF polymer powder and heat it in a drying oven at 100°C for 1 hour to remove as much water molecules adsorbed in the powder as possible; weigh DMF solution according to the mass volume ratio of PVDF:DMF=1:(8-12), and put both into a flask at the same time for stirring and dissolving; weigh [EMIM]TF2N ionic solution according to the mass ratio of [EMIM]TF2N ionic liquid:PVDF=1:(3-5), add it to the DMF solution containing PVDF, and stir for 5 hours in a 60°C water bath to dissolve it. The prepared ion gel solution is stored at 4°C in the dark for use.

[0048] (2) Pretreatment of glass substrate: Place the glass substrate in an acid cleaning solution (concentrated sulfuric acid: hydrogen peroxide = 7:3), heat and soak at 90°C for 1 hour to clean the organic residues on its surface; take it out and wash it with deionized water for 3 times, place it in acetone for ultrasonic cleaning for 1 hour to make its surface hydrophobic, and blow dry it with nitrogen for later use.

[0049] (3) Ion gel film formation: The ion gel solution is evenly dropped on the surface of the pretreated glass substrate, and the film is formed by spin coating with a gel coater. After the film is evenly coated, it is placed on a heating plate for drying. After naturally cooling to room temperature, it is stored away from light for later use.

[0050] Step 2: Figure 2As shown, a VGFET (Vertical Graphene Field Effect Transistor) structure is prepared.

[0051] (1) Graphene pretreatment: Graphene is placed on the surface of a copper foil substrate, and the first electrode (gold electrode) and the first organic layer (fullerene C) are sequentially deposited on the surface of the graphene layer. 60 ), and etching away the graphene not covered by the first organic layer by oxygen plasma etching.

[0052] (2) Graphene transfer: The copper foil substrate is corroded by FeCl3 solution to separate the graphene from the copper foil substrate to obtain a graphene / first organic composite film, i.e., graphene / C 60 Composite membrane, graphene / C 60 The composite membrane was transferred to deionized water for cleaning; the cleaned graphene / C 60 The composite film was transferred by wet method (using 30% ethanol solution as the solution matrix) to the surface of the ion gel layer with glass substrate (ITO glass) and dried; C 60 The layer remains on the graphene surface to complete a one-step transfer, forming a heterojunction structure with graphene, which becomes the basis for the preparation of VGFET structure.

[0053] (3) Preparation of the second organic layer and the second electrode (source electrode): 60 The second organic layer (fullerene C) was deposited on the surface and edge of the composite film. 60 ), and evaporate the second electrode (aluminum electrode) at an appropriate position to obtain a VGFET structure;

[0054] Step 3: Prepare the biosensor.

[0055] (1) Device leads: Since all source and drain contacts cannot be used for signal transmission using probes or other methods after sealing, the source and drain (first electrode and second electrode) of the VGFET structure need to be wired before the sealing operation, using silver glue as the connection point.

[0056] (2) Preparation of liquid PDMS: Silica gel, ethyl orthosilicate and dibutyltin dilaurate were mixed uniformly in a mass ratio of 90:9:1 to obtain liquid PDMS.

[0057] (3) Device sealing: Drop liquid PDMS on the surface of the VGFET structure until it completely covers the VGFET structure, let it stand to dry and solidify, and obtain a VGFET structure sealed by a sealing layer.

[0058] (4) Separation of glass substrate: The VGFET structure enclosed by the sealing layer is placed in deionized water for ultrasonic treatment to complete the separation of the ion gel membrane of the biosensor and the glass substrate to obtain the biosensor.

[0059] Example 3

[0060] like Figure 3 and Figure 4 As shown, this embodiment provides an assembly method of the biosensor in Embodiment 2 or Embodiment 3, and the steps are as follows:

[0061] Step 1: Prepare sample wells (such as culture wells / addition wells).

[0062] (1) Pretreatment of silicon wafer substrate: Place the silicon wafer substrate in an acid pickling solution (concentrated sulfuric acid: hydrogen peroxide = 7:3), heat and soak at 90°C for 1 hour to clean the organic residue on its surface; take it out and wash it with deionized water for 3 times, place it in acetone for ultrasonic cleaning for 1 hour, and blow dry it with nitrogen for later use.

[0063] (2) Etching sample holes: The silicon wafer substrate is composed of SiO2 layer, Si layer and Si3N4 layer. Photolithography is performed on the SiO2 layer to expose the sample hole area that needs to be etched and removed; the SiO2 layer corresponding to the sample hole is removed by hydrofluoric acid treatment; the Si layer corresponding to the sample hole is etched away by wet etching, and then removed and washed in deionized water; the Si3N4 layer corresponding to the sample hole is removed by reactive ion etching, and after preparation, it is stored for future use.

[0064] Step 2: Paste and assemble.

[0065] The ion gel layer of the biosensor is bonded to the Si3N4 layer of the silicon wafer substrate with the sample hole etched therein, so that the overlapping area of ​​the graphene layer and the first organic layer and the second organic layer can completely cover the sample hole; liquid PDMS is used to seal the edge of the biosensor and fix the silicon wafer substrate to complete the assembly of the biosensor.

[0066] Example 4

[0067] This example adopts the method of Example 2 to prepare the biosensor, and the specific steps are as follows:

[0068] Step 1: Prepare ion gel membrane.

[0069] (1) Preparation of ion gel solution: Weigh 0.8 g of PVDF polymer powder and heat it in a drying oven at 100°C for 1 hour to remove as much water molecules adsorbed in the powder as possible; weigh 8 mL of DMF solution according to the mass volume ratio of PVDF:DMF=1:10, put both into a flask at the same time, and stir with a magnetic stirrer for 2 hours in a 60°C water bath to dissolve; weigh 0.2 g of [EMIM]TF2N ionic solution according to the mass ratio of [EMIM]TF2N ionic liquid:PVDF=1:4, add it to the DMF solution containing PVDF, and continue to stir in a 60°C water bath for 5 hours to dissolve. The prepared ion gel solution is stored at 4°C in the dark for use.

[0070] (2) Pretreatment of glass substrate: Place the glass substrate (2x2 cm) in an acid cleaning solution (concentrated sulfuric acid: hydrogen peroxide = 7:3), heat and soak at 90°C for 1 h to clean the organic residues on its surface; take it out and wash it with deionized water for 3 times, place it in acetone for ultrasonic cleaning for 1 h to make its surface hydrophobic, and blow dry it with nitrogen for later use.

[0071] (3) Ion gel film formation: The ion gel solution was evenly dropped on the surface of the pretreated glass substrate, and the film was formed by spin coating with a gel coater. The speed was adjusted to 2500 rpm and the time was 15 s. After the spin coating was evenly applied, it was placed on a heating plate for drying at a temperature of 150°C for 30 min. After cooling naturally to room temperature, it was stored away from light for future use. Figure 5 Shown is a transparent ion gel film.

[0072] (4) Detection of electrical properties of ion gel membrane: Figure 6 As shown in the figure, aluminum electrodes are directly deposited on the ion gel film and SiO2 surface, and a capacitor structure is formed with ITO glass as the substrate. The cross area of ​​the upper and lower electrodes is 4mm 2 The capacitance (C) of the ion gel film sandwiched between the aluminum electrode and ITO was measured using a digital source meter. The calculation formula is as follows:

[0073] C=-1 / (2πfZ)

[0074] Where Z is impedance and f is voltage frequency. The capacitance of the ion gel membrane was measured to be as high as 9 μF / cm at low frequency. 2 .

[0075] Step 2: Prepare a VGFET structure.

[0076] (1) Graphene pretreatment: Graphene is placed on the surface of the copper foil substrate. The graphene is shielded by the electrode mask, leaving a position for drain electrode evaporation, and placed in a vacuum coating chamber. When the vacuum degree reaches 3*10 -3 The coating machine was turned on at 12:00 p.a., and the gold electrode was evaporated to a thickness of 50 nm. Then the graphene was covered by the organic layer mask to expose the organic layer (fullerene C60 ) is deposited at the position of the organic layer, and the thickness of the organic layer is 100 nm to replace PMMA as the graphene protection layer and transfer layer, and the graphene not covered by the organic layer is etched away by oxygen plasma. Figure 7 As shown, the black frame is the gold electrode evaporated on the graphene surface.

[0077] (2) Graphene transfer (one-step transfer): FeCl3 solution is used to corrode the copper foil substrate to separate the graphene from the copper foil substrate to obtain graphene / C 60 Composite membrane, graphene / C 60 The composite membrane was transferred to deionized water for washing 2-3 times; the cleaned graphene / C 60 The composite film was transferred to the surface of the ion gel layer with ITO glass substrate by wet method and dried at 80℃. In view of the hydrophobic surface of the ion gel film, 30% ethanol solution was selected as the solution matrix for wet transfer to promote the graphene / C 60 The composite membrane is laterally spread on the surface of the ion gel membrane; C 60 The layer remains on the graphene surface to complete a one-step transfer, forming a heterojunction structure with graphene, which becomes the basis for the preparation of VGFET structure.

[0078] (3) Raman spectroscopy characterization.

[0079] The ion gel film without graphene transfer and the ion gel film after graphene transfer were characterized by RENISHAW0963G1 Raman spectrometer and SIGMA500 scanning electron microscope, respectively, to verify whether the graphene was successfully transferred and to observe the graphene surface morphology. Figure 8 The Raman spectra of the ion gel film without graphene transfer (curve 2) and the ion gel film after graphene transfer (curve 1) are shown. Curve 2 is the Raman spectrum of the ion gel film substrate, and only at 2980 cm -1 There is an obvious characteristic peak at 1580cm, which does not overlap with the characteristic peak of graphene. Curve 1 is the Raman spectrum of graphene transferred to the ion gel membrane. It can be clearly seen that graphene has a peak at 1580cm -1 and 2680cm -1 The characteristic Raman peaks at , which are the characteristic peaks G and 2D peaks produced by the vibration of graphene atomic lattice, indicate that graphene has been successfully transferred to the surface of the ion gel membrane. At the same time, the perfect single Lorentz peak at the 2D peak indicates that the transferred graphene is a single layer.

[0080] The C 60 The layer was characterized and C 60 The surface morphology and crystal state of the layer are shown in Figure 2. Fig. 9As shown. 60 The molecule is a 20-sided sphere composed of 60 carbon atoms, with 46 different vibration modes, but the vibration modes visible in the Raman spectrum are: 2A g +8H g , where A g The mode is non-degenerate, H g The mode is 5-fold degenerate. The corresponding scattering frequency position (cm -1 ) is 273(H g )、433(H g )、496(A g 1) 711(H g )、775(H g )、1101(H g )、1251(H g )、1427(H g )、1469(A g 2) 1578(H g ), where A g Mode 1 reflects the completely symmetrical radial motion mode of carbon atoms. g 2 reacts to the tangential motion of the carbon atoms in the pentagonal ring. g Mode 496cm -1 The reaction is the radial motion mode of the hexagonal carbon atoms, H g Mode 433cm -1 The reaction at 1469cm -1 The characteristic peak signal at strongly indicates that most of the film is crystalline structure.

[0081] (4) Scanning electron microscopy characterization.

[0082] Fig.10 SEM images showing the surface of the ion gel membrane without graphene transfer (a) and the surface of the ion gel membrane after graphene transfer (b). By comparing the images, it can be seen that after the graphene is transferred to the ion gel membrane, it is completely attached to the membrane surface, the PMMA is basically removed within the field of view, and the graphene surface is basically intact.

[0083] Fig.11 Display undeposited C 60 Graphene surface (a) and evaporated C 60 (b) SEM image of the graphene surface after C 60 The surface morphology of the film is basically consistent with that of the graphene surface, and it can be evenly adhered to the graphene surface. The molecules are adsorbed on the surface of the graphene texture structure through van der Waals forces, self-assembled and arranged in an orderly manner to form crystal structures with different orientations and grow layer by layer, eventually becoming a solid organic film with uniform epitaxy on the graphene surface.

[0084] (5) Transmission electron microscopy characterization.

[0085] Fig.12 Displayed is C 60 TEM high-resolution image (a) and crystal electron diffraction image (b) of the film surface show that the C 60 The layered crystal structure is mainly composed of polycrystalline and a small amount of amorphous phase, with crystals of a few nanometers embedded in the amorphous structure. 60 The lattice fcc (111) plane distance is 0.81nm and the lattice length is 1.417nm.

[0086] (6) Preparation of organic layer and source electrode: Use organic layer mask to cover graphene / C 60 Composite film, so that the evaporation area can cover graphene / C 60 The edge of the composite film is then placed in the vacuum coating chamber. When the vacuum degree reaches 3*10 -3 The heated tungsten basket evaporation was turned on at 1000 nm, and the thickness of the organic layer was about 100 nm. After the organic layer was prepared, the sample was shielded by an electrode mask to leave a position for evaporation of the source electrode. The thickness of the aluminum electrode was 100 nm, and a VGFET structure was obtained.

[0087] Step 3: Prepare the biosensor.

[0088] (1) Device leads: Since all source and drain contacts cannot be used for signal transmission using probes or other methods after sealing, the source and drain (gold electrodes and aluminum electrodes) of the VGFET structure need to be wired before the sealing operation, using silver glue as the connection points.

[0089] (2) Preparation of liquid PDMS: Silica gel, ethyl orthosilicate and dibutyltin dilaurate were mixed uniformly in a mass ratio of 90:9:1 to obtain liquid PDMS.

[0090] (3) Device sealing: Liquid PDMS is dropped onto the surface of the VGFET structure until it completely covers the VGFET structure, and then allowed to stand at room temperature for 2 h to dry and solidify, thereby obtaining a VGFET structure with a sealing layer. Fig.13 shown.

[0091] (4) Testing of electrical properties of VGFET structure enclosed by enclosed layer.

[0092] like Fig.14 As shown in FIG. 1 , the electrical performance of the VGFET structure enclosed by the enclosed layer is tested. When the gate voltage is applied to the gate dielectric layer, the source-drain current is regulated by the interface electric field. The VGFET structure with ion gel gate dielectric prepared in this embodiment is adjusted by changing the gate voltage from -10V to +10V (such as Fig.15), showing an on / off ratio (Jon / Joff) of 10 3 ; From the output characteristic curve (such as Fig.16 As shown in the figure, it can be seen that as the source-drain voltage changes, the source-drain current increases exponentially, which is consistent with the volt-ampere characteristics of the heterojunction curve.

[0093] (5) Separation from glass substrate: Since both the surface of the ion gel membrane and the surface of the glass substrate are hydrophobic, the VGFET structure enclosed by the sealing layer is placed in deionized water and ultrasonically treated for 1 to 5 minutes. When water penetrates into the interface between the two, the separation of the ion gel membrane and the glass substrate of the biosensor is completed, and the biosensor is obtained.

[0094] Example 5

[0095] This embodiment adopts the method of embodiment 3 to assemble the biosensor, and the specific steps are as follows:

[0096] Step 1: Prepare sample wells (such as culture wells / addition wells).

[0097] (1) Pretreatment of silicon wafer substrate: Place the silicon wafer substrate in an acid pickling solution (concentrated sulfuric acid: hydrogen peroxide = 7:3), heat and soak at 90°C for 1 hour to clean the organic residue on its surface; take it out and wash it with deionized water for 3 times, place it in acetone for ultrasonic cleaning for 1 hour, and blow dry it with nitrogen for later use.

[0098] (2) Etching sample holes: The silicon wafer substrate is composed of a SiO2 layer, a Si layer, and a Si3N4 layer. Before etching, the silicon wafer substrate is placed on a heating plate and pre-treated by heating at 60°C.

[0099] ① Photolithography on the SiO2 layer:

[0100] a. The photoresist used was RZJ-304 positive photoresist (the solubility in the developer increases after exposure), and the coating conditions were a rotation speed of 2100 rpm and a time of 30 s;

[0101] b. After the coating is completed, place it on the surface of a heating plate and heat it at 100°C for 90 seconds to make the photoresist film closely adhere to the surface of the silicon wafer substrate;

[0102] c. After drying, place the mask on the appropriate position on the surface of the silicon wafer substrate and calibrate it strictly. Use the hard contact mode for exposure processing, and the processing time is 3s;

[0103] d. Place the exposed silicon wafer substrate in a positive photoresist developer. The silicon wafer substrate should be completely immersed in the developer so that the photoresist surface is in full contact with the developer. Remove the photoresist on the exposed part. The development time is 30 seconds. After the development is completed, place it in a rinse solution (deionized water) to remove the residual developer. The rinse time is 30 seconds.

[0104] e. After rinsing, blow dry with nitrogen and place on a hot plate for drying at 100°C for 90 seconds to make the photoresist adhere more firmly to the SiO2 surface.

[0105] ② Hydrofluoric acid treatment: After the silicon wafer substrate is photoetched, the SiO2 layer in the micropore area to be etched is exposed and placed in a 25% HF solution for etching for 30 seconds to remove the SiO2 and keep the surrounding photoresist layer intact.

[0106] ③ Wet etching: Place the silicon wafer substrate in a plastic flask containing 25% TMAH solution, heat it in a water bath at 90°C for 12 hours, and wait for transparent holes (about 0.5mm in side length) to appear in the suspended area, then take it out and wash it in deionized water to complete the etching of the Si layer corresponding to the sample hole.

[0107] ④ Reactive ion etching: The Si3N4 layer in the suspended area needs to be removed by RIE etching. The silicon wafer substrate is placed in the chamber of the reactive ion etcher. The reaction conditions are etching power, gas pressure 5Pa, reaction time 120s, and the reaction gas is a mixed gas of 20sccm trifluoromethane (CHF3) and 10sccm tetrafluoromethane (CF4). After the reaction is completed, the etching situation is observed through an optical microscope. After preparation, it is stored for future use.

[0108] Step 2: Paste and assemble.

[0109] The ion gel layer of the biosensor is laminated to the Si3N4 layer of the silicon wafer substrate with the sample hole etched therein, so that the overlapping area of ​​the graphene layer and the first organic layer and the second organic layer can completely cover the sample hole; liquid PDMS is used to seal the edge of the biosensor and fix the silicon wafer substrate to complete the assembly of the biosensor. Fig.17 Figure 2 is a plan view of the sample hole of the biosensor.

[0110] Example 6

[0111] The growth of organoids is particularly dependent on the in vitro culture environment. As the environment changes (such as temperature, pH value, drug intervention, etc.), the activity of organoids will also change accordingly. For example, the concentration of charged molecules / groups (H+, OH-, amino, carboxyl, etc.) in cells will fluctuate significantly, which can cause changes in local field effects. This change can be detected in real time in vivo through electrochemical sensors.

[0112] like Fig.18 As shown, this embodiment is based on the principle that the charged macromolecules produced by the organoids adsorbed on the surface of the ion gel membrane will produce a local field effect and affect the conductivity of graphene. The activity of the organoids is positively correlated with the order of magnitude of the charged macromolecules produced. The digital source meter is used to monitor the change of electrical signals to complete label-free real-time electrochemical detection. The specific steps are as follows:

[0113] (1) Organoid in vitro modeling and culture is performed according to the existing mature organoid culture process according to the sample type;

[0114] (2) The modeled organoid samples are transferred into the culture wells / sample wells containing cell culture medium in the biosensor;

[0115] (3) After the organoids are attached to the ion gel membrane, the cell culture medium is replaced with the organoid culture medium and the test drug (4 groups for comparison) intervention test is carried out;

[0116] (4) Record the changes in the biosensor current signal and calculate the rate of change in organoid activity based on the current change ratio; the calculation formula is as follows:

[0117] R=(II s ) / I s *100

[0118] In the formula, I s is the starting current signal value;

[0119] (5) Comparison of the effects of the four drugs on changes in organoid activity (e.g. Fig.19 As shown in the figure, it can be assessed that the organoid sample is most sensitive to drug B and least sensitive to drug D.

[0120] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the protection scope of the present invention.

Claims

1. A biosensor, characterized in that: The invention comprises an ion gel layer, a graphene layer arranged on the surface of the ion gel layer, a first organic layer and a first electrode arranged on the surface of the graphene layer, a second organic layer arranged on the surface of the first organic layer and a second electrode arranged on the surface of the second organic layer.

2. The biosensor according to claim 1, characterized in that The invention also comprises a sealing layer, wherein the sealing layer is coated on the outside of the ion gel layer, the graphene layer, the first organic layer, the second organic layer, the first electrode and the second electrode.

3. The biosensor according to claim 2, characterized in that The first electrode and the second electrode are connected with leads extending out of the sealing layer.

4. The biosensor according to claim 1, characterized in that The first organic layer and the second organic layer are both fullerene C 60 layer.

5. The biosensor according to claim 1, characterized in that The first electrode is a gold electrode, and the second electrode is an aluminum electrode.

6. The biosensor according to claim 1, characterized in that The thickness of the first electrode is 50 nm, and the thickness of the second electrode is 100 nm.

7. The biosensor according to claim 1, characterized in that The thickness of the first organic layer and the second organic layer are both 100 nm.

Citation Information

Cited By

  • Biosensor as well as preparation method, assembly method and application thereof

    CN117269263A

  • Monatomic layer graphene sperm detection sensor and preparation method thereof

    CN120522060A