Casting mold
By designing multiple inlet port groups and external eight-character structures in large die-casting molds, the problem of metal liquid stagnation is solved, the product molding pass rate and efficiency are improved, and the production cost and the demand for die-casting equipment are reduced.
Patent Information
- Application Number
- CN202420608066.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-27
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-03-27
AI Technical Summary
In large die-casting molds, metal liquids travel too long inside the mold, causing stagnation, affecting the product molding pass rate.
Multiple inlet port groups are designed, including two or more inlet gates, located on different facades of the mold, forming an outer eight-character structure, reducing the flow route of metal liquid inside the mold, and improving the efficiency of quickly filling the cavity.
It improves the product forming pass rate and efficiency, reduces the injection pressure and production costs, reduces the tonnage demand of die-casting die forging machines, and enhances the efficiency of the walking route of pressurized metal materials in the mold.
Smart Images

Figure CN222020635U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a casting mould for non-ferrous metal materials, more specifically, it relates to a combined casting mould for the same or different non-ferrous metal materials. Background Art
[0002] The die-casting mold is a kind of mold for casting liquid forging. The die-casting mold completes the molding of metal products on a special die-casting forging machine. The basic molding process is: the molten metal is first cast and filled into the mold cavity at a low or high speed. The mold has a movable cavity surface, which is pressurized and forged as the molten metal cools, which not only eliminates the shrinkage defects of the blank, but also makes the internal structure of the blank reach the broken grains of the forged state.
[0003] However, when the metal liquid flows in the die-casting mold, it is also a cooling process. For larger molds, due to the large size of the mold, the metal liquid has a long path inside the mold and stagnates at the end, affecting the product molding, resulting in a decrease in the product qualification rate. Utility Model Content
[0004] The utility model aims to provide a combined casting mold, which adopts multiple feed port groups to feed solid, semi-solid and liquid non-ferrous metal materials into the mold cavity, so that the non-ferrous metal materials with pressure can quickly fill the mold cavity, and the qualified rate of large and super-large product workpieces can be improved.
[0005] The above technical objectives of the utility model are achieved through the following technical solutions:
[0006] A combined casting mold comprises a mold body, wherein the mold body comprises at least two feed port groups, the feed port groups are located on the outer facade of the mold body, and the feed port groups are connected with a mold cavity in the mold body.
[0007] Preferably, there are two feed port groups, which are symmetrically located on two sides of the mold body.
[0008] Preferably, one feed port group includes at least one pouring port, and the pouring port is a circular port or a special-shaped port.
[0009] Preferably, one feed port group includes two pouring ports.
[0010] Preferably, the diameter of the pouring gate is A, the distance between two adjacent pouring gates is greater than 5A, and the two adjacent pouring gates form an outward-facing "X" structure.
[0011] Preferably, the mold body comprises an upper mold and a lower mold, and the pouring gate is located at the parting surface between the upper mold and the lower mold.
[0012] In summary, the utility model has the following beneficial effects:
[0013] (1) This design uses more than two pouring gates. This design increases the route for the molten metal to enter the die-casting mold, and the pouring gates are on different facades of the die-casting mold, so that the molten metal can quickly enter the mold and form quickly inside the mold; for large die-casting molds. More than two pouring gates can quickly fill the molten metal into the die-casting mold, avoiding the situation where the molten metal has a long route inside the mold and stagnates at the end, affecting the product molding, thereby improving the qualification rate and efficiency. The injected molten metal can also be replaced by metal particles or semi-solid metal.
[0014] Moreover, due to the two pouring gates, the injection route is shortened, the injection pressure is reduced, and the tonnage of the die-casting forging machine can also be reduced, reducing the purchase cost; unlike the large die-casting mold with a single pouring gate, the die-casting does not need to have a very high clamping pressure, so the tonnage of the die-casting forging machine is also larger.
[0015] Therefore, the die-casting mold with multiple pouring gates in this design has the advantage of lowering the product molding cost compared to the die-casting mold with a single pouring gate.
[0016] (2) The symmetrical arrangement of the pouring gates can most effectively shorten the travel path of the pressurized metal material in the mold. The pressurized metal material at one pouring gate only needs to travel halfway before it can merge with the pressurized metal material on the other side, which can greatly improve the molding rate of the product.
[0017] (3) If two adjacent pouring gates on one side are too close, the molten metal on both sides will mix quickly, and the effect is similar to injection from one pouring gate. Therefore, it is necessary to increase the distance between the two pouring gates on the same side. This design effectively improves the problem by making the distance between the two pouring gates more than 5 times the diameter of the pouring gate.
[0018] Moreover, the outward-facing X-shaped layout increases the flow intersection distance between two adjacent pouring gates, thereby increasing the efficiency of the molten metal quickly filling the interior of the mold.
[0019] (4) The special-shaped opening can be a hexagonal opening, a semicircular opening or an elliptical opening, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 is a front view of Example 1;
[0021] Figure 2 is a top view of the lower mold in Example 1;
[0022] Figure 3 is a top view of Example 2;
[0023] Figure 4 This is a cross-sectional view of Example 3 when the mold is closed.
[0024] In the figure:
[0025] 1. Mold body; 11. Upper mold; 12. Lower mold; 2. Feed inlet group; 21. Pouring gate; 3. Cavity; 41. Protruding ring; 42. Groove. DETAILED DESCRIPTION
[0026] The utility model is further described in detail below in conjunction with the accompanying drawings.
[0027] Example 1, a casting mold, referring to Figure 1-Figure 2 The present invention comprises a die body 1 for pressure casting of nonferrous metals. The die body 1 comprises an upper die 11 and a lower die 12.
[0028] The mold body 1 includes two feed port groups 2 symmetrically located on two sides of the mold body 1 .
[0029] The feed inlet group is located on the outer facade of the mold body; the outer facade in other embodiments may refer to the bottom surface or the top surface, and the feed inlet group is used for injection, pressing and extrusion.
[0030] The feed port group 2 is located on the side of the mold body 1 , and the feed port group 2 is connected to the cavity 3 in the mold body 1 .
[0031] One feed port group 2 includes two pouring ports 21, which are circular ports; the pouring ports 21 are located at the parting surface of the upper mold 11 and the lower mold 12. The parting surface is the fitting surface of the upper mold 11 and the lower mold 12, and the position of the pouring ports 21 is designed to facilitate demoulding.
[0032] The diameter of the pouring gate 21 is A. On the same side, the distance between two adjacent pouring gates 21 is 6A. The two adjacent pouring gates 21 form an outward-facing "X" structure. The metal liquid injection syringe is horizontally arranged at the two pouring gates 21. The metal liquid flows in an outward-facing "X" shape at the two pouring gates 21, thereby achieving the purpose of rapid flow of metal toward both sides of the mold cavity and slowing down the time for the metal liquids of the two pouring gates 21 on the same side to impact each other in the cavity.
[0033] In the present design, the mold uses more than two pouring ports 21 for pouring at different sides, thus shortening the path of the molten metal in a single pouring port 21 in the mold.
[0034] It should be noted that for a large die-casting mold, a pouring gate 21 is used. Even if multiple internal diversion channels are used, in order to fill the entire die-casting mold with molten metal, the molten metal must flow from the only pouring gate 21 to the entire cavity 3 inside the mold. In large die-casting molds, such as automobile frame die-casting molds, in order to allow the molten metal to quickly fill the inside of the die-casting mold, extremely high injection pressure has to be used, which places higher requirements on the mold closing pressure of the die-casting equipment. Some die-casting molds have a pressure requirement of 2,000 tons. Because the injection pressure is too high, if the die-casting mold is closed, it is easy to leak, which causes the mold closing pressure to increase simultaneously.
[0035] This increases the production difficulty and production cost of die-casting equipment, and this design can solve this technical defect. This design uses multiple injection ports, which are located on both sides or multiple sides of the die-casting mold. For large die-casting molds, it uses two symmetrical injection ports to inject molten metal. The actual flow route of the molten metal in the die-casting mold is only half of the die-casting mold cavity 3, so that the molten metal can quickly fill the inside of the die-casting mold without requiring a large injection pressure. It can greatly reduce the cost of large die-casting molds when producing products. It also provides a feasible solution for large die-casting molds to produce products.
[0036] Embodiment 2, a combined casting mold, which is different from embodiment 1 in that, with reference to Figure 3 There are three pouring ports 21 , which are located on three sides of the mold body 1 .
[0037] Embodiment 3, a combined casting mold, which is different from Embodiment 1 or Embodiment 2 in that, with reference to Figure 4 The upper die 11 is fixed with a convex ring 41, and the lower die 12 is provided with a groove 42. The convex ring 41 is located at the periphery of the cavity 3, and the convex ring 41 and the groove 42 are matched with each other in upper and lower clearances.
[0038] The convex ring 41 is annular as a whole, and is disconnected at the pouring port 21. Such a design increases the route when the upper mold 11 and the lower mold 12 are closed, making it more difficult for the molten metal to leak from the mold closing state. Because the pouring port of the mold is increased in this design, it is necessary to improve the sealing performance of the mold closing edge.
[0039] The above is only a preferred embodiment of the present invention. The protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A casting mold, comprising a mold body (1), characterized in that: The mold body (1) comprises at least two feed port groups (2), the feed port groups (2) are located on the outer facade of the mold body (1), and the feed port groups (2) are connected to the mold cavity (3) in the mold body (1).
2. The combined casting mold according to claim 1, characterized in that: There are two feed port groups (2), which are symmetrically located on two sides of the mold body (1).
3. The combined casting mold according to claim 1, characterized in that: One feed port group (2) comprises at least one pouring port (21), and the pouring port (21) is a circular port or a special-shaped port.
4. The combined casting mold according to claim 3 is characterized in that: One feed port group (2) includes two pouring ports (21).
5. The combined casting mold according to claim 4 is characterized in that: The diameter of the pouring opening (21) is A, the distance between two adjacent pouring openings (21) is greater than 5A, and the two adjacent pouring openings (21) form an outward-facing "X" structure.
6. The combined casting mold according to claim 3 is characterized in that: The mold body (1) comprises an upper mold (11) and a lower mold (12), and a pouring port (21) is located on the parting surface between the upper mold (11) and the lower mold (12).
7. The combined casting mold according to claim 6 is characterized in that: The upper die (11) is fixed with a convex ring (41), the lower die (12) is provided with a groove (42), the convex ring (41) is located at the periphery of the cavity (3), and the convex ring (41) and the groove (42) are matched with each other in upper and lower clearances.