Cement seal structure for oil pipe of coal-bed gas well

The cement sealing structure of the oil pipe of the coalbed methane well is used to isolate the cement and liquid in the wellbore by isolating the mixing of the cement and the liquid in the wellbore, which can effectively seal the coal seam deep buried or perforated sections on the upper part, and solve the poor sealing effect in the existing technology Problem, wellbore integrity and pressure bearing capacity have been restored.

CN222066702UActive Publication Date: 2024-11-26SHANXI LANYAN COALBED METHANE ENG RES CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420261414.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-02
Publication Date
2024-11-26
Estimated Expiration
2034-02-02

Smart Images

  • Figure CN222066702U_ABST
    Figure CN222066702U_ABST
Patent Text Reader

Abstract

The utility model provides a coal-bed gas well oil pipe cementing sealing layer structure, which belongs to the technical field of coal-bed gas well completion transformation and comprises a well mouth and a shaft positioned below the well mouth. The well mouth comprises a well mouth I used for injecting cement paste into the shaft and a well mouth II used for injecting displacing fluid into the shaft; the size of the plunger of the wellhead I is larger than that of the plunger of the wellhead II; the shaft comprises a surface casing, a production casing, an oil pipe, a pen point, a clear water layer, a cement paste layer, a sand filling layer and a bridge plug. When the burial depth of a target coal seam is large or a perforation section exists on the upper portion of the target coal seam, the coal-bed gas well oil pipe cementing sealing layer structure is used for blocking the developed coal seam, the sealing layer effect can be effectively achieved, the integrity of a shaft can be recovered after a cement paste layer in a production casing pipe is drilled, and the well quality is improved. And the problems that the drift diameter is reduced and the pressure bearing capacity is reduced due to a casing patching sealing layer method can also be effectively solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of coalbed methane well completion and transformation, and specifically discloses a coalbed methane well oil pipe cementing sealing structure. Background Art

[0002] In the process of coalbed methane well development, different coal seams revealed by drilling are usually developed sequentially or in coordination. In order to test different coal seams, or when some coal seams have a large water production, it is sometimes necessary to plug some coal seams so that other coal seams can be developed.

[0003] At present, the commonly used sealing method is mainly the casing patching method. This method inserts an expansion tube into the casing, expands it in the diameter direction by mechanical or hydraulic methods, directly patches and seals the perforation section, and achieves the sealing effect. This method is widely used in the field of coalbed methane wells, but it has two obvious disadvantages. First, the wall thickness of the lining expansion tube will become thinner after expansion, resulting in a decrease in the pressure bearing capacity. If the sealing layer needs to be fracturing to develop other coal seams later, it is obviously not applicable; second, after the casing is patched, the diameter of the expansion tube will inevitably become smaller, which will affect the operation of the pipe string in the well in the later stage or the operation of the drainage and production equipment underground, and it is easy to cause underground accidents. In view of this situation, the use of oil well cement to seal the target coal seam can effectively solve the above two problems.

[0004] When the target plugging coal seam is buried at a large depth, if the bare casing cementing method is used, due to the large volume of the wellbore and the large amount of liquid in the wellbore, the density of the cement slurry will decrease rapidly after mixing with the liquid in the wellbore, affecting the cement bonding effect; if there is a perforation section on the upper part of the target plugging coal seam, the bare casing cementing method cannot be used. Utility Model Content

[0005] The utility model provides a coalbed methane well oil pipe cementing sealing structure to solve the problem that when the target plugging coal seam is buried deep or there is a perforation section on the upper part of the target plugging coal seam, it is impossible to use the bare casing cementing method for plugging, and the use of the casing supplement sealing method will lead to a smaller diameter and a reduced pressure bearing capacity.

[0006] The above-mentioned coalbed methane well oil pipe cementing sealing structure includes a wellhead and a wellbore located below the wellhead; the wellhead includes wellhead I for injecting cement slurry into the wellbore and wellhead II for injecting displacement fluid into the wellbore; the plunger size of wellhead I is larger than the plunger size of wellhead II; the wellbore includes surface casing, production casing, oil pipe, pen tip, clear water layer, cement slurry layer, sand filling layer and bridge plug; the production casing is located in the surface casing; a perforation section is arranged at a position of the production casing corresponding to the target blocked coal seam; the oil pipe is located in the production casing, and a pen tip is installed at the bottom end, and the pen tip is located above the perforation section of the production casing; the clear water layer and the cement slurry layer are located in the production casing and in the oil pipe and the pen tip; the cement slurry layer is located below the clear water layer, and extends from the pen tip and the perforation section of the production casing to the target blocked coal seam; the sand filling layer and the bridge plug are located in the production casing, the sand filling layer is located below the cement slurry layer, and the bridge plug is located below the sand filling layer.

[0007] The boundary layer between the clear water layer and the cement slurry layer is located at the connection between the oil pipe and the pen tip.

[0008] The wellhead also includes backwash wellhead I and backwash wellhead II.

[0009] Compared with the prior art, the utility model has the following beneficial effects:

[0010] When the target coal seam is buried at a great depth, or there is a perforated section on the upper part of the target coal seam, the developed coal seam can be sealed by using the above-mentioned coalbed methane well tubing cement sealing structure, which can effectively achieve the sealing effect. After drilling through the cement slurry layer in the production casing, the integrity of the wellbore can be restored. It can also effectively solve the problems of reduced diameter and decreased pressure bearing capacity caused by the casing supplement sealing method. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0012] Figure 1 Schematic diagram of the pipe string used for cementing and sealing structure of oil pipe in coalbed methane well;

[0013] Figure 2 Schematic diagram of a wellhead used for cementing and sealing structures of oil pipes in coalbed methane wells;

[0014] Figure 3 Schematic diagram of a cement sealing structure for a coalbed methane well oil pipe in state 1;

[0015] Figure 4A schematic diagram of a cement sealing structure for a coalbed methane well oil pipe in state 2;

[0016] Figure 5 A schematic diagram of a cement sealing structure for a coalbed methane well oil pipe in state 3;

[0017] Figure 6 Schematic diagram of the cementing seal structure of the coalbed methane well oil pipe in state 4 (completed state).

[0018] In the figure: 1-wellhead I; 2-wellhead II; 3-backwash wellhead I; 4-backwash wellhead II; 5-surface casing; 6-production casing; 7-oil pipe; 8-pen tip; 9-clear water layer; 10-cement slurry layer; 11-sand filling layer; 12-bridge plug; 100-target plugging coal seam; 200-upper perforation section. DETAILED DESCRIPTION

[0019] The technical solution of the utility model will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] Example 1

[0021] This embodiment provides a coalbed methane well oil pipe cementing sealing structure, including a wellhead and a wellbore located below the wellhead.

[0022] The wellheads include wellhead Ⅰ1 for injecting cement slurry into the wellbore, wellhead Ⅱ2 for injecting displacement fluid into the wellbore, backwash wellhead Ⅰ3 and backwash wellhead Ⅱ4.

[0023] In order to achieve a better sealing effect, it is necessary to accurately calculate the volume of cement slurry and displacement fluid used to seal the formation. In this embodiment, the plunger size of wellhead Ⅰ1 is larger and is used to inject cement slurry. The construction speed can be increased during the cement injection process to prevent cement from being cemented and remaining in the ground pipe column and the wellhead; the plunger size of wellhead Ⅱ2 is smaller and is used to inject displacement fluid. The injection speed of the displacement fluid can be better controlled to achieve accurate displacement.

[0024] The wellbore includes a surface casing 5, a production casing 6, an oil pipe 7, a pen tip 8, a clear water layer 9, a cement slurry layer 10, a sand filling layer 11 and a bridge plug 12; the production casing 6 is located in the surface casing 5; a perforation section is provided at a position of the production casing 6 corresponding to the target plugged coal seam 100; the oil pipe 7 is located in the production casing 6, and a pen tip 8 is installed at the bottom end, and the pen tip 8 is located above the perforation section of the production casing 6; the clear water layer 9 and the cement slurry layer 10 are located in the production casing 6 and in the oil pipe 7 and the pen tip 8; the cement slurry layer 10 is located below the clear water layer 9, and extends from the pen tip 8 and the perforation section of the production casing 6 to the target plugged coal seam 100; the sand filling layer 11 and the bridge plug 12 are located in the production casing 6, the sand filling layer 11 is located below the cement slurry layer 10, and the bridge plug 12 is located below the sand filling layer 11. The boundary layer between the clear water layer 9 and the cement slurry layer 10 is located at the connection between the oil pipe 7 and the pen tip 8.

[0025] When the target layer is buried deep, if the bare casing cementing method is used, due to the large volume of the wellbore and the large amount of liquid in the wellbore, the density of the cement slurry will decrease rapidly after the cement slurry mixes with the liquid in the wellbore, affecting the cement bonding effect; if there is a perforated section above the target layer, the bare casing cementing method cannot be used. Figure 1 The pipe string shown in the figure is cemented, and the oil pipe 7 is lowered to the upper part of the target plugged coal seam 100. The cement slurry is injected from the oil pipe 7, which can effectively isolate the cement slurry from mixing with the liquid outside the oil pipe and protect the density of the cement slurry. At the same time, the use of the attached Figure 2 As shown in the fracturing wellhead, wellhead II2, backwash wellhead I3 and backwash wellhead II4 are closed during cementing process to ensure that cement slurry does not flow upward in the wellbore, prevent cement slurry from entering the annulus, and protect the upper perforated layer from being contaminated.

[0026] Example 2

[0027] Taking the SX-008 well in the Shixi block as an example, the specific implementation method of the above-mentioned coalbed methane well oil pipe cement sealing structure is introduced.

[0028] The SX-008 well was drilled to a depth of 1892m and completed with casing. The production casing is N80 casing with a diameter of 139.7mm and a wall thickness of 9.17mm. After fracturing, the 3# coal seam at 1645-1649m in the well produced a large amount of water and poor gas production. In order to develop other coal seams below, the 3# coal seam must be cemented. In view of the deep coal seam of the well, tubing cementing was selected for plugging.

[0029] (1) Well cleaning and pipe scraping

[0030] The Ф116mm×1500mm well-drilling gauge and 5 1 / 2" casing scraper were successively lowered into the well to the artificial well bottom, and the scraping was repeated 3 times 1m above and below the target plugging coal seam 100 (1645-1649m) and 1m above and below the intended sealing position of the bridge plug below the target plugging coal seam 100 (1679m).

[0031] Lift out the drilling string and check whether there are any marks on the drilling gauge. If there are marks, the well should be drilled again for detailed inspection and measures should be formulated to determine the integrity of the casing. If there are no marks, it is qualified.

[0032] (2) Well washing

[0033] Well washing should be carried out in a continuous cycle for more than two weeks until the inlet and outlet fluids have the same performance and the content of mechanical impurities is less than 0.2%.

[0034] (3) Bridge plugging

[0035] The well washing string was pulled out and the bridge plug was lowered from 12 to 1679m. According to the casing size, the bridge plug sealing tool combination from bottom to top was: 5 1 / 2" casing bridge plug + bridge plug setting tool + 3 1 / 2" N80 external thickened oil pipe to the wellhead.

[0036] (4) Pressure test

[0037] The pressure test string was lowered (packer position 1669m), and the bridge plug 12 was tested at 25MPa. The pressure drop within 30min was less than 0.5MPa, which was considered qualified. The pressure test string was pulled out after the pressure was released. In order to prevent the bridge plug from being fixed by cement and difficult to salvage, 20m of sand was filled after the pressure test string was pulled out.

[0038] (5) Lowering the pipe string

[0039] The tubing is lowered to 20 m above the perforation section of the production casing 6. The tubing string structure is as shown in the attached Figure 1 .

[0040] (6) Calculate the water absorption index

[0041] Fill the well with clean water. Maintain the pressure at 25MPa from wellhead Ⅰ1, record the amount of water entering the well per minute, and record the data for at least 5 minutes continuously.

[0042] (7) Low replacement cement slurry

[0043] After wellhead pressure relief, 6 tons of oil well cement was prepared to a density of 1.85 g / cm 3 Cement slurry 4.82m 3 , low-displace cement slurry into the wellbore from wellhead Ⅰ1, low-displace cement slurry to 4m 3 Close the casing gates (backwash wellhead Ⅰ3, backwash wellhead Ⅱ4) to prevent cement slurry from entering the annulus. At this time, there is 4m of cement slurry in the wellbore. 3(State 1). Then continue to replace the cement slurry until it is completely replaced, and then continue to squeeze 1m from the wellhead 1. 3 Clean water, at this time there is 4.1m of cement slurry in the wellbore 3 (State 2).

[0044] (8) Squeeze cement slurry into the ground

[0045] Close and clean wellhead Ⅰ1 and connect it for standby. Start pressurizing from wellhead Ⅱ2 to squeeze cement toward the perforation section; squeeze 3.6m of clean water from wellhead Ⅱ2 3 When the remaining cement slurry in the wellbore is 0.5m 3 (State 3). If the wellhead pressure is lower than 20MPa, stop working for 1 minute, then squeeze for 1 minute, and repeat this process, and ensure that the construction pressure does not exceed 30MPa.

[0046] (9) Hou Ning

[0047] A total of 3.87m of clean water was squeezed in from wellhead Ⅱ2 3 After that, the remaining cement slurry in the wellbore is 0.23m 3 (State 4). Open the casing gate and backwash the well from the backwash wellhead Ⅰ3; after the backwash is unblocked, pull out 10 oil pipes 7, set the wellhead, and wash the well again until it is unblocked. Then pressurize the wellhead to 15-20MPa, shut in the well and wait for 72h.

[0048] (10) Pressure test

[0049] After the wellhead is depressurized, the wellhead is removed and the cementing pipe string is pulled out. The cement slurry layer 10 is drilled and pressure tested. After the pressure test is qualified, sand is flushed to prepare for the next operation.

[0050] Note:

[0051] 1. The pump truck should accurately measure the amount of cement slurry and clean water;

[0052] 2. From the beginning of mixing cement to the beginning of setting, it must be completed within 45 minutes.

[0053] 3. Raw material preparation: clean water ≥ 100m 3 , oil well cement ≥ 6t (if it is bulk cement, 10% surplus should be prepared; if it is bagged cement, 30% surplus should be prepared);

[0054] 4. Check the tools and accessories before entering the well, measure the dimensions clearly and accurately, and draw a sketch;

[0055] 5. After the tool is lowered, the tool position must be calculated and confirmed to be correct before going down to the wellhead. When the downhole tool is connected to the oil pipe, the on-site technicians and the tool manufacturer's technicians must confirm it on site before going down to the well.

[0056] The above-mentioned coalbed methane well oil pipe cementing sealing structure is used in conjunction with a specific wellhead, and the amount of oil well cement and displacement fluid is accurately calculated to achieve effective sealing of the target coal seam. It is mainly suitable for layers with a large burial depth or a perforated section on the upper part. When different coal seams need to be tested, or certain specific coal seams need to be sealed due to geological or engineering reasons, this structure can be used for sealing.

[0057] The above is only a preferred embodiment of the utility model, and does not limit the utility model in other forms. Any person skilled in the art can use the above disclosed technical content to change or modify it into an equivalent embodiment with equivalent changes. However, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the utility model without departing from the technical solution of the utility model still belongs to the protection scope of the technical solution of the utility model.

Claims

1. A cementing sealing structure for a coalbed methane well oil pipe, comprising a wellhead and a wellbore located below the wellhead; The wellhead includes a wellhead I for injecting cement slurry into the wellbore and a wellhead II for injecting displacement fluid into the wellbore; It is characterized in that The plunger size of the wellhead I is larger than the plunger size of the wellhead II; The wellbore includes a surface casing, a production casing, a tubing, a pen tip, a clear water layer, a cement slurry layer, a sand filling layer and a bridge plug; The production casing is located inside the surface casing; The production casing is provided with a perforation section at a position corresponding to the target plugged coal seam; The oil pipe is located in the production casing, and a pen tip is installed at the bottom end, and the pen tip is located above the perforation section of the production casing; the clear water layer and the cement slurry layer are located in the production casing and in the oil pipe and the pen tip; The cement slurry layer is located below the clear water layer and extends from the pen tip and the perforation section of the production casing to the target plugging coal seam; The sand filling layer and the bridge plug are located in the production casing, the sand filling layer is located below the cement slurry layer, and the bridge plug is located below the sand filling layer.

2. The coalbed methane well oil pipe cementing sealing structure according to claim 1, characterized in that: The boundary layer between the clear water layer and the cement slurry layer is located at the connection between the oil pipe and the pen tip.