Protective structure for thermal breakage of silicon material

By using a quartz isolation chamber and a high-purity quartz isolation layer in the thermal break of silicon materials, the diffusion of impurities is prevented, and the problem of increased impurities on the surface of polycrystalline silicon raw material rods is solved, and the product quality and the processing capacity of the heating device are improved.

CN222076808UActive Publication Date: 2024-11-29JIANGSU XINHUA SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420286152.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-05
Publication Date
2024-11-29
Estimated Expiration
2034-02-05

AI Technical Summary

Technical Problem

In the heating furnace of electronic-grade polycrystalline silicon raw material rods, due to the diffusion of impurities in the isolation layer under high temperature environment, the impurity content on the surface of the silicon raw material rod increases, which increases the difficulty of the subsequent pickling process and affects product quality.

Method used

The outer quartz isolation chamber and the inner high-purity quartz isolation layer are used to surround the silicon raw material rod through the storage space surrounded by high-purity quartz parts and quartz plates, and a composite silver layer is provided on the surface of the corrugated plate structure to prevent impurities and ions. Diffusion while ensuring heat conduction performance.

Benefits of technology

It effectively prevents impurity ions in the quartz isolation layer from diffusing to the surface of the silicon raw material rod, reduces the difficulty of processing in the subsequent pickling process, and improves the impurity level on the product surface and the processing capacity of the heating device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222076808U_ABST
    Figure CN222076808U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of silicon raw material rod crushing, in particular to a protective structure for silicon material thermal breaking, which comprises an outer quartz isolation chamber and an inner high-purity quartz isolation layer, a first accommodating space is arranged in the quartz isolation chamber, and a support part is arranged in the first accommodating space and used for supporting a silicon raw material rod; the high-purity quartz isolation layer comprises high-purity quartz pieces on the two sides and a high-purity quartz plate on the top, the two high-purity quartz pieces are connected with the two sides of the supporting piece respectively, a second containing space is defined by the high-purity quartz pieces and the high-purity quartz plate, and the silicon raw material rod is surrounded by the second containing space; the high-purity quartz isolation layer prevents impurity ions in the quartz isolation layer from diffusing to the surface of the silicon raw material rod in the normal heat transfer process of crushing heat radiation of the electronic-grade polycrystalline silicon raw material rod, so that the treatment difficulty of a rear-end pickling process is reduced, the surface impurity level of the electronic-grade polycrystalline silicon raw material rod is ensured, and the service life of the electronic-grade polycrystalline silicon raw material rod is prolonged. Meanwhile, the processing capacity of the heating device on the silicon raw material rod is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of silicon raw material rod crushing, in particular to a protective structure for thermal crushing of silicon materials. Background Art

[0002] The existing hot quenching and crushing method is to place the silicon raw material rod in a heating furnace, change the binding force between the crystals according to the principle of thermal expansion and contraction, first heat it in a high temperature environment of 600~700℃, then immediately take it out and put it in water, and quickly immerse it in cold water to cause cracks to form on the main body of the silicon rod, and then tap it gently manually to achieve the purpose of breaking the silicon rod.

[0003] However, in the heating furnace for electronic-grade polysilicon raw material rods, since the polysilicon raw material rods are in a high-temperature environment for a long time, there is a certain temperature difference between the surface and the inside of the silicon raw material rods and the isolation layer. The impurity atoms in the isolation layer diffuse under high temperature conditions, which increases the difficulty of removing impurities in the subsequent pickling process, resulting in an increase in the impurity content on the surface of the polysilicon raw material rod products and a decrease in product quality.

[0004] The information disclosed in this background technology section is only intended to deepen the understanding of the overall background technology of the present invention, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art already known to those skilled in the art. Utility Model Content

[0005] The utility model provides a protective structure for thermal breakage of silicon materials, thereby effectively solving the problems in the background technology.

[0006] In order to achieve the above-mentioned purpose, the technical solution adopted by the utility model is: a protective structure for thermal break of silicon material, comprising: an outer quartz isolation chamber and an inner high-purity quartz isolation layer;

[0007] A first accommodating space is provided in the quartz isolation chamber, and a supporting member is provided in the first accommodating space for supporting the silicon raw material rod;

[0008] The high-purity quartz isolation layer includes high-purity quartz parts on both sides and a high-purity quartz plate on the top. The two high-purity quartz parts are respectively connected to the two sides of the support member. The high-purity quartz parts and the high-purity quartz plates are arranged to form a second accommodating space, and the second accommodating space surrounds the silicon raw material rod.

[0009] Furthermore, the cross-section of the high-purity quartz isolation layer is a corrugated plate structure, and a composite silver layer is provided on the surface of the corrugated plate structure.

[0010] Furthermore, the cross-section of the corrugated plate structure is one of a V-shape and a rectangle.

[0011] Furthermore, the extension direction of the corrugated plate structure is arranged parallel to the length direction of the silicon raw material rod.

[0012] Furthermore, the composite silver layer is a silver steel plate layer provided on the surface of the corrugated plate structure, and the silver steel plate layer and the corrugated plate structure are bonded and fixed with high temperature resistant glue.

[0013] Furthermore, the composite silver layer is a silver coating applied on the surface of the corrugated plate structure.

[0014] Furthermore, a first connecting piece is provided at the connection between the high-purity quartz plate and the high-purity quartz piece, so that the top of the second containing space can be opened.

[0015] Furthermore, a second connecting member is provided between the supporting member and the high-purity quartz member.

[0016] Furthermore, a detection device is provided on the high-purity quartz isolation layer for detecting whether the second containing space is closed.

[0017] Furthermore, a support platform is provided in the quartz isolation chamber, and the support member is provided on the support platform.

[0018] The beneficial effects of the utility model are as follows: the utility model provides an outer quartz isolation chamber and an inner high-purity quartz isolation layer, wherein the high-purity quartz isolation layer ensures the normal heat transfer process of the electronic-grade polysilicon raw material rod crushing heat radiation, prevents the impurity ions in the quartz isolation layer from diffusing to the surface of the silicon raw material rod, reduces the processing difficulty of the back-end pickling process, thereby ensuring the surface impurity level of the electronic-grade polysilicon raw material rod, and at the same time improves the processing capacity of the heating device for the silicon raw material rod. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0020] Figure 1 A schematic diagram of a protective structure for thermal breakage of silicon material;

[0021] Figure 2 It is a schematic diagram of the structure of a high-purity quartz isolation layer;

[0022] Figure 3 Schematic diagram of the structure of a high-purity quartz plate;

[0023] Figure 4 For Figure 3A partial enlarged view of the middle A;

[0024] Figure 5 It is a schematic diagram of the structure of silicon raw material rod and V-shaped corrugated plate;

[0025] Figure 6 It is a schematic diagram of the structure of silicon raw material rods and rectangular corrugated plates.

[0026] Reference numerals: 1, quartz isolation chamber; 11, first accommodation space; 2, high-purity quartz isolation layer; 21, second accommodation space; 22, high-purity quartz member; 23, high-purity quartz plate; 231, corrugated plate structure; 232, composite silver layer; 24, first connecting member; 25, second connecting member; 3, support member; 4, support platform;

[0027] 01. Silicon raw material rod. DETAILED DESCRIPTION

[0028] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.

[0029] In the description of the present invention, it should be noted that the directions or positional relationships indicated by “center”, “up”, “down”, “left”, “right”, “vertical”, “horizontal”, “inside” and “outside”, etc., are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0030] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0031] like Figures 1 to 6 As shown: A protective structure for thermal breakage of silicon material, comprising: an outer quartz isolation chamber 1 and an inner high-purity quartz isolation layer 2;

[0032] A first accommodating space 11 is provided in the quartz isolation chamber 1, and a supporting member 3 is provided in the first accommodating space 11 for supporting the silicon raw material rod 01;

[0033] The high-purity quartz isolation layer 2 includes high-purity quartz parts 22 on both sides and a high-purity quartz plate 23 on the top. The two high-purity quartz parts 22 are respectively connected to the two sides of the support member 3. The high-purity quartz parts 22 and the high-purity quartz plate 23 are arranged to form a second accommodating space 21, and the second accommodating space 21 surrounds the silicon raw material rod 01.

[0034] When in use, after placing the electronic grade polysilicon raw material rod 01 on the support 3, the high purity quartz parts 22 on both sides are installed on the support 3, and the high purity quartz plate 23 is installed on the top of the high purity quartz parts 22 to form a second accommodating space 21, so that the entire silicon raw material rod 01 is placed in the high purity quartz interlayer, thereby preventing the surface of the silicon raw material rod 01 from contacting with the impurity ions formed by thermal diffusion under high temperature conditions.

[0035] By providing an outer quartz isolation chamber 1 and an inner high-purity quartz isolation layer 2, the high-purity quartz isolation layer ensures the normal heat transfer process of the broken heat radiation of the electronic-grade polysilicon raw material rod 01, prevents the impurity ions in the quartz isolation layer from diffusing to the surface of the silicon raw material rod 01, and reduces the processing difficulty of the back-end pickling process, thereby ensuring the surface impurity level of the electronic-grade polysilicon raw material rod 01, and at the same time improves the processing capacity of the heating device for the silicon raw material rod 01.

[0036] As a priority of the above-mentioned embodiment, the cross-section of the high-purity quartz isolation layer 2 is a corrugated plate structure 231, and a composite silver layer 232 is provided on the surface of the corrugated plate structure 231. Specifically, the composite silver layer 232 has a high thermal conductivity, so the surface is provided with this layer can significantly improve the thermal conductivity of the quartz isolation layer, which helps to more effectively transfer the heat from the heating source to the silicon raw material rod 01 and increase the heating rate; the design of the corrugated plate structure 231 increases the surface area of ​​the isolation layer, which helps to enhance the heat exchange efficiency, so that the high-purity quartz isolation layer 2 absorbs and releases heat more effectively, increases the heating rate, and further accelerates the processing capacity of the silicon raw material rod 01.

[0037] In this embodiment, the cross section of the corrugated plate structure 231 is V-shaped or rectangular, one of which is specifically, Figure 5 As shown, the corrugated plate structure 231 is a schematic diagram of a V-shaped structure; Figure 6 As shown, the corrugated plate structure 231 is a schematic diagram of a rectangular structure; on the one hand, the V-shaped and rectangular cross-section corrugated plate structure 231 can increase the surface area, thereby improving the heat conduction effect; on the other hand, the corrugated structure can reduce the stress and deformation caused by thermal expansion, which is very important for maintaining the integrity of the thermal break protection structure of the silicon raw material rod 01 in a high temperature environment.

[0038] The extension direction of the corrugated plate structure 231 is parallel to the length direction of the silicon raw material rod 01, which effectively conducts heat along the length direction of the silicon raw material rod 01, helps to improve the heating or cooling efficiency, and ensures that the temperature of the silicon raw material rod 01 is more uniform.

[0039] One implementation of the composite silver layer 232 is as follows: the composite silver layer 232 is a silver steel plate layer provided on the surface of the corrugated plate structure 231, and the silver steel plate layer and the corrugated plate structure 231 are bonded and fixed with high-temperature resistant glue. Specifically, on the one hand, silver is an excellent light-reflecting material, and thus the silver steel plate layer can enhance the light-reflecting properties of the composite silver layer 232, and help to reflect light radiation from the heating source back to the silicon raw material rod 01, thereby improving the utilization efficiency of thermal energy, and increasing the surface heating rate of the silicon raw material rod 01, thereby improving efficiency; on the other hand, the silver steel plate layer as a supporting structure can increase the strength of the entire protective structure, can provide sufficient mechanical support, maintain the shape of the corrugated plate structure 231, and maintain the overall structural integrity under high temperature conditions. In addition, the use of high-temperature resistant glue for bonding and fixing can simplify the manufacturing process, reduce manufacturing costs, and make it easier to achieve integrated assembly of the structure.

[0040] Another implementation of the composite silver layer 232: The composite silver layer 232 is a silver coating applied to the surface of the corrugated plate structure 231. On the one hand, the silver coating can be relatively evenly applied to the surface of the corrugated plate structure 231, and has strong adaptability, and can meet the needs of protective structures of different shapes and sizes; on the other hand, compared to thick silver steel plates, the silver coating helps to reduce the weight of the overall structure while maintaining excellent light reflection and thermal conductivity, thereby making the protective structure for thermal rupture of silicon materials lighter; in addition, applying the silver coating is simpler than making silver steel plates, which can simplify the manufacturing process, improve production efficiency, and may reduce manufacturing costs.

[0041] Among them, a first connecting member 24 is provided at the connection between the high-purity quartz plate 23 and the high-purity quartz part 22, so that the top of the second accommodating space 21 can be opened. Specifically, an implementation manner of the first connecting member 24 is that the first connecting member 24 uses high-purity quartz to make a snap body, and the snap body can be fixed on the high-purity quartz part 22. The handle of the snap can be rotated, and a connecting structure is provided between the body and the handle. By rotating the handle, the handle is pressed against the top of the high-purity quartz plate 23, thereby pressing the connection between the high-purity quartz plate 23 and the high-purity quartz part 22.

[0042] As a priority of the above-mentioned embodiment, a second connecting member 25 is provided between the support member 3 and the high-purity quartz member 22. The above-mentioned second connecting member 25 is made of high-purity quartz, and the high-purity quartz members 22 on both sides can be fixed to the support member 3 by plugging, clamping, thread locking, etc., so as to facilitate the disassembly and assembly of the high-purity quartz members 22, and the replacement and maintenance of the high-purity quartz members 22 on both sides.

[0043] Both the first connector 24 and the second connector 25 are detachable connections. On the one hand, the detachable connection has the characteristics of quick installation and disassembly, so that the structure can be quickly disassembled when necessary, which is convenient for repair or replacement of parts and improves maintenance efficiency; on the other hand, the use of detachable connection can avoid the use of accessories such as bolts and nuts, simplifying the structural design, making the entire silicon raw material rod 01 thermal break protection structure more compact and lightweight; in addition, the design of the first connector 24 and the second connector 25 can ensure the sealing of the connection and prevent the external environment from interfering with the thermal break of the silicon raw material rod 01, which is crucial for maintaining a high-purity environment and ensuring the stable operation of the thermal break of the silicon raw material rod 01.

[0044] In this embodiment, a detection device is provided on the high-purity quartz isolation layer 2 to detect whether the second accommodating space 21 is closed. Specifically, the detection device helps to improve the control accuracy of the thermal breaking process of the silicon raw material rod 01 and ensure that the equipment operates under optimal working conditions. The presence of the detection device can reduce human errors and provide an automated monitoring system to promptly detect and report the situation of unclosed structure, thereby reducing the possibility of human negligence. By promptly detecting and resolving the situation of unclosed structure, the risk of failure caused by structural problems in the thermal breaking of the silicon raw material rod 01 can be reduced, thereby improving the reliability and stability of the equipment.

[0045] The above-mentioned detection device can be at least one of a high-temperature photoelectric sensor, a high-temperature pressure sensor, a high-temperature resistant ultrasonic sensor and a high-temperature resistant micro switch.

[0046] Among them, a support platform 4 is provided in the quartz isolation chamber 1, and a support member 3 is provided on the support platform 4. Specifically, the existence of the support platform 4 provides a stable foundation, so that the support member 3 is arranged upward, so that when the silicon raw material rod 01 is placed on the support member 3, it is just at the height of the middle of the first accommodating space 11, which helps to distribute heat more evenly and prevent problems caused by uneven heat. It is very important in the process of processing silicon raw materials in a high-temperature environment, and can improve the stability and efficiency of the process.

[0047] Those skilled in the art should understand that the present invention is not limited by the above embodiments. The above embodiments and the description are only for explaining the principle of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which are within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A protective structure for thermal breakage of silicon material, characterized in that: It includes an outer quartz isolation chamber and an inner high-purity quartz isolation layer; A first accommodating space is provided in the quartz isolation chamber, and a supporting member is provided in the first accommodating space for supporting the silicon raw material rod; The high-purity quartz isolation layer includes high-purity quartz parts on both sides and a high-purity quartz plate on the top. The two high-purity quartz parts are respectively connected to the two sides of the support member. The high-purity quartz parts and the high-purity quartz plates are arranged to form a second accommodating space, and the second accommodating space surrounds the silicon raw material rod.

2. The protective structure for thermal breakage of silicon materials according to claim 1, characterized in that: The cross section of the high-purity quartz isolation layer is a corrugated plate structure, and a composite silver layer is provided on the surface of the corrugated plate structure.

3. The protective structure for thermal breakage of silicon material according to claim 2, characterized in that: The cross section of the corrugated plate structure is one of a V-shape and a rectangle.

4. The protective structure for thermal breakage of silicon material according to claim 2, characterized in that: The extending direction of the corrugated plate structure is arranged parallel to the length direction of the silicon raw material rod.

5. The protective structure for thermal breakage of silicon material according to claim 2, characterized in that: The composite silver layer is a silver steel plate layer arranged on the surface of the corrugated plate structure, and the silver steel plate layer and the corrugated plate structure are bonded and fixed by high temperature resistant glue.

6. The protective structure for thermal breakage of silicon material according to claim 2, characterized in that: The composite silver layer is a silver coating coated on the surface of the corrugated plate structure.

7. The protective structure for thermal breakage of silicon material according to claim 1, characterized in that: A first connecting piece is provided at the connection between the high-purity quartz plate and the high-purity quartz piece, so that the top of the second containing space can be opened.

8. The protective structure for thermal breakage of silicon material according to claim 1, characterized in that: A second connecting member is provided between the supporting member and the high-purity quartz member.

9. The protective structure for thermal breakage of silicon materials according to claim 1, characterized in that: A detection device is provided on the high-purity quartz isolation layer for detecting whether the second containing space is closed.

10. The protective structure for thermal breakage of silicon material according to any one of claims 1 to 9, characterized in that: A support platform is provided in the quartz isolation chamber, and the support member is provided on the support platform.