Industrial silicon furnace structure convenient for furnace bottom voltage measurement
By setting a carbonaceous conductive rod at the bottom of an industrial silicon furnace and detecting the voltage value using a voltage sensor, the problem of inaccurate adjustment of the electrode insertion depth is solved, and the accuracy of the electrode insertion depth and the stability and output of the industrial silicon furnace are improved.
Patent Information
- Application Number
- CN202420589759.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-25
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2034-03-25
AI Technical Summary
When the electrode depth is adjusted in the furnace, the accuracy of existing industrial silicon furnaces is insufficient, resulting in uneven insertion depth of the three-phase electrode, affecting the furnace condition and output.
Three carbonaceous conductive rods are installed inside the bottom of the industrial silicon furnace, and the voltage value at the conductive rod is detected through a voltage sensor, and the height position of the electrode relative to other electrodes is determined, providing an accurate reference for the electrode insertion depth.
It improves the accuracy of judging the depth of electrode insertion, enhances the operating stability and output of industrial silicon furnaces, and reduces the requirements for distribution workers' experience.
Smart Images

Figure CN222086643U_ABST
Abstract
Description
Technical field:
[0001] The utility model relates to an industrial silicon furnace structure, in particular to an industrial silicon furnace structure which is convenient for measuring furnace bottom voltage. Background technology:
[0002] In the normal production process of industrial silicon furnace, it is necessary to adjust the depth of the electrode into the furnace so that the three-phase electrodes are as equal as possible or within a reasonable error range to achieve the three-phase electrodes working on the same plane as much as possible. At present, the depth of the electrode into the furnace is usually determined based on the primary current of the transformer, the voltage of the copper tube at the output port, the collapse of the material in the furnace, and the sound of the electrode arcing. Due to the unevenness of the furnace charge, the unbalanced load of the three-phase electrode, and the drift of the neutral point in the furnace, this method of judging the electrode insertion depth based on the primary current of the transformer, the voltage of the copper tube at the output port, the collapse of the material in the furnace, and the sound of the electrode arcing is not accurate enough, resulting in inexperienced power distribution workers being unable to accurately judge the depth of the electrode inserted into the furnace bottom, resulting in uneven insertion depth of the three-phase electrode, which seriously affects the furnace condition and output of the industrial silicon electric furnace. Utility model content:
[0003] In order to solve the above problems, the utility model aims to provide an industrial silicon furnace structure which is convenient for measuring furnace bottom voltage.
[0004] The utility model is implemented by the following technical solutions:
[0005] An industrial silicon furnace structure convenient for furnace bottom voltage measurement comprises a furnace body consisting of a furnace bottom and a furnace wall, wherein the furnace bottom and the furnace wall are both built with high-aluminum refractory bricks; asbestos boards are arranged on the outer sides of the furnace bottom and the furnace wall;
[0006] An aluminum silicate fiber blanket and a side wall high aluminum refractory castable layer are sequentially arranged between the high aluminum refractory bricks of the furnace wall and the asbestos board of the furnace wall from the outside to the inside; a side wall carbonaceous cold ramming paste layer and a side wall carbon brick layer are sequentially arranged at the lower part of the inner side of the high aluminum refractory bricks of the furnace wall from the outside to the inside;
[0007] A bottom carbon brick layer is laid on the high-aluminum refractory bricks of the furnace bottom inside the side wall carbon cold ramming paste layer, and a bottom carbon cold ramming paste layer is laid on the bottom carbon brick layer inside the side wall carbon brick layer; a bottom high-aluminum refractory castable layer and a clay brick layer are laid in sequence from bottom to top between the high-aluminum refractory bricks of the furnace bottom and the asbestos board of the furnace bottom;
[0008] A furnace eye is provided at the lower part of the furnace wall, the furnace eye is arranged to be inclined downward from the inside to the outside, and a semi-graphite carbon-silicon carbide brick layer is provided around the furnace eye;
[0009] Three carbonaceous conductive rods are inserted between the high-alumina refractory bricks at the bottom of the furnace and the bottom carbon brick layer. The three carbonaceous conductive rods are arranged in a circular array and are respectively located directly below the three electrodes; and the distance between the inner end of the three carbonaceous conductive rods and the center of the circle where they are located is 1 to 1.5 m;
[0010] The three carbonaceous conductive rods are all connected to a voltage sensor disposed outside the furnace body through a wire, and a signal output end of the voltage sensor is signal-connected to a signal input end of a DCS.
[0011] Furthermore, the thickness of the asbestos board is 20-25 mm.
[0012] Furthermore, the thickness of the aluminum silicate fiber blanket is 15 to 25 mm.
[0013] Furthermore, the thickness of the side wall high-aluminum refractory castable layer is 20-25 mm; the thickness of the bottom high-aluminum refractory castable layer is 65-75 mm.
[0014] Furthermore, the thickness of the carbonaceous cold-ramming paste layer on the side wall is 50 to 70 mm; the thickness of the carbonaceous cold-ramming paste layer on the bottom is 180 to 230 mm.
[0015] Furthermore, the thickness of the side wall carbon brick layer is 350-450 mm; the thickness of the bottom carbon brick layer is 1000-1200 mm.
[0016] Furthermore, the thickness of the clay brick layer is 250-350 mm.
[0017] Furthermore, the thickness of the high-alumina refractory bricks at the furnace bottom is 250 to 350 mm.
[0018] Furthermore, the height of the side wall carbonaceous cold ramming paste layer and the side wall carbon brick layer is 800-1000 mm.
[0019] Advantages of the utility model:
[0020] The utility model arranges a carbon conductive rod inside the furnace bottom, and can detect the voltage value at the carbon conductive rod through the carbon conductive rod and the voltage sensor, thereby judging the height position of the electrode directly above the carbon conductive rod relative to the other two electrodes, thereby improving the accuracy of judging the insertion depth of the electrode, providing a reliable reference and basis for adjusting the depth of the electrode into the furnace, improving the stability and output of the industrial silicon furnace operation, and reducing the requirements for the working experience of the power distribution worker. Description of the drawings:
[0021] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0022] Figure 1 Schematic diagram of the overall structure of this embodiment;
[0023] Figure 2 for Figure 1 A partial enlarged view of the middle A;
[0024] Figure 3 for Figure 1 Schematic cross-section of the middle BB;
[0025] Figure 4 Schematic diagram of electrical signal in this embodiment.
[0026] In the figure: high alumina refractory brick 1, asbestos board 2, aluminum silicate fiber blanket 3, side wall high alumina refractory castable layer 4, side wall carbonaceous cold ramming paste layer 5, side wall carbon brick layer 6, bottom carbon brick layer 7, bottom carbonaceous cold ramming paste layer 8, bottom high alumina refractory castable layer 9, clay brick layer 10, furnace eye 11, semi-graphite carbon-silicon carbide brick layer 12, carbonaceous conductive rod 13, voltage sensor 14, DCS 15. Specific implementation method:
[0027] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0028] Embodiment 1:
[0029] like Figure 1-4 The structure of an industrial silicon furnace for convenient furnace bottom voltage measurement shown in the figure includes a furnace body composed of a furnace bottom and a furnace wall, the furnace body has a diameter of 9400 mm and a height of 4980 mm. The furnace bottom and the furnace wall are both built with high-aluminum refractory bricks 1; asbestos boards 2 are provided on the outer sides of the furnace bottom and the furnace wall;
[0030] Between the high-aluminum refractory bricks 1 of the furnace wall and the asbestos board 2 of the furnace wall, an aluminum silicate fiber blanket 3 and a side wall high-aluminum refractory castable layer 4 are sequentially arranged from the outside to the inside; at the lower part of the inner side of the high-aluminum refractory bricks 1 of the furnace wall, a side wall carbonaceous cold ramming paste layer 5 and a side wall carbon brick layer 6 are sequentially arranged from the outside to the inside;
[0031] A bottom carbon brick layer 7 is laid on the high-aluminum refractory bricks 1 of the furnace bottom inside the side wall carbon cold ramming paste layer 5, and a bottom carbon cold ramming paste layer 8 is laid on the bottom carbon brick layer 7 inside the side wall carbon brick layer 6; a bottom high-aluminum refractory castable layer 9 and a clay brick layer 10 are laid in sequence from bottom to top between the high-aluminum refractory bricks 1 of the furnace bottom and the asbestos board 2 of the furnace bottom;
[0032] A furnace eye 11 is provided at the lower part of the furnace wall, and the furnace eye 11 is tilted downward from the inside to the outside, with an inclination angle of 3°; a semi-graphite carbon-silicon carbide brick layer 12 is provided around the furnace eye 11;
[0033] Three carbonaceous conductive rods 13 are inserted between the high-alumina refractory bricks 1 at the bottom of the furnace and the bottom carbon brick layer 7. The three carbonaceous conductive rods 13 are arranged in a circular array and are respectively located directly below the three electrodes; and the distance between the relatively inner end of the three carbonaceous conductive rods 13 and the center of the circle in which they are located is 1 to 1.5 m.
[0034] In this embodiment, the thickness of the asbestos board 2 is 22mm, the horizontal thickness of the aluminum silicate fiber blanket 3 is 20mm, the horizontal thickness of the side wall high aluminum refractory castable layer 4 is 23mm; the thickness of the bottom high aluminum refractory castable layer 9 is 68mm; the horizontal thickness of the side wall carbonaceous cold ramming paste layer 5 is 60mm; the thickness of the bottom carbonaceous cold ramming paste layer 8 is 200mm; the side wall carbon brick layer 6 is made of semi-graphite roasted ring bricks, and the horizontal thickness is 400mm; the bottom The upper carbon brick layer 7 is composed of an upper semi-graphite baked carbon brick layer, a middle furnace bottom baked carbon brick layer and a lower furnace bottom baked carbon brick layer, wherein the upper semi-graphite baked carbon brick layer is made of semi-graphite baked carbon bricks with a length of 400 mm, a width of 1200 mm and a height of 400 mm, and the middle furnace bottom baked carbon brick layer and the lower furnace bottom baked carbon brick layer are both made of semi-graphite baked carbon bricks with a length of 345 mm, a width of 1200 mm and a height of 345 mm; therefore, the total thickness of the bottom carbon brick layer 7 is 1090 mm. The thickness of the clay brick layer 10 is 300 mm. The high-aluminum refractory bricks 1 of the furnace wall extend to the top of the carbonaceous cold-rammed paste layer 5 of the wall and the carbon brick layer 6 of the side wall, which improves the integrity of the overall structure, and the horizontal thickness of the high-aluminum refractory bricks 1 of the furnace wall can be gradually reduced from the top of the side wall carbon brick layer 6 to the top of the high-aluminum refractory bricks 1 of the furnace wall; the thickness of the high-aluminum refractory bricks 1 of the furnace bottom is 300mm. The vertical height of the carbonaceous cold-rammed paste layer 5 of the side wall and the carbon brick layer 6 of the side wall is 900mm. In this embodiment, all brick joints are no more than 1mm, and each layer must be strictly leveled. The top of the high-aluminum refractory castable layer 4 of the side wall extends to the top of the high-aluminum refractory brick 1 of the furnace wall, thereby making the overall performance of the two better; a carbonaceous cold-rammed paste layer with a horizontal thickness of 60mm is provided at the junction of the bottom of the inner side of the side wall carbon brick layer 6 and the bottom carbon brick layer 7; the bottom carbonaceous cold-rammed paste layer 8 at the furnace eye 11 is provided with a slope inclined downward in the direction of the furnace eye 11 to facilitate the silicon water out of the furnace.
[0035] The three carbon conductive rods 13 are all connected to a voltage sensor 14 disposed outside the furnace body through a wire, and a signal output end of the voltage sensor 14 is signal-connected to a signal input end of a DCS 15 .
[0036] Working principle:
[0037] In this embodiment, a carbonaceous conductive rod 13 is arranged inside the furnace bottom. Since the working voltages of the three electrodes are the same, the charge in the furnace body will consume electricity, and the bottom carbonaceous cold ramming paste layer 8 and the bottom carbon brick layer 7 arranged at the furnace bottom are both conductive materials with the same voltage drop. If the heights of the electrodes are different, the voltage drop generated by the charge will be different. Therefore, the voltage value at the carbonaceous conductive rod 13 can be detected by the carbonaceous conductive rod 13 and the voltage sensor 14, and then the height position of the electrode directly above the carbonaceous conductive rod 13 relative to the other two electrodes can be determined.
[0038] The outer layer materials of the furnace bottom and furnace wall act as insulators to prevent the furnace shell from conducting electricity. The high-alumina refractory bricks 1 are resistant to high temperatures and can prevent heat loss and deformation of the steel plates outside the furnace body caused by heat conduction. The carbon brick layer is conductive. The three-phase electrodes and the bottom carbon brick layer 7 generate arc heat to cause a reduction reaction in the materials in the furnace.
[0039] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An industrial silicon furnace structure for convenient furnace bottom voltage measurement, comprising a furnace body consisting of a furnace bottom and a furnace wall, characterized in that: The furnace bottom and the furnace wall are both built with high-aluminum refractory bricks; asbestos boards are provided on the outer sides of the furnace bottom and the furnace wall; An aluminum silicate fiber blanket and a side wall high aluminum refractory castable layer are sequentially arranged between the high aluminum refractory bricks of the furnace wall and the asbestos board of the furnace wall from the outside to the inside; a side wall carbonaceous cold ramming paste layer and a side wall carbon brick layer are sequentially arranged at the lower part of the inner side of the high aluminum refractory bricks of the furnace wall from the outside to the inside; A bottom carbon brick layer is laid on the high-aluminum refractory bricks of the furnace bottom inside the side wall carbon cold ramming paste layer, and a bottom carbon cold ramming paste layer is laid on the bottom carbon brick layer inside the side wall carbon brick layer; a bottom high-aluminum refractory castable layer and a clay brick layer are laid in sequence from bottom to top between the high-aluminum refractory bricks of the furnace bottom and the asbestos board of the furnace bottom; A furnace eye is provided at the lower part of the furnace wall, the furnace eye is arranged to be inclined downward from the inside to the outside, and a semi-graphite carbon-silicon carbide brick layer is provided around the furnace eye; Three carbonaceous conductive rods are inserted between the high-alumina refractory bricks at the bottom of the furnace and the bottom carbon brick layer. The three carbonaceous conductive rods are arranged in a circular array and are respectively located directly below the three electrodes; and the distance between the inner end of the three carbonaceous conductive rods and the center of the circle where they are located is 1 to 1.5 m; The three carbonaceous conductive rods are all connected to a voltage sensor disposed outside the furnace body through a wire, and a signal output end of the voltage sensor is signal-connected to a signal input end of a DCS.
2. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the asbestos board is 20-25 mm.
3. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the aluminum silicate fiber blanket is 15 to 25 mm.
4. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the side wall high-aluminum refractory castable layer is 20-25 mm; the thickness of the bottom high-aluminum refractory castable layer is 65-75 mm.
5. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the carbonaceous cold ramming paste layer on the side wall is 50 to 70 mm; the thickness of the carbonaceous cold ramming paste layer on the bottom is 180 to 230 mm.
6. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the side wall carbon brick layer is 350-450 mm; the thickness of the bottom carbon brick layer is 1000-1200 mm.
7. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the clay brick layer is 250-350 mm.
8. The industrial silicon furnace structure for convenient furnace bottom voltage measurement according to claim 1, characterized in that: The thickness of the high-alumina refractory bricks at the furnace bottom is 250-350 mm.