Single-sided thinned ultrathin glass cutting dissociation structure

By using a combined structure of spacer paper and acid-resistant film during ultra-thin glass etching, single-side thinning dissociation is achieved by using laser cutting, which solves the curling of dissociation film and the defect of edges during ultra-thin glass etching in the prior art. Problem, improving product integrity and production efficiency.

CN222097226UActive Publication Date: 2024-12-03CHONGQING YONGXIN TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420633911.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-29
Publication Date
2024-12-03
Estimated Expiration
2034-03-29

AI Technical Summary

Technical Problem

In the prior art, ultra-thin glass is prone to cracks due to the dissociation film curling during the etching process, poor edges and damage, and products that are too thin after etching are easily scrapped.

Method used

Using a combined structure of spacer paper and acid-resistant film, the single-side thinning and dissociation of the glass substrate is achieved through laser cutting, avoiding light dissociation, protecting the unetched surface of the glass substrate, and ensuring edge integrity.

Benefits of technology

It achieves rapid and reliable dissociation of ultra-thin glass, reduces loss rate and edge problems, and avoids product scrapping due to thinness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222097226U_ABST
    Figure CN222097226U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of ultra-thin glass, and relates to a single-face-thinned ultra-thin glass cutting and dissociating structure. Comprising spacing paper (1) and an anti-acid film (2), the size of the spacing paper (1) is larger than that of an effective area (4) of a glass substrate (3), the size of the anti-acid film (2) is larger than that of the effective area (4) of the glass substrate (3), and the size of the glass substrate (3) before cutting is larger than that of a finished product of the glass substrate (3). The cutting dissociation structure for the single-sided thinned ultra-thin glass is simple in structure, after a glass product is etched, rapid dissociation of the ultra-thin glass after single-sided thinning can be conveniently and rapidly achieved, meanwhile, the product is reliably protected, deformation of the product is avoided, the damage rate of the product is reduced, and poor edges of the product are avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of ultra-thin glass, and more specifically relates to a single-sided thinned ultra-thin glass cutting and dissociation structure. Background Art

[0002] In recent years, with the development of modern science and technology and the upgrading of electronic products, electronic products are developing in the direction of being smaller and lighter. Under-screen fingerprint sensing screens, ultra-thin folding screens and other products are more widely used in current electronic products. The glass thickness of such products is often below 50um. Therefore, when etching, ultra-thin products are basically mounted on the backplane. The disadvantages of the prior art are: Disadvantage 1: The unetched surface of the glass substrate (product) is adhered with a dissociation film, which will curl and warp after exposure to light, causing cracks in the product and causing damage; Disadvantage 2: During the etching process, the product ends have no protective measures, and the edges of the product are prone to defects after etching; Disadvantage 3: The product is too thin (50um) after etching, and the film is torn and dissociated, causing serious damage and scrapping. Therefore, the prior art affects the production and preparation of glass products.

[0003] In the prior art, there is a technology named "A process for dissociating glass carriers from ultra-thin wafers by penetration debonding of organic solvents" and the publication number is "CN112289734A". This technology discloses a process for dissociating glass carriers from ultra-thin wafers by penetration debonding of organic solvents, which includes the following steps: modification, bonding, thinning, debonding, immersion dissolution, and cleaning. The present invention uses a glass carrier with holes in combination with a composite adhesive film, which can provide a high-strength foundation for the process of back grinding and thinning of ultra-thin wafers, with low cost and good mass production. After the release layer is dissociated, the glass carrier can be freed from adhesion and has no adhesion, and the effect of dissociating the bonding is good, avoiding the risk of fragmentation of the ultra-thin wafer due to external stress during removal. This solves the problem that the release layer between the glass carrier and the adhesive can be deconstructed when the ultra-thin wafer is debonded in the prior art, but the stress change caused by the adhesive itself peeling off from the wafer surface still poses a high risk to the production of ultra-thin wafers. The pure immersion method is used, and the time required to achieve complete dissolution and peeling is relatively long, resulting in poor efficiency and feasibility.

[0004] However, this technology does not involve the technical problems and technical solutions of the present application. Utility Model Content

[0005] The technical problem to be solved by the utility model is: in view of the deficiencies in the prior art, a single-sided thinned ultra-thin glass cutting and dissociation structure is provided which has a simple structure and can conveniently and quickly realize the rapid dissociation after the ultra-thin glass is thinned on one side after etching of the glass product, while reliably protecting the product, avoiding deformation of the product, reducing the product damage rate, and avoiding poor product edge.

[0006] To solve the above-mentioned technical problems, the technical solution adopted by the utility model is:

[0007] The utility model discloses a single-sided thinned ultra-thin glass cutting and dissociation structure, comprising spacer paper and an acid-resistant film. The size of the spacer paper is larger than the size of the effective area of ​​the glass substrate, the size of the acid-resistant film is larger than the size of the effective area of ​​the glass substrate, and the size of the glass substrate before cutting is larger than the size of the finished glass substrate.

[0008] The acid-resistant film comprises a main body and a folded edge portion, wherein the folded edge portion is arranged along a circumference of a surface of one side of the main body, and the horizontal cross-sectional size of the groove formed by the main body and the folded edge portion is equal to the size of the spacer paper.

[0009] The size of the spacer paper includes the length and width of the spacer paper, and the size of the acid-resistant film includes the length and width of the acid-resistant film.

[0010] The effective area size of the glass substrate includes the length and width of the effective area; the size of the glass substrate before cutting includes the length and width, and the size of the finished glass substrate includes the length and width.

[0011] The glass substrate comprises an effective area located in the middle part and an ineffective area located along a peripheral edge of one side surface.

[0012] Before etching the single-sided thinned ultra-thin glass, the folded edge of the acid-resistant film is configured to fit the ineffective area of ​​the edge of the glass substrate, and the spacing paper is configured to be located in the groove body.

[0013] The length of the acid-resistant film is equal to the length of the glass substrate before cutting, and the width of the acid-resistant film is equal to the width of the glass substrate before cutting.

[0014] The length of the glass substrate before cutting is greater than the length of the finished glass substrate by more than 1 mm, and the width of the glass substrate before cutting is greater than the width of the finished glass substrate by more than 1 mm.

[0015] The acid-resistant film is a UV film.

[0016] The technical solution of the utility model is adopted, and the working principle and beneficial effects are as follows:

[0017] The single-sided thinning ultra-thin glass cutting and dissociation structure described in the utility model is to manufacture spacer paper and acid-resistant film according to the model and size of the specific glass substrate. And the respective sizes and corresponding sizes of the spacer paper, the acid-resistant film and the glass substrate are set. In this way, the cutting and dissociation requirements of the single-sided thinning ultra-thin glass are met. When the single-sided thinning ultra-thin glass is processed, the spacer paper is placed in the effective area of ​​the unetched surface of the glass substrate, and then the acid-resistant film is arranged on the unetched surface, so that the spacer paper is set to be located in the groove body, and the folded edge of the acid-resistant film fits the invalid area of ​​the edge of the glass substrate to protect the unetched surface of the glass substrate. After the glass substrate is completed, it needs to be dissociated, and the dissociation adopts a cutting method. The glass product is placed horizontally on the cutting platform, fixed by vacuum adsorption, laser cutting is adopted, and cutting is performed along the cutting icon, and the acid-resistant film, release paper, and the invalid area of ​​the product are directly cut off. Then, the vacuum adsorption is turned off, the cut part is removed, and the acid-resistant film and the release paper are removed together, and the product can be taken out with a suction cup to complete the dissociation. In this way, the glass substrate is no longer dissociated by light, and there is no problem of curling and warping of the acid-proof film (dissociated film) after light exposure, which naturally avoids cracks and damage defects in the product. During the etching process of the product, there is an invalid area on the glass substrate. After the etching is completed, the invalid area is cut, that is, the end of the product is an unaffected structure, eliminating the problem that the edge of the product is easily damaged after etching in the method of the prior art; in addition, the film is torn off after cutting, and the folded edge of the acid-proof film is mainly cut during cutting. After cutting, the acid-proof film has been separated from the glass substrate, and removing the acid-proof film will not generate external force on the glass substrate, so there will be no serious problem of damage and scrapping when the product is too thin after etching. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The following is a brief description of the contents and symbols in the drawings of this specification:

[0019] Figure 1 It is a structural schematic diagram of the spacing paper of the single-sided thinned ultra-thin glass cutting and dissociation structure described in the utility model;

[0020] Figure 2 It is a structural schematic diagram of the acid-proof film of the single-sided thinned ultra-thin glass cutting and dissociation structure described in the utility model;

[0021] Figure 3 A schematic structural diagram of a glass substrate of a single-sided thinned ultra-thin glass cutting and dissociation structure according to the utility model;

[0022] Figure 4 It is a schematic diagram of the cross-sectional structure of the single-sided thinned ultra-thin glass before cutting and dissociation according to the utility model;

[0023] The markings in the attached drawings are: 1, spacer paper; 2, acid-resistant film; 3, glass substrate; 4, effective area; 5, main body; 6, folded edge; 7, groove body; 8, ineffective area. DETAILED DESCRIPTION

[0024] The following is a detailed description of the embodiments of the present invention, such as the shapes, structures, positions and connection relationships of the components involved, the functions and working principles of the components, etc., by referring to the accompanying drawings:

[0025] As attached Figure 1 -Attached Figure 4As shown, the utility model is a single-sided thinning ultra-thin glass cutting and dissociation structure, including a spacer paper 1 and an acid-resistant film 2. The size of the spacer paper 1 is larger than the size of the effective area 4 of the glass substrate 3, the size of the acid-resistant film 2 is larger than the size of the effective area 4 of the glass substrate 3, and the size of the glass substrate 3 before cutting is larger than the finished size of the glass substrate 3. The above structure proposes an improved technical solution for the deficiencies in the prior art. When the structure is set, the spacer paper 1 and the acid-resistant film 2 are made according to the model and size of the specific glass substrate 3. And the respective sizes and corresponding sizes of the spacer paper 1, the acid-resistant film 2, and the glass substrate 3 are set. In this way, the single-sided thinning ultra-thin glass cutting and dissociation requirements are met. When the single-sided thinning ultra-thin glass is processed, the spacer paper 1 is placed in the effective area 4 of the unetched surface of the glass substrate, and then the acid-resistant film 2 is arranged on the unetched surface, so that the spacer paper 1 is set to be located in the groove body 7, and the folded edge portion 6 of the acid-resistant film 2 is attached to the invalid area 8 at the edge of the glass substrate 3, so as to protect the unetched surface of the glass substrate 3. After the glass substrate 3 is completed, it needs to be dissociated, and the dissociation adopts the cutting method instead of the illumination method. The glass substrate (glass product, product) is placed horizontally on the cutting platform, the glass substrate is fixed by vacuum adsorption, and laser cutting is adopted to cut along the cutting icon, and the ineffective areas of the acid-resistant film 2, the release paper 1, and the glass substrate 3 are directly cut off. Then, the vacuum adsorption is turned off, the cut part is removed, and the acid-resistant film and the release paper are removed together, and the product can be taken out with a suction cup to complete the dissociation. In this way, the glass substrate is no longer dissociated by illumination, and there is no problem that the acid-resistant film (dissociation film) 2 will curl and warp after illumination, which naturally avoids cracks in the glass product and produces damage defects. During the etching process of the product, the glass substrate 3 has an invalid area 8. After the etching is completed, the invalid area 8 is cut, that is, the end of the finished glass is not affected, eliminating the problem that the edge of the product is easily defective after etching in the method in the prior art; in addition, the film is torn off after cutting, and the acid-proof film folding part is mainly cut during cutting. Therefore, the acid-proof film has been separated from the glass substrate after cutting, and removing the acid-proof film will not generate external force on the glass substrate, and there will be no serious problem of damage and scrapping when the product is too thin (50um) after etching. The single-sided thinned ultra-thin glass cutting and dissociation structure described in the utility model has a simple structure. After the glass product is etched, it can conveniently and quickly realize the rapid dissociation of ultra-thin glass after single-sided thinning, and at the same time reliably protect the product, avoid deformation of the product, reduce the product damage rate, and avoid product edge defects.

[0026] The acid-resistant film 2 comprises a main body 5 and a folded edge 6, the folded edge 6 is arranged along a circumference of a surface of one side of the main body 5, and the horizontal cross-sectional size of the groove 7 formed by the main body 5 and the folded edge 6 is equal to the size of the spacer paper 1. In the above structure, the spacer paper, the acid-resistant film, and the glass substrate can all be square or rectangular. When processing single-sided thinned ultra-thin glass, the spacer paper 1 is placed in the effective area 4 of the unetched surface of the glass substrate, and then the acid-resistant film 2 is arranged on the unetched surface, so that the spacer paper 1 is arranged to be located in the groove 7, and the folded edge 6 of the acid-resistant film 2 is attached to the invalid area 8 of the edge of the glass substrate 3, so as to protect the unetched surface of the glass substrate 3.

[0027] The size of the spacer paper 1 includes the length and width of the spacer paper 1, and the size of the acid-resistant film 2 includes the length and width of the acid-resistant film 2. The size of the effective area 4 of the glass substrate 3 includes the length and width of the effective area 4; the size of the glass substrate 3 before cutting includes the length and width, and the size of the finished glass substrate 3 includes the length and width. The glass substrate 3 includes an effective area 4 located in the middle part and an invalid area 8 located along a peripheral edge of one side surface. Before the above structure is carried out, it is necessary to use spacer paper and acid-resistant film to protect the unetched surface of the glass substrate. The size of the glass substrate before cutting is slightly larger, which is convenient for subsequent cutting. After cutting, it is exactly the size of the required finished glass substrate. When the edge is cut, the edge is a structure that is not affected by etching, thereby effectively ensuring the quality of the end edge and eliminating the problems of the prior art.

[0028] When the single-sided thinned ultra-thin glass is etched, the folded edge portion 6 of the acid-resistant film 2 is set to a structure that can fit the invalid area 8 at the edge of the glass substrate 3, and the spacer paper 1 is set to a structure located in the groove body 7. The length of the acid-resistant film 2 is equal to the length of the glass substrate 3 before cutting, and the width of the acid-resistant film 2 is equal to the width of the glass substrate 3 before cutting. In the above structure, before etching, the glass substrate, the acid-resistant film, and the spacer paper are attached together, so as to reliably protect the unetched surface of the glass substrate. Then etching is performed, and cutting is performed after etching to obtain a finished glass product.

[0029] The length of the glass substrate 3 before cutting is greater than the length of the finished glass substrate 3 by more than 1 mm, and the width of the glass substrate 3 before cutting is greater than the width of the finished glass substrate 3 by more than 1 mm. With the above structure, when preparing the glass substrate, each of the four sides is increased by more than 1 cm to form an invalid area for subsequent cutting, and after cutting, a finished glass substrate that meets the size requirements is obtained, thereby solving the existing problems.

[0030] Because the single-sided thinned ultra-thin glass cutting and dissociation structure described in the utility model does not use a light dissociation method, UV can be replaced by a common acid-resistant film to reduce costs.

[0031] The single-sided thinning ultra-thin glass cutting and dissociation structure described in the utility model, when the structure is set, according to the model and size of the specific glass substrate 3, the spacer paper 1 and the acid-resistant film 2 are made. And the respective sizes and corresponding sizes of the spacer paper 1, the acid-resistant film 2 and the glass substrate 3 are set. In this way, the single-sided thinning ultra-thin glass cutting and dissociation requirements are met. When the single-sided thinning ultra-thin glass is specifically processed, the spacer paper 1 is placed in the effective area 4 of the unetched surface of the glass substrate, and then the acid-resistant film 2 is arranged on the unetched surface, so that the spacer paper 1 is set to be located in the tank body 7, and the folding part 6 of the acid-resistant film 2 fits the invalid area 8 of the edge of the glass substrate 3, so as to protect the unetched surface of the glass substrate 3. And after the glass substrate 3 is completed, it is necessary to dissociate, and the dissociation adopts the cutting method, and no longer adopts the illumination method. The glass substrate (glass product, product) is placed horizontally on the cutting platform, the glass substrate is fixed by vacuum adsorption, and laser cutting is adopted, and cutting is performed along the cutting icon, and the invalid areas of the acid-resistant film 2, the release paper 1 and the glass substrate 3 are directly cut out. Then, close the vacuum adsorption, remove the cut part, remove the acid-proof film together with the release paper, and then take out the product with a sucker to complete the dissociation. In this way, the glass substrate no longer dissociates by illumination, and there is no problem that the acid-proof film (dissociation film) 2 will curl and warp after illumination, which naturally avoids the glass product from cracking and producing a damage defect. In the etching process of the product, there is an invalid area 8 in the glass substrate 3. After etching is completed, the invalid area 8 is cut, that is, the end of the finished glass is not affected, eliminating the method in the prior art that the edge of the product is easily caused by the bad edge after etching; in addition, the film is torn after cutting, and the acid-proof film folding part is mainly cut during cutting, so that the acid-proof film is separated from the glass substrate after cutting, and taking away the acid-proof film will not produce external force on the glass substrate, and there will not be a serious problem of damage and scrapping when the product is too thin (50um) after etching.

[0032] The above is an exemplary description of the utility model in conjunction with the accompanying drawings. It is obvious that the specific implementation of the utility model is not limited to the above-mentioned method. As long as various improvements are made using the method concept and technical solution of the utility model, or the concept and technical solution of the utility model are directly applied to other occasions without improvement, they are all within the protection scope of the utility model.

Claims

1. A single-sided thinned ultra-thin glass cutting and dissociation structure, characterized in that: The invention comprises a spacer paper (1) and an acid-resistant film (2); the size of the spacer paper (1) is larger than the size of an effective area (4) of a glass substrate (3); the size of the acid-resistant film (2) is larger than the size of the effective area (4) of the glass substrate (3); and the size of the glass substrate (3) before cutting is larger than the size of the finished glass substrate (3).

2. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 1, characterized in that: The acid-resistant film (2) comprises a main body (5) and a folded edge (6), wherein the folded edge (6) is arranged along a circumference of a surface of one side of the main body (5), and the horizontal cross-sectional size of the groove (7) formed by the main body (5) and the folded edge (6) is equal to the size of the spacer paper (1).

3. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 1 or 2, characterized in that: The size of the spacer paper (1) includes the length and width of the spacer paper (1), and the size of the acid-resistant film (2) includes the length and width of the acid-resistant film (2).

4. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 1 or 2, characterized in that: The size of the effective area (4) of the glass substrate (3) includes the length and width of the effective area (4); the size of the glass substrate (3) before cutting includes the length and width; and the size of the finished glass substrate (3) includes the length and width.

5. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 2, characterized in that: The glass substrate (3) comprises an effective area (4) located in the middle and an ineffective area (8) located along a peripheral edge of one side surface.

6. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 5, characterized in that: When etching the single-sided thinned ultra-thin glass, the folded edge portion (6) of the acid-resistant film (2) is configured to be in contact with the ineffective area (8) at the edge of the glass substrate (3), and the spacer paper (1) is configured to be located within the groove body (7).

7. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 3, characterized in that: The length of the acid-resistant film (2) is equal to the length of the glass substrate (3) before cutting, and the width of the acid-resistant film (2) is equal to the width of the glass substrate (3) before cutting.

8. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 4, characterized in that: The length of the glass substrate (3) before cutting is greater than the length of the finished glass substrate (3) by more than 1 mm, and the width of the glass substrate (3) before cutting is greater than the width of the finished glass substrate (3) by more than 1 mm.

9. The single-sided thinned ultra-thin glass cutting and dissociation structure according to claim 1 or 2, characterized in that: The acid-resistant film (2) is a UV film.