NMP recovery system for coating area of lithium battery factory
By introducing a direct expansion system into the NMP recycling system of the lithium battery factory, the NMP and moisture in the NMP waste gas are removed by using the evaporator and condenser, and the problem of high energy consumption of the equipment is solved through the heat exchange between the refrigerant and the regenerated air, and the problem of high equipment consumption is achieved. Efficient recycling of NMP waste liquid and reduced energy consumption.
Patent Information
- Application Number
- CN202420108722.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-16
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-01-16
AI Technical Summary
The existing waste heat recovery + deep condensation device + rotary wheel process. During the NMP recycling process in lithium battery factories, the equipment consumes a high energy consumption, especially in the rotary wheel regeneration area.
Set up a direct expansion system in front of the rotor, including an evaporator and a condenser, and use low-temperature refrigerant to remove most of the NMP and moisture in the NMP exhaust gas, and exchange high-temperature refrigerant with regenerated air through the compressor and condenser to reduce heat transfer to reduce The energy consumption of the regenerating heater while simplifying the structure.
It effectively reduces the energy consumption of the NMP recycling system in the lithium battery coating area, improves the recycling efficiency of NMP waste liquid, and simplifies the system structure.
Smart Images

Figure CN222110917U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of NMP recovery, in particular to an NMP recovery system in a coating area of a lithium battery factory. Background Art
[0002] N-Methylpyrrolidone, or NMP, is a solvent with strong solubility, stable chemical properties and good thermal stability. It is widely used in the chemical industry. In the field of lithium battery production, NMP is often used as a solvent for positive electrode materials. During the coating process, the NMP used is constantly volatilized. Usually, the volatilized NMP is extracted during the production process and recycled to form NMP waste liquid.
[0003] At present, the mainstream NMP recovery technologies include waste heat recovery + spray tower, waste heat recovery + deep condensation device + spray tower and waste heat recovery + deep condensation device + rotary wheel. Compared with the first two processes, the waste heat recovery + deep condensation device + rotary wheel process has no spray tower structure and does not require the addition of pure water spray. Therefore, it is also called dry recovery. This process has the advantages of low return air dew point and is widely used in lithium battery factories with high requirements on battery cell quality and high ambient humidity. For example, the patent with announcement number CN211837113U discloses an NMP recovery structure, which includes: a recovery chamber; a heat exchanger, which cools the gas to be recovered for the first time; a secondary heat exchanger, which cools the gas to be recovered for the second time to form liquid NMP and preliminary recovery gas; a liquid receiving tray, which is located below the heat exchanger and the secondary heat exchanger, and part of the preliminary recovery gas at the outlet of the secondary heat exchanger can enter the heat exchanger; a zeolite rotor, which adsorbs the NMP in the remaining preliminary recovery gas to form exhaust gas from the preliminary recovery gas, and part of the exhaust gas is discharged; a regeneration heater, which is located on one side of the zeolite rotor and can heat the remaining exhaust gas to form hot exhaust gas, and the hot exhaust gas flows through the zeolite rotor and mixes with the gas to be recovered. However, in the waste heat recovery + deep condensation device + rotor process, the regeneration wind entering the rotor regeneration zone needs to be heated by the regeneration heater, which consumes a lot of electricity, and the overall energy consumption of the equipment is high. Utility Model Content
[0004] Based on this, it is necessary to provide a NMP recovery system for the coating area of a lithium battery factory to address the technical problem that the current process of using waste heat recovery + deep condensation device + rotary wheel to recover NMP requires a surface cooler to be added in front of the rotary wheel, and the regeneration air entering the rotary regeneration area needs to be heated by a regeneration heater, which consumes a large amount of electricity and has a high overall energy consumption of the equipment.
[0005] The utility model proposes an NMP recovery system for a coating area of a lithium battery factory, comprising a rotor and a regeneration heater, and also comprising a direct expansion system, wherein the condenser of the direct expansion system is used to adjust the temperature of the gas entering the regeneration heater and the evaporator thereof is used to adjust the temperature of the gas entering the adsorption area of the rotor.
[0006] The utility model sets a direct expansion system, the refrigerant in the evaporator is in a low-temperature state, the NMP waste gas passes through the evaporator, most of the NMP and moisture are removed, the compressor of the direct expansion system transports the high-temperature refrigerant that has completed heat exchange in the evaporator to the condenser, the high-temperature refrigerant exchanges heat with the regeneration air passing through the condenser, the regeneration air changes from a low temperature state to a high temperature state, and finally the regeneration heater heats the regeneration air to supplement the surplus, which can effectively reduce the energy consumption of the NMP recovery system in the lithium battery coating area, and the structure is relatively simple, so as to realize the efficient recovery and utilization of the NMP waste liquid.
[0007] As a further improvement of the above scheme of the utility model, it also includes a first fan. The direct expansion system includes an evaporator, a compressor, a condenser and an expansion valve which are connected in sequence through pipelines to form a cycle. The inlet of the first fan is connected to the rotor preheating zone and the outlet is connected to the air inlet of the condenser. The air outlet of the condenser is connected to the air inlet of the regeneration heater, and the air outlet of the regeneration heater is connected to the rotor regeneration zone.
[0008] As a further improvement of the above solution of the utility model, it also includes a second fan, and the inlet and outlet of the second fan are respectively connected to the adsorption area and the preheating area of the rotor through pipelines.
[0009] As a further improvement of the above scheme of the utility model, it also includes a third fan, a primary surface cooler and a secondary surface cooler. The evaporator is arranged between the primary surface cooler and the secondary surface cooler, and its inlet and outlet are connected with the primary surface cooler outlet and the secondary surface cooler inlet through pipes respectively. The inlet of the third fan is connected with the secondary surface cooler outlet through a pipe, and its outlet is connected with the rotor adsorption area.
[0010] As a further improvement of the above scheme of the utility model, it also includes an oven, a fourth fan, a heat exchanger and a fifth fan, the heat exchanger has a high-temperature inlet, a dry air outlet, a low-temperature outlet and a dry air inlet; the inlet of the fourth fan is connected with the oven through a pipeline, and its outlet is connected with the high-temperature inlet of the heat exchanger; the inlet of the fifth fan is connected with the dry air outlet of the heat exchanger through a pipeline, and its outlet is connected with the oven; the low-temperature outlet of the heat exchanger is connected with the inlet of the primary surface cooler in sequence through a pipeline; the outlet of the third fan is also connected with the dry air inlet of the heat exchanger.
[0011] As a further improvement of the above scheme of the utility model, it also includes an NMP waste liquid storage tank, which is connected to the exhaust port of the primary surface cooler, the secondary surface cooler and the evaporator through a pipeline.
[0012] As a further improvement of the above solution of the utility model, it also includes a primary filter, which is arranged on the connecting pipe between the fourth fan and the high-temperature inlet of the heat exchanger.
[0013] As a further improvement of the above solution of the utility model, it also includes a medium efficiency filter, which is arranged on the connecting pipe between the fourth fan and the high-temperature inlet of the heat exchanger and is located downstream of the primary filter.
[0014] Compared with the prior art, the utility model has the following beneficial effects:
[0015] 1. The utility model sets a direct expansion system, the refrigerant inside the evaporator is in a low-temperature state, the NMP waste gas passes through the evaporator, most of the NMP and moisture are removed, the compressor of the direct expansion system transports the high-temperature refrigerant that has completed heat exchange in the evaporator to the condenser, the high-temperature refrigerant exchanges heat with the regeneration air passing through the condenser, the regeneration air changes from a low temperature state to a high temperature state, and finally the regeneration heater heats the regeneration air to supplement the surplus, which can effectively reduce the energy consumption of the NMP recovery system in the lithium battery coating area, and the structure is relatively simple, so as to realize the efficient recovery and utilization of the NMP waste liquid.
[0016] 2. The air intake of the preheating zone of the rotor of the utility model comes from the air treated in the adsorption zone of the rotor. Since the NMP gas content after treatment is low, the temperature of the air treated by the rotor is higher than that of the fresh air, which can improve the treatment efficiency of the rotor. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 This is a structural schematic diagram of an NMP recovery system in a coating area of a lithium battery factory proposed in an embodiment of the utility model.
[0018] Figure numerals: 1. rotor; 2. first fan; 3. regeneration heater; 4. condenser; 5. second fan; 6. primary surface cooler; 7. evaporator; 8. secondary surface cooler; 9. oven; 10. fourth fan; 11. heat exchanger; 12. third fan; 13. fifth fan; 14. compressor; 15. expansion valve; 16. NMP waste liquid storage tank; 17. primary filter; 18. medium filter; 19. sixth fan. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0020] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "or / and" used herein includes any and all combinations of one or more related listed items.
[0021] Example
[0022] Reference Figure 1 The NMP recovery system of the coating area of the lithium battery factory of this embodiment includes a rotor 1, a regeneration heater 3 and a direct expansion system, and may also include a first fan 2, a second fan 5, a third fan 12, a primary surface cooler 6, a secondary surface cooler 8, an oven 9, a fourth fan 10, a heat exchanger 11, a fifth fan 13, an NMP waste liquid storage tank 16, a primary filter 17 and a medium filter 18.
[0023] The head 901 and tail 902 of the coating machine in the coating section of the lithium battery factory are located on both sides of the oven 9. The high temperature in the oven 9 is used to dry out the NMP in the electrode. The top of each oven 9 is connected to an exhaust duct and the bottom is connected to an induced draft duct. The exhaust duct is connected to the air inlet of the fourth fan 10.
[0024] The direct expansion system includes an evaporator 7, a compressor 14, a condenser 4 and an expansion valve 15 which are connected in sequence through pipelines to form a cycle. The refrigerant inside the evaporator 4 is in a low-temperature state, and the compressor transports the high-temperature refrigerant that has completed heat exchange in the evaporator 4 to the condenser 7.
[0025] The heat exchanger 11 has a high temperature inlet, a low temperature outlet, a dry air inlet and a dry air outlet. The high temperature inlet of the heat exchanger 11 is connected to the air outlet of the fourth fan 10 through a pipeline, and the pipeline is provided with a primary filter 17 and a medium filter 18. The medium filter 18 is located downstream of the primary filter 17. The NMP waste gas entering the heat exchanger 11 is initially filtered by the primary filter 17 and the medium filter 18. The primary filter 17 is of G4 specification and can filter 90% of impurities with a diameter greater than 5 μm. The medium filter 18 is of F8 specification and can filter 95% of impurities with a diameter greater than 5 μm. The low temperature outlet of the heat exchanger 11 is connected to the primary surface cooler 6, the evaporator 7, and the secondary surface cooler 8 in sequence through a pipeline, wherein the primary surface cooler 6 uses circulating cooling water as a cold source, and the secondary surface cooler 8 uses chilled water as a cold source. The evaporator 7 is connected to the sixth fan 19 and the compressor 14 in sequence through pipelines. The compressor 14 is connected to the condenser 4. The condenser 4 is connected to the expansion valve 15 and the evaporator 7 through pipelines. The refrigerant evaporates in the evaporator 7 to absorb heat and then enters the condenser 4 to liquefy and release heat.
[0026] The NMP waste liquid storage tank 16 is connected to the bottom of the primary surface cooler 6, the evaporator 7, and the secondary surface cooler 8 through a pipeline to store the NMP waste liquid.
[0027] The air inlet of the third fan 12 is connected to the outlet of the secondary surface cooler 8 through a pipeline, and the outlet of the third fan 12 is connected to the dry air inlet of the heat exchanger 11 and the adsorption area of the wheel 1 through pipelines.
[0028] The air inlet and the air outlet of the second fan 5 are respectively connected with the adsorption zone and the preheating zone of the wheel 1 through pipelines.
[0029] The air inlet and the air outlet of the first fan 2 are connected to the preheating zone of the wheel 1 and the air inlet of the condenser 4 respectively through pipelines.
[0030] The air outlet of the condenser 4 is connected to the air inlet of the regeneration heater 3 through a pipeline, the air outlet of the regeneration heater 3 is connected to the regeneration zone of the runner 1 through a pipeline, and the regeneration zone is connected to the air inlet of the primary surface cooler 6 through a pipeline. In this embodiment, the regeneration heater 3 can be electrically heated, steam heated, gas heated or heat-conducting oil.
[0031] Through the above structural setting, the working principle of this embodiment is:
[0032] The fourth fan 10 is started to send the NMP exhaust gas in the coating machine oven 9 to the primary filter 17, and 90% of the impurities with a diameter greater than 5 μm are filtered out by the primary filter 17. The NMP exhaust gas filtered by the primary filter 17 enters the medium filter 18, and 95% of the impurities with a diameter greater than 5 μm are filtered out by the medium filter 18; the NMP exhaust gas filtered by the medium filter 18 enters the high-temperature inlet of the heat exchanger 11, and the temperature of the NMP exhaust gas at the high-temperature inlet is 130°C. The dry air entering the heat exchanger 11 from the dry air inlet of the heat exchanger 11 reaches a temperature of 95°C after heat exchange, and the heat exchange efficiency is more than 75%. The dry air after heat exchange is introduced into the oven 9 through the fifth fan 13;
[0033] The NMP waste gas after heat exchange discharged from the low-temperature outlet of the heat exchanger 11 enters the primary surface cooler 6, the evaporator 7, and the secondary surface cooler 8 in sequence. The primary surface cooler 6 can cool the NMP waste gas to 37°C and remove most of the NMP and moisture in the waste gas; the evaporator 7 further processes the NMP waste gas after primary cooling and can reduce the temperature of the NMP waste gas to 20°C; further, the secondary surface cooler 8 uses chilled water to cool the outlet air of the evaporator 7. The secondary surface cooler 8 is a chilled water surface cooler, which can reduce the temperature of the NMP waste gas to 14°C and the NMP content in the waste gas to 200ppm; the NMP waste liquid generated by the primary surface cooler 6, the evaporator 7, and the secondary surface cooler 8 is stored in the NMP waste liquid storage tank 16;
[0034] 95% of the exhaust air of the secondary surface cooler 8 is introduced into the dry air inlet of the heat exchanger 11 through the third fan 12, and the gas is sent back to the oven 9 by the fifth fan 13; another 5% of the exhaust air is introduced into the adsorption zone of the rotor 1 by the third fan 12. The rotor 1 is made of zeolite. The zeolite rotor 1 is used to adsorb the remaining NMP components in the exhaust gas. The NMP concentration of the exhaust gas after adsorption is reduced to 10ppm, and the temperature is increased to 20-30°C, which can be directly discharged to maintain the negative pressure in the oven 9; the second fan 5 is used to introduce a small part of the gas in the adsorption zone into the preheating zone of the rotor 1, and the gas is heated by the waste heat of regeneration. After heating, the gas temperature is increased to 60°C, and then the first fan 2 is used to introduce the outlet air of the preheating zone into the condenser 4, which can increase the temperature to 85°C. Further, the regeneration heater 3 is used to increase the gas temperature to 130°C, and the heated gas is passed into the regeneration zone of the rotor 1 to achieve heating and desorption of NMP and moisture in the rotor 1, and transferred to the primary surface cooler 6.
[0035] By using the NMP recovery system of the coating area of the lithium battery factory of this embodiment, the NMP in the exhaust gas of the coating area can be effectively recovered. The liquefaction and recovery of the NMP component in the gas are realized through the primary surface cooler 6, the evaporator 7, and the secondary surface cooler 8. Then, the rotor 1 is used to further process a small amount of condensed gas and partially discharge it to maintain the negative pressure of the oven 9. In addition, compared with the traditional rotor-type NMP recovery system, the present system adds a direct expansion system. The direct expansion system has no intermediate heat exchange medium (refrigerant) and has high heat exchange efficiency. It can effectively reduce the energy consumption required for the deep condensation system and the regeneration heating of the rotor 1. At the same time, the pipeline line is simple and the layout space is saved. In addition, the air intake of the preheating zone of the rotor 1 of the present system comes from the wind treated by the rotor 1. Compared with the fresh air, the wind treated by the rotor 1 has a higher temperature, which can further improve the processing efficiency of the rotor 1 and reduce the energy consumption of the equipment.
[0036] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0037] The above-mentioned embodiments only express several implementation methods of the utility model, and the description is relatively specific and detailed, but it cannot be understood as limiting the scope of the utility model patent. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the utility model, which all belong to the protection scope of the utility model. Therefore, the protection scope of the utility model patent shall be based on the attached claims.
Claims
1. A NMP recovery system for a coating area of a lithium battery factory, comprising a rotor (1) and a regeneration heater (3), characterized in that: It also includes a direct expansion system, wherein the condenser (4) of the direct expansion system is used to adjust the temperature of the gas entering the regeneration heater, and the evaporator (7) of the direct expansion system is used to adjust the temperature of the gas entering the adsorption zone of the rotor (1).
2. The NMP recovery system for coating area of a lithium battery factory according to claim 1, characterized in that: It also includes a first fan (2), and the direct expansion system includes an evaporator (7), a compressor (14), a condenser (4) and an expansion valve (15) which are connected in sequence through pipelines to form a cycle, the inlet of the first fan (2) is connected to the preheating zone of the wheel (1) and the outlet is connected to the air inlet of the condenser (4), the air outlet of the condenser (4) is connected to the air inlet of the regeneration heater (3), and the air outlet of the regeneration heater (3) is connected to the regeneration zone of the wheel (1).
3. The NMP recovery system in the coating area of a lithium battery factory according to claim 1, characterized in that: It also comprises a second fan (5), the inlet and outlet of the second fan (5) being respectively connected to the adsorption zone and the preheating zone of the rotor (1) through pipelines.
4. The NMP recovery system for coating area of a lithium battery factory according to claim 1, characterized in that: It also includes a third fan (12), a primary surface cooler (6) and a secondary surface cooler (8); the evaporator (7) is arranged between the primary surface cooler (6) and the secondary surface cooler (8), and its inlet and outlet are respectively connected to the outlet of the primary surface cooler (6) and the inlet of the secondary surface cooler (8) through pipelines; the inlet of the third fan (12) is connected to the outlet of the secondary surface cooler (8) through a pipeline, and its outlet is connected to the adsorption area of the wheel (1).
5. The NMP recovery system for coating area of a lithium battery factory according to claim 4, characterized in that: The invention also comprises a drying oven (9), a fourth fan (10), a heat exchanger (11) and a fifth fan (13); the heat exchanger (11) has a high-temperature inlet, a dry air outlet, a low-temperature outlet and a dry air inlet; the inlet of the fourth fan (10) is connected to the drying oven (9) through a pipeline, and its outlet is connected to the high-temperature inlet of the heat exchanger (11); the inlet of the fifth fan (13) is connected to the dry air outlet of the heat exchanger (11) through a pipeline, and its outlet is connected to the drying oven (9); the low-temperature outlet of the heat exchanger (11) is connected to the inlet of the primary surface cooler (6) in sequence through a pipeline; and the outlet of the third fan (12) is also connected to the dry air inlet of the heat exchanger (11).
6. The NMP recovery system for coating area of a lithium battery factory according to claim 4, characterized in that: The invention also comprises an NMP waste liquid storage tank (16), which is connected to the waste outlets of the primary surface cooler (6), the secondary surface cooler (8) and the evaporator (7) through pipelines.
7. The NMP recovery system for coating area of a lithium battery factory according to claim 5, characterized in that: It also includes a primary filter (17), which is arranged on a connecting pipe between the fourth fan (10) and the high-temperature inlet of the heat exchanger (11).
8. The NMP recovery system for coating area of a lithium battery factory according to claim 7, characterized in that: It also includes a medium-efficiency filter (18), which is arranged on a connecting pipe between the fourth fan (10) and the high-temperature inlet of the heat exchanger (11), and the medium-efficiency filter (18) is located downstream of the primary filter (17).
Citation Information
Patent Citations
NMP recovery structure
CN211837113U