Casting mold of self-locking structure
By adopting a self-locking structure in the casting mold, using the combination of locking rod, locking tongue rod and return spring, the problem of insufficient stability of die-casting molds during locking molds is solved, and a stable and uniform locking effect is achieved, and the The service life of the mold.
Patent Information
- Application Number
- CN202420797551.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-17
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-04-17
AI Technical Summary
Existing die-casting molds require a large locking pressure when locking molds, but it is difficult to maintain stability, resulting in uneven internal tissue of the blank and prone to mechanical failures after long-term use.
A casting mold with a self-locking structure is designed. Through the mechanical locking rod and the locking tongue rod, the upper and lower inclined surface resistance and return spring mechanism is used to achieve stable locking between the first template and the second template to ensure the locking mold. The pressure is uniform and continuous.
The mold is stable locking state after pressing, enhances the mold locking effect, ensures uniform molding of non-ferrous metal materials, extends the service life of the power parts, and simplifies the maintenance process.
Smart Images

Figure CN222113494U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a casting mould for nonferrous metal materials, more specifically, it relates to a casting mould with a self-locking structure for the same or different nonferrous metal materials. Background Art
[0002] The die-casting mold is a tool used to complete the die-casting process on a die-casting forging machine. The process is as follows: the molten metal is first cast and filled into the mold cavity at a low or high speed, and then forged under pressure as the molten metal cools, which not only eliminates the shrinkage defects of the blank, but also makes the internal structure of the blank reach the broken grains in the forged state.
[0003] The die-casting mold requires a large clamping pressure when clamping, so a die-casting mold that can provide a stable clamping force is needed. Utility Model Content
[0004] The utility model aims to provide a casting mold with a self-locking structure, which can maintain a continuous and stable locking pressure between a first mold plate and a second mold plate through mechanical locking of a locking rod.
[0005] The above technical objectives of the utility model are achieved through the following technical solutions:
[0006] A casting mold of a self-locking structure comprises a first template and a second template which are opened and closed with each other, wherein a vertical locking rod is fixed on the first template, and a vertical hole for inserting the locking rod is provided on the second template, and the locking rod and the vertical hole are clearance-matched; a transverse hole is provided on the second template, and the transverse hole and the vertical hole are connected, and a locking tongue rod slides in the transverse hole, and the locking tongue rod and the transverse hole are clearance-matched; a transverse locking hole is provided on the locking rod, and the locking tongue rod is provided with a lower inclined surface, and the locking hole is provided with an upper inclined surface; when the first template is pressed against the second template, the locking tongue rod is aligned with the locking hole, and the second template is provided with a power piece which pushes the locking tongue rod to be inserted into the locking hole along the transverse hole, and the upper inclined surface and the lower inclined surface are in conflict with each other.
[0007] Preferably, the power member is a cylinder or a hydraulic cylinder.
[0008] Preferably, the piston rod of the power member and the locking tongue rod are fixedly connected.
[0009] Preferably, a return spring is provided in the transverse hole to push the lock tongue rod to slide out of the vertical hole, and the piston rod of the power member is in abutting connection with the lock tongue rod.
[0010] Preferably, the number of locking rods is 2, 3, 4 or 5.
[0011] Preferably, there are four locking rods, which are located at the four corners of the first template.
[0012] Preferably, the first template is an upper template and the second template is a lower template.
[0013] Preferably, the first mold is a lower mold and the second mold is an upper mold.
[0014] Preferably, the vertical opening is a vertical hole or a vertical groove; and the transverse opening is a transverse hole or a transverse groove.
[0015] In summary, the utility model has the following beneficial effects:
[0016] (1) In this design, the locking rod and the locking tongue rod between the first template and the second template are locked through a blocking relationship, so that the locking state of the two can be stable. The vertical opening and the locking rod play a positioning and guiding role when the mold is closed. Therefore, the locking rod here is not only used for mechanical locking, but also has a positioning and guiding role.
[0017] (2) This design uses mechanical barrier locking, which can achieve a large locking force even for smaller die-casting molds after the mold is pressed together.
[0018] (3) The upper and lower inclined surfaces in this design have a more stable contact force between the first and second templates, and the clamping effect is more stable.
[0019] (4) The clamping of the four corners makes the pressing force of the first mold and the second mold more uniform, and the clamping pressure of the two is more stable.
[0020] Casting molds are used to process and produce metal products. Non-ferrous metals are the materials used in mold die-casting, such as the same metal such as aluminum, and heterogeneous non-ferrous metal materials such as aluminum-magnesium alloys. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 is a front view of the die-casting mold in Example 1;
[0022] Figure 2 is a schematic diagram of the position of the locking rod in the first template in Example 1;
[0023] Figure 3 yes Figure 2 A magnified view of part A in FIG.
[0024] Figure 4 is an exploded schematic diagram of the lock tongue rod, the second template, and the first template in Example 1;
[0025] Figure 5 is a schematic diagram of the vertical hole and the transverse hole in Example 2;
[0026] Figure 6 yes Figure 5 A magnified view of part B in FIG.
[0027] Figure 7 is a schematic structural diagram of the second template in Example 3;
[0028] Figure 8 It is a cross-sectional view of the locking rod of Example 4.
[0029] In the figure:
[0030] 11. First template; 12. Second template;
[0031] 2. Locking rod; 21. Locking hole;
[0032] 31. Vertical opening; 32. Horizontal opening;
[0033] 4. Locking tongue lever;
[0034] 51. Lower slope; 52. Upper slope;
[0035] 6. Power parts;
[0036] 7. Return spring. DETAILED DESCRIPTION
[0037] The utility model is further described in detail below in conjunction with the accompanying drawings.
[0038] Example 1, a casting mold with a self-locking structure, referring to Figure 1-Figure 4 , including a first template 11 and a second template 12, solid, semi-solid, liquid non-ferrous metal material is fed into the mold cavity, so that the non-ferrous metal material with pressure quickly fills the mold cavity. The first template 11 is an upper mold and the second template 12 is a lower mold. In other embodiments, the first template 11 is a lower mold and the second template 12 is an upper mold.
[0039] The first template 11 is fixed with vertical locking rods 2 . The number of the locking rods 2 is four and they are located at the four corners of the first template 11 .
[0040] The locking rod 2 is a cylindrical rod; the second template 12 is provided with a vertical opening 31 for inserting the locking rod 2, the vertical opening 31 is a vertical hole, the vertical hole is a circular blind hole, and the locking rod 2 and the vertical opening 31 are clearance-matched;
[0041] During the pressing process of the first template 11 and the second template 12 , the insertion relationship between the locking rod 2 and the vertical opening 31 plays a guiding role, so that the cavities of the first template 11 and the second template 12 can be accurately aligned.
[0042] The second template 12 is provided with a transverse opening 32, which is a transverse hole. The transverse opening 32 and the vertical opening 31 are connected. A lock tongue rod 4 slides in the transverse opening 32, and the lock tongue rod 4 and the transverse opening 32 are clearance-matched. The transverse opening 32 is a circular hole, and one end of the lock tongue rod 4 is cylindrical, so the lock tongue rod 4 slides in the transverse opening 32. The second template 12 is provided with a power member 6 for pushing the lock tongue rod 4 to be inserted into the lock hole 21 along the transverse opening 32. The power member 6 is a hydraulic cylinder, and the piston rod of the power member 6 is fixedly connected to the lock tongue rod 4.
[0043] The lock rod 2 is provided with a transverse lock hole 21, the lock hole 21 is provided with an upper inclined surface 52, and the lock tongue rod 4 is provided with a lower inclined surface 51. The lock hole 21 is a through hole.
[0044] Working principle, when the first template 11 and the second template 12 are pressed together, the locking rod 2 is inserted into the vertical opening 31, at which time the lock hole 21 and the lock tongue rod 4 are aligned, and then the power member 6 drives the lock tongue rod 4 to move toward the lock hole 21, at which time the lower inclined surface 51 and the upper inclined surface 52 are in conflict, and the conflicting relationship between the two inclined surfaces keeps the locking rod 2 in the locked position, so that the first template 11 and the second template 12 are pressed together.
[0045] Example 2, a casting mold with a self-locking structure, which is different from Example 1, refer to Figure 5-Figure 6 A return spring 7 is provided in the transverse opening 32 to push the bolt rod 4 to slide out of the vertical opening 31, and the piston rod of the power member 6 is in contact with the bolt rod 4. The return spring 7 slides on the inner wall of the transverse opening 32, and a baffle is fixed on the inner wall of the transverse opening 32. One end of the return spring 7 contacts the baffle, so the return spring 7 gives an external force to the baffle, and the other end of the return spring 7 contacts the shoulder position of the bolt rod 4.
[0046] When the power member 6 pushes the lock tongue rod 4, the return spring 7 is compressed. When the power member 6 and the lock tongue rod 4 are separated, the compressed return spring 7 pushes the lock tongue rod 4 and the lock hole 21 to separate. The advantage of this design is that it can effectively ensure the accuracy and service life of the power member, and provide a convenient operating space for the maintenance of old molds.
[0047] The casting mold will inevitably wear out after years of use, resulting in excessive resistance of the inclined surface of the lock tongue rod 4 when locked, and the lock tongue rod 4 will tend to bend. If the piston rod of the power member 6 and the lock tongue rod 4 are fixed, the lock tongue rod 4 will drive the piston rod of the power member 6 to bend together, which prolongs the scrap cycle of the power member 6. The design of this embodiment, in which the power member 6 and the lock tongue rod 4 are in a contact connection, effectively avoids the occurrence of this technical defect.
[0048] Secondly, when the lock tongue rod 4 is repaired, due to the split design, the power part 6 can be quickly removed from the mold, so that the operation space for removing the lock tongue rod 4 from the mold is larger, making it easier to remove the lock tongue rod 4;
[0049] In other embodiments, a threaded hole is provided at one end of the lock tongue rod 4 facing the power member 6, so that when removing the lock tongue rod, an external rod body can be extended from the horizontal opening 32 to connect the rod body and the threaded hole of the lock tongue rod 4, so as to quickly and conveniently pull out the lock tongue rod 4.
[0050] Embodiment 3, a casting mold with a self-locking structure, which is different from Embodiment 1 or Embodiment 2, refer to Figure 7 The horizontal opening 32 is a vertical slide groove, and the vertical opening 31 is a vertical slide groove.
[0051] Embodiment 4, a casting mold with a self-locking structure, which is different from Embodiment 1 or Embodiment 2 or Embodiment 3, refer to Figure 8 , the lock hole 21 is a blind hole. In other embodiments, the lock hole 21 can also be a groove.
[0052] The above is only a preferred embodiment of the present invention. The protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A casting mold with a self-locking structure, comprising a first mold plate (11) and a second mold plate (12) that open and close to each other, characterized in that: The first template (11) is fixed with a vertical locking rod (2), and the second template (12) is provided with a vertical opening for the locking rod (2) to be inserted; The locking rod (2) slides in the vertical opening (31); The second template (12) is provided with a transverse opening (32); The transverse opening (32) and the vertical opening (31) are connected, a lock tongue rod (4) is slidably disposed in the transverse opening (32), and the lock tongue rod (4) and the transverse opening (32) are clearance-matched; The lock rod (2) is provided with a transverse lock hole (21), the lock tongue rod (4) is provided with a lower inclined surface (51), and the lock hole (21) is provided with an upper inclined surface (52); When the first template (11) is pressed against the second template (12), the lock tongue rod (4) is aligned with the lock hole (21), and the second template (12) is provided with a power member (6) for pushing the lock tongue rod (4) along the transverse opening (32) to be inserted into the lock hole (21), and the upper inclined surface (52) and the lower inclined surface (51) are in contact with each other.
2. The casting mold of the self-locking structure according to claim 1 is characterized in that: The vertical opening (31) is a vertical hole or a vertical groove; the transverse opening (32) is a transverse hole or a transverse groove.
3. The casting mold of the self-locking structure according to claim 1 is characterized in that: The locking hole (21) is a blind hole or a through hole.
4. The casting mold of the self-locking structure according to claim 2 is characterized in that: The power member (6) is a cylinder or a hydraulic cylinder.
5. The casting mold of the self-locking structure according to claim 4 is characterized in that: The piston rod of the power member (6) and the lock tongue rod (4) are fixedly connected.
6. The casting mold of the self-locking structure according to claim 4 is characterized in that: A return spring (7) is arranged in the transverse opening (32) to push the lock tongue rod (4) to slide out of the vertical opening (31), and the piston rod of the power member (6) and the lock tongue rod (4) are in abutting connection.
7. The casting mold of the self-locking structure according to claim 1 is characterized in that: The number of the locking rods (2) is 2, 3, 4 or 5.
8. The casting mold of the self-locking structure according to claim 7 is characterized in that: The number of locking rods (2) is four and they are located at the four corners of the first template (11).
9. The casting mold of the self-locking structure according to claim 1 is characterized in that: The first mold plate (11) is an upper mold and the second mold plate (12) is a lower mold.
10. The casting mold of the self-locking structure according to claim 1 is characterized in that: The first mold plate (11) is a lower mold and the second mold plate (12) is an upper mold.