Metal silicide barrier layer and contact hole test structure and multi-group test structure
By designing a test structure between the metal silicide barrier layer and the contact hole in semiconductor manufacturing, and detecting the offset by the resistance ratio change, the problem of the distance between the metal silicide barrier layer and the contact hole in semiconductor manufacturing is solved, and the device is improved Yield and reliability.
Patent Information
- Application Number
- CN202421678117.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-07-15
AI Technical Summary
During semiconductor manufacturing, the distance deviation between the metal silicide barrier layer and the contact hole is difficult to detect, resulting in device failure or reduced reliability, and the prior art lacks an effective detection structure.
A test structure for metal silicide barrier layer and contact hole is designed. By setting the distance between the first chain contact hole and the metal silicide barrier layer is less than the preset distance, and the distance between the second chain contact hole and the metal silicide barrier layer is greater than that of Equivalent to the preset distance, the offset is detected using the change in the resistance ratio measured by the test pin.
The detection of the distance between the metal silicide barrier layer and the contact hole is achieved, ensuring that the distance is within the minimum safe range, avoiding device failure, and improving the yield and reliability of the device.
Smart Images

Figure CN222126519U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductor manufacturing, in particular to a test structure of a metal silicide barrier layer and a contact hole. Background Art
[0002] In the manufacture of integrated circuits, electrostatic discharge devices such as gate-grounded NMOS devices (GGNMOS), laterally diffused metal oxide semiconductor (LDMOS) devices with a barrier layer (SAB, Salicide Block) structure, and non-metallic silicide resistor devices are commonly used. Considering the layout area and chip cost, in the basic units of these devices, the number of contact holes (CT) is basically in a row and the distance to the SAB is relatively close (generally following the minimum design rule or slightly less than the minimum design rule). However, in the semiconductor manufacturing process, process fluctuations may cause the critical dimension (CD) of the SAB to be too large or the overlay error between the SAB and the CT to shift, making the distance between the SAB and the CT less than the minimum safety distance or too large. If the distance between the SAB and the CT is too small, the CT will not be able to form an effective ohmic contact with the single crystal silicon or polycrystalline silicon, resulting in device failure. If the distance between the SAB and the CT is too large, the yield and reliability of the device will be affected.
[0003] In actual production, the prior art lacks a detection structure for detecting whether the distance between SAB and CT is offset. Therefore, it is only possible to detect whether the distance between SAB and CT is offset through terminal detection or slicing. However, when the distance between SAB and CT is offset, huge losses have already occurred.
[0004] Therefore, providing a test structure that can detect the offset between SAB and CT has become a technical problem that needs to be solved urgently in the industry. Utility Model Content
[0005] The technical problem solved by the utility model is to provide a test structure of a metal silicide barrier layer and a contact hole and a plurality of test structures, thereby solving the problem of detecting the offset between the metal silicide barrier layer and the contact hole.
[0006] In order to solve the above technical problems, the technical solution of the utility model provides a test structure of a metal silicide barrier layer and a contact hole, wherein the test structure of the metal silicide barrier layer and the contact hole is arranged in a cutting path of a wafer, and the test structure comprises:
[0007] A first structure in the form of a plurality of strips arranged at a preset interval;
[0008] a metal silicide barrier layer located on the first structure, the metal silicide barrier layer being rectangular in shape, and having a long side perpendicular to the first structure, the metal silicide barrier layer along the long side completely covering a plurality of the first structures, and the metal silicide barrier layer along the short side being located within the first structure;
[0009] A first chain contact hole and a second chain contact hole located on the first structure, wherein the first chain contact hole and the second chain contact hole are respectively located on both sides of the metal silicide barrier layer along the short side;
[0010] The distance between the first chain contact hole and the metal silicide barrier layer is less than a preset distance; the distance between the second chain contact hole and the metal silicide barrier layer is greater than or equal to a preset distance; the two ends of the first chain contact hole are led out by a first test pin and a third test pin, and the two ends of the second chain contact hole are led out by a second test pin and a fourth test pin; the resistance values of the contact holes measured at the two ends of the second chain contact hole are used as a reference for the resistance value of the first chain contact hole;
[0011] The preset distance is used to characterize a minimum safety distance between the metal silicide barrier layer and the first chain contact hole.
[0012] Optionally, the first structure is an ion-doped active region or an ion-doped polysilicon gate.
[0013] Optionally, the ion-doped active region is P+ doped and N-well doped, and a shallow trench isolation structure is formed between the plurality of strip-shaped active regions.
[0014] Optionally, the ion-doped active region is N+ doped, and a shallow trench isolation structure is formed between the plurality of strip-shaped active regions.
[0015] Optionally, the ion-doped polysilicon is an N-type or P-type doped polysilicon gate; and a plurality of strip-shaped polysilicon gates are arranged on a shallow trench isolation structure.
[0016] Correspondingly, the technical solution of the utility model also provides multiple groups of test structures of metal silicide blocking layers and contact holes, including: multiple groups of test structures of the metal silicide blocking layers and contact holes, in which the distances between the first chain contact holes and the metal silicide blocking layer are different in different groups of test structures, and the distances between the second chain contact holes and the metal silicide blocking layer are the same; and the two ends of the first chain contact holes in each group are led out by two test pins.
[0017] Optionally, between the plurality of groups of the first chain contact holes, two adjacent groups of the first chain contact holes share a test pin.
[0018] Optionally, the layers in the multiple groups of test structures are a whole, spanning across a plurality of strip-shaped first structures in the multiple groups of test structures of the metal silicide barrier layers and contact holes.
[0019] Correspondingly, the technical solution of the present invention also provides another set of test structures of metal silicide barrier layer and contact hole, including the test structure of metal silicide barrier layer and contact hole provided by the technical solution of the present invention, and also including a second set of test structures of metal silicide barrier layer and contact hole, wherein the second set of test structures of metal silicide barrier layer and contact hole is a structure obtained by rotating the test structure of metal silicide barrier layer and contact hole provided by the technical solution of the present invention by 90 degrees.
[0020] Compared with the prior art, the technical solution provided by the embodiment of the utility model has the following beneficial effects:
[0021] In the test structure of the metal silicide barrier layer and the contact hole provided by the utility model, by setting the distance between the first chain contact hole and the metal silicide barrier layer to be less than the preset distance, and the distance between the second chain contact hole and the metal silicide barrier layer to be greater than or equal to the preset distance, it is realized to detect whether the metal silicide barrier layer and the first chain contact hole are offset. This is because the preset distance represents the minimum safe distance between the metal silicide barrier layer and the first chain contact hole. If the metal silicide barrier layer is offset or the critical dimension changes, the distance between the metal silicide barrier layer and the first chain contact hole will change, resulting in a change in the first resistance ratio, thereby realizing the detection of whether the metal silicide barrier layer and the first chain contact hole are offset. Among them, the first resistance ratio is used to represent the ratio of the resistance measured between the first test pin and the third test pin and the resistance measured between the second test pin and the fourth test pin.
[0022] In addition, in the multiple groups of test structures of the metal silicide blocking layer and the contact holes provided by the utility model, by setting up multiple groups of test structures of the metal silicide blocking layer and the contact holes, and setting the distance between the first chain contact holes and the metal silicide blocking layer in each group of test structures to be different, the size of the preset distance can be obtained by analyzing the first resistance ratio corresponding to different groups of test structures.
[0023] In addition, in the multiple groups of test structures of metal silicide barrier layers and contact holes provided by the present invention, a second group of test structures of metal silicide barrier layers and contact holes is further provided on the basis of the aforementioned test structures of metal silicide barrier layers and contact holes, wherein the second group of test structures of metal silicide barrier layers and contact holes is a test structure obtained by rotating the aforementioned test structures of metal silicide barrier layers and contact holes by 90 degrees, thereby being able to detect whether an offset occurs between the metal silicide barrier layer and the first chain contact hole in the vertical direction. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0025] Figure 1 A structural top view of a GGNMOS device embodiment;
[0026] Figure 2 A top view of the structure of a high resistance resistor embodiment;
[0027] Figure 3 A top view of the structure of the metal silicide barrier layer and the contact hole test structure provided by the technical solution of the utility model;
[0028] Figure 4 A top view of a structure of a metal silicide barrier layer 40 and a test structure of a contact hole provided by an embodiment of the present utility model;
[0029] Figure 5 for Figure 4 Schematic diagram of the cross-sectional structure along the AA' direction;
[0030] Figure 6 for Figure 4 Schematic diagram of the cross-sectional structure along the BB' direction;
[0031] Figure 7 A top view of a structure of a metal silicide barrier layer 40 and a contact hole test structure provided by another embodiment of the present invention;
[0032] Figure 8 for Figure 7 Schematic diagram of the cross-sectional structure along the AA' direction;
[0033] Fig. 9 for Figure 7 Schematic diagram of the cross-sectional structure along the BB' direction;
[0034] Fig.10 A top view of a structure of a test structure of a metal silicide barrier layer and a contact hole provided by another embodiment of the utility model;
[0035] Fig.11 for Fig.10 Schematic diagram of the cross-sectional structure along the AA' direction;
[0036] Fig.12 for Fig.10 Schematic diagram of the cross-sectional structure along the BB' direction;
[0037] Fig.13 A top view of a structure of a metal silicide barrier layer and a contact hole test structure provided by another embodiment of the utility model;
[0038] Fig.14 for Fig.13 Schematic diagram of the cross-sectional structure along the AA' direction;
[0039] Fig.15 for Fig.13 Schematic diagram of the cross-sectional structure along the BB' direction;
[0040] Fig.16 An external connection structure diagram of a metal silicide barrier layer and a contact hole test structure provided by an embodiment of the utility model;
[0041] Fig.17 The dotted line distribution diagram is obtained by the first ratio value of each test structure.
[0042] Reference numerals:
[0043] 10- first structure;
[0044] 11-N+ doped active region;
[0045] 12-metal silicide layer;
[0046] 13-P+ doped active region;
[0047] 14-P type polysilicon;
[0048] 15-N-type polysilicon;
[0049] 20-first chain contact hole;
[0050] 21- a first conductive plug;
[0051] 22-first metal connecting wire;
[0052] 30-second chain contact hole;
[0053] 31- a second conductive plug;
[0054] 32- a second metal connecting wire;
[0055] 40-metal silicide barrier layer;
[0056] 50-P type substrate;
[0057] 60- shallow trench isolation structure;
[0058] 70-N well doping layer;
[0059] 80-isolation layer;
[0060] PIN1-first test pin;
[0061] PIN 2 - Second test pin;
[0062] PIN 3 - the third test pin;
[0063] PIN 4-the fourth test pin;
[0064] PAD1-first test pad;
[0065] PAD 2-second test pad;
[0066] PAD 3-the third test pad;
[0067] PAD4 - fourth test pad. DETAILED DESCRIPTION
[0068] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the utility model. The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the utility model and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the utility model described here can be implemented in an order other than those illustrated or described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0069] Figure 1 A top view of the structure of a GGNMOS device embodiment.
[0070] Please refer to Figure 1The coverage of the drain by SAB102 is conducive to the safe release of the pulse current during the ESD process to the substrate. However, the CT102 of the drain needs to contact the metal silicide 100 to form an ohmic contact. Therefore, in GGNMOS, if the distance between SAB102 and CT102 is too small, CT102 may not be able to form an effective ohmic contact with the metal silicide 100, resulting in device failure and circuit failure. If the distance between SAB102 and CT102 is too large, the pulse current may flow on the drain surface, causing overheating and damage to the device, affecting product yield and reliability.
[0071] Figure 2 A top view of the structure of a high-resistance resistor embodiment.
[0072] Please refer to Figure 2 , the high resistance resistor needs to be covered with SAB201 on the surface of the resistor to prevent the formation of low resistance metal silicide 200. In the high resistance resistor, if the distance between SAB201 and CT202 is too small, CT202 may not form an effective ohmic contact with metal silicide 200 due to process fluctuations, resulting in device failure and circuit failure. If the distance between SAB201 and CT202 is too large, it will cause unnecessary waste of chip area and increase manufacturing costs.
[0073] As described in the background art, in actual production, the prior art lacks a test structure for detecting whether the distance between SAB and CT is offset. Therefore, it is only possible to detect whether the distance between SAB and CT is offset through terminal detection or slicing. However, when the distance between SAB and CT is found to be offset, huge losses have already occurred.
[0074] In view of this, the present application provides a test structure of a metal silicide barrier layer and a contact hole.
[0075] in, Figure 3 A top view of the structure of the metal silicide barrier layer and the contact hole test structure provided by the technical solution of the utility model.
[0076] Please refer to Figure 3 The metal silicide barrier layer and contact hole test structure provided in the present application is arranged in the cutting path of the wafer, and the specific structure includes:
[0077] A plurality of first strip-shaped structures 10 arranged at a preset interval;
[0078] a metal silicide barrier layer 40 located on the first structure 10, wherein the metal silicide barrier layer 40 is rectangular in shape, and the direction along the long side of the metal silicide barrier layer 40 is perpendicular to the first structure 10, the metal silicide barrier layer 40 along the long side completely covers a plurality of the first structures 10, and the metal silicide barrier layer 40 along the short side is located within the first structure 10;
[0079] A first chain contact hole 20 and a second chain contact hole 30 located on the first structure 10, wherein the first chain contact hole 20 and the second chain contact hole 30 are respectively located on both sides of the metal silicide barrier layer 40 along the short side;
[0080] The distance between the first chain contact hole 20 and the metal silicide barrier layer 40 is less than a preset distance; the distance between the second chain contact hole 30 and the metal silicide barrier layer 40 is greater than or equal to a preset distance; both ends of the first chain contact hole 20 are led out by a first test pin PIN1 and a third test pin PIN3, and both ends of the second chain contact hole 30 are led out by a second test pin PIN2 and a fourth test pin PIN4; the resistance values of the contact holes measured at both ends of the second chain contact hole 30 are used as a reference for the resistance value of the first chain contact hole 20;
[0081] The preset distance is used to represent a minimum safety distance between the metal silicide barrier layer 40 and the first chain contact hole 20 .
[0082] pass Figure 3 The above technical means shown in the utility model can detect the offset of the distance between the metal silicide barrier layer 40 and the first chain contact hole 20. The specific reasons are as follows:
[0083] For the convenience of description, the resistance values measured between the first test pin PIN1 and the third test pin PIN3 are collectively referred to as the first resistance, that is, the first resistance is the equivalent resistance of the first chain contact hole 20. The resistance values measured between the second test pin PIN2 and the fourth test pin PIN4 are collectively referred to as the second resistance, that is, the second resistance is the equivalent resistance of the second chain contact hole 30.
[0084] Before explaining the specific reasons, the relationship between the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 and the first resistor is explained as follows: on the basis that the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is greater than the minimum safety distance, no matter how the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 changes, the resistance value of the first resistor does not change. If the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is less than the minimum safety distance, as the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 continues to decrease, it will affect the formation of metal silicide in the region of the first chain contact hole 20, thereby increasing the contact resistance of the first chain contact hole 20, resulting in the resistance value of the first resistor continuously increasing. The relationship between the distance between the metal silicide barrier layer 40 and the second chain contact hole 30 and the second resistor is the same as the relationship between the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 and the first resistor, which will not be repeated here.
[0085] Based on the above description of the relationship between the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 and the first resistor, by setting the distance between the first chain contact hole and the metal silicide barrier layer to be less than a preset distance, and the distance between the second chain contact hole and the metal silicide barrier layer to be greater than or equal to the preset distance, it is possible to detect whether the metal silicide barrier layer and the first chain contact hole are offset. Because, when the metal silicide barrier layer 40 and the first chain contact hole 20 are offset or the critical size of the metal silicide barrier layer 40 becomes larger, the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is reduced, and the ratio of the first resistor to the second resistor increases. When the metal silicide barrier layer 40 and the first chain contact hole 20 are offset, so that the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is increased, the ratio of the first resistor to the second resistor decreases, thereby realizing the detection of whether the metal silicide barrier layer and the first chain contact hole are offset.
[0086] At the same time, by setting the first chain contact hole 20 as a variable and setting the second chain contact hole 30 as a control group, the spacing offset between the metal silicide barrier layer 40 and the first chain contact hole 20 is detected by changing the ratio of the first resistor to the second resistor.
[0087] The test structure provided by the technical solution of the utility model is further described in detail below through specific embodiments:
[0088] Figure 4A top view of a test structure of a metal silicide barrier layer and a contact hole provided by an embodiment of the present invention. Figure 5 for Figure 4 Schematic diagram of the cross-sectional structure along the AA' direction. Figure 6 for Figure 4 Schematic diagram of the cross-sectional structure along the BB' direction.
[0089] Please refer to Figure 4 , Figure 5 and Figure 6 , a plurality of strip-shaped N+ doped active regions 11 are arranged on a P-type substrate 50. A shallow trench isolation structure 60 is provided between the plurality of strip-shaped N+ doped active regions 11.
[0090] The metal silicide barrier layer 40 is disposed in the middle region of the N+ doped active region 11 and completely covers a plurality of N+ doped active regions 11. The region of each N+ doped active region 11 not covered by the metal silicide barrier layer 40 is covered by the metal silicide layer 12.
[0091] The first chain contact hole 20 and the second chain contact hole 30 are respectively disposed on the metal silicide layer 12 on both sides of the metal silicide barrier layer 40 .
[0092] The first chain contact hole 20 is composed of a first conductive plug 21 and a first metal connection line 22. Two first conductive plugs 21 are provided on each N+ doped active region 11, and the first metal connection line 22 connects the first conductive plugs 21 on adjacent N+ doped active regions 11. The first conductive plug 21 on the rightmost N+ doped active region 11 serves as the first end of the first chain contact hole 20, connected to the first test pin PIN1, and the first conductive plug 21 on the leftmost N+ doped active region 11 serves as the second end of the first chain contact hole 20, connected to the third test pin PIN3.
[0093] The second chain contact hole 30 is composed of a second conductive plug 31 and a second metal connection line 32. Two second conductive plugs 23 are provided on each N+ doped active region 11, and the second metal connection line 24 connects the second conductive plugs 23 on adjacent N+ doped active regions 11. The second conductive plug 23 on the rightmost N+ doped active region 11 serves as the first end of the second chain contact hole 30, connected to the second test pin PIN2, and the second conductive plug 23 on the leftmost N+ doped active region 11 serves as the second end of the second chain contact hole 30, connected to the fourth test pin PIN4.
[0094] By setting the distance between the first chain contact hole 20 and the metal silicide barrier layer 40 to be less than the preset distance; the distance between the second chain contact hole 30 and the metal silicide barrier layer 40 is greater than or equal to the preset distance. If the metal silicide barrier layer 40 is offset or the critical dimension is enlarged, so that the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is closer, the ratio of the first resistance and the second resistance obtained by detection will increase. If the metal silicide barrier layer 40 is offset, so that the distance between the metal silicide barrier layer 40 and the first chain contact hole 20 is farther, the ratio of the first resistance and the second resistance obtained by detection will decrease, and the minimum is 1.
[0095] Figure 7 A top view of a test structure of a metal silicide barrier layer and a contact hole provided by another embodiment of the present invention. Figure 8 for Figure 7 Schematic diagram of the cross-sectional structure along the AA' direction. Fig. 9 for Figure 7 Schematic diagram of the cross-sectional structure along the BB' direction.
[0096] Please refer to Figure 7 , Figure 8 and Fig. 9 An N-well doped layer 70 is disposed on the P-type substrate 50, and a plurality of strip-shaped P+ doped active regions 13 are disposed on the N-well doped layer 70. A shallow trench isolation structure 60 is provided between the plurality of strip-shaped P+ doped active regions 13.
[0097] The structural arrangements of the metal silicide barrier layer 40 , the metal silicide layer 12 , the first chain contact holes 20 and the second chain contact holes 30 on the P+ doped active region 13 are the same as those in the above embodiment and will not be described again.
[0098] Fig.10 A top view of a test structure of a metal silicide barrier layer and a contact hole provided by another embodiment of the present invention. Fig.11 for Fig.10 Schematic diagram of the cross-sectional structure along the AA' direction. Fig.12 for Fig.10 Schematic diagram of the cross-sectional structure along the BB' direction.
[0099] Please refer to Fig.10 , Fig.11 and Fig.12 An isolation layer 80 is disposed on the P-type substrate 50 , and a plurality of strip-shaped P-type polysilicon 14 are disposed on the isolation layer 80 .
[0100] The structural arrangements of the metal silicide barrier layer 40, the metal silicide layer 12, the first chain contact holes 20 and the second chain contact holes 30 on the P-type polysilicon 14 are the same as those in the above embodiment, and will not be repeated here.
[0101] Fig.13 A top view of a test structure of a metal silicide barrier layer and a contact hole provided by another embodiment of the present invention. Fig.14 for Fig.13 Schematic diagram of the cross-sectional structure along the AA' direction. Fig.15 for Fig.13 Schematic diagram of the cross-sectional structure along the BB' direction.
[0102] Please refer to Fig.13 , Fig.14 and Fig.15 An isolation layer 80 is disposed on the P-type substrate 50 , and a plurality of strip-shaped N-type polysilicon 15 are disposed on the isolation layer 80 .
[0103] The structural arrangements of the metal silicide barrier layer 40 , the metal silicide layer 12 , the first chain contact holes 20 and the second chain contact holes 30 on the N-type polysilicon 15 are the same as those in the above embodiment and will not be described again.
[0104] As a specific implementation, when the metal silicide barrier layer is offset or the critical dimension increases, the change in the first resistor can be set to account for at least 10% of the total resistance of the first resistor. This can be achieved by adjusting the number of first structures. Of course, the specific value of the change in the first resistor to the total resistance can be adjusted according to actual needs and is not limited here.
[0105] Fig.16 This is a diagram of the external connection structure of the metal silicide barrier layer and the contact hole test structure provided by one embodiment of the utility model.
[0106] Please refer to Fig.16 , the first test pin PIN1 is connected to the external first test pad PAD1, the second test pin PIN2 is connected to the external second test pad PAD2, the third test pin PIN3 is connected to the external third test pad PAD3, and the fourth test pin PIN4 is connected to the external fourth test pad PAD4. The test machine applies voltage to the first test pad PAD1 and the third test pad PAD3 to measure the first resistance; the test machine applies voltage to the second test pad PAD2 and the fourth test pad PAD4 to measure the second resistance.
[0107] In summary, the test structure of the metal silicide barrier layer and the contact hole provided in the embodiment of the utility model realizes the detection of the offset of the spacing between the metal silicide barrier layer and the first chain contact hole by setting the distance between the metal silicide barrier layer and the first chain contact hole to be less than the minimum safety distance, and the distance between the metal silicide barrier layer and the second chain contact hole to be greater than or equal to the minimum safety distance. At the same time, since the first chain contact hole is set as a variable and the second chain contact hole is set as a control group, the offset of the spacing between the metal silicide barrier layer and the first chain contact hole is detected by the change in the ratio of the first resistor and the second resistor, eliminating the interference factors caused by the non-metal silicide barrier layer factor.
[0108] The technical solution of the utility model also provides a plurality of groups of test structures of metal silicide barrier layers and contact holes, including a plurality of groups of test structures of the metal silicide barrier layers and contact holes, wherein the distances between the first chain contact holes and the metal silicide barrier layers in different groups of test structures are different, and the distances between the second chain contact holes and the metal silicide barrier layers are the same; the two ends of the first chain contact holes in each group are led out by two test pins.
[0109] Through the above technical means, the technical solution of the utility model can measure the size of the preset distance, that is, the size of the minimum safety distance. The specific reasons are as follows:
[0110] According to preset requirements, the distance D1 between the first chain contact holes and the metal silicide barrier layer in all test structures is arranged in descending order, and the resistance value of the first resistor and the resistance value of the second resistor in each test structure are tested, and the first ratio of each test structure is obtained according to the following formula;
[0111] X=(R1-R2) / R2;Formula (1)
[0112] Among them, X is used to characterize the first ratio; R1 is used to characterize the first resistance; and R2 is used to characterize the second resistance.
[0113] based on Fig.17As shown in the dotted line distribution diagram obtained by the first ratio of each test structure, as the distance between the first chain contact hole and the metal silicide barrier layer continues to increase, the first ratio continues to decrease. Similarly, as the distance between the first chain contact hole and the metal silicide barrier layer continues to decrease, the first ratio continues to increase. According to the above principle description, when the distance between the first chain contact hole and the metal silicide barrier layer and the distance between the second chain contact hole and the metal silicide barrier layer are both greater than or equal to the minimum safety distance, the ratio of the first resistor to the second resistor is 1, that is, the first ratio is 0. Therefore, when the distance between the first chain contact hole and the metal silicide barrier layer is exactly the minimum safety distance, the first ratio is exactly reduced to 0, corresponding to the intersection of the curve and the horizontal axis in the dotted line distribution diagram. Therefore, the minimum safety distance can be determined by the intersection of the curve and the horizontal axis in the dotted line distribution diagram. Specifically, in the 0.18μm process, the minimum safety distance is 0.22μm.
[0114] As a specific implementation, in a plurality of test structures, the first chain contact holes of two adjacent test structures are arranged to share a test pin, so as to reduce the overall manufacturing cost of the plurality of test structures.
[0115] As a specific implementation, multiple groups of test structures are set to share the same metal silicide barrier layer, so that the metal silicide barrier layer spans the first structure in the multiple groups of test structures, and by adjusting the position of the first chain contact hole on the first structure in each group of test structures, the distances between the first chain contact holes and the metal silicide barrier layer in different groups of test structures are different. Since each group of test structures shares a metal silicide barrier layer, it is only necessary to adjust the position of the first chain contact hole to achieve the detection of the minimum safety distance, further reducing the overall manufacturing cost of the multiple groups of test structures.
[0116] In summary, the embodiments of the utility model provide multiple groups of test structures of metal silicide blocking layers and contact holes. By setting multiple groups of test structures of metal silicide blocking layers and contact holes, and setting the distance between the first chain contact holes and the metal silicide blocking layers in each group of test structures to be different, the size of the preset distance can be obtained by analyzing the first resistance ratio corresponding to different groups of test structures.
[0117] Furthermore, by arranging the first chain contact holes of two adjacent groups of test structures to share one test pin, the overall manufacturing cost of the multiple groups of test structures can be reduced.
[0118] Furthermore, by arranging multiple groups of test structures to share the same metal silicide barrier layer, the metal silicide barrier layer spans across the first structures in the multiple groups of test structures, so as to further reduce the overall manufacturing cost of the multiple groups of test structures.
[0119] The technical solution of the utility model also provides a plurality of test structures of metal silicide barrier layer and contact hole, including two test structures of metal silicide barrier layer and contact hole, wherein one test structure is rotated 90 degrees compared with the other test structure.
[0120] Through the above technical means, the technical solution of the utility model can improve the offset test range of the metal silicide barrier layer. The specific reasons are as follows:
[0121] On the basis of the aforementioned test structure of the metal silicide barrier layer and the contact hole, a second group of test structures of the metal silicide barrier layer and the contact hole is also provided, wherein the second group of test structures of the metal silicide barrier layer and the contact hole is a test structure obtained by rotating the aforementioned test structure of the metal silicide barrier layer and the contact hole by 90 degrees. The first group of test structures is used to detect the longitudinal offset of the metal silicide barrier layer. The second group of test structures is used to detect the lateral offset of the metal silicide barrier layer. If the first ratios of the two groups of test structures change, it indicates that the metal silicide barrier layer is offset along the oblique direction.
[0122] For example, if the first ratio corresponding to the test structure arranged horizontally increases, while the first ratio corresponding to the test structure arranged vertically decreases, it indicates that the metal silicide barrier layer is offset along the upper right side. If the first ratio corresponding to the test structure arranged horizontally increases, while the first ratio corresponding to the test structure arranged vertically also increases, it indicates that the metal silicide barrier layer is offset along the upper left side. If the first ratio corresponding to the test structure arranged horizontally decreases, while the first ratio corresponding to the test structure arranged vertically also decreases, it indicates that the metal silicide barrier layer is offset along the lower right side. If the first ratio corresponding to the test structure arranged horizontally decreases, while the first ratio corresponding to the test structure arranged vertically increases, it indicates that the metal silicide barrier layer is offset along the lower left side.
[0123] In summary, the multiple groups of test structures for metal silicide barrier layers and contact holes provided in the embodiments of the present invention further include a second group of test structures for metal silicide barrier layers and contact holes on the basis of the aforementioned test structures for metal silicide barrier layers and contact holes, wherein the second group of test structures for metal silicide barrier layers and contact holes is a test structure obtained by rotating the aforementioned test structures for metal silicide barrier layers and contact holes by 90 degrees, thereby being able to detect whether an offset occurs between the metal silicide barrier layer and the first chain contact hole in the vertical direction.
[0124] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solution deviate from the scope of the technical solution of the embodiments of the utility model.
Claims
1. A test structure of a metal silicide barrier layer and a contact hole, wherein the test structure of the metal silicide barrier layer and the contact hole is arranged in a cutting path of a wafer, characterized in that: The test structure includes: A plurality of first structures in the form of strips arranged at a preset interval; a metal silicide barrier layer located on the first structure, the metal silicide barrier layer being rectangular in shape, and having a long side perpendicular to the first structure, the metal silicide barrier layer along the long side completely covering a plurality of the first structures, and the metal silicide barrier layer along the short side being located within the first structure; A first chain contact hole and a second chain contact hole located on the first structure, wherein the first chain contact hole and the second chain contact hole are respectively located on both sides of the metal silicide barrier layer along the short side; The distance between the first chain contact hole and the metal silicide barrier layer is less than a preset distance; the distance between the second chain contact hole and the metal silicide barrier layer is greater than or equal to a preset distance; the two ends of the first chain contact hole are led out by a first test pin and a third test pin, and the two ends of the second chain contact hole are led out by a second test pin and a fourth test pin; the resistance values of the contact holes measured at the two ends of the second chain contact hole are used as a reference for the resistance value of the first chain contact hole; The preset distance is used to characterize a minimum safety distance between the metal silicide barrier layer and the first chain contact hole.
2. The metal silicide barrier layer and contact hole test structure according to claim 1, characterized in that: The first structure is an ion-doped active region or an ion-doped polysilicon gate.
3. The metal silicide barrier layer and contact hole test structure according to claim 2, characterized in that: The ion-doped active region is P+ doped and N-well doped, and a shallow trench isolation structure is formed between the plurality of strip-shaped active regions.
4. The metal silicide barrier layer and contact hole test structure according to claim 2, characterized in that: The ion-doped active region is N+ doped, and a shallow trench isolation structure is formed between the plurality of strip-shaped active regions.
5. The metal silicide barrier layer and contact hole test structure according to claim 2, characterized in that: The ion-doped polysilicon is an N-type or P-type doped polysilicon gate; a plurality of strip-shaped polysilicon gates are arranged on a shallow trench isolation structure.
6. A test structure of multiple groups of metal silicide barrier layers and contact holes, characterized in that: It comprises a plurality of test structures of metal silicide barrier layers and contact holes as described in claim 1, wherein the distances between the first chain contact holes and the metal silicide barrier layers in different test structures are different, and the distances between the second chain contact holes and the metal silicide barrier layers are the same; and the two ends of the first chain contact holes in each group are led out by two test pins.
7. The multiple test structures of metal silicide barrier layer and contact hole according to claim 6, characterized in that: Among the plurality of groups of the first chain contact holes, two adjacent groups of the first chain contact holes share a test pin.
8. The multiple test structures of metal silicide barrier layer and contact holes according to claim 7, characterized in that: The metal silicide barrier layers in the multiple test structures are a whole, spanning across the multiple metal silicide barrier layers and a plurality of strip-shaped first structures in the test structures of the contact holes.
9. A test structure of multiple groups of metal silicide barrier layers and contact holes, characterized in that: The test structure includes the metal silicide barrier layer and the contact hole as described in claim 1, and also includes a second group of test structures of metal silicide barrier layers and contact holes, wherein the second group of test structures of metal silicide barrier layers and contact holes is a structure obtained by rotating the test structure of the metal silicide barrier layer and contact holes as described in claim 1 by 90 degrees.
Citation Information
Cited By
Semiconductor test structure and manufacturing method thereof
CN119381388A