Liquid silica gel aluminum piece double-face rubber coating integrated forming mold

Through the design of the liquid silicone aluminum double-bread glue integrated mold, the double-point glue injection is achieved using the ejection module and heating system, which solves the problem of excessive silicone forming time and risk of degumming, improves work efficiency and reduces production costs .

CN222201497UActive Publication Date: 2024-12-20XIAMEN WAEXIM RUBBER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323521097.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-22
Publication Date
2024-12-20
Estimated Expiration
2033-12-22

AI Technical Summary

Technical Problem

The existing double-sided bread glue products are too long in the silicone molding process due to poor heat dissipation effect, and the molding time is prone to degumming and damage to aluminum parts during the turning of bread glue. The residual gel in the glue-injected pipe is difficult to clean, which affects work efficiency. and cost.

Method used

A liquid silicone aluminum double-sided bread glue integrated mold is designed, including the mold rear mold and the cold mold half. The rear mold is equipped with an ejection module, a heating system and an auxiliary heat system, and the cold mold half is equipped with a top surface and The bottom surface cold nozzle achieves integrated molding through double-point glue injection, shortening the molding cycle and reducing risks.

Benefits of technology

It has achieved shortening the overall forming cycle, reducing the risk of glue wrapping, reducing processes and operators, reducing production costs, and improving the structural strength and service life of the mold.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222201497U_ABST
    Figure CN222201497U_ABST
Patent Text Reader

Abstract

The utility model discloses a liquid silica gel aluminum piece double-face rubber coating integrated forming die which comprises a die rear die and a die cold half die correspondingly connected with the die rear die, the die rear die comprises a rear die base, an ejection module is correspondingly arranged in the rear die base, a plurality of ejector pins are correspondingly arranged in the ejection module, and the ejector pins are arranged in the rear die base. The rear mold base is correspondingly connected with the rear mold frame, a plurality of ejector pin holes are formed in the rear mold frame, the ejector pins are sequentially matched with the ejector pin holes, and the rear mold frame is correspondingly connected with the rear mold core; the mold cold half mold comprises a cold half mold body which is correspondingly connected with the front mold core, and the front mold core is matched with the rear mold core. According to the utility model, the integral molding is realized through double-point glue feeding on the front and back surfaces of a product, the top cold nozzle of the front glue feeding point is arranged on the product, and the bottom cold nozzle of the back glue feeding point feeds glue through burrs, so that the integral molding period is shortened, and the risk of glue coating is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of rubber moulds, in particular to a liquid silicone aluminium part double-sided glue-coated integrated mould. Background Art

[0002] With the rapid development of material technology, silicone encapsulation is more common in the manufacturing industry. Silicone encapsulation is used to wrap a layer of liquid silicone on some metals, rubbers, plastics and other materials. By using the material properties of silicone, it has the advantages of good hand feel, aging resistance, good release, and anti-slip. Silicone encapsulation is the best packaging material for products.

[0003] However, during the product encapsulation process, the existing double-sided encapsulation products will have a long cooling time for the silicone molded product due to poor heat dissipation, which will increase the time required for the overall molding of a product, resulting in low work efficiency. In addition, the need to turn over the encapsulation will cause many special situations during the molding process, such as debonding, damage to the secondary encapsulation of aluminum parts, etc. During the silicone heating molding process, due to poor insulation effect, residual glue will condense in the injection pipe, making it difficult to clean. Therefore, it is necessary to provide a liquid silicone aluminum double-sided encapsulation integrated molding mold. Utility Model Content

[0004] In order to overcome the defects in the prior art, a liquid silicone aluminum double-sided adhesive-coated one-piece molding mold is provided.

[0005] The utility model is achieved through the following scheme:

[0006] A liquid silicone aluminum double-sided coated one-piece molding mold, comprising a mold rear mold and a mold cold half mold correspondingly connected thereto, the mold rear mold comprising a rear mold mold base, an ejection module correspondingly arranged in the rear mold mold base, a plurality of ejector pins correspondingly arranged in the ejection module, the rear mold mold base correspondingly connected to a rear mold mold frame, a plurality of ejector pin holes arranged in the rear mold mold frame, the ejector pins and the ejector pin holes matched in sequence, the rear mold mold frame correspondingly connected to a rear mold mold core, a pin hole correspondingly opened on the rear mold mold core, the ejector pins pass through the ejector pin holes and the pin hole in sequence; the mold cold half mold comprising a cold half mold, the cold half mold correspondingly connected to a front mold mold core, the front mold mold core matched with the rear mold mold core.

[0007] A plurality of fixing frames are correspondingly arranged around the ejection module, and positioning holes are correspondingly opened in the rear mold frame, and the fixing frames are fixedly connected with the positioning holes in a one-to-one correspondence.

[0008] A corresponding inwardly recessed slot is provided in the rear mold frame, and the slot is correspondingly connected to the rear mold core.

[0009] A heating system is correspondingly arranged on the side of the rear mold frame.

[0010] The cold half mold is provided with an inwardly recessed fixing groove, and the fixing groove is provided with a plurality of top surface cold nozzles and a plurality of bottom surface cold nozzles. The top surface cold nozzles and the bottom surface cold nozzles are connected with the front mold core accordingly.

[0011] The height of the top surface cold nozzle is smaller than the height of the bottom surface cold nozzle.

[0012] A plurality of mold spring blocks are correspondingly arranged in the mold core of the front mold.

[0013] The cold half mold is also provided with an auxiliary heating system and a water system.

[0014] The beneficial effects of the utility model are:

[0015] 1. The utility model is a liquid silicone aluminum double-sided gluing integrated molding mold that realizes integrated molding by gluing at two points on the front and back sides of a product. The top cold nozzle of the front glue injection point is on the product, and the bottom cold nozzle of the back glue injection point injects glue through the burr, which not only shortens the overall molding cycle, but also reduces the risk of gluing.

[0016] 2. The utility model provides a liquid silicone aluminum double-sided gluing integrated molding mold, which reduces the molding process of the product, reduces the increase in operators, and reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a schematic diagram of a partial explosion structure of a liquid silicone aluminum double-sided gluing integrated molding mold of the utility model;

[0018] In the figure: 1 is the rear mold base, 2 is the ejector module, 3 is the ejector pin, 4 is the fixing frame, 5 is the rear mold frame, 6 is the positioning hole, 7 is the ejector pin hole, 8 is the rear mold core, 9 is the slot, 10 is the heating system, 11 is the cold half mold, 12 is the front mold core, 13 is the fixing slot, 14 is the top surface cold nozzle, 15 is the bottom surface cold nozzle, 16 is the mold spring block, 17 is the auxiliary heating system, 18 is the water system, and 19 is the pinhole. DETAILED DESCRIPTION

[0019] The utility model is further described below in conjunction with the accompanying drawings:

[0020] A liquid silicone aluminum double-sided glue-coated one-piece molding mold comprises a mold rear mold and a mold cold half mold correspondingly connected thereto, wherein the mold rear mold comprises a rear mold base 1, and an ejection module 2 is correspondingly arranged in the rear mold base 1. When the product completes the vulcanization time and slides into place, the ejection module 2 automatically ejects the product to help demold the product. A plurality of ejector pins 3 are correspondingly arranged in the ejection module 2, the rear mold base 1 is correspondingly connected to the rear mold frame 5, the rear mold frame 5 is provided with a plurality of ejector pin holes 7, the ejector pins 3 and the ejector pin holes 7 are matched in sequence, the rear mold frame 5 is correspondingly connected to the rear mold core 8, and the rear mold core 8 is also correspondingly provided with a pinhole 19, the ejector pins 3 pass through the ejector pin holes 7 and the pinholes 19 in sequence, the rear mold core 8 is a key operating precision part in the center part of the mold, has no glue inlet and has pinholes, in the utility model, the ejector pins 3 are arranged in a rectangular array of four rows and three columns, the ejector pins 3 can be inserted into the ejector pin holes 7 and the pinholes 19 one by one, so that the ejection module 2 can eject the product from the mold core of the rear mold core 8 and demold it.

[0021] The cold half mold of the mold includes a cold half mold 11, and the cold half mold 11 is correspondingly connected to the front mold core 12. The front mold core 12 is a key operating precision part in the center of the mold, and is respectively provided with two top cold nozzles 14 and two bottom cold nozzles 15, with a total of four glue inlets. The front mold core 12 matches the rear mold core 8. A heating system 10 is correspondingly provided on the side of the rear mold frame 5. The cold half mold 11 is where the main body of the mold is located, and an auxiliary heating system 17 and a water system 18 are also correspondingly provided in the cold half mold 11. The utility model realizes one-piece molding by double-point gluing on the front and back sides of a product. The top cold nozzle of the front glue feeding point is on the product, and the bottom cold nozzle of the back glue feeding point is glued through the burr, which not only shortens the overall molding cycle, but also reduces the risk of glue encapsulation.

[0022] A plurality of fixing frames 4 are correspondingly arranged around the ejection module 2, and positioning holes 6 are correspondingly opened in the rear mold frame 5, and the fixing frames 4 are fixedly connected with the positioning holes 6 in a one-to-one correspondence. In the utility model, four fixing frames 4 are arranged, and the fixing frames 4 are inserted into the positioning holes 6 to strengthen the connection between the rear mold frame 5 and the rear mold base 1, enhance the structural strength, and improve the service life.

[0023] The rear mold frame 5 is provided with an inwardly recessed slot 9, and the slot 9 is correspondingly connected to the rear mold core 8. The utility model fixes the rear mold core 8 in the rear mold frame 5 through the slot 9, thereby enhancing the structural strength.

[0024] The cold half mold 11 is provided with a corresponding inwardly recessed fixing groove 13, and the fixing groove 13 is provided with a plurality of top cold nozzles 14 and a plurality of bottom cold nozzles 15, and the top cold nozzles 14 and the bottom cold nozzles 15 are connected to the front mold core 12. The height of the top cold nozzle 14 is less than the height of the bottom cold nozzle 15. In the utility model, the top cold nozzle 14, i.e., the top glue inlet, contacts the top product sealing ring, and glue is directly dispensed on the product, and the bottom cold nozzle 15, i.e., the bottom glue inlet, contacts the burr of the product, and glue is dispensed onto the product through the burr, so as to realize the one-piece molding of double-point glue injection on the front and back sides of a product, which can shorten the overall molding cycle and reduce the risk of glue encapsulation.

[0025] A plurality of mold spring blocks 16 are correspondingly arranged in the front mold core 12. In the present invention, four mold spring blocks 16 are arranged to prevent the product from sticking to the front mold core 12 and being difficult to demold. When the mold spring blocks 16 are activated after vulcanization molding, the product is positioned in the rear mold core 8. After the rear mold slides into place, the ejector module 2 ejects the product out of the mold core of the rear mold core 8 through the ejector pin 3.

[0026] In a specific embodiment, liquid silicone enters the top cold nozzle 14 and the bottom cold nozzle 15 at the same time, and then the glue inlet of the top cold nozzle 14 is injected into the mold cavity on the product, and at the same time, the glue inlet of the bottom cold nozzle 15 is injected into the mold cavity through the burr to perform vulcanization molding. After vulcanization molding, the mold spring block 16 is activated to position the product in the rear mold core 8. After the rear mold of the mold slides into place, the ejection module 2 ejects the product out of the mold core of the rear mold core 8 through the ejector pin 3 to complete the double-sided gluing integrated molding of the product.

[0027] Although the technical solutions of the present invention have been described and listed in detail, it should be understood that it is obvious to those skilled in the art to make modifications to the above-mentioned embodiments or adopt equivalent alternatives. These modifications or improvements made without departing from the spirit of the present invention are within the scope of protection required by the present invention.

Claims

1. A liquid silicone aluminum double-sided gluing integrated molding mold, comprising a mold back mold and a mold cold half mold correspondingly connected thereto, characterized in that: The rear mold of the mold comprises a rear mold base (1), an ejection module (2) is correspondingly arranged in the rear mold base (1), a plurality of ejector pins (3) are correspondingly arranged in the ejector module (2), the rear mold base (1) is correspondingly connected to a rear mold frame (5), a plurality of ejector pin holes (7) are arranged in the rear mold frame (5), the ejector pins (3) and the ejector pin holes (7) are matched in sequence, the rear mold frame (5) is correspondingly connected to a rear mold core (8), a pin hole (19) is correspondingly opened on the rear mold core (8), and the ejector pins (3) pass through the ejector pin holes (7) and the pin hole (19) in sequence; the cold half mold of the mold comprises a cold half mold (11), the cold half mold (11) is correspondingly connected to a front mold core (12), and the front mold core (12) is matched with the rear mold core (8).

2. A liquid silicone aluminum double-sided adhesive integrated molding mold according to claim 1, characterized in that: A plurality of fixing frames (4) are correspondingly arranged around the ejection module (2), and positioning holes (6) are correspondingly opened in the rear mold frame (5), and the fixing frames (4) are fixedly connected to the positioning holes (6) in a one-to-one corresponding manner.

3. The liquid silicone aluminum double-sided adhesive integrated molding mold according to claim 1, characterized in that: The rear mold frame (5) is provided with an inwardly recessed slot (9), and the slot (9) is correspondingly connected to the rear mold core (8).

4. A liquid silicone aluminum double-sided adhesive-coated integrated molding mold according to claim 3, characterized in that: A heating system (10) is correspondingly provided on the side of the rear mold frame (5).

5. The liquid silicone aluminum double-sided adhesive-coated integrated molding mold according to claim 1, characterized in that: The cold half mold (11) is provided with an inwardly recessed fixing groove (13), and the fixing groove (13) is provided with a plurality of top surface cold nozzles (14) and a plurality of bottom surface cold nozzles (15). The top surface cold nozzles (14) and the bottom surface cold nozzles (15) are connected to the front mold core (12) accordingly.

6. The liquid silicone aluminum double-sided adhesive-coated integrated molding mold according to claim 5, characterized in that: The height of the top surface cold nozzle (14) is smaller than the height of the bottom surface cold nozzle (15).

7. The liquid silicone aluminum double-sided adhesive-coated integrated molding mold according to claim 1, characterized in that: A plurality of mold spring blocks (16) are correspondingly arranged in the front mold core (12).

8. The liquid silicone aluminum double-sided adhesive-coated integrated molding mold according to claim 1, characterized in that: The cold half mold (11) is also provided with an auxiliary heating system (17) and a water system (18).