Corrosion-resistant hot-rolled coiled plate
By setting auxiliary cutting lines and corrosion-resistant layers on the hot-rolled coil plate, the problems of high labor cost and easy corrosion in cutting of hot-rolled coil plates are solved, and the effect of reducing costs and extending service life is achieved.
Patent Information
- Application Number
- CN202421517848.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-30
- Publication Date
- 2025-05-13
- Estimated Expiration
- 2034-06-30
AI Technical Summary
Hot-rolled coils need to be marked manually during cutting, resulting in high labor costs and prone to errors, affecting product quality, and metal products are prone to corrosion and shorten their service life.
A corrosion-resistant hot-rolled coil is designed, and the hot-rolled coil body is used in conjunction with auxiliary cutting lines to reduce friction and resistance of the cutting knife; corrosion-resistant layers, heat insulation layers, sound silence layers and reinforcement ribs are provided on the surface and inside.
By setting the auxiliary cutting line, manual positioning errors are reduced and labor and maintenance costs are reduced; corrosion-resistant layer extends service life, thermal insulation layer and sound silence layer improve practicality, and reinforcement ribs improve rigidity.
Smart Images

Figure CN222858932U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of hot-rolled coils, and more specifically, particularly relates to a corrosion-resistant hot-rolled coil. Background Art
[0002] Hot rolled coil, also known as hot rolled coil, is made of slab (mainly continuous casting slab) as raw material, and is made into strip steel by rough rolling unit and finishing rolling unit after heating. The hot steel strip coming out of the last rolling mill of finishing rolling is cooled to the set temperature by laminar flow, and is rolled into steel strip coil by coiler. The cooled steel strip coil.
[0003] Before using the hot-rolled coil, it is necessary to flatten it and then cut it. During cutting, the staff is required to mark the cutting length on the hot-rolled coil, which increases the labor cost and is prone to errors, affecting product quality. The material of the hot-rolled coil is usually metal, which can easily cause wear on the cutting knife of the cutting machine during cutting, increasing maintenance costs. In addition, the surface of metal products exposed to the air for a long time is prone to corrosion, affecting the service life of the hot-rolled coil.
[0004] Therefore, in view of this, the existing structure and defects are studied and improved, and a corrosion-resistant hot-rolled coil is provided to achieve a more practical purpose. Utility Model Content
[0005] In order to solve the above technical problems, the utility model provides a corrosion-resistant hot-rolled coil, which is achieved by the following specific technical means:
[0006] A corrosion-resistant hot-rolled coil comprises a hot-rolled coil body, a plurality of auxiliary cutting lines are equidistantly arranged on one side of the hot-rolled coil body, U-shaped frames are symmetrically installed on both sides of the hot-rolled coil body, a first threaded hole is arranged on one side of the U-shaped frame, a limit plate is rotatably installed on one side of the U-shaped frame, a second threaded hole is penetrated by the limit plate at one end close to the first threaded hole, and a fastening bolt is threadedly connected to the inner surface of the second threaded hole.
[0007] Furthermore, one end of the fastening bolt is threadedly connected to the first threaded hole.
[0008] Furthermore, a corrosion-resistant layer is provided on the surface of the hot-rolled coil body.
[0009] Furthermore, a heat insulation layer is provided inside the hot-rolled coil body.
[0010] Furthermore, a sound-absorbing layer is provided inside the hot-rolled coil body.
[0011] Furthermore, reinforcing ribs are provided inside the hot-rolled coil body.
[0012] Compared with the prior art, the utility model has the following beneficial effects:
[0013] The corrosion-resistant hot-rolled coil in the utility model, through the coordinated use of the hot-rolled coil body and the auxiliary cutting line, is convenient for workers to quickly locate the length of the hot-rolled coil that needs to be cut, and reduces the friction and resistance of the cutting knife during cutting, thereby reducing labor costs and maintenance costs.
[0014] The corrosion-resistant hot-rolled coil in the utility model, through the coordinated use of the corrosion-resistant layer, the heat-insulating layer and the sound-absorbing layer, is convenient for slowing down the speed at which the surface of the hot-rolled coil is damaged due to corrosion. At the same time, when the hot-rolled coil is used as a building material or a factory consumable material, heat and noise are blocked and absorbed, thereby extending the service life of the hot-rolled coil and improving the practicality of the hot-rolled coil. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a three-dimensional schematic diagram of the utility model.
[0016] Figure 2 It is a top view and cross-sectional schematic diagram of a partial structure of the utility model.
[0017] Figure 3 It is a top view schematic diagram of the hot-rolled coil body of the utility model when it is unfolded.
[0018] Figure 4 It is a side cross-sectional schematic diagram of the internal structure of the hot-rolled coil of the utility model.
[0019] In the figure, the corresponding relationship between the component names and the figure numbers is as follows:
[0020] 1. Hot-rolled coil body; 2. Auxiliary cutting line; 3. U-shaped frame; 4. First threaded hole; 5. Limiting plate; 6. Second threaded hole; 7. Fastening bolt; 8. Corrosion-resistant layer; 9. Heat insulation layer; 10. Sound-absorbing layer; 11. Reinforcement ribs. DETAILED DESCRIPTION
[0021] The following is a further detailed description of the implementation of the present invention in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but cannot be used to limit the scope of the present invention.
[0022] In the description of the present invention, unless otherwise specified, "multiple" means two or more; the terms "upper", "lower", "left", "right", "inner", "outer", "front end", "rear end", "head", "tail" and the like indicate the orientation or positional relationship based on the orientation or positional relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", "third" and the like are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0023] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "connected" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0024] Example:
[0025] As attached Figure 1 To Attachment Figure 4 As shown:
[0026] The utility model provides a corrosion-resistant hot-rolled coil, comprising a hot-rolled coil body 1, a plurality of auxiliary cutting lines 2 are equidistantly arranged on one side of the hot-rolled coil body 1, U-shaped frames 3 are symmetrically installed on both sides of the hot-rolled coil body 1, a first threaded hole 4 is arranged on one side of the U-shaped frame, a limiting plate 5 is rotatably installed on one side of the U-shaped frame, a second threaded hole 6 is penetrated at one end of the limiting plate 5 close to the first threaded hole 4, and a fastening bolt 7 is threadedly connected to the inner thread of the second threaded hole 6.
[0027] Among them, one end of the fastening bolt 7 is threadedly connected to the first threaded hole 4, and the fastening bolt 7 is screwed into the first threaded hole 4 and the second threaded hole 6 in sequence, so that the limit plate 5 is fixed to one side of the U-shaped frame, thereby clamping and fixing the hot-rolled coil body 1 to prevent the hot-rolled coil body 1 from spreading due to shaking.
[0028] The surface of the hot-rolled coil body 1 is provided with a corrosion-resistant layer 8 to reduce the corrosion of the hot-rolled coil body 1 during long-term use.
[0029] The interior of the hot-rolled coil body 1 is provided with a heat insulation layer 9, and when the outside temperature is high, the heat insulation layer 9 can block the heat.
[0030] A sound-absorbing layer 10 is provided inside the hot-rolled coil body 1 to isolate external noise.
[0031] Among them, a reinforcing rib 11 is provided inside the hot-rolled coil body 1 to improve the rigidity of the hot-rolled coil.
[0032] The working principle of this embodiment is as follows: when the coil is placed, the fastening bolt 7 is located in the first threaded hole 4 and the second threaded hole 6, so that the limit plate 5 is fixed to one side of the U-shaped frame, so as to clamp and fix the hot-rolled coil body 1, and prevent the hot-rolled coil body 1 from spreading due to shaking. When the hot-rolled coil needs to be used, the fastening bolt 7 is unscrewed and the limit plate 5 is rotated so that the limit plate 5 no longer limits the hot-rolled coil. At this time, the U-shaped frame 3 can be removed, and the hot-rolled coil can be unfolded for subsequent processing. The setting of the auxiliary cutting line 2 can facilitate the staff to quickly locate the position where the hot-rolled coil body 1 needs to be cut, and reduce the wear on the cutting machine during cutting. In addition, the corrosion-resistant layer 8 on the surface of the hot-rolled coil body 1 can reduce the corrosion of the hot-rolled coil body 1 during long-term use. The heat insulation layer 9 inside the hot-rolled coil can block heat, the sound-absorbing layer 10 can absorb noise, and the reinforcing ribs 11 can improve the rigidity of the hot-rolled coil.
[0033] The embodiments of the present invention are provided for the purpose of illustration and description, and are not intended to be exhaustive or to limit the present invention to the disclosed forms. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiments are selected and described to better illustrate the principles and practical applications of the present invention, and to enable those of ordinary skill in the art to understand the present invention and thereby design various embodiments with various modifications suitable for specific uses.
Claims
1. A corrosion-resistant hot-rolled coil, comprising a hot-rolled coil body (1), characterized in that: A plurality of auxiliary cutting lines (2) are equidistantly arranged on one side of the hot-rolled coil body (1); U-shaped frames (3) are symmetrically installed on both sides of the hot-rolled coil body (1); a first threaded hole (4) is arranged on one side of the U-shaped frame (3); a limit plate (5) is rotatably installed on one side of the U-shaped frame; a second threaded hole (6) is penetrated through the limit plate (5) at one end close to the first threaded hole (4); a fastening bolt (7) is connected to the inner thread of the second threaded hole (6).
2. The corrosion-resistant hot-rolled coil according to claim 1, characterized in that: One end of the fastening bolt (7) is threadedly connected to the first threaded hole (4).
3. The corrosion-resistant hot-rolled coil according to claim 1, characterized in that: The surface of the hot-rolled coil body (1) is provided with a corrosion-resistant layer (8).
4. The corrosion-resistant hot-rolled coil according to claim 1, characterized in that: A heat insulation layer (9) is provided inside the hot-rolled coil body (1).
5. The corrosion-resistant hot-rolled coil according to claim 1, characterized in that: A sound-absorbing layer (10) is provided inside the hot-rolled coil body (1).
6. The corrosion-resistant hot-rolled coil according to claim 1, characterized in that: A reinforcing rib (11) is provided inside the hot-rolled coil body (1).