Capacitor low voltage etching aluminum foil electrolytic processing device
Patent Information
- Application Number
- CN202522644831.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-13
- Publication Date
- 2026-11-03
- Estimated Expiration
- 2035-12-13
AI Technical Summary
Existing electrolytic treatment equipment for low-voltage corrosion of aluminum foil in capacitors has poor production efficiency and is not convenient for cleaning and drying, which makes the aluminum foil prone to oxidation during storage and transportation, affecting its performance.
An electrolytic etching device for low-voltage corrosion of aluminum foil for capacitors, comprising an electrolytic structure and a cleaning structure, is designed. The electrolytic structure provides electrolytic etching through conductive rollers and titanium pillars, while the cleaning structure achieves cleaning and drying through a cleaning tank and a drying seat.
This method achieves effective electrolytic etching of aluminum foil, facilitates cleaning and drying, prevents oxidation, and improves the performance of the aluminum foil and the practicality of the device.
Smart Images

Figure CN224930690U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of aluminum foil electrolytic etching technology, and in particular to an electrolytic etching device for low-voltage corrosion of aluminum foil for capacitors. Background Technology
[0002] The aluminum foil used in capacitors can affect key performance parameters such as capacitance, rated voltage, leakage current, loss and lifespan. Electrolytic etching is an essential process in the production of these capacitors.
[0003] To this end, patent CN202671701U discloses an aluminum foil electrolysis device, belonging to the technical field of aluminum foil electrolysis equipment. The technical problem to be solved is to provide an aluminum foil electrolysis device that can effectively improve the production efficiency of aluminum foil and reduce the production cost. The technical solution adopted is as follows: multiple conductive electrode rollers for aluminum foil transmission are set on the frame, an electrolysis tank filled with bath liquid is installed below the frame, a pair of graphite electrodes are inserted into the top of the electrolysis tank and the graphite electrodes are immersed in the bath liquid, a through hole is set at the top of the electrolysis tank for the aluminum foil to pass through, and a bottom roller for the aluminum foil transmission is set at the bottom inside the electrolysis tank. This utility model is mainly used for the electrolysis of aluminum foil.
[0004] The electrolysis device described above is not convenient for quickly electrolytic etching, cleaning, and drying of aluminum foil during actual use, which may lead to oxidation during subsequent storage and transportation, affecting the performance. Utility Model Content
[0005] The purpose of this invention is to provide an electrolytic treatment device for low-voltage corrosion of aluminum foil in capacitors, in order to solve the defects of existing electrolytic treatment devices for low-voltage corrosion of aluminum foil in capacitors, which have poor production effect and are inconvenient to clean and dry.
[0006] To solve the above-mentioned technical problems, this utility model provides the following technical solution: a capacitor low-voltage corrosion aluminum foil electrolytic treatment device, including a base and an unwinding shaft;
[0007] A roll unwinding shaft is installed on one side of the base, and an electrolytic structure is provided on one side of the base.
[0008] The electrolysis structure includes an electrolysis cell disposed on one side of the base. Each electrolysis cell is equipped with a protective shaft at its top. A power source is installed on the outside of the electrolysis cell. Conductive rollers are evenly arranged on one side of the power source. Titanium columns are evenly installed on the side of the power source away from the conductive rollers. A heat exchanger is installed inside the electrolysis cell. A temperature sensor is installed on the inner wall of the electrolysis cell.
[0009] A winding motor is installed on one side of the base, a winding shaft is provided on one side of the winding motor, and a cleaning structure is provided on one side of the base.
[0010] Preferably, the protective shafts are symmetrically distributed at the top of the electrolytic cell, and the conductive rollers extend into the interior of the electrolytic cell.
[0011] Preferably, the titanium pillar extends into the interior of the electrolytic cell, and the conductive roller and the titanium pillar are symmetrically distributed on one side of the power source.
[0012] Preferably, the temperature sensor is externally connected to a microcontroller, and the output terminal of the microcontroller is electrically connected to the input terminal of the heat exchanger.
[0013] Preferably, the cleaning structure includes a cleaning tank disposed on one side of the base, with fixed shafts evenly installed inside the cleaning tank, a drying seat disposed on one side of the cleaning tank, reserved slots evenly opened inside the drying seat, electric hot air blowers installed inside each of the reserved slots, and guide shafts installed on both sides of the drying seat.
[0014] Preferably, the fixed shafts are evenly distributed inside the cleaning tank, and the reserved slots are evenly distributed at the top of the drying seat.
[0015] Preferably, the guide shafts are symmetrically distributed on both sides of the drying seat.
[0016] The advantages of the electrolytic treatment device for low-voltage corrosion of aluminum foil in capacitors provided by this utility model are as follows:
[0017] By incorporating an electrolytic structure, the aluminum foil passes through the interior of the electrolytic cell via a protective shaft and a conductive roller, powered by a power source. The positive terminal of the power source is connected to the conductive roller, and the negative terminal is connected to the titanium pillar. The conductive roller and the aluminum foil come into contact with each other, thereby introducing current into the interior of the aluminum foil to meet the electrode requirements of electrolysis. A temperature sensor and a heat exchanger are provided to control the temperature of the liquid inside the electrolytic cell, thus facilitating the electrolytic etching process on the aluminum foil.
[0018] The system incorporates a cleaning structure, where the electrolyzed aluminum foil is washed in a cleaning tank and then passes through a drying chamber. The drying chamber has pre-drilled slots with electric hot air blowers installed inside to dry the aluminum foil. This process effectively removes and dries the acidic solution from the surface of the electrolyzed aluminum foil. Attached Figure Description
[0019] Figure 1 This is a front-view three-dimensional schematic diagram of the present invention;
[0020] Figure 2 This is a frontal three-dimensional schematic diagram of the present invention;
[0021] Figure 3 This is a three-dimensional schematic diagram of the splitting of this utility model;
[0022] Figure 4 This is a side view three-dimensional schematic diagram of the present invention;
[0023] Figure 5 This is a top-view three-dimensional schematic diagram of the present invention.
[0024] The following are the annotations in the figure: 1. Base; 2. Unwinding shaft; 3. Electrolysis structure; 301. Electrolytic cell; 302. Protective shaft; 303. Power supply; 304. Conductive roller; 305. Titanium column; 306. Heat exchanger; 307. Temperature sensor; 4. Rewinding motor; 5. Rewinding shaft; 6. Cleaning structure; 601. Cleaning tank; 602. Fixed shaft; 603. Drying seat; 604. Reserved slot; 605. Electric hot air blower; 606. Guide shaft. Detailed Implementation
[0025] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the protection scope of the present utility model.
[0026] Please see Figure 1 - Figure 5 The capacitor low-voltage corrosion aluminum foil electrolytic treatment device provided by this utility model includes a base 1 and an unwinding shaft 2.
[0027] Reference Figure 1 - Figure 3 As shown, a unwinding shaft 2 is installed on one side of the base 1, and an electrolysis structure 3 is provided on one side of the base 1. The electrolysis structure 3 includes an electrolysis cell 301 located on one side of the base 1. A protective shaft 302 is installed at the top of each electrolysis cell 301. A power supply 303 is installed on the outside of the electrolysis cell 301. Conductive rollers 304 are evenly arranged on one side of the power supply 303. Titanium pillars 305 are evenly installed on the side of the power supply 303 away from the conductive rollers 304. A heat exchanger 306 is installed inside the electrolysis cell 301. A temperature sensor 307 is installed on the inner wall of the electrolysis cell 301. The protective shafts 302 are symmetrically distributed at the top of the electrolysis cell 301. The conductive rollers 304 extend into the interior of the electrolysis cell 301. The titanium pillars 305 extend into the interior of the electrolysis cell 301. The conductive rollers 304 and titanium pillars 305 are symmetrically distributed on one side of the power supply 303. A microcontroller is externally connected to the temperature sensor 307. The output terminal of the microcontroller is electrically connected to the input terminal of the heat exchanger 306.
[0028] During the production and processing of capacitor aluminum foil, it needs to undergo electrolytic etching to electrochemically corrode and form a porous structure, increasing the surface area by tens to hundreds of times to improve the performance of the capacitor aluminum foil. During electrolysis, an electrolytic structure 3 is incorporated, ensuring that the aluminum foil enters the electrolytic cell 301 while protective shafts 302 are fixed on both sides of the top of the electrolytic cell 301 to prevent scratches or other damage during entry. The top of the aluminum foil also abuts against the bottom of the conductive roller 304. The conductive roller 304 conducts electrical conductivity to the aluminum foil, and the conductive roller 304 is connected to the positive terminal of the power supply 303. The titanium pillar 305 is connected to the negative terminal of the power supply 303, thereby meeting the electrolysis requirements. The temperature of the solution inside the electrolytic cell 301 is changed by the heat exchanger 306 and monitored by the temperature sensor 307. The microcontroller connected to the temperature sensor 307 controls the heat exchanger 306 at all times to keep the temperature inside the electrolytic cell 301 at the appropriate electrolysis temperature, thereby greatly increasing the practicality of the device.
[0029] Reference Figure 1 , Figure 2 , Figure 4 and Figure 5 As shown, a winding motor 4 is installed on one side of the base 1, and a winding shaft 5 is provided on one side of the winding motor 4. A cleaning structure 6 is provided on one side of the base 1. The cleaning structure 6 includes a cleaning tank 601 provided on one side of the base 1. Fixed shafts 602 are evenly installed inside the cleaning tank 601. A drying seat 603 is provided on one side of the cleaning tank 601. Reserved slots 604 are evenly opened inside the drying seat 603. Electric hot air blowers 605 are installed inside each of the reserved slots 604. Guide shafts 606 are installed on both sides of the drying seat 603. The fixed shafts 602 are evenly distributed inside the cleaning tank 601. The reserved slots 604 are evenly distributed at the top of the drying seat 603. The guide shafts 606 are symmetrically distributed on both sides of the drying seat 603.
[0030] After electrolytic etching of aluminum foil, a cleaning structure 6 is provided to facilitate the cleaning and drying of the aluminum foil surface. The aluminum foil is washed by water through the cleaning tank 601 via the fixed shaft 602. The washed aluminum foil is then passed through the drying seat 603 and dried by the electric hot air blower 605 inside the pre-reserved groove 604 at the top of the drying seat 603. This prevents oxidation of the aluminum foil during storage and transportation, thereby protecting the aluminum foil and improving its performance. This greatly increases the practicality of the device.
[0031] Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A capacitor low-voltage corrosion aluminum foil electrolytic treatment device, comprising a base (1) and an unwinding shaft (2); Its features are: A roll unwinding shaft (2) is installed on one side of the base (1), and an electrolytic structure (3) is provided on one side of the base (1); The electrolysis structure (3) includes an electrolysis cell (301) disposed on one side of the base (1). A protective shaft (302) is installed at the top of the electrolysis cell (301). A power supply (303) is installed on the outside of the electrolysis cell (301). Conductive rollers (304) are uniformly arranged on one side of the power supply (303). Titanium columns (305) are uniformly installed on the side of the power supply (303) away from the conductive rollers (304). A heat exchanger (306) is installed inside the electrolysis cell (301). A temperature sensor (307) is installed on the inner wall of the electrolysis cell (301). A winding motor (4) is installed on one side of the base (1), a winding shaft (5) is provided on one side of the winding motor (4), and a cleaning structure (6) is provided on one side of the base (1).
2. The capacitor low-voltage corrosion aluminum foil electrolytic treatment apparatus according to claim 1, characterized in that: The protective shaft (302) is symmetrically distributed at the top of the electrolytic cell (301), and the conductive roller (304) extends into the interior of the electrolytic cell (301).
3. The electrolytic treatment apparatus for low-voltage corrosion of aluminum foil in capacitors according to claim 1, characterized in that: The titanium pillar (305) extends into the interior of the electrolytic cell (301), and the conductive roller (304) and the titanium pillar (305) are symmetrically distributed on one side of the power source (303).
4. The electrolytic treatment apparatus for low-voltage corrosion of aluminum foil in capacitors according to claim 1, characterized in that: The temperature sensor (307) is externally connected to a microcontroller, and the output terminal of the microcontroller is electrically connected to the input terminal of the heat exchanger (306).
5. The electrolytic treatment apparatus for low-voltage corrosion of aluminum foil in capacitors according to claim 1, characterized in that: The cleaning structure (6) includes a cleaning tank (601) disposed on one side of the base (1). Fixed shafts (602) are evenly installed inside the cleaning tank (601). A drying seat (603) is disposed on one side of the cleaning tank (601). Reserved slots (604) are evenly opened inside the drying seat (603). Electric hot air blowers (605) are installed inside each of the reserved slots (604). Guide shafts (606) are installed on both sides of the drying seat (603).
6. The electrolytic treatment apparatus for low-voltage corrosion of aluminum foil in capacitors according to claim 5, characterized in that: The fixed shafts (602) are evenly distributed inside the cleaning tank (601), and the reserved slots (604) are evenly distributed at the top of the drying seat (603).
7. The electrolytic treatment apparatus for low-voltage corrosion of aluminum foil in capacitors according to claim 5, characterized in that: The guide shaft (606) is symmetrically distributed on both sides of the drying seat (603).