Pipe die for rapid cooling of material
By setting an arc-shaped groove structure on the outer wall of the ductile iron pipe mold, the problem of low cooling efficiency in traditional methods is solved, enabling rapid cooling and efficient production, improving the production efficiency and quality of ductile iron pipes, and extending the service life of the pipe mold.
Patent Information
- Application Number
- CN202522106369.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-29
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-09-29
AI Technical Summary
Traditional ductile iron pipe molds have low cooling efficiency, which leads to longer production cycles and affects production efficiency and product quality.
An arc-shaped groove structure is set on the outer wall of the tube mold to increase the contact area between the coolant and the tube mold. This includes annular, threaded, and oblique arc-shaped groove designs to improve heat exchange efficiency.
It significantly improves cooling efficiency, shortens production cycle, increases production efficiency and product quality, and extends the service life of tube molds.
Smart Images

Figure CN224950940U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of tube mold equipment technology, specifically to a tube mold for rapidly cooling materials. Background Technology
[0002] In the production process of ductile iron pipes, the pipe mold is a key tool for forming, and its cooling efficiency directly affects the forming speed, production efficiency, and quality of the final product.
[0003] Traditional ductile iron pipe molds typically employ a cylindrical planar design. This design limits the contact area between the mold and the cooling water during the cooling process, resulting in a relatively slow cooling rate of the molten iron within the mold. This, in turn, prolongs the production cycle, reduces production efficiency, and may adversely affect the internal structure and mechanical properties of the ductile iron pipe.
[0004] Specifically, traditional cylindrical planar tube molds rely primarily on heat conduction between the mold wall and cooling water for heat dissipation during cooling.
[0005] However, due to the small contact area and low heat transfer efficiency, especially during large-scale continuous production, the cooling effect of the tube mold is even more difficult to meet the needs of efficient and high-quality production. Utility Model Content
[0006] In view of this, the present invention provides a tube mold for rapid cooling of materials. The present invention can increase the heat exchange efficiency between cooling water and tube mold through arc groove, thereby enabling rapid cooling of cast iron pipe, which can effectively increase the production efficiency of ductile iron pipe.
[0007] To solve the above-mentioned technical problems, this utility model provides a tube mold for rapid cooling of materials, including a tube mold and a plurality of arc-shaped groove structures disposed on the outer wall of the tube mold. The arc-shaped grooves can increase the contact area between the coolant and the outer wall of the tube mold.
[0008] The arc groove is an annular arc groove set on the outer wall of the tube mold. The cross-section of the annular arc groove is a circular ring structure and it is located on the same axis as the tube mold.
[0009] The arc-shaped groove is a threaded arc-shaped groove set on the outer wall of the tube mold, and the axis of the threaded arc-shaped groove is located on the same axis as the tube mold.
[0010] The middle part of the tube mold is cylindrical, and one end is frustum-shaped. The outer surface of the cylindrical structure in the middle part of the tube mold is provided with an annular arc groove, and the outer surface of the frustum-shaped structure at one end of the tube mold is provided with a threaded arc groove.
[0011] The arc-shaped grooves are set on the outer surface of the tube mold in an oblique arc shape, and the arc-shaped grooves are arranged at an angle on the outer surface of the tube mold.
[0012] In summary, compared with the prior art, this application includes at least one of the following beneficial technical effects:
[0013] 1. Significantly improved cooling efficiency:
[0014] Traditional cylindrical, planar mold designs result in slow cooling due to limited contact area. This invention utilizes an arc-shaped groove structure to increase the contact area between the coolant and the mold several times (e.g., a threaded design can increase the contact area by 5-6 times), thereby accelerating molten iron cooling, shortening the forming cycle of ductile iron pipes, and improving production efficiency.
[0015] 2. Dual optimization of production efficiency and quality:
[0016] Rapid cooling reduces the residence time of molten iron at high temperatures, lowering the risk of grain coarsening and contributing to a finer internal microstructure, thus improving the mechanical properties and surface quality of ductile iron pipes. Simultaneously, the shortened production cycle directly increases output per unit time, meeting the demands of large-scale continuous production.
[0017] 3. Strong structural adaptability and flexible application:
[0018] This invention provides various arc-shaped groove designs (annular, threaded, and oblique), which can be selected or combined according to actual production needs. For example, an annular arc-shaped groove in the middle cylindrical section can ensure uniform cooling, a threaded arc-shaped groove in the frustum section at one end can adapt to changes in the shape of the mold tube, and an oblique arc-shaped groove further optimizes the flow path of the coolant and enhances the local heat exchange effect.
[0019] 5. Extend the service life of the pipe mold:
[0020] Rapid cooling reduces thermal fatigue damage to the tube mold caused by prolonged high temperatures, lowers the risk of cracking or deformation, extends the service life of the tube mold, and further reduces replacement costs. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the structure of a tube mold for rapidly cooling materials according to this utility model;
[0022] Figure 2 This is a schematic diagram of the threaded arc groove of this utility model;
[0023] Figure 3 This is a schematic diagram of the integrated structure of the threaded arc groove and the annular arc groove of this utility model;
[0024] Figure 4 This is a schematic diagram of the oblique arc-shaped groove of this utility model.
[0025] Explanation of reference numerals in the attached figures:
[0026] 1. Tube mold; 2. Annular arc groove; 3. Threaded arc groove; 4. Inclined arc groove. Detailed Implementation
[0027] To make the objectives, technical solutions, and advantages of the embodiments of this utility model clearer, the following will be described in conjunction with the appendices of the embodiments of this utility model. Figure 1-4 The technical solutions of the embodiments of this utility model are clearly and completely described herein. Obviously, the described embodiments are only some, not all, of the embodiments of this utility model. All other embodiments obtained by those skilled in the art based on the described embodiments of this utility model are within the protection scope of this utility model.
[0028] Example 1:
[0029] A tube mold 1 for rapidly cooling materials, such as Figure 1 As shown: It includes a pipe mold 1 and multiple arc-shaped grooves disposed on the outer wall of the pipe mold 1. Each arc-shaped groove is an annular arc-shaped groove 2. The annular arc-shaped groove 2 and the pipe mold 1 are located on the same axis, and the distance between any two adjacent annular arc-shaped grooves 2 is the same. That is, after the coolant is sprayed onto the outer surface of the pipe mold 1, it can flow into the annular arc-shaped groove 2, thereby effectively increasing the contact area between the pipe mold 1 and the coolant. This allows the ductile iron pipe inside the pipe mold 1 to be cooled quickly, thereby improving the production efficiency of ductile iron pipes.
[0030] Example 2:
[0031] like Figure 2 As shown: The difference from Embodiment 1 is that the arc groove on the outer wall of the pipe mold 1 is a threaded arc groove 3. The threaded arc groove 3 is easier to process than the annular arc groove 2, that is, the threaded arc groove 3 can be processed in one go, and it can also increase the contact area between the coolant and the pipe mold 1, thereby improving the production efficiency of ductile iron pipes.
[0032] Example 3:
[0033] like Figure 3 As shown, the difference from Embodiments 1 and 2 is that: the outer surface of the pipe mold 1 is provided with an annular arc groove 2 and a threaded arc groove 3; the middle part of the pipe mold 1 is a cylindrical structure, and one end of the pipe mold 1 is a frustum-shaped structure with a T-shaped cross-section, that is, the end with the larger cross-section is located at the end face of the pipe mold 1; the outer surface of the middle part of the pipe mold 1 is provided with a threaded groove, and the outer wall surface of the frustum structure at one end of the pipe mold 1 is provided with an annular arc groove 2 (the annular arc groove 2 on the outer surface of the frustum structure is easier to machine than the threaded arc groove 3). This also increases the contact area between the coolant and the pipe mold 1, thereby improving the production efficiency of ductile iron pipes.
[0034] Example 4:
[0035] like Figure 4 As shown: The difference from Embodiment 1 is that the outer surface of the pipe mold 1 is provided with an inclined arc groove 4, that is, the arc groove is arranged at an inclination on the outer wall of the pipe mold 1, and can also increase the contact area between the coolant and the pipe mold 1, thereby improving the production efficiency of ductile iron pipe.
[0036] Furthermore, it should be noted that, in the description of this utility model, unless otherwise explicitly specified and limited, the terms "installation," "connection," and "joining" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection of two components. Those skilled in the art can understand the specific meaning of the above terms in this utility model according to the specific circumstances.
[0037] The above description is the preferred embodiment of this utility model. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of this utility model, and these improvements and modifications should also be considered within the protection scope of this utility model.
Claims
1. A tube mold for rapidly cooling materials, characterized in that, It includes a tube mold (1) and several arc-shaped groove structures on the outer wall of the tube mold (1). The arc-shaped grooves can increase the contact area between the coolant and the outer wall of the tube mold (1).
2. The tube mold (1) for rapidly cooling materials as described in claim 1, characterized in that, The arc groove is an annular arc groove (2) set on the outer wall of the tube mold (1). The cross-section of the annular arc groove (2) is a circular ring structure and is located on the same axis as the tube mold (1).
3. The tube mold (1) for rapidly cooling materials as described in claim 1, characterized in that, The arc groove is a threaded arc groove (3) set on the outer wall of the tube mold (1), and the axis of the threaded arc groove (3) is located on the same axis as the tube mold (1).
4. The tube mold (1) for rapid cooling of materials as described in claim 1, characterized in that, The middle part of the tube mold (1) is a cylindrical structure, and one end is a frustum-shaped structure. The outer surface of the cylindrical structure in the middle part of the tube mold (1) is provided with an annular arc groove (2), and the outer surface of the frustum-shaped structure at one end of the tube mold (1) is provided with a threaded arc groove (3).
5. The tube mold (1) for rapidly cooling materials as described in claim 1, characterized in that, The arc-shaped groove is set on the inclined arc-shaped groove (4) on the outer surface of the tube mold (1), and the inclined arc-shaped groove (4) is arranged obliquely on the outer surface of the tube mold (1).