A steel-lined ceramic centrifugal pump
By designing a steel-lined ceramic structure, the solidified body and buffer sleeve are used to disperse the fastening force. Combined with the anti-corrosion layer and wear-resistant ceramic layer, the problems of cracking and insufficient wear resistance of ceramic centrifugal pumps are solved, and stable transportation in high-temperature and high-corrosion environments is achieved.
Patent Information
- Application Number
- CN202522615187.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-10
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-12-10
AI Technical Summary
Existing ceramic centrifugal pumps are prone to cracking under clamping forces and have insufficient wear and corrosion resistance. Their performance deteriorates, especially in high and low temperature environments, making them unable to effectively transport high-temperature, highly abrasive corrosive slurries.
The pump cover adopts a steel-lined ceramic structure, with a solid body and a liner inside. The fastening force is dispersed by a fixing ring and a buffer sleeve. Combined with the anti-corrosion layer and the wear-resistant ceramic layer, a multi-layer composite structure is formed to enhance crack resistance and wear resistance.
It significantly improves the crack resistance, wear resistance and corrosion resistance of centrifugal pumps, expands the applicable temperature range, and meets the needs of conveying highly corrosive slurries in the chemical and metallurgical fields.
Smart Images

Figure CN224955947U_ABST
Abstract
Description
Technical Field
[0001] This utility model belongs to the field of anti-corrosion centrifugal pump technology, and in particular relates to a steel-lined ceramic centrifugal pump that is resistant to high temperature, has high wear resistance, is not easy to crack under stress, and can transport corrosive slurries. Background Technology
[0002] A ceramic centrifugal pump is a centrifugal pump used for corrosive slurries. It is mainly used in the chemical and metallurgical industries for conveying corrosive and abrasive slurries, especially for conveying highly corrosive and abrasive slurries with a temperature of around 100℃.
[0003] However, existing ceramic centrifugal pumps generally use a steel-lined ceramic structure, meaning the outer shell of the pump casing is made of metal, while the flow-through components are made of ceramic (such as alumina, silicon carbide, etc.). However, ceramic flow-through components are brittle; even a slight tightening force applied between the pump casing and the pump cover can cause the inner ceramic flow-through components to crack.
[0004] To address the aforementioned shortcomings, industry technicians mixed epoxy resin with silicon carbide particles and cast it to obtain a ceramic centrifugal pump liner that is wear-resistant, acid-resistant, and possesses a certain degree of toughness. When the pump cover and casing are subjected to tightening forces, the ceramic flow-through components of the liner will no longer crack. However, the wear and corrosion resistance of this tough ceramic centrifugal pump liner is often insufficient, especially when used with slurries at 100°C, where the wear resistance of the tough ceramic centrifugal pump drops sharply. Therefore, there is still no suitable corrosion-resistant pump for transporting high-temperature, high-wear-resistance, and highly corrosive slurries, and the steel-lined ceramic structure corrosion-resistant centrifugal pump, which originally had a risk of cracking, must still be used to transport this slurry.
[0005] In addition, in low-temperature regions of -5℃, the pressure inside the pump chamber changes greatly. If the anti-corrosion centrifugal pump with a steel-lined ceramic structure that is prone to cracking continues to be used, the damage rate of the pump and pump cover will be very high.
[0006] Therefore, there is still much room for improvement in existing centrifugal pumps. Utility Model Content
[0007] The purpose of this invention is to overcome the shortcomings of the existing technology and provide a steel-lined ceramic centrifugal pump.
[0008] This steel-lined ceramic centrifugal pump includes a main shaft, bearings, bearing brackets, impeller, shaft seal, pump casing, pump cover, mounting base, and motor. The pump cover is made of metal.
[0009] The pump cover has a solidified body inside its cavity; the solidified body has a liner inside its cavity; the outer ring of the liner has a fixing ring; the fixing ring is pressed between the pump cover and the pump casing; the pump casing, the fixing ring, and the pump cover are tightly sealed to enclose the fluid in the pump cavity; the liner is clamped between the fixing ring and the solidified body; the outer circumference of the liner is smaller than the pressure-bearing surface of the pump cover and the pump casing when subjected to the tightening pressure; the tightening pressure is still borne by the solidified body, thus preventing the liner from cracking due to the tightening pressure.
[0010] Preferably, the retaining ring is fixed to the liner; the retaining ring is a composite of metal and non-metal, or the retaining ring is made of metal, or the retaining ring is made of plastic, including resin.
[0011] As a preferred embodiment: the fixing ring is cast and solidified on the pump casing, and the pump cover, the solidified body and the liner are cast and solidified as a whole to form a combined pump cover; the inner wall of the pump casing is also lined with a layer of wear-resistant ceramic; the fixing ring is a composite of metal and non-metal, or the fixing ring is made of plastic, including resin.
[0012] As a preferred option:
[0013] A buffer sleeve is provided on one side of the suction inlet section of the liner and on the inside of the pump cover to resist the tightening pressure. When the pipeline at the pump cover inlet is fixed, the buffer sleeve can prevent the clamping force / tightening force on the pipeline from acting directly on the pump cover and the liner. The clamping force on the pipeline still acts on the fixed body inside the pump cover cavity, thereby preventing the liner from cracking and being damaged due to the clamping force in the axial direction, and ensuring the overall anti-cracking performance and corrosion and wear resistance of the steel-lined ceramic centrifugal pump.
[0014] The cushioning sleeve is made of plastic, or a mixture of resin and mineral particles.
[0015] As a preferred option:
[0016] An anti-corrosion layer is also provided between the pump cover and the solid body, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer is at least one of the following materials: plastic material or anti-corrosion coating material, the plastic material includes resin material; when the anti-corrosion layer is plastic material, the anti-corrosion layer is lined or coated with plastic in the inner cavity of the pump cover.
[0017] The solidified body is a castable mixture of resin and minerals, which is also filled with metal fibers and / or non-metal fibers; or the solidified body is a mixture of cement and minerals; or the solidified body is made of concrete.
[0018] Preferably, the liner is made of ceramic, metal alloy, concrete, or a mixture of resin and mineral; wherein the ceramic material is silicon carbide or silicon nitride, and the metal alloy is alumina; the metal pump cover and the ceramic liner are wear-resistant and temperature-resistant.
[0019] Preferably, a concave-convex coupling is provided on the contact portion between the pump cover and the solid body, and on the contact portion between the solid body and the outer periphery of the liner suction inlet section, to prevent the liner from rotating and to improve the bonding strength between the liner and the solid body, and between the pump cover and the solid body; the liner is recessed within the metal flange of the pump cover inlet.
[0020] Preferably, the concave-convex coupling is provided only on the contact portion between the outer periphery of the solidified body and the liner intake section.
[0021] Preferably, the steel-lined ceramic centrifugal pump is a horizontal or vertical centrifugal pump.
[0022] As a preferred option, the steel-lined ceramic centrifugal pump is either a front-suction centrifugal pump or a side-suction ceramic centrifugal pump.
[0023] The beneficial effects of this utility model are:
[0024] This invention features a three-layer composite structure consisting of a metal pump cover, a solidified body, and a ceramic liner, which significantly improves the durability and applicability of the centrifugal pump.
[0025] Improved crack resistance: The solidified body (resin / concrete composite material) is located between the pump cover and the liner, concentrating the fastening pressure of the pump casing and pump cover on the pressure-bearing surface. The solidified body bears the mechanical stress, which can prevent the ceramic liner from cracking due to direct stress. The buffer sleeve of the suction section can disperse the axial thrust during pipeline installation and prevent the liner from being damaged by external fastening force.
[0026] Enhanced wear resistance, corrosion resistance, and impact resistance: The inner wall of the pump cover is equipped with an anti-corrosion layer (plastic / resin material) that can resist chemical corrosion; the silicon carbide / silicon nitride ceramic liner provides a wear-resistant flow channel for the pump; the pump casing is also lined with a wear-resistant ceramic layer, and the above three form a layered protective structure; the solidified body is also filled with metal / non-metal fibers, which can improve impact resistance.
[0027] Improved pump structural stability: The addition of a concave-convex coupling body embedded in the contact surface of the pump cover, solid body and liner can prevent the liner from rotating and enhance the bonding force between components; the pump cover, solid body and liner can be cast and solidified into a whole, which can simplify installation and improve sealing performance.
[0028] The application scenarios of the pumps have been expanded: the pumps can withstand a temperature range of -5℃ to 100℃, and can be of various types such as horizontal / vertical, front suction / side suction, etc., to meet the needs of conveying highly corrosive slurries in chemical, metallurgical and other fields. Attached Figure Description
[0029] Figure 1 Cross-sectional views of the horizontal centrifugal pumps in Examples 1 and 2;
[0030] Figure 2These are cross-sectional views of the steel-lined ceramic centrifugal pumps in Examples 3 and 4;
[0031] Figure 3 These are cross-sectional views of the steel-lined ceramic centrifugal pumps in Examples 5 and 6;
[0032] Figure 4 Cross-sectional views of the steel-lined ceramic centrifugal pumps in Examples 7 and 8;
[0033] Figure 5 This is an enlarged schematic diagram of the concave-convex coupling in Examples 7 and 8.
[0034] Explanation of reference numerals in the attached drawings: 1. Pump casing; 2. Pump cover; 3. Impeller; 4. Main shaft; 5. Shaft seal; 6. Bearing bracket; 7. Bearing; 8. Mounting seat; 9. Motor; 10. Anti-corrosion layer; 11. Solid body; 12. Liner; 13. Fixing ring; 14. Pressurized force-bearing surface; 15. Concave-convex coupling; 16. Buffer sleeve; 17. Flange. Detailed Implementation
[0035] The present invention will be further described below with reference to embodiments. The description of the embodiments below is only for the purpose of helping to understand the present invention. It should be noted that, for those skilled in the art, several modifications can be made to the present invention without departing from the principle of the present invention, and these improvements and modifications also fall within the protection scope of the claims of the present invention.
[0036] Example 1
[0037] A horizontal, side-suction, steel-lined ceramic centrifugal pump, such as Figure 1 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0038] The inner cavity of the pump cover 2 is provided with a solid body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solid body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of plastic and is lined with the inner cavity of the pump cover 2.
[0039] The inner cavity of the solidified body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13. The fixing ring 13 is pressed between the pump cover 2 and the pump housing 1. The pump housing, the fixing ring, and the pump cover are tightly sealed to enclose the fluid in the pump cavity. The liner 12 is clamped between the fixing ring 13 and the solidified body 11. The outer circumference of the liner 12 is smaller than the pressing force surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure. The tightening pressure is still borne by the solidified body to prevent the liner from cracking due to the tightening pressure.
[0040] The fixing ring 13 is fixed to the liner 12; the fixing ring 13 is a composite of metal and non-metal.
[0041] The solidified body 11 is a casting mixture of resin and mineral, and the casting mixture is also filled with metal fibers;
[0042] The liner 12 is made of silicon carbide ceramic; the metal pump cover and the ceramic liner are wear-resistant and temperature-resistant.
[0043] Among them, the main shaft 4, bearing bracket 6, shaft seal 5 and mounting base 8 are all processed by conventional machining methods or directly purchased; the pump casing 1 adopts a steel-lined ceramic structure.
[0044] Impeller 3 is made of silicon carbide ceramic material;
[0045] The manufacturing method and process of pump cover 2 are as follows: First, the metal pump cover is machined according to the drawing. Then, a 3-5 mm thick polyethylene fixing ring 13 is coated on the inner side of the metal pump cover using a plastic coating process. Next, the silicon carbide liner 12 is fixed to the inner anti-corrosion layer 10 of the metal pump cover using a resin and mineral casting mixture. The fixing ring 13 is made of polypropylene by injection molding and fixed on the liner 12 to form an integral pump cover. The area of the pump cover with high wear resistance requirements at the suction inlet is lined with silicon carbide wear-resistant material. All parts involving fluid entry are provided with anti-corrosion layer 10. There is no ceramic body in the force-bearing parts where the pump casing 1 and pump cover 2 are fastened. This pump cover is wear-resistant, corrosion-resistant and pressure-resistant.
[0046] In this embodiment, the steel-lined ceramic centrifugal pump is installed as follows: First, the bearing bracket 6, main shaft 4, bearing 7, etc. are assembled into a transmission assembly. Then, the shaft seal 5, pump casing 1, impeller 3, and pump cover 2 are assembled onto the transmission assembly in sequence to obtain the pump head. Then, the pump head, mounting base 8, and motor 9 are assembled together. After debugging, painting, and packaging, the steel-lined ceramic centrifugal pump of this embodiment, which can transport corrosive slurries, is obtained. This steel-lined ceramic centrifugal pump can withstand high temperatures, has high wear resistance, and is not easy to crack under stress.
[0047] Example 2
[0048] A horizontal, side-suction, steel-lined ceramic centrifugal pump, such as Figure 1 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0049] The inner cavity of the pump cover 2 is provided with a solid body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solid body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of plastic and is lined with the inner cavity of the pump cover 2; the inner cavity of the solid body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13, which is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to seal the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solid body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure, so that the tightening pressure is still borne by the solid body, and the liner is prevented from cracking due to the tightening pressure;
[0050] The fixing ring 13 is cast and solidified on the pump casing 1. The pump cover 2, the solidified body 11 and the liner 12 are cast and solidified as a whole to form a combined pump cover. The inner wall of the pump casing 1 is also lined with a layer of wear-resistant ceramic. The fixing ring 13 is made of polyethylene.
[0051] The solidified body 11 is a casting mixture of resin and mineral, and the casting mixture is also filled with non-metallic fibers.
[0052] Liner 12 is made of silicon carbide.
[0053] Example 3
[0054] A vertical steel-lined ceramic centrifugal pump, such as Figure 2 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0055] The pump cover 2 has a solidified body 11 in its inner cavity; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of resin; the solidified body 11 has a liner 12 in its inner cavity, and a fixing ring 13 is provided on the outer ring of the liner 12. The fixing ring 13 is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to enclose the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure. The tightening pressure is still borne by the solidified body to prevent the liner from cracking due to the tightening pressure; the solidified body 11 is a mixture of cement and minerals; the liner 12 is made of silicon nitride ceramic;
[0056] The fixing ring 13 is fixed to the liner 12; the fixing ring 13 is made of plastic.
[0057] A concave-convex coupling 15 is provided on the contact portion between the outer periphery of the consolidation body 11 and the suction inlet section of the liner 12.
[0058] Example 4
[0059] A vertical steel-lined ceramic centrifugal pump, such as Figure 2 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0060] The pump cover 2 has a solidified body 11 in its inner cavity; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of anti-corrosion coating material; the solidified body 11 has a liner 12 in its inner cavity, and a fixing ring 13 is provided on the outer ring of the liner 12. The fixing ring 13 is pressed between the pump cover 2 and the pump casing 1, and the pump casing, the fixing ring, and the pump cover are tightly sealed to seal the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump casing 1 when subjected to the tightening pressure. The tightening pressure is still borne by the solidified body to prevent the liner from cracking due to the tightening pressure; the solidified body 11 is made of concrete.
[0061] The fixing ring 13 is cast and solidified on the pump casing 1. The pump cover 2, the solidified body 11 and the liner 12 are cast and solidified as a whole to form a combined pump cover. The inner wall of the pump casing 1 is also lined with a layer of wear-resistant ceramic. The fixing ring 13 is made of resin. The liner 12 is made of alumina.
[0062] A concave-convex coupling 15 is provided on the contact portion between the outer periphery of the consolidation body 11 and the suction inlet section of the liner 12.
[0063] Example 5
[0064] A horizontal steel-lined ceramic centrifugal pump, such as Figure 3 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0065] The inner cavity of the pump cover 2 is provided with a solidified body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of plastic and is lined with the inner cavity of the pump cover 2; the inner cavity of the solidified body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13, which is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to seal the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure, so that the tightening pressure is still borne by the solidified body, and the liner is prevented from cracking due to the tightening pressure; the solidified body 11 is a cast mixture of resin and mineral, and the cast mixture is also filled with metal fibers.
[0066] The fixing ring 13 is fixed to the liner 12. The fixing ring 13 is a composite of metal and non-metal.
[0067] The tightening force of the pipeline can easily generate axial pushing pressure on the ceramic liner of the pump cover, causing the ceramic to crack. By shortening the length of the liner, the liner is recessed inside the pump cover, and a buffer sleeve is installed on the anti-corrosion layer of the shortened part. Specifically, a buffer sleeve 16 is provided on the suction section side of the liner 12 and the inner side of the pump cover 2 to resist tightening pressure. When the pipeline at the pump cover inlet is fixed, the buffer sleeve can prevent the clamping force / tightening force on the pipeline from acting directly on the pump cover and the liner. The clamping force on the pipeline still acts on the fixed body inside the pump cover cavity, thereby preventing the liner from cracking and being damaged due to the axial clamping force, and ensuring the overall anti-cracking performance and anti-corrosion and wear-resistant performance of the steel-lined ceramic centrifugal pump. The buffer sleeve 16 is made of plastic; the liner 12 is made of silicon carbide ceramic.
[0068] A concave-convex coupling 15 is provided on the contact portion between the outer periphery of the consolidation body 11 and the suction inlet section of the liner 12.
[0069] Example 6
[0070] A horizontal steel-lined ceramic centrifugal pump, such as Figure 3 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0071] The inner cavity of the pump cover 2 is provided with a solidified body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of anti-corrosion coating material; the inner cavity of the solidified body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13, which is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to seal the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure, so that the tightening pressure is still borne by the solidified body, and the liner is prevented from cracking due to the tightening pressure; the solidified body 11 is a cast mixture of resin and mineral, and the cast mixture is also filled with non-metallic fibers.
[0072] The fixing ring 13 is cast and solidified on the pump casing 1. The pump cover 2, the solidified body 11 and the liner 12 are cast and solidified as a whole to form a combined pump cover. The inner wall of the pump casing 1 is also lined with a layer of wear-resistant ceramic. The fixing ring 13 is made of plastic. The liner 12 is made of silicon nitride ceramic.
[0073] The tightening force of the pipeline can easily generate axial pushing pressure on the ceramic liner of the pump cover, causing the ceramic to crack. By shortening the length of the liner, the liner is recessed inside the pump cover, and a buffer sleeve is installed on the anti-corrosion layer of the shortened part. That is, a buffer sleeve 16 is provided on the suction section side of the liner 12 and the inner side of the pump cover 2 to resist tightening pressure. When the pipeline at the pump cover inlet is fixed, the buffer sleeve can prevent the clamping force / tightening force on the pipeline from acting directly on the pump cover and the liner. The clamping force on the pipeline still acts on the fixed body inside the pump cover cavity, thereby preventing the liner from cracking and being damaged due to the clamping force in the axial direction, and ensuring the overall anti-cracking performance and anti-corrosion and wear-resistant performance of the steel-lined ceramic centrifugal pump. The buffer sleeve 16 is a mixture of resin and mineral particles.
[0074] A concave-convex coupling 15 is provided on the contact portion between the outer periphery of the consolidation body 11 and the suction inlet section of the liner 12.
[0075] Example 7
[0076] A vertical steel-lined ceramic centrifugal pump, such as Figure 4 As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0077] The inner cavity of the pump cover 2 is provided with a solidified body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of resin; the inner cavity of the solidified body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13, which is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to enclose the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure, so that the tightening pressure is still borne by the solidified body, and the liner is prevented from cracking due to the tightening pressure; the solidified body 11 is a mixture of cement and minerals;
[0078] The fixing ring 13 is fixed to the liner 12; the fixing ring 13 is made of metal.
[0079] like Figure 5 As shown, a concave-convex coupling body 15 is provided on the contact portion between the pump cover 2 and the solid body 11, and on the contact portion between the outer periphery of the solid body 11 and the suction section of the liner 12, to prevent the liner from rotating and to improve the bonding strength between the liner and the solid body, and between the pump cover and the solid body; the liner 12 is recessed within the metal flange 17 at the inlet of the pump cover 2; the liner 12 is made of alumina.
[0080] Example 8
[0081] A vertical steel-lined ceramic centrifugal pump, such as Figure 4As shown, it includes a main shaft 4, a bearing 7, a bearing bracket 6, an impeller 3, a shaft seal 5, a pump casing 1, a pump cover 2, a mounting base 8, and a motor 9. The pump cover 2 is made of metal.
[0082] The inner cavity of the pump cover 2 is provided with a solidified body 11; an anti-corrosion layer 10 is also provided between the pump cover 2 and the solidified body 11, that is, an anti-corrosion layer is provided on all contact surfaces of the metal pump cover and the conveyed slurry; the anti-corrosion layer 10 is made of plastic and is coated on the inner cavity of the pump cover 2; the inner cavity of the solidified body 11 is provided with a liner 12, and the outer ring of the liner 12 is provided with a fixing ring 13, which is pressed between the pump cover 2 and the pump housing 1, and the pump housing, the fixing ring, and the pump cover are tightly sealed to seal the fluid in the pump cavity; the liner 12 is clamped between the fixing ring 13 and the solidified body 11, and the outer circumference of the liner 12 is smaller than the pressure-bearing surface 14 of the pump cover 2 and the pump housing 1 when subjected to the tightening pressure, so that the tightening pressure is still borne by the solidified body, and the liner is prevented from cracking due to the tightening pressure; the solidified body 11 is a cast mixture of resin and mineral, and the cast mixture is also filled with metal fibers.
[0083] The fixing ring 13 is cast and solidified on the pump casing 1. The pump cover 2, the solidified body 11 and the liner 12 are cast and solidified as a whole to form a combined pump cover. The inner wall of the pump casing 1 is also lined with a layer of wear-resistant ceramic. The fixing ring 13 is made of resin. The liner 12 is made of concrete.
[0084] like Figure 5 As shown, a concave-convex coupling body 15 is provided on the contact portion between the pump cover 2 and the solid body 11, and on the contact portion between the outer periphery of the solid body 11 and the suction section of the liner 12, to prevent the liner from rotating and to improve the bonding strength between the liner and the solid body, and between the pump cover and the solid body; the liner 12 is recessed within the metal flange 17 at the inlet of the pump cover 2.
Claims
1. A steel-lined ceramic centrifugal pump, comprising a main shaft (4), bearings (7), bearing brackets (6), impellers (3), shaft seals (5), pump casing (1), pump cover (2), mounting base (8), and motor (9), characterized in that: The pump cover (2) is made of metal; The inner cavity of the pump cover (2) is provided with a solid body (11); the inner cavity of the solid body (11) is provided with a liner (12), and the outer ring of the liner (12) is provided with a fixing ring (13), which is pressed between the pump cover (2) and the pump housing (1); the liner (12) is clamped between the fixing ring (13) and the solid body (11), and the outer circumference of the liner (12) is smaller than the pressing force surface (14) of the pump cover (2) and the pump housing (1) when subjected to the fastening pressure.
2. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: The fixing ring (13) is fixed on the liner (12); the fixing ring (13) is a composite of metal and non-metal, or the fixing ring (13) is made of metal, or the fixing ring (13) is made of plastic, and the plastic material includes resin material.
3. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: The fixing ring (13) is cast and solidified on the pump housing (1), and the pump cover (2), the solidified body (11) and the liner (12) are cast and solidified as one piece; the inner wall of the pump housing (1) is also lined with a layer of wear-resistant ceramic. The fixing ring (13) is a composite of metal and non-metal, or the fixing ring (13) is made of plastic, including resin.
4. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: A buffer sleeve (16) is provided on one side of the suction port section of the liner (12) and on the inner side of the pump cover (2). The buffer sleeve (16) is made of plastic, or the buffer sleeve (16) is a mixture of resin and mineral particles.
5. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: A corrosion-resistant layer (10) is also provided between the pump cover (2) and the solid body (11); the corrosion-resistant layer (10) is at least one of the following materials: plastic material or corrosion-resistant coating material, wherein the plastic material includes resin material; when the corrosion-resistant layer (10) is plastic material, the corrosion-resistant layer (10) is lined or coated with plastic in the inner cavity of the pump cover (2); The solidified body (11) is a castable mixture of resin and mineral, and the castable mixture is also filled with metal fibers and / or non-metal fibers; or the solidified body (11) is a mixture of cement and mineral; or the solidified body (11) is made of concrete.
6. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: The liner (12) is made of ceramic, metal alloy, concrete or a mixture of resin and mineral; wherein the ceramic material is silicon carbide or silicon nitride and the metal alloy is alumina.
7. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: On the contact portion between the pump cover (2) and the solid body (11), and on the contact portion between the solid body (11) and the outer periphery of the suction inlet section of the liner (12), there is also a concave-convex coupling body (15); the liner (12) is recessed inside the flange (17) of the inlet portion of the pump cover (2).
8. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: An uneven coupling body (15) is provided only on the contact portion between the outer periphery of the consolidation body (11) and the inlet section of the liner (12).
9. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: The steel-lined ceramic centrifugal pump is either a horizontal or vertical centrifugal pump.
10. The steel-lined ceramic centrifugal pump according to claim 1, characterized in that: The steel-lined ceramic centrifugal pump is either a front-suction centrifugal pump or a side-suction ceramic centrifugal pump.