A large-size chain pin-sleeve pair with a composite texture and coating
By designing a specific groove-shaped microtexture on the pin surface and covering it with a friction-reducing and wear-resistant coating, the lubrication and wear resistance problems of large-size chain pin-sleeve pairs under high load and long service conditions are solved, achieving a synergistic effect of stable lubrication and wear resistance.
Patent Information
- Application Number
- CN202522511796.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-26
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-11-26
AI Technical Summary
In existing technologies, in the pin and sleeve pairs of large-scale transmission chains, a single micro-texture or friction-reducing coating cannot simultaneously guarantee lubrication durability and wear resistance under high load and long service life conditions, and the process sequence affects the continuity and bonding strength of the coating.
By employing a composite structure of microtexture with specific geometric parameters and friction-reducing and wear-resistant coating, groove-shaped microtexture is first machined on the pin surface, and then covered with friction-reducing and wear-resistant coating to ensure stable supply of lubricating oil and optimization of oil film, and to provide low friction and high wear resistance protection through the coating.
It achieves stable lubrication and wear resistance throughout the entire operating cycle, improving the reliability and service life of chain drives, and exhibiting excellent tribological properties, especially in low-speed heavy loads and harsh environments.
Smart Images

Figure CN224956185U_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the technical field of lubrication and wear-resistant structure of mechanical transmission components, specifically relating to a large-size chain pin-sleeve pair with a composite texture and coating. Background Technology
[0002] Large-scale transmission chains generally employ high-strength, high-reliability roller chains. Operating under harsh conditions of low speed and heavy load, these chains place extremely high demands on the wear resistance and reliability of the core friction pair—the pins and bushings. Surface engineering technology is an effective means to improve their tribological properties. Currently, friction-reducing and lubrication-enhancing surface technologies have mainly formed two branches: one is processing microtextures on the surface of parts to improve lubrication; the other is applying friction-reducing and wear-resistant coatings to the surface of parts to enhance surface properties. Both have been applied in multiple fields.
[0003] However, the aforementioned existing technical solutions all have limitations. Relying solely on microtexturing to optimize the lubricating oil film fails to improve the intrinsic wear resistance of the material; or they focus only on coating materials and processes, neglecting the active regulatory role of microtexturing on the lubrication state. Even in composite technologies combining texture and coating, the choice of process path profoundly affects the final surface performance. Using a process path of coating first and then texturing, the texturing process can damage the pre-prepared complete coating, potentially affecting not only the continuity of the coating but also directly limiting the geometric depth of the texture to the initial coating thickness. This inherent characteristic resulting from the process sequence means that the lubrication durability and wear resistance reliability of such composite surfaces still face challenges when dealing with demanding conditions requiring high loads and long service lives.
[0004] In actual chain operation, the lubrication state of the pin-sleeve pair changes dynamically with operating conditions. While single anti-friction coatings, such as MGC or phosphating films, can effectively reduce the coefficient of friction and increase hardness, their surfaces are often too smooth and flat, hindering the capture and retention of lubricating oil. This is especially true during startup or when oil supply is insufficient, resulting in poor lubrication and preventing the coating from achieving its optimal performance. Furthermore, the wear debris generated after coating wear can adversely affect subsequent operations. On the other hand, while a single microtexture design can optimize oil film formation through oil storage and diversion functions, under extreme loads or boundary lubrication conditions caused by lubrication failure, the microtexture itself cannot compensate for the insufficient wear resistance of the base material. Its edges easily become wear origins and may even lead to stress concentration, accelerating material failure. Therefore, a composite technology combining surface texture and anti-friction coatings is considered an ideal way to address these challenges. Its core objective is to ensure a stable supply of lubricating oil and optimized oil film through texture, while utilizing the coating to provide an inherent low-friction and high-wear-resistance barrier, thereby achieving a synergistic effect of long-term lubrication and durable wear resistance. Utility Model Content
[0005] To address the problems of existing technologies, this invention discloses a large-size chain pin-sleeve pair that combines a textured structure with a coating. By combining the lubricating oil guiding and storage function of the micro-texture with the inherent friction-reducing and wear-resistant properties of the coating material, the oil film can be stably maintained and friction and wear reduced throughout the entire operating cycle. This significantly improves the transmission reliability and service life of large-size chains in low-speed, heavy-load, and harsh environments.
[0006] To achieve the above objectives, the technical solution of this utility model is as follows: A large-size chain pin-sleeve assembly combining texture and coating includes a sleeve fitted around the pin, wherein the inner wall of the sleeve is clearance-fitted with the outer wall of the pin, and the pin surface is uniformly machined with a plurality of parallel groove-shaped micro-textures, the pin surface covering the groove-shaped micro-textures is coated with a friction-reducing and wear-resistant coating, wherein the width of the groove-shaped micro-textures is 0.8~1.2 mm, the depth is 0.4~0.6 mm, and the center-to-center distance between adjacent textures is 2.5~3.5 mm.
[0007] Preferably, the grooved microtexture is a straight grooved microtexture, which is arranged along the axial direction of the pin and evenly distributed around the pin axis.
[0008] Preferably, the surface area of the straight groove microtexture accounts for 25% to 30% of the total surface area of the pin.
[0009] Preferably, the friction-reducing and wear-resistant coating is an MGC coating or a phosphate film.
[0010] Preferably, the thickness of the MGC coating is 15~30μm, and the thickness of the phosphating film is 5~20μm.
[0011] Preferably, the part where the pin mates with the sleeve is formed by expanding the diameter to create an expanded section, and a straight groove microtexture and a friction-reducing and wear-resistant coating are provided on the surface of the expanded section.
[0012] The beneficial effects of this novel large-size chain pin-sleeve pair, which combines texture and coating, are as follows: (1) The straight groove microtexture designed on the surface of the pin shaft in this novel design, with its specific combination of width, spacing and area ratio, can efficiently guide the lubricating oil to flow along the axial direction and promote its uniform distribution in the contact area. This not only enhances the oil film formation ability and load-bearing performance, but also effectively improves the continuity of lubrication, especially under harsh working conditions such as start-up or insufficient oil supply; (2) The present invention first processes a straight groove microtexture with specific geometric parameters on the surface of the chain pin, and then prepares a friction-reducing and wear-resistant coating on the basis of the microtexture, thereby constructing a pin-sleeve pair with composite texture and coating functions, so that it has both the lubrication guiding function of the microtexture and the surface strengthening function of the coating, and can still maintain excellent tribological properties under insufficient lubrication or extreme load conditions. Attached Figure Description
[0013] Figure 1 This is a schematic diagram of the structure of the novel microtextured-coated composite pin-sleeve pair.
[0014] Figure 2 This is a schematic diagram of a pin-shaped microtexture structure with a width of 1 mm, a depth of 0.5 mm, and an area ratio of 27%.
[0015] Figure 3 This is a schematic diagram of the coating structure of the pin shaft.
[0016] Reference numerals: 1-pin, 2-sleeve, 3-straight groove microtexture, 4-friction-reducing and wear-resistant coating, 5-expanded diameter section. Detailed Implementation
[0017] The following description is merely a preferred embodiment of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
[0018] The following embodiments can be understood as a part of the local structure or method of the present invention, or as a combination of embodiments to explain the connotation of a larger range of structures or methods of the present invention.
[0019] Example 1: A large-size chain pin-sleeve assembly combining texture and coating, reference Figure 1-3 As shown, it includes a sleeve 2 fitted outside the pin 1. The inner wall of the sleeve 2 is clearance-fitted with the outer wall of the pin 1. The surface of the pin 1 is uniformly machined with several parallel groove-shaped micro-textures. The pin surface covering the groove-shaped micro-textures is provided with a friction-reducing and wear-resistant coating 4. The width of the groove-shaped micro-textures is 0.8 mm, the depth is 0.4 mm, and the center-to-center distance between adjacent textures is 2.5 mm.
[0020] In this embodiment, the groove microtexture can be a straight groove, a spiral, or a groove structure of other shapes.
[0021] Example 2: Unlike Example 1, a large-size chain pin-sleeve assembly combining texture and coating is described, as referenced. Figure 1-3 As shown, it includes a sleeve 2 fitted outside the pin 1. The inner wall of the sleeve 2 is clearance-fitted with the outer wall of the pin 1. The surface of the pin 1 is uniformly machined with several parallel groove-shaped micro-textures. The pin surface covering the groove-shaped micro-textures is provided with a friction-reducing and wear-resistant coating 4. The width of the groove-shaped micro-textures is 1.2 mm, the depth is 0.6 mm, and the center-to-center distance between adjacent textures is 3.5 mm.
[0022] Example 3: like Figure 1-3 As shown, the groove-shaped microtexture is a straight groove-shaped microtexture 3, which is arranged along the axial direction of the pin 1 and evenly distributed around the axis of the pin 1.
[0023] Example 4: like Figure 1-3 As shown, the surface area of the straight groove microtexture 3 accounts for 25% of the total surface area of the pin 1.
[0024] The friction-reducing and wear-resistant coating is an MGC coating.
[0025] Example 5: like Figure 1-3 As shown, the surface area of the straight groove microtexture 3 accounts for 30% of the total surface area of the pin shaft.
[0026] The friction-reducing and wear-resistant coating is a phosphate film.
[0027] Example 6: like Figure 1-3 As shown, the thickness of the MGC coating is 15 μm, and the thickness of the phosphating film is 5 μm.
[0028] Example 7: like Figure 1-3 As shown, the thickness of the MGC coating is 30 μm, and the thickness of the phosphating film is 20 μm.
[0029] Example 8: like Figure 1 , 2 As shown, the part where the pin 1 and the sleeve 2 mate is formed by expanding the diameter to form an expanded diameter section 5, and a straight groove micro-texture 3 and a friction-reducing and wear-resistant coating 4 are provided on the surface of the expanded diameter section 5.
[0030] The working principle of this new type: For the special working conditions of large-size chain pin-sleeve pairs, a process path of first weaving and then coating is adopted. First, a deep-scale straight groove-like micro-texture, which is not constrained by thickness, is machined on the pin substrate. Then, a functional anti-friction coating is applied over the entire structure. This design guides lubrication through geometric texture and provides comprehensive anti-friction protection through a complete coating. It not only ensures the continuity and bonding strength of the coating, but also achieves greater lubricant reserve and wear tolerance through deep texture. This effectively solves the problems of lubrication retention and premature coating failure in existing technologies under high load and long service conditions, significantly improving the long-term reliability of chain drives.
[0031] In the specific processing, a texture is first machined onto the pin substrate. Its depth, shape, and other geometric parameters are independently designed, unaffected by the thickness of subsequent coatings, providing conditions for achieving large-capacity oil storage and optimizing hydrodynamic effects. Subsequently, a functional anti-friction coating is completely applied to the texture surface, completely avoiding damage from subsequent textures while ensuring a strong bond between the texture and coating, guaranteeing the coating's bonding strength. This composite structure exhibits adaptive characteristics throughout its entire life cycle. The anti-friction and wear-resistant coating effectively synergizes with the micro-texture during the break-in period, jointly mitigating severe wear of the chain under extreme operating conditions during this phase. During the stable period, the lubricating oil within the texture grooves effectively captures and removes wear debris from the coating and workpiece, preventing its adverse effects and ensuring the long service life of the components.
[0032] In practical use, after mounting rollers on the outside of the sleeve, the pin-sleeve pair is connected by a chain plate to form a large-scale chain transmission unit. During chain operation, the transmission system supplies oil to the contact interface between the pin and the sleeve under a certain pressure through preset lubricating oil nozzles. After the lubricating oil enters the straight groove microtexture on the pin surface, it is intercepted by the groove structure and flows along the axial direction. As the pin rotates, the oil in the groove migrates to the edge of the friction interface under pressure, forming a continuous lubricating oil film, thereby reducing frictional resistance.
[0033] After the microtexture is fabricated on the pin surface, a friction-reducing and wear-resistant coating, either MGC or a phosphating film, is further deposited. The coating completely covers the outer surface of the pin, forming a continuous and dense film on the walls and bottom of the microtextured grooves and in the untextured areas, achieving overall friction reduction and wear resistance protection. During chain engagement, relative sliding occurs between the pin and the sleeve, and the lubricating oil is periodically squeezed and released within the grooves, achieving dynamic replenishment of the lubricating oil. The straight groove microtexture acts as an oil reservoir and guide, while the coating provides a low-friction contact interface, ensuring stable lubrication of the pin-sleeve pair under low-speed, heavy-load conditions.
[0034] When the chain drive system operates intermittently or has insufficient lubrication, the residual lubricating oil in the groove can be released under vibration, maintaining boundary lubrication. After long-term operation, the coating remains intact, the wear on the pin surface is significantly reduced, and the smoothness of the chain drive is improved.
[0035] This novel microtextured-coated composite pin-sleeve pair structure is not only suitable for large-scale chain systems, but can also be widely applied to sliding friction pairs such as internal combustion engine cylinder liners, sliding bearings, cam-follower mechanisms, and hydraulic actuators, and has broad industrial application prospects.
Claims
1. A large-size chain pin-sleeve assembly combining texture and coating, comprising a sleeve fitted around the pin, wherein the inner wall of the sleeve and the outer wall of the pin are clearance-fitted, characterized in that: The pin shaft surface is uniformly machined with several parallel groove-shaped micro-textures. The pin shaft surface covering the groove-shaped micro-textures is coated with a friction-reducing and wear-resistant coating. The width of the groove-shaped micro-textures is 0.8~1.2 mm, the depth is 0.4~0.6 mm, and the center-to-center distance between adjacent textures is 2.5~3.5 mm.
2. The large-size chain pin-sleeve assembly with textured and coated composite structure as described in claim 1, characterized in that: The grooved microtexture is a straight grooved microtexture, which is arranged along the axial direction of the pin and evenly distributed around the pin axis.
3. The large-size chain pin-sleeve assembly with textured and coated composite structure as described in claim 2, characterized in that: The surface area of the straight groove microtexture accounts for 25% to 30% of the total surface area of the pin.
4. A large-size chain pin-sleeve assembly combining texture and coating as described in claim 1, 2, or 3, characterized in that: The friction-reducing and wear-resistant coating is an MGC coating or a phosphate film.
5. A large-size chain pin-sleeve assembly combining texture and coating as described in claim 4, characterized in that, The thickness of the MGC coating is 15~30μm, and the thickness of the phosphating film is 5~20μm.
6. A large-size chain pin-sleeve assembly combining texture and coating as described in claim 1, characterized in that, The part where the pin and the sleeve mate is formed by expanding the diameter to create an expanded section, and a straight groove micro-texture and a friction-reducing and wear-resistant coating are provided on the surface of the expanded section.