A bimetallic wear-resistant liner and its plateless casting device

The use of a non-partitioned casting device for bimetallic wear-resistant liners has solved the problem of short service life of wear-resistant liners, achieving a combination of high efficiency, long service life, wear resistance, and toughness, and reducing operation and maintenance costs and equipment downtime.

CN224977439UActive Publication Date: 2026-11-17TANGSHAN CERAMIC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522506747.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-26
Publication Date
2026-11-17
Estimated Expiration
2035-11-26

AI Technical Summary

Technical Problem

Existing wear-resistant liners have a short service life in wet mills, and frequent replacements lead to high labor intensity, long equipment downtime, and high maintenance costs. The insufficient toughness of high-chromium cast iron limits its application under high-impact conditions.

Method used

A plateless casting device using bimetallic wear-resistant liners achieves composite molding of high-chromium cast iron and carbon steel by optimizing the structural and process parameters of the cast iron and carbon steel casting systems. The bonding surface is reasonably designed, and the ratio of wear-resistant layer to toughness layer is appropriate.

Benefits of technology

It significantly extends the service life of the liner, reduces operation and maintenance costs, and improves the working efficiency and economic benefits of the equipment in corrosive mineral slurry environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224977439U_ABST
    Figure CN224977439U_ABST
Patent Text Reader

Abstract

This utility model relates to the field of bimetallic composite casting technology, and in particular to a bimetallic wear-resistant liner and its diaphragmless casting device, to alleviate the problem of imbalance between hardness and toughness in conventional liners. The device includes a molding cavity, a cast iron casting system, and a carbon steel casting system; the cast iron casting system and the carbon steel casting system are respectively located on both sides of the molding cavity; the cast iron casting system is connected to the side of the molding cavity through a first ingate and to the bottom of the molding cavity through a first bottom gate; the carbon steel casting system is connected to the side of the molding cavity through a second ingate; the horizontal height of the second ingate is higher than that of the first ingate. The horizontal sand mold diaphragmless sequential casting method achieves good metallurgical bonding between the two metal layers. Compared with traditional high-manganese steel liners and single-metal liners, the service life is significantly extended under the same working conditions, and the manufacturing process is simple, the performance is stable and reliable, and it has good manufacturability and low overall cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of bimetallic composite casting technology, and in particular to a bimetallic wear-resistant liner and its diaphragmless casting device. Background Technology

[0002] Wear-resistant liners are critical and vulnerable components in ball mills used in the mineral processing industry. During the operation of wet mills, the liners are constantly exposed to a corrosive slurry environment and subjected to intense impacts and abrasion from the materials and grinding balls, leading to a combination of wear forms, including shear wear, impact wear, fatigue wear, abrasive wear, and chemical corrosion. Therefore, liners are a vital consumable in ore processing, directly impacting production cost control. Currently, the widely used high-manganese steel and alloy steel liners generally suffer from short service life, typically less than seven months on average. Frequent liner replacements not only increase the workload of workers but also prolong equipment downtime, complicate maintenance procedures, and waste significant human, material, and financial resources, severely hindering production efficiency and the improvement of enterprise economic benefits.

[0003] High-chromium cast iron, as an excellent wear-resistant material, is particularly suitable for wet abrasive wear conditions due to its metallographic structure and performance characteristics. However, high-chromium cast iron, which is mainly composed of eutectic structures, often exhibits poor performance in terms of strength and toughness, making it difficult to simultaneously meet the requirements of high hardness and high toughness. Therefore, developing a liner material that possesses both excellent wear resistance and good impact toughness is an urgent practical need and has significant application value. Utility Model Content

[0004] To alleviate the above-mentioned technical problems, the technical solution provided by this utility model is as follows:

[0005] This utility model provides a plateless casting device for bimetallic wear-resistant liners, including a molding cavity, a cast iron casting system and a carbon steel casting system;

[0006] The cast iron gating system and the carbon steel gating system are respectively located on both sides of the forming cavity;

[0007] The cast iron gating system is connected to the side of the forming cavity through the first ingate and to the bottom of the forming cavity through the first bottom gate;

[0008] The carbon steel gating system is connected to the side of the forming cavity through the second ingate;

[0009] The second ingate is at a higher level than the first ingate.

[0010] Furthermore,

[0011] The cast iron gating system includes a cast iron gate, a first straight runner, and a first cross runner;

[0012] The cast iron gate is located at the top of the first straight-flow runner.

[0013] The first crossflow channel is located in the middle of the first direct flow channel and is connected to it;

[0014] The first cross runner is connected to multiple first ingates;

[0015] The lower part of the first sprue is connected to the first straight channel.

[0016] Furthermore, the carbon steel gating system includes a carbon steel gate, a second straight runner, and a second cross runner;

[0017] The middle part of the second crossflow channel and the second direct flow channel, and connected to them;

[0018] The second cross runner is connected to multiple second ingates.

[0019] Furthermore, the molding cavity is provided with a first overflow groove and a second overflow groove;

[0020] The first overflow groove is located at the upper part of the first crossflow channel and is connected to the molding cavity;

[0021] The second overflow channel is located at the lower part of the second cross channel and is connected to the molding cavity.

[0022] Furthermore, the upper parts of the first overflow trough and the second overflow trough are respectively provided with multiple vent holes.

[0023] Furthermore, multiple temperature measuring couplers are respectively inserted into the first overflow tank and the second overflow tank.

[0024] Furthermore, a feeding riser is provided at the top of the molding cavity.

[0025] Furthermore, ceramic filter plates are provided in the first ingate, the sprue, and the second ingate.

[0026] A bimetallic wear-resistant liner is cast using the aforementioned plateless casting device, comprising a wear-resistant layer and a toughness layer; the thickness of the wear-resistant layer accounts for 40%-55% of the total thickness; the thickness of the toughness layer accounts for 45%-60% of the total thickness; and the bonding surfaces of the wear-resistant layer and the toughness layer are parallel to each other.

[0027] The beneficial effects of this utility model are analyzed as follows:

[0028] This device includes a molding cavity, a cast iron gating system, and a carbon steel gating system; the cast iron gating system and the carbon steel gating system are respectively located on both sides of the molding cavity; the cast iron gating system is connected to the side of the molding cavity through a first ingate and to the bottom of the molding cavity through a first bottom gating system; the carbon steel gating system is connected to the side of the molding cavity through a second ingate; the horizontal height of the second ingate is higher than that of the first ingate.

[0029] The method of sequentially pouring molten metal into the cast iron gating system and the carbon steel gating system using a horizontal sand mold without partitions achieves a good metallurgical bond between the two metal layers. Compared with traditional high manganese steel liners and single metal liners, the service life is significantly extended under the same working conditions. In addition, the liner structure is reasonably designed, the manufacturing process is simple, the performance is stable and reliable, and it has good manufacturability and low overall cost. Attached Figure Description

[0030] To more clearly illustrate the technical solutions in the specific embodiments or related technologies of this utility model, the drawings used in the description of the specific embodiments or related technologies will be briefly introduced below. Obviously, the drawings described below are some embodiments of this utility model. For those skilled in the art, other drawings can be obtained from these drawings without creative effort.

[0031] Figure 1 A schematic diagram of the sand mold cross-section of the plateless casting device provided for an embodiment of this utility model;

[0032] Figure 2 A schematic diagram of the gating structure of the diaphragmless casting device provided for an embodiment of this utility model;

[0033] Figure 3 This is a flowchart of the forming process for bimetallic wear-resistant liners.

[0034] Figure 4 This is a schematic diagram of a cross-section of a bimetallic wear-resistant liner.

[0035] icon:

[0036] 100 - Molding cavity; 110 - First overflow groove; 120 - Second overflow groove; 130 - Thermocouple; 140 - Feeding riser;

[0037] 200 - Cast iron gating system; 210 - First inch gate; 220 - First sprue; 230 - Cast iron gate; 240 - First straight runner; 250 - First cross runner;

[0038] 300 - Carbon steel gating system; 320 - Carbon steel gate; 330 - Second straight runner; 340 - Second cross runner;

[0039] 400 - Wear-resistant layer;

[0040] 500 - Toughness layer. Detailed Implementation

[0041] In ball mills used in the mineral processing industry, wear-resistant liners are key vulnerable components that are constantly exposed to corrosive slurry environments and continuously subjected to multiple combined losses, including strong impacts, shearing, fatigue, and abrasive wear from the materials and grinding balls, resulting in a generally short service life.

[0042] Currently, the widely used high-manganese steel and alloy steel liners are difficult to meet the production requirements of high efficiency and long service life. Frequent replacements not only increase labor intensity, but also cause prolonged equipment downtime and increased maintenance costs. Although high-chromium cast iron has excellent wear resistance and microstructure suitable for wet abrasive wear conditions, its insufficient toughness limits its application under high impact conditions.

[0043] In view of this, such as Figures 1 to 4 As shown, this solution provides a diaphragmless casting device for bimetallic wear-resistant liners to alleviate the above-mentioned problems.

[0044] This device includes a molding cavity 100, a cast iron gating system 200, and a carbon steel gating system 300; the cast iron gating system 200 and the carbon steel gating system 300 are respectively disposed on both sides of the molding cavity 100; the cast iron gating system 200 is connected to the side of the molding cavity 100 through a first ingate 210 and to the bottom of the molding cavity 100 through a first bottom gating system 220; the carbon steel gating system 300 is connected to the side of the molding cavity 100 through a second ingate 310; the horizontal height of the second ingate 310 is higher than that of the first ingate 210; the cast iron gating system 200 includes a cast iron gate 230, a first bottom gate 220, and a second bottom gate 220. The system includes a first straight runner 240 and a first cross runner 250; a cast iron gate 230 is located at the upper part of the first straight runner 240, and the first cross runner 250 is located at the middle part of the first straight runner 240 and is connected to it; the first cross runner 250 is connected to a plurality of first ingates 210; a first sprue 220 is connected to the lower part of the first straight runner 240; the carbon steel gating system 300 includes a carbon steel gate 320, a second straight runner 330 and a second cross runner 340; the second cross runner 340 is located at the middle part of the second straight runner 330 and is connected to it; the second cross runner 340 is connected to a plurality of second ingates 310.

[0045] Specifically, the cast iron gating system 200 uses a bottom-pouring method to pour molten cast iron into the forming cavity 100. After the molten cast iron enters the first straight channel 240 through the cast iron gate 230, a portion of the molten cast iron enters the first bottom gating 220, and another portion enters the first cross channel 250, entering the forming cavity 100 from both directions. Preferably, the first ingate 210 can be set as a wedge shape, so that the liquid discharge speed is faster, thereby continuously flushing the molten cast iron entering the forming cavity 100 and removing the oxidized parts; the carbon steel gating system 300... The injection position is higher than the cast iron gating system 200. After the carbon steel liquid is introduced into the second direct channel 330 from the carbon steel gate 320, it flows through the second cross channel 340 and then enters the forming cavity 100 through the second ingate 310. Preferably, the second cross channel 340 is relatively deep, which slows down the flow rate of the carbon steel liquid entering the second cross channel 340. The specific gravity difference is used to make the slag and impurities float up and remain at the top of the second cross channel 340. The second ingate 310 is relatively wide, which increases the flow rate of the carbon steel liquid entering the forming cavity 100 and realizes rapid stamping.

[0046] In this design, the molding cavity 100 is provided with a first overflow groove 110 and a second overflow groove 120; the first overflow groove 110 is located at the upper part of the first crossflow channel 250 and communicates with the molding cavity 100; the second overflow groove 120 is located at the lower part of the second crossflow channel 340 and communicates with the molding cavity 100; the upper parts of the first overflow groove 110 and the second overflow groove 120 are respectively provided with multiple vent holes; multiple temperature measuring couplers 130 are respectively inserted into the first overflow groove 110 and the second overflow groove 120.

[0047] Specifically, the second overflow tank 120 is used to collect the overflow oxidized portion of the molten iron in the forming cavity 100, and to guide and vent the molten iron through the vent hole at the top of the second overflow tank 120, ensuring that the molten iron entering the forming cavity 100 is pure and has a uniform temperature. At the same time, the temperature in the second overflow tank 120 is monitored by the thermocouple 130, thereby predicting the solidification process of the molten iron. Furthermore, the scum and oxides in the second overflow tank 120 are located in the upper part of the molten iron, which has the function of riser feeding when the molten iron in the lower part solidifies.

[0048] The first overflow tank 110 is used to collect oxide scale and slag in the molten carbon steel. It is also equipped with an exhaust port and a thermocouple 130 to contact the overflowing molten carbon steel at the first moment and monitor its temperature, thereby predicting the solidification process of the molten carbon steel.

[0049] In this design, a feeding riser 140 is provided at the top of the forming cavity 100. Two feeding operations are performed when pouring molten carbon steel. The first operation assists in the pouring when the molten carbon steel reaches 95% of its pouring mass, ensuring that the top of the forming cavity 100 is completely filled. The second operation is performed after the pouring is completed, further enhancing the feeding effect.

[0050] Preferably, the first ingate 210, the sprue, and the second ingate 310 are each provided with a ceramic filter plate. The ceramic filter plate filters the molten metal, which can perform slag blocking and rectification, and reduce the turbulence effect of the molten metal.

[0051] This solution also provides a bimetallic wear-resistant liner plate cast by the above-mentioned plateless casting device, including a wear-resistant layer 400 and a toughness layer 500; the thickness of the wear-resistant layer 400 accounts for 40%-55% of the total thickness; the thickness of the toughness layer 500 accounts for 45%-60% of the total thickness; the bonding surfaces of the wear-resistant layer 400 and the toughness layer 500 are parallel to each other.

[0052] The molding process using this device is as follows:

[0053] First, the high-chromium cast iron is smelted: In a medium-frequency induction furnace, scrap steel and ferromolybdenum are added to the bottom of the furnace and melted by electricity. Then, high-carbon ferrochrome and an appropriate amount of low-carbon ferrochrome are added to adjust the composition. When all of them have melted and the furnace temperature has risen to 1400~1450℃, ferromanganese, electrolytic nickel and the required copper are added in sequence. After melting evenly, rare earth ferrosilicon is used for treatment and aluminum blocks are added for final deoxidation and slag removal. After settling, the high-chromium cast iron is tapped from the furnace at a temperature of 1380~1430℃ and then cooled in the ladle to the target pouring temperature of 1400±30℃ for later use. Carbon steel smelting is carried out in another medium-frequency furnace: first, ultra-low carbon scrap steel is added and melted, then pig iron and ferromanganese are added, and the temperature is raised to 1600~1630℃. After that, aluminum blocks are used to fully deoxidize and remove slag, and the furnace temperature is controlled at 1580~1620℃. After being transferred to a ladle and cooled, it is ready to be cast at the target temperature of 1560~1580℃.

[0054] Before casting, the forming cavity 100 needs to be preheated to approximately 80-100℃. During casting, molten high-chromium cast iron is first poured into the forming cavity 100 through the cast iron gating system 200 at a flow rate of approximately 1.5~5 kg / s. During the casting process, a thermocouple 130 is used to monitor the temperature change in real time, with a focus on the solidification process of the wear-resistant layer.

[0055] A portion of the molten cast iron, after being filtered through a ceramic filter plate, smoothly enters the molding cavity 100 from the first bottom gating 220. Simultaneously, another portion of the molten cast iron enters the molding cavity 100 from the first inner gating 210. Due to the faster flow rate of this portion of molten cast iron, excess molten cast iron, surface oxide scale, slag, etc., flow into the second overflow tank 120. At the same time, the vent is opened, resulting in rapid filling and a regular flow direction within the molding cavity 100. Once it enters the semi-solid zone (temperature drops to 1195~1215℃, solid fraction approximately 40%-60%), within a time window of approximately 60 to 150 seconds after the initial pouring, molten carbon steel is rapidly poured into the carbon steel gating system 300 at a flow rate of approximately 1.5~5 kg / s.

[0056] Molten carbon steel is poured in through carbon steel gate 320, filtered by ceramic filter plate, and then enters molding cavity 100 through second inner gating 310, flushing oxide scale, slag, etc. into first overflow tank 110.

[0057] After casting, closely monitor the solidification of the riser. The first overflow groove 110 and the second overflow groove 120 can play a feeding role during solidification, and feeding is performed twice during solidification: the first time is when the carbon steel liquid is poured to 95% of its volume, molten steel at 1600℃ is poured in through the feeding riser 140; the second time is when the root of the feeding riser 140 solidifies to about 20% solids. After the entire casting is cooled and held in the sand mold, it is opened to obtain the blank casting. When the blank temperature is slowly cooled to 100-150℃, the cast iron gating system 200, the carbon steel gating system 300 and the feeding riser 140 are removed, and the cut parts are ground and cleaned to obtain the final as-cast liner. If necessary, stress-relieving annealing can be performed.

[0058] This solution has at least the following beneficial effects:

[0059] This solution provides a diaphragmless casting device for bimetallic wear-resistant liners. By optimizing the structural and process parameters of the cast iron and carbon steel casting systems, it achieves efficient and high-quality composite molding of high-chromium cast iron and carbon steel. The resulting bimetallic wear-resistant liners possess both excellent wear resistance and toughness, effectively extending their service life. This reduces the increased labor intensity and prolonged equipment downtime caused by frequent liner replacements, while also lowering maintenance costs and significantly improving the working efficiency and economic benefits of ball mills in corrosive slurry environments.

[0060] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this utility model, and not to limit it. Although the utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this utility model.

Claims

1. A plateless casting apparatus for bimetallic wear-resistant liners, characterized in that, It includes a forming cavity (100), a cast iron gating system (200), and a carbon steel gating system (300). The cast iron gating system (200) and the carbon steel gating system (300) are respectively disposed on both sides of the forming cavity (100); The cast iron gating system (200) is connected to the side of the forming cavity (100) through the first ingate (210) and to the bottom of the forming cavity (100) through the first bottom gate (220); The carbon steel gating system (300) is connected to the side of the forming cavity (100) through the second ingate (310); The second ingate (310) is at a higher level than the first ingate (210).

2. A plateless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 1, characterized in that, The cast iron gating system (200) includes a cast iron gating gate (230), a first straight flow channel (240), and a first cross flow channel (250). The cast iron gate (230) is located at the upper part of the first direct current channel (240). The first crossflow channel (250) is located in the middle of the first direct flow channel (240) and is connected to it; The first cross runner (250) is connected to a plurality of first ingates (210); The first bottom gating (220) is connected to the lower part of the first straight gating (240).

3. A plateless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 2, characterized in that, The carbon steel gating system (300) includes a carbon steel gating gate (320), a second straight runner (330), and a second cross runner (340). The second crossflow channel (340) is located at the middle of the second direct flow channel (330) and is connected to it; The second cross runner (340) is connected to a plurality of second ingates (310).

4. A diaphragmless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 3, characterized in that, The molding cavity (100) is provided with a first overflow groove (110) and a second overflow groove (120); The first overflow groove (110) is disposed on the upper part of the first crossflow channel (250) and communicates with the molding cavity (100); The second overflow groove (120) is disposed at the lower part of the second crossflow channel (340) and communicates with the molding cavity (100).

5. A diaphragmless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 4, characterized in that, The upper parts of the first overflow trough (110) and the second overflow trough (120) are respectively provided with multiple vent holes.

6. A diaphragmless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 5, characterized in that, The first overflow trough (110) and the second overflow trough (120) are respectively connected to multiple temperature measuring couplers (130).

7. A diaphragmless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 6, characterized in that, The top of the forming cavity (100) is provided with a feeding riser (140).

8. A diaphragmless casting apparatus for a bimetallic wear-resistant liner includes the bimetallic wear-resistant liner as described in claim 7, characterized in that, The first ingate (210), the bottom gate and the second ingate (310) are respectively provided with ceramic filter plates.

9. A bimetallic wear-resistant liner is cast using a non-partitioned casting apparatus for bimetallic wear-resistant liners as described in any one of claims 1-8, characterized in that, It includes a wear-resistant layer (400) and a toughness layer (500); the thickness of the wear-resistant layer (400) accounts for 40%-55% of the total thickness; the thickness of the toughness layer (500) accounts for 45%-60% of the total thickness; the bonding surfaces of the wear-resistant layer (400) and the toughness layer (500) are parallel to each other.