A multilayer composite material
By introducing a three-dimensional interwoven intermediate mixing layer and an ultrafine fiber coating structure into wood pulp meltblown composites, the problems of weak interlayer bonding and poor water absorption are solved, thereby improving the material's fluffiness, softness, and liquid absorption performance.
Patent Information
- Application Number
- CN202522057568.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-09-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-09-24
AI Technical Summary
Existing wood pulp meltblown composite materials suffer from weak interlayer bonding, dense structure, poor fluffiness and softness due to the independent molding of the meltblown layer and the wood pulp layer. The wood pulp is unevenly distributed, the surface meltblown layer is too dense, and the water absorption is poor.
The structure is made of a multi-layer composite material, consisting of a surface layer, at least two intermediate mixed layers and a bottom layer. The intermediate mixed layers are formed by the interlacing of wood pulp fibers and microfibers to form a three-dimensional interwoven structure. The microfibers of the surface layer and the bottom layer cover the intermediate mixed layers and are solidified by hot rolling process to form an integrated structure.
It improves the interlayer bonding strength, enhances the fluffiness, softness and water absorption of the material, solves the problems of traditional products such as tight structure, stiff feel and poor water absorption, and enhances the overall structural stability and liquid absorption performance of the material.
Smart Images

Figure CN224979326U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of nonwoven fabric technology, and in particular to a multilayer composite material. Background Technology
[0002] In existing wood pulp meltblown composite material manufacturing technologies, a three-layer structure design of "meltblown-wood pulp-meltblown" is commonly used. This type of material is usually made by separately molding the meltblown layer and the wood pulp layer, and then combining the two.
[0003] Because the meltblown layer and the wood pulp layer are formed independently and then composited, the interlayer bonding is weak, resulting in insufficient overall structural density. This leads to a lack of fluffiness and softness in the final fabric, resulting in a poor user experience. Secondly, the overall thickness of the material is relatively thin, making it difficult to meet the requirements of applications demanding high fluffiness and a three-dimensional structure. Furthermore, during the molding process of the wood pulp layer, the uneven distribution of wood pulp fibers easily leads to agglomeration or voids, severely affecting the material's uniformity, strength, and liquid absorption properties. Moreover, the meltblown material used as the surface layer is usually too dense, creating high surface resistance that significantly hinders the rapid penetration and absorption of liquids, resulting in poor overall water absorption of the composite material and failing to leverage the excellent water absorption characteristics that the wood pulp layer should possess. Summary of the Invention
[0004] This invention provides a multilayer composite material to overcome the technical problems of existing wood pulp meltblown composite materials, which have weak interlayer bonding, dense structure, poor fluffiness and softness due to the independent molding of the meltblown layer and the wood pulp layer, and uneven distribution of wood pulp and excessively dense surface meltblown layer, resulting in poor water absorption.
[0005] To achieve the above objectives, the technical solution of this utility model is as follows: A multilayer composite material is composed of a top layer, at least two intermediate mixing layers and a bottom layer stacked sequentially; wherein, the intermediate mixing layers are composed of wood pulp fibers and ultrafine fibers interlaced and distributed in a three-dimensional interwoven pattern in space; the ultrafine fibers of the top layer and the bottom layer cover and partially embed in the intermediate mixing layers to form an integrated structure.
[0006] Furthermore, the angle between the overall laying direction of the ultrafine fibers in the intermediate mixing layer and the running direction of the web forming curtain on the processing machine is the first angle α1, and the overall laying direction of the wood pulp fibers and the running direction of the web forming curtain on the processing machine is the second angle β1; wherein, the first angle α1 and the second angle β1 are different, so that the overall laying directions of the two fiber networks are intersecting.
[0007] Furthermore, the third angle α2 is 100°-150°, the fourth angle β2 is 40°-50°, the fifth angle α3 is 30°-70°, and the sixth angle β3 is 130°-140°.
[0008] Further, the intermediate mixing layer includes a first intermediate mixing layer and a second intermediate mixing layer; the angle between the overall laying direction of the microfibers in the first intermediate mixing layer and the running direction of the web-forming curtain on the processing machine is a third angle α2, and the overall laying direction of the wood pulp fibers and the running direction of the web-forming curtain on the processing machine is a fourth angle β2; the angle between the overall laying direction of the microfibers in the second intermediate mixing layer and the running direction of the web-forming curtain on the processing machine is a fifth angle α3, and the overall laying direction of the wood pulp fibers and the running direction of the web-forming curtain on the processing machine is a sixth angle β3; wherein, the third angle α2 is different from the fourth angle β2, and the fifth angle α3 is different from the sixth angle β3, so that the overall laying directions of the two fiber networks in any intermediate mixing layer are intersecting.
[0009] Furthermore, the third angle α2 is 100°-150°, the fourth angle β2 is 40°-50°, the fifth angle α3 is 30°-70°, and the sixth angle β3 is 130°-140°.
[0010] Furthermore, the microfiber is made of a synthetic polymer.
[0011] Furthermore, the synthetic polymer contains antibacterial and hydrophilic additives.
[0012] Furthermore, the diameter of the ultrafine fibers is 1-5 micrometers.
[0013] Furthermore, the wood pulp fiber accounts for 40%–90% of the mass of the intermediate mixing layer.
[0014] Furthermore, the surface layer, intermediate mixed layer and bottom layer are bonded together by hot rolling process to form hot-rolled bonding points, the single point size of the hot-rolled bonding points is L; the bonding area accounts for the proportion of the total area is W; the range of L is 0.3–1.5 mm, and the range of W is 2%–15%.
[0015] Beneficial effects: This invention features an intermediate composite layer, achieved through the interlacing of wood pulp fibers and microfibers in the intermediate layer, resulting in uniform fiber distribution and a three-dimensional, fluffy structure. The surface and bottom layers, made of microfiber, effectively enhance surface smoothness and suppress lint shedding. Based on this design, the overall structure strengthens interlayer bonding, improving upon the shortcomings of traditional products such as insufficient fluffiness, stiffness, poor water absorption, and lint shedding. This significantly enhances the material's softness, liquid absorption, and user experience. Attached Figure Description
[0016] To more clearly illustrate the technical solutions in the embodiments of this utility model or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0017] Figure 1 This is a schematic diagram of the structure of this utility model; In the diagram: 1: Top layer; 2: First intermediate mixing layer; 3: Second intermediate mixing layer; 4: Bottom layer. Detailed Implementation
[0018] To make the objectives, technical solutions, and advantages of the embodiments of this utility model clearer, the technical solutions of the embodiments of this utility model will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this utility model, not all embodiments. Based on the embodiments of this utility model, all other embodiments obtained by those skilled in the art without creative effort are within the protection scope of this utility model.
[0019] This embodiment provides a multilayer composite material, such as Figure 1 As shown, it is composed of a surface layer 1, at least two intermediate mixing layers and a bottom layer 4 stacked in sequence; wherein, the intermediate mixing layer is composed of wood pulp fibers and microfibers interlaced and distributed in a three-dimensional interwoven pattern in space; the microfibers of the surface layer 1 and the bottom layer 4 cover and partially embed in the intermediate mixing layer to form an integrated structure.
[0020] The intermediate mixed layer is composed of interwoven wood pulp fibers and microfibers, which are distributed in a three-dimensional interweaving pattern. Both the top and bottom layers are made of microfibers, forming an upper and lower covering structure for the intermediate mixed layer. This structure, through the three-dimensional interweaving of wood pulp fibers and microfibers in the intermediate mixed layer, improves the uniformity of fiber distribution and the three-dimensional bulkiness of the material. The microfiber covering structure of the top layer 1 and bottom layer 4 enhances the surface smoothness and effectively reduces shedding, while also improving interlayer bonding, giving the material good water absorption, a soft feel, and structural integrity.
[0021] Furthermore, when the structures of the intermediate mixing layers are identical, the ultrafine fibers in the intermediate mixing layers are laid on the formed mesh curtain at an angle of 100°-150° (relative to the direction of mesh curtain operation); the wood pulp fibers, after being crushed by a crusher, are conveyed by airflow and sprayed onto the ultrafine fiber layer at an angle of 40°-50°, where they interweave to form a three-dimensional cross-network structure and are deposited on the formed mesh curtain. Alternatively, the ultrafine fibers in the intermediate mixing layers are laid on the formed mesh curtain at an angle of 30°-70°, and the wood pulp fibers are sprayed onto the fiber layer by airflow at an angle of 130°-140°, where they interweave to form a three-dimensional cross-network structure.
[0022] Furthermore, when the structures of the intermediate mixing layers differ, the intermediate mixing layers include a first intermediate mixing layer 2 and a second intermediate mixing layer 3. In the first intermediate mixing layer 2, the ultrafine fibers are laid on the formed mesh curtain at an angle of 100°-150° (relative to the direction of mesh curtain operation). The wood pulp fibers, after being crushed by a crusher, are conveyed by airflow and sprayed onto the ultrafine fiber layer at an angle of 40°-50°, where they interlock and overlap to form a three-dimensional cross-network structure, which is then deposited onto the formed mesh curtain. In the second intermediate mixing layer 3, the ultrafine fibers are laid on the formed mesh curtain at an angle of 30°-70°, and the wood pulp fibers are sprayed onto the fiber layer by airflow at an angle of 130°-140°, where they interlock and overlap to form a cross-network structure with another orientation. In each intermediate mixing layer, the mass ratio of wood pulp fibers is 40%-90%. By controlling the laying angles of the ultrafine fibers and wood pulp fibers in different intermediate mixing layers, the fiber network forms an orderly, interlocking three-dimensional structure in multiple directions, improving the overall strength and structural stability of the material. Meanwhile, the multi-angle cross-overlapping expands the pore space between fibers, which is conducive to the rapid penetration and multi-directional diffusion of liquids, and improves the bulkiness and resilience of the material.
[0023] Specifically, in the process corresponding to the multilayer composite material described in this utility model, the weight of the intermediate mixing layer can be set to 25 g / m², composed of 7 g / m polypropylene and 18 g / m fluff pulp (wood pulp fiber), and is formed and composited in two separate upper and lower layers. During the upper layer forming process, the polypropylene is melted by a screw extruder to form a high-viscosity melt, which then enters the spinning die assembly. The spinning die and the forming mesh are arranged at a 135° angle, and the melt is stretched into ultrafine fibers under the stretching action of the high-temperature airflow. At the same time, the wood pulp fiber is broken down into single fibers by a crusher and blown into the forming ultrafine fiber web at a 45° angle through a fan and conveying pipe. The fibers are fully cross-mixed with the ultrafine fibers under the action of the airflow and are laid together on the forming mesh to form a uniform fiber web structure. The fan operating speed is set to 1500 rpm, 1550 rpm, 1600 rpm, and 1650 rpm to adjust the fiber dispersion and conveying effect. In the lower layer forming process, polypropylene is also extruded by a screw to form a high-viscosity melt, which then enters another spinning die assembly. This die is at a 48° angle to the forming mesh, and under the stretching action of a high-temperature airflow, it forms ultrafine fibers. After being crushed and dispersed, the fluff pulp is also blown onto this layer of ultrafine fiber mesh at a 134° angle via a fan and conveying pipe, achieving cross-mixing and composite web formation of the two types of fibers. The fan speed for this layer is set at 1550 rpm, 1620 rpm, 1650 rpm, and 1710 rpm to optimize fiber transport and distribution uniformity. The two layers are continuously composited on the forming mesh, ultimately forming a multilayer fiber material with specific structure and properties.
[0024] Furthermore, the top layer 1 and the bottom layer 4 are ultrafine fiber layers made of polypropylene through melt spinning.
[0025] The ultrafine fibers are ultrafine fiber layers made of polypropylene through melt spinning. The fiber diameter is 1-5 micrometers, and the unit area mass is set at 2-8 gsm, which is conducive to forming a dense and uniform fiber web, improving the surface smoothness of the material and effectively blocking liquid side leakage. The fiber layer contains 5% silver-loaded zeolite antibacterial masterbatch and 5% polyethylene glycol hydrophilic masterbatch, which are evenly distributed on the fiber surface. This can give the material long-lasting antibacterial properties, improve the wettability of the fiber surface, promote rapid liquid penetration, and synergistically improve the safety and water absorption efficiency of the material.
[0026] Specifically, the top layer has a basis weight of 5 gsm and uses 90% high melt index isotactic polypropylene as the base material, combined with 5% antibacterial masterbatch and 5% hydrophilic masterbatch. After thorough mixing, it enters the screw extruder. The screw extruder has six heating zones, with temperatures set sequentially to 220℃, 230℃, 235℃, 240℃, 240℃, and 240℃ to ensure uniform plasticization of the material. The melt enters the spinning die (die temperature maintained at 240℃), where it is stretched into ultrafine fibers by high-speed airflow under the action of high-temperature drawing air (air temperature 245℃), and directly laid on the forming screen to form a surface structure with excellent hydrophilicity, antibacterial properties, and a soft surface. The bottom layer also has a basis weight of 5 gsm, and the material formulation is the same as the top layer, namely, 90% high melt index isotactic polypropylene, 5% antibacterial masterbatch, and 5% hydrophilic masterbatch are mixed evenly before entering the screw extruder. The extrusion process has six temperature zones set at 220℃, 230℃, 235℃, 250℃, 250℃, and 250℃, with the die temperature also set at 250℃, to accommodate material flowability and fiber forming requirements. The fibers are spun through the die and stretched under high-temperature airflow to form ultrafine fibers, which are then laid up to form a bottom layer that is functionally symmetrical and structurally complete with the surface layer.
[0027] Furthermore, the surface layer 1, the intermediate mixing layer, and the bottom layer 4 are bonded together by a hot rolling process, with the mill temperature set at 100°C. The hot rolling employs a dotted or linear pattern, forming hot-rolled bonding points. The width of each point is 0.3-1.5 mm, and the bonded area accounts for 2%-15% of the total area. This dotted or linear hot-rolled pattern effectively bonds the layers while further optimizing stress distribution, reducing stress concentration, and avoiding the stiffness caused by large-scale pressing. The smaller size of each point helps to evenly distribute the bonding points within a limited bonding area, improving the overall stability and consistency of the bond.
[0028] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of this utility model, and are not intended to limit it. Although the utility model has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this utility model.
Claims
1. A multilayer composite material, characterized in that: It is composed of a surface layer (1), at least two intermediate mixed layers and a bottom layer (4) stacked in sequence; wherein, the intermediate mixed layer is composed of wood pulp fibers and microfibers interlaced and distributed in a three-dimensional interwoven manner in space; the microfibers of the surface layer (1) and the bottom layer (4) cover and partially embed the intermediate mixed layer to form an integrated structure.
2. The multilayer composite material according to claim 1, characterized in that: The angle between the overall laying direction of the ultrafine fibers in the intermediate mixing layer and the running direction of the netting curtain on the processing machine is the first angle α1, and the overall laying direction of the wood pulp fibers and the running direction of the netting curtain on the processing machine is the second angle β1; wherein, the first angle α1 and the second angle β1 are different, so that the overall laying directions of the two fiber networks are intersecting.
3. The multilayer composite material according to claim 2, characterized in that: The first angle α1 is 100°-150° and the second angle β1 is 40°-50°, or the first angle α1 is 30°-70° and the second angle β1 is 130°-140°.
4. The multilayer composite material according to claim 1, characterized in that: The intermediate mixing layer includes a first intermediate mixing layer (2) and a second intermediate mixing layer (3); the angle between the overall laying direction of the ultrafine fibers in the first intermediate mixing layer (2) and the running direction of the web forming curtain on the processing machine is a third angle α2, and the overall laying direction of the wood pulp fibers and the running direction of the web forming curtain on the processing machine is a fourth angle β2; the angle between the overall laying direction of the ultrafine fibers in the second intermediate mixing layer (3) and the running direction of the web forming curtain on the processing machine is a fifth angle α3, and the overall laying direction of the wood pulp fibers and the running direction of the web forming curtain on the processing machine is a sixth angle β3; wherein, the third angle α2 is different from the fourth angle β2, and the fifth angle α3 is different from the sixth angle β3, so that the overall laying directions of the two fiber networks in any intermediate mixing layer are intersecting.
5. A multilayer composite material according to claim 4, characterized in that: The third angle α2 is 100°-150°, the fourth angle β2 is 40°-50°, the fifth angle α3 is 30°-70°, and the sixth angle β3 is 130°-140°.
6. A multilayer composite material according to claim 1, characterized in that: The microfibers are made from synthetic polymers.
7. A multilayer composite material according to claim 6, characterized in that: The synthetic polymer contains antibacterial and hydrophilic additives.
8. A multilayer composite material according to claim 1 or 2, characterized in that: The diameter of the ultrafine fibers is 1-5 micrometers.
9. A multilayer composite material according to claim 1, characterized in that: The mass proportion of wood pulp fiber in the intermediate mixing layer is 40%–90%.
10. A multilayer composite material according to claim 1, characterized in that: The surface layer (1), intermediate mixed layer and bottom layer (4) are bonded together by hot rolling process and form hot rolled bonding points. The single point size of the hot rolled bonding point is L; the bonding area accounts for the proportion of the total area to W; the range of L is 0.3–1.5 mm and the range of W is 2%–15%.