A novel welding structure for ceramic pressure sensor welding pins
By using a welding structure of tin ring and bimetallic mechanical compensation ring, the problem of weld pin detachment caused by welding gaps and temperature changes is solved, achieving high stability and reliability of ceramic pressure sensors and adapting to wide temperature range operation.
Patent Information
- Application Number
- CN202522272575.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-28
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-10-28
AI Technical Summary
The existing welding method for ceramic pressure sensors is prone to gaps at the connection between the welding pin and the pad due to excessive flux ratio, and the pin is easily detached under thermal shock, affecting the stability and reliability of the sensor.
The welding structure employs a tin ring and a bimetallic mechanical compensation ring. The tin ring reduces voids through precise dimensional matching and a low flux ratio, while the bimetallic compensation ring compensates for temperature changes through the difference in thermal expansion coefficients, ensuring the strength of the weld and the stability of the electrical connection.
It significantly improves the production yield of ceramic pressure sensor modules, enhances welding strength and resistance to thermal shock, widens the operating temperature range, and improves the environmental adaptability and reliability of the sensor.
Smart Images

Figure CN224984964U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of welding structure technology, and in particular to a novel welding structure for a ceramic pressure sensor welding needle. Background Technology
[0002] The ceramic pressure sensor module is mainly composed of a ceramic substrate and a ceramic strain gauge. The ceramic substrate has through holes, and welding pins that are welded to the pads of the ceramic strain gauge are installed through the through holes.
[0003] The current soldering method involves applying solder paste into the through-hole, inserting solder pins, and then reflow soldering. Generally, to maintain good fluidity of the solder paste, the flux content in the solder paste is between 16% and 20%. However, flux increases the volume shrinkage of the solder paste after curing, resulting in more gaps at the connection between the solder pins and the pads. After being subjected to thermal shock, the solder pins are prone to detaching from the pads, leading to abnormal pressure sensor output. Utility Model Content
[0004] The purpose of this utility model is to solve the technical problems mentioned in the background section.
[0005] The present invention adopts the following technical solution: a novel welding structure for a ceramic pressure sensor welding needle, comprising a ceramic substrate, wherein a ceramic strain gauge is fixedly mounted on the bottom of the ceramic substrate by means of glass slurry, the ceramic substrate is provided with a through hole, and a tin ring and a welding needle body are sequentially arranged in the through hole, and a bimetallic mechanical compensation ring is installed between the tail of the welding needle body and the ceramic substrate.
[0006] Preferably, the inner diameter of the tin ring matches the outer diameter of the solder pin body, and the outer diameter of the tin ring matches the inner diameter of the through-hole in the ceramic substrate. This precise dimensional fit ensures the tin ring functions effectively during the soldering process. Firstly, it guarantees the installation accuracy of the solder pin body within the through-hole, preventing pin movement or misalignment, thus ensuring accurate connection between the solder pin and the ceramic strain gauge pad. Secondly, the appropriate dimensional fit facilitates uniform heating and melting of the tin ring during reflow soldering, resulting in good weld filling within the through-hole, reducing weld voids, improving weld strength and electrical connection stability, and lowering the probability of soldering defects such as cold solder joints and solder detachment.
[0007] Preferably, the glass slurry is used to fix the ceramic substrate and ceramic strain gauge into a semi-finished structure via a reflow soldering process. Here, using a reflow soldering process to solidify the glass slurry and fix the ceramic substrate and ceramic strain gauge into a semi-finished structure offers several advantages. The reflow soldering process allows for precise temperature control, ensuring that the glass slurry melts uniformly at a specific temperature and fully wets the connection surfaces of the ceramic substrate and ceramic strain gauge, ensuring a strong and stable connection. Compared to other connection methods, such as manual welding, this process offers higher consistency and reliability, guaranteeing that the connection quality of each semi-finished structure meets standards. This facilitates large-scale production, improving production efficiency while enhancing the overall quality of the product.
[0008] Preferably, the bimetallic mechanical compensation ring is in a straight state at room temperature, maintaining a pre-tight connection between the welding needle body and the ceramic substrate. This pre-tight connection ensures a stable and reliable electrical connection between the welding needle and the ceramic substrate when the sensor is not in operation or at room temperature, preventing poor contact caused by vibration, minor external forces, or other factors. Simultaneously, the pre-tightening force provides the initial conditions for the bimetallic mechanical compensation ring to perform its compensating function during temperature changes, ensuring that the entire welding structure maintains good performance under different operating conditions.
[0009] Preferably, the inner brass layer of the bimetallic mechanical compensation ring, due to its higher coefficient of thermal expansion than the outer Invar layer, bends towards the ceramic substrate, causing a slight axial contraction of the welding needle body (compensation amount ≤ +0.15mm). Here, when the temperature changes, the inner brass layer of the bimetallic mechanical compensation ring, due to its higher coefficient of thermal expansion than the outer Invar layer, bends towards the ceramic substrate, causing a slight axial contraction of the welding needle body (compensation amount ≤ +0.15mm). In practical applications, due to the differences in the coefficients of thermal expansion of materials such as the ceramic substrate and the welding needle body, the degree of expansion of each component varies with temperature increases, which may lead to thermal stress at the welding site, affecting the stability of the welding and the performance of the sensor. This characteristic of the bimetallic mechanical compensation ring can effectively compensate for dimensional changes caused by temperature increases, adjust the position of the welding needle body through its own deformation, alleviate thermal stress, ensure good contact between the welding needle and the ceramic strain gauge pad, and maintain the normal operation of the sensor in high-temperature environments.
[0010] Preferably, the bimetallic mechanical compensation ring bends towards the metal side, pushing the welding needle body to extend slightly axially (compensation amount ≥ -0.15mm), maintaining the stress fluctuation at the interface between the welding needle body and the ceramic substrate ≤ ±5MPa. Here, the bimetallic mechanical compensation ring bends towards the metal side, pushing the welding needle body to extend slightly axially (compensation amount ≥ -0.15mm), maintaining the stress fluctuation at the interface between the welding needle body and the ceramic substrate ≤ ±5MPa. When the temperature decreases, the components shrink, which may loosen the connection between the welding needle and the ceramic substrate, reducing the interface stress. The bimetallic mechanical compensation ring bends towards the metal side at this time, pushing the welding needle body to extend slightly, which can effectively maintain the appropriate stress between the welding needle and the ceramic substrate, avoiding damage to the welding structure due to excessive stress changes, ensuring the normal operation of the sensor in low-temperature environments, widening the sensor's operating temperature range, and improving its adaptability and reliability under different temperature conditions.
[0011] Preferably, the thickness of the bimetallic mechanical compensation ring is 0.08 mm, achieving dynamic compensation for thermal stress through elastic deformation. Here, the thickness of the bimetallic mechanical compensation ring is 0.08 mm, achieving dynamic compensation for thermal stress through elastic deformation. The thinner thickness gives the bimetallic mechanical compensation ring high elasticity, allowing it to deform significantly even with small temperature changes, responding promptly to dimensional differences caused by temperature variations. Within different temperature ranges, it can continuously adjust its shape according to real-time temperature changes, dynamically compensating for thermal stress and ensuring the welded structure remains in good working condition. Moreover, compared to other rigid structure compensation methods, this elastic deformation method can more effectively absorb and buffer thermal stress, reducing the adverse effects of thermal stress on the welded parts and the entire sensor structure.
[0012] Preferably, the flux ratio of the solder ring is lower than that of traditional solder paste, and the volume shrinkage rate after reflow soldering is ≤5%, reducing the gap at the connection between the solder pin body and the pad. Here, the lower flux ratio of the solder ring compared to traditional solder paste, and the ≤5% volume shrinkage rate after reflow soldering, effectively reduces the gap at the connection between the solder pin body and the pad. Traditional solder paste, due to its higher flux ratio and other factors, may experience significant volume shrinkage after curing during reflow soldering, resulting in numerous gaps between the solder pin and the pad. These gaps not only affect the mechanical strength of the solder joint but may also affect the stability of the electrical connection, increase resistance, and even lead to problems such as cold solder joints. The solder ring design in this structure, by optimizing the flux ratio and reducing the volume shrinkage rate, enables a tighter and more reliable connection during soldering, improving soldering quality and thus enhancing the overall performance and reliability of the sensor.
[0013] Compared with the prior art, the advantages and positive effects of this utility model are as follows:
[0014] 1. In this invention, a solder ring is used as a pre-formed solder, ensuring a fixed amount of solder. This solves the problem of precise quantity control in traditional solder paste, avoiding short circuits due to excessive solder paste and cold solder joints due to insufficient solder paste, significantly improving the production yield of ceramic pressure sensor modules. Its low flux ratio and ≤5% volume shrinkage after reflow soldering significantly reduce the gap between the solder pin and the pad, increasing the contact area. Furthermore, the melted ring-shaped solder joint evenly surrounds the solder pin, effectively improving welding strength and resistance to thermal shock, extending product lifespan, and enhancing long-term stability.
[0015] 2. In this utility model, a bimetallic mechanical compensation ring is provided, consisting of an outer layer of Invar steel (CTE≈12×10⁻). 6 Composed of a core and an inner brass layer, 0.08mm thick, the sensor's flatness at room temperature ensures pre-tightening between the welding pin and the ceramic substrate, guaranteeing stable electrical contact. At high temperatures, the high expansion rate of brass compensates for the bending of the compensation ring towards the ceramic side, causing the welding pin to shrink slightly (≤+0.15mm) and offset the tensile stress caused by the difference in thermal expansion. At low temperatures, the high contraction rate of brass compensates for the bending of the compensation ring towards the metal side, pushing the welding pin to extend slightly (≥-0.15mm) and offset the relaxation stress. Through elastic deformation, the sensor dynamically adjusts the welding pin position, controlling interface stress fluctuations within ≤±5MPa, mitigating thermal stress damage, and allowing the sensor to operate stably over a wide temperature range of -40℃ to +125℃, thus improving environmental adaptability and reliability. Attached Figure Description
[0016] Figure 1 A three-dimensional structural diagram of a novel welding structure for a ceramic pressure sensor welding pin is provided for this utility model.
[0017] Figure 2 An exploded structural diagram of a novel welding structure for a ceramic pressure sensor welding needle is provided for this utility model.
[0018] Figure 3 A schematic diagram of a ceramic substrate structure for a novel welding structure of a ceramic pressure sensor welding pin is provided for this utility model.
[0019] Figure 4 This utility model proposes a novel welding structure for a ceramic pressure sensor welding needle, and presents a schematic diagram of the welding needle body structure.
[0020] Legend:
[0021] 1. Welding pin body; 2. Tin ring; 3. Ceramic substrate; 4. Glass paste; 5. Ceramic strain gauge; 6. Bimetallic mechanical compensation ring. Detailed Implementation
[0022] To better understand the above-mentioned objectives, features, and advantages of this utility model, the present utility model will be further described below with reference to the accompanying drawings and embodiments. It should be noted that, unless otherwise specified, the embodiments and features described in these embodiments can be combined with each other.
[0023] Many specific details are set forth in the following description in order to provide a full understanding of the present invention. However, the present invention may also be implemented in other ways different from those described herein. Therefore, the present invention is not limited to the specific embodiments disclosed in the following specification.
[0024] Example 1
[0025] Please see Figures 1-4 This utility model provides a technical solution: a novel welding structure for a ceramic pressure sensor welding needle, including a ceramic substrate 3, a ceramic strain gauge 5 fixedly mounted on the bottom of the ceramic substrate 3 by a glass slurry 4, a through hole on the ceramic substrate 3, and a tin ring 2 and a welding needle body 1 arranged sequentially in the through hole, and a bimetallic mechanical compensation ring 6 installed between the tail of the welding needle body 1 and the ceramic substrate 3.
[0026] The inner diameter of the solder ring 2 matches the outer diameter of the solder needle body 1, and the outer diameter of the solder ring 2 matches the inner diameter of the through hole in the ceramic substrate 3. This precise dimensional fit ensures that the solder ring 2 functions effectively during the soldering process. Firstly, it guarantees the installation accuracy of the solder needle body 1 within the through hole, preventing the solder needle from shifting or deviating, thus ensuring accurate connection between the solder needle and the ceramic strain gauge 5 pad. Secondly, the appropriate dimensional fit facilitates uniform heating and melting of the solder ring 2 during reflow soldering, resulting in good weld filling within the through hole, reducing weld voids, improving weld strength and electrical connection stability, and lowering the probability of soldering defects such as incomplete soldering or detachment.
[0027] The glass slurry 4 is used in a reflow soldering process to fix the ceramic substrate 3 and ceramic strain gauge 5 into a semi-finished structure. Here, the reflow soldering process is used to solidify the glass slurry 4 and fix the ceramic substrate 3 and ceramic strain gauge 5 into a semi-finished structure, which has several advantages. The reflow soldering process allows for precise temperature control, ensuring that the glass slurry 4 melts uniformly at a specific temperature and fully wets the connection surface between the ceramic substrate 3 and ceramic strain gauge 5, ensuring a strong and stable connection. Compared to other connection methods, such as manual welding, this process offers higher consistency and reliability, guaranteeing that the connection quality of each semi-finished structure meets standards. This is beneficial for large-scale production, improving production efficiency while enhancing the overall quality of the product.
[0028] The bimetallic mechanical compensation ring 6 is in a straight state at room temperature, maintaining a pre-tight connection between the welding needle body 1 and the ceramic substrate 3. This pre-tight connection ensures a stable and reliable electrical connection between the welding needle and the ceramic substrate 3 when the sensor is not in operation or at room temperature, preventing poor contact caused by vibration, minor external forces, or other factors. Simultaneously, the pre-tightening force provides the initial conditions for the bimetallic mechanical compensation ring 6 to perform its compensation function under temperature changes, ensuring that the entire welding structure maintains good performance under different operating conditions.
[0029] The inner brass layer of the bimetallic mechanical compensation ring 6, due to its higher coefficient of thermal expansion than the outer Invar steel layer, bends towards the ceramic substrate 3, causing a slight axial contraction of the welding needle body 1 (compensation amount ≤ +0.15mm). Here, when the temperature changes, the inner brass layer of the bimetallic mechanical compensation ring 6, due to its higher coefficient of thermal expansion than the outer Invar steel layer, bends towards the ceramic substrate 3, causing a slight axial contraction of the welding needle body 1 (compensation amount ≤ +0.15mm). In practical applications, due to the difference in the coefficients of thermal expansion of materials such as the ceramic substrate 3 and the welding needle body 1, the expansion degrees of each component differ when the temperature rises, which may lead to thermal stress at the welding point, affecting the welding stability and sensor performance. This characteristic of the bimetallic mechanical compensation ring 6 can effectively compensate for the dimensional changes caused by temperature increases, adjust the position of the welding needle body 1 through its own deformation, alleviate thermal stress, ensure good contact between the welding needle and the ceramic strain gauge 5 welding pad, and maintain the normal operation of the sensor in high-temperature environments.
[0030] The bimetallic mechanical compensation ring 6 bends towards the metal side, pushing the welding needle body 1 to extend slightly axially (compensation amount ≥ -0.15mm), maintaining the stress fluctuation at the interface between the welding needle body 1 and the ceramic substrate 3 ≤ ±5MPa. Here, the bimetallic mechanical compensation ring 6 bends towards the metal side, pushing the welding needle body 1 to extend slightly axially (compensation amount ≥ -0.15mm), maintaining the stress fluctuation at the interface between the welding needle body 1 and the ceramic substrate 3 ≤ ±5MPa. When the temperature decreases, the components shrink, which may cause the connection between the welding needle and the ceramic substrate 3 to loosen, reducing the interface stress. At this time, the bimetallic mechanical compensation ring 6 bends towards the metal side, pushing the welding needle body 1 to extend slightly, which can effectively maintain the appropriate stress between the welding needle and the ceramic substrate 3, avoiding damage to the welding structure due to excessive stress changes, ensuring the normal operation of the sensor in low-temperature environments, widening the sensor's operating temperature range, and improving its adaptability and reliability under different temperature conditions.
[0031] The bimetallic mechanical compensation ring 6 has a thickness of 0.08 mm and achieves dynamic compensation for thermal stress through elastic deformation. The thinner thickness gives the bimetallic mechanical compensation ring 6 high elasticity, allowing it to deform significantly even with small temperature changes, responding promptly to dimensional differences caused by temperature variations. Within different temperature ranges, it can continuously adjust its shape according to real-time temperature changes, dynamically compensating for thermal stress and ensuring the welded structure remains in good working condition. Moreover, compared to other rigid structure compensation methods, this elastic deformation method can more effectively absorb and buffer thermal stress, reducing the adverse effects of thermal stress on the welded parts and the entire sensor structure.
[0032] The flux ratio of the solder ring 2 is lower than that of traditional solder paste, resulting in a volume shrinkage rate of ≤5% after reflow soldering and curing, thus reducing the gap at the connection between the solder pin body 1 and the pad. Here, the lower flux ratio of the solder ring 2 compared to traditional solder paste, with a volume shrinkage rate of ≤5% after reflow soldering and curing, effectively reduces the gap at the connection between the solder pin body 1 and the pad. Traditional solder paste, due to its higher flux ratio and other factors, may experience significant volume shrinkage after curing during reflow soldering, leading to numerous gaps between the solder pin and the pad. These gaps not only affect the mechanical strength of the solder joint but may also affect the stability of the electrical connection, increase resistance, and even cause problems such as cold solder joints. In this structure, the design of the solder ring 2, by optimizing the flux ratio and reducing the volume shrinkage rate, enables a tighter and more reliable connection during soldering, improving soldering quality and thus enhancing the overall performance and reliability of the sensor.
[0033] Working principle: First, prepare the materials: ceramic substrate 3, glass paste 4, and ceramic strain gauge 5. Ensure the surface of ceramic substrate 3 is clean and free of impurities, and the pads of ceramic strain gauge 5 are accurately positioned. Next, evenly apply glass paste 4 to the area on the bottom of ceramic substrate 3 where the ceramic strain gauge 5 will be fixed, covering the connection surface. Then, place the ceramic substrate 3 coated with glass paste 4 and the ceramic strain gauge 5 into a reflow soldering machine. Sinter the glass paste 4 by setting a precise temperature curve for heating, holding, and cooling according to its curing characteristics, allowing the glass paste 4 to solidify and fixing the two into a firmly connected, electrically stable semi-finished structure. Afterward, install the solder ring 2 and solder pins. First, measure the inner diameter of the through-hole on the ceramic substrate 3 to select a suitable solder ring 2. The outer diameter of the solder ring 2 must be... The solder ring 2 is placed in each of the four through holes of the glass slurry, ensuring it fits snugly against the inner diameter of the through hole and matches the outer diameter of the solder needle body 1. Then, a tin ring 2 is placed completely at the bottom and centered in each of the four through holes. The solder needle body 1 is then vertically inserted into the tin ring 2 within the through hole, leaving space between the tail of the solder needle and the surface of the ceramic substrate 3 for installing a bimetallic compensation ring, thus initially fixing the solder needle to prevent displacement or tilting. Next, the finished product is soldered. First, it is confirmed that the tin ring 2 and solder needle are installed in place. A reflow soldering machine with a temperature profile set higher than the melting point of the tin ring 2 is prepared. The semi-finished product with the assembled tin ring 2 and solder needle is then placed into the machine, allowing the tin ring 2 to melt at high temperature. Flux assists in the soldering process, forming annular solder joints that fill the gaps. Because the tin ring 2 has a low flux ratio and a volume shrinkage rate of ≤5%, it reduces solder joint gaps and improves solderability. After welding, the weld is allowed to cool naturally or forcibly to room temperature. A preliminary inspection is performed to check for any incomplete welds or detachments, ensuring a reliable connection between the welding needle and the ceramic strain gauge 5 pad. Then, the bimetallic mechanical compensation ring 6 is installed. A bimetallic mechanical compensation ring 6, with an outer layer of Invar and an inner layer of brass, 0.08mm thick, and straight at room temperature to ensure a pre-tight connection between the welding needle and the ceramic substrate 3, is prepared. The compensation ring is embedded in the gap between the tail of the welding needle body 1 and the ceramic substrate 3, ensuring a tight fit without misalignment with the tail of the welding needle and the surface of the ceramic substrate 3. In high-temperature environments, the high expansion rate of the brass layer causes the compensation ring to bend towards the ceramic side, pulling the welding needle axially slightly (compensation amount ≤ +0.15mm), offsetting the tensile stress caused by the difference in thermal expansion between the metal and ceramic. Under warm conditions, the high shrinkage rate of the brass layer causes the compensation ring to bend towards the metal side, pushing the welding pin to extend slightly axially (compensation amount ≥ -0.15mm), offsetting the relaxation stress caused by shrinkage, and ultimately maintaining the interface stress fluctuation ≤ ±5MPa, ensuring the stability of the sensor in a wide temperature range; finally, finished product testing and performance verification are carried out. Visual inspection and X-ray inspection are used to confirm that there are no gaps in the solder joints and the welding pin position is accurate. The electrical conductivity between the welding pin and the ceramic strain gauge 5 is tested. The axial displacement of the welding pin and the interface stress change are monitored in a high and low temperature cycling environment of -40℃ to +125℃ to verify whether the compensation amount and stress fluctuation meet the standards, evaluate the life and long-term stability of the sensor under thermal shock, and confirm the comprehensive effect of the tin ring 2 welding and bimetallic strip compensation.
[0034] The above description is merely a preferred embodiment of the present utility model and is not intended to limit the present utility model in any other way. Any person skilled in the art may make changes or modifications to the above-disclosed technical content to create equivalent embodiments for application in other fields. However, any simple modifications, equivalent changes, and modifications made to the above embodiments based on the technical essence of the present utility model without departing from the technical solution of the present utility model shall still fall within the protection scope of the technical solution of the present utility model.
Claims
1. A novel welding structure for a ceramic pressure sensor welding pin, comprising a ceramic substrate (3), characterized in that: A ceramic strain gauge (5) is fixedly installed on the bottom of the ceramic substrate (3) by glass paste (4). The ceramic substrate (3) has a through hole, and a tin ring (2) and a welding needle body (1) are arranged in sequence in the through hole. A bimetallic mechanical compensation ring (6) is installed between the tail of the welding needle body (1) and the ceramic substrate (3).
2. The novel welding structure of a ceramic pressure sensor welding pin according to claim 1, characterized in that: The inner diameter of the tin ring (2) matches the outer diameter of the solder needle body (1), and the outer diameter of the tin ring (2) matches the inner diameter of the through hole of the ceramic substrate (3).
3. The novel welding structure of a ceramic pressure sensor welding pin according to claim 1, characterized in that: The glass slurry (4) is used to fix the ceramic substrate (3) and ceramic strain gauge (5) into a semi-finished structure through a reflow soldering process.
4. The novel welding structure of a ceramic pressure sensor welding pin according to claim 1, characterized in that: The bimetallic mechanical compensation ring (6) is in a straight state at room temperature, so that the welding needle body (1) and the ceramic substrate (3) are pre-tightly connected.
5. The novel welding structure of a ceramic pressure sensor welding pin according to claim 1, characterized in that: The inner brass of the bimetallic mechanical compensation ring (6) has a higher expansion rate than the outer Invar steel, so it bends toward the ceramic substrate (3) and pulls the welding needle body (1) to shrink axially (compensation amount ≤ +0.15mm).
6. The novel welding structure of a ceramic pressure sensor welding pin according to claim 1, characterized in that: The bimetallic mechanical compensation ring (6) bends toward the metal side, pushing the welding needle body (1) to extend slightly axially (compensation amount ≥ -0.15mm), maintaining the stress fluctuation at the interface between the welding needle body (1) and the ceramic substrate (3) ≤ ±5MPa.
7. The novel welding structure of a ceramic pressure sensor welding pin according to claim 6, characterized in that: The thickness of the bimetallic mechanical compensation ring (6) is 0.08 mm, and it achieves dynamic compensation for thermal stress through elastic deformation.
8. The novel welding structure of a ceramic pressure sensor welding pin according to claim 6, characterized in that: The flux ratio of the tin ring (2) is lower than that of traditional solder paste, and the volume shrinkage rate after reflow soldering is ≤5%, which reduces the gap between the solder pin body (1) and the solder pad.